{"id":228861,"date":"2021-10-30T06:27:14","date_gmt":"2021-10-29T22:27:14","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=228861"},"modified":"2021-10-29T21:44:04","modified_gmt":"2021-10-29T13:44:04","slug":"mof%e9%bc%bb%e7%a5%96%e6%9c%80%e6%96%b0science%ef%bc%9a-%e6%94%b9%e5%96%84%e5%a4%a7%e6%b0%94%e9%9b%86%e6%b0%b4%e7%9a%84%e9%87%91%e5%b1%9e-%e6%9c%89%e6%9c%ba%e6%a1%86%e6%9e%b6%e4%b8%ad%e6%b0%b4","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=228861","title":{"rendered":"MOF\u9f3b\u7956\u6700\u65b0Science\uff1a\u00a0\u6539\u5584\u5927\u6c14\u96c6\u6c34\u7684\u91d1\u5c5e-\u6709\u673a\u6846\u67b6\u4e2d\u6c34\u7ed3\u6784\u7684\u6f14\u53d8"},"content":{"rendered":"<p>\u7b2c\u4e00\u4f5c\u8005\uff1aNikita Hanikel<\/p>\n<p>\u901a\u8baf\u4f5c\u8005\uff1aJoachim Sauer\uff0cLaura Gagliardi\uff0cOmar M. Yaghi<\/p>\n<p>\u6700\u8fd1\u53d1\u73b0\u591a\u5b54\u91d1\u5c5e\u6709\u673a\u6846\u67b6\uff08MOF\uff09\u53ef\u4ee5\u4ece\u6c99\u6f20\u4e2d\u63d0\u53d6\u5927\u6c14\u4e2d\u7684\u6c34\u6765\u751f\u4ea7\u996e\u7528\u6c34\u3002\u8fd9\u5c31\u5f15\u51fa\u4e86\u8fd9\u6837\u4e00\u4e2a\u95ee\u9898\uff1a\u8fd9\u4e9bMOF\u662f\u5982\u4f55\u4ece\u5e72\u65f1\u7684\u7a7a\u6c14\u4e2d\u201c\u62bd\u51fa\u201d\u6c34\u5206\u5e76\u8f7b\u6613\u91ca\u653e\u51fa\u6765\u7684\uff0c\u5c24\u5176\u662f\u5728\u5206\u5b50\u6c34\u5e73\u7684\u539f\u7406\u4e0a\u3002\u4e8b\u5b9e\u4e0a\uff0cMOF\u548c\u5408\u6210\u6676\u4f53\u4e2d\u6c34\u7ed3\u6784\u7684\u6f14\u53d8\u662f\u4eba\u4eec\u6240\u8ffd\u6c42\u7684\uff0c\u4f46\u5bf9\u5176\u5438\u6c34\u884c\u4e3a\u7684\u5b8c\u6574\u673a\u68b0\u7406\u89e3\u4ecd\u7136\u7f3a\u4e4f\u3002<\/p>\n<p>\u6765\u81ea<strong><b>\u52a0\u5229\u798f\u5c3c\u4e9a\u5927\u5b66\u4f2f\u514b\u5229\u5206\u6821\u3001\u6d2a\u5821\u5927\u5b66\u548c\u829d\u52a0\u54e5\u5927\u5b66<\/b><\/strong>\u7684\u5b66\u8005\u901a\u8fc7\u5927\u91cf\u7684\u5355\u6676x\u5c04\u7ebf\u884d\u5c04\u6d4b\u91cf\u548c\u5bc6\u5ea6\u6cdb\u51fd\u7406\u8bba\u8ba1\u7b97\uff0c\u89e3\u91ca\u4e86\u6700\u5148\u8fdb\u7684\u96c6\u6c34\u91d1\u5c5e\u6709\u673a\u9aa8\u67b6MOF-303\u7684\u5145\u6c34\u673a\u7406\u3002\u7b2c\u4e00\u6c34\u5206\u5b50\u4e0e\u6781\u6027\u6709\u673a\u8fde\u63a5\u7269\u5f3a\u7ed3\u5408\uff1b\u63a5\u7740\u662f\u989d\u5916\u7684\u6c34\u5206\u5b50\u5f62\u6210\u5b64\u7acb\u7684\u56e2\u7c07\uff0c\u7136\u540e\u5f62\u6210\u56e2\u7c07\u94fe\uff0c\u6700\u540e\u5f62\u6210\u6c34\u7f51\u7edc\u3002\u6c34\u7ed3\u6784\u7684\u8fd9\u79cd\u6f14\u53d8\u5bfc\u81f4\u6211\u4eec\u53ef\u4ee5\u901a\u8fc7\u591a\u5143\u65b9\u6cd5\u6765\u4fee\u6539\u5b54\u9699\uff0c\u4ece\u800c\u7cbe\u786e\u5730\u8c03\u8282\u7b2c\u4e00\u4e2a\u6c34\u5206\u5b50\u7684\u7ed3\u5408\u5f3a\u5ea6\uff0c\u5e76\u63a7\u5236\u5438\u6c34\u884c\u4e3a\u3002\u8fd9\u5bfc\u81f4\u4e86\u66f4\u9ad8\u7684\u4ea7\u6c34\u91cf\uff0c\u4ee5\u53ca\u518d\u751f\u6e29\u5ea6\u548c\u7113\u7684\u53ef\u8c03\u6027\uff0c\u5e76\u4e14\u4e0d\u4f1a\u5f71\u54cd\u5bb9\u91cf\u548c\u7a33\u5b9a\u6027\u3002\u76f8\u5173\u5de5\u4f5c\u4ee5\u9898\u4e3a\u201cEvolution of water structures in metal-organic frameworks for improved atmospheric water harvesting\u201d\u7684\u7814\u7a76\u6027\u6587\u7ae0\u5728\u300aScience\u300b\u4e0a\u53d1\u8868\u3002<\/p>\n<p>\u94fe\u63a5\uff1ahttps:\/\/www.science.org\/doi\/10.1126\/science.abj0890<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228862\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/\u56fe\u7247-1-11.png\" alt=\"\" width=\"600\" height=\"392\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/\u56fe\u7247-1-11.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/\u56fe\u7247-1-11-300x196.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>MOF-303\u7684\u5438\u6c34\u7b49\u6e29\u7ebf\u548c\u6676\u4f53\u7ed3\u6784<\/b><\/strong><\/p>\n<p>\u672c\u6587\u901a\u8fc7\u5355\u6676X\u5c04\u7ebf\u884d\u5c04(SCXRD)\u5b9a\u4f4d\u4e86\u5176\u5b54\u9699\u4e2d\u7684\u6240\u6709\u6c34\u5206\u5b50\uff0c\u5e76\u786e\u5b9a\u4e86\u586b\u5145\u8fd9\u4e9b\u4f4d\u7f6e\u7684\u9010\u4e2a\u5206\u5b50\u7684\u5e8f\u5217\uff0c\u4ece\u800c\u6210\u529f\u5730\u786e\u5b9a\u4e86MOF-303{[Al(OH)(PZDC)]\uff0c\u5176\u4e2dPZDC2-=1-H-\u5421\u5511-3\uff0c5-\u4e8c\u7fa7\u9178\u76d0}\u662f\u6700\u5148\u8fdb\u7684\u96c6\u6c34MOF(\u56fe1A)\u3002MOF-303\u7684\u7ed3\u6784\u662f\u57fa\u4e8e\u65e0\u9650\u68d2\u72b6\u7684\u6b21\u7ea7\u7ed3\u6784\u5355\u5143(SBUs)\uff0c\u7531\u4ea4\u66ff\u7684\u987a\u53cd\u89d2\u5171\u4eab\u7684AlO<sub>6<\/sub>\u516b\u9762\u4f53\u7ec4\u6210\uff0c\u8fd9\u4e9b\u516b\u9762\u4f53\u901a\u8fc7PZDC2\u8fde\u63a5\u4ef6\u8fde\u63a5(\u56fe1)\u3002\u8be5MOF\u7684\u62d3\u6251\u91cd\u5efa\u63d0\u4f9b\u4e86<strong><b>xhh<\/b><\/strong>\u62d3\u6251\u7ed3\u6784\u3002\u8fd9\u79cd\u6392\u5217\u5177\u6709\u76f8\u4e92\u6307\u5411\u7684\u76f8\u90bb\u5421\u5511\u5b98\u80fd\u56e2\uff0c\u5e76\u5f62\u6210\u7531\u6bcf\u4e2a\u8fde\u63a5\u57fa\u4e0a\u7684\u4e09\u4e2a\u03bc<sub>2<\/sub>-OH\u57fa\u56e2\u548c\u4e24\u4e2aN(H)\u9650\u5b9a\u7684\u53e3\u888b\u7ed3\u6784(\u56fe1A\u548cB)\u3002\u6c34\u5438\u9644\u5230\u8fd9\u79cd\u73af\u5883\u4e2d\u5bfc\u81f4\u4e86\u4e0d\u5bfb\u5e38\u7684\u6c34\u5438\u9644\u7b49\u6e29\u7ebf\uff0c\u5728\u4f4e\u84b8\u6c7d\u538b\u4e0b\uff0c\u7b49\u6e29\u7ebf\u663e\u793a\u51fa\u4e00\u4e2a\u5c0f\u7684\u4f46\u529f\u80fd\u4e0a\u6709\u5f71\u54cd\u7684\u6b65\u9aa4(\u6807\u8bb0\u4e3aS\uff1b\u56fe1A\u4e2d\u7684\u7ea2\u8272\u90e8\u5206)\u3002\u6b65\u9aa4S\u4f7f\u8be5MOF\u7684\u6bcf\u4e2a\u5faa\u73af\u7684\u96c6\u6c34\u4ea7\u91cf(\u5de5\u4f5c\u80fd\u529b)\u51cf\u5c11\u4e86\u7ea620wt%\uff0c\u5982\u679c\u5e7f\u6cdb\u5faa\u73af\uff0c\u8fd9\u79cd\u51cf\u5c11\u5c06\u5bfc\u81f4\u76f8\u5f53\u4e8e\u591a\u7684\u4ea7\u6c34\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228863\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/\u56fe\u7247-2-11.png\" alt=\"\" width=\"600\" height=\"301\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/\u56fe\u7247-2-11.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/\u56fe\u7247-2-11-300x151.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe1.MOF-303\u7684\u5438\u6c34\u7b49\u6e29\u7ebf\u548c\u6676\u4f53\u7ed3\u6784\u3002<\/p>\n<p><strong><b>MOF303\u4e2d<\/b><\/strong><strong><b>\u7684<\/b><\/strong><strong><b>\u79cd\u5b50\u6c34\u5438\u9644\u4f4d\u70b9\u7684\u6676\u4f53\u7ed3\u6784<\/b><\/strong><\/p>\n<p>SCXRD\u5206\u6790\u8868\u660e\uff0c\u9aa8\u67b6\u7684\u7b2c\u4e00\u4e2a\u4e5f\u662f\u6700\u5f3a\u7684\u5438\u6c34\u70b9\u4f4d\u4e8e\u5421\u5511\u4e4b\u95f4\uff0c\u5176\u4e2d\u6c34\u5206\u5b50\u4e0e\u4e24\u4e2a\u5421\u5511\u57fa\u56e2\u548c\u4e00\u4e2a\u03bc<sub>2<\/sub>-OH\u57fa\u56e2\u5f62\u6210\u4e86\u4e09\u4e2a\u6c22\u952e(H\u952e)\uff0c\u6742\u539f\u5b50\u4e4b\u95f4\u7684\u8ddd\u79bb\u5206\u522b\u4e3a2.797\u57c3\uff0c2.887\u57c3\u548c2.798\u57c3\u00a0(\u56fe2A)\u3002\u7b2c\u4e8c\u4e2a\u6c34\u5206\u5b50(II)\u4e5f\u4f4d\u4e8e\u5421\u5511\u4e4b\u95f4\uff0c\u5f62\u6210\u4e86\u4e24\u4e2a\u6c22\u952e\uff0cN\u22eeO<sub>water<\/sub>\u8ddd\u79bb\u5206\u522b\u4e3a2.72\u57c3\u548c2.96\u57c3(\u56fe2B)\u3002\u8fd9\u4e24\u4e2a\u4f4d\u70b9\u90fd\u4f4d\u4e8eMOF-303\u7684\u4eb2\u6c34\u6027\u53e3\u888b\u5185\uff0c\u5e76\u53ef\u80fd\u4e0e\u4f4e\u84b8\u6c7d\u538b\u4e0b\u7684\u6b65\u9aa4S\u6709\u5173\u3002\u4e0b\u4e00\u4e2a\u6c34\u5206\u5b50\u5360\u636e\u4e86\u7b2c\u4e09\u4f4d\uff0c\u53ea\u4e0e\u5269\u4f59\u7684\u03bc<sub>2<\/sub>-OH\u57fa\u56e2\u57282.89\u57c3\u7684\u8ddd\u79bb\u4e0a\u76f8\u4e92\u4f5c\u7528(\u56fe2C)\u3002\u7b2c\u56db\u4e2a\u6c34\u5206\u5b50(IV)\u4e0eI\u548cII\u5904\u7684\u6c34\u5206\u5b50\u6c22\u952e\uff0c\u4f46\u4e0d\u4e0e\u9aa8\u67b6\u76f8\u8fde\uff0c\u4ece\u800c\u5f62\u6210\u4e00\u4e2a\u4e09\u805a\u4f53\u7c07\u5408\u7269(I\uff0cII\u548cIV\uff1b\u56fe2D)\uff0cIII\u5904\u7684\u6c34\u5206\u5b50\u4ecd\u7136\u4e0e\u5176\u5206\u79bb\u3002\u5728\u8fd9\u4e2a\u52a0\u8f7d\u9636\u6bb5\uff0c\u8fd9\u6837\u7684\u57fa\u56e2\u4e0e\u90bb\u8fd1\u5bf9\u79f0\u7b49\u6548\u53e3\u888b\u4e2d\u7684\u5176\u4ed6\u57fa\u56e2\u662f\u9694\u79bb\u7684(\u56fe2E)\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228864\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/\u56fe\u7247-3-12.png\" alt=\"\" width=\"600\" height=\"335\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/\u56fe\u7247-3-12.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/\u56fe\u7247-3-12-300x168.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe2.MOF303\u4e2d\u79cd\u5b50\u6c34\u5438\u9644\u4f4d\u70b9\u7684\u6676\u4f53\u7ed3\u6784\u3002<\/p>\n<p><strong><b>\u8d1f\u8377\u589e\u52a0\u65f6MOF-303\u6c34\u7ed3\u6784\u7684\u6f14\u53d8<\/b><\/strong><\/p>\n<p>\u7ed3\u6676\u5b66\u7814\u7a76\u8868\u660e\uff0c\u53e6\u5916\u5438\u9644\u7684\u6c34\u5206\u5b50\u662f\u901a\u8fc7\u4e0e\u5176\u4ed6\u6c34\u5206\u5b50\u76f8\u4e92\u4f5c\u7528\u800c\u4e0d\u662f\u4e0e\u9aa8\u67b6\u672c\u8eab\u76f8\u4e92\u4f5c\u7528\u6765\u586b\u5145\u5b54\u9699\u7684(\u56fe3)\u3002\u5728V\u548cVI\u4e0a\u5438\u9644\u4e24\u4e2a\u989d\u5916\u7684\u6c34\u5206\u5b50\u4ea7\u751f\u4e86\u4e00\u79cd\u7ed3\u6784\uff0c\u5176\u4e2d\u76f8\u90bb\u7684\u7c07(I\uff0cII\u548cIV)\u901a\u8fc7\u65b0\u7684\u6c34\u56db\u805a\u4f53\u7c07\u76f8\u4e92\u8fde\u63a5(\u56fe3A)\u3002\u5f53\u5728VII\u548cVIII\u6dfb\u52a0\u6c34\u5206\u5b50\u65f6\uff0c\u56db\u805a\u4f53\u8f6c\u53d8\u4e3a\u516d\u805a\u4f53(V\u5230VII)\uff0c\u5728VIII\u6709\u4e00\u4e2a\u60ac\u6302\u7684\u6c34\u5206\u5b50\u8fde\u63a5\u5230VII(\u56fe3B)\u3002\u5728\u8f83\u9ad8\u7684\u6c34\u8d1f\u8377\u4e0b\uff0c\u7b2cIX\u81f3XIV\u4f4d\u7684\u987a\u5e8f\u90e8\u5206\u586b\u5145\u4e0e\u5b8c\u5168\u5360\u636e\u7684\u7b2cI\u81f3VIII\u4f4d\u4e00\u8d77\u4ea7\u751f\u4e86\u7fa4\u96c6\u5355\u5143\u7684\u65e0\u9650\u6c22\u952e\u6c34\u94fe(\u56fe1A\u4e2d\u7684\u84dd\u8272\u90e8\u5206)\u3002\u9996\u5148\uff0c\u76f8\u4e92\u6392\u65a5\u7684\u65e0\u5e8f\u4f4d\u70b9IX\u548cX\u540c\u65f6\u88ab\u586b\u5145\uff0c\u76f8\u5173\u7684\u6c34\u5206\u5b50\u5728II\u3001IV\u548cVIII\u4e0e\u6c34\u5206\u5b50H\u952e(\u56fe3C)\u3002\u7b2c\u4e8c\uff0c\u8fde\u63a5\u5230II\u3001IV\u548cVII\u7684XI\u4f4d\u70b9\u88ab\u90e8\u5206\u586b\u6ee1(\u56fe3D)\u3002\u7b2c\u4e09\uff0cXII\u7ad9\u70b9\u7684\u90e8\u5206\u79cd\u7fa4\u8fde\u63a5II\u3001III\u548cVIII(\u56fe3E)\u3002\u8fd9\u4e9b\u5bf9\u6c34\u7f51\u7edc\u6846\u67b6\u7684\u6539\u53d8\u548c\u91cd\u7ec4\u5bfc\u81f4\u4e86XIV\u4f4d\u70b9\u7684\u90e8\u5206\u586b\u5145\uff0c\u5176\u4e2d\u6c34\u5206\u5b50H\u4e0e\u7fa7\u57fa\u7684O\u539f\u5b50\u76f8\u8fde(\u56fe3F)\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228865\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/\u56fe\u7247-4-12.png\" alt=\"\" width=\"600\" height=\"724\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/\u56fe\u7247-4-12.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/\u56fe\u7247-4-12-249x300.png 249w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe3.\u8d1f\u8377\u589e\u52a0\u65f6MOF-303\u6c34\u7ed3\u6784\u7684\u6f14\u53d8\u3002<\/p>\n<p><strong><b>\u591a\u53d8\u91cfMOF\u5e8f\u5217\u7684\u7279\u5f81<\/b><\/strong><\/p>\n<p>\u63a5\u4e0b\u6765\uff0c\u672c\u6587\u5bf9MOF-333\u8fdb\u884c\u4e86\u5438\u6c34\u5206\u6790\uff0c\u89c2\u5bdf\u5230\u7406\u60f3\u5f62\u72b6\u7684\u5438\u6c34\u7b49\u6e29\u7ebf\uff0c\u572822%\u76f8\u5bf9\u6e7f\u5ea6\u4e0b\u6709\u4e00\u4e2a\u9661\u5ced\u7684\u53f0\u9636\uff0c\u5e76\u4e14\u6ca1\u6709\u89c2\u5bdf\u5230MOF-303\u7684\u53f0\u9636\uff08\u56fe4A\uff09\u3002\u672c\u6587\u8bbe\u7f6e\u4e86\u4e00\u4e2a\u8f83\u4f4e\u7684\u76f8\u5bf9\u6e7f\u5ea6\u622a\u6b62\u503c\uff0c\u5728\u8be5\u503c\u4e0b\uff0c\u672c\u6587\u7684\u65b0MOF\u53ef\u4ee5\u8fd0\u884c\u3002\u4e3a\u4e86\u5c06\u5176\u5de5\u4f5c\u8303\u56f4\u6269\u5c55\u5230\u66f4\u5e72\u65f1\u7684\u6761\u4ef6\uff0c\u672c\u6587\u5236\u5907\u4e86\u4e00\u7cfb\u5217\u7531PZDC2-\u548cFDC2-\u7ec4\u6210\u7684\u591a\u5143MOF\u3002\u7c89\u672bx\u5c04\u7ebf\u884d\u5c04\uff08PXRD\uff09\u5206\u6790\u8868\u660e\uff0c\u6240\u6709\u4e5d\u79cd\u4ea7\u54c1\u5747\u4e3a\u540c\u6784\u3002\u901a\u8fc7\u5bf9\u5b8c\u5168\u78b1\u6c34\u89e3MOF\u6676\u4f53\u7684\u6838\u78c1\u5171\u632f\uff08NMR\uff09\u5206\u6790\u548c\u5143\u7d20\u5fae\u91cf\u5206\u6790\u786e\u5b9a\u7684\u591a\u5143\u5e8f\u5217\u4e2d\u6bcf\u4e2aMOF\u7684\u8fde\u63a5\u7269\u6bd4\u7387\u51e0\u4e4e\u4e0e\u8f93\u5165\u6bd4\u7387\u6210\u6b63\u6bd4\uff08\u56fe4B\uff09\u3002<img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228866\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/\u56fe\u7247-5-6.png\" alt=\"\" width=\"600\" height=\"734\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/\u56fe\u7247-5-6.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/\u56fe\u7247-5-6-245x300.png 245w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe4.\u591a\u53d8\u91cfMOF\u5e8f\u5217\u7684\u7279\u5f81<\/p>\n<p><strong>\u7ed3\u8bed<\/strong><\/p>\n<p>\u672c\u6587\u7684\u65b9\u6cd5\u53ef\u7528\u4e8e\u8bbe\u8ba1\u5177\u6709\u8d85\u4f4e\u89e3\u5438\u6e29\u5ea6\u7684\u5438\u6c34\u5242\uff0c\u5982\u20188\/0\u2019\u3001\u20184\/4\u2019\u548c\u20180\/8\u2019\u5728\u6c34\u84b8\u6c14\u538b\u529b\u4ecb\u4e8e0.85\u81f31.70 kPa\uff08\u76f8\u5f53\u4e8e30\u2103\u4e0b20%\u81f340%RH\uff09\u4e0b\u7684\u7b49\u538b\u89e3\u5438\u66f2\u7ebf\u6240\u793a\u3002\u7b49\u538b\u7ebf\u5448\u73b0\u51fa\u4e00\u4e2a\u9661\u5ced\u7684\u53f0\u9636\uff0c\u968f\u7740\u84b8\u6c7d\u538b\u7684\u5347\u9ad8\u800c\u589e\u52a0\u3002\u6700\u540e\uff0c\u672c\u6587\u8bc1\u5b9e\uff0c\u5728\u4e00\u4e2aMOF\u6676\u4f53\u4e2d\u6df7\u5408PZDC<sup>2-<\/sup>\u548cFDC<sup>2-<\/sup>\u4e0d\u4f1a\u635f\u5bb3\u5355\u94fe\u6846\u67b6\u7684\u6c34\u89e3\u7a33\u5b9a\u6027\uff0c\u65b9\u6cd5\u662f\u5c06\u201c4\/4\u201d\u66b4\u9732\u57281.7kPa\u7684\u6c34\u84b8\u6c14\u538b\u529b\u4e0b\uff0c\u5e76\u572830\u00b0\u523085\u00b0C\u4e4b\u95f4\u5faa\u73af\u6e29\u5ea6\u3002\u8fd9\u4e00\u6d4b\u8bd5\u53ef\u9760\u5730\u9a8c\u8bc1\u4e86MOF\u7684\u5bff\u547d\u3002\u57282000\u6b21\u5438\u9644\u548c\u91ca\u653e\u5faa\u73af\u540e\uff0c\u5438\u9644\u5242\u7684\u5de5\u4f5c\u5bb9\u91cf\u4fdd\u6301\u572897%\u5de6\u53f3\u3002<\/p>\n<p>\u672c\u6587\u7531SSC\u4f9b\u7a3f\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u7b2c\u4e00\u4f5c\u8005\uff1aNikita Hanikel \u901a\u8baf\u4f5c\u8005\uff1aJoachim Sauer\uff0cLaura Gagliardi\uff0cOmar M. Yaghi \u6700\u8fd1\u53d1\u73b0\u591a\u5b54\u91d1\u5c5e\u6709\u673a\u6846&#8230;<\/p>\n","protected":false},"author":11454,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-228861","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/228861"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/11454"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=228861"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/228861\/revisions"}],"predecessor-version":[{"id":228925,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/228861\/revisions\/228925"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=228861"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=228861"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=228861"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}