{"id":232000,"date":"2022-01-17T06:01:51","date_gmt":"2022-01-16T22:01:51","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=232000"},"modified":"2022-01-16T18:32:33","modified_gmt":"2022-01-16T10:32:33","slug":"%e6%b8%a4%e6%b5%b7%e5%a4%a7%e5%ad%a6%e9%84%82%e6%b6%9bjclp-%e9%92%bc%e7%84%b6%e7%a6%bb%e5%8e%bb%ef%bc%8c%e7%a1%ab%e4%b8%8b%e6%b4%bb%e5%8a%9b%ef%bc%9a%e4%b8%8d","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=232000","title":{"rendered":"\u6e24\u6d77\u5927\u5b66\u9102\u6d9bJCLP\uff1a \u201c\u94bc\u201d\u7136\u79bb\u53bb\uff0c\u201c\u786b\u201d\u4e0b\u6d3b\u529b\uff1a\u4e0d\u9971\u548c\u94bc\u7a7a\u4f4d\u4fee\u9970MoS2\/TiO2\u6784\u5efaZ\u578b\u5f02\u8d28\u7ed3&#038;\u63d0\u9ad8\u7535\u5b50\u8fc1\u79fb\u7387"},"content":{"rendered":"<p><strong>\u3010\u7814\u7a76\u80cc\u666f\u3011<\/strong><\/p>\n<p>\u8fd1\u5e74\u6765\uff0c2D\u8fc7\u6e21\u91d1\u5c5e\u786b\u5316\u7269\uff08TMDs\uff09\u6750\u6599\u5907\u53d7\u5173\u6ce8\uff0c\u5176\u4e2d\u6700\u5177\u4ee3\u8868\u6027\u7684\u662fMoS<sub>2<\/sub>\u3002\u7531\u4e8e\u5176\u53ef\u8c03\u63a7\u7684\u5e26\u9699\u3001\u8f83\u4f4e\u7684\u6210\u672c\u548c\u4e30\u5bcc\u7684\u6d3b\u6027\u8fb9\u7f18\u4f4d\u70b9\uff0c\u88ab\u5e7f\u6cdb\u5e94\u7528\u4e8e\u5149\u7535\u50ac\u5316\u3001\u7535\u6781\u6750\u6599\u53ca\u50a8\u80fd\u6750\u6599\u4e2d\u3002\u7136\u800c\uff0c\u6d3b\u6027\u4f4d\u70b9\u8fb9\u7f18\u5316\u7684\u95ee\u9898\u5c06\u5f71\u54cdMoS<sub>2<\/sub>\u7684\u50ac\u5316\u6027\u80fd\u3002\u56e0\u6b64\uff0c\u5728MoS<sub>2<\/sub>\u60f0\u6027\u886c\u5e95\u4e2d\u5f15\u5165\u7a7a\u4f4d\u7f3a\u9677\u53ef\u4ee5\u6fc0\u6d3b\u60f0\u6027\u57fa\u9762\uff0c\u66b4\u9732\u5927\u91cf\u7684\u6d3b\u6027\u4f4d\u70b9\uff0c\u63d0\u9ad8\u6750\u6599\u7684\u5149\u50ac\u5316\u6027\u80fd\u3002\u5728\u6cbb\u7406\u53d7\u6c61\u67d3\u6c34\u4f53\u7684\u5b9e\u9645\u5e94\u7528\u4e2d\u5177\u6709\u91cd\u8981\u610f\u4e49\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/1-9.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-232002\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/1-9.jpg\" alt=\"\" width=\"670\" height=\"899\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/1-9.jpg 670w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/1-9-224x300.jpg 224w\" sizes=\"(max-width: 670px) 100vw, 670px\" \/><\/a><\/p>\n<p><strong>\u3010\u6587\u7ae0\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c\u6e24\u6d77\u5927\u5b66\u5316\u5b66\u4e0e\u6750\u6599\u5de5\u7a0b\u5b66\u9662\u5468\u745e\u5cf0\u7855\u58eb\u7814\u7a76\u751f\u4e3a\u7b2c\u4e00\u4f5c\u8005\uff0c\u6768\u59dd\u5b9c\u526f\u6559\u6388\u548c\u9102\u6d9b\u6559\u6388\u4e3a\u901a\u8baf\u4f5c\u8005\u7684\u7814\u7a76\u6210\u679c\u300aThe defect is perfect: MoS<sub>2<\/sub>\/TiO<sub>2<\/sub> modified with unsaturated Mo vacancies to construct Z-scheme heterojunction &amp; improve mobility of e<sup>&#8211;<\/sup>\u300b\u5728\u73af\u5883\u9886\u57df\u56fd\u9645\u8457\u540d\u671f\u520a\u300aJournal of Cleaner Production\u300b\uff08IF=9.3\uff09\u53d1\u8868\u3002\u672c\u6587\u901a\u8fc7\u4e00\u6b65\u6c34\u70ed\u6cd5\u5236\u5907\u4e86\u7f3a\u9677\u578bMoS<sub>2<\/sub>\/TiO<sub>2<\/sub>\u5149\u50ac\u5316\u5242\u5e76\u7814\u7a76\u4e86\u7f3a\u9677\u5f62\u6210\u673a\u7406\u53ca\u4e0d\u540c\u7f3a\u9677\u5ea6\u4e0b\u50ac\u5316\u5242\u5bf9\u7f57\u4e39\u660eB\uff08Rh-B\uff09\u964d\u89e3\u7684\u5f71\u54cd\u3002\u7ed3\u679c\u8868\u660e\uff0c\u5728MoS<sub>2<\/sub>\u60f0\u6027\u57fa\u9762\u5f15\u5165\u7a7a\u4f4d\u7f3a\u9677\u5c06\u66b4\u9732\u5927\u91cfMo-S\u60ac\u7a7a\u952e\uff0c\u589e\u52a0MoS<sub>2<\/sub>\u8868\u9762\u6d3b\u6027\u4f4d\u70b9\u4fc3\u8fdb\u7535\u5b50\u7684\u6355\u83b7\uff0c\u63d0\u9ad8\u5149\u751f\u7535\u5b50-\u7a7a\u7a74\u5bf9\u7684\u5206\u79bb\u7387\u3002\u6b64\u5916\uff0c\u4fdd\u7559\u4e8c\u6c27\u5316\u949b\u8f83\u5f3a\u6c27\u5316\u8fd8\u539f\u80fd\u529b\u7684\u540c\u65f6\uff0c\u589e\u5f3a\u4e86\u4e8c\u786b\u5316\u94bc\u7684\u6297\u5149\u8150\u8680\u80fd\u529b\u3002\u8fdb\u4e00\u6b65\u7a81\u51fa\u4e86MoS<sub>2<\/sub>\u4f5c\u4e3a\u52a9\u50ac\u5316\u5242\u7684\u4f18\u52bf\uff0c\u5e76\u4e3a\u5149\u50ac\u5316\u6cbb\u7406\u53d7\u6c61\u67d3\u6c34\u4f53\u63d0\u4f9b\u4e86\u53ef\u884c\u7684\u9014\u5f84\u3002<\/p>\n<p><strong>\u3010\u672c\u6587\u8981\u70b9\u3011<\/strong><\/p>\n<p>\u8981\u70b9\u4e00:MoS<sub>2<\/sub>\/TiO<sub>2<\/sub>\u7684\u5236\u5907<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/2-8.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-232003\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/2-8.jpg\" alt=\"\" width=\"1263\" height=\"940\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/2-8.jpg 1263w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/2-8-300x223.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/2-8-768x572.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/2-8-1024x762.jpg 1024w\" sizes=\"(max-width: 1263px) 100vw, 1263px\" \/><\/a><\/p>\n<p>\u56fe1\uff1a<\/p>\n<p>(a)\u5236\u5907\u5149\u50ac\u5316\u5242\u5b9e\u9a8c\u6d41\u7a0b\u56fe;<\/p>\n<p>(b) MoS<sub>2<\/sub>\u548cMoS<sub>2<\/sub>\/TiO<sub>2<\/sub>\u7684SEM\u3001TEM\u3001EDS\u56fe\u3002(b1\u4e3a\u7eafMoS<sub>2<\/sub>\u7684SEM\u56fe\uff0cb2\u4e3a\u8d1f\u8f7d\u5728MoS<sub>2<\/sub>\u8584\u7247\u4e0a\u7684TiO<sub>2<\/sub>\u7684SEM\u56fe\uff0cb3\u4e3aMoS<sub>2<\/sub>\/TiO<sub>2<\/sub>\u7684TEM\u56fe\uff0cb4\u4e3aMoS<sub>2<\/sub>\/TiO<sub>2<\/sub>\u5728\u9ad8\u5206\u8fa8\u900f\u5c04\u7535\u955c\u4e0b\u7684\u6676\u683c\u6761\u7eb9\u56fe\uff0cEDS Mapping\u5305\u62ecMo\u3001S\u3001O\u548cTi);<\/p>\n<p>(c)\u7eafMoS<sub>2<\/sub>\u548cMoS<sub>2<\/sub>\/TiO<sub>2<\/sub>\u4e0d\u540c\u7f3a\u9677\u7a0b\u5ea6\u7684FI-IR\u5149\u8c31\u3001(d) XRD\u5149\u8c31\u3001(e)\u62c9\u66fc\u5149\u8c31;(f) MoS<sub>2<\/sub>\u548cMoS<sub>2<\/sub>\/TiO<sub>2<\/sub>\u7684TGA\u56fe(\u63d2\u56fe:DTG\u56fe)\uff0c(g) DSC\u56fe\u3002<\/p>\n<p>\u8981\u70b9\u4e8c\uff1a\u5149\u50ac\u5316\u964d\u89e3Rh-B<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/3-9.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-232004\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/3-9.jpg\" alt=\"\" width=\"1267\" height=\"960\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/3-9.jpg 1267w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/3-9-300x227.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/3-9-768x582.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/3-9-1024x776.jpg 1024w\" sizes=\"(max-width: 1267px) 100vw, 1267px\" \/><\/a><\/p>\n<p>\u56fe2\uff1a<\/p>\n<p>(a)\u5149\u50ac\u5316\u53cd\u5e94\u8fc7\u7a0b\u793a\u610f\u56fe\uff1b<\/p>\n<p>(b)MoS<sub>2<\/sub>\/TiO<sub>2<\/sub>-0.045\u30010.09\u30010.2\u30010.3\u5728\u5149\u50ac\u5316\u53cd\u5e94\u4e2d\u5bf9Rh-B\u7684\u964d\u89e3\u7387;<\/p>\n<p>(c)\u4e0d\u540c\u5149\u50ac\u5316\u5242\u7684\u964d\u89e3\u901f\u7387\u5e38\u6570\uff1b<\/p>\n<p>(d)MoS<sub>2<\/sub>\/TiO<sub>2<\/sub>-0.09\u7684\u5438\u5149\u5ea6\u968f\u65f6\u95f4\u53d8\u5316\uff1b<\/p>\n<p>(e)\u548c(f)\u4e0d\u540cpH\u548c\u6295\u52a0\u91cf\u4e0bRh-B\u7684\u964d\u89e3\u7387\u3002<\/p>\n<p>\u8981\u70b9\u4e09\uff1a\u6750\u6599\u7f3a\u9677\u7684\u8868\u5f81<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/4-8.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-232005\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/4-8.jpg\" alt=\"\" width=\"1267\" height=\"960\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/4-8.jpg 1267w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/4-8-300x227.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/4-8-768x582.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/4-8-1024x776.jpg 1024w\" sizes=\"(max-width: 1267px) 100vw, 1267px\" \/><\/a><\/p>\n<p>\u56fe3\uff1a<\/p>\n<p>(a) MoS<sub>2<\/sub>\u7684\u900f\u5c04\u7535\u955c\u56fe\uff1b<\/p>\n<p>(b)-(d)\u4e0d\u540c\u7f3a\u9677\u5ea6\u7684MoS<sub>2<\/sub>\u548c\u7f3a\u9677\u578bMoS<sub>2<\/sub>\u7684XRD\u3001\u62c9\u66fc\u5149\u8c31\uff1b\u7eafMoS<sub>2<\/sub>\u548cMoS<sub>2<\/sub>-0.09\u7684\u7535\u5b50\u987a\u78c1\u5171\u632f\u56fe\uff1b<\/p>\n<p>(e)-(g) Mo3d\u3001S2p\u7684XPS\u5149\u8c31\u53caMoS<sub>2<\/sub>\uff0cMoS<sub>2<\/sub>\/TiO<sub>2<\/sub>-0.09\u603b\u8c31\u56fe\uff1b<\/p>\n<p>(h)-(i) O1s\u3001Ti2p\u53caMoS<sub>2<\/sub>\/TiO<sub>2<\/sub>-0.09\u7684XPS\u5149\u8c31\u3002<\/p>\n<p>\u8981\u70b9\u56db\uff1a\u5bc6\u5ea6\u6cdb\u51fd\u7406\u8bba\uff08DFT\uff09\u8ba1\u7b97<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/5-2.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-232006\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/5-2.png\" alt=\"\" width=\"1267\" height=\"940\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/5-2.png 1267w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/5-2-300x223.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/5-2-768x570.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/5-2-1024x760.png 1024w\" sizes=\"(max-width: 1267px) 100vw, 1267px\" \/><\/a><\/p>\n<p>\u56fe4\uff1a<\/p>\n<p>(a)\u7eafMoS<sub>2<\/sub>\u7684\u4fef\u89c6\u7ed3\u6784\u6a21\u578b\u3001\u4fa7\u89c6\u7ed3\u6784\u6a21\u578b\u3001\u80fd\u5e26\u8c31\u548cDOS\u56fe\uff1b<\/p>\n<p>(b)\u7f3a\u9677\u578bMoS<sub>2<\/sub>\u7684\u4fef\u89c6\u7ed3\u6784\u6a21\u578b\u3001\u4fa7\u89c6\u7ed3\u6784\u6a21\u578b\u3001\u80fd\u5e26\u8c31\u548cDOS\u56fe\uff1b<\/p>\n<p>(c)MoS<sub>2<\/sub>\/TiO<sub>2<\/sub>-0.09\u7684\u7ed3\u6784\u6a21\u578b\u548cDOS\u56fe\u3002<\/p>\n<p>\u8981\u70b9\u4e94\uff1a\u5f02\u8d28\u7ed3\u7684\u5f62\u6210\u548c\u4f5c\u7528<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/6-4.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-232007\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/6-4.jpg\" alt=\"\" width=\"1260\" height=\"795\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/6-4.jpg 1260w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/6-4-300x189.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/6-4-768x485.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/6-4-1024x646.jpg 1024w\" sizes=\"(max-width: 1260px) 100vw, 1260px\" \/><\/a><\/p>\n<p>\u56fe5\uff1a<\/p>\n<p>(a)MoS<sub>2<\/sub>\/TiO<sub>2<\/sub>-0.09\u5149\u50ac\u5316\u5242\u7684TEM\u56fe\uff1b<\/p>\n<p>(b)\u4e0e\u5f02\u8d28\u7ed3\u76f8\u5173\u7684\u7535\u5b50\u4f20\u8f93\u7684\u793a\u610f\u56fe\uff1b<\/p>\n<p>(c)-(f)MoS<sub>2<\/sub>-0.09\u3001TiO<sub>2<\/sub>\u3001MoS<sub>2<\/sub>\/TiO<sub>2<\/sub>-0.09\u7684UV-DRS\u56fe\u53caKubelka-Munk\u56fe<\/p>\n<p>(g)\u7eaf\u76f8\u3001\u5f02\u8d28\u7ed3\u548c\u6df7\u5408\u6001\u5149\u50ac\u5316\u5242\u5bf9Rh-B\u7684\u53bb\u9664\u7387\u3002<\/p>\n<p>\u8981\u70b9\u516d: \u7535\u5b50\u8fc1\u79fb\u548c\u5bff\u547d<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/7-1.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-232008\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/7-1.jpg\" alt=\"\" width=\"1267\" height=\"619\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/7-1.jpg 1267w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/7-1-300x147.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/7-1-768x375.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/7-1-1024x500.jpg 1024w\" sizes=\"(max-width: 1267px) 100vw, 1267px\" \/><\/a><\/p>\n<p>\u56fe6:<\/p>\n<p>(a)MoS<sub>2<\/sub>\u5c42\u95f4\u7535\u5b50\u4f20\u8f93\u8def\u5f84\u793a\u610f\u56fe\uff1b<\/p>\n<p>(b)\u4e09\u7535\u6781\u7535\u5316\u5b66\u5de5\u4f5c\u7ad9\u793a\u610f\u56fe\uff1b<\/p>\n<p>(c)MoS<sub>2<\/sub>\u3001MoS<sub>2<\/sub>\/TiO<sub>2<\/sub>-0.045\u30010.09\u30010.2\u30010.3\u7684\u7535\u5316\u5b66\u963b\u6297\u56fe\uff1b<\/p>\n<p>(d)MoS<sub>2<\/sub>\u3001MoS<sub>2<\/sub>\/TiO<sub>2<\/sub>-0.09\u7684\u5149\u81f4\u53d1\u5149\u5149\u8c31\uff1b<\/p>\n<p>(e)-(f)MoS<sub>2<\/sub>\u3001MoS<sub>2<\/sub>\/TiO<sub>2<\/sub>-0.09\u7684\u8367\u5149\u5bff\u547d\u56fe\u3002<\/p>\n<p>\u8981\u70b9\u4e03: Z\u578b\u5f02\u8d28\u7ed3\u7684\u50ac\u5316\u673a\u7406<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/8-1.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-232009\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/8-1.jpg\" alt=\"\" width=\"1267\" height=\"749\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/8-1.jpg 1267w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/8-1-300x177.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/8-1-768x454.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/8-1-1024x605.jpg 1024w\" sizes=\"(max-width: 1267px) 100vw, 1267px\" \/><\/a><\/p>\n<p>\u56fe7:<\/p>\n<p>(a)\u4e0d\u540c\u6dec\u706d\u5242\u5bf9Rh-B\u964d\u89e3\u7684\u5f71\u54cd;<\/p>\n<p>(b)\u3001(c)\u5149\u7167\u548c\u9ed1\u6697\u6761\u4ef6\u4e0b\u00b7O<sub>2<\/sub><sup>&#8211;<\/sup>\u548c\u00b7OH\u7684ESR\u56fe;<\/p>\n<p>(d)\u5728\u6a21\u62df\u5149\u7167\u6761\u4ef6\u4e0b\u4ea7\u751f\u6d3b\u6027\u7269\u8d28\u6a21\u578b\u56fe;<\/p>\n<p>(e)\u7535\u8377\u8f6c\u79fb\u673a\u7406\u56fe\u3002<\/p>\n<p>\u8981\u70b9\u516b: \u7535\u5b50\u8fc1\u79fb\u548c\u5bff\u547d<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/9-1.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-232010\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/9-1.jpg\" alt=\"\" width=\"1269\" height=\"1168\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/9-1.jpg 1269w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/9-1-300x276.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/9-1-768x707.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/9-1-1024x942.jpg 1024w\" sizes=\"(max-width: 1269px) 100vw, 1269px\" \/><\/a><\/p>\n<p>\u56fe8:<\/p>\n<p>(a) MT-0.09\u964d\u89e3Rh-B\u7684\u5faa\u73af\u4f7f\u7528\u6b21\u6570;<\/p>\n<p>(b) MT-0.09\u5149\u50ac\u5316\u53cd\u5e94\u524d\u540e\u7684XRD\u8c31\u56fe(\u9644\u56fe:MT-0.09\u5149\u50ac\u5316\u53cd\u5e94\u524d\u540e\u7684SEM\u56fe);<\/p>\n<p>(c) Rh-B\u53ef\u80fd\u7684\u964d\u89e3\u9014\u5f84\u3002<\/p>\n<p><strong>\u7ed3\u8bba<\/strong><\/p>\n<p>\u672c\u7814\u7a76\u901a\u8fc7\u5f15\u5165\u7a7a\u4f4d\u7f3a\u9677\u4fee\u9970MoS<sub>2<\/sub>\u60f0\u6027\u57fa\u9762\u589e\u52a0\u6d3b\u6027\u4f4d\u70b9\u6765\u63d0\u9ad8\u5176\u5149\u50ac\u5316\u6027\u80fd\u3002\u540c\u65f6\uff0c\u6784\u5efa\u5f02\u8d28\u7ed3\u6539\u5584\u4e86\u7535\u5b50\u8fc1\u79fb\u8def\u5f84\uff0c\u6709\u6548\u63d0\u9ad8\u4e86\u7535\u5b50-\u7a7a\u7a74\u5bf9\u7684\u5206\u79bb\uff0c\u5ef6\u957f\u4e86\u5149\u751f\u8f7d\u6d41\u5b50\u7684\u54cd\u5e94\u65f6\u95f4\u3002\u56e0\u6b64\uff0c\u901a\u8fc7\u5f15\u5165\u7f3a\u9677\u4fee\u9970MoS<sub>2 <\/sub>\u60f0\u6027\u57fa\u9762\u505a\u52a9\u50ac\u5316\u5242\u6709\u671b\u6269\u5c55\u534a\u5bfc\u4f53\u5149\u50ac\u5316\u6750\u6599\u5728\u73af\u5883\u4fee\u590d\u4e2d\u7684\u8bbe\u8ba1\u548c\u5e94\u7528\u3002<\/p>\n<p><strong>\u4f5c\u8005\u7b80\u4ecb<\/strong><\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/10-1.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-232011\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/10-1.jpg\" alt=\"\" width=\"499\" height=\"666\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/10-1.jpg 499w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/10-1-225x300.jpg 225w\" sizes=\"(max-width: 499px) 100vw, 499px\" \/><\/a><\/p>\n<p><strong>\u901a\u8baf\u4f5c\u8005<\/strong> <strong>\u9102\u6d9b\uff1a<\/strong>\u535a\u58eb\uff0c\u6559\u6388\uff0c\u6e24\u6d77\u5927\u5b66\u73af\u5883\u5de5\u7a0b\u4e13\u4e1a\u5e26\u5934\u4eba\uff0c\u7855\u58eb\u7814\u7a76\u751f\u5bfc\u5e08\u3002\u8fbd\u5b81\u7701\u6bdb\u76ae\u7eff\u8272\u5236\u9020\u4ea7\u4e1a\u6280\u672f\u521b\u65b0\u6218\u7565\u8054\u76df\u7406\u4e8b\u957f\uff0c\u9526\u5dde\u5e02\u91d1\u5c5e\u6750\u6599\u4ea7\u4e1a\u521b\u65b0\u8054\u76df\u4e13\u5bb6\u59d4\u5458\uff0c\u6e24\u6d77\u5927\u5b66\u73af\u4fdd\u4ea7\u4e1a\u6280\u672f\u7814\u7a76\u6240\u6240\u957f\u3002\u7814\u7a76\u5174\u8da3\uff1a\u5316\u5de5\u6e05\u6d01\u751f\u4ea7\u5de5\u827a\uff0c\u571f\u58e4\u4e0e\u6c34\u6c61\u67d3\u4fee\u590d\u6280\u672f\u3001\u4f4e\u78b3\u51cf\u78b3\u5de5\u827a\u6280\u672f\u5f00\u53d1\u53ca\u949b\u57fa\u529f\u80fd\u6750\u6599\u7684\u5236\u5907\u5de5\u827a\u53ca\u5e94\u7528\u3002\u5728<em>ACS Appl Mater Interfaces<\/em>\uff0c<em>J Hazard Mater<\/em><em>\uff0c<\/em><em>Sep Purif Technol<\/em><em>\uff0c<\/em><em>J CLEAN PROD<\/em> <em>\uff0c<\/em><em>J. Environ. Chem. Eng<\/em>\u7b49\u56fd\u9645\u8457\u540d\u671f\u520a\u4e0a\u4ee5\u7b2c\u4e00\/\u901a\u8baf\u4f5c\u8005\u53d1\u8868SCI\u6536\u5f55\u8bba\u658722\u7bc7\uff0c\u4e3b\u630124\u9879\u79d1\u7814\u9879\u76ee\uff0c\u4ee5\u7b2c\u4e00\u53d1\u660e\u4eba\u83b7\u5f97\u6388\u6743\u53d1\u660e\u4e13\u522913\u9879\uff0c\u5355\u9879\u4e13\u5229\u8f6c\u5316\u989d\u5ea6\u8d85100\u4e07\uff0c\u8fd1\u4e09\u5e74\u79d1\u6280\u6210\u679c\u8f6c\u5316\u5408\u540c\u91d1\u989d623\u4e07\u3002<\/p>\n<p>\u7535\u5b50\u90ae\u7bb1\uff1aetao@bhu.edu.cn<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/11-1.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-232012\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/11-1.jpg\" alt=\"\" width=\"443\" height=\"665\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/11-1.jpg 443w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/11-1-200x300.jpg 200w\" sizes=\"(max-width: 443px) 100vw, 443px\" \/><\/a><\/p>\n<p><strong>\u901a\u8baf\u4f5c\u8005<\/strong> <strong>\u6768\u59dd\u5b9c\uff1a<\/strong>\u6e24\u6d77\u5927\u5b66\u73af\u5883\u5de5\u7a0b\u4e13\u4e1a\u526f\u6559\u6388\uff0c\u7855\u58eb\u751f\u5bfc\u5e08\u3002\u7814\u7a76\u5174\u8da3\uff1a\u571f\u58e4\u4fee\u590d\u6280\u672f\u548c\u56fa\u4f53\u5e9f\u7269\u8d44\u6e90\u5316\u3002\u5728<em>J Hazard Mater<\/em><em>\uff0c<\/em><em>J CLEAN PROD<\/em><em>\uff0c<\/em><em>ACS Appl Mater Interfaces, Sep Purif Technol<\/em><em>\uff0c<\/em><em> J. Alloys Compd<\/em>\u7b49\u56fd\u9645\u8457\u540d\u671f\u520a\u4e0a\u4ee5\u7b2c\u4e00\/\u901a\u8baf\u4f5c\u8005\u53d1\u8868SCI\u6536\u5f55\u8bba\u658714\u7bc7\uff0c\u62c5\u4efb\u300a<em>Journal of Alloys and Compounds<\/em>\u300b\uff0c\u300a<em>Journal of Cleaner Production<\/em>\u300b\uff0c\u300a<em>Journal of Polymers and the Environment<\/em>\u300b\u7b49SCI\u77e5\u540d\u671f\u520a\u5ba1\u7a3f\u4eba\u3002<\/p>\n<p>\u7535\u5b50\u90ae\u7bb1\uff1ayangshuyi@bhu.edu.cn<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/12-1.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-232013\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/12-1.jpg\" alt=\"\" width=\"313\" height=\"430\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/12-1.jpg 313w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/01\/12-1-218x300.jpg 218w\" sizes=\"(max-width: 313px) 100vw, 313px\" \/><\/a><\/p>\n<p><strong>\u7b2c\u4e00\u4f5c\u8005<\/strong> <strong>\u5468\u745e\u5cf0\uff1a<\/strong>\u6e24\u6d77\u5927\u5b66\u5316\u5b66\u5de5\u827a\u4e13\u4e1a\u7855\u58eb\u7814\u7a76\u751f\u3002\u7814\u7a76\u5174\u8da3\uff1a\u5149\u50ac\u5316\u9ad8\u7ea7\u6c27\u5316\u6280\u672f\u3002\u76ee\u524d\u5728J Solid State Chem.\u548cJ. Clean. Prod.\u671f\u520a\u4e0a\u53d1\u8868SCI\u6536\u5f55\u8bba\u6587\u51712\u7bc7\u3002<\/p>\n<p>\u7535\u5b50\u90ae\u7bb1\uff1a864554129@qq.com<\/p>\n<p><strong>\u6587\u7ae0\u4fe1\u606f<\/strong><\/p>\n<p>Zhou, S. Yang*, T. E*,L. Liu, J. Qian, The defect is perfect: MoS<sub>2<\/sub>\/TiO<sub>2<\/sub> modified with unsaturated Mo vacancies to construct Z-scheme heterojunction &amp; improve mobility of e<sup>&#8211;<\/sup>, Journal of Cleaner Production, <strong><em>Journal of Cleaner Production.<\/em><\/strong>DOI: 10.1016\/j.jclepro.2022.130511<\/p>\n<p>\u4f9b\u7a3f\u4eba\uff1a\u6e24\u6d77\u5927\u5b66\uff1a\u5468\u745e\u5cf0<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u7814\u7a76\u80cc\u666f\u3011 \u8fd1\u5e74\u6765\uff0c2D\u8fc7\u6e21\u91d1\u5c5e\u786b\u5316\u7269\uff08TMDs\uff09\u6750\u6599\u5907\u53d7\u5173\u6ce8\uff0c\u5176\u4e2d\u6700\u5177\u4ee3\u8868\u6027\u7684\u662fMoS2\u3002\u7531\u4e8e\u5176\u53ef\u8c03\u63a7\u7684\u5e26\u9699\u3001\u8f83\u4f4e\u7684\u6210\u672c\u548c\u4e30\u5bcc\u7684\u6d3b\u6027\u8fb9\u7f18\u4f4d\u70b9\uff0c\u88ab\u5e7f\u6cdb\u5e94\u7528\u4e8e\u5149&#8230;<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-232000","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/232000"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=232000"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/232000\/revisions"}],"predecessor-version":[{"id":232015,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/232000\/revisions\/232015"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=232000"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=232000"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=232000"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}