{"id":231759,"date":"2022-01-09T06:47:57","date_gmt":"2022-01-08T22:47:57","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=231759"},"modified":"2022-01-08T20:26:37","modified_gmt":"2022-01-08T12:26:37","slug":"%e4%bf%9e%e4%b9%a6%e5%ae%8f%e9%99%a2%e5%a3%ab%e5%9b%a2%e9%98%9f2021%e5%b9%b4%e5%b7%a5%e4%bd%9c%e9%9b%86%e9%94%a6","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=231759","title":{"rendered":"\u4fde\u4e66\u5b8f\u9662\u58eb\u56e2\u961f2021\u5e74\u5de5\u4f5c\u96c6\u9526"},"content":{"rendered":"<p>\u4eca\u5929\u5411\u5927\u5bb6\u6c47\u603b\u4fde\u4e66\u5b8f\u9662\u58eb\u56e2\u961f2021\u5e74\u4e00\u4e9b\u5de5\u4f5c\uff0c\u4e00\u517117\u7bc7\u3002<\/p>\n<p><strong>Nat. Commun.<\/strong><strong>\uff1a\u901a\u8fc7\u8fd1\u7ea2\u5916\u6d3b\u6027\u6676\u683c\u5339\u914d\u5f62\u6001\u5f02\u8d28\u7ed3\u63d0\u9ad8\u5149\u7535\u5316\u5b66\u6548\u7387<\/strong><\/p>\n<p>\u5149\u7535\u50ac\u5316\u662f\u4e00\u79cd\u4ece\u592a\u9633\u80fd\u76f4\u63a5\u5236\u6c22\u7684\u6709\u5438\u5f15\u529b\u7684\u65b9\u6cd5\u3002\u7136\u800c\uff0c\u4e0e\u53ef\u89c1\u5149\u548c\u7d2b\u5916\u7ebf\u533a\u57df\u76f8\u6bd4\uff0c\u8fd1\u7ea2\u5916\u533a\u57df\u7684\u5149\u6536\u96c6\u6548\u7387\u6709\u9650\u3002\u5728\u8fd9\u91cc\uff0c\u4f5c\u8005\u4ecb\u7ecd\u4e86\u4e00\u79cd\u5177\u6709\u6676\u683c\u5339\u914d\u5f62\u6001\u7684\u5f02\u8d28\u7eb3\u7c73\u7ed3\u6784\u7684\u8fd1\u7ea2\u5916\u6d3b\u6027\u5149\u9633\u6781\u3002\u8fd9\u662f\u4e00\u79cd\u901a\u8fc7\u540c\u65f6\u589e\u52a0\u5149\u6355\u83b7\u5149\u8c31\u8303\u56f4\u548c\u7535\u8377\u5206\u79bb\u6548\u7387\u6765\u63d0\u9ad8\u80fd\u91cf\u8f6c\u6362\u6548\u7387\u7684\u7b56\u7565\u3002\u5177\u4f53\u800c\u8a00\uff0c\u4f5c\u8005\u8bbe\u8ba1\u4e86\u7531BiSeTe\u4e09\u5143\u5408\u91d1\u7eb3\u7c73\u7ba1\u548c\u8d85\u8584\u7eb3\u7c73\u7247\u7ec4\u6210\u7684\u8fd1\u7ea2\u5916\u6d3b\u6027\u5f62\u6001\u5f02\u8d28\u7ed3\uff0c\u5f02\u8d28\u7ed3\u7684\u5206\u5c42\u7eb3\u7c73\u7ed3\u6784\u5c06\u4e24\u79cd\u5f62\u6001\u6210\u5206\u7684\u6676\u683c\u5339\u914d\u754c\u9762\u5904\u7684\u7535\u8377\u5206\u5f00\uff0c\u9632\u6b62\u8fdb\u4e00\u6b65\u7684\u8f7d\u6d41\u5b50\u590d\u5408\u3002\u7ed3\u679c\uff0c\u5728\u4e0d\u542b\u52a9\u50ac\u5316\u5242\u7684\u542b\u7a7a\u7a74\u6e05\u9664\u5242\u7684\u7535\u89e3\u8d28\u6eb6\u6db2\u4e2d\uff0c\u5149\u7535\u9633\u6781\u5728800 nm \u5904\u5b9e\u73b0\u4e8636%\u7684\u5165\u5c04\u5149\u5b50\u5230\u7535\u6d41\u8f6c\u6362\u6548\u7387\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cBoosting photoelectrochemical efficiency by near-infrared-active lattice-matched morphological heterojunctions\u201d \u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728Nat. Commun.\u4e0a\u3002DOI: 10.1038\/s41467-021-24569-9<\/p>\n<p>\u56fe1 \u5149\u8c31\u8868\u5f81\u548c\u80fd\u5e26\u793a\u610f\u56fe<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/1-4.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231763\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/1-4.jpg\" alt=\"\" width=\"600\" height=\"557\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/1-4.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/1-4-300x279.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p><strong>Nat. Commun.<\/strong><strong>\uff1a\u4e00\u79cd\u591a\u54cd\u5e94\u53ef\u4fee\u590d\u8d85\u7ea7\u7535\u5bb9\u5668<\/strong><\/p>\n<p>\u81ea\u4fee\u590d\u5bf9\u4e8e\u63d0\u9ad8\u8d85\u7ea7\u7535\u5bb9\u5668\u7684\u53ef\u9760\u6027\u548c\u4f7f\u7528\u5bff\u547d\u81f3\u5173\u91cd\u8981\u3002\u7136\u800c\uff0c\u7f3a\u4e4f\u901a\u7528\u7684\u81ea\u4fee\u590d\u673a\u5236\u5bfc\u81f4\u4f4e\u7535\u5bb9\u6027\u80fd\u548c\u4e0d\u4ee4\u4eba\u6ee1\u610f\u7684\u81ea\u4fee\u590d\u6548\u679c\u3002\u5728\u8fd9\u91cc\uff0c\u4f5c\u8005\u5c55\u793a\u4e86\u4e00\u79cd\u5177\u6709\u96c6\u6210\u914d\u7f6e\u7684\u591a\u54cd\u5e94\u53ef\u4fee\u590d\u8d85\u7ea7\u7535\u5bb9\u5668\uff0c\u7531\u78c1\u6027Fe<sub>3<\/sub>O<sub>4<\/sub>@Au\/\u805a\u4e19\u70ef\u9170\u80fa (MFP) \u6c34\u51dd\u80f6\u57fa\u7535\u6781\u548c\u7535\u89e3\u8d28\u4ee5\u53ca\u4f5c\u4e3a\u96c6\u6d41\u4f53\u7684Ag\u7eb3\u7c73\u7ebf\u8584\u819c\u7ec4\u88c5\u800c\u6210\u3002\u9664\u4e86\u9ad8\u673a\u68b0\u5f3a\u5ea6\u5916\uff0cMFP\u6c34\u51dd\u80f6\u8fd8\u8868\u73b0\u51fa\u7531\u4e0d\u540c\u7684\u5149\u70ed\u548c\u78c1\u70ed\u89e6\u53d1\u754c\u9762\u91cd\u6784\u4ea7\u751f\u7684\u5feb\u901f\u5149\u5b66\u548c\u78c1\u4fee\u590d\u7279\u6027\u3002\u901a\u8fc7\u5c06\u7535\u6d3b\u6027\u805a\u5421\u54af\u7eb3\u7c73\u7c92\u5b50\u4f5c\u4e3a\u7535\u6781\u751f\u957f\u5230MFP\u6846\u67b6\u4e2d\uff0c\u7ec4\u88c5\u7684\u8d85\u7ea7\u7535\u5bb9\u5668\u5728\u5149\u3001\u7535\u548c\u78c1\u523a\u6fc0\u4e0b\u8868\u73b0\u51fa\u4e09\u91cd\u54cd\u5e94\u7684\u4fee\u590d\u6027\u80fd\u3002\u503c\u5f97\u6ce8\u610f\u7684\u662f\uff0c\u8be5\u5668\u4ef6\u5728\u62a5\u9053\u7684\u53ef\u4fee\u590d\u8d85\u7ea7\u7535\u5bb9\u5668\u4e2d\u63d0\u4f9b\u4e861264 mF cm<sup>-2<\/sup>\u7684\u6700\u9ad8\u9762\u7535\u5bb9\uff0c\u5e76\u5728\u5341\u4e2a\u4fee\u590d\u5468\u671f\u5185\u6062\u590d\u4e86\u7ea690%\u7684\u521d\u59cb\u7535\u5bb9\u3002\u8fd9\u4e9b\u7a81\u51fa\u7684\u6027\u80fd\u4f18\u52bf\u4ee5\u53ca\u7b80\u4fbf\u7684\u5668\u4ef6\u7ec4\u88c5\u65b9\u6cd5\u4f7f\u8fd9\u79cd\u65b0\u5174\u7684\u8d85\u7ea7\u7535\u5bb9\u5668\u5728\u4e0b\u4e00\u4ee3\u7535\u5b50\u4ea7\u54c1\u4e2d\u5177\u6709\u5de8\u5927\u7684\u6f5c\u529b\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cA multi-responsive healable supercapacitor\u201d \u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728Nat. Commun.\u4e0a\u3002DOI: 10.1038\/s41467-021-24568-w<\/p>\n<p>\u56fe2\u53ef\u81ea\u4fee\u590d\u8d85\u7ea7\u7535\u5bb9\u5668\u8bbe\u5907\u7684\u7ec4\u88c5<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/2-3.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231764\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/2-3.jpg\" alt=\"\" width=\"600\" height=\"571\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/2-3.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/2-3-300x286.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p><strong>Chem. Soc. Rev.<\/strong><strong>\uff1a\u8f6f\u5316\u5b66\u8c03\u63a7\u4e9a\u7a33\u6001\u91d1\u5c5e\u786b\u65cf\u5316\u5408\u7269\u7eb3\u7c73\u7ed3\u6784<\/strong><\/p>\n<p>\u5728\u8be5\u7bc7\u7efc\u8ff0\u4e2d\uff0c\u4f5c\u8005\u8be6\u7ec6\u5206\u6790\u4e86\u91d1\u5c5e\u786b\u65cf\u5316\u5408\u7269\u7eb3\u7c73\u7ed3\u6784\u4e9a\u7a33\u7279\u6027\u7684\u5177\u4f53\u8868\u73b0\u5f62\u5f0f\uff0c\u5982\u79bb\u5b50\u7684\u8fc1\u79fb\u548c\u7a7a\u4f4d\u3001\u70ed\u4e0d\u7a33\u5b9a\u6027\u548c\u7ed3\u6784\u4e0d\u7a33\u5b9a\u6027\u3001\u5316\u5b66\u53cd\u5e94\u6d3b\u6027\u548c\u6676\u76f8\u8f6c\u53d8\uff0c\u4ee5\u53ca\u57fa\u4e8e\u4ee5\u4e0a\u7279\u5f81\u8bbe\u8ba1\u76f8\u5e94\u7684\u201c\u8f6f\u5316\u5b66\u53cd\u5e94\u201d\u8def\u5f84\uff0c\u5305\u62ec\u79bb\u5b50\u4ea4\u6362\u3001\u50ac\u5316\u751f\u957f\u3001\u5206\u79bb\u6216\u8026\u5408\u3001\u6a21\u677f\u5ac1\u63a5\u6216\u5316\u5b66\u8f6c\u5316\u53ca\u6676\u76f8\u7684\u7a33\u5b9a\u6216\u6784\u5efa\u3002\u4f5c\u8005\u91cd\u70b9\u4ecb\u7ecd\u4e86\u5229\u7528\u4ee5\u4e0a\u8bbe\u8ba1\u539f\u5219\u548c\u8f6c\u5316\u89c4\u5f8b\u5bf9\u4e9a\u7a33\u6001\u91d1\u5c5e\u786b\u65cf\u5316\u5408\u7269\u7eb3\u7c73\u7ed3\u6784\u8fdb\u884c\u5408\u6210\u3001\u4fee\u9970\u548c\u529f\u80fd\u5316\u7684\u6700\u65b0\u8fdb\u5c55\u3002\u6700\u540e\uff0c\u4f5c\u8005\u5bf9\u4e9a\u7a33\u6001\u91d1\u5c5e\u786b\u65cf\u5316\u5408\u7269\u7eb3\u7c73\u7ed3\u6784\u201c\u8f6f\u5316\u5b66\u201d\u8c03\u63a7\u7814\u7a76\u7684\u672a\u6765\u53d1\u5c55\u8fdb\u884c\u4e86\u5c55\u671b\uff0c\u5e76\u63d0\u51fa\u4e86\u5bf9\u8fd9\u4e2a\u9886\u57df\u4e3b\u8981\u5b58\u5728\u7684\u673a\u9047\u53ca\u6311\u6218\u7684\u4e2a\u4eba\u89c1\u89e3\u3002\u76f8\u5173\u7efc\u8ff0\u4ee5\u201cSoft chemistry of metastable metal chalcogenide nanomaterials\u201d \u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728Chem. Soc. Rev.\u4e0a\u3002DOI: 10.1039\/d0cs00881h<\/p>\n<p>\u56fe3 \u5168\u6587\u6982\u8981\u56fe<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/3-4.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231765\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/3-4.jpg\" alt=\"\" width=\"396\" height=\"396\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/3-4.jpg 396w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/3-4-150x150.jpg 150w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/3-4-300x300.jpg 300w\" sizes=\"(max-width: 396px) 100vw, 396px\" \/><\/a><\/p>\n<p><strong>J. Am. Chem. Soc.<\/strong><strong>\uff1a<\/strong><strong>3D<\/strong><strong>\u6709\u5e8f\u901a\u9053\u4e2d\u7684\u5fae\u5316\u5b66\u5de5\u7a0b\u589e\u5f3a\u7535\u50ac\u5316<\/strong><\/p>\n<p>\u5305\u62ec\u4f20\u8d28\u548c\u8868\u9762\u53cd\u5e94\u5728\u5185\u7684\u7535\u6781\u53cd\u5e94\u52a8\u529b\u5b66\u5728\u7535\u50ac\u5316\u4e2d\u662f\u5fc5\u4e0d\u53ef\u5c11\u7684\uff0c\u56e0\u4e3a\u5b83\u51b3\u5b9a\u4e86\u8868\u89c2\u53cd\u5e94\u901f\u7387\uff0c\u5c24\u5176\u662f\u5728\u7eb3\u7c73\u7ed3\u6784\u7535\u50ac\u5316\u5242\u4e0a\u3002\u7136\u800c\uff0c\u5728\u4f18\u5316\u5177\u6709\u5408\u9002\u6210\u5206\u3001\u5f62\u6001\u548c\u6676\u4f53\u8bbe\u8ba1\u7684\u7ed9\u5b9a\u50ac\u5316\u5242\u7684\u52a8\u529b\u5b66\u4ee5\u6700\u5927\u5316\u7535\u50ac\u5316\u6027\u80fd\u65b9\u9762\u4ecd\u7136\u5b58\u5728\u91cd\u8981\u6311\u6218\u3002\u4f5c\u8005\u8fd9\u91cc\u63d0\u51fa\u4e86\u4e00\u79cd\u5728\u7eb3\u7c73\u50ac\u5316\u5242\u4fee\u9970\u7684\u7535\u6781\u8868\u9762\u4e0a\u8026\u5408\u4f20\u8d28\u548c\u8868\u9762\u53cd\u5e94\u7684\u7efc\u5408\u52a8\u529b\u5b66\u6a21\u578b\uff0c\u4ee5\u63a2\u7d22\u548c\u9610\u660e\u7535\u50ac\u5316\u7684\u52a8\u529b\u5b66\u4f18\u5316\u3002\u6b64\u5916\uff0c\u7406\u8bba\u6307\u5bfc\u7684\u5fae\u5316\u5b66\u5de5\u7a0b\uff08MCE\uff09\u7b56\u7565\u5df2\u88ab\u8bc1\u660e\u53ef\u4ee5\u5408\u7406\u5730\u91cd\u65b0\u8bbe\u8ba1\u5177\u6709\u4f18\u5316\u52a8\u529b\u5b66\u7684\u50ac\u5316\u5242\u3002\u5177\u6709\u53ef\u8c03\u901a\u9053\u5c3a\u5bf8\u76843D\u6709\u5e8f\u901a\u9053\u4e2d\u7532\u9187\u6c27\u5316\u53cd\u5e94\u7684\u5b9e\u9a8c\u6d4b\u91cf\u8bc1\u5b9e\u4e86\u8ba1\u7b97\u9884\u6d4b\u3002\u5728\u4f18\u5316\u7684\u901a\u9053\u5c3a\u5bf8\u4e0b\uff0c\u901a\u9053\u5fae\u53cd\u5e94\u5668\u4e2d\u7684\u4f20\u8d28\u548c\u8868\u9762\u53cd\u5e94\u90fd\u5f97\u5230\u4e86\u5f88\u597d\u7684\u8c03\u8282\u3002\u8fd9\u79cdMCE\u7b56\u7565\u5c06\u5728\u7ed3\u6784\u5316\u50ac\u5316\u5242\u8bbe\u8ba1\u548c\u52a8\u529b\u5b66\u8c03\u8282\u65b9\u9762\u5e26\u6765\u91cd\u5927\u98de\u8dc3\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cMicrochemical Engineering in a 3D Ordered Channel Enhances Electrocatalysis\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728J. Am. Chem. Soc.\u4e0a\u3002DOI: 10.1021\/jacs.1c04653<\/p>\n<p>\u56fe4\u4ece\u5de5\u4e1a\u89c4\u6a21\u5230\u5fae\u89c2\u89c4\u6a21\u7684\u5206\u5c42\u6784\u9020\u5316\u5b66\u5de5\u7a0b\u7684\u793a\u610f\u56fe<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/4-2.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231766\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/4-2.png\" alt=\"\" width=\"554\" height=\"343\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/4-2.png 554w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/4-2-300x186.png 300w\" sizes=\"(max-width: 554px) 100vw, 554px\" \/><\/a><\/p>\n<p><strong>J.Am. Chem. Soc.<\/strong><strong>\uff1a\u4e00\u7ef4\u8d85\u6676\u683c\u5f02\u8d28\u7ed3\u6784\u5e93<\/strong><\/p>\n<p>\u5728\u8f74\u5411\u4e0a\uff0c\u5c06\u4e0d\u540c\u6210\u5206\u548c\u7ed3\u6784\u7684\u7eb3\u7c73\u7269\u4f53\u5916\u5ef6\u7ec4\u7ec7\u6210\u8d85\u6676\u683c\u7eb3\u7c73\u7ebf\uff0c\u53ef\u4ee5\u5145\u5206\u5229\u7528\u9633\u5149\u3001\u6613\u4e8e\u8bbe\u8ba1\u7684\u80fd\u5e26\u7ed3\u6784\u548c\u53ef\u8c03\u51e0\u4f55\u53c2\u6570\u6765\u9002\u5e94\u8f7d\u6d41\u5b50\u4f20\u8f93\uff0c\u4ece\u800c\u4e3a\u5149\u7535\u5b50\u5b66\u548c\u592a\u9633\u80fd\u5230\u71c3\u6599\u7684\u8f6c\u6362\u5e26\u6765\u5e7f\u9614\u524d\u666f\u3002\u4e3a\u4e86\u6700\u5927\u9650\u5ea6\u5730\u63d0\u9ad8\u5b83\u4eec\u7684\u6548\u7387\uff0c\u5177\u6709\u53ef\u7f16\u7a0b\u6210\u5206\u548c\u7ed3\u6784\u7684\u80f6\u4f53\u8f74\u5411\u8d85\u6676\u683c\u7eb3\u7c73\u7ebf\uff08ASLNWs\uff09\u7684\u901a\u7528\u548c\u9ad8\u7cbe\u5ea6\u5408\u6210\u662f\u5148\u51b3\u6761\u4ef6\u3002\u7136\u800c\uff0c\u4ecd\u7136\u5177\u6709\u6311\u6218\u6027\u3002\u5728\u8fd9\u91cc\uff0c\u4f5c\u8005\u5411ASLNW\u5e93\u62a5\u9053\u4e86\u4e00\u79cd\u8f74\u5411\u7f16\u7801\u65b9\u6cd5\uff0c\u53ef\u4ee5\u7cbe\u786e\u63a7\u5236\u5b83\u4eec\u7684\u6210\u5206\u3001\u5c3a\u5bf8\u3001\u6676\u76f8\u3001\u754c\u9762\u548c\u5468\u671f\u6027\u3002\u4f7f\u7528\u63d0\u4f9b\u5408\u6210\u9009\u62e9\u6027\u7684\u9884\u5148\u8bbe\u8ba1\u7684\u3001\u53ef\u7f16\u8f91\u7684\u7eb3\u7c73\u7c92\u5b50\u6846\u67b6\uff0c\u4f5c\u8005\u80fd\u591f\u5316\u5b66\u89e3\u8026ASLNW\u4e2d\u7684\u76f8\u90bb\u5b50\u5bf9\u8c61\uff0c\u4ece\u800c\u4ee5\u53d7\u63a7\u65b9\u6cd5\u5236\u4f5c\u5b83\u4eec\uff0c\u4ea7\u751f\u4e0d\u540c\u7684ASLNW\u5e93\u3002\u4f5c\u8005\u5728\u5176\u4e2d\u96c6\u6210\u4e86\u7b49\u79bb\u5b50\u4f53\u3001\u91d1\u5c5e\u6216\u8fd1\u7ea2\u5916\u6d3b\u6027\u786b\u5c5e\u5143\u7d20\u5316\u7269\uff0c\u5b83\u4eec\u5728\u592a\u9633\u80fd\u8f6c\u6362\u65b9\u9762\u5177\u6709\u5de8\u5927\u6f5c\u529b\u3002\u8fd9\u79cd\u5408\u6210\u80fd\u529b\u53ef\u4ee5\u63d0\u9ad8\u76ee\u6807\u5e94\u7528\u7684\u6027\u80fd\uff0c\u4f5c\u8005\u62a5\u9053\u4e86\u4e0e\u76f8\u5e94\u7684\u5355\u72ec\u7269\u4f53\u76f8\u6bd4\uff0c\u4f7f\u7528\u4f18\u5316\u7684ASLNW\u63d0\u5347\u4e86\u6570\u91cf\u7ea7\u7684\u5149\u50ac\u5316\u5236\u6c22\u901f\u7387\u3002\u6b64\u5916\uff0c\u8fd9\u79cd\u72ec\u7279\u7684\u8d85\u6676\u683c\u7eb3\u7c73\u7ebf\u6709\u671b\u5e26\u6765\u65b0\u7684\u73b0\u8c61\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cOne-Dimensional Superlattice Heterostructure Library\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728J. Am. Chem. Soc.\u4e0a\u3002DOI: 10.1021\/jacs.1c01514<\/p>\n<p>\u56fe5\u4e00\u7ef4\u5f02\u8d28\u7ed3\u6784\u4f53\u7cfb\u7ed3\u6784<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/5-4.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231767\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/5-4.jpg\" alt=\"\" width=\"500\" height=\"500\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/5-4.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/5-4-150x150.jpg 150w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/5-4-300x300.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/a><\/p>\n<p><strong>Angew<\/strong><strong>\uff1a\u5927\u9762\u79ef\u7ed3\u6676\u6cb8\u77f3\u54aa\u5511\u9aa8\u67b6\u8584\u819c<\/strong><\/p>\n<p>\u4f5c\u8005\u62a5\u9053\u4e86\u5177\u6709\u9ad8\u5ea6\u53ef\u63a7\u7684\u539a\u5ea6\uff08\u4ece44\u52305100 nm\uff09\u7684\u8fde\u7eedMOF\u8584\u819c\u53ef\u4ee5\u901a\u8fc7\u4e00\u79cd\u7b80\u4fbf\u3001\u5feb\u901f\u4e14\u5177\u6709\u6210\u672c\u6548\u76ca\u7684\u55b7\u6d82\u65b9\u6cd5\u6c89\u79ef\u5728\u8d85\u8fc780\u5398\u7c73\u7684\u957f\u5ea6\u5c3a\u5ea6\u4e0a\u3002\u8fd9\u79cd\u6210\u529f\u4f9d\u8d56\u4e8e\u4f5c\u8005\u53d1\u73b0\u4e86\u524d\u6240\u672a\u6709\u7684\u7531\u65e0\u5b9a\u5f62 MOF \u7eb3\u7c73\u9897\u7c92\u7ec4\u6210\u7684\u5b8c\u7f8e\u5206\u6563\u7684\u80f6\u4f53\u6eb6\u6db2\uff0c\u4f5c\u8005\u5c06\u5176\u7528\u4f5c\u524d\u9a71\u4f53\uff0c\u5728\u4f4e\u6e29\u539f\u4f4d\u52a0\u70ed\u65f6\u5f88\u5bb9\u6613\u8f6c\u5316\u4e3a\u7ed3\u6676\u8584\u819c\u3002\u80f6\u4f53\u6eb6\u6db2\u5141\u8bb8\u5728\u5927\u91cf\u57fa\u6750\u4e0a\u5236\u9020\u81f4\u5bc6\u4e14\u5747\u5300\u7684MOF\u8584\u819c\uff0c\u4f8b\u5982\u63ba\u6c1f\u6c27\u5316\u9521\u3001\u73bb\u7483\u3001SiO<sub>2<\/sub>\u3001Al<sub>2<\/sub>O<sub>3<\/sub>\u3001Si\u3001Cu\uff0c\u751a\u81f3\u67d4\u6027\u805a\u78b3\u9178\u916f\uff0c\u62d3\u5bbd\u4e86\u5b83\u4eec\u5728\u57fa\u6750\u5fc5\u4e0d\u53ef\u5c11\u7684\u6280\u672f\u5e94\u7528\uff0c\u5c3d\u7ba1\u76ee\u524d\u7684\u5de5\u4f5c\u91cd\u70b9\u662f\u5236\u5907\u5747\u5300\u7684ZIF\u8584\u819c\uff0c\u4f46\u8be5\u53d1\u73b0\u6807\u5fd7\u7740\u5927\u89c4\u6a21\u751f\u4ea7\u5176\u4ed6\u9ad8\u8d28\u91cfMOF\u8584\u819c\u7684\u53ef\u80fd\u6027\u5f88\u5927\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cLarge-area crystalline zeolitic imidazolate framework thin films\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728Angew\u4e0a\u3002DOI: 10.1002\/anie.202104366<\/p>\n<p>\u56fe6 \u5236\u5907\u4e0e\u8868\u5f81<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/6-1.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231768\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/6-1.jpg\" alt=\"\" width=\"554\" height=\"374\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/6-1.jpg 554w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/6-1-300x203.jpg 300w\" sizes=\"(max-width: 554px) 100vw, 554px\" \/><\/a><\/p>\n<p>AM\uff1a\u7528\u4e8e\u667a\u80fd\u632f\u52a8\u548c\u78c1\u6027\u4f20\u611f\u5668\u7684\u9ad8\u5ea6\u53ef\u538b\u7f29\u548c\u53ef\u62c9\u4f38\u7684\u78b3\u5f39\u7c27<\/p>\n<p>\u8fd9\u91cc\uff0c\u4f5c\u8005\u5f15\u5165\u72ec\u7279\u7684\u957f\u7a0b\u5c42\u72b6\u591a\u62f1\u5fae\u7ed3\u6784\uff0c\u53ef\u4ee5\u5728-80%\u523080%\u7684\u5927\u5e94\u53d8\u4e0b\u540c\u65f6\u5b9e\u73b0\u5f39\u6027\u538b\u7f29\u6027\u548c\u62c9\u4f38\u6027\u7684\u591a\u5b54\u5168\u78b3\u6750\u6599\u3002\u4ee4\u4eba\u5370\u8c61\u6df1\u523b\u7684\u662f\uff0c\u591a\u5b54\u5168\u78b3\u6750\u6599\u5728\u5faa\u73af\u538b\u7f29-\u62c9\u4f38\u8fc7\u7a0b\u7684\u52a0\u8f7d\u6761\u4ef6\u4e0b\u53ef\u4ee5\u4fdd\u6301\u53ef\u9760\u7684\u7ed3\u6784\u575a\u56fa\u6027\u548c\u8010\u4e45\u6027\uff0c\u7c7b\u4f3c\u4e8e\u771f\u6b63\u7684\u91d1\u5c5e\u5f39\u7c27\u3002\u72ec\u7279\u7684\u6027\u80fd\u4f7f\u5176\u6210\u4e3a\u5236\u9020\u667a\u80fd\u632f\u52a8\u548c\u78c1\u6027\u4f20\u611f\u5668\u7684\u6709\u524d\u9014\u7684\u5e73\u53f0\uff0c\u751a\u81f3\u80fd\u591f\u5728\u6781\u7aef\u6e29\u5ea6\u4e0b\u8fd0\u884c\u3002\u6b64\u5916\uff0c\u8fd9\u9879\u7814\u7a76\u4e3a\u4ece\u5176\u4ed6\u7eaf\u65e0\u673a\u6210\u5206\u4e2d\u521b\u9020\u9ad8\u5ea6\u53ef\u62c9\u4f38\u548c\u53ef\u538b\u7f29\u7684\u591a\u5b54\u6750\u6599\u63d0\u4f9b\u4e86\u5b9d\u8d35\u7684\u89c1\u89e3\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cA Highly Compressible and Stretchable Carbon Spring for Smart Vibration and Magnetism Sensors\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728AM\u4e0a\u3002DOI: 10.1002\/adma.202102724<\/p>\n<p>\u56fe7 \u5236\u5907\u3001\u7ed3\u6784\u4e0e\u529b\u5b66\u8868\u5f81<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/7.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231769\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/7.jpg\" alt=\"\" width=\"554\" height=\"401\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/7.jpg 554w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/7-300x217.jpg 300w\" sizes=\"(max-width: 554px) 100vw, 554px\" \/><\/a><\/p>\n<p>AM\uff1a\u4e00\u79cd\u7528\u4e8e\u8fde\u7eed\u56de\u6536\u7c98\u6027\u539f\u6cb9\u7684\u78c1\u52a0\u70ed\u4e9a\u94c1\u78c1\u6d77\u7ef5<\/p>\n<p>\u4e3a\u4e86\u5f00\u53d1\u7c98\u6027\u539f\u6cb9\u7684\u975e\u63a5\u89e6\u5f0f\u56de\u6536\uff0c\u8fd9\u91cc\u4f5c\u8005\u62a5\u9053\u4e86\u4e00\u79cd\u5236\u9020\u4e00\u7cfb\u5217\u5177\u6709\u758f\u6c34\u6027\u591a\u5b54\u901a\u9053\u7684\u4e9a\u94c1\u78c1\u6d77\u7ef5 (FMS) \u7684\u65b0\u65b9\u6cd5\u3002\u5728\u4ea4\u53d8\u78c1\u573a\u4e2d\uff08f = 274 kHz\uff0cH = 30 kA m<sup>-1<\/sup>\uff09\uff0c\u5176\u8868\u9762\u53ef\u4ee5\u572810\u79d2\u5185\u8fdc\u7a0b\u52a0\u70ed\u5230 120\u00b0C\u3002\u7531\u4e8e\u591a\u5b54\u901a\u9053\u4e2d\u7684\u70ed\u4f20\u9012\u53d7\u5230\u9650\u5236\uff0cFMS\u4e2d\u7684\u6574\u4f53\u78c1\u52a0\u70ed\u4f1a\u5bfc\u81f4\u6d77\u7ef5\u7684\u5185\u90e8\u6e29\u5ea6\u5347\u9ad8\uff0c\u8fd9\u6709\u52a9\u4e8e\u6cb9\u7c98\u5ea6\u6025\u5267\u964d\u4f4e\uff0c\u5e76\u663e\u8457\u589e\u52a0\u6d41\u5165FMS\u5b54\u9699\u7684\u6cb9\u3002\u6b64\u5916\uff0c\u4e0e\u81ea\u5438\u6cf5\u7ec4\u88c5\u5728\u4e00\u8d77\u7684FMS\u53ef\u4ee5\u901a\u8fc7\u8fdc\u7a0b\u78c1\u52a0\u70ed\u5b9e\u73b0\u7c98\u6027\u539f\u6cb9\uff0833.05 g h<sup>-1<\/sup> cm<sup>-2<\/sup>\uff09\u7684\u8fde\u7eed\u56de\u6536\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cA Magneto-Heated Ferrimagnetic Sponge for Continuous Recovery of Viscous Crude Oil\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728AM\u4e0a\u3002DOI: 10.1002\/adma.202100074<\/p>\n<p>\u56fe8 \u4e9a\u94c1\u78c1\u6d77\u7ef5\u56de\u6536\u539f\u6cb9\u793a\u610f\u56fe<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/8.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231770\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/8.jpg\" alt=\"\" width=\"554\" height=\"324\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/8.jpg 554w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/8-300x175.jpg 300w\" sizes=\"(max-width: 554px) 100vw, 554px\" \/><\/a><\/p>\n<p><strong>AM<\/strong><strong>\uff1a\u65b0\u5174\u4eff\u751f\u4eba\u9020\u6728\u6750<\/strong><\/p>\n<p>\u5728\u672c\u6587\u4e2d\uff0c\u4f5c\u8005\u4ece\u8bbe\u8ba1\u6982\u5ff5\u3001\u5236\u9020\u7b56\u7565\u3001\u6027\u80fd\u548c\u53ef\u80fd\u7684\u5e94\u7528\u7b49\u65b9\u9762\u5bf9\u4e8e\u4eff\u751f\u4eba\u9020\u6728\u6750\u8fdb\u884c\u4e86\u8ba8\u8bba\u3002\u76ee\u524d\u7684\u6311\u6218\u548c\u8fdb\u4e00\u6b65\u7684\u7814\u7a76\u673a\u9047\u4e5f\u4e3a\u4eba\u9020\u6728\u6750\u7684\u84ec\u52c3\u53d1\u5c55\u63d0\u4f9b\u4e86\u673a\u4f1a\u3002\u4e3a\u4e86\u5b9e\u73b0\u6700\u7ec8\u7684\u751f\u6001\u53cb\u597d\u578b\u4eba\u9020\u6728\u6750\uff0c\u5e94\u5728\u751f\u7269\u6750\u6599\u548c\u805a\u5408\u7269\u7684\u53ef\u751f\u7269\u964d\u89e3\u6216\u53ef\u56de\u6536\u5de5\u7a0b\u65b9\u9762\u505a\u51fa\u66f4\u591a\u52aa\u529b\uff0c\u6765\u540c\u65f6\u83b7\u5f97\u9ad8\u673a\u68b0\u6027\u80fd\u548c\u73af\u5883\u53ef\u6301\u7eed\u6027\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cEmerging Bioinspired Artificial Woods\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728AM\u4e0a\u3002DOI: 10.1002\/adma.202001086<\/p>\n<p>\u56fe9 \u4eba\u9020\u6728\u6750\u8bbe\u8ba1\u7684\u57fa\u672c\u539f\u5219<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/9.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231771\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/9.jpg\" alt=\"\" width=\"554\" height=\"311\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/9.jpg 554w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/9-300x168.jpg 300w\" sizes=\"(max-width: 554px) 100vw, 554px\" \/><\/a><\/p>\n<p><strong>AM<\/strong><strong>\uff1a\u78b1\u6027\u6c34\u5206\u89e3\u7684\u7814\u7a76\u8fdb\u5c55<\/strong><\/p>\n<p>\u5728\u8fd9\u91cc\uff0c\u4f5c\u8005\u6982\u8ff0\u4e86\u6c34\u7535\u89e3\u7684\u5386\u53f2\u53d1\u5c55\uff0c\u5e76\u8ba8\u8bba\u4e86\u51e0\u4e2a\u5173\u952e\u7684\u7535\u5316\u5b66\u53c2\u6570\u3002\u4e4b\u540e\uff0c\u8ba8\u8bba\u4e86\u6700\u8fd1\u51fa\u73b0\u7684\u7528\u4e8e\u5904\u7406\u78b1\u6027\u6790\u6c27\u53cd\u5e94 (OER) \u548c\u6790\u6c22\u53cd\u5e94 (HER) \u7684\u5148\u8fdb\u975e\u8d35\u91d1\u5c5e\u7535\u50ac\u5316\u5242\uff0c\u7279\u522b\u5173\u6ce8\u50ac\u5316\u5242\u5408\u6210\u3001\u6d3b\u6027\u548c\u7a33\u5b9a\u6027\u6311\u6218\uff0c\u4ee5\u53ca\u6027\u80fd\u6539\u8fdb\u548c\u884c\u4e1a\u76f8\u5173\u53d1\u5c55\u3002\u6700\u8fd1\u4e00\u4e9b\u5173\u4e8e\u6309\u6bd4\u4f8b\u653e\u5927\u50ac\u5316\u5242\u5408\u6210\u3001\u65b0\u578b\u7535\u6781\u8bbe\u8ba1\u548c\u78b1\u6027\u6d77\u6c34\u7535\u89e3\u7684\u5de5\u4f5c\u4e5f\u53d7\u5230\u5173\u6ce8\u3002\u6700\u540e\uff0c\u5c55\u671b\u4e86\u78b1\u6027\u6c34\u5206\u89e3\u7684\u672a\u6765\u6311\u6218\u548c\u673a\u9047\uff0c\u5e76\u63a8\u6d4b\u4e86\u672a\u6765\u7684\u6f5c\u5728\u65b9\u5411\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cClean and Affordable Hydrogen Fuel from Alkaline Water Splitting: Past, Recent Progress, and Future Prospects\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728AM\u4e0a\u3002DOI: 10.1002\/adma.202007100<\/p>\n<p>\u56fe10 \u6c34\u5206\u89e3\u7684\u53d1\u5c55\u5386\u53f2<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/10.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231772\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/10.jpg\" alt=\"\" width=\"554\" height=\"222\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/10.jpg 554w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/10-300x120.jpg 300w\" sizes=\"(max-width: 554px) 100vw, 554px\" \/><\/a><\/p>\n<p><strong>AM<\/strong><strong>\uff1a\u53d7\u73cd\u73e0\u5c42\u542f\u53d1\u7684\u53cc\u5c42\u805a\u9170\u4e9a\u80fa<\/strong><strong>&#8211;<\/strong><strong>\u4e91\u6bcd\u7eb3\u7c73\u590d\u5408\u8584\u819c<\/strong><\/p>\n<p>\u805a\u9170\u4e9a\u80fa\uff08PI\uff09\u590d\u5408\u8584\u819c\u88ab\u5e7f\u6cdb\u5e94\u7528\u4e8e\u822a\u5929\u5668\u7684\u5916\u8868\u9762\uff0c\u4ee5\u4fdd\u62a4\u822a\u5929\u5668\u514d\u53d7\u4f4e\u5730\u7403\u8f68\u9053\uff08LEO\uff09\u7684\u4e0d\u5229\u6761\u4ef6\u7684\u5f71\u54cd\u3002\u7136\u800c\uff0c\u76ee\u524d\u7684PI\u590d\u5408\u8584\u819c\u7684\u673a\u68b0\u6027\u80fd\u548c\u6297\u539f\u5b50\u6c27 (AO) \u6027\u80fd\u4e0d\u8db3\u3002\u8be5\u5de5\u4f5c\u901a\u8fc7\u5c06\u4e91\u6bcd\u7eb3\u7c73\u7247\u4e0ePI\u96c6\u6210\u5230\u72ec\u7279\u7684\u53cc\u5c42\u73cd\u73e0\u5c42\u7ed3\u6784\u4e2d\uff0c\u5728\u9876\u5c42\u5177\u6709\u66f4\u9ad8\u5bc6\u5ea6\u7684\u4e91\u6bcd\u7eb3\u7c73\u7247\uff0c\u4ece\u800c\u5236\u9020\u51fa\u4e00\u79cd\u65b0\u7684\u57fa\u4e8ePI\u7684\u7eb3\u7c73\u590d\u5408\u8584\u819c\uff0c\u8be5\u8584\u819c\u5177\u6709\u5927\u5927\u589e\u5f3a\u7684\u673a\u68b0\u6027\u80fd\u548c\u6297\u6c27\u5316\u6027\u3002\u6b64\u5916\uff0c\u4e91\u6bcd\u72ec\u7279\u7684\u5fae\u89c2\u7ed3\u6784\u548c\u56fa\u6709\u7279\u6027\u4e5f\u8d4b\u4e88\u7eb3\u7c73\u590d\u5408\u8584\u819c\u826f\u597d\u7684\u6297\u7d2b\u5916\u7ebf\u548c\u8010\u9ad8\u6e29\u6027\u80fd\u3002\u8fd9\u79cd\u53cc\u5c42\u7eb3\u7c73\u590d\u5408\u8584\u819c\u4f5c\u4e3a\u7528\u4e8e\u4f4e\u5730\u7403\u8f68\u9053\u7684\u822a\u7a7a\u822a\u5929\u6750\u6599\u663e\u793a\u51fa\u5de8\u5927\u7684\u6f5c\u529b\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cDouble-Layer Nacre-Inspired Polyimide-Mica Nanocomposite Films with Excellent Mechanical Stability for LEO Environmental Conditions\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728AM\u4e0a\u3002DOI: 10.1002\/adma.202105299<\/p>\n<p>\u56fe11 \u6750\u6599\u5236\u5907\u4e0e\u8868\u5f81<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/11.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231774\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/11.jpg\" alt=\"\" width=\"554\" height=\"448\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/11.jpg 554w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/11-300x243.jpg 300w\" sizes=\"(max-width: 554px) 100vw, 554px\" \/><\/a><\/p>\n<p><strong>AM<\/strong><strong>\uff1a\u57fa\u4e8e\u6b8b\u4f59\u5e94\u529b\u8bf1\u5bfc\u7684\u5916\u5728\u589e\u97e7\u673a\u5236\u7684\u4eff\u751f\u9676\u74f7<\/strong><\/p>\n<p>\u9676\u74f7\u6750\u6599\u56fa\u6709\u7684\u8106\u6027\u662f\u5176\u4f5c\u4e3a\u627f\u91cd\u6750\u6599\u7684\u4e00\u4e2a\u91cd\u8981\u7f3a\u9677\u3002\u800c\u6dfb\u52a0\u8fc7\u91cf\u7684\u97e7\u6027\u6210\u5206\u5219\u4f1a\u5bfc\u81f4\u660e\u663e\u7684\u5f3a\u5ea6\u635f\u5931\u3002\u7814\u7a76\u53d1\u73b0\uff0c\u8f6f\u4f53\u52a8\u7269\u73cd\u73e0\u5c42\u5448\u73b0\u4e86\u7531\u53ef\u5ef6\u5c55\u7684\u751f\u7269\u805a\u5408\u7269\u7c98\u5408\u7684\u6613\u788e\u7684\u6587\u77f3\u7247\u6676\u7684\u5b9e\u4f53\u5fae\u89c2\u7ed3\u6784\u3002\u8fd9\u63d0\u4f9b\u4e86\u4e00\u79cd\u5f88\u597d\u7684\u7b56\u7565\uff0c\u53ef\u4ee5\u5728\u4e0d\u635f\u5931\u592a\u591a\u5f3a\u5ea6\u7684\u60c5\u51b5\u4e0b\u4ece\u5916\u90e8\u589e\u97e7\u9676\u74f7\u3002\u8fd9\u91cc\uff0c\u4f5c\u8005\u8bc1\u660e\u4e86\u5177\u6709\u9ad8\u65e0\u673a\u542b\u91cf\u7684\u4eba\u9020\u9676\u74f7\u7684\u65ad\u88c2\u97e7\u6027\u53ef\u4ee5\u901a\u8fc7\u6b8b\u4f59\u5e94\u529b\u8bf1\u5bfc\u7684\u7247\u6676\u5f3a\u5316\u6765\u63d0\u9ad8\uff0c\u8fd9\u53ef\u4ee5\u8bf1\u5bfc\u66f4\u6709\u6548\u7684\u5916\u5728\u589e\u97e7\u673a\u5236\uff0c\u8fd9\u4e9b\u673a\u5236\u7279\u5b9a\u4e8e\u73cd\u73e0\u5c42\u6a21\u62df\u7ed3\u6784\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cArtificial Nacre with High Toughness Amplification Factor: Residual Stress-Engineering Sparks Enhanced Extrinsic Toughening Mechanisms\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728AM\u4e0a\u3002DOI: 10.1002\/adma.202108267<\/p>\n<p>\u56fe12 \u6750\u6599\u7684\u591a\u5c3a\u5ea6\u7ed3\u6784<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/12.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231773\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/12.jpg\" alt=\"\" width=\"554\" height=\"289\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/12.jpg 554w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/12-300x156.jpg 300w\" sizes=\"(max-width: 554px) 100vw, 554px\" \/><\/a><\/p>\n<p><strong>AFM<\/strong><strong>\uff1a\u5177\u6709\u751f\u7269\u50ac\u5316\u5316\u7597\u548c\u539f\u4f4d\u5fae\u73af\u5883\u8c03\u8282\u7684\u751f\u7269\u652f\u67b6\u7528\u4e8e\u672f\u540e\u7ec4\u7ec7\u4fee\u590d<\/strong><\/p>\n<p>\u5177\u6709\u6297\u80bf\u7624\u548c\u7ec4\u7ec7\u4fee\u590d\u529f\u80fd\u7684\u65b0\u578b\u751f\u7269\u6750\u6599\u5bf9\u4e8e\u9ed1\u8272\u7d20\u7624\u624b\u672f\u7684\u672f\u540e\u62a4\u7406\u8d8a\u6765\u8d8a\u91cd\u8981\u3002\u4e3a\u6b64\uff0c\u4f5c\u8005\u8bbe\u8ba1\u4e86\u4e00\u79cd\u751f\u7269\u53ef\u5438\u6536\u590d\u5408\u652f\u67b6\uff0c\u8be5\u652f\u67b6\u662f\u901a\u8fc7\u9759\u7535\u7eba\u4e1d\u5c06\u6cbb\u7597\u6027\u65e0\u5b9a\u5f62\u78b3\u9178\u9499 (ACC) \u57fa\u7eb3\u7c73\u5236\u5242\u6c89\u79ef\u5728\u660e\u80f6\/\u805a\u5df1\u5185\u916f (GP) \u7eb3\u7c73\u7ea4\u7ef4\u4e2d\u5236\u6210\u7684\u3002ACC\u7eb3\u7c73\u5236\u5242\u4e0eFe<sup>2+<\/sup>\u9884\u6d3b\u5316\u7684\u535a\u6765\u9709\u7d20\u7ed3\u5408\u4ee5\u63d0\u4f9b\u751f\u7269\u50ac\u5316\u589e\u5f3a\u7684\u6cbb\u7597\u6548\u679c\uff0c\u800cACC\u53ef\u4f5c\u4e3a\u8d28\u5b50\u6e05\u9664\u5242\u539f\u4f4d\u6539\u5584\u80bf\u7624\u7ec4\u7ec7\u7684\u9178\u6027\uff0c\u4ece\u800c\u6301\u7eed\u6291\u5236\u80bf\u7624\u7684\u590d\u53d1\u548c\u8f6c\u79fb\u3002\u9178\u5f15\u53d1\u7684ACC\u5206\u89e3\u8fd8\u91ca\u653eCa<sup>2+<\/sup>\u6fc0\u6d3b\u4e0b\u6e38Wnt\/\u03b2-catenin\u4fe1\u53f7\u901a\u8def\uff0c\u53ef\u914d\u5408GP\u5e95\u7269\u7684\u6108\u5408\u4f5c\u7528\uff0c\u52a0\u901f\u4f24\u53e3\u518d\u751f\u3002\u7eb3\u7c73\u5de5\u7a0b\u652f\u67b6\u53ef\u7528\u4f5c\u9ed1\u8272\u7d20\u7624\u672f\u540e\u7ba1\u7406\u7684\u8865\u5145\u6cbb\u7597\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cBioresorbable Scaffolds with Biocatalytic Chemotherapy and In Situ Microenvironment Modulation for Postoperative Tissue Repair\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728AFM\u4e0a\u3002DOI: 10.1002\/adfm.202008732<\/p>\n<p>\u56fe13 \u652f\u67b6\u5236\u5907\u4e0e\u4f5c\u7528\u673a\u5236<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/13.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231775\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/13.jpg\" alt=\"\" width=\"554\" height=\"449\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/13.jpg 554w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/13-300x243.jpg 300w\" sizes=\"(max-width: 554px) 100vw, 554px\" \/><\/a><\/p>\n<p><strong>AFM<\/strong><strong>\uff1a\u7528\u4e8e\u8f6f\u7259\u9f88\u7ec4\u7ec7\u518d\u751f\u7684\u4eff\u751f\u5c42\u72b6\u58f3\u805a\u7cd6\u652f\u67b6<\/strong><\/p>\n<p>\u9ecf\u9f88\u624b\u672f\u5df2\u6210\u4e3a\u7259\u79d1\u4e34\u5e8a\u5b9e\u8df5\u4e2d\u8f6f\u7259\u9f88\u7ec4\u7ec7\u4fee\u590d\u7684\u5e38\u89c1\u624b\u672f\uff0c\u4e3b\u8981\u4f9d\u8d56\u4e8e\u81ea\u4f53\u79fb\u690d\u6216\u5546\u4e1a\u80f6\u539f\u819c\uff08CM\uff09\u3002\u7136\u800c\uff0c\u81ea\u4f53\u79fb\u690d\u7269\u5728\u6765\u6e90\u53ef\u7528\u6027\u548c\u957f\u671f\u672f\u540e\u75bc\u75db\u7ba1\u7406\u65b9\u9762\u9762\u4e34\u5de8\u5927\u6311\u6218\uff0c\u800cCM\u5728\u6c34\u6027\u73af\u5883\u4e2d\u53d7\u5230\u5176\u8f83\u5dee\u7684\u673a\u68b0\u6027\u80fd\u7684\u9650\u5236\u3002\u5728\u8fd9\u91cc\uff0c\u4f5c\u8005\u901a\u8fc7\u53cc\u5411\u51b7\u51bb\u65b9\u6cd5\u5236\u9020\u7684\u5177\u6709\u957f\u7a0b\u6709\u5e8f\u591a\u5b54\u7ed3\u6784\u7684\u4eff\u751f\u5c42\u72b6\u58f3\u805a\u7cd6\u652f\u67b6\uff08LCS\uff09\u4f5c\u4e3a\u4e00\u79cd\u6709\u524d\u9014\u7684\u7259\u9f88\u7ec4\u7ec7\u5de5\u7a0b\u6750\u6599\u3002 LCS\u4e0d\u4ec5\u5728\u6c34\u5408\u72b6\u6001\u4e0b\u8868\u73b0\u51fa\u4f18\u5f02\u7684\u673a\u68b0\u6027\u80fd\uff0c\u800c\u4e14\u5728\u4f53\u5185\u52a0\u901f\u8840\u7ba1\u5f62\u6210\u548c\u8f6f\u7ec4\u7ec7\u518d\u751f\u3002\u6700\u6709\u8da3\u7684\u662f\uff0c\u53d1\u73b0LCS\u80fd\u591f\u8bf1\u5bfc\u5de8\u566c\u7ec6\u80de\u5206\u5316\u4e3aM2\u5de8\u566c\u7ec6\u80de\uff0c\u8fd9\u88ab\u8ba4\u4e3a\u5728\u7ec4\u7ec7\u518d\u751f\u4e2d\u8d77\u91cd\u8981\u4f5c\u7528\u3002\u8fd9\u4e9b\u4f18\u52bf\u4e0e\u5176\u7b80\u5355\u4e14\u4f4e\u6210\u672c\u7684\u5236\u5907\u8fc7\u7a0b\u76f8\u7ed3\u5408\uff0c\u4f7fLCS\u6210\u4e3a\u7259\u79d1\u4e34\u5e8a\u5e94\u7528\u7684\u6709\u5e0c\u671b\u7684\u5019\u9009\u8005\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cBiomimetic Lamellar Chitosan Scaffold for Soft Gingival Tissue Regeneration\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728AFM\u4e0a\u3002DOI: 10.1002\/adfm.202105348<\/p>\n<p>\u56fe14 \u6750\u6599\u5236\u5907\u4e0e\u4f5c\u7528\u673a\u5236<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/14.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231776\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/14.jpg\" alt=\"\" width=\"554\" height=\"358\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/14.jpg 554w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/14-300x194.jpg 300w\" sizes=\"(max-width: 554px) 100vw, 554px\" \/><\/a><\/p>\n<p><strong>AFM<\/strong><strong>\uff1a\u7528\u4e8e\u9ad8\u6027\u80fd\u8d85\u7ea7\u7535\u5bb9\u5668\u7684\u53ef\u6301\u7eed<\/strong><strong>3D<\/strong><strong>\u7ed3\u6784\u7c98\u5408\u5242<\/strong><\/p>\n<p>\u67d4\u6027\u8d85\u7ea7\u7535\u5bb9\u5668\u4ee3\u8868\u4e86\u4f5c\u4e3a\u7535\u6e90\u7684\u4e0b\u4e00\u4ee3\u53ef\u7a7f\u6234\u6d88\u8d39\u7535\u5b50\u4ea7\u54c1\u7684\u4e00\u9879\u6709\u5438\u5f15\u529b\u7684\u6280\u672f\uff0c\u4f46\u901a\u5e38\u5177\u6709\u76f8\u5bf9\u8f83\u4f4e\u7684\u80fd\u91cf\u5bc6\u5ea6\u3002\u975e\u5e38\u9700\u8981\u4e3a\u8d85\u7ea7\u7535\u5bb9\u5668\u7684\u5b9e\u9645\u5e94\u7528\u6784\u5efa\u9ad8\u6027\u80fd\u7535\u6781\u3002\u5728\u8fd9\u91cc\uff0c\u53d7\u5230\u8718\u86db\u7f51\u81ea\u7136\u7ed3\u6784\u7684\u542f\u53d1\uff0c\u4f5c\u8005\u901a\u8fc7\u751f\u7269\u5408\u6210\u8fc7\u7a0b\u7cbe\u5fc3\u8bbe\u8ba1\u4e86\u7c98\u5408\u5242\uff0c\u6765\u6784\u5efa\u5177\u6709\u4f18\u5f02\u673a\u68b0\u6027\u80fd\u548c\u7535\u5316\u5b66\u6027\u80fd\u7684\u67d4\u6027\u7535\u6781\u3002\u901a\u8fc7\u8fd9\u79cd\u7b56\u7565\uff0c\u53d7\u8718\u86db\u7f51\u542f\u53d1\u76843D\u7ed3\u6784\u7c98\u5408\u5242\u53ef\u5b9e\u73b0\u5927\u7684\u79bb\u5b50\u53ef\u53ca\u8868\u9762\u79ef\u548c\u6d3b\u6027\u7535\u6781\u6750\u6599\u7684\u9ad8\u5806\u79ef\u5bc6\u5ea6\u4ee5\u53ca\u6709\u6548\u7684\u79bb\u5b50\u4f20\u8f93\u9014\u5f84\u3002\u7ed3\u679c\uff0c\u5728\u590d\u5408\u7535\u6781\u548c\u5bf9\u79f0\u8d85\u7ea7\u7535\u5bb9\u5668\u4e2d\u5206\u522b\u5b9e\u73b0\u4e864.62 F cm<sup>-2<\/sup>\u7684\u9ad8\u9762\u7535\u5bb9\u548c0.18 mW h cm<sup>-2<\/sup>\u7684\u9ad8\u9762\u80fd\u91cf\u5bc6\u5ea6\uff0c\u5c55\u793a\u4e86\u6784\u5efa\u67d4\u6027\u50a8\u80fd\u8bbe\u5907\u7684\u6f5c\u529b\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cSustainable 3D Structural Binder for High-Performance Supercapacitor by Biosynthesis Process\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728AFM\u4e0a\u3002DOI: 10.1002\/adfm.202105070<\/p>\n<p>\u56fe15\u53d7\u8718\u86db\u7f51\u542f\u53d1\u7684\u590d\u5408\u7535\u6781\u7684\u5236\u9020<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/15.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231777\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/15.jpg\" alt=\"\" width=\"554\" height=\"299\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/15.jpg 554w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/15-300x162.jpg 300w\" sizes=\"(max-width: 554px) 100vw, 554px\" \/><\/a><\/p>\n<p><strong>AFM<\/strong><strong>\uff1a\u6838\u58f3<\/strong><strong>ZnTe@N<\/strong><strong>\u63ba\u6742\u78b3\u7eb3\u7c73\u7ebf\u7528\u4e8e\u78b1\u91d1\u5c5e\u79bb\u5b50\u5b58\u50a8<\/strong><\/p>\n<p>\u5728\u8fd9\u91cc\uff0c\u4f5c\u8005\u901a\u8fc7\u7b80\u5355\u7684\u79bb\u5b50\u4ea4\u6362\u548c\u78b3\u5316\u6280\u672f\u8bbe\u8ba1\u548c\u5236\u5907\u4e86\u4e00\u7ef4\u6c2e\u63ba\u6742\u7684\u78b3\u5305\u8986\u7684ZnTe\u6838\u58f3\u7eb3\u7c73\u7ebf\uff08ZnTe@C\uff09\u3002\u5f53\u88ab\u8bc4\u4f30\u4e3a\u91d1\u5c5e\u79bb\u5b50\u7535\u6c60\u7684\u8d1f\u6781\u65f6\uff0c\u5b83\u5728\u9502\u79bb\u5b50\u548c\u94a0\u79bb\u5b50\u5b58\u50a8\u65b9\u9762\u8868\u73b0\u51fa\u4f18\u5f02\u7684\u7535\u5316\u5b66\u6027\u80fd\uff0c\u4f18\u5f02\u7684\u9ad8\u500d\u7387\u6027\u80fd\u548c\u957f\u671f\u5faa\u73af\u7a33\u5b9a\u6027\u3002\u5728\u9ad8\u5bfc\u7535\u7eb3\u7c73\u7ed3\u6784\u4e2d\u5d4c\u5165\u9ad8\u5bc6\u5ea6\u548c\u9ad8\u6027\u80fd\u6d3b\u6027\u6750\u6599\u7684\u7b56\u7565\u4ee3\u8868\u4e86\u5b9e\u73b0\u5177\u6709\u4f18\u5f02\u91cd\u91cf\u548c\u4f53\u79ef\u5bb9\u91cf\u7684\u7535\u6781\u6750\u6599\u4ee5\u5b9e\u73b0\u5353\u8d8a\u50a8\u80fd\u7cfb\u7edf\u7684\u6709\u6548\u65b9\u6cd5\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cRational Design of Core-Shell ZnTe@N-Doped Carbon Nanowires for High Gravimetric and Volumetric Alkali Metal Ion Storage\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728AFM\u4e0a\u3002DOI: 10.1002\/adfm.202006425<\/p>\n<p>\u56fe16 ZnTe@C\u7eb3\u7c73\u7ebf\u5236\u5907<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/16.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231778\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/16.jpg\" alt=\"\" width=\"554\" height=\"140\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/16.jpg 554w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/16-300x76.jpg 300w\" sizes=\"(max-width: 554px) 100vw, 554px\" \/><\/a><\/p>\n<p><strong>AFM<\/strong><strong>\uff1a\u751f\u7269\u5408\u6210\u7684\u53ef\u98df\u7528\u3001\u8d85\u5f3a\u548c\u65e0\u5fae\u5851\u6599\u7684\u7ec6\u83cc\u7ea4\u7ef4\u7d20\u57fa\u5438\u7ba1<\/strong><\/p>\n<p>\u5728\u8fd9\u91cc\uff0c\u4f5c\u8005\u62a5\u9053\u4e86\u4e00\u79cd\u7531\u7ec6\u83cc\u7ea4\u7ef4\u7d20 (BC) \u901a\u8fc7\u751f\u7269\u5408\u6210\u5236\u6210\u7684\u65b0\u578b\u53ef\u98df\u7528\u65e0\u5fae\u5851\u6599\u5438\u7ba1\u3002\u901a\u8fc7\u85fb\u9178\u76d0\u6d82\u5c42\uff0c\u8fd9\u79cd\u57fa\u4e8eBC\u7684\u5438\u7ba1\u5b9e\u73b0\u4e86\u6bd4\u7eb8\u5438\u7ba1\u66f4\u597d\u7684\u673a\u68b0\u6027\u80fd\uff0c\u5e76\u4e14\u907f\u514d\u4e86\u989d\u5916\u7684\u7c98\u5408\u5242\u3002\u7531\u4e8e3D\u7eb3\u7c73\u7ea4\u7ef4\u7f51\u7edc\u548c\u5f3a\u5927\u7684\u5c42\u95f4\u8fde\u63a5\uff0c\u8fd9\u79cd\u57fa\u4e8eBC\u7684\u79f8\u79c6\u7684\u7efc\u5408\u6027\u80fd\u8d85\u8fc7\u4e86\u5e02\u552e\u540c\u7c7b\u4ea7\u54c1\uff0c\u6ee1\u8db3\u4e86\u5b9e\u9645\u4f7f\u7528\u7684\u8981\u6c42\u3002\u7279\u522b\u503c\u5f97\u6ce8\u610f\u7684\u662f\uff0c\u53ef\u98df\u7528\u7279\u6027\u4e3a\u5438\u7ba1\u63d0\u4f9b\u4e86\u66f4\u597d\u7684\u7528\u6237\u4f53\u9a8c\u548c\u65b0\u7684\u62a5\u5e9f\u9009\u62e9\uff0c\u4f7f\u57fa\u4e8eBC\u7684\u5438\u7ba1\u6210\u4e3a\u5851\u6599\u5438\u7ba1\u7684\u66f4\u5065\u5eb7\u3001\u66f4\u73af\u4fdd\u7684\u66ff\u4ee3\u54c1\u3002\u76f8\u5173\u7814\u7a76\u4ee5\u201cEdible, Ultrastrong, and Microplastic-Free Bacterial Cellulose-Based Straws by Biosynthesis\u201d\u4e3a\u9898\u76ee\uff0c\u53d1\u8868\u5728AFM\u4e0a\u3002DOI: 10.1002\/adfm.202111713<\/p>\n<p>\u56fe17 \u6750\u6599\u5236\u5907\u8fc7\u7a0b<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/17.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-231779\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/17.jpg\" alt=\"\" width=\"554\" height=\"265\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/17.jpg 554w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/17-300x144.jpg 300w\" sizes=\"(max-width: 554px) 100vw, 554px\" \/><\/a><\/p>\n<p><strong>\u666f\u884c\u4f9b\u7a3f<\/strong><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4eca\u5929\u5411\u5927\u5bb6\u6c47\u603b\u4fde\u4e66\u5b8f\u9662\u58eb\u56e2\u961f2021\u5e74\u4e00\u4e9b\u5de5\u4f5c\uff0c\u4e00\u517117\u7bc7\u3002 Nat. Commun.\uff1a\u901a\u8fc7\u8fd1\u7ea2\u5916\u6d3b\u6027\u6676\u683c\u5339\u914d\u5f62\u6001\u5f02\u8d28\u7ed3\u63d0\u9ad8\u5149\u7535\u5316\u5b66\u6548\u7387 \u5149\u7535\u50ac\u5316\u662f\u4e00\u79cd\u4ece\u592a\u9633\u80fd&#8230;<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[1187],"tags":[],"class_list":["post-231759","post","type-post","status-publish","format-standard","hentry","category-zhuanlan"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/231759"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=231759"}],"version-history":[{"count":5,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/231759\/revisions"}],"predecessor-version":[{"id":231781,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/231759\/revisions\/231781"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=231759"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=231759"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=231759"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}