{"id":233110,"date":"2022-02-15T06:39:27","date_gmt":"2022-02-14T22:39:27","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=233110"},"modified":"2022-02-14T20:41:16","modified_gmt":"2022-02-14T12:41:16","slug":"%e5%9f%ba%e4%ba%8e%e4%ba%8c%e7%bb%b4%e6%9d%90%e6%96%99%e5%92%8c%e5%ae%bd%e7%a6%81%e5%b8%a6%e5%8d%8a%e5%af%bc%e4%bd%93%e5%bc%82%e8%b4%a8%e7%bb%93%e6%9e%84%e7%9a%84%e6%9c%80%e6%96%b0%e8%bf%9b%e5%b1%95","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=233110","title":{"rendered":"\u57fa\u4e8e\u4e8c\u7ef4\u6750\u6599\u548c\u5bbd\u7981\u5e26\u534a\u5bfc\u4f53\u5f02\u8d28\u7ed3\u6784\u7684\u6700\u65b0\u8fdb\u5c55"},"content":{"rendered":"<p>\u968f\u7740\u4eba\u4eec\u5bf9\u4e8c\u7ef4\uff08Two dimensional\uff0c2D\uff09\u6750\u6599\u7814\u7a76\u7684\u5174\u8da3\u65e5\u76ca\u6d53\u539a\uff0c\u8fd1\u5e74\u6765\u5bf9\u4e8c\u7ef4\u5f02\u8d28\u7ed3\u6784\u8fdb\u884c\u4e86\u8bb8\u591a\u7efc\u8ff0\u548c\u62a5\u9053\uff0c\u4f46\u76ee\u524d\u8fd8\u6ca1\u6709\u5bf9\u5bbd\u7981\u5e26\u534a\u5bfc\u4f53\uff08Wide Bandgap Semiconductor\uff0cWBS\uff0c\u4e3b\u8981\u662fSiC\u6216GaN\uff09\u57fa\u4e8c\u7ef4\u5f02\u8d28\u7ed3\u6784\u7684\u7cfb\u7edf\u63cf\u8ff0\u3002\u4e8c\u7ef4\u6750\u6599\u7684\u8ff7\u4eba\u7279\u6027\uff0c\u5982\u65e0\u60ac\u7a7a\u952e\u8868\u9762\u548c\u5c42\u6570\u53ef\u8c03\u5e26\u9699\u7b49\uff0c\u548c\u5bbd\u7981\u5e26\u534a\u5bfc\u4f53\u9ad8\u8f7d\u6d41\u5b50\u8fc1\u79fb\u7387\u3001\u9ad8\u70ed\u5bfc\u7387\u548c\u5927\u5e26\u9699\u3001\u9ad8\u51fb\u7a7f\u7535\u538b\u7684\u7279\u6027\uff0c\u6fc0\u53d1\u4e86\u4eba\u4eec\u5bf9\u4e24\u8005\u4e4b\u95f4\u5f02\u8d28\u7ed3\u6784\u65b0\u7269\u7406\u63a2\u7d22\u7684\u7814\u7a76\u5174\u8da3\u3002\u6b64\u5916\uff0c2D\/WBS\u5f02\u8d28\u7ed3\u6784\u7684\u826f\u597d\u6676\u683c\u5339\u914d\u6709\u671b\u63d0\u9ad8\u5916\u5ef6\u4e8c\u7ef4\u6750\u6599\u7684\u6676\u4f53\u8d28\u91cf\u548c\u76f8\u5173\u5f02\u8d28\u7ed3\u7684\u754c\u9762\u8d28\u91cf\u3002\u8003\u8651\u5230\u4e8c\u7ef4\u5f02\u8d28\u7ed3\u6784\u9886\u57df\u7684\u5feb\u901f\u8fdb\u5c55\u548c\u524d\u666f\uff0c\u6709\u5fc5\u8981\u53ca\u65f6\u5730\u6982\u8ff02D\/WBS\u5f02\u8d28\u7ed3\u6784\u53ca\u5176\u5668\u4ef6\u7684\u6700\u65b0\u53d1\u5c55\uff0c\u8fd9\u5c06\u6709\u5229\u4e8e\u63a8\u8fdb\u8be5\u9886\u57df\u7684\u7814\u7a76\u548c\u5f00\u53d1\u3002<\/p>\n<p>\u8fd1\u65e5\u6d59\u6c5f\u5927\u5b66\u676d\u5dde\u56fd\u9645\u79d1\u521b\u4e2d\u5fc3\u7684\u738b\u4f69\u5251\u7814\u7a76\u5458\u548c\u5218\u5f71\u535a\u58eb\u540e\u5728\u56fd\u9645\u8001\u724c\u7269\u7406\u5b66\u671f\u520a<em>Journal of Physics: Condensed Matter<\/em><em>\u4e0a<\/em>\u53d1\u8868\u4e86\u9898\u4e3aRecent Progress of Heterostructures Based on Two Dimensional Materials and Wide Bandgap Semiconductors\u7684\u7279\u9080\u7efc\u8ff0\u6587\u7ae0\uff0c\u6982\u8ff0\u4e862D\u6750\u6599\u548cWBS\u6750\u6599\u5f02\u8d28\u7ed3\u5e94\u7528\u7684\u591a\u6837\u6027\u548c\u6700\u65b0\u8fdb\u5c55\uff0c\u63d0\u51fa\u4e862D\/WBS\u5f02\u8d28\u7ed3\u6784\u5f53\u524d\u9762\u4e34\u7684\u6311\u6218\u548c\u672a\u6765\u6709\u524d\u666f\u7684\u7814\u7a76\u65b9\u5411\u3002<\/p>\n<p>\u4e8c\u7ef4\uff082D\uff09\u6750\u6599\u5177\u6709\u4e30\u5bcc\u591a\u6837\u7684\u7279\u6027\uff0c\u4f8b\u5982\u5c42\u6570\u76f8\u5173\u80fd\u5e26\u7ed3\u6784\u3001\u6709\u8da3\u7684\u81ea\u65cb-\u80fd\u8c37\u81ea\u7531\u5ea6\u548c\u4e30\u5bcc\u7684\u76f8\u7ed3\u6784\uff0c\u5728\u5fae\u7eb3\u5668\u4ef6\u4e2d\u5c55\u73b0\u51fa\u5e7f\u9614\u7684\u5e94\u7528\u524d\u666f\u3002\u540c\u65f6\uff0c\u5177\u6709\u9ad8\u51fb\u7a7f\u7535\u538b\u3001\u9ad8\u8fc1\u79fb\u7387\u548c\u9ad8\u70ed\u5bfc\u7387\u7684\u5bbd\u5e26\u9699\u534a\u5bfc\u4f53\uff08WBS\uff09\u5728\u9ad8\u9891\u5fae\u6ce2\u5668\u4ef6\u3001\u9ad8\u6e29\u548c\u5927\u529f\u7387\u7535\u5b50\u5668\u4ef6\u4e2d\u663e\u793a\u51fa\u91cd\u8981\u7684\u5e94\u7528\u3002\u591a\u529f\u80fd2D\/WBS\u5f02\u8d28\u7ed3\u6784\u53ef\u4ee5\u4fc3\u8fdb\u754c\u9762\u5904\u7684\u8f7d\u6d41\u5b50\u4f20\u8f93\uff0c\u53ef\u80fd\u63d0\u4f9b\u65b0\u7684\u7269\u7406\u73b0\u8c61\u548c\u5e94\u7528\uff0c\u5e76\u63d0\u9ad8\u7535\u5b50\u548c\u5149\u7535\u5668\u4ef6\u7684\u6027\u80fd\u3002\u672c\u7efc\u8ff0\u6982\u8ff0\u4e862D\u6750\u6599\u548cWBS\u6750\u6599\u5f02\u8d28\u7ed3\u6784\u7684\u4f18\u52bf\uff0c\u4ecb\u7ecd\u4e862D\/WBS\u5f02\u8d28\u7ed3\u6784\u5728\u4e0d\u540c\u5e94\u7528\u9886\u57df\u7684\u4e3b\u8981\u5236\u5907\u65b9\u6cd5\u548c\u8fdb\u5c55\uff0c\u63a2\u8ba8\u4e86\u5f02\u8d28\u7ed3\u6784\u4f18\u5f02\u6027\u80fd\u7684\u7269\u7406\u673a\u5236\uff0c\u603b\u7ed3\u4e862D\/WBS\u5f02\u8d28\u7ed3\u6784\u5728\u5149\u7535\u63a2\u6d4b\u5668\u3001\u5149\u50ac\u5316\u5242\u3001\u4f20\u611f\u5668\u3001\u53d1\u5149\u4e8c\u6781\u7ba1\u548c\u50a8\u80fd\u5668\u4ef6\u7b49\u65b9\u9762\u7684\u6f5c\u5728\u5e94\u7528\uff0c\u5e76\u63d0\u51fa\u4e86\u672a\u6765\u9700\u8981\u514b\u670d\u7684\u4e3b\u8981\u969c\u788d\u3002\u8be5\u5de5\u4f5c\u4e3a\u672a\u6765\u57fa\u4e8eSiC\u548cGaN\u7684\u4e8c\u7ef4\u5f02\u8d28\u7ed3\u6784\u7684\u53d1\u5c55\u65b9\u5411\u63d0\u4f9b\u4e86\u975e\u5e38\u6709\u7528\u7684\u53c2\u8003\u3002<\/p>\n<p>2D\/WBS\u5f02\u8d28\u7ed3\u5668\u4ef6\u5e94\u7528\u524d\u666f\u793a\u610f\u56fe:<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-233112\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/02\/\u56fe\u72471-7.jpg\" alt=\"\" width=\"265\" height=\"263\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/02\/\u56fe\u72471-7.jpg 265w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/02\/\u56fe\u72471-7-150x150.jpg 150w\" sizes=\"(max-width: 265px) 100vw, 265px\" \/><\/p>\n<p>\u5bf9\u4e8e2D\/SiC\u5f02\u8d28\u7ed3\u6784\uff0c\u76ee\u524d\u5bf92D\/SiC\u7684\u7814\u7a76\u4e3b\u8981\u96c6\u4e2d\u5728\u77f3\u58a8\u70ef\/SiC\u5f02\u8d28\u7ed3\u6784\uff0c\u5176\u6b21\u662fSiC\u4e0eTMDs\u548cMXene\u7684\u5f02\u8d28\u7ed3\u6784\u7b49\u3002\u77f3\u58a8\u70ef\/SiC\u5f02\u8d28\u7ed3\u6784\u7684\u5149\u7535\u63a2\u6d4b\u5668\u8868\u73b0\u51fa\u826f\u597d\u7684\u6027\u80fd\uff0c\u5982\u9ad8\u5149\u54cd\u5e94\u5ea6\u3001EQE\u548c\u63a2\u6d4b\u7387\u3002\u53e6\u5916\uff0c\u7531\u4e8e\u754c\u9762\u80fd\u5e26\u7ed3\u6784\u548c\u9ad8\u7684\u754c\u9762\u8d28\u91cf\uff0c\u5404\u79cd2D\/SiC\u5f02\u8d28\u7ed3\u6784\u5df2\u88ab\u7528\u4f5c\u9ad8\u6548\u5149\u50ac\u5316\u5242\uff0c\u4f8b\u5982SnO<sub>2<\/sub>\/SiC\u5f02\u8d28\u7ed3\u6784\u5668\u4ef6\u5728\u4f4e\u7535\u538b\u4e0b\u8868\u73b0\u51fa\u9ad8\u6790\u6c22\u901f\u7387\u548c\u5927\u7535\u6d41\u5bc6\u5ea6\u3002\u7528\u4e8e\u50a8\u80fd\u7684CuS\/SiC\u5f02\u8d28\u7ed3\u6784\u8d85\u7ea7\u7535\u5bb9\u5668\u4e5f\u8868\u73b0\u51fa\u9ad8\u7535\u5bb9\u3002\u6b64\u5916\uff0cEGNWs\/SiC\/Si\u6c14\u4f53\u4f20\u611f\u5668\u5b9e\u73b0\u4e86\u524d\u6240\u672a\u6709\u7684\u7075\u654f\u5ea6\u548c\u5feb\u901f\u54cd\u5e94\u3002<\/p>\n<p>2D SiC\u590d\u5408\u6750\u6599\u5149\u50ac\u5316\u6027\u80fd\u7684\u7269\u7406\u6839\u6e90\uff1a<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-233113\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/02\/\u56fe\u72472-5.jpg\" alt=\"\" width=\"529\" height=\"378\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/02\/\u56fe\u72472-5.jpg 529w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/02\/\u56fe\u72472-5-300x214.jpg 300w\" sizes=\"(max-width: 529px) 100vw, 529px\" \/><\/p>\n<p>\u5bf9\u4e8e2D\/GaN\u5f02\u8d28\u7ed3\u6784\uff0c\u7531\u4e8eGaN\u4f18\u5f02\u7684\u7535\u5b50\u8fc1\u79fb\u7387\u548c2D\/GaN\u754c\u9762\u80fd\u5e26\u6392\u5217\uff0c\u5b83\u4eec\u5728\u5149\u7535\u5668\u4ef6\u7684\u53d1\u5c55\u4e2d\u8868\u73b0\u51fa\u660e\u663e\u7684\u4f18\u52bf\uff0c\u5c24\u5176\u662fMoS<sub>2<\/sub>\/GaN\u5f02\u8d28\u7ed3\u6784\u3002\u4e0d\u540cMoS<sub>2<\/sub>\/GaN\u5f02\u8d28\u7ed3\u6784\u7684\u5149\u7535\u63a2\u6d4b\u5668\u8868\u73b0\u51fa\u9ad8\u54cd\u5e94\u5ea6\u548c\u63a2\u6d4b\u7387\uff0c\u5bbd\u7981\u5e26\/\u7a84\u7981\u5e26\u7684\u642d\u914d\u4e5f\u4f7f\u5f97\u63a2\u6d4b\u8303\u56f4\u540c\u65f6\u6db5\u76d6\u4e86\u7d2b\u5916\u548c\u53ef\u89c1\u6ce2\u6bb5\u3002TMDs\/GaN\u7684\u5f02\u8d28\u7ed3\u6784\u5728\u5149\u50ac\u5316\u548c\u5149\u89e3\u6c34\u65b9\u9762\u4e5f\u8868\u73b0\u51fa\u826f\u597d\u7684\u524d\u666f\u3002\u6b64\u5916\uff0cn-SnO<sub>2<\/sub>\/p-GaN\u5f02\u8d28\u7ed3\u6784\u7684\u53cc\u8272LED\u3001\u9ad8\u7075\u654f\u5ea6\u6c14\u4f53\u4f20\u611f\u5668\u548c\u65b0\u578bMoS<sub>2<\/sub>\/GaN\u5f02\u8d28\u7ed3\u6784\u7684PEC\u9002\u914d\u4f53\u4f20\u611f\u5668\u7b49\u591a\u79cd\u5668\u4ef6\uff0c\u63ed\u793a\u4e862D\/GaN\u5f02\u8d28\u7ed3\u6784\u7684\u5de8\u5927\u5e94\u7528\u6f5c\u529b\u3002<\/p>\n<p>2D MoS<sub>2<\/sub>\/GaN\u5f02\u8d28\u7ed3\u6784\u80fd\u5e26\u7ed3\u6784\u53ca\u76f8\u5173\u6c14\u654f\u4f20\u611f\u5668\u7684\u6027\u80fd\uff1a<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-233114\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/02\/\u56fe\u72473-5.jpg\" alt=\"\" width=\"554\" height=\"322\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/02\/\u56fe\u72473-5.jpg 554w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/02\/\u56fe\u72473-5-300x174.jpg 300w\" sizes=\"(max-width: 554px) 100vw, 554px\" \/><\/p>\n<p>\u5bf9\u6bd4\u57fa\u4e8e2D\/GaN\u548c2D\/SiC\u7684\u5f02\u8d28\u7ed3\u6784\u5149\u7535\u63a2\u6d4b\u5668\uff0c\u6240\u63cf\u8ff0\u76842D\/GaN\u5f02\u8d28\u7ed3\u6784\u8868\u73b0\u51fa\u66f4\u597d\u7684\u6027\u80fd\uff0c\u5176\u4e2d\uff0cMoS<sub>2<\/sub>\/GaN\u7684\u54cd\u5e94\u5ea6\u8fdc\u9ad8\u4e8e\u5176\u4ed6\u5f02\u8d28\u7ed3\u6784\u3002MoS<sub>2<\/sub>\/GaN\u5982\u6b64\u4f18\u5f02\u7684\u5149\u7535\u6027\u80fd\u5f52\u56e0\u4e8e\u4ee5\u4e0b\u56e0\u7d20\uff1a\uff081\uff09MoS<sub>2<\/sub>\/WBS\u7684\u754c\u9762\u5185\u5efa\u7535\u573a\u548c\u5f02\u8d28\u7ed3\u6784\u7684II\u578b\u80fd\u5e26\u6392\u5217\uff0c\u8fd9\u662f\u77f3\u58a8\u70ef\/WBS\u6240\u4e0d\u5177\u5907\u7684\u3002(2) \u4e0eSiC\u7684\u95f4\u63a5\u5e26\u9699\u4e0d\u540c\uff0cGaN\u7684\u76f4\u63a5\u5e26\u9699\u5177\u6709\u66f4\u9ad8\u7684\u5149\u751f\u8f7d\u6d41\u5b50\u6fc0\u53d1\u6548\u7387\uff0c\u80fd\u591f\u589e\u5f3aMoS<sub>2<\/sub>\/GaN\u5f02\u8d28\u7ed3\u7684\u5149\u54cd\u5e94\u5ea6\uff1b(3) MoS<sub>2<\/sub>\/GaN\u7684\u5e26\u8fb9\u504f\u79fb\u6bd4MoS<sub>2<\/sub>\/SiC\u5927\uff0c\u5bfc\u81f4\u754c\u9762\u4e0a\u7535\u8377\u8f6c\u79fb\u52bf\u80fd\u66f4\u5927\uff1b(4) GaN\u7684\u7535\u5b50\u8fc1\u79fb\u7387(1300 cm<sup>2<\/sup>\/V\u00b7s)\u9ad8\u4e8eSiC(\u5178\u578b4H-SiC\u7684900 cm<sup>2<\/sup>\/V\u00b7s)\uff0c\u4f7f\u5f972D\/GaN\u5f02\u8d28\u7ed3\u4e2d\u5149\u751f\u8f7d\u6d41\u5b50\u7684\u62bd\u53d6\u901f\u5ea6\u66f4\u5feb\u3002<\/p>\n<p>MoS<sub>2<\/sub>\/GaN\u5f02\u8d28\u7ed3\u6784\u5149\u7535\u63a2\u6d4b\u5668\u7684\u793a\u610f\u56fe\u548c\u5bf9\u5e94\u7684\u5149\u54cd\u5e94\u5ea6\u548c\u63a2\u6d4b\u7387\u7b49\u6027\u80fd\uff1a<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-233115\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/02\/\u56fe\u72474-4.jpg\" alt=\"\" width=\"529\" height=\"349\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/02\/\u56fe\u72474-4.jpg 529w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/02\/\u56fe\u72474-4-300x198.jpg 300w\" sizes=\"(max-width: 529px) 100vw, 529px\" \/><\/p>\n<p>\u603b\u800c\u8a00\u4e4b\uff0c\u672c\u7efc\u8ff0\u4e3b\u8981\u5173\u6ce82D\/WBS\u5f02\u8d28\u7ed3\u6784\u6750\u6599\u7684\u5e94\u7528\uff0c\u6db5\u76d6\u591a\u4e2a\u4e3b\u9898\uff0c\u5305\u62ec\u5149\u7535\u63a2\u6d4b\u5668\u3001\u5149\u50ac\u5316\u3001\u5149\u7535\u5316\u5b66\u3001\u5149\u7535\u4e8c\u6781\u7ba1\u3001\u65b0\u578b\u4f20\u611f\u5668\u3001\u50a8\u80fd\u5668\u4ef6\u548c\u5fc6\u963b\u5668\u5668\u4ef6\u3002\u5f02\u8d28\u7ed3\u6784\u7684\u754c\u9762\u6548\u5e94\uff0c\u5982\u80fd\u5e26\u6392\u5217\u3001\u5185\u5efa\u7535\u573a\u3001\u7f3a\u9677\u3001\u63ba\u6742\u6216\u754c\u9762\u5904\u7684\u8d85\u4ea4\u6362\u76f8\u4e92\u4f5c\u7528\uff0c\u5bf9\u5668\u4ef6\u7684\u6027\u80fd\u5177\u6709\u81f3\u5173\u91cd\u8981\u7684\u5f71\u54cd\u3002\u672c\u7efc\u8ff0\u4e2d\u4ecb\u7ecd\u7684\u5404\u79cd2D\/SiC\u548c2D\/GaN\u5f02\u8d28\u7ed3\u6784\u5c55\u793a\u4e862D\/WBS\u5f02\u8d28\u7ed3\u6784\u5e94\u7528\u7684\u591a\u6837\u6027\uff0c\u5177\u6709\u5f00\u53d1\u5b9e\u7528\u9ad8\u6027\u80fd\u5668\u4ef6\u7684\u6f5c\u529b\u3002<\/p>\n<p>\u5c3d\u7ba1\u5173\u4e8e2D\/WBS\u5f02\u8d28\u7ed3\u6784\u7684\u7406\u8bba\u9884\u6d4b\u6216\u5b9e\u9a8c\u5df2\u6709\u62a5\u9053\u548c\u8bc1\u5b9e\uff0c\u4f46\u5bf9\u5b83\u4eec\u7684\u7814\u7a76\u4ecd\u5904\u4e8e\u521d\u6b65\u9636\u6bb5\u30022D\/WBS\u5f02\u8d28\u7ed3\u6784\u7684\u57fa\u7840\u7814\u7a76\u548c\u5b9e\u7528\u5668\u4ef6\u90fd\u9762\u4e34\u7740\u8bb8\u591a\u6311\u6218\uff0c\u4f46\u4e5f\u9762\u4e34\u7740\u673a\u9047\u3002\u8fd9\u4e9b\u95ee\u9898\u9700\u8981\u5728\u8fdb\u4e00\u6b65\u7684\u5e94\u7528\u4e2d\u5f97\u5230\u89e3\u51b3\uff0c\u4f8b\u5982(i) \u529f\u80fd\u5728\u5f88\u5927\u7a0b\u5ea6\u4e0a\u53d6\u51b3\u4e8e\u5f02\u8d28\u7ed3\u6784\u7684\u8d28\u91cf\uff0c\u5305\u62ec\u6750\u6599\u548c\u754c\u9762\u7684\u8d28\u91cf\u3002(ii) \u63a2\u7d22\u65b0\u7269\u7406\uff0c\u66f4\u6df1\u5165\u5730\u7814\u7a76\u4e8c\u7ef4\/WBS\u5f02\u8d28\u7ed3\u6784\u7684\u5149\u5b66\u3001\u7535\u5b66\u6216\u78c1\u5b66\u6027\u8d28\u7684\u8c03\u5236\u673a\u5236\u5bf9\u5b9e\u73b0\u591a\u529f\u80fd\u81f3\u5173\u91cd\u8981\u3002(iii) \u8bbe\u8ba1\u548c\u5b9e\u73b0\u9ad8\u6027\u80fd\u548c\u9ad8\u4e00\u81f4\u6027\u7684\u8bbe\u5907\u6a21\u578b\uff0c\u7a81\u7834\u5f02\u8d28\u7ed3\u6784\u96c6\u6210\u7684\u5173\u952e\u79d1\u5b66\u95ee\u9898\uff0c\u5b9e\u73b0\u4e8c\u7ef4\/WBS\u5668\u4ef6\u7684\u6709\u6548\u548c\u53ef\u6269\u5c55\u7684\u96c6\u6210\u4e92\u8054\u7b49\u95ee\u9898\u4e5f\u8feb\u5728\u7709\u776b\u3002<\/p>\n<p>2D\/WBS\u5f02\u8d28\u7ed3\u6784\u6750\u6599\u7684\u96c6\u6210\u5c06\u7ed3\u5408\u4e24\u8005\u7684\u72ec\u7279\u7279\u6027\uff0c\u4e0d\u4ec5\u4e3a\u6784\u5efa\u5177\u6709\u591a\u79cd\u6750\u6599\u6df7\u5408\u7ed3\u6784\u7684\u9009\u62e9\u63d0\u4f9b\u7075\u6d3b\u6027\uff0c\u800c\u4e14\u8fd8\u80fd\u63d0\u4f9b\u5355\u79cd\u6750\u6599\u65e0\u6cd5\u5b9e\u73b0\u7684\u65b0\u529f\u80fd\u3002\u6b64\u5916\uff0c\u7814\u7a76\u7279\u5b9a\u4e8c\u7ef4\u901a\u9053\u4e0a\u7684\u754c\u9762\u63ba\u6742\u6216\u7f3a\u9677\u5bf9\u4e8e\u5f02\u8d28\u7ed3\u6784\u5668\u4ef6\u5c0f\u578b\u5316\u5f88\u91cd\u8981\u3002\u4ece\u5668\u4ef6\u5c0f\u578b\u5316\u7684\u89d2\u5ea6\u6765\u770b\uff0c\u5f53\u901a\u9053\u5c3a\u5bf8\u53d8\u5f97\u4e0e\u91cf\u5b50\u7269\u7406\u5360\u636e\u4e3b\u5bfc\u7684\u7a7a\u95f4\u5c3a\u5bf8\u76f8\u5f53\u65f6\uff0c\u4f1a\u5bf9\u5668\u4ef6\u5de5\u4f5c\u6709\u660e\u663e\u7684\u5f71\u54cd\u3002\u5c3d\u7ba1\u5bf9\u4e8c\u7ef4\u7cfb\u7edf\u4e2d\u754c\u9762\u7279\u6027\u7684\u4e86\u89e3\u8d8a\u6765\u8d8a\u591a\uff0c\u4f46\u5bf9\u4e8c\u7ef4\u5f02\u8d28\u7ed3\u6784\u754c\u9762\u7279\u6027\u7684\u8be6\u7ec6\u7814\u7a76\u548c\u5206\u6790\u4ecd\u7136\u975e\u5e38\u6709\u9650\u3002\u76f8\u4fe1\u8fd9\u4e00\u6fc0\u52a8\u4eba\u5fc3\u7684\u9886\u57df\u5c06\u4e3a\u5b9e\u73b0\u4e0b\u4e00\u4ee3\u7535\u5b50\u5b66\u548c\u5149\u7535\u5b50\u5b66\u5668\u4ef6\u5f00\u8f9f\u4e00\u6761\u65b0\u9014\u5f84\u3002<\/p>\n<p>\u8bba\u6587\u94fe\u63a5\uff1a<a href=\"https:\/\/iopscience.iop.org\/article\/10.1088\/1361-648X\/ac5310\">https:\/\/iopscience.iop.org\/article\/10.1088\/1361-648X\/ac5310<\/a><\/p>\n<p>\u4f5c\u8005\u4ecb\u7ecd\uff1a<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-233116\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/02\/\u56fe\u72475-4.jpg\" alt=\"\" width=\"83\" height=\"107\" \/><\/p>\n<p>\u738b\u4f69\u5251 \u7814\u7a76\u5458<\/p>\n<p>\u5728\u5317\u4eac\u5927\u5b66\u5143\u57f9\u5b66\u9662, \u7f8e\u56fdUniversity of Pennsylvania, \u7f8e\u56fdUniversity of Massachusetts, Amherst\u5206\u522b\u83b7\u5f97\u7269\u7406\u5b66\u5b66\u58eb\u3001\u6750\u6599\u79d1\u5b66\u4e0e\u5de5\u7a0b\u7855\u58eb\u3001\u7269\u7406\u5b66\u535a\u58eb\u5b66\u4f4d\uff0c\u968f\u540e\u5728\u7f8e\u56fd\u7ebd\u7ea6\u5dde\u7acb\u5927\u5b66(Buffalo)\u7269\u7406\u7cfb\u505a\u535a\u58eb\u540e\u7814\u7a76\u30022021\u5e74\u8fdb\u5165\u6d59\u6c5f\u5927\u5b66\u56fd\u9645\u79d1\u521b\u4e2d\u5fc3\uff0c\u5165\u9009\u79d1\u521b\u767e\u4eba\u8ba1\u5212\u3002\u8fd1\u4e09\u5e74\u6765\u5728ACS Nano, Nano Lett., Appl. Phys. Rev., Nat. Comm., Adv. Mater., Chem. Sci.\u7b49\u56fd\u9645\u6743\u5a01\u671f\u520a\u53d1\u8868\u8bba\u658714\u7bc7(8\u7bc7\u4e2d\u79d1\u9662\u4e00\u533a)\uff0c\u5176\u4e2d\u7b2c\u4e00\u4f5c\u8005\/\u5171\u540c\u4e00\u4f5c\/\u901a\u8baf\u4f5c\u80059\u7bc7\uff0c\u5df2\u6388\u67432\u9879\u4e13\u5229\uff0c4\u9879\u5728\u5ba1\u3002\u4e3b\u6301\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u9752\u5e74\u57fa\u91d1\u4e00\u9879\u3002\u53d7\u9080\u4e3aJ. Magn. Magn. Mater.\u3001Nanoscale\u3001JPCC\u7b49\u56fd\u9645\u520a\u7269\u5ba1\u7a3f\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-233117\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/02\/\u56fe\u72476-1.jpg\" alt=\"\" width=\"191\" height=\"262\" \/><\/p>\n<p>\u5218\u5f71 \u535a\u58eb\u540e<\/p>\n<p>2021\u5e74\u535a\u58eb\u6bd5\u4e1a\u4e8e\u6e56\u5317\u5927\u5b66\uff0c\u535a\u58eb\u671f\u95f4\u5728\u7f8e\u56fdOakland University\u8fdb\u884c\u4e86\u4e24\u5e74\u7684\u8054\u5408\u57f9\u517b\u3002\u76ee\u524d\u4e3b\u8981\u7814\u7a76\u4e8c\u7ef4\u6750\u6599\u53ca\u5176\u5f02\u8d28\u7ed3\u7684\u5236\u5907\u3001\u5149\u7535\u7279\u6027\u548c\u5fc6\u963b\u7279\u6027\u7684\u7814\u7a76\uff0c\u4ee5\u53ca\u4e8c\u7ef4\u5f02\u8d28\u7ed3\u6784\u5149\u7535\u63a2\u6d4b\u5668\u548c\u5fc6\u963b\u5668\u7684\u8bbe\u8ba1\u4e0e\u5f00\u53d1\u3002\u5171\u53d1\u8868SCI\u8bba\u658720\u4f59\u7bc7\uff0c\u5176\u4e2d\u4ee5\u7b2c\u4e00\u4f5c\u8005\u8eab\u4efd\u5728Sci. Rep.\u3001Mater. Res. Bull.\u3001JAP\u7b49\u671f\u520a\u4e0a\u53d1\u8868\u4e866\u7bc7\u6587\u7ae0\uff0c\u76ee\u524d\u6b63\u5728\u7533\u8bf7\u4e00\u9879\u4e8c\u7ef4\u6750\u6599\u5236\u5907\u6280\u672f\u7684\u53d1\u660e\u4e13\u5229\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u968f\u7740\u4eba\u4eec\u5bf9\u4e8c\u7ef4\uff08Two dimensional\uff0c2D\uff09\u6750\u6599\u7814\u7a76\u7684\u5174\u8da3\u65e5\u76ca\u6d53\u539a\uff0c\u8fd1\u5e74\u6765\u5bf9\u4e8c\u7ef4\u5f02\u8d28\u7ed3\u6784\u8fdb\u884c\u4e86\u8bb8\u591a\u7efc\u8ff0\u548c\u62a5\u9053\uff0c\u4f46\u76ee\u524d\u8fd8\u6ca1\u6709\u5bf9\u5bbd\u7981\u5e26\u534a\u5bfc\u4f53\uff08Wide B&#8230;<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-233110","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/233110"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=233110"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/233110\/revisions"}],"predecessor-version":[{"id":233118,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/233110\/revisions\/233118"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=233110"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=233110"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=233110"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}