{"id":231402,"date":"2021-12-31T06:28:53","date_gmt":"2021-12-30T22:28:53","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=231402"},"modified":"2021-12-30T19:44:58","modified_gmt":"2021-12-30T11:44:58","slug":"%e9%a6%99%e6%b8%af%e5%9f%8e%e5%b8%82%e5%a4%a7%e5%ad%a6%e6%9d%a8%e6%b6%9bmaterials-today%ef%bc%9a%e5%8c%96%e5%ad%a6%e5%a4%8d%e6%9d%82%e5%9e%8b%e9%87%91%e5%b1%9e%e9%97%b4%e5%8c%96%e5%90%88%e7%89%a9","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=231402","title":{"rendered":"\u9999\u6e2f\u57ce\u5e02\u5927\u5b66\u6768\u6d9bMaterials Today\uff1a\u5316\u5b66\u590d\u6742\u578b\u91d1\u5c5e\u95f4\u5316\u5408\u7269\u5408\u91d1\u2014\u2014\u6750\u6599\u521b\u65b0\u7684\u65b0\u524d\u6cbf"},"content":{"rendered":"<p><strong><b>\u3010\u7814\u7a76\u6982\u8ff0\u3011<\/b><\/strong><\/p>\n<p>\u91d1\u5c5e\u95f4\u5316\u5408\u7269\u6750\u6599\u62e5\u6709\u591a\u79cd\u591a\u6837\u7684\u6709\u5e8f\u8d85\u70b9\u9635\u7ed3\u6784\u548c\u8bb8\u591a\u4e0d\u540c\u5bfb\u5e38\u7684\u7269\u7406\u5316\u5b66\u7279\u6027\u3002\u7279\u522b\u662f<strong><b>\u5316\u5b66\u590d\u6742\u578b\u91d1\u5c5e\u95f4\u5316\u5408\u7269\u5408\u91d1\uff08<\/b><\/strong><strong><b>CCIMAs<\/b><\/strong><strong><b>\uff1b\u4ea6\u6216\u88ab\u79f0\u4e4b\u4e3a\u591a\u7ec4\u5143\u8d85\u70b9\u9635\u5408\u91d1\uff0c\u9ad8\u71b5\u91d1\u5c5e\u95f4\u5316\u5408\u7269\u5408\u91d1\u7b49<\/b><\/strong><strong><b>\uff09<\/b><\/strong>\u7684\u51fa\u73b0\u5728\u8fd1\u5e74\u6765\u53d7\u5230\u4e86\u76f8\u5f53\u5927\u7684\u5173\u6ce8\uff0c\u5e76\u4e3a\u5f00\u53d1\u7528\u4e8e\u9ad8\u7ea7\u7ed3\u6784\u5e94\u7528\u7684\u65b0\u578b\u91d1\u5c5e\u6750\u6599\u63d0\u4f9b\u4e86\u5d2d\u65b0\u7684\u8bbe\u8ba1\u8def\u5f84\u3002\u8fd9\u4e9b\u65b0\u578bCCIMAs\u53ef\u8868\u73b0\u51fa\u975e\u5e38<strong><b>\u72ec\u7279\u7684<\/b><\/strong><strong><b>\u7ed3\u6784\u548c\u5316\u5b66\u7684\u534f\u540c\u8c03\u8282<\/b><\/strong>\uff0c\u4f8b\u5982\u81ea\u7ec4\u88c5\u957f\u7a0b\u5bc6\u6392\u7684\u539f\u5b50\u6709\u5e8f\u6392\u5217\u3001\u590d\u6742\u8d85\u6676\u683c\u7684\u4e9a\u70b9\u9635\u5360\u4f4d\u548c\u754c\u9762\u7eb3\u7c73\u7ea7\u7684\u591a\u5143\u7d20\u5171\u504f\u805a\u548c\u65e0\u5e8f\u76f8\u53d8\u7b49\uff0c\u4ece\u800c\u663e\u793a\u51fa\u4e86\u8bf8\u591a\u4f20\u7edf\u91d1\u5c5e\u6750\u6599\u6240\u65e0\u6cd5\u62e5\u6709\u7684\u4f18\u5f02\u7684\u7269\u7406\u548c\u673a\u68b0\u6027\u80fd\uff0c\u5982\u53cd\u5e38\u5c48\u670d\u3001\u9ad8\u5f3a\u97e7\u3001\u6297\u8815\u53d8\u3001\u8d85\u5f39\u6027\u3001\u5f62\u72b6\u8bb0\u5fc6\u6548\u5e94\u7b49\u7b49\u3002\u9999\u6e2f\u57ce\u5e02\u5927\u5b66\u6768\u6d9b\u8bfe\u9898\u7ec4\u63d0\u51fa\u7684CCIMAs\u7684\u5408\u91d1\u8bbe\u8ba1\u7b56\u7565\u5927\u5927\u62d3\u5bbd\u4e86\u65b0\u6750\u6599\u521b\u65b0\u4e0e\u7814\u53d1\u7684\u601d\u8def\u4e0e\u8303\u56f4\u3002\u6beb\u65e0\u7591\u95ee\uff0c\u8fd9\u4e00\u521b\u65b0\u7406\u5ff5\u4e5f\u5c06\u6210\u4e3a\u5f00\u53d1\u65b0\u578b\u9ad8\u6027\u80fd\u5408\u91d1\u4e0e\u7279\u79cd\u88c5\u5907\u7684\u65b0\u524d\u6cbf,\u00a0\u6709\u671b\u5728\u822a\u7a7a\u822a\u5929\u3001\u6838\u80fd\u3001\u6c7d\u8f66\u3001\u5316\u5b66\u5de5\u7a0b\u7b49\u5173\u952e\u9886\u57df\u53d1\u6325\u5341\u5206\u91cd\u8981\u7684\u4f5c\u7528\u3002\u76f8\u5173\u6210\u679c\u4ee5<strong><b>\u00a0<\/b><\/strong><strong><em><b><i>\u201c<\/i><\/b><\/em><\/strong><strong><em><b><i>Chemically complex intermetallic alloys: a new frontier for innovative structural materials\u201d<\/i><\/b><\/em><\/strong><strong><b>\u4e3a\u6807\u9898<\/b><\/strong><strong><b>\u53d1\u8868\u5728<\/b><\/strong><strong><em><b><i>M<\/i><\/b><\/em><\/strong><strong><em><b><i>aterials Today<\/i><\/b><\/em><\/strong><strong><b>\u671f\u520a<\/b><\/strong><strong><b>\u00a0(<\/b><\/strong><strong><u><b>https:\/\/doi.org\/10.1016\/j.mattod.2021.12.004<\/b><\/u><\/strong><strong><b>; IF:31.041)<\/b><\/strong>\u00a0\u3002\u8be5\u8bba\u6587\u7b2c\u4e00\u4f5c\u8005\u548c\u901a\u8baf\u4f5c\u8005\u4e3a\u9999\u6e2f\u57ce\u5e02\u5927\u5b66\u6750\u6599\u79d1\u5b66\u4e0e\u5de5\u7a0b\u5b66\u9662\u7684<strong><b>\u6768\u6d9b\u6559\u6388\uff08T<\/b><\/strong><strong><b>. Y<\/b><\/strong><strong><b>ang\uff09\uff0c<\/b><\/strong>\u9999\u6e2f\u57ce\u5e02\u5927\u5b66\u7684\u5218\u9526\u5ddd\u6559\u6388(C.T. Liu)\u4e3a\u8be5\u8bba\u6587\u5171\u540c\u901a\u8baf\u4f5c\u8005\u3002\u5408\u4f5c\u8005\u5305\u62ec\u9999\u6e2f\u57ce\u5e02\u5927\u5b66B.X. Cao\u535a\u58eb\u3001T.L. Zhang\u535a\u58eb\u3001J.H. Luan\u535a\u58eb\uff0cH.J. Kong\uff0c\u4ee5\u53ca\u54c8\u5c14\u6ee8\u5de5\u4e1a\u5927\u5b66\u7684Y.L. Zhao\u6559\u6388\u3001W.H. Liu\u6559\u6388\u7b49\u7b49\u3002\u8bba\u6587\u94fe\u63a5\uff1a<strong><u><b>https:\/\/doi.org\/10.1016\/j.mattod.2021.12.004<\/b><\/u><\/strong><strong><b>\u3002<\/b><\/strong><\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/1-24.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231411\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/1-24.png\" alt=\"\" width=\"928\" height=\"525\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/1-24.png 928w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/1-24-300x170.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/1-24-768x434.png 768w\" sizes=\"(max-width: 928px) 100vw, 928px\" \/><\/a><\/p>\n<p><strong><b>\u3010\u56fe\u6587\u6458\u8981\u3011<\/b><\/strong><\/p>\n<p><strong><b>\u56fe1<\/b><\/strong><strong><b>.<\/b><\/strong>\u00a0\u4e09\u79cd\u5177\u6709L1<sub>2<\/sub>\u578b\u6676\u4f53\u7ed3\u6784\u7684\u4e8c\u5143\u91d1\u5c5e\u95f4\u5316\u5408\u7269\u5408\u91d1\u7684\u53cd\u5e38\u5c48\u670d\u884c\u4e3a<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/2-25.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231412\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/2-25.png\" alt=\"\" width=\"675\" height=\"656\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/2-25.png 675w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/2-25-300x292.png 300w\" sizes=\"(max-width: 675px) 100vw, 675px\" \/><\/a><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>2.<\/b><\/strong>\u00a0\u4e8c\u5143\u91d1\u5c5e\u95f4\u5316\u5408\u7269\u5408\u91d1\u4e2d\u6700\u5e38\u89c1\u768420\u79cd\u6bcd\u4f53\u6676\u4f53\u7ed3\u6784\u7684\u7edf\u8ba1\u4e0e\u5206\u5e03<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/3-23.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231414\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/3-23.png\" alt=\"\" width=\"1174\" height=\"574\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/3-23.png 1174w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/3-23-300x147.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/3-23-768x375.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/3-23-1024x501.png 1024w\" sizes=\"(max-width: 1174px) 100vw, 1174px\" \/><\/a><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>3.<\/b><\/strong>\u00a0\u65b0\u578b\u5316\u5b66\u590d\u6742\u578bL1<sub>2<\/sub>\u548cB2\u8d85\u70b9\u9635\u5408\u91d1\u4e0e\u4f20\u7edf\u4e8c\u5143\u8d85\u70b9\u9635\u5408\u91d1\u7684\u539f\u5b50\u5360\u4f4d\u793a\u610f\u56fe<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/4-22.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231417\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/4-22.png\" alt=\"\" width=\"764\" height=\"704\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/4-22.png 764w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/4-22-300x276.png 300w\" sizes=\"(max-width: 764px) 100vw, 764px\" \/><\/a><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>5.<\/b><\/strong>\u00a0\u5316\u5b66\u590d\u6742\u578b\u91d1\u5c5e\u95f4\u5316\u5408\u7269\u5408\u91d1\u4e2d\u72ec\u7279\u7684\u6676\u754c\u7eb3\u7c73\u65e0\u5e8f\u5316\u548c\u591a\u5143\u7d20\u534f\u540c\u5171\u504f\u805a\u884c\u4e3a<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/5-21.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231418\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/5-21.png\" alt=\"\" width=\"789\" height=\"892\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/5-21.png 789w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/5-21-265x300.png 265w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/5-21-768x868.png 768w\" sizes=\"(max-width: 789px) 100vw, 789px\" \/><\/a><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>6.<\/b><\/strong>\u00a0\u5316\u5b66\u590d\u6742\u578b\u91d1\u5c5e\u95f4\u5316\u5408\u7269\u5408\u91d1\uff08\u5355\u6676\u6001\uff09\u4e2d\u7684\u8d85\u5f39\u6027\u4e0e\u975e\u4f20\u7edf\u7684\u76f8\u53d8\u884c\u4e3a<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/6-16.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231420\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/6-16.png\" alt=\"\" width=\"1076\" height=\"761\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/6-16.png 1076w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/6-16-300x212.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/6-16-768x543.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/6-16-1024x724.png 1024w\" sizes=\"(max-width: 1076px) 100vw, 1076px\" \/><\/a><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>8.<\/b><\/strong>\u00a0\u5316\u5b66\u590d\u6742\u578b\u91d1\u5c5e\u95f4\u5316\u5408\u7269\u5408\u91d1\u7684\u9ad8\u6e29\u8815\u53d8\u884c\u4e3a<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/7-14.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231419\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/7-14.png\" alt=\"\" width=\"1002\" height=\"869\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/7-14.png 1002w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/7-14-300x260.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/7-14-768x666.png 768w\" sizes=\"(max-width: 1002px) 100vw, 1002px\" \/><\/a><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>9.<\/b><\/strong>\u00a0\u5177\u6709\u7a33\u5b9a\u7eb3\u7c73\u6676\u7ed3\u6784\u7684\u5316\u5b66\u590d\u6742\u578b\u91d1\u5c5e\u95f4\u5316\u5408\u7269\u5408\u91d1\u7684\u8bbe\u8ba1\u601d\u8def\u4e0e\u6784\u60f3<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/8-12.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231421\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/8-12.png\" alt=\"\" width=\"1085\" height=\"782\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/8-12.png 1085w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/8-12-300x216.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/8-12-768x554.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/12\/8-12-1024x738.png 1024w\" sizes=\"(max-width: 1085px) 100vw, 1085px\" \/><\/a><\/p>\n<p><strong><b>\u3010\u4f5c\u8005\u7b80\u4ecb\u3011<\/b><\/strong><\/p>\n<p>\u6768\u6d9b\uff0c\u9999\u6e2f\u57ce\u5e02\u5927\u5b66\u6750\u6599\u79d1\u5b66\u4e0e\u5de5\u7a0b\u7cfb\u52a9\u7406\u6559\u6388\uff0c\u535a\u5bfc\uff0c\u9999\u6e2f\u57ce\u5e02\u5927\u5b66\u6df1\u5733\u7814\u7a76\u9662\u526f\u7814\u7a76\u5458\uff0c\u9999\u6e2f\u4e09\u7ef4\u539f\u5b50\u63a2\u9488\u8054\u5408\u7814\u7a76\u5b9e\u9a8c\u5ba4\u7684\u6838\u5fc3\u6210\u5458\u7b49\u3002\u5148\u540e\u8363\u83b7\u9999\u6e2f\u9ad8\u7b49\u7814\u7a76\u9662(HKIAS)\u6770\u51fa\u535a\u58eb\u540e\u7814\u7a76\u5458\uff0c\u00a0Rising Star Award\uff0c\u9999\u6e2f\u6770\u51fa\u9752\u5e74\u5b66\u8005\u7b49\u79f0\u53f7\u3002\u957f\u671f\u4ece\u4e8b\u5148\u8fdb\u91d1\u5c5e\u6750\u6599\u7684\u5408\u91d1\u8bbe\u8ba1\u4e0e\u7ec4\u7ec7\u7ed3\u6784\u8c03\u63a7\u7684\u7814\u7a76\uff0c\u4e3b\u8981\u901a\u8fc7\u4e09\u7ef4\u539f\u5b50\u63a2\u9488\u5c42\u6790\uff083D-APT\uff09\u548c\u900f\u5c04\u7535\u955c\uff08HR-TEM\uff09\u7b49\u6280\u672f\u624b\u6bb5\u7814\u7a76\u5408\u91d1\u6750\u6599\u7684\u6210\u5206\u8bbe\u8ba1\u3001\u6750\u6599\u70ed\u529b\u5b66\u4e0e\u52a8\u529b\u5b66\u884c\u4e3a\u3001\u56fa\u6001\u76f8\u53d8\u884c\u4e3a\u4e0e\u53d8\u5f62\u673a\u5236\u7b49\u3002\u76ee\u524d\u7684\u7814\u7a76\u8bfe\u9898\u4e3b\u8981\u96c6\u4e2d\u5728\u591a\u4e3b\u5143\u91d1\u5c5e\u95f4\u5316\u5408\u7269\uff0c\u9ad8\u71b5\u5408\u91d1\uff0c\u949b\u5408\u91d1\u3001\u6676\u754c\u5de5\u7a0b\u30013D\u6253\u5370\u7b49\u76f8\u5173\u9886\u57df\u3002\u8bfe\u9898\u7ec4\u5185\u62e5\u6709\u975e\u5e38\u9f50\u5168\u7684\u91d1\u5c5e\u6750\u6599\u52a0\u5de5\u4e0e\u663e\u5fae\u8868\u5f81\u7684\u4eea\u5668\u8bbe\u5907\u3002\u8fd1\u5e74\u6765\u5148\u540e\u53d6\u5f97\u4e86\u591a\u9879\u5f00\u62d3\u6027\u7684\u7814\u7a76\u6210\u679c\u3002\u622a\u81f3\u76ee\u524d\u4e3a\u6b62\uff0c\u5df2\u5728\u6750\u6599\u9886\u57df\u7684\u77e5\u540d\u671f\u520aActa Materialia, Scripta Materialia, Science, Advanced Materials, Journal of Alloys and Compounds, Intermetallic, Nature Communications, Materials Research Letters\u7b49\u53d1\u8868\u5b66\u672f\u8bba\u658750\u4f59\u00a0\u7bc7\uff0c\u5176\u4e2d\u4ee5\u7b2c\u4e00\u4f5c\u8005\u548c\u901a\u8baf\u4f5c\u8005\u5728Science\u671f\u520a\u53d1\u8868\u5b66\u672f\u8bba\u6587\u4e09\u7bc7\u3002\u5148\u540e\u62c5\u4efbActa Materialia, Scripta Materialia, Science, Advanced Materials, Journal of Alloys and Compounds, Intermetallics, Materials Today Physics\u7b49\u671f\u520a\u7684\u5ba1\u7a3f\u4eba\u3002\u4e0e\u6b64\u540c\u65f6\uff0c\u62c5\u4efbAdvanced Powder Materials\u671f\u520a\u7279\u8058\u7f16\u59d4\u3001\u300a\u7c89\u672b\u51b6\u91d1\u6750\u6599\u79d1\u5b66\u4e0e\u5de5\u7a0b\u300b\u671f\u520a\u7f16\u59d4\u3001Frontier in Materials\u5ba2\u5ea7\u7f16\u59d4\uff0c\u56fd\u9645\u79d1\u5b66\u7ec4\u7ec7Vebleo\u534f\u4f1a\u4f1a\u58eb\uff08Vebleo Fellow\uff09\u7b49\u3002<\/p>\n<p><strong><b>\u3010\u53c2\u8003\u6587\u732e\u3011<\/b><\/strong><\/p>\n<p>\u30101\u3011Yang, T., et al. &#8221; Chemically complex intermetallic alloys: a new frontier for innovative structural materials &#8221;\u00a0Materials Today\u00a0(2021).<\/p>\n<p>\u30102\u3011Yang, T., et al. &#8220;Ultrahigh-strength and ductile superlattice alloys with nanoscale disordered interfaces.&#8221; Science 369.6502 (2020): 427-432.<\/p>\n<p>\u30103\u3011Yang, T., et al. &#8220;Towards superior mechanical properties of hetero-structured high-entropy alloys via engineering multicomponent intermetallic nanoparticles.&#8221; Scripta Materialia 183 (2020): 39-44.<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u7814\u7a76\u6982\u8ff0\u3011 \u91d1\u5c5e\u95f4\u5316\u5408\u7269\u6750\u6599\u62e5\u6709\u591a\u79cd\u591a\u6837\u7684\u6709\u5e8f\u8d85\u70b9\u9635\u7ed3\u6784\u548c\u8bb8\u591a\u4e0d\u540c\u5bfb\u5e38\u7684\u7269\u7406\u5316\u5b66\u7279\u6027\u3002\u7279\u522b\u662f\u5316\u5b66\u590d\u6742\u578b\u91d1\u5c5e\u95f4\u5316\u5408\u7269\u5408\u91d1\uff08CCIMAs\uff1b\u4ea6\u6216\u88ab\u79f0\u4e4b\u4e3a\u591a\u7ec4\u5143\u8d85\u70b9\u9635&#8230;<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-231402","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/231402"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=231402"}],"version-history":[{"count":4,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/231402\/revisions"}],"predecessor-version":[{"id":231423,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/231402\/revisions\/231423"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=231402"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=231402"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=231402"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}