{"id":226040,"date":"2021-08-16T06:35:59","date_gmt":"2021-08-15T22:35:59","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=226040"},"modified":"2021-08-15T21:36:09","modified_gmt":"2021-08-15T13:36:09","slug":"top%e6%9c%9f%e5%88%8a%e4%b8%ad%e8%83%bd%e6%ba%90%e6%9d%90%e6%96%99%e8%ae%a1%e7%ae%97%e6%97%a0%e5%a4%84%e4%b8%8d%e5%9c%a8","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=226040","title":{"rendered":"TOP\u671f\u520a\u4e2d\u80fd\u6e90\u6750\u6599\u8ba1\u7b97\u65e0\u5904\u4e0d\u5728"},"content":{"rendered":"<p>\u5982\u4eca\uff0c\u7406\u8bba\u8ba1\u7b97\u4e0e\u5b9e\u9a8c\u76f8\u7ed3\u5408\u5df2\u7ecf\u6210\u4e86TOP\u671f\u520a\u6700\u4e3b\u6d41\u7684\u7814\u7a76\u65b9\u5f0f\uff0c\u5c24\u5176\u662f\u5728\u6d89\u53ca\u5230\u673a\u7406\u5206\u6790\u65b9\u9762\uff0c\u7406\u8bba\u8ba1\u7b97\u51e0\u4e4e\u5fc5\u4e0d\u53ef\u5c11\u3002\u7136\u800c\uff0c\u7406\u8bba\u8ba1\u7b97\u4e0e\u5b9e\u9a8c\u4e4b\u95f4\u4ecd\u7136\u5b58\u5728\u5f88\u5927\u7684\u9e3f\u6c9f\uff0c\u8bb8\u591a\u80fd\u6e90\u9886\u57df\u7684\u7814\u7a76\u4eba\u5458\u5e76\u4e0d\u77e5\u9053\u53ef\u4ee5\u7528\u7406\u8bba\u8ba1\u7b97\u6765\u5e72\u4ec0\u4e48\uff0c\u6240\u4ee5\u4e5f\u96be\u4ee5\u60f3\u5230\u91c7\u7528\u7406\u8bba\u8ba1\u7b97\u6765\u89e3\u51b3\u81ea\u5df1\u8bfe\u9898\u4e2d\u7684\u95ee\u9898\u3002\u5728\u6b64\uff0c\u6211\u4eec\u5bf9\u7406\u8bba\u8ba1\u7b97\u5728\u80fd\u6e90\u9886\u57df\u7684\u8fd1\u671f\u5e94\u7528\u8fdb\u884c\u6c47\u603b\uff0c\u5e0c\u671b\u80fd\u7ed9\u5927\u5bb6\u4ee5\u542f\u53d1\u3002<\/p>\n<p><strong><b>EEM\uff1a\u8d85\u7ea7\u7535\u5bb9\u5668\u7535\u8377\u5b58\u50a8\u673a\u5236\u7684\u8ba1\u7b97\u5206\u6790<\/b><\/strong><\/p>\n<p>\u8ba1\u7b97\u5efa\u6a21\u65b9\u6cd5\uff0c\u5305\u62ec\u5206\u5b50\u52a8\u529b\u5b66(MD)\u548c\u8499\u7279\u5361\u7f57(MC)\u6a21\u62df\u548c\u5bc6\u5ea6\u6cdb\u51fd\u7406\u8bba(DFT)\u662f\u7814\u7a76\u7535\u5316\u5b66\u50a8\u80fd\u5668\u4ef6\u7535\u8377\u5b58\u50a8\u673a\u5236\u7684\u70ed\u70b9\u3002\u8fd9\u4e9b\u65b9\u6cd5\u53ef\u4ee5\u6709\u6548\u5730\u83b7\u53d6\u5206\u5b50\u5c3a\u5ea6\u7684\u5c40\u90e8\u4fe1\u606f\uff0c\u6216\u8005\u4e3a\u5b9e\u9a8c\u7814\u7a76\u65e0\u6cd5\u76f4\u63a5\u89e3\u91ca\u7684\u65b0\u5b9e\u9a8c\u53d1\u73b0\u63d0\u4f9b\u6e05\u6670\u7684\u89e3\u91ca\u3002\u56db\u5ddd\u5927\u5b66Zifeng Lin\u3001\u5357\u4eac\u5de5\u4e1a\u5927\u5b66Jixin Zhu\u7740\u91cd\u4e8e\u8ba1\u7b97\u6a21\u62df\u65b9\u6cd5\u5728\u63a2\u7d22\u5178\u578b\u7eb3\u7c73\u5c3a\u5ea6\u6750\u6599\u7684\u7535\u8377\u5b58\u50a8\u673a\u5236\u65b9\u9762\u7684\u6700\u65b0\u8fdb\u5c55\uff0c\u5982\u7eb3\u7c73\u591a\u5b54\u78b3\u6750\u6599\u3001\u4e8c\u7ef4MXene\u6750\u6599\u548c\u91d1\u5c5e\u6709\u673a\u9aa8\u67b6\u7535\u6781\u3002\u9664\u4e86\u66f4\u597d\u5730\u4e86\u89e3\u7535\u8377\u5b58\u50a8\u673a\u5236\u548c\u5b9e\u9a8c\u89c2\u5bdf\u5916\uff0c\u8db3\u591f\u5feb\u901f\u51c6\u786e\u7684\u6a21\u578b\u5c06\u6709\u52a9\u4e8e\u4e3a\u65b0\u578b\u9ad8\u6027\u80fd\u7535\u5316\u5b66\u50a8\u80fd\u5668\u4ef6\u7684\u8bbe\u8ba1\u63d0\u4f9b\u7406\u8bba\u6307\u5bfc\u548c\u5b9e\u9a8c\u57fa\u7840\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cComputational Insights into Charge Storage Mechanisms of\u00a0Supercapacitors\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728EEM\u4e0a\u3002DOI: 10.1002\/eem2.12124<\/p>\n<p>\u56fe1\u00a0a)EDL\u7535\u5bb9\u5668\u5e38\u7528\u7684\u6a21\u62df\u8bbe\u7f6eb) CCM\u548cCPM\u6a21\u62df\u8fc7\u7a0b\u53ca\u7535\u6781\u7535\u8377\u6f14\u5316\u793a\u610f\u56fec)\u5927\u5c0f\u534a\u5f84\u78b3\u5b54\u7684\u6bcf\u78b3\u7535\u8377\u8865\u507f(CCpC)<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-226041\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1-12.png\" alt=\"\" width=\"600\" height=\"186\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1-12.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1-12-300x93.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>E<\/b><\/strong><strong><b>EM<\/b><\/strong><strong><b>\uff1a<\/b><\/strong><strong><b>\u5355\u94bc\u539f\u5b50\u951a\u5b9a\u7684\u8ba1\u7b97\u8bbe\u8ba1\u7f3a\u9677\u787c\u78f7\u5316\u5355\u5206\u5b50\u5c42<\/b><\/strong><strong><b>\u7528\u4e8e<\/b><\/strong><strong><b>\u9ad8\u6027\u80fd\u7684\u6c2e\u8fd8\u539f\u7535\u50ac\u5316<\/b><\/strong><\/p>\n<p>\u50ac\u5316\u8fd8\u539f\u5206\u5b50\u6c2e(N<sub>2<\/sub>)\u4e3a\u6c28(NH<sub>3<\/sub>)\u662f\u6700\u91cd\u8981\u548c\u6700\u5177\u6311\u6218\u6027\u7684\u5de5\u4e1a\u53cd\u5e94\u4e4b\u4e00\u3002\u7535\u5316\u5b66\u8fd8\u539f\u6280\u672f\u88ab\u8ba4\u4e3a\u662f\u4e00\u79cd\u4eba\u5de5\u56fa\u5b9a\u73af\u5883\u6c2e\u7684\u8282\u80fd\u6280\u672f\uff0c\u6b63\u5728\u6210\u4e3a\u66ff\u4ee3Haber\u2013Bosch\u5de5\u827a\u7684\u6700\u4f18\u6f5c\u5728\u53ef\u6301\u7eed\u7b56\u7565\u3002\u7136\u800c\uff0c\u8fd9\u4e00\u8fc7\u7a0b\u9700\u8981\u9ad8\u6548\u7684\u50ac\u5316\u5242\u6765\u8fdb\u884cN<sub>2<\/sub>\u8fd8\u539f\u53cd\u5e94\u3002\u5728\u8fd9\u91cc\uff0c\u6b66\u6c49\u7406\u5de5\u5927\u5b66Yan Zhao\u3001\u5357\u4eac\u5de5\u4e1a\u5927\u5b66Yuping Wu\u7b49\u4eba\u901a\u8fc7\u7b2c\u4e00\u6027\u539f\u7406\u8ba1\u7b97\uff0c\u7cfb\u7edf\u5730\u63a2\u7d22\u4e86\u5355\u8fc7\u6e21\u91d1\u5c5e\u539f\u5b50(Pd\uff0cAg, Rh, Cu, Ti, Mo, Mn, Zn, Fe, Co, Ru\uff0c\u548cPt)\u5d4c\u5165\u5355\u5206\u5b50\u5c42\u7684\u7f3a\u9677\u787c\u78f7\u5316(TMs\/BP)\u5355\u5206\u5b50\u5c42\u4e0e\u78f7\u5355\u7a7a\u4f4d\uff0c\u7528\u4e8e\u73af\u5883NH<sub>3<\/sub>\u7684\u751f\u4ea7\u3002\u5176\u4e2d\uff0cMo\/BP\u901a\u8fc7\u5178\u578b\u7684\u9176\u50ac\u5316\u548c\u8fde\u7eed\u5316\u7684\u53cd\u5e94\u9014\u5f84\uff0c\u8868\u73b0\u51fa\u6700\u4f73\u7684\u73af\u5883\u8fd8\u539fN<sub>2<\/sub>\u7684\u50ac\u5316\u6027\u80fd\uff0c\u6d3b\u5316\u5c4f\u969c\u4e3a0.68 eV\uff0c\u8bf4\u660eMo\/BP\u662f\u4e00\u79cd\u6709\u6548\u7684N<sub>2<\/sub>\u56fa\u5b9a\u50ac\u5316\u5242\u3002\u8fd9\u9879\u5de5\u4f5c\u53ef\u4ee5\u63d0\u4f9b\u4e00\u4e2a\u65b0\u7684\u9014\u5f84\uff0c\u5229\u7528\u8bbe\u8ba1\u7684\u5355\u539f\u5b50\u7535\u50ac\u5316\u5242\u5408\u6210NH<sub>3<\/sub>\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cComputational Design of Single Mo Atom Anchored\u00a0Defective Boron Phosphide Monolayer as a High-performance Electrocatalyst for the Nitrogen Reduction\u00a0Reaction\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728EEM\u4e0a\u3002DOI: 10.1002\/eem2.12120<\/p>\n<p>\u56fe2\u00a0\u901a\u8fc7a)\u8fdc\u7aef\uff0cb)\u4ea4\u66ff\uff0cc)\u9176\u50ac\u5316\u548cd)\u8fde\u7eed\u673a\u5236\u8ba1\u7b97Mo\/BP\u5355\u5206\u5b50\u819c\u50ac\u5316NRR\u7684\u81ea\u7531\u80fd\u5206\u5e03\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-226042\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_2-1.png\" alt=\"\" width=\"600\" height=\"355\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_2-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_2-1-300x178.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>AM\uff1a\u901a\u8fc7\u6676\u4f53\u6b63\u6781\u7684\u975e\u6676\u5316\u4fc3\u8fdb\u4f4e\u6e29\u6761\u4ef6\u4e0b\u7684\u79bb\u5b50\u52a8\u529b\u5b66<\/b><\/strong><\/p>\n<p>\u9502\u79bb\u5b50\u7535\u6c60(LIBs)\u5728\u8d85\u4f4e\u6e29\u4e0b\u7684\u6b63\u5e38\u5de5\u4f5c(&lt; -40\u00b0C)\u5bf9\u5bd2\u51b7\u6c14\u5019\u7684\u5e94\u7528\u5f88\u91cd\u8981;\u7136\u800c\uff0c\u7531\u4e8e\u4f20\u7edf\u63d2\u5c42\u9634\u6781\u52a8\u529b\u5b66\u8fdf\u7f13\u548c\u9502\u79bb\u5b50\u5728\u5176\u6846\u67b6\u5185\u7684\u56fa\u4f53\u6269\u6563\u7f13\u6162\uff0c\u5bfc\u81f4\u63d2\u5c42\u9634\u6781\u5bb9\u91cf\u4f4e\uff0c\u963b\u788d\u4e86\u5176\u8fd0\u884c\u3002\u7ed3\u679c\u8868\u660e\uff0c\u975e\u6676\u5316\u662f\u4e00\u79cd\u6709\u6548\u7684\u4fc3\u8fdb\u9634\u6781\u4f4e\u6e29\u52a8\u529b\u5b66\u7684\u7b56\u7565\uff0c\u5b83\u7f13\u89e3\u4e86\u4f4e\u6e29\u6761\u4ef6\u4e0b\u81f4\u5bc6\u6676\u683c\u7ed3\u6784\u5bf9\u79bb\u5b50\u8f93\u8fd0\u7684\u963b\u585e\u6548\u5e94\u3002\u8fd1\u65e5\uff0c\u82cf\u5dde\u5927\u5b66\u664f\u6210\u6797\u6559\u6388\u7b49\u4eba\u62a5\u9053\u4e86\u91cd\u70b9\u7814\u7a76\u4e86\u4e0d\u540c\u7f29\u5408\u53cd\u5e94\u6761\u4ef6\u4e0b\u5408\u6210\u7684\u5171\u4ef7\u7ed3\u6676\u805a\u5408\u7269\uff08CCP\uff09\u548c\u5171\u4ef7\u975e\u6676\u805a\u5408\u7269\uff08CAP\uff09\u7684\u4f4e\u6e29\u7279\u6027\u3002\u7ed3\u679c\u8868\u660e\uff0c\u975e\u6676\u5316\u662f\u4e00\u79cd\u6709\u6548\u7684\u4fc3\u8fdb\u9634\u6781\u4f4e\u6e29\u52a8\u529b\u5b66\u7684\u7b56\u7565\uff0c\u5b83\u7f13\u89e3\u4e86\u4f4e\u6e29\u6761\u4ef6\u4e0b\u81f4\u5bc6\u6676\u683c\u7ed3\u6784\u5bf9\u79bb\u5b50\u8f93\u8fd0\u7684\u963b\u585e\u6548\u5e94\u3002CCP\u7684\u5bc6\u96c6\u5806\u79ef\u7ed3\u6784\u963b\u788d\u4e86Li<sup>+<\/sup>\u5728\u4f4e\u6e29\u4e0b\u5230\u8fbe\u6750\u6599\u5185\u90e8\u7684\u6d3b\u6027\u4e2d\u5fc3\uff0c\u5bfc\u81f4\u4e86\u8f83\u9ad8\u7684\u754c\u9762\u963b\u6297\u548c\u8f83\u4f4e\u7684\u79bb\u5b50\u6269\u6563\u7cfb\u6570\u3002\u800c\u7531\u4e8e\u7535\u8377\u4f20\u8f93\u963b\u6297\u7684\u964d\u4f4e\u548cLi<sup>+<\/sup>\u6269\u6563\u901f\u7387\u7684\u52a0\u5feb\uff0c\u5f97\u5230\u7684\u5177\u6709\u4e30\u5bcc\u5421\u55ea\u548c\u7fb0\u57fa\u6d3b\u6027\u4e2d\u5fc3\u7684\u5171\u4ef7\u975e\u6676\u6001\u805a\u5408\u7269\u5728\u221280 \u00b0C\u4e0b\u7684\u6bd4\u5bb9\u91cf\u9ad8\u8fbe141 mAh g<sup>\u22121<\/sup>\uff0c\u4f18\u4e8e\u5176\u7ed3\u6784\u7c7b\u4f3c\u7684\u5171\u4ef7\u7ed3\u6676\u805a\u5408\u7269\uff0843.8 mAh g<sup>\u22121<\/sup>\uff09\u3002\u6b64\u5916\uff0c\u5728\u221260\u2103\u4e0b\u8fdb\u884c500\u6b21\u5145\u653e\u7535\u540e\uff0cCAP\u7684\u521d\u59cb\u5bb9\u91cf\u53ef\u4fdd\u630184.7%\u3002\u5206\u5b50\u52a8\u529b\u5b66\u6a21\u62df\u8868\u660e\uff0c\u5bcc\u542b\u901a\u9053\u7684\u975e\u6676\u7ed3\u6784\u975e\u5e38\u6709\u5229\u4e8e\u9502\u79bb\u5b50\u5728\u6709\u673a\u56fa\u4f53\u7684\u95f4\u9699\u4e2d\u5feb\u901f\u6269\u6563\u3002\u8fd9\u9879\u5de5\u4f5c\u4e3a\u4f4e\u6e29\u7535\u6c60\u7684\u6676\u4f53\u9634\u6781\u975e\u6676\u5316\u63d0\u4f9b\u4e86\u4e00\u79cd\u6709\u6548\u7684\u7b56\u7565\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cAccelerating Ion Dynamics Under Cryogenic Conditions\u00a0by the Amorphization of Crystalline Cathodes\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728AM\u4e0a\u3002DOI: 10.1002\/adma.202102634<\/p>\n<p>\u56fe3\u00a0CAP\u6216CCP\u57faLIB\u7535\u5316\u5b66\u884c\u4e3a\u7684\u52a8\u529b\u5b66\u5206\u6790<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-226043\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_3.png\" alt=\"\" width=\"600\" height=\"423\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_3.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_3-300x212.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>A<\/b><\/strong><strong><b>M<\/b><\/strong><strong><b>\uff1a\u534a\u76f8\u5e72\u754c\u9762\u53ef\u63a7\u5f02\u8d28\u7ed3<\/b><\/strong><strong><b>\u4fc3\u8fdbCoSe<\/b><\/strong><strong><sub><b>2<\/b><\/sub><\/strong><strong><b>\/ FeS<\/b><\/strong><strong><b>e<\/b><\/strong><strong><sub><b>2<\/b><\/sub><\/strong><strong><b>\u7684\u94be\u50a8\u5b58<\/b><\/strong><\/p>\n<p>\u5f02\u8d28\u7ed3\u6784\u662f\u8fc7\u6e21\u91d1\u5c5e\u7852\u5316\u7269\u589e\u5f3aK<sup>+<\/sup>\u5b58\u50a8\u7684\u6709\u6548\u65b9\u6cd5\u3002\u81ea\u53d1\u5f62\u6210\u7684\u5185\u90e8\u7535\u573a\u5927\u5927\u4fc3\u8fdb\u4e86\u7535\u8377\u8f93\u8fd0\uff0c\u663e\u8457\u964d\u4f4e\u4e86\u6d3b\u5316\u80fd\u3002\u7136\u800c\uff0c\u57fa\u4e8e\u80fd\u7ea7\u68af\u5ea6\u548c\u6676\u683c\u5339\u914d\u5ea6\u7684\u754c\u9762\u533a\u57df\u7684\u5b8c\u5584\u4ecd\u7136\u662f\u4e00\u4e2a\u5de8\u5927\u7684\u6311\u6218\u3002\u8fd1\u65e5\uff0c\u897f\u5b89\u7406\u5de5\u5927\u5b66\u674e\u559c\u98de\u3001\u79e6\u622c\u7b49\u4eba\u62a5\u9053\u4e86\u91c7\u7528\u9ad8\u6548\u7684\u7b80\u5316\u65b9\u6cd5\u5408\u6210\u4e86\u540c\u65f6\u5177\u6709\u4e30\u5bcc\u7684\u7a7a\u4f4d\u548c\u5177\u6709\u534a\u5171\u683c\u76f8\u754c\u7684\u8d85\u7ec6CoSe<sub>2<\/sub>-FeSe<sub>2<\/sub>\u5f02\u8d28\u7ed3\uff0c\u5176\u5177\u6709\u72ec\u7279\u7684\u7535\u5b50\u7ed3\u6784\u548c\u4e30\u5bcc\u7684\u6d3b\u6027\u4e2d\u5fc3\uff0c\u8fd9\u79cd\u8bbe\u8ba1\u4e0d\u4ec5\u6539\u53d8\u4e86\u7535\u5b50\u7ed3\u6784\uff0c\u800c\u4e14\u4fc3\u8fdb\u4e86K<sup>+<\/sup>\u7684\u6269\u6563\u3002DFT\u8ba1\u7b97\u8868\u660e\uff0c\u5f3a\u5316\u7684\u754c\u9762K<sup>+<\/sup>\u5438\u9644\u53cd\u5e94\u4fc3\u8fdb\u4e86\u94be\u5316\u8fc7\u7a0b\u3002\u56e0\u6b64\uff0c\u6240\u8bbe\u8ba1\u7684\u7ed3\u6784\u5f3a\u5316\u7684\u7535\u6781\u6750\u6599\u5177\u6709\u4f18\u5f02\u7684\u5faa\u73af\u8010\u4e45\u6027\u548c\u4f18\u5f02\u7684\u500d\u7387\u6027\u80fd\u3002\u5b9e\u9a8c\u7ed3\u679c\u663e\u793a\uff0c\u57fa\u4e8e\u4f18\u5316\u540e\u7684CoSe<sub>2<\/sub>\/FeSe<sub>2<\/sub>@C\u5f02\u8d28\u7ed3\u8d1f\u6781\u7684PIBs\u5728100 mA g<sup>\u2212<\/sup><sup>1<\/sup>\u4e0b\u7684\u53ef\u9006\u5bb9\u91cf\u4e3a401.1 mAh g<sup>\u2212<\/sup><sup>1<\/sup>\uff0c\u57282 A g<sup>\u2212<\/sup><sup>1<\/sup>\u4e0b\u7684\u53ef\u9006\u5bb9\u91cf\u4e3a275mAh g<sup>\u2212<\/sup><sup>1<\/sup>\u3002\u7406\u8bba\u8ba1\u7b97\u4e5f\u8868\u660e\uff0cCoSe<sub>2<\/sub>-FeSe<sub>2<\/sub>\u5f02\u8d28\u7ed3\u53ef\u663e\u8457\u4fc3\u8fdb\u94be\u79bb\u5b50\u7684\u6269\u6563\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cControllable Heterojunctions with a Semicoherent Phase\u00a0Boundary Boosting the Potassium Storage of CoSe<sub>2<\/sub>\/FeSe<sub>2<\/sub>\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728AM\u4e0a\u3002<\/p>\n<p>\u56fe4\u00a0a)\u8ba1\u7b97\u6001\u5bc6\u5ea6(DOS)\u5206\u6790\u548cb-d) CoSe<sub>2<\/sub>, FeSe<sub>2<\/sub>@C\u548cCoSe<sub>2<\/sub>\/FeSe<sub>2<\/sub>@C\u7684\u7535\u8377\u5bc6\u5ea6\u5dee\u3002e) CoSe<sub>2<\/sub>\/FeSe<sub>2<\/sub>@C\u5236\u9020\u539f\u7406\u56fe<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-226044\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_4.png\" alt=\"\" width=\"600\" height=\"484\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_4.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_4-300x242.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>E<\/b><\/strong><strong><b>ES<\/b><\/strong><strong><b>\uff1a<\/b><\/strong><strong><b>\u5168\u56fa\u6001\u7535\u6c60\u7684\u70ed\u529b\u5b66\u7ea6\u675f\u4e2d\u56fa\u7535\u89e3\u8d28\u754c\u9762\u76f8\u8bbe\u8ba1<\/b><\/strong><\/p>\n<p>\u56fa\u6001\u7535\u6c60(SSBs)\u662f\u50a8\u80fd\u9886\u57df\u6700\u6709\u524d\u9014\u7684\u53d1\u5c55\u65b9\u5411\u4e4b\u4e00\u3002\u7136\u800c\uff0c\u76ee\u524d\u56fa\u4f53\u7535\u89e3\u8d28(SSE)\u9897\u7c92\u754c\u9762\u4e0a\u4e0d\u53ef\u907f\u514d\u5730\u53d1\u751f\u590d\u6742\u7684\u7535\u5316\u5b66\u53cd\u5e94\uff0c\u9650\u5236\u4e86\u56fa\u4f53\u7535\u89e3\u8d28\u7684\u53d1\u5c55\u3002\u6b64\u5916\uff0c\u8003\u8651\u5230\u8fd9\u7c7b\u7cfb\u7edf\u7684\u7269\u8d28\u590d\u6742\u6027\uff0c\u6ca1\u6709\u76f4\u63a5\u7684\u65b9\u6cd5\u6765\u89e3\u51b3\u8fd9\u4e9b\u754c\u9762\u4e0d\u7a33\u5b9a\u6027\u3002\u5728\u8fd9\u9879\u5de5\u4f5c\u4e2d\uff0c\u8fd1\u65e5\uff0c\u7f8e\u56fd\u54c8\u4f5b\u5927\u5b66\u674e\u946b\u6559\u6388\u7b49\u4eba\u5bf9\u5168\u56fa\u6001\u7535\u6c60\u7684\u70ed\u529b\u5b66\u7ea6\u675f\u7cfb\u7efc\u7684\u7406\u8bba\u8fdb\u884c\u4e86\u91cd\u8981\u53d1\u5c55\uff0c\u9996\u6b21\u63d0\u51fa\u4e86\u6291\u5236\u7535\u6c60\u754c\u9762\u5206\u89e3\u53cd\u5e94\u7684\u4e34\u754c\u6750\u6599\u53c2\u6570Kcrit\u3002\u7ed3\u5408\u9ad8\u901a\u91cf\u4ece\u5934\u8ba1\u7b97\u548c\u673a\u5668\u5b66\u4e60\u65b9\u6cd5\uff0c\u4f7f\u7528\u6211\u4eec\u72ec\u7279\u7684\u7ea6\u675f\u96c6\u6210\u63cf\u8ff0\uff0c\u7814\u7a76\u548c\u8bbe\u8ba1\u5177\u6709\u53ef\u8c03\u8c10\u7535\u5316\u5b66\u7a33\u5b9a\u6027\u7684\u56fa\u6001-\u56fa\u6001-\u7535\u89e3\u8d28-\u754c\u9762\u76f8(SEI)\u3002\u673a\u5668\u5b66\u4e60\u63ed\u793a\u4e86\u7531\u673a\u68b0\u6536\u7f29\u6548\u5e94\u7a33\u5b9a\u7684\u56fa\u6001SEI\u7684\u80fd\u529b\u662f\u4e00\u4e2a\u975e\u51f8\u548c\u975e\u7ebf\u6027\u7684\uff0c\u4f46\u4ecd\u7136\u662f\u786e\u5b9a\u6027\u7684\u7ec4\u6210\u529f\u80fd\u3002\u8fd9\u79cd\u65b9\u6cd5\u7684\u51c6\u786e\u6027\u901a\u8fc7\u56fa\u4f53\u7535\u89e3\u8d28\u7684\u73bb\u7483\u548c\u9676\u74f7\u786b\u5316\u7269\u65cf\u7684\u754c\u9762\u5f97\u5230\u4e86\u8bc1\u660e\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cSolid\u2013electrolyte-interphase design in constrained\u00a0ensemble for solid-state batteries\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728EES\u4e0a\u3002DOI: 10.1039\/d1ee00754h<\/p>\n<p>\u56fe5\u00a0\u57fa\u4e8e\u7ea6\u675f\u7cfb\u7efc\u7406\u8bba\u7684\u754c\u9762\u4e34\u754c\u6a21\u91cf<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-226045\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_5.png\" alt=\"\" width=\"600\" height=\"411\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_5.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_5-300x206.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>npj Comput. Mater.<\/b><\/strong><strong><b>\uff1a<\/b><\/strong><strong><b>\u6df7\u5408\u7b49\u4f4d\u7535\u5b50\u548c\u7b2c\u4e00\u6027\u539f\u7406\u8ba1\u7b97<\/b><\/strong><strong><b>\u5206\u6790<\/b><\/strong><strong><b>\u56fa\u4f53\u7f3a\u9677\u4e2d\u7684\u81ea\u65cb-\u81ea\u65cb\u76f8\u4e92\u4f5c\u7528<\/b><\/strong><\/p>\n<p>\u8981\u7406\u89e3\u81ea\u65cb\u7f3a\u9677\u7684\u91cf\u5b50\u52a8\u529b\u5b66\u53ca\u5176\u76f8\u5e72\u7279\u6027\uff0c\u9700\u8981\u5bf9\u56fa\u4f53\u548c\u5206\u5b50\u4e2d\u7684\u81ea\u65cb-\u81ea\u65cb\u76f8\u4e92\u4f5c\u7528\u8fdb\u884c\u7cbe\u786e\u7684\u5efa\u6a21\uff0c\u4f8b\u5982\u4f7f\u7528\u4ece\u7b2c\u4e00\u6027\u539f\u7406\u8ba1\u7b97\u5f97\u5230\u7684\u81ea\u65cb\u54c8\u5bc6\u987f\u53c2\u91cf\u3002\u5bc6\u6b47\u6839\u5927\u5b66Vikram Gavini\u3001\u829d\u52a0\u54e5\u5927\u5b66Giulia Galli\u7b49\u4eba\u63d0\u51fa\u4e86\u4e00\u79cd\u57fa\u4e8e\u5bc6\u5ea6\u6cdb\u51fd\u7406\u8bba\u7684\u5b9e\u7a7a\u95f4\u65b9\u6cd5\u6765\u8ba1\u7b97\u81ea\u65cb\u54c8\u5bc6\u987f\u91cf\u53c2\u6570\uff0c\u5176\u4e2d\u53ea\u5728\u5168\u7535\u5b50\u6c34\u5e73\u4e0a\u5904\u7406\u9009\u5b9a\u7684\u539f\u5b50\uff0c\u800c\u7cfb\u7edf\u7684\u5176\u4f59\u90e8\u5206\u7528\u8d5d\u52bf\u8fd1\u4f3c\u63cf\u8ff0\u3002\u7814\u7a76\u7684\u65b9\u6cd5\u5141\u8bb8\u8ba1\u7b97\u5305\u542b\u8d85\u8fc71000\u4e2a\u539f\u5b50\u7684\u7cfb\u7edf\uff0c\u5c31\u50cf\u91d1\u521a\u77f3\u548c\u78b3\u5316\u7845\u7684\u7f3a\u9677\u4e00\u6837\u3002\u7814\u7a76\u8868\u660e\uff0c\u53ea\u6709\u5c11\u6570\u539f\u5b50\u5468\u56f4\u7684\u7f3a\u9677\u9700\u8981\u5904\u7406\u5728\u5168\u7535\u5b50\u6c34\u5e73\uff0c\u4ee5\u83b7\u5f97\u4e00\u4e2a\u6574\u4f53\u5168\u7535\u5b50\u7cbe\u5ea6\u7684\u8d85\u7cbe\u7ec6\u548c\u96f6\u573a\u5206\u88c2\u5f20\u91cf\u3002\u7814\u7a76\u8fd8\u7ed9\u51fa\u4e86\u7528\u7c07\u76f8\u5173\u5c55\u5f00\u6cd5\u8ba1\u7b97\u7684\u76f8\u5e72\u65f6\u95f4\u7684\u7ed3\u679c\uff0c\u5f3a\u8c03\u4e86\u7cbe\u786e\u7684\u81ea\u65cb\u54c8\u5bc6\u987f\u91cf\u53c2\u6570\u5bf9\u4e8e\u5b9a\u91cf\u9884\u6d4b\u81ea\u65cb\u52a8\u529b\u5b66\u7684\u91cd\u8981\u6027\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cSpin\u2013spin interactions in defects in solids from mixed allelectron and pseudopotential first-principles calculations\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728npj Comput. Mater.\u4e0a\u3002DOI: 10.1038\/s41524-021-00590-w<\/p>\n<p>\u56fe6\u00a0\u4e24\u4e2a\u81ea\u65cb\u91cf\u5b50\u4f4d\u7cfb\u7edf\u7684\u81ea\u65cb\u5bc6\u5ea6<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-226046\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_6.png\" alt=\"\" width=\"600\" height=\"226\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_6.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_6-300x113.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>Nature Commun.\uff1a\u5355\u539f\u5b50\u8584\u7247AgInP<\/b><\/strong><strong><sub><b>2S6<\/b><\/sub><\/strong><strong><b>\u4e0aCO<\/b><\/strong><strong><sub><b>2<\/b><\/sub><\/strong><strong><b>\u5149\u8fd8\u539f\u7684\u7a7a\u4f4d-\u7f3a\u9677\u8c03\u5236\u8def\u5f84<\/b><\/strong><\/p>\n<p>\u4eba\u5de5\u5149\u5408\u4f5c\u7528\uff0c\u5373\u5149\u9a71\u52a8\u4e8c\u6c27\u5316\u78b3\u8f6c\u5316\u4e3a\u78b3\u6c22\u71c3\u6599\uff0c\u662f\u540c\u6b65\u514b\u670d\u5168\u7403\u53d8\u6696\u548c\u80fd\u6e90\u4f9b\u5e94\u95ee\u9898\u7684\u4e00\u4e2a\u6709\u524d\u9014\u7684\u7b56\u7565\u3002\u8fd1\u65e5\uff0c\u5357\u4eac\u5927\u5b66\u5468\u52c7\u3001\u4e2d\u79d1\u5927\u718a\u5b87\u6770\u7b49\u4eba\u62a5\u9053\u4e86\u901a\u8fc7\u7b80\u5355\u7684\u63a2\u9488\u8d85\u58f0\u5265\u79bb\u76f8\u5e94\u7684\u5927\u5757\u6676\u4f53\uff08BC\uff09\uff0c\u6210\u529f\u5236\u5907\u51fa\u539a\u5ea6\u7ea60.70 nm\u7684AgInP<sub>2<\/sub>S<sub>6<\/sub>\u5355\u539f\u5b50\u5c42\uff08SAL\uff09\u3002\u7136\u540e\u901a\u8fc7H<sub>2<\/sub>O<sub>2<\/sub>\u6eb6\u6db2\u523b\u8680\u5de5\u827a\u5728\u5f97\u5230\u7684SAL\u4e2d\u5f15\u5165\u786b\u7a7a\u4f4d\uff08VS\uff09\u7f3a\u9677\uff08VS-SAL\uff09\uff0c\u4ece\u800c\u7528\u4e8e\u5728\u6c34\u84b8\u6c14\u5b58\u5728\u4e0b\u7684\u5149\u50ac\u5316CO<sub>2<\/sub>\u8fd8\u539f\u3002\u4ea7\u7269\u9009\u62e9\u6027\u8fbe\u523073%\uff0c\u7535\u5b50\u9009\u62e9\u6027\u8fbe\u523089%\uff0c\u91cf\u5b50\u4ea7\u7387\u4e3a0.51%\u3002DFT\u8ba1\u7b97\u548c\u539f\u4f4dFTIR\u8c31\u56fe\u8868\u660e\uff0c\u7531\u4e8eAgInP<sub>2<\/sub>S<sub>6<\/sub>\u4e2dS\u7a7a\u4f4d\u7684\u5f15\u5165\uff0c\u5bfc\u81f4S\u7a7a\u4f4d\u9644\u8fd1Ag\u539f\u5b50\u7684\u7535\u8377\u79ef\u7d2f\uff0c\u66b4\u9732\u7684Ag\u4f4d\u70b9\u53ef\u4ee5\u6709\u6548\u6355\u83b7\u5f62\u6210\u7684*CO\u5206\u5b50\u3002\u4f7f\u50ac\u5316\u5242\u8868\u9762\u5bcc\u96c6\u4e86\u5173\u952e\u53cd\u5e94\u4e2d\u95f4\u4f53\uff0c\u964d\u4f4e\u4e86C-C\u7ed3\u5408\u7684\u5076\u8054\u969c\u788d\uff0c\u6709\u5229\u4e8e\u4e59\u70ef\u7684\u751f\u4ea7\u3002\u8fd9\u9879\u5de5\u4f5c\u6709\u671b\u4e3a\u8bbe\u8ba1\u7528\u4e8eCO<sub>2<\/sub>\u8fd8\u539f\u7684\u539f\u5b50\u8584\u5149\u50ac\u5316\u5242\u6846\u67b6\u63d0\u4f9b\u65b0\u7684\u89c1\u89e3\uff0c\u5e76\u4e3a\u91cd\u7533\u7f3a\u9677\u5de5\u7a0b\u5728\u8c03\u8282\u50ac\u5316\u6d3b\u6027\u548c\u9009\u62e9\u6027\u65b9\u9762\u7684\u591a\u529f\u80fd\u6027\u5efa\u7acb\u4e00\u4e2a\u7406\u60f3\u7684\u5e73\u53f0\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cVacancy-defect modulated pathway of\u00a0photoreduction of CO<sub>2<\/sub>\u00a0on single atomically thin\u00a0AgInP<sub>2<\/sub>S<sub>6<\/sub>\u00a0sheets into olefiant gas\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728Nature\u00a0Commun.\u4e0a\u3002DOI: 10.1038\/s41467-021-25068-7<\/p>\n<p>\u56fe7\u00a0\u5236\u5907\u7684SAL\u548cVS-SAL10\u7684\u5f62\u6001\u7ed3\u6784\u8868\u5f81<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-226047\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_7.png\" alt=\"\" width=\"600\" height=\"398\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_7.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-1_7-300x199.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>Angew.\uff1a\u9ad8\u8d1f\u8f7d\u91cf\u6c2e\u5316<\/b><\/strong><strong><b>\u78b3<\/b><\/strong><strong><b>\u57fa<\/b><\/strong><strong><b>\u94c1\u5355\u539f\u5b50\u50ac\u5316\u6d3b\u5316\u8fc7\u6c27\u5355\u786b\u9178\u6839<\/b><\/strong><strong><b>\uff0c<\/b><\/strong><strong><b>100%\u9009\u62e9<\/b><\/strong><strong><b>\u6027\u4ea7\u751f<\/b><\/strong><strong><sup><b>1<\/b><\/sup><\/strong><strong><b>O<\/b><\/strong><strong><sub><b>2<\/b><\/sub><\/strong><\/p>\n<p>\u5355\u7ebf\u6001\u6c27(<sup>1<\/sup>O<sub>2<\/sub>)\u662f\u9009\u62e9\u6027\u964d\u89e3\u6709\u673a\u6c61\u67d3\u7269\u7684\u4f18\u826f\u6d3b\u6027\u7269\u79cd\u3002\u7136\u800c\uff0c\u5728\u5236\u5907<sup>1<\/sup>O<sub>2<\/sub>\u7684\u8fc7\u7a0b\u4e2d\u5f88\u96be\u8fbe\u5230\u9ad8\u6548\u7387\u548c\u9009\u62e9\u6027\u3002\u5728\u672c\u5de5\u4f5c\u4e2d\uff0c\u5357\u660c\u822a\u7a7a\u5927\u5b66\u90b9\u5efa\u5e73\u6559\u6388\u7b49\u4eba\u5f00\u53d1\u4e86\u4e00\u79cd\u77f3\u58a8\u6c2e\u5316\u78b3\u8d1f\u8f7d\u7684\u5355\u539f\u5b50\u94c1\u50ac\u5316\u5242(Fe1\/CN)\uff0c\u8be5\u50ac\u5316\u5242\u542b\u6709\u9ad8\u5ea6\u5747\u5300\u7684Fe-N4\u6d3b\u6027\u4f4d\u70b9\uff0c\u9ad8\u94c1\u8d1f\u8f7d\u7387\u4e3a11.2 wt%\u3002Fe1\/CN\u901a\u8fc7\u6d3b\u5316\u8fc7\u6c27\u5355\u786b\u9178\u76d0(PMS)\u53ef\u751f\u6210100% <sup>1<\/sup>O<sub>2<\/sub>\uff0c\u5bf9\u6c2f\u915a\u7684\u964d\u89e3\u6548\u7387\u6781\u9ad8\u3002\u5bc6\u5ea6\u6cdb\u51fd\u7406\u8bba\u8ba1\u7b97\u7ed3\u679c\u8868\u660e\uff0c\u4e0eCo\u548cNi\u5355\u539f\u5b50\u4f4d\u76f8\u6bd4\uff0cFe1\/CN\u4e2d\u7684Fe-N4\u4f4d\u5438\u9644\u5728PMS\u7684\u672b\u7aefO\u4e0a\uff0c\u6709\u5229\u4e8ePMS\u6c27\u5316\u751f\u6210SO5\u2022-\uff0c\u5e76\u4ee5100%\u7684\u9009\u62e9\u6027\u9ad8\u6548\u751f\u6210<sup>1<\/sup>O<sub>2<\/sub>\u3002\u6b64\u5916\uff0cFe1\/CN\u5728PMS\u5b58\u5728\u4e0b\u964d\u89e3\u6709\u673a\u6c61\u67d3\u7269\u65f6\uff0c\u5bf9\u65e0\u673a\u79bb\u5b50\u3001\u5929\u7136\u6709\u673a\u7269\u548cpH\u503c\u8868\u73b0\u51fa\u8f83\u5f3a\u7684\u6297\u6027\u3002\u672c\u5de5\u4f5c\u5f00\u53d1\u4e86\u4e00\u79cd\u65b0\u578b\u50ac\u5316\u5242\uff0c100%\u9009\u62e9\u6027\u5730\u751f\u4ea7<sup>1<\/sup>O<sub>2<\/sub>\uff0c\u7528\u4e8e\u9ad8\u5ea6\u9009\u62e9\u6027\u548c\u9ad8\u6548\u5730\u964d\u89e3\u6c61\u67d3\u7269\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cCarbon Nitride Supported High-Loading Fe Single-Atom Catalyst for Activating of Peroxymonosulfate to Generate\u00a0<sup>1<\/sup>O<sub>2<\/sub>\u00a0with 100% Selectivity\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728Angew.\u4e0a\u3002DOI:\u00a010.1002\/ange.202109488<\/p>\n<p>\u56fe8\u00a0Fe1\/CN\u8868\u5f81<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-226048\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-33-2.png\" alt=\"\" width=\"491\" height=\"425\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-33-2.png 491w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/08\/\u56fe\u7247-33-2-300x260.png 300w\" sizes=\"(max-width: 491px) 100vw, 491px\" \/><\/p>\n<p>\u6587\u4e2d\u6240\u8ff0\u5982\u6709\u4e0d\u59a5\u4e4b\u5904\uff0c\u6b22\u8fce\u8bc4\u8bba\u533a\u7559\u8a00~<\/p>\n<p>\u672c\u6587\u7531Junas\u4f9b\u7a3f\u3002<\/p>\n<p>\u672c\u5185\u5bb9\u4e3a\u4f5c\u8005\u72ec\u7acb\u89c2\u70b9\uff0c\u4e0d\u4ee3\u8868\u6750\u6599\u4eba\u7f51\u7acb\u573a\u3002<\/p>\n<p>\u672a\u7ecf\u5141\u8bb8\u4e0d\u5f97\u8f6c\u8f7d\uff0c\u6388\u6743\u4e8b\u5b9c\u8bf7\u8054\u7cfbkefu@cailiaoren.com\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1: tougao@cailiaoren.com.<\/p>\n<p>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaorenVIP\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u5982\u4eca\uff0c\u7406\u8bba\u8ba1\u7b97\u4e0e\u5b9e\u9a8c\u76f8\u7ed3\u5408\u5df2\u7ecf\u6210\u4e86TOP\u671f\u520a\u6700\u4e3b\u6d41\u7684\u7814\u7a76\u65b9\u5f0f\uff0c\u5c24\u5176\u662f\u5728\u6d89\u53ca\u5230\u673a\u7406\u5206\u6790\u65b9\u9762\uff0c\u7406\u8bba\u8ba1\u7b97\u51e0\u4e4e\u5fc5\u4e0d\u53ef\u5c11\u3002\u7136\u800c\uff0c\u7406\u8bba\u8ba1\u7b97\u4e0e\u5b9e\u9a8c\u4e4b\u95f4\u4ecd\u7136\u5b58\u5728\u5f88\u5927\u7684\u9e3f\u6c9f\uff0c\u8bb8\u591a&#8230;<\/p>\n","protected":false},"author":11454,"featured_media":226049,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[1187],"tags":[],"class_list":["post-226040","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-zhuanlan"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/226040"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/11454"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=226040"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/226040\/revisions"}],"predecessor-version":[{"id":226051,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/226040\/revisions\/226051"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/226049"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=226040"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=226040"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=226040"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}