{"id":225544,"date":"2021-08-05T08:11:27","date_gmt":"2021-08-05T00:11:27","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=225544"},"modified":"2021-08-05T08:11:27","modified_gmt":"2021-08-05T00:11:27","slug":"nature%e6%97%a0%e5%ba%8f%e9%87%91%e5%b1%9e%e6%8e%ba%e6%9d%82%e5%bc%95%e8%b5%b7%e7%9a%84%e6%99%b6%e4%bd%93%e7%bb%9d%e7%bc%98%e4%bd%93%e4%b8%ad%e7%9a%84%e8%b5%9d%e8%83%bd%e9%9a%99","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=225544","title":{"rendered":"Nature:\u65e0\u5e8f\u91d1\u5c5e\u63ba\u6742\u5f15\u8d77\u7684\u6676\u4f53\u7edd\u7f18\u4f53\u4e2d\u7684\u8d5d\u80fd\u9699"},"content":{"rendered":"<p><strong><b>\u3010\u5f15\u8a00\u3011<\/b><\/strong><\/p>\n<p>\u57281960\u5e74\u4ee3\uff0c\u5bf9\u6db2\u6001\u91d1\u5c5e\u7684\u80fd\u5e26\u7ed3\u6784\u8fdb\u884c\u4e86\u4e00\u7cfb\u5217\u5f00\u521b\u6027\u7684\u7406\u8bba\u7814\u7a76\u3002\u5c31\u50cf\u73bb\u7483\u6750\u6599\u5177\u6709\u660e\u786e\u5b9a\u4e49\u7684\u590d\u6298\u5c04\u7387\u4e00\u6837\uff0c\u5728\u591a\u91cd\u6563\u5c04\u5f71\u54cd\u4e0b\u7684\u7535\u5b50\u6ce2\u83b7\u5f97\u590d\u6ce2\u6570\u4f4d\u79fb\u0394\u00a0k\uff0c\u5176\u5e45\u5ea6\u5728\u5171\u632f\u65f6\u5927\u3002\u7406\u89e3\u7535\u5b50\u5728\u6676\u4f53\u56fa\u4f53\u4e2d\u7684\u884c\u4e3a\u65b9\u5f0f\u7684\u5173\u952e\u662f\u5c06\u7535\u5b50\u6ce2\u7684\u80fd\u91cf\u4e0e\u5176\u6ce2\u6570\u8054\u7cfb\u8d77\u6765\u7684\u80fd\u5e26\u7ed3\u6784\u3002\u5373\u4f7f\u5728\u53ea\u6709\u77ed\u7a0b\u6709\u5e8f\u7684\u7269\u8d28\u76f8\uff08\u6db2\u4f53\u6216\u65e0\u5b9a\u5f62\u56fa\u4f53\uff09\u4e2d\uff0c\u7535\u5b50\u6ce2\u7684\u76f8\u5e72\u90e8\u5206\u4ecd\u7136\u5177\u6709\u80fd\u5e26\u7ed3\u6784\u3002\u6db2\u6001\u91d1\u5c5e\u80fd\u5e26\u7ed3\u6784\u7684\u7406\u8bba\u6a21\u578b\u662f\u5728\u51e0\u5341\u5e74\u524d\u5c31\u63d0\u51fa\u4e86\u7684\uff0c\u4f46\u5230\u76ee\u524d\u4e3a\u6b62\uff0c\u5171\u632f\u6563\u5c04\u5f15\u8d77\u7684\u80fd\u5e26\u7ed3\u6784\u91cd\u6574\u5316\u548c\u8d5d\u80fd\u9699\u4ecd\u672a\u88ab\u89c2\u5bdf\u5230\u3002<\/p>\n<p>\u4eca\u65e5\uff0c<strong><b>\u97e9\u56fd\u5ef6\u4e16\u5927\u5b66Keun\u00a0Su\u00a0Kim<\/b><\/strong><strong><b>\uff08\u901a\u8baf\u4f5c\u8005\uff09<\/b><\/strong>\u62a5\u9053\u4e86\u5728\u7ed3\u6676\u7edd\u7f18\u4f53\uff08\u9ed1\u78f7\uff09\u548c\u65e0\u5e8f\u63ba\u6742\u5242\uff08\u78b1\u91d1\u5c5e\uff09\u7684\u754c\u9762\u5904\u89c2\u5bdf\u5230\u7684\u5f02\u5e38\u80fd\u5e26\u7ed3\u6784\u3002\u9ed1\u78f7\u662f\u4e00\u79cd\u5c42\u72b6\u6750\u6599\uff0c\u5176\u4e2d\u78f7\u539f\u5b50\u7684\u8702\u7a9d\u72b6\u6676\u683c\u88ab\u8c03\u5236\u5f62\u6210\u4e00\u7cfb\u5217\u952f\u9f7f\u72b6\u7684\u810a\u548c\u8c37\u3002\u78b1\u91d1\u5c5e\u5728\u9ed1\u78f7\u4e0a\u7684\u5206\u5e03\u663e\u793a\u5f84\u5411\uff08\u548c\u5404\u5411\u5f02\u6027\uff09\u7ed3\u6784\uff0c\u8fd9\u79cd\u5f84\u5411\u5f62\u72b6\u662f\u6db2\u76f8\u6216\u73bb\u7483\u76f8\u7684\u5173\u952e\u7279\u5f81\uff0c\u5e76\u53cd\u6620\u4e86\u5728\u6392\u65a5\u76f8\u4e92\u4f5c\u7528\u4e0b\u968f\u673a\u5206\u5e03\u7684\u63ba\u6742\u5242\u7684\u5e73\u5747\u539f\u5b50\u95f4\u8ddd\u79bb\uff08\u6216\u77ed\u7a0b\u6709\u5e8f\uff09\u3002\u540c\u65f6\uff0c\u53d1\u73b0\u81ea\u7531\u7535\u5b50\u7684\u4f20\u7edf\u629b\u7269\u7ebf\u80fd\u5e26\u7ed3\u6784\u5411\u96f6\u6ce2\u6570\u5f2f\u66f2\uff0c\u5176\u8d5d\u80fd\u9699\u4e3a\u8d39\u7c73\u80fd\u7ea730-240\u6beb\u7535\u5b50\u4f0f\u7279\u3002\u8fd9\u662f\u7531\u5171\u632f\u6563\u5c04\u5f15\u8d77\u7684\u6ce2\u6570\u91cd\u6574\u5316\uff0c\u5bfc\u81f4\u5728\u78b1\u91d1\u5c5e\u79bb\u5b50\u7684\u6563\u5c04\u52bf\u4e2d\u5f62\u6210\u51c6\u675f\u7f1a\u6001\u3002\u7531\u4e0d\u540c\u79cd\u7c7b\u7684\u65e0\u5e8f\u78b1\u91d1\u5c5e\uff08\u94a0\u3001\u94be\u3001\u94f7\u548c\u94ef\uff09\u8c03\u8282\u7684\u8fd9\u79cd\u7535\u4f4d\u7684\u6df1\u5ea6\u5141\u8bb8\u5bf9p\u6ce2\u548cd\u6ce2\u5171\u632f\u7684\u8d5d\u80fd\u9699\u8fdb\u884c\u5206\u7c7b\u3002\u672c\u6587\u7684\u7814\u7a76\u7ed3\u679c\u53ef\u80fd\u4e3a\u65e0\u5e8f\u63ba\u6742\u5242\u63ba\u6742\u7684\u5404\u79cd\u6676\u4f53\u7edd\u7f18\u4f53\u7684\u4ee4\u4eba\u56f0\u60d1\u7684\u5149\u8c31\u63d0\u4f9b\u4e86\u7ebf\u7d22\uff0c\u5982\u5728\u94dc\u6c27\u5316\u7269\u4e2d\u89c2\u5bdf\u5230\u7684\u7011\u5e03\u5206\u6563\u3002\u76f8\u5173\u7814\u7a76\u6210\u679c\u4ee5\u201c<strong><b>Pseudogap in a crystalline insulator doped by disordered metals<\/b><\/strong>\u201d\u4e3a\u9898\u53d1\u8868\u5728<strong><em><b><i>Nature<\/i><\/b><\/em><\/strong>\u4e0a\u3002<\/p>\n<p><strong><b>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/b><\/strong><\/p>\n<p><strong><b>\u56fe\u4e00<\/b><\/strong><strong><b>\u3001\u6db2\u6001\u91d1\u5c5e\u7684\u80fd\u5e26\u7ed3\u6784<\/b><\/strong><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-225545\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe1.jpg\" alt=\"\" width=\"600\" height=\"281\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe1-300x141.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong><\/p>\n<p><strong><b>\u56fe\u4e8c<\/b><\/strong><strong><b>\u3001\u65e0\u5e8f\u78b1\u91d1\u5c5e\u63ba\u6742\u9ed1\u78f7\u7684\u7535\u5b50\u7ed3\u6784<\/b><\/strong><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-225546\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe2.jpg\" alt=\"\" width=\"600\" height=\"448\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe2.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe2-300x224.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong><\/p>\n<p><strong><b>\u56fe\u4e09<\/b><\/strong><strong><b>\u3001\u6db2\u6001\u91d1\u5c5e\u7684\u5171\u632f\u6563\u5c04\u548c<\/b><\/strong><strong><b>\u80fd<\/b><\/strong><strong><b>\u5e26\u91cd\u6574\u5316<\/b><\/strong><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-225547\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe3.jpg\" alt=\"\" width=\"600\" height=\"342\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe3.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe3-300x171.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>\u56db<\/b><\/strong><strong><b>\u3001\u6db2\u6001\u91d1\u5c5e\u4e2d\u7684\u6001\u5bc6\u5ea6\u548c\u5149\u8c31\u6a21\u62df<\/b><\/strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-225548\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe4.jpg\" alt=\"\" width=\"600\" height=\"360\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe4.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe4-300x180.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>\u4e94<\/b><\/strong><strong><b>\u3001<\/b><\/strong><strong><b>\u8d5d\u80fd\u9699<\/b><\/strong><strong><b>\u548c\u76f8\u56fe<\/b><\/strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-225549\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe5.jpg\" alt=\"\" width=\"600\" height=\"343\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe5.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe5-300x172.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u6587\u732e\u94fe\u63a5<\/b><\/strong>\uff1a\u201c<a href=\"https:\/\/www.nature.com\/articles\/s41586-021-03683-0\"><strong><u><b>Pseudogap in a crystalline insulator doped by disordered<\/b><\/u><\/strong><strong><u><b>\u00a0<\/b><\/u><\/strong><strong><u><b>metals<\/b><\/u><\/strong><\/a>\u201d<strong><b>(<\/b><\/strong><strong><b>Nature<\/b><\/strong><strong><b>\uff0c202<\/b><\/strong><strong><b>1<\/b><\/strong><strong><b>\uff0c<\/b><\/strong><strong><b>10.1038\/s41586-021-03683-0<\/b><\/strong><strong><b>)<\/b><\/strong><\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4ebaCYM\u7f16\u8bd1\u4f9b\u7a3f\u3002\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\u3002<\/p>\n<p>\u6750\u6599\u4eba\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaokefu\u3002<\/p>\n<p>&nbsp;<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u57281960\u5e74\u4ee3\uff0c\u5bf9\u6db2\u6001\u91d1\u5c5e\u7684\u80fd\u5e26\u7ed3\u6784\u8fdb\u884c\u4e86\u4e00\u7cfb\u5217\u5f00\u521b\u6027\u7684\u7406\u8bba\u7814\u7a76\u3002\u5c31\u50cf\u73bb\u7483\u6750\u6599\u5177\u6709\u660e\u786e\u5b9a\u4e49\u7684\u590d\u6298\u5c04\u7387\u4e00\u6837\uff0c\u5728\u591a\u91cd\u6563\u5c04\u5f71\u54cd\u4e0b\u7684\u7535\u5b50\u6ce2\u83b7\u5f97\u590d\u6ce2\u6570\u4f4d\u79fb\u0394\u00a0k&#8230;<\/p>\n","protected":false},"author":9629,"featured_media":225545,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[293],"class_list":["post-225544","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu","tag-nature"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/225544"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/9629"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=225544"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/225544\/revisions"}],"predecessor-version":[{"id":225550,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/225544\/revisions\/225550"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/225545"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=225544"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=225544"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=225544"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}