{"id":229340,"date":"2021-11-08T06:48:40","date_gmt":"2021-11-07T22:48:40","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=229340"},"modified":"2021-11-07T20:48:50","modified_gmt":"2021-11-07T12:48:50","slug":"10%e6%9c%88nature-science%e7%9b%98%e7%82%b9%ef%bc%9a%e4%b8%ad%e7%a7%91%e5%a4%a7%e5%8c%97%e8%88%aa%e5%87%ad%e7%87%83%e6%96%99%e7%94%b5%e6%b1%a0%e7%99%bbscience%ef%bc%8c%e6%9c%a8%e5%a4%b4%e5%a4%a7","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=229340","title":{"rendered":"10\u6708Nature\/Science\u76d8\u70b9\uff1a\u4e2d\u79d1\u5927&#038;\u5317\u822a\u51ed\u71c3\u6599\u7535\u6c60\u767bScience\uff0c\u6728\u5934\u5927\u738b\u8fde\u7eed\u4e24\u5929\u53d1\u9876\u520a"},"content":{"rendered":"<p>\u672c\u7bc7\u6587\u7ae0\u4e3a\u5927\u5bb6\u68b3\u7406\u4e8610\u6708\u4efd\u6750\u6599\u3001\u5316\u5b66\u9886\u57dfNS\u53d1\u6587\u60c5\u51b5\u3002\u76f8\u5173\u6210\u679c\u5df2\u6536\u5f55\u5165\u6750\u6599\u4eba\u6700\u65b0\u4e0a\u7ebf\u4ea7\u54c1\u5e93\u3002<\/p>\n<p><strong>1. Nature\uff1a\u8ba9\u6240\u6709\u4eba\u559d\u4e0a\u53ef\u996e\u7528\u6c34<\/strong><\/p>\n<p><strong>X<\/strong><strong>\u767b\u6708\u8ba1\u5212\u5de5\u5382<\/strong><strong>Jackson Lord<\/strong><strong>\u3001<\/strong><strong>Philipp H. Schmaelzle<\/strong>\uff08\u901a\u8baf\u4f5c\u8005\uff09\u7b49\u4eba\u9610\u91ca\u4e86\u5982\u4f55\u5229\u7528AWH\u4e3a\u5341\u4ebf\u4eba\u63d0\u4f9bSMDW\u7684\u65b9\u6848\u3002\u5229\u7528\u8c37\u6b4c\u5730\u7403\u5f15\u64ce\uff0c\u4f5c\u8005\u5f15\u5165\u4e86\u5047\u5b9a\u7684\u4e00\u5e73\u65b9\u7c73\u8bbe\u5907\uff0c\u53d1\u73b0\u76f8\u5bf9\u6e7f\u5ea6\u4ece30%\u523090%\u65f6\uff0cSY\u66f2\u7ebf\u5219\u4ece0.2\u4e0a\u5347\u81f32.5\u5347\/\u5343\u74e6\u65f6(\u5bf9\u4e8e2\u5e73\u65b9\u7c73\u8bbe\u5907\uff0cSY\u66f2\u7ebf\u5219\u4ece0.1\u4e0a\u5347\u81f31.25\u5347\/\u5343\u74e6\u65f6)\u3002\u8fd9\u4e00\u8bbe\u5907\u8868\u73b0\u53ef\u4ee5\u6ee1\u8db3\u6bcf\u4eba\u6bcf\u5929\u5e73\u57475\u5347\u996e\u7528\u6c34\u9700\u6c42\u6307\u6807\u3002\u6b64\u5916\uff0c\u4f5c\u8005\u8fd8\u5206\u6790\u7ed8\u5236\u4e86\u73b0\u6709\u8bbe\u5907\u548c\u65b0\u578b\u5438\u9644\u5242\u7c7b\u522b\u7684\u5f71\u54cd\u6f5c\u529b\uff0c\u8ba4\u4e3a\u968f\u7740\u6280\u672f\u7684\u4e0d\u65ad\u8fdb\u6b65\uff0c\u5728\u70ed\u529b\u5b66\u6781\u9650\u4e4b\u5185\u5b8c\u5168\u53ef\u4ee5\u8fbe\u5230\u4e0a\u8ff0\u6307\u6807\u3002\u4e8b\u5b9e\u4e0a\uff0c\u8fd9\u4e9b\u6027\u80fd\u6307\u6807\u5df2\u7ecf\u5728\u5438\u9644\u5242\u6750\u6599\u7684\u76f8\u5173\u5b9e\u9a8c\u4e2d\u4ed8\u8bf8\u5b9e\u73b0\u3002\u603b\u800c\u8a00\u4e4b\uff0c\u8be5\u7814\u7a76\u63d0\u4f9b\u7684\u5de5\u5177\u53ef\u4ee5\u4e3a\u65e8\u5728\u6700\u5927\u5316\u5168\u7403\u5f71\u54cd\u529b\u7684\u5927\u6c14\u6c34\u5bcc\u96c6\u8bbe\u5907\u5f00\u8f9f\u65b0\u7684\u8bbe\u8ba1\u601d\u8def\uff0c\u540c\u65f6\u8fd8\u53ef\u4ee5\u4e3a\u5229\u7528\u73b0\u6709\u6280\u672f\u5b9e\u73b0\u53ef\u6301\u7eed\u53d1\u5c55\u76ee\u6807(SDGs)\u7684\u6301\u7eed\u52aa\u529b\u63d0\u4f9b\u4fe1\u606f\u548c\u5e2e\u52a9\u3002Jackson Lord\u540c\u65f6\u4e5f\u4e3a\u7b2c\u4e00\u4f5c\u8005\uff0c2021\u5e7410\u670827\u65e5\uff0c\u76f8\u5173\u6210\u679c\u4ee5\u9898\u4e3a\u201c<strong>Global potential for harvesting drinking water from air using solar energy<\/strong>\u201d\u7684\u6587\u7ae0\u53d1\u8868\u5728<strong>Nature<\/strong>\u4e0a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228951\" src=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/1-10.jpg\" sizes=\"(max-width: 600px) 100vw, 600px\" srcset=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/1-10.jpg 600w, http:\/\/dn.cailiaoniu.com\/2021\/10\/1-10-300x276.jpg 300w\" alt=\"\" width=\"600\" height=\"552\" \/><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"https:\/\/www.nature.com\/articles\/s41586-021-03900-w\" target=\"_blank\" rel=\"noopener\">Global potential for harvesting drinking water from air using solar energy<\/a>\uff08Nature, 2021, DOI: 10.1038\/s41586-021-03900-w\uff09<\/p>\n<p><strong>2. Nature\uff1aSnO2\u7535\u6781\u4e0a\u5177\u6709\u539f\u5b50\u76f8\u5e72\u5c42\u7684\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60<\/strong><\/p>\n<p>\u6765\u81ea\u97e9\u56fd\u6d66\u9879\u79d1\u6280\u5927\u5b66Min Gyu Kim\u548c\u97e9\u56fd\u851a\u5c71\u56fd\u7acb\u79d1\u5b66\u6280\u672f\u9662Tae Joo Shin\u3001Sang Il Seok\u8bfe\u9898\u7ec4\uff0c\u62a5\u9053\u4e86\u9499\u949b\u77ff\u8584\u819c\u548c\u7528\u542bCl\u7684FAPbI<sub>3<\/sub>\u9499\u949b\u77ff\u524d\u9a71\u4f53(Cl-cPP)\u6eb6\u6db2\u6d82\u8986\u7684Cl<sup>&#8211;<\/sup>\u952e\u5408SnO<sub>2<\/sub>\u00a0(Cl-bSO)\u7535\u6781\u4e4b\u95f4\u7684\u76f8\u5e72\u5939\u5c42\u7684\u5f62\u6210\u3002\u672c\u5de5\u4f5c\u901a\u8fc7\u8868\u9762\u654f\u611f\u7684\u63a0\u5165\u5c04X\u5c04\u7ebf\u5438\u6536\u7cbe\u7ec6\u7ed3\u6784(XAFS)\uff0c\u540c\u6b65\u8f90\u5c04\u63a0\u5165\u5c04\u5e7f\u89d2X\u5c04\u7ebf\u884d\u5c04(GI-WAXD)\u548c\u9ad8\u5206\u8fa8\u900f\u5c04\u7535\u5b50\u663e\u5fae\u955c(HR-TEM)\u63a2\u7a76\u4e86\u8fd9\u79cd\u5939\u5c42\u7684\u5b58\u5728\u3002\u901a\u8fc7\u8fd9\u4e9b\u5206\u6790\u8868\u5f81\uff0c\u672c\u5de5\u4f5c\u63a8\u65ad<strong><b>\u5728\u9499\u949b\u77ff\u548cSnO<\/b><\/strong><strong><sub><b>2<\/b><\/sub><\/strong><strong><b>\u4e4b\u95f4\u5f62\u6210\u4e86\u6676\u6001\u7684FASnCl<\/b><\/strong><strong><sub><b>x<\/b><\/sub><\/strong><strong><b>\u76f8\u4f5c\u4e3a\u539f\u5b50\u5171\u683c\u7684\u4e2d\u95f4\u5c42\u3002\u8fd9\u79cd\u9499\u949b\u77ff\u548cETL\u4e4b\u95f4\u7684\u4e2d\u95f4\u5c42\u964d\u4f4e\u4e86\u754c\u9762\u7535\u8377\u590d\u5408\u635f\u5931\u548c\u63a5\u89e6\u7535\u963b\uff0c\u4ece\u800c\u5b9e\u73b0\u4e86\u529f\u7387\u8f6c\u6362\u6548\u7387\u4e3a25.8%\u7684PSC<\/b><\/strong>\u3002\u76f8\u5173\u8bba\u6587\u4ee5\u9898\u4e3a\u201cPerovskite solar cells with atomically coherent interlayers on SnO<sub>2\u00a0<\/sub>electrodes\u201d\u53d1\u8868\u5728Nature\u4e0a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228736\" src=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/%E5%9B%BE%E7%89%87-183.png\" sizes=\"(max-width: 600px) 100vw, 600px\" srcset=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/\u56fe\u7247-183.png 600w, http:\/\/dn.cailiaoniu.com\/2021\/10\/\u56fe\u7247-183-300x228.png 300w\" alt=\"\" width=\"600\" height=\"456\" \/><\/p>\n<p>\u8bba\u6587doi\uff1a<\/p>\n<p>https:\/\/doi-org-443.webvpn.bjmu.edu.cn\/10.1038\/s41586-021-03964-8<\/p>\n<p><strong>3. \u80e1\u826f\u5175\u56fa\u6001\u7535\u6c60Nature<\/strong><\/p>\n<p>\u7f8e\u56fd\u5e03\u6717\u5927\u5b66Yue Qi\u3001\u7f8e\u56fd\u9a6c\u91cc\u5170\u5927\u5b66\u80e1\u826f\u5175\u6559\u6388\u8bfe\u9898\u7ec4<strong>\u63a2\u7d22\u4e86\u4e00\u79cd\u805a\u5408\u7269\u79bb\u5b50\u5bfc\u4f53\u7684\u8bbe\u8ba1\u7b56\u7565\uff0c\u5373\u6269\u5c55\u5206\u5b50\u95f4\u805a\u5408\u7269\u7ed3\u6784\uff0c\u5c06Li<\/strong><strong><sup>+<\/sup><\/strong><strong>\u7684\u8f93\u8fd0\u4e0e\u805a\u5408\u7269\u7684\u8282\u6bb5\u5f1b\u8c6b\u89e3\u8026\uff0c\u4ece\u800c\u83b7\u5f97\u9ad8\u79bb\u5b50\u7535\u5bfc\u7387<\/strong>\u3002\u672c\u5de5\u4f5c\u8868\u660e\uff0c\u901a\u8fc7\u94dc\u79bb\u5b50(Cu<sup>2+<\/sup>)\u4e0e\u4e00\u7ef4\u7ea4\u7ef4\u7d20\u7eb3\u7c73\u7ea4\u7ef4\u7684\u914d\u4f4d\uff0c\u5728\u901a\u5e38\u79bb\u5b50\u7edd\u7f18\u7684\u7ea4\u7ef4\u7d20\u4e2d\uff0c\u5206\u5b50\u901a\u9053\u7684\u5f00\u653e\u53ef\u4ee5\u4f7fLi+\u79bb\u5b50\u6cbf\u7740\u805a\u5408\u7269\u94fe\u5feb\u901f\u4f20\u8f93\u3002\u9664\u4e86\u5177\u6709\u8f83\u9ad8\u7684Li<sup>+<\/sup>\u7535\u5bfc\u7387\u5916\uff0cCu<sup>2+<\/sup>\u914d\u4f4d\u7684\u7ea4\u7ef4\u7d20\u79bb\u5b50\u5bfc\u4f53\u8fd8\u5177\u6709\u8f83\u9ad8\u7684\u8fc1\u79fb\u6570(0.78\uff0c\u800c\u5176\u4ed6\u805a\u5408\u7269\u4ec5\u4e3a0.2~0.5)\u548c\u8f83\u5bbd\u7684\u7535\u5316\u5b66\u7a33\u5b9a\u7a97\u53e3(0-4.5V)\uff0c\u53ef\u4ee5\u540c\u65f6\u5bb9\u7eb3Li\u91d1\u5c5e\u8d1f\u6781\u548c\u9ad8\u7535\u538b\u6b63\u6781\u3002\u8fd9\u79cd\u4e00\u7ef4\u79bb\u5b50\u5bfc\u4f53\u8fd8\u5141\u8bb8\u5728\u539a\u7684LiFePO<sub>4<\/sub>\u56fa\u6001\u6b63\u6781\u4e2d\u8fdb\u884c\u79bb\u5b50\u6e17\u900f\uff0c\u4ee5\u5e94\u7528\u4e8e\u5177\u6709\u9ad8\u80fd\u91cf\u5bc6\u5ea6\u7684\u7535\u6c60\u3002\u6b64\u5916\uff0c\u672c\u5de5\u4f5c\u8fd8\u9a8c\u8bc1\u4e86\u8fd9\u79cd\u5206\u5b50\u901a\u9053\u5de5\u7a0b\u65b9\u6cd5\u4e0e\u5176\u4ed6\u805a\u5408\u7269\u548c\u9633\u79bb\u5b50\u7684\u666e\u9002\u6027\uff0c\u5b9e\u73b0\u4e86\u7c7b\u4f3c\u7684\u9ad8\u7535\u5bfc\u7387\uff0c\u5176\u610f\u4e49\u53ef\u80fd\u8d85\u8d8a\u5b89\u5168\u3001\u9ad8\u6027\u80fd\u7684\u56fa\u6001\u7535\u6c60\u8303\u7574\u3002<strong>\u76f8\u5173\u7814\u7a76\u6210\u679c\u4ee5\u201cCopper-coordinated cellulose ion conductors for solid-state batteries\u201d\u4e3a\u9898\u53d1\u8868\u5728Nature\u4e0a<\/strong>\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-229343\" src=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/1-15.jpg\" sizes=\"(max-width: 584px) 100vw, 584px\" srcset=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/1-15.jpg 584w, http:\/\/dn.cailiaoniu.com\/2021\/10\/1-15-229x300.jpg 229w\" alt=\"\" width=\"584\" height=\"764\" \/><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a\u201cCopper-coordinated cellulose ion conductors for solid-state batteries\u201d. Nature (2021). https:\/\/doi-org-443.webvpn.bjmu.edu.cn\/10.1038\/s41586-021-03885-6\u00a0<\/p>\n<p><strong>4. Nature\uff1a\u7535\u8377\u590d\u5408\u5bf9\u6709\u673a\u592a\u9633\u7535\u6c60\u4e2d\u4e09\u91cd\u6001\u6fc0\u5b50\u7684\u4f5c\u7528<\/strong><\/p>\n<p>\u6765\u81ea\u5251\u6865\u5927\u5b66\uff0c\u8499\u65af\u5927\u5b66\uff0c\u52a0\u5dde\u5927\u5b66\u5723\u5df4\u5df4\u62c9\u5206\u6821\u7684\u79d1\u7814\u56e2\u961f\u53d1\u73b0\u5728\u5927\u591a\u6570\u4f7f\u7528NFA\u7684\u6709\u673a\u592a\u9633\u80fd\u7535\u6c60\u4e2d\uff0c\u5f00\u8def\u6761\u4ef6\u4e0b\u7684\u5927\u90e8\u5206\u7535\u8377\u590d\u5408\u662f\u901a\u8fc7\u5f62\u6210\u975e\u53d1\u5c04\u7684NFA\u4e09\u91cd\u6001\u6fc0\u5b50\u8fdb\u884c\u7684\uff1b\u5728\u57fa\u51c6PM6:Y6\u6df7\u5408\u7269\u4e2d\u8fd9\u4e00\u6bd4\u4f8b\u8fbe\u523090%\uff0c\u4ece\u800c\u4f7f\u5f00\u8def\u7535\u538b\u964d\u4f4e60mV\u3002\u672c\u6587\u901a\u8fc7\u8bbe\u8ba1NFA\u4e09\u91cd\u6001\u6fc0\u5b50\u548c\u81ea\u65cb\u4e09\u91cd\u6001\u7535\u8377\u8f6c\u79fb\u6fc0\u5b50\u4e4b\u95f4\u7684\u5b9e\u8d28\u6027\u6742\u4ea4\u6765\u963b\u6b62\u901a\u8fc7\u8fd9\u79cd\u65e0\u8f90\u5c04\u901a\u9053\u7684\u590d\u5408\u3002\u6a21\u578b\u8868\u660e\uff0c\u4ece\u81ea\u65cb\u4e09\u91cd\u6001\u7535\u8377\u8f6c\u79fb\u6fc0\u5b50\u5230\u5206\u5b50\u4e09\u91cd\u6001\u6fc0\u5b50\u7684\u80cc\u7535\u8377\u8f6c\u79fb\u901f\u7387\u53ef\u4ee5\u964d\u4f4e\u4e00\u4e2a\u6570\u91cf\u7ea7\uff0c\u4f7f\u81ea\u65cb\u4e09\u91cd\u6001\u7535\u8377\u8f6c\u79fb\u6fc0\u5b50\u91cd\u65b0\u89e3\u79bb\u3002\u672c\u6587\u5c55\u793a\u4e86\u6291\u5236\u4e09\u91cd\u6001\u6fc0\u5b50\u5f62\u6210\u7684NFA\u7cfb\u7edf\u3002\u8fd9\u9879\u5de5\u4f5c\u4e3a\u592a\u9633\u80fd\u7535\u6c60\u7684\u8bbe\u8ba1\u63d0\u4f9b\u4e86\u4e00\u6761\u9014\u5f84\uff0c\u5176\u80fd\u91cf\u8f6c\u6362\u6548\u7387\u53ef\u8fbe20%\u6216\u66f4\u9ad8\u3002\u76f8\u5173\u5de5\u4f5c\u4ee5\u9898\u4e3a\u201cThe role of charge recombination to triplet excitons in organic solar cells\u201d\u7684\u6587\u7ae0\u5728\u300aNature\u300b\u53d1\u8868\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228011\" src=\"http:\/\/dn.cailiaoniu.com\/2021\/09\/%E5%9B%BE%E7%89%87-2-13.png\" sizes=\"(max-width: 600px) 100vw, 600px\" srcset=\"http:\/\/dn.cailiaoniu.com\/2021\/09\/\u56fe\u7247-2-13.png 600w, http:\/\/dn.cailiaoniu.com\/2021\/09\/\u56fe\u7247-2-13-285x300.png 285w\" alt=\"\" width=\"600\" height=\"632\" \/><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1aThe role of charge recombination to triplet excitons in organic solar cells\u201d. Nature (2021). The role of charge recombination to triplet excitons in organic solar cells | Nature<\/p>\n<p><strong>5. \u51af\u65b0\u4eaeNature\uff1a\u7eaf\u6709\u673a\u6750\u6599\u4e2d\u7684\u5f3a\u76f8\u5173\u6027<\/strong><\/p>\n<p>\u6765\u81ea\u5fb7\u56fd\u5fb7\u7d2f\u65af\u987f\u5de5\u4e1a\u5927\u5b66\u548c\u9a6c\u666e\u5fae\u7ed3\u6784\u7269\u7406\u7814\u7a76\u6240\u7684<strong>\u51af\u65b0\u4eae<\/strong>\u3001\u745e\u58eb\u8054\u90a6\u6750\u6599\u79d1\u5b66\u4e0e\u6280\u672f\u5b9e\u9a8c\u5ba4\u7684Pascal Ruffieux\u3001\u8461\u8404\u7259\u56fd\u9645\u4f0a\u6bd4\u5229\u4e9a\u7eb3\u7c73\u6280\u672f\u5b9e\u9a8c\u5ba4\u7684Joaqu\u00edn Fern\u00e1ndez-Rossier\u8bfe\u9898\u7ec4\uff0c<strong>\u91c7\u7528\u8868\u9762\u5408\u6210\u7684\u65b9\u6cd5\u5236\u5907\u4e86\u4e00\u7ef4\u542bS=1\u591a\u73af\u82b3\u9999\u70c3\u4e09\u89d2\u70ef\u7684\u81ea\u65cb\u94fe<\/strong>\u3002\u5229\u7528\u626b\u63cf\u96a7\u9053\u663e\u5fae\u955c\u548c4.5 K\u4e0b\u7684\u5149\u8c31\uff0c\u5728\u539f\u5b50\u5c3a\u5ea6\u4e0a\u63a2\u6d4b\u4e86\u5f00\u653e\u81ea\u65cb\u94fe\u548c\u5faa\u73af\u81ea\u65cb\u94fe\u4e2d\u957f\u5ea6\u4f9d\u8d56\u7684\u78c1\u6fc0\u53d1\uff0c\u5e76\u76f4\u63a5\u89c2\u5bdf\u5230\u5176\u4e2d\u7684\u95f4\u9699\u81ea\u65cb\u6fc0\u53d1\u548c\u5206\u6570\u9636\u8fb9\u6001\u3002\u7cbe\u786e\u7684\u5bf9\u89d2\u5316\u8ba1\u7b97\u63d0\u4f9b\u4e86\u51b3\u5b9a\u6027\u7684\u8bc1\u636e\uff0c\u8bc1\u660e\u81ea\u65cb\u94fe\u5728Haldane\u5bf9\u79f0\u4fdd\u62a4\u62d3\u6251\u76f8\u4e2d\u662f\u7531S=1\u53cc\u7ebf\u6027-\u53cc\u4e8c\u6b21\u54c8\u5bc6\u987f\u91cf\u63cf\u8ff0\u7684\u3002<strong>\u76f8\u5173\u8bba\u6587\u4ee5\u9898\u4e3a\u201cObservation of fractional edge excitations in nanographene spin chains\u201d\u53d1\u8868\u5728Nature\u4e0a<\/strong>\u3002\u200b<strong>\u00a0<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-229350\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/11.jpg\" alt=\"\" width=\"692\" height=\"520\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/11.jpg 692w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/10\/11-300x225.jpg 300w\" sizes=\"(max-width: 692px) 100vw, 692px\" \/><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a\u201cObservation of fractional edge excitations in nanographene spin chains\u201d. Nature 598, 287\u2013292 (2021). https:\/\/doi-org-443.webvpn.bjmu.edu.cn\/10.1038\/s41586-021-03842-3<\/p>\n<p><strong>6. Nature\uff1a\u53cc\u5c42\u77f3\u58a8\u70ef\u4e2d\u8f68\u9053\u78c1\u9a71\u52a8\u7684\u91cf\u5b50\u53cd\u5e38\u970d\u5c14\u6548\u5e94<\/strong><\/p>\n<p><strong><b>\u7f8e\u56fd\u5fb7\u5dde\u5927\u5b66\u7406\u67e5\u68ee\u8fbe\u62c9\u65af\u5206\u6821Fan Zhang\u56e2\u961f\u548c\u6155\u5c3c\u9ed1\u5927\u5b66R. Thomas Weitz\u63d0\u51fa\u4e86<\/b><\/strong>\u7535\u5bfc\u7387\u4e3a2\u00a0<em><i>e<\/i><\/em><sup>2<\/sup><em><i>h<\/i><\/em><sup>-1<\/sup>(\u5176\u4e2d<em><i>e<\/i><\/em>\u4e3a\u7535\u8377\uff0c<em><i>h<\/i><\/em>\u4e3a\u666e\u6717\u514b\u5e38\u6570)\u7684\u53cc\u5c42\u77f3\u58a8\u70ef\uff0c\u8fd9\u79cd\u53cc\u5c42\u77f3\u58a8\u70ef\u4e0d\u4ec5\u80fd\u5728\u5f02\u5e38\u5c0f\u7684\u78c1\u573a\u548c5\u5f00\u5c14\u6587\u4e0b\u5de5\u4f5c\uff0c\u800c\u4e14\u8fd8\u8868\u73b0\u51fa\u78c1\u6ede\u73b0\u8c61\u3002\u672c\u5de5\u4f5c\u901a\u8fc7\u5b9e\u9a8c\u8868\u5f81\u4e3a\u8f68\u9053\u78c1\u9a71\u52a8\u7684QAH\u884c\u4e3a\u63d0\u4f9b\u4e86\u4ee4\u4eba\u4fe1\u670d\u7684\u8bc1\u636e\uff0c\u8fd9\u79cd\u884c\u4e3a\u53ef\u4ee5\u901a\u8fc7\u7535\u573a\u3001\u78c1\u573a\u4ee5\u53ca\u8f7d\u6ce2\u4fe1\u53f7\u8fdb\u884c\u8c03\u8282\u3002\u672c\u5de5\u4f5c\u5236\u5907\u7684\u53cc\u5c42\u77f3\u58a8\u70ef\u6240\u89c2\u6d4b\u5230\u7684QAH\u76f8\u4e0d\u540c\u4e8e\u4ee5\u5f80\u7684\u89c2\u6d4b\uff0c\u8fd9\u662f\u7531\u4e8e\u5176\u72ec\u7279\u7684\u94c1\u78c1\u548c\u94c1\u7535\u987a\u5e8f\uff0c\u5176\u7279\u5f81\u662f\u91cf\u5b50\u5316\u7684\u5f02\u5e38\u7535\u8377\u3001\u81ea\u65cb\u3001\u8c37\u548c\u81ea\u65cb\u8c37\u970d\u5c14\u884c\u4e3a\u3002<strong><b>\u76f8\u5173\u6210\u679c\u4ee5\u9898\u4e3a\u201cQuantum anomalous Hall octet driven by orbital magnetism in bilayer graphene\u201d\u53d1\u8868\u5728\u4e86nature\u4e0a\u3002<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228218\" src=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/%E5%9B%BE%E7%89%87-162.png\" sizes=\"(max-width: 600px) 100vw, 600px\" srcset=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/\u56fe\u7247-162.png 600w, http:\/\/dn.cailiaoniu.com\/2021\/10\/\u56fe\u7247-162-242x300.png 242w\" alt=\"\" width=\"600\" height=\"743\" \/><\/p>\n<p>\u8bba\u6587doi\uff1ahttps:\/\/doi.org\/10.1038\/s41586-021-03849-w<\/p>\n<p><strong>7. Nature\u4e09\u5251\u5408\u74a7\uff01\u897f\u4ea4\u91d1\u660e\u5c1a\u3001\u52a0\u5dde\u5927\u5b66\u6bb7\u4e9a\u4e1c\u3001\u4e0a\u4ea4\u90ac\u5251\u6ce2\u5171\u540c\u8c03\u63a7\u94c2\u50ac\u5316\u5242\u6027\u80fd<\/strong><\/p>\n<p><strong>\u897f\u5b89\u4ea4\u901a\u5927\u5b66\u7684\u91d1\u660e\u5c1a\u3001\u7f8e\u56fd\u52a0\u5dde\u5927\u5b66\u6cb3\u6ee8\u5206\u6821\u7684\u6bb7\u4e9a\u4e1c\u548c\u4e0a\u6d77\u4ea4\u901a\u5927\u5b66\u7684\u90ac\u5251\u6ce2<\/strong>\u7b49\u4eba\u8054\u5408\u53d1\u73b0\uff0c\u5f53\u8d85\u8584\u94c2\u58f3\u5c42\u6c89\u79ef\u5728\u94af\u57fa\u7eb3\u7c73\u7ba1\u4e0a\u65f6\uff0c\u7eb3\u7c73\u7ba1\u901a\u8fc7\u78f7\u5316\u4f5c\u7528\u548c\u53bb\u78f7\u5316\u4f5c\u7528\u53ef\u53d1\u751f\u6269\u5f20\u6216\u6536\u7f29\uff0c\u4ece\u800c\u5f15\u53d1Pt\uff08100\uff09\u6676\u683c\u7684\u5e94\u53d8\u53d8\u5316\uff0c\u5176\u53d8\u5316\u8303\u56f4\u53ef\u4ece\u22125.1%\u8c03\u6574\u52305.9%\u3002\u4f5c\u8005\u5229\u7528\u8fd9\u4e00\u5e94\u53d8\u63a7\u5236\u7b56\u7565\u8c03\u63a7\u94c2\u58f3\u5c42\u7684\u7535\u50ac\u5316\u6d3b\u6027\uff0c\u5e76\u53d1\u73b0\u9488\u5bf9\u7532\u9187\u6c27\u5316\u548c\u6790\u6c22\u53cd\u5e94\u7684\u5e94\u53d8-\u6d3b\u6027\u7684\u76f8\u5173\u5173\u7cfb\u5206\u522b\u9075\u5faaM\u578b\u66f2\u7ebf\u548c\u7a79\u5f62\u706b\u5c71\u578b\u66f2\u7ebf\u3002\u8be5\u65b9\u6cd5\u672a\u6765\u53ef\u7528\u4e8e\u7b5b\u9009\u6676\u683c\u5e94\u53d8\uff0c\u4ece\u800c\u4f18\u5316\u91d1\u5c5e\u50ac\u5316\u5242\u7684\u6027\u80fd\u3002\u8be5\u6587\u7ae0\u8fd1\u65e5\u4ee5\u9898\u4e3a\u201c<strong>Mastering the surface strain of platinum catalysts for efficient electrocatalysis<\/strong>\u201d\u53d1\u8868\u5728\u77e5\u540d\u9876\u520a<strong>Nature<\/strong>\u4e0a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228145\" src=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/1-3.png\" sizes=\"(max-width: 600px) 100vw, 600px\" srcset=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/1-3.png 600w, http:\/\/dn.cailiaoniu.com\/2021\/10\/1-3-300x252.png 300w\" alt=\"\" width=\"600\" height=\"503\" \/><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"https:\/\/www.nature.com\/articles\/s41586-021-03870-z\" target=\"_blank\" rel=\"noopener\">Mastering the surface strain of platinum catalysts for efficient electrocatalysis\u00a0<\/a>(<em>Nature<\/em>\u00a0<strong>2021<\/strong>, doi: 10.1126\/science.abf3427)<\/p>\n<p><strong>8. \u65e2\u662f\u4e00\u4f5c\u53c8\u5f53\u901a\u8baf\uff0cNature\u6559\u4f60\u5982\u4f55\u6210\u50cf\u7535\u5b50\u6676\u683c<\/strong><\/p>\n<p><strong>\u52a0\u5dde\u5927\u5b66\u4f2f\u514b\u5229\u5206\u6821\u7684<\/strong><strong>Shaowei Li<\/strong><strong>\uff08\u540c\u65f6\u4e3a\u5171\u540c\u7b2c\u4e00\u4f5c\u8005\uff09\u3001<\/strong><strong>Michael F. Crommie<\/strong><strong>\u548c<\/strong><strong>Feng Wang<\/strong>\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\uff09\u7b49\u4eba\u5408\u4f5c\u8bbe\u8ba1\u4e86\u4e00\u79cd\u975e\u4fb5\u5165\u6027\u7684STM\u5149\u8c31\u6280\u672f\u5bf9WSe<sub>2<\/sub>\/WS<sub>2<\/sub>\u6469\u5c14\u5f02\u8d28\u7ed3\u6784\u4e2d\u7684\u4e8c\u7ef4\u7ef4\u683c\u7eb3\u6676\u4f53\u8fdb\u884c\u5b9e\u7a7a\u95f4\u6210\u50cf\u3002\u8fd9\u79cd\u65b9\u6cd5\u5229\u7528\u4e86\u9760\u8fd1WSe<sub>2<\/sub>\/WS<sub>2<\/sub>\u6469\u5c14\u8d85\u6676\u683c\u7684\u77f3\u58a8\u70ef\u4f20\u611f\u5c42\uff0c\u8fdb\u5165\u77f3\u58a8\u70ef\u5c42\u7684\u5c40\u90e8STM\u96a7\u9053\u7535\u6d41\u7531WSe<sub>2<\/sub>\/WS<sub>2<\/sub>\u6469\u5c14\u5f02\u8d28\u7ed3\u6784\u4e2d\u7684\u5e95\u5c42\u7ef4\u683c\u7eb3\u6d78\u63d0\u7684\u7535\u5b50\u6676\u683c\u8fdb\u884c\u8c03\u5236\u3002\u7814\u7a76\u5bf9\u5728\u90e8\u5206\u7535\u5b50\u586b\u5145\uff08<em>n<\/em>\u00a0= 1\/3, 1\/2 \uff0c2\/3\uff09\u7684\u7ef4\u683c\u7eb3\u6676\u683c\u6784\u8c61\u5b9e\u73b0\u4e86\u76f4\u63a5\u53ef\u89c6\u5316\uff08\u5176\u4e2d<em>n<\/em>\u662f\u6bcf\u4e2a\u4f4d\u70b9\u7684\u7535\u5b50\u6570\uff09\u3002\u7814\u7a76\u53d1\u73b0\uff0c<em>n<\/em>\u00a0= 1\/3\u548c2\/3\u7684\u7ef4\u683c\u7eb3\u6676\u4f53\u5206\u522b\u5177\u6709\u4e09\u89d2\u548c\u8702\u7a9d\u72b6\u6676\u683c\uff0c\u53ef\u6700\u5927\u7a0b\u5ea6\u4e0a\u5730\u51cf\u5c11\u6700\u8fd1\u90bb\u8f68\u9053\u5360\u636e\u60c5\u51b5\u3002\u800c<em>n<\/em>\u00a0= 1\/2\u6001\u7ef4\u683c\u7eb3\u6676\u4f53\u53ef\u81ea\u53d1\u6253\u7834\u539f\u59cbC3\u5bf9\u79f0\u5e76\u5f62\u6210\u6761\u7eb9\u76f8\u3002\u8be5\u7814\u7a76\u4e3a\u7406\u89e3WSe<sub>2<\/sub>\/WS<sub>2<\/sub>\u6469\u5c14\u5f02\u8d28\u7ed3\u6784\u4e2d\u7684\u7ef4\u683c\u7eb3\u6676\u4f53\u72b6\u6001\u5960\u5b9a\u4e86\u575a\u5b9e\u7684\u57fa\u7840\uff0c\u5e76\u63d0\u4f9b\u4e86\u4e00\u79cd\u9002\u7528\u5728\u4e8e\u5176\u4ed6\u7cfb\u7edf\u4e2d\u6210\u50cf\u65b0\u578b\u76f8\u5173\u7535\u5b50\u6676\u683c\u7684\u65b9\u6cd5\u3002<strong>\u672c\u6587\u5171\u540c\u7b2c\u4e00\u4f5c\u8005\u4e3a<\/strong><strong>Hongyuan Li<\/strong><strong>\u548c<\/strong><strong>Shaowei Li<\/strong>\uff0c\u7814\u7a76\u6210\u679c\u4ee5\u9898\u4e3a<strong>\u201cImaging two-dimensional generalized Wigner crystals\u201d<\/strong>\u53d1\u5e03\u5728\u56fd\u9645\u8457\u540d\u671f\u520a<strong>Nature<\/strong>\u4e0a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228096\" src=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/1-1.jpg\" sizes=\"(max-width: 600px) 100vw, 600px\" srcset=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/1-1.jpg 600w, http:\/\/dn.cailiaoniu.com\/2021\/10\/1-1-300x197.jpg 300w\" alt=\"\" width=\"600\" height=\"394\" \/><\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><a href=\"https:\/\/doi.org\/10.1038\/s41586-021-03874-9\" target=\"_blank\" rel=\"noopener\">Imaging two-dimensional generalized Wigner crystals<\/a>,\u00a0<em>Nature<\/em>,\u00a0<strong>2021<\/strong>, DOI: 10.1038\/s 41586-021-03874-9.<\/p>\n<p><strong>9. Nature\uff1a\u4e09\u7ef4\u591a\u5b54\u91d1\u5c5e\u6709\u673a\u6676\u4f53<\/strong><\/p>\n<p>\u5728\u81ea\u7136\u754c\u4e2d\u5df2\u7ecf\u53d1\u73b0\u4e86\u5404\u79cd\u673a\u68b0\u4e92\u9501\u7ed3\u6784\uff0c\u5176\u51e0\u4f55\u5f62\u72b6\u548c\u53d1\u6325\u72ec\u7279\u529f\u80fd\u7684\u5de8\u5927\u6f5c\u529b\u5177\u6709\u91cd\u8981\u7684\u79d1\u5b66\u610f\u4e49\u3002\u81ea20\u4e16\u7eaa70\u5e74\u4ee3\u9996\u6b21\u62a5\u9053\u805a\u7d22\u70c3\u548c\u805a\u8f6e\u70f7\u4ee5\u6765\uff0c\u7531\u4e92\u9501\u9aa8\u67b6\u7ec4\u6210\u7684\u6750\u6599\u5177\u6709\u7684\u7279\u6b8a\u529b\u5b66\u6027\u80fd\u4e00\u76f4\u662f\u6750\u6599\u79d1\u5b66\u4e2d\u957f\u671f\u63a2\u8ba8\u7684\u95ee\u9898\u3002\u65e5\u672c\u4e1c\u4eac\u5927\u5b66Hiroshi Sato\u548cTakuzo Aida\u62a5\u544a\u4e86\u4e00\u79cd\u4e09\u7ef4\u591a\u5b54\u91d1\u5c5e\u6709\u673a\u6676\u4f53\uff0c\u5b83\u7684\u7279\u6b8a\u4e4b\u5904\u5728\u4e8e\u5176\u7ecf\u7ebf\u548c\u7eac\u7ebf\u4ec5\u901a\u8fc7\u94fe\u8fde\u63a5\u3002\u8fd9\u79cd\u591a\u5b54\u6676\u4f53\u7531\u56db\u65b9\u6676\u683c\u7ec4\u6210\uff0c\u5e76\u5728\u5ba2\u4f53\u5206\u5b50\u4e2d\u91ca\u653e\uff0c\u5438\u6536\u548c\u4ea4\u6362\u65f6\u52a8\u6001\u6539\u53d8\u5176\u51e0\u4f55\u5f62\u72b6\uff0c\u751a\u81f3\u5728\u4f4e\u6e29\u8303\u56f4\u5185\u4e5f\u968f\u6e29\u5ea6\u53d8\u5316\u800c\u52a8\u6001\u53d8\u5316\u3002\u4f5c\u8005\u6cbfa\/b\u8f74\u5c06\u6676\u4f53\u7f29\u8fdb\uff0c\u5728N,N-\u4e8c\u7532\u57fa\u7532\u9170\u80fa\uff08DMF\uff09\u4e2d\u7684\u6768\u6c0f\u6a21\u91cf\u4e3a1.77\u00b10.16GPa\uff0c\u5728\u56db\u6c22\u544b\u5583\u4e2d\u7684\u6768\u6c0f\u6a21\u91cf\u4e3a1.63\u00b10.13GPa\uff0c\u662f\u76ee\u524d\u62a5\u9053\u7684\u591a\u5b54\u91d1\u5c5e-\u6709\u673a\u6676\u4f53\u4e2d\u6700\u4f4e\u503c\u3002\u66f4\u52a0\u91cd\u8981\u7684\u662f\uff0c\u6d41\u4f53\u9759\u529b\u538b\u7f29\u8868\u660e\uff0c\u8be5\u5f39\u6027\u591a\u5b54\u6676\u4f53\u6cbf\u5176c\u8f74\u53d8\u5f62\u6700\u591a\uff0c\u5728\u538b\u7f29\u81f30.88 GPa\u65f6\u53d1\u751f5%\u7684\u6536\u7f29\u800c\u6ca1\u6709\u7ed3\u6784\u635f\u574f\u3002\u540c\u65f6\u57280.46 GPa\u4e0b\u83b7\u5f97\u7684\u6676\u4f53\u7ed3\u6784\u8868\u660e\uff0c\u94fe\u63a5\u7684\u5927\u73af\u5728\u6536\u7f29\u65f6\u5e73\u79fb\u3002\u9884\u8ba1\u672c\u6587\u57fa\u4e8e\u673a\u68b0\u4e92\u9501\u5206\u5b50\u7684\u8bbe\u8ba1\u5c06\u6210\u4e3a\u5f00\u53d1\u5177\u6709\u4f18\u5f02\u673a\u68b0\u6027\u80fd\u591a\u5b54\u6750\u6599\u7684\u8d77\u70b9\uff0c\u4e3a\u53d1\u5c55\u5177\u6709\u4f18\u5f02\u6027\u80fd\u7684\u53ef\u6324\u538b\u591a\u5b54\u6676\u4f53\u94fa\u5e73\u4e86\u9053\u8def\u3002\u76f8\u5173\u7814\u7a76\u6210\u679c\u4ee5\u201cAn elastic metal\u2013organic crystal with a densely catenated backbone\u201d\u4e3a\u9898\u5728\u7ebf\u53d1\u8868\u5728Nature\u3002<\/p>\n<p><img decoding=\"async\" class=\"aligncenter\" src=\"https:\/\/www.cailiaoren.com\/\/_file\/211014\/013252_611.jpg\" border=\"0\" \/><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1ahttps:\/\/www.nature.com\/articles\/s41586-021-03880-x<\/p>\n<p><strong>10. Nature\uff1a\u626d\u66f2\u53cc\u5c42\u77f3\u58a8\u70ef\u4e2d\u975e\u5e38\u89c4\u8d85\u5bfc\u6027\u7684\u8bc1\u636e<\/strong><\/p>\n<p>\u6b63\u5982Bardeen-Cooper-Schrieffer (BCS) \u7406\u8bba\u6240\u63cf\u8ff0\u7684\uff0c\u8d85\u5bfc\u6027\u548c\u76f8\u5173\u7edd\u7f18\u4f53\u5728\u9b54\u89d2\u626d\u66f2\u53cc\u5c42\u77f3\u58a8\u70ef\uff08MATBG\uff09\u4e2d\u7684\u51fa\u73b0\u589e\u52a0\u4e86\u4e00\u79cd\u6709\u8da3\u7684\u53ef\u80fd\u6027\uff0c\u5373\u5176\u914d\u5bf9\u673a\u5236\u4e0d\u540c\u4e8e\u4f20\u7edf\u8d85\u5bfc\u4f53\u7684\u914d\u5bf9\u673a\u5236\u3002\u7136\u800c\uff0c\u6700\u8fd1\u7684\u7814\u7a76\u8868\u660e\uff0c\u5373\u4f7f\u5e93\u4ed1\u76f8\u4e92\u4f5c\u7528\u88ab\u90e8\u5206\u5c4f\u853d\uff0c\u8d85\u5bfc\u6027\u4ecd\u7136\u5b58\u5728\u3002\u8fd9\u8868\u660eMATBG\u4e2d\u7684\u914d\u5bf9\u5728\u672c\u8d28\u4e0a\u53ef\u80fd\u662f\u5e38\u89c4\u7684\uff0c\u5e76\u4e14\u662f\u5176\u5e73\u5e26\u7684\u5927\u6001\u5bc6\u5ea6 (DOS) \u7684\u7ed3\u679c\u3002\u7f8e\u56fd\u5dde\u666e\u6797\u65af\u987f\u5927\u5b66Ali Yazdani\u6559\u6388\u5c06\u96a7\u9053\u548cAndreev\u53cd\u5c04\u5149\u8c31\u4e0e\u626b\u63cf\u96a7\u9053\u663e\u5fae\u955c\uff08STM\uff09\u76f8\u7ed3\u5408\uff0c\u4ee5\u89c2\u5bdfMATBG\u4e2d\u975e\u5e38\u89c4\u8d85\u5bfc\u6027\u7684\u51e0\u4e2a\u5173\u952e\u5b9e\u9a8c\u7279\u5f81\u3002\u7814\u7a76\u8868\u660e\uff0c\u4f4e\u4e8e\u8f6c\u53d8\u6e29\u5ea6Tc\u7684\u96a7\u9053\u5149\u8c31\u4e0e\u4f20\u7edfs\u6ce2\u8d85\u5bfc\u4f53\u7684\u96a7\u9053\u5149\u8c31\u4e0d\u4e00\u81f4\uff0c\u800c\u662f\u7c7b\u4f3c\u4e8e\u5177\u6709\u5404\u5411\u5f02\u6027\u914d\u5bf9\u673a\u5236\u7684\u8282\u70b9\u8d85\u5bfc\u4f53\u7684\u96a7\u9053\u5149\u8c31\u3002\u540c\u65f6\u89c2\u5bdf\u5230\u96a7\u9053\u95f4\u9699\u0394T\u4e4b\u95f4\u5b58\u5728\u5f88\u5927\u5dee\u5f02\uff0c\u8fd9\u8fdc\u8fdc\u8d85\u8fc7\u5e73\u5747\u573a\uff0c\u4ee5\u53ca\u4eceAndreev\u53cd\u5c04\u5149\u8c31\u4e2d\u63d0\u53d6\u7684\u95f4\u9699 \u0394AR\u00a0\u3002\u5373\u4f7f\u8d85\u5bfc\u53d7\u5230\u6291\u5236\uff0c\u96a7\u7a7f\u95f4\u9699\u4ecd\u7136\u5b58\u5728\uff0c\u8868\u660e\u5b83\u662f\u4ece\u8d5d\u95f4\u9699\u76f8\u4e2d\u51fa\u73b0\u7684\u3002\u6b64\u5916\uff0c\u5f53MATBG\u4e0e\u516d\u65b9\u6c2e\u5316\u787c (hBN) \u5bf9\u9f50\u65f6\uff0c\u8d5d\u9699\u548c\u8d85\u5bfc\u6027\u5747\u4e0d\u5b58\u5728\u3002\u6b64\u5904\u62a5\u544a\u7684\u8fd9\u4e9b\u53d1\u73b0\u548c\u5176\u4ed6\u89c2\u5bdf\u7ed3\u679c\u4e3aMATBG\u4e2d\u8d85\u5bfc\u6027\u7684\u975e BCS\u673a\u5236\u63d0\u4f9b\u4e86\u5927\u91cf\u8bc1\u636e\u3002\u76f8\u5173\u7814\u7a76\u6210\u679c\u4ee5\u201cEvidence for unconventional superconductivity in twisted bilayer graphene\u201d\u4e3a\u9898\u5728\u7ebf\u53d1\u8868\u5728Nature\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1ahttps:\/\/www.nature.com\/articles\/s41586-021-04121-x<\/p>\n<p style=\"text-align: center;\"><strong>science<\/strong><\/p>\n<p style=\"text-align: left;\"><strong>1. MOF\u9f3b\u7956\u6700\u65b0Science\uff1a\u00a0\u6539\u5584\u5927\u6c14\u96c6\u6c34\u7684\u91d1\u5c5e-\u6709\u673a\u6846\u67b6\u4e2d\u6c34\u7ed3\u6784\u7684\u6f14\u53d8<\/strong><\/p>\n<p>\u6765\u81ea<strong><b>\u52a0\u5229\u798f\u5c3c\u4e9a\u5927\u5b66\u4f2f\u514b\u5229\u5206\u6821\u3001\u6d2a\u5821\u5927\u5b66\u548c\u829d\u52a0\u54e5\u5927\u5b66<\/b><\/strong>\u7684\u5b66\u8005\u901a\u8fc7\u5927\u91cf\u7684\u5355\u6676x\u5c04\u7ebf\u884d\u5c04\u6d4b\u91cf\u548c\u5bc6\u5ea6\u6cdb\u51fd\u7406\u8bba\u8ba1\u7b97\uff0c\u89e3\u91ca\u4e86\u6700\u5148\u8fdb\u7684\u96c6\u6c34\u91d1\u5c5e\u6709\u673a\u9aa8\u67b6MOF-303\u7684\u5145\u6c34\u673a\u7406\u3002\u7b2c\u4e00\u6c34\u5206\u5b50\u4e0e\u6781\u6027\u6709\u673a\u8fde\u63a5\u7269\u5f3a\u7ed3\u5408\uff1b\u63a5\u7740\u662f\u989d\u5916\u7684\u6c34\u5206\u5b50\u5f62\u6210\u5b64\u7acb\u7684\u56e2\u7c07\uff0c\u7136\u540e\u5f62\u6210\u56e2\u7c07\u94fe\uff0c\u6700\u540e\u5f62\u6210\u6c34\u7f51\u7edc\u3002\u6c34\u7ed3\u6784\u7684\u8fd9\u79cd\u6f14\u53d8\u5bfc\u81f4\u6211\u4eec\u53ef\u4ee5\u901a\u8fc7\u591a\u5143\u65b9\u6cd5\u6765\u4fee\u6539\u5b54\u9699\uff0c\u4ece\u800c\u7cbe\u786e\u5730\u8c03\u8282\u7b2c\u4e00\u4e2a\u6c34\u5206\u5b50\u7684\u7ed3\u5408\u5f3a\u5ea6\uff0c\u5e76\u63a7\u5236\u5438\u6c34\u884c\u4e3a\u3002\u8fd9\u5bfc\u81f4\u4e86\u66f4\u9ad8\u7684\u4ea7\u6c34\u91cf\uff0c\u4ee5\u53ca\u518d\u751f\u6e29\u5ea6\u548c\u7113\u7684\u53ef\u8c03\u6027\uff0c\u5e76\u4e14\u4e0d\u4f1a\u5f71\u54cd\u5bb9\u91cf\u548c\u7a33\u5b9a\u6027\u3002\u76f8\u5173\u5de5\u4f5c\u4ee5\u9898\u4e3a\u201cEvolution of water structures in metal-organic frameworks for improved atmospheric water harvesting\u201d\u7684\u7814\u7a76\u6027\u6587\u7ae0\u5728\u300aScience\u300b\u4e0a\u53d1\u8868\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228863\" src=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/%E5%9B%BE%E7%89%87-2-11.png\" sizes=\"(max-width: 600px) 100vw, 600px\" srcset=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/\u56fe\u7247-2-11.png 600w, http:\/\/dn.cailiaoniu.com\/2021\/10\/\u56fe\u7247-2-11-300x151.png 300w\" alt=\"\" width=\"600\" height=\"301\" \/><\/p>\n<p>\u94fe\u63a5\uff1ahttps:\/\/www.science.org\/doi\/10.1126\/science.abj0890<\/p>\n<p><strong>2. \u9499\u949b\u77ff\u518d\u767bScience\uff1a\u5177\u6709\u9ad8\u7a33\u5b9a\u6027\u3001\u9ad8\u53d1\u5149\u6548\u7387\u7684MOF\u57fa\u65e0\u673a\u9499\u949b\u77ff<\/strong><\/p>\n<p><strong>\u6fb3\u5927\u5229\u4e9a\u6606\u58eb\u5170\u5927\u5b66\u4faf\u7ecf\u7eac\u535a\u58eb\u3001\u738b\u8fde\u6d32\u6559\u6388\u8054\u5408\u6765\u81ea\u5df4\u9ece\u5927\u5b66\u3001\u6fb3\u6d32\u53ca\u6b27\u6d32\u540c\u6b65\u8f90\u5c04\u7814\u7a76\u4e2d\u5fc3\u3001\u5229\u5179\u5927\u5b66\u3001\u82f1\u56fd\u5251\u6865\u5927\u5b66<\/strong><strong>Thomas D. Bennett<\/strong><strong>\u6559\u6388\u548c\u5229\u5179\u5927\u5b66<\/strong><strong>Sean M. Collins<\/strong><strong>\u6559\u6388\u7b49<\/strong>\u8054\u5408\u5236\u5907\u4e86\u4e00\u79cd\u57fa\u4e8e\u91d1\u5c5e\u6709\u673a\u9aa8\u67b6\uff08MOF\uff09\u73bb\u7483\u548c\u5168\u65e0\u673a\u9499\u949b\u77ff\u7684\u590d\u5408\u6750\u6599\u3002\u7814\u7a76\u4eba\u5458\u5229\u7528\u4f20\u7edf\u7684\u6db2\u76f8\u70e7\u7ed3\u6280\u672f\u52a0\u5de5\u4e86\u4e00\u7cfb\u5217\u7684\u5168\u65b0\u590d\u5408\u6750\u6599\uff0c\u8bc1\u660e\u4e86\u8be5\u79cd\u5de5\u4e1a\u9886\u57df\u5e7f\u6cdb\u5e94\u7528\u7684\u70e7\u7ed3\u6280\u672f\u53ef\u4ee5\u9002\u7528\u4e8eMOF\u73bb\u7483\u53ca\u9499\u949b\u77ff\u6676\u4f53\u8fd9\u4e00\u5168\u65b0\u7684\u6750\u6599\u7ec4\u5408\u3002\u53ef\u52a0\u5de5\u7684\u590d\u5408\u6750\u6599\u5bf9\u6d78\u5165\u6c34\u548c\u6709\u673a\u6eb6\u5242\u4ee5\u53ca\u66b4\u9732\u5728\u70ed\u3001\u5149\u3001\u7a7a\u6c14\u548c\u73af\u5883\u6e7f\u5ea6\u4e2d\u8868\u73b0\u51fa\u5f88\u9ad8\u7684\u7a33\u5b9a\u6027\u3002\u5149\u81f4\u53d1\u5149\u81f3\u5c11\u6bd4\u7eaf\u9499\u949b\u77ff\u5927\u4e24\u4e2a\u6570\u91cf\u7ea7\u3002\u73bb\u7483\u5728\u9ad8\u6fc0\u5149\u6fc0\u53d1\u4e0b\u7a33\u5b9a\u9499\u949b\u77ff\uff0c\u5e76\u4e14\u5728\u6d78\u6c3410000\u5c0f\u65f6\u540e\u4ecd\u4fdd\u6301\u7ea680%\u7684\u5149\u81f4\u53d1\u5149\u3002\u8be5\u6587\u7ae0\u8fd1\u65e5\u4ee5\u9898\u4e3a\u201c<strong>Liquid-phase sintering of lead halide perovskites and metal-organic framework glasses<\/strong>\u201d\u53d1\u8868\u5728\u77e5\u540d\u9876\u520a<strong>Science<\/strong>\u4e0a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228972\" src=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/1-11.jpg\" sizes=\"(max-width: 600px) 100vw, 600px\" srcset=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/1-11.jpg 600w, http:\/\/dn.cailiaoniu.com\/2021\/10\/1-11-274x300.jpg 274w\" alt=\"\" width=\"600\" height=\"657\" \/><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"https:\/\/www.science.org\/doi\/10.1126\/science.abf4460\" target=\"_blank\" rel=\"noopener\">Liquid-phase sintering of lead halide perovskites and metal-organic framework glasses<\/a>\u00a0(<em>Science<\/em>\u00a0<strong>2021<\/strong>, doi: 10.1126\/science.abf4460)<\/p>\n<p><strong>3. \u4e2d\u79d1\u5927&amp;\u5317\u822aScience\uff1a\u94c2\u91d1\u5c5e\u95f4\u5316\u5408\u7269\u7eb3\u7c73\u50ac\u5316\u5242\u7684\u786b\u951a\u5b9a\u5408\u6210\u7528\u4e8e\u71c3\u6599\u7535\u6c60<\/strong><\/p>\n<p>\u4e2d\u56fd\u79d1\u5b66\u6280\u672f\u5927\u5b66\u6881\u6d77\u4f1f\u6559\u6388\u3001\u6797\u5cb3\u535a\u58eb\u4e0e\u5317\u4eac\u822a\u7a7a\u822a\u5929\u5927\u5b66\u6c34\u6c5f\u6f9c\u6559\u6388\u8bfe\u9898\u7ec4\u5408\u4f5c\uff0c\u901a\u8fc7\u4e00\u79cd\u9ad8\u6e29\u786b\u951a\u5b9a\u5408\u6210\u65b9\u6cd5\uff0c<strong>\u5728\u591a\u5b54\u786b\u63ba\u6742\u78b3\uff08<\/strong><strong>S-C<\/strong><strong>\uff09\u8f7d\u4f53\u4e0a\u5236\u5907\u4e86\u5e73\u5747\u7c92\u5f84<\/strong><strong>&lt; 5 nm<\/strong><strong>\u7684\u94c2\u91d1\u5c5e\u95f4\u5316\u5408\u7269\u3002<\/strong>\u672c\u5de5\u4f5c\u5408\u6210\u4e86\u753146\u79cd\u94c2\u4e0e\u5176\u4ed616\u79cd\u91d1\u5c5e\u5143\u7d20\u7ec4\u6210\u7684\u5c0f\u5c3a\u5bf8\u91d1\u5c5e\u95f4\u5316\u5408\u7269\u50ac\u5316\u5242\u5e93\uff0c\u5e76\u5c06\u5176\u7528\u4e8e\u7814\u7a76IMCs\u7535\u50ac\u5316\u6c27\u8fd8\u539f\u6d3b\u6027\u4e0e\u5176\u4e8c\u7ef4\u6676\u9762\u5e94\u529b\u4e4b\u95f4\u7684\u5173\u8054\u6027\u3002\u6240\u5236\u5907\u7684\u90e8\u5206\u91d1\u5c5e\u95f4\u5316\u5408\u7269\u50ac\u5316\u5242\u5728\u8d28\u5b50\u4ea4\u6362\u819c\u71c3\u6599\u7535\u6c60\u4e2d\u5177\u6709\u5f88\u9ad8\u7684\u8d28\u91cf\u6548\u7387\uff0c\u53ef\u4ee5\u57280.9V\u4e0b\u5b9e\u73b01.3\uff5e1.8 A mg<sub>Pt<\/sub><sup>-1<\/sup>\u7684\u9ad8\u6d3b\u6027\u3002\u76f8\u5173\u8bba\u6587\u4ee5\u9898\u4e3a\u201cSulfur-anchoring synthesis of platinum intermetallic nanoparticle catalysts for fuel cells\u201d\u53d1\u8868\u5728Science\u4e0a\u3002<\/p>\n<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228797\" src=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/2-10.png\" sizes=\"(max-width: 600px) 100vw, 600px\" srcset=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/2-10.png 600w, http:\/\/dn.cailiaoniu.com\/2021\/10\/2-10-208x300.png 208w\" alt=\"\" width=\"600\" height=\"867\" \/><\/strong><\/p>\n<p>\u8bba\u6587doi\uff1aDOI: 10.1126\/science.abj9980<\/p>\n<p><strong>4. \u80e1\u826f\u5175Science\u5c01\u9762<\/strong><\/p>\n<p><strong>\u9a6c\u91cc\u5170\u5927\u5b66\u80e1\u826f\u5175<\/strong>\uff08\u901a\u8baf\u4f5c\u8005\uff09\u7b49\u4eba\u62a5\u544a\u4e86\u4e00\u79cd\u5229\u7528\u7ec6\u80de\u58c1\u5de5\u7a0b\u5c06\u786c\u6728\u5e73\u677f\u5851\u9020\u6210\u591a\u529f\u80fd\u4e09\u7ef4\uff083D\uff09\u7ed3\u6784\u7684\u52a0\u5de5\u7b56\u7565\u3002\u901a\u8fc7\u8131\u6728\u7d20\u548c\u6c34\u5206\u6e05\u9664\u4ee5\u5206\u89e3\u6728\u6750\u6210\u5206\u5e76\u5c01\u95ed\u5bfc\u7ba1\u548c\u7ea4\u7ef4\u540e\uff0c\u4f5c\u8005\u5c06\u6536\u7f29\u7684\u6728\u6750\u6d78\u5165\u6c34\u4e2d\uff0c\u5728\u5feb\u901f\u6c34\u51b2\u51fb\u8fc7\u7a0b\u4e2d\u90e8\u5206\u91cd\u65b0\u81a8\u80c0\u6728\u6750\uff0c\u9009\u62e9\u6027\u5730\u6253\u5f00\u5bfc\u7ba1\u3002\u7531\u6b64\u53ef\u5f62\u6210\u4e00\u4e2a\u72ec\u7279\u7684\u8d77\u76b1\u7ec6\u80de\u58c1\u7ed3\u6784\uff0c\u4f7f\u6750\u6599\u53ef\u4ee5\u6298\u53e0\u5e76\u6a21\u5236\u6210\u6240\u9700\u7684\u5f62\u72b6\u3002\u7531\u6b64\u4ea7\u751f\u76843D\u6a21\u5236\u6728\u6750\u5f3a\u5ea6\u662f\u539f\u59cb\u6728\u6750\u7684\u516d\u500d\uff0c\u5236\u9020\u7684\u8702\u7a9d\u82af\u6750\u6599\u7684\u62c9\u4f38\u5f3a\u5ea6\u53ef\u8fbe\u5230300MPa\uff0c\u4e0e\u5e7f\u6cdb\u4f7f\u7528\u7684\u8f7b\u8d28\u6750\u6599\uff08\u5982\u94dd\u5408\u91d1\uff09\u76f8\u5f53\uff0c\u800c\u5176\u5bc6\u5ea6\u4ec5\u4e3a0.75 g cm<sup>-3<\/sup>\uff0c\u6210\u672c\u5927\u5927\u964d\u4f4e\u3002\u8fd9\u79cd\u65b9\u6cd5\u62d3\u5bbd\u4e86\u6728\u6750\u4f5c\u4e3a\u7ed3\u6784\u6750\u6599\u7684\u6f5c\u529b\uff0c\u964d\u4f4e\u4e86\u5bf9\u5efa\u7b51\u548c\u4ea4\u901a\u5e94\u7528\u7684\u73af\u5883\u5f71\u54cd\u3002Shaoliang Xiao\u3001Chaoji Chen\u3001Qinqin Xia\u548cYu Liu\u4e3a\u5171\u540c\u7b2c\u4e00\u4f5c\u8005\uff0c2021\u5e7410\u670822\u65e5\uff0c\u76f8\u5173\u6210\u679c\u4ee5\u9898\u4e3a\u201c<strong>Lightweight, strong, moldable wood via cell wall engineering as a sustainable structural material<\/strong>\u201d\u7684\u6210\u4e3a<strong>Science<\/strong>\u6700\u65b0\u5c01\u9762\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228747\" src=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/1-8.jpg\" sizes=\"(max-width: 600px) 100vw, 600px\" srcset=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/1-8.jpg 600w, http:\/\/dn.cailiaoniu.com\/2021\/10\/1-8-150x150.jpg 150w, http:\/\/dn.cailiaoniu.com\/2021\/10\/1-8-300x297.jpg 300w\" alt=\"\" width=\"600\" height=\"594\" \/><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"https:\/\/www.science.org\/doi\/10.1126\/science.abg9556\" target=\"_blank\" rel=\"noopener\">Lightweight, strong, moldable wood via cell wall engineering as a sustainable structural material<\/a>\uff08Science, 2021, DOI: 10.1126\/science.abg9556\uff09<\/p>\n<p><strong>5. Science\uff1a\u626d\u66f2\u53cc\u5c42\u534a\u5bfc\u4f53\u4e2d\u7684\u7535\u53ef\u8c03\u8c10Feshbach\u5171\u632f<\/strong><\/p>\n<p><strong>\u82cf\u9ece\u4e16\u8054\u90a6\u7406\u5de5\u5b66\u9662\u91cf\u5b50\u7535\u5b50\u7814\u7a76\u6240<\/strong><strong>ATA\u00c7 IMAMO\u011eLU<\/strong><strong>\u6559\u6388\u548c<\/strong><strong>IDO SCHWARTZ<\/strong><strong>\u535a\u58eb<\/strong>\u7814\u7a76\u4e86\u4e00\u79cdMoSe<sub>2<\/sub>\u540c\u8d28\u53cc\u5c42\u7ed3\u6784\uff0c\u5176\u4e2d\u5c42\u95f4\u76f8\u5e72\u96a7\u7a7f\u5141\u8bb8\u7535\u573a\u63a7\u5236\u7684\u64cd\u7eb5\u548c\u57fa\u6001\u7a7a\u7a74\u5c42\u8d5d\u81ea\u65cb\u7684\u6d4b\u91cf\u3002\u672c\u5b9e\u9a8c\u8bc1\u660e\uff0c\u5373\u4f7f\u5f53\u5c42\u5185\u4e09\u5b50\u7684\u80fd\u91cf\u9ad8\u4e8e\u6563\u5c04\u6001\u7684\u80fd\u91cf\u65f6\uff0c\u5177\u6709\u76f8\u5e72\u5c42\u95f4\u7a7a\u7a74\u96a7\u7a7f\u7684\u53cc\u5c42TMD\u7cfb\u7edf\u4e5f\u4f1a\u8868\u73b0\u51fa\u8bf1\u5bfc\u5c42\u95f4Feshbach\u5206\u5b50\u76842D Feshbach\u5171\u632f\u3002\u8fd9\u6837\u7684\u5171\u632f\u7528\u4e8e\u901a\u8fc7\u7535\u8c03\u8c10Feshbach\u5206\u5b50\u7684\u7ed3\u5408\u80fd\u6765\u589e\u5f3a\u9a7b\u7559\u5728\u4e0d\u540c\u5c42\u7684\u6fc0\u5b50\u548c\u7a7a\u7a74\u4e4b\u95f4\u7684\u76f8\u4e92\u4f5c\u7528\u3002\u76f8\u4e92\u4f5c\u7528\u5f3a\u5ea6\u662f\u8c37\u9009\u62e9\u6027\u7684\uff0c\u5e76\u4e14\u53ef\u4ee5\u8bf1\u5bfc\u76f8\u90bbMM\u4f4d\u7a7a\u7a74\u4e4b\u95f4\u7684\u6fc0\u5b50\u4ecb\u5bfc\u7684\u94c1\u78c1\u76f8\u4e92\u4f5c\u7528\u3002\u56e0\u6b64\uff0c\u672c\u5de5\u4f5c\u5728\u63a2\u7d22\u83ab\u5c14\u6676\u683c\u4e2d\u7684\u91cf\u5b50\u78c1\u6027\u65b9\u9762\u53ef\u4ee5\u53d1\u6325\u4f5c\u7528\u3002\u672c\u7814\u7a76\u6210\u679c\u53ef\u4ee5\u5b9e\u73b0\u5177\u6709\u53ef\u8c03\u76f8\u4e92\u4f5c\u7528\u7684\u7b80\u5e76\u73bb\u8272-\u8d39\u7c73\u6df7\u5408\u7269\u3002\u8be5\u6587\u7ae0\u8fd1\u65e5\u4ee5\u9898\u4e3a\u201c<strong>Electrically tunable Feshbach resonances in twisted bilayer semiconductors<\/strong>\u201d\u53d1\u8868\u5728\u77e5\u540d\u9876\u520a<strong>Science<\/strong>\u4e0a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228491\" src=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/1-4.jpg\" sizes=\"(max-width: 600px) 100vw, 600px\" srcset=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/1-4.jpg 600w, http:\/\/dn.cailiaoniu.com\/2021\/10\/1-4-300x212.jpg 300w\" alt=\"\" width=\"600\" height=\"423\" \/><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"https:\/\/www.science.org\/doi\/10.1126\/science.abj3831\" target=\"_blank\" rel=\"noopener\">Electrically tunable Feshbach resonances in twisted bilayer semiconductors\u00a0<\/a>(<em>Science<\/em>\u00a0<strong>2021<\/strong>, doi: 10.1126\/science.abj3831)<\/p>\n<p><strong>6. Science\uff1aNi\u591a\u6676\u4f53\u4e2d\u6676\u754c\u901f\u5ea6\u548c\u66f2\u7387\u4e0d\u76f8\u5173<\/strong><\/p>\n<p><strong><b>\u672c<\/b><\/strong><strong><b>\u5de5\u4f5c<\/b><\/strong><strong><b>\u4ecb\u7ecd\u4e86\u4e00\u79cd\u901a\u8fc7\u6d4b\u91cf\u4e0d\u540c\u65f6\u95f4\u95f4\u9694\u7684\u5fae\u89c2\u7ec4\u7ec7\u6765\u786e\u5b9a\u6676\u754c\u901f\u5ea6\u7684\u7b80\u5355\u65b9\u6cd5\u3002\u5229\u7528\u954d\u5728800\u00b0C\u9000\u706b\u8fc7\u7a0b\u4e2d6\u6b21\u6210\u50cf\u7684\u4e09\u7ef4\u7ec4\u7ec7\uff0c\u6d4b\u91cf\u4e86\u5df2\u77e5\u6676\u4f53\u5b66\u4e2d\u8d85\u8fc75 \u00d7 10<\/b><\/strong><strong><sup><b>4<\/b><\/sup><\/strong><strong><b>\u4e2a\u6676\u9762\u7684\u6676\u754c\u66f2\u7387\u548c\u901f\u5ea6\u3002<\/b><\/strong>\u672c\u5de5\u4f5c\u7684Ni\u591a\u6676\u8bd5\u6837\u5728950\u00b0C\u4e0b\u9000\u706b6\u5c0f\u65f6\uff0c\u7136\u540e\u5728800\u00b0C\u4e0b\u8fdb\u884c\u6676\u7c92\u751f\u957f\u5b9e\u9a8c\uff0c\u4ee5\u83b7\u5f97\u6700\u5c0f\u4e14\u6052\u5b9a\u7684\u4f4d\u9519\u5bc6\u5ea6\u3002\u53d1\u73b0\u6676\u754c\u901f\u5ea6\u4e0e\u63cf\u8ff0\u6676\u754c\u6676\u4f53\u5b66\u7684\u4e94\u4e2a\u5b8f\u89c2\u53c2\u6570\u4e4b\u95f4\u6709\u5f88\u5f3a\u7684\u76f8\u5173\u6027\u3002\u901f\u5ea6\u5bf9\u6676\u754c\u6676\u4f53\u5b66\u7684\u654f\u611f\u6027\u53ef\u80fd\u662f\u7f3a\u9677\u4ecb\u5bfc\u7684\u6676\u754c\u8fc1\u79fb\u6216\u6676\u754c\u80fd\u5404\u5411\u5f02\u6027\u7684\u7ed3\u679c\u3002<strong><b>\u6676\u754c\u901f\u5ea6\u548c\u66f2\u7387\u4e4b\u95f4\u4e0d\u5b58\u5728\u76f8\u5173\u6027\u5f88\u53ef\u80fd\u662f\u7531\u4e8e\u6676\u754c\u7f51\u7edc\u65bd\u52a0\u7ea6\u675f<\/b><\/strong><strong><b>\u7684\u7ed3\u679c<\/b><\/strong>\u3002\u8be5\u6587\u7ae0\u8fd1\u65e5\u4ee5\u9898\u4e3a\u201cExtremely anisotropic van der Waals thermal conductors\u201d\u53d1\u8868\u5728\u77e5\u540d\u9876\u520a<strong>Science<\/strong>\u4e0a\u3002<\/p>\n<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228261\" src=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/%E5%9B%BE%E7%89%87-205.png\" sizes=\"(max-width: 600px) 100vw, 600px\" srcset=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/\u56fe\u7247-205.png 600w, http:\/\/dn.cailiaoniu.com\/2021\/10\/\u56fe\u7247-205-300x141.png 300w\" alt=\"\" width=\"600\" height=\"282\" \/><\/strong><\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1ahttps:\/\/www.science.org\/doi\/10.1126\/science.abj3210<\/p>\n<p><strong>7. \u738b\u6625\u751f&amp;Oleg Borodin\u7535\u6c60\u767b\u9876Science\u5c01\u9762\uff0c\u54c8\u5de5\u5927\u5c39\u9e3d\u5e73&amp;\u5de6\u670b\u5efa\u4eae\u70b9\u8bc4\u8bba<\/strong><\/p>\n<p><strong><b>\u7f8e\u56fd<\/b><\/strong><strong><b>\u9a6c\u91cc\u5170\u5927\u5b66\u738b\u6625\u751f\u6559\u6388\u548c\u7f8e\u56fd\u9646\u519b\u7814\u7a76\u5b9e\u9a8c\u5ba4Oleg Borodin<\/b><\/strong><strong><b>\uff08<\/b><\/strong><strong><b>\u5171\u540c<\/b><\/strong><strong><b>\u901a\u8baf\u4f5c\u8005\uff09<\/b><\/strong>\u53d1\u73b0\u4e86\u4e00\u7cfb\u5217\u7532\u6c27\u57fa\u4e59\u80fa\u87af\u5408\u5242\uff0c\u901a\u8fc7\u6eb6\u5242\u5316\u9798\u91cd\u7ec4\u6781\u5927\u5730\u4fc3\u8fdb\u4e86\u754c\u9762\u7535\u8377\u8f6c\u79fb\u52a8\u529b\u5b66\uff0c\u5e76\u6291\u5236\u4e86\u6b63\u6781\u548c\u91d1\u5c5e\u526f\u6781\u4e0a\u7684\u526f\u53cd\u5e94\uff0c\u4ece\u800c\u5b9e\u73b0\u4e86\u80fd\u91cf\u5bc6\u5ea6\u4e3a\u5206\u522b\u4e3a412Wh\/kg\u548c471Wh\/kg\u3002\u57fa\u4f53\u800c\u8a00\uff0c\u8bc1\u660e\u4e86\u5728Mg<sup>2+<\/sup>\u548cCa<sup>2+<\/sup>\u7684\u7b2c\u4e00\u4e2a\u6eb6\u5242\u5316\u9798\u4e2d\uff0c\u591a\u9f7f\u7532\u6c27\u57fa\u4e59\u57fa\u80fa\u87af\u5408\u5242[-(CH<sub>2<\/sub>OCH<sub>2<\/sub>CH<sub>2<\/sub>N)<sub>n<\/sub>-]\u80fd\u591f\u5b9e\u73b0\u9ad8\u5ea6\u53ef\u9006\u7684Mg\u548cCa\u8d1f\u6781\uff0c\u5e76\u5feb\u901f\u5c06Mg<sup>2+<\/sup>\u548cCa<sup>2+<\/sup>\u63d2\u5165\u9ad8\u538b\u5c42\u72b6\u6c27\u5316\u7269\u6b63\u6781\u4e2d\u3002\u503c\u5f97\u6ce8\u610f\u7684\u662f\uff0c\u8fd9\u4e9b\u87af\u5408\u5242\u5bf9Mg<sup>2+<\/sup>\u7684\u4eb2\u548c\u529b\u662f\u4f20\u7edf\u919a\u7c7b\u6eb6\u5242\u76846-41\u500d\uff0c\u4f46\u5bcc\u542b\u87af\u5408\u5242\u7684\u6eb6\u5242\u5316\u9798\u901a\u8fc7\u91cd\u7ec4\u7ed5\u8fc7\u4e86\u80fd\u91cf\u4e0d\u5229\u7684\u53bb\u6eb6\u5242\u8fc7\u7a0b\uff0c\u4ece\u800c\u51cf\u5c11\u4e86\u8fc7\u7535\u4f4d\uff0c\u6d88\u9664\u4e86\u8d1f\u6781\u548c\u6b63\u6781\u4f34\u968f\u7684\u526f\u53cd\u5e94\u3002\u6b64\u5916\uff0c\u8fd9\u4e9b\u7535\u89e3\u6db2\u7684\u91cd\u7ec4\u80fd\u53ef\u4ee5\u901a\u8fc7\u6539\u53d8\u87af\u5408\u5242\u7684\u4ecb\u7535\u5e38\u6570\u548c\u5927\u5c0f\u6765\u8c03\u6574\u3002\u8fd9\u9879\u5de5\u4f5c\u4e3a\u4e8c\u4ef7\u91d1\u5c5e\u7535\u6c60\u63d0\u4f9b\u4e86\u4e00\u79cd\u901a\u7528\u7684\u7535\u89e3\u8d28\u8bbe\u8ba1\u7b56\u7565\u3002\u76f8\u5173\u7814\u7a76\u6210\u679c\u4ee5\u201c<strong><b>Solvation sheath reorganization enables divalent metal batteries with fast interfacial charge transfer kinetics<\/b><\/strong>\u201d\u4e3a\u9898\u53d1\u8868\u5728<strong><em><b><i>Science<\/i><\/b><\/em><\/strong>\u4e0a\u3002<\/p>\n<p>\u5bf9\u6b64\uff0c<strong><b>\u54c8\u5c14\u6ee8\u5de5\u4e1a\u5927\u5b66\u5c39\u9e3d\u5e73\u6559\u6388\u548c\u5de6\u670b\u5efa\u6559\u6388<\/b><\/strong>\u505a\u51fa\u91cd\u8981\u5c55\u671b\uff0c\u8ba4\u4e3a\u738b\u6625\u751f\u6559\u6388\u548cOleg Borodin\u535a\u58eb\u6240\u63d0\u51fa\u7684\u6eb6\u5242\u5316\u9798\u91cd\u7ec4\u7b56\u7565\u4e3a\u5b9e\u73b0\u90e8\u5206\u53bb\u6eb6\u5242\u5316\u4ee5\u5339\u914d\u6d3b\u6027\u6750\u6599\u6846\u67b6\u7ed3\u6784\u63d0\u4f9b\u4e86\u6307\u5bfc\u3002\u6eb6\u5242\u9798\u91cd\u7ec4\u7684\u5e94\u7528\u5e94\u6269\u5c55\u5230\u5176\u4ed6\u9ad8\u6bd4\u80fd\u91cf\u6b63\u6781\u6750\u6599\u3002\u56e0\u6b64\uff0c\u5bf9\u4e8c\u4ef7\u91d1\u5c5e\u9633\u79bb\u5b50\u6eb6\u5242\u5316\u9798\u7684\u7814\u7a76\u5c06\u6709\u52a9\u4e8e\u65b0\u7535\u89e3\u6db2\u7684\u5f00\u53d1\uff0c\u4ece\u800c\u4f7f\u5f97\u7535\u6781-\u6eb6\u5242\u5316\u91d1\u5c5e\u9633\u79bb\u5b50\u754c\u9762\u6a21\u578b\u7684\u5efa\u7acb\u5f97\u5230\u5e7f\u6cdb\u7814\u7a76\u3002\u76f8\u5173\u8bc4\u8bba\u4ee5\u201c<strong><b>Chelated electrolytes for divalent metal ions<\/b><\/strong>\u201d\u4e3a\u9898\u53d1\u8868\u5728<strong><em><b><i>Science<\/i><\/b><\/em><\/strong>\u4e0a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228198\" src=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/%E8%AF%84%E8%AE%BA.jpg\" sizes=\"(max-width: 600px) 100vw, 600px\" srcset=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/\u8bc4\u8bba.jpg 600w, http:\/\/dn.cailiaoniu.com\/2021\/10\/\u8bc4\u8bba-300x134.jpg 300w\" alt=\"\" width=\"600\" height=\"267\" \/><\/p>\n<p><strong><b>\u6587\u732e\u94fe\u63a5<\/b><\/strong>\uff1a\u201c<a href=\"https:\/\/www.science.org\/doi\/10.1126\/science.abg3954\"><strong><u><b>Solvation sheath reorganization enables divalent metal batteries with fast interfacial charge transfer kinetics<\/b><\/u><\/strong><\/a>\u201d<strong><b>(<\/b><\/strong><strong><b>Science<\/b><\/strong><strong><b>\uff0c202<\/b><\/strong><strong><b>1<\/b><\/strong><strong><b>\uff0c<\/b><\/strong><strong><b>10.1126\/science.abg3954<\/b><\/strong><strong><b>)<\/b><\/strong><\/p>\n<p>\u201c<a href=\"https:\/\/www.science.org\/doi\/10.1126\/science.abi6643\"><strong><u><b>Chelated electrolytes for divalent metal ions<\/b><\/u><\/strong><\/a>\u00a0\u201d<strong><b>(<\/b><\/strong><strong><b>Science<\/b><\/strong><strong><b>\uff0c202<\/b><\/strong><strong><b>1\uff0c 10.1126\/science.abi6643\u00a0<\/b><\/strong><strong><b>)<\/b><\/strong><\/p>\n<p><strong>8. Science\u89e3\u8bfb\uff1a\u901a\u8fc7\u6291\u5236\u6b20\u63ba\u6742YBa2Cu3O7-\u03b4\u4e2d\u7684\u7535\u8377\u5bc6\u5ea6\u6ce2\u6062\u590d\u5947\u5f02\u91d1\u5c5e\u76f8<\/strong><\/p>\n<p><strong><b>\u67e5\u5c14\u9ed8\u65af\u7406\u5de5\u5927\u5b66Riccardo Arpaia\u3001Floriana Lombardi\u56e2\u961f\u5229\u7528\u5176\u5355\u80de\u5728\u886c\u5e95\u8bf1\u5bfc\u7684\u5f3a\u5e94\u53d8\u4e0b\u7684\u51e0\u4f55\u4fee\u9970\u8c03\u8c10\u94dc\u9178\u76d0\u6750\u6599YBa<\/b><\/strong><strong><sub><b>2<\/b><\/sub><\/strong><strong><b>Cu<\/b><\/strong><strong><sub><b>3<\/b><\/sub><\/strong><strong><b>O<\/b><\/strong><strong><sub><b>7-\u03b4<\/b><\/sub><\/strong><strong><b>(YBCO)\u8584\u819c\u4e2d\u7684\u57fa\u6001<\/b><\/strong><strong><b>\u6765\u63a2\u7a76<\/b><\/strong><strong><b>CDW\u4e0eT\u7ebf\u6027\u884c\u4e3a\u504f\u79bb\u4e4b\u95f4\u7684<\/b><\/strong><strong><b>\u5173\u7cfb<\/b><\/strong>\u3002\u672c\u5de5\u4f5c\u53d1\u73b0\uff0c\u5f53\u6291\u5236\u5171\u632f\u975e\u5f39\u6027x\u5c04\u7ebf\u6563\u5c04\u68c0\u6d4b\u5230\u7684CDW\u632f\u5e45\u65f6\uff0c\u9ad8\u5e94\u53d8\u3001\u8d85\u8584\u3001\u6b20\u63ba\u6742\u7684YBa<sub>2<\/sub>Cu<sub>3<\/sub>O<sub>7-\u03b4<\/sub>\u8584\u819c\u7684T\u7ebf\u6027\u7535\u963b\u7387\u5f97\u5230\u6062\u590d\u3002\u8fd9\u4e00\u53d1\u73b0\u6697\u793a\u4e86\u6b20\u63ba\u6742\u94dc\u9178\u76d0\u4e2dCDWs\u7684\u51fa\u73b0\u4e0eT\u7ebf\u7535\u963b\u7387\u7684\u504f\u79bb\u5bc6\u5207\u76f8\u5173\u3002\u672c\u5de5\u4f5c\u7684\u7ed3\u679c\u8bf4\u660e\u4e86\u4f7f\u7528\u5e94\u53d8\u63a7\u5236\u6765\u64cd\u7eb5\u91cf\u5b50\u6750\u6599\u57fa\u6001\u7684\u6f5c\u529b\u3002<strong><b>\u76f8\u5173\u6210\u679c\u4ee5\u9898\u4e3a\u201cRestored strange metal phase through suppression of charge density waves in underdoped YBa2Cu3O7\u2013\u03b4\u201d\u53d1\u8868\u5728\u4e86Science\u4e0a\u3002<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-227825\" src=\"http:\/\/dn.cailiaoniu.com\/2021\/09\/%E5%9B%BE%E7%89%87-150.png\" sizes=\"(max-width: 600px) 100vw, 600px\" srcset=\"http:\/\/dn.cailiaoniu.com\/2021\/09\/\u56fe\u7247-150.png 600w, http:\/\/dn.cailiaoniu.com\/2021\/09\/\u56fe\u7247-150-300x145.png 300w\" alt=\"\" width=\"600\" height=\"289\" \/><\/p>\n<p>\u8bba\u6587doi\uff1ahttps:\/\/doi.org\/10.1126\/science.abc8372<\/p>\n<p><strong>9. \u5357\u7b56\u6587&amp;\u6797\u5143\u534e&amp;\u91d1\u594e\u5a1fScience:\u8d85\u987a\u7535\u5f1b\u8c6b\u94c1\u7535\u4f53\u4e2d\u7684\u8d85\u9ad8\u80fd\u91cf\u5b58\u50a8<\/strong><\/p>\n<p><strong><b>\u6e05\u534e\u5927\u5b66\u5357\u7b56\u6587\u9662\u58eb<\/b><\/strong><strong><b>\uff0c<\/b><\/strong><strong><b>\u6797\u5143\u534e<\/b><\/strong><strong><b>\u6559\u6388<\/b><\/strong><strong><b>\u548c\u4e2d\u56fd\u79d1\u5b66\u9662\u7269\u7406\u6240\u91d1\u594e\u5a1f\u6559\u6388<\/b><\/strong><strong><b>\uff08<\/b><\/strong><strong><b>\u5171\u540c<\/b><\/strong><strong><b>\u901a\u8baf\u4f5c\u8005\uff09<\/b><\/strong>\u5c55\u793a\u4e86\u901a\u8fc7\u8d85\u987a\u7535\u6001\uff08SPE\uff09\u8bbe\u8ba1\u53ef\u5927\u5e45\u5ea6\u63d0\u9ad8\u5f1b\u8c6b\u94c1\u7535\u8584\u819c\u7684\u80fd\u91cf\u5b58\u50a8\u6027\u80fd\u3002\u7a76\u5176\u539f\u56e0\uff0c\u8584\u819c\u7eb3\u7c73\u57df\u6309\u6bd4\u4f8b\u7f29\u5c0f\u4e3a\u51e0\u4e2a\u5355\u5143\u7684\u6781\u6027\u7c07\uff0c\u56e0\u6b64\u51e0\u4e4e\u6d88\u9664\u4e86\u6781\u5316\u5207\u6362\u6ede\u540e\uff0c\u540c\u65f6\u4fdd\u6301\u4e86\u76f8\u5bf9\u8f83\u9ad8\u7684\u6781\u5316\u3002\u5177\u4f53\u800c\u8a00\uff0c\u4f5c\u8005\u5236\u5907\u4e86\u4e00\u7cfb\u5217\u9490\uff08Sm\uff09\u63ba\u6742\u7684yBiFeO<sub>3<\/sub>-(1-y)BaTiO<sub>3<\/sub>\uff08Sm-BFBT\uff1by=0.1 \u52300.9\uff09\u5f1b\u8c6b\u94c1\u7535\u8584\u819c\uff0cSm\u63ba\u6742\u5242\u53ef\u4ee5\u6709\u6548\u5730\u589e\u52a0\u5c40\u90e8\u5f02\u8d28\u6027\u3002\u540c\u65f6\uff0c\u6a21\u62df\u4e86\u4e0e\u6e29\u5ea6\u76f8\u5173\u7684\u4ecb\u7535\u5e38\u6570\u3001\u57df\u7ed3\u6784\u7b49\u3002\u572830%\u8d85\u987a\u7535Sm\u63ba\u6742\u94c1\u9178\u94cb-\u949b\u9178\u94a1\u8584\u819c\u4e2d\u5b9e\u73b0\u4e86\u6bcf\u7acb\u65b9\u5398\u7c73152\u7126\u8033\u7684\u8d85\u9ad8\u80fd\u91cf\u50a8\u5b58\u5bc6\u5ea6\uff0c\u5e76\u663e\u8457\u63d0\u9ad8\u4e86\u50a8\u80fd\u6548\u7387\uff08\u57283.5\u5146\u4f0f\/\u5398\u7c73\u7684\u7535\u573a\u4e0b\u8d85\u8fc7\u4e8690%\uff09\u3002\u66f4\u52a0\u91cd\u8981\u7684\u662f\uff0c\u5145\u653e\u7535\u7684\u53ef\u9760\u6027\u548c\u5728\u5bbd\u6e29\u5ea6\u8303\u56f4\u5185\u7684\u6027\u80fd\u7a33\u5b9a\u6027\u4e5f\u5145\u5206\u8bc1\u660e\u4e86\u5f1b\u8c6b\u94c1\u7535\u8584\u819c\u51fa\u8272\u6027\u80fd\u3002\u76f8\u5173\u7814\u7a76\u6210\u679c\u4ee5\u201c<strong><b>Ultrahigh energy storage in superparaelectric relaxor ferroelectrics<\/b><\/strong>\u201d\u4e3a\u9898\u53d1\u8868\u5728<strong><em><b><i>Science<\/i><\/b><\/em><\/strong>\u4e0a\u3002<\/p>\n<p><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-228027\" src=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/%E5%9B%BE1.jpg\" sizes=\"(max-width: 600px) 100vw, 600px\" srcset=\"http:\/\/dn.cailiaoniu.com\/2021\/10\/\u56fe1.jpg 600w, http:\/\/dn.cailiaoniu.com\/2021\/10\/\u56fe1-300x218.jpg 300w\" alt=\"\" width=\"600\" height=\"435\" \/><\/b><\/strong><\/p>\n<p><strong><b>\u6587\u732e\u94fe\u63a5<\/b><\/strong>\uff1a\u201c<a href=\"https:\/\/www.science.org\/doi\/10.1126\/science.abi7687\"><strong><u><b>Ultrahigh energy storage in superparaelectric relaxor ferroelectrics<\/b><\/u><\/strong><\/a>\u201d<strong><b>(<\/b><\/strong><strong><b>Science<\/b><\/strong><strong><b>\uff0c202<\/b><\/strong><strong><b>1<\/b><\/strong><strong><b>\uff0c<\/b><\/strong><strong><b>10.1126\/science.abi7687<\/b><\/strong><strong><b>)<\/b><\/strong><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u672c\u7bc7\u6587\u7ae0\u4e3a\u5927\u5bb6\u68b3\u7406\u4e8610\u6708\u4efd\u6750\u6599\u3001\u5316\u5b66\u9886\u57dfNS\u53d1\u6587\u60c5\u51b5\u3002\u76f8\u5173\u6210\u679c\u5df2\u6536\u5f55\u5165\u6750\u6599\u4eba\u6700\u65b0\u4e0a\u7ebf\u4ea7\u54c1\u5e93\u3002 1. Nature\uff1a\u8ba9\u6240\u6709\u4eba\u559d\u4e0a\u53ef\u996e\u7528\u6c34 X\u767b\u6708\u8ba1\u5212\u5de5\u5382Jack&#8230;<\/p>\n","protected":false},"author":11454,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[1187],"tags":[],"class_list":["post-229340","post","type-post","status-publish","format-standard","hentry","category-zhuanlan"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/229340"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/11454"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=229340"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/229340\/revisions"}],"predecessor-version":[{"id":229363,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/229340\/revisions\/229363"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=229340"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=229340"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=229340"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}