{"id":236213,"date":"2022-04-25T06:01:41","date_gmt":"2022-04-24T22:01:41","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=236213"},"modified":"2022-04-24T16:01:49","modified_gmt":"2022-04-24T08:01:49","slug":"%e6%b1%aa%e6%b7%8f%e7%94%b0-nature-catalysis%ef%bc%9a%e7%ba%af%e5%ba%a6%ef%bc%9e99%e3%80%81%e5%9b%9e%e6%94%b6%e7%8e%8790%ef%bc%81pse%e5%8f%8d%e5%ba%94%e5%99%a8%e5%8a%a9%e5%8a%9bco2rr","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=236213","title":{"rendered":"\u6c6a\u6dcf\u7530 Nature Catalysis\uff1a\u7eaf\u5ea6\uff1e99%\u3001\u56de\u6536\u738790%\uff01PSE\u53cd\u5e94\u5668\u52a9\u529bCO2RR"},"content":{"rendered":"<p><strong>\u3010\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p>\u5229\u7528\u4e8c\u6c27\u5316\u78b3\u8fd8\u539f\u53cd\u5e94\uff08CO<sub>2<\/sub>RR\uff09\u5c06CO<sub>2<\/sub>\u7535\u5316\u5b66\u8f6c\u5316\u6210\u57fa\u672c\u7684\u5316\u5b66\u539f\u6599\u662f\u4e00\u79cd\u5728\u7f13\u89e3\u6c14\u5019\u53d8\u5316\u7684\u65b9\u6cd5\uff0c\u540c\u65f6\u50a8\u5b58\u548c\u4f7f\u7528\u53ef\u518d\u751f\u7535\u529b\u3002\u5176\u4e2d\uff0c\u50ac\u5316\u6750\u6599\u8bbe\u8ba1\u548c\u53cd\u5e94\u5668\u5de5\u7a0b\u4e00\u76f4\u662f\u8be5\u9886\u57df\u7684\u4e24\u5927\u91cd\u70b9\u3002\u867d\u7136\u5f00\u53d1\u4e86\u591a\u79cd\u50ac\u5316\u5242\u6765\u63d0\u9ad8\u5bf9C<sub>1<\/sub>\uff08CO\u7b49\uff09\u3001C<sub>2<\/sub>\uff08\u4e59\u9187\u7b49\uff09\u4ea7\u7269\u7684\u9009\u62e9\u6027\u548c\u6d3b\u6027\uff0c\u4f46CO<sub>2<\/sub>\u7535\u89e3\u69fd\u7684\u53d1\u5c55\uff0c\u5c24\u5176\u662f\u5728\u6d41\u901a\u6c60\u548c\u819c\u7535\u6781\u7ec4\u4ef6\uff08MEA\uff09\u7535\u6c60\u53cd\u5e94\u5668\u4e2d\u4f7f\u7528\u6c14\u4f53\u6269\u6563\u5c42\uff08GDL\uff09\u7535\u6781\uff0c\u5728\u8fbe\u5230\u5de5\u4e1a\u76f8\u5173\u6307\u6807\u65b9\u9762\u53d1\u6325\u6838\u5fc3\u4f5c\u7528\u3002\u5c3d\u7ba1CO<sub>2<\/sub>RR\u6027\u80fd\u7684\u53d6\u5f97\u4e0d\u9519\u8fdb\u5c55\uff0c\u4f46\u5b58\u5728\u4e00\u4e2a\u57fa\u672c\u4f46\u7ecf\u5e38\u88ab\u5ffd\u89c6\u7684\u6311\u6218\uff0c\u5b83\u53ef\u80fd\u4f1a\u6781\u5927\u5730\u9650\u5236CO<sub>2<\/sub>RR\u7684\u5546\u4e1a\u5316\u6f5c\u529b\uff1a\u78b3\u9178\u76d0\u4ea4\u53c9\u5bfc\u81f4\u7684\u5927\u91cf\u78b3\u635f\u5931\u3002\u5728CO<sub>2<\/sub>RR\u7535\u89e3\u8fc7\u7a0b\u4e2d\uff0c\u7279\u522b\u662f\u5728\u5927\u7535\u6d41\u5bc6\u5ea6\u4e0b\uff0c\u9634\u6781\u7535\u89e3\u8d28\u754c\u9762\u4f1a\u4ea7\u751f\u5927\u91cf\u6c22\u6c27\u6839\u79bb\u5b50\uff08OH<sup>&#8211;<\/sup>\uff09\uff0c\u4e0eCO<sub>2<\/sub>\u5feb\u901f\u53cd\u5e94\u5f62\u6210\u78b3\u9178\u6839\u6216\u78b3\u9178\u6c22\u6839\u79bb\u5b50\u3002\u5728\u7535\u573a\u9a71\u52a8\u4e0b\uff0c\u8fd9\u4e9b\u78b3\u9178\u6839\u79bb\u5b50\u7a7f\u8fc7\u9634\u6781-\u9633\u6781\u754c\u9762\uff08\u6c34\u6eb6\u6db2\u6216\u9634\u79bb\u5b50\u4ea4\u6362\u819c\uff09\u5411\u53cd\u5e94\u5668\u7684\u9633\u6781\u4fa7\u8fc1\u79fb\uff0c\u5e76\u4e0e\u6790\u6c27\u53cd\u5e94\uff08OER\uff09\u4e2d\u5c40\u90e8\u4ea7\u751f\u7684\u8d28\u5b50\uff08H<sup>+<\/sup>\uff09\u91cd\u65b0\u7ed3\u5408\uff0c\u518d\u6b21\u5f62\u6210CO<sub>2<\/sub>\u6c14\u4f53\u3002\u8fd9\u4e9b\u4ea4\u53c9CO<sub>2<\/sub>\u6c14\u4f53\u5206\u5b50\u4e0d\u80fd\u76f4\u63a5\u7528\u4e8eCO<sub>2<\/sub>RR\uff0c\u5bfc\u81f4\u663e\u8457\u7684\u78b3\u635f\u5931\uff0c\u4ece\u800c\u964d\u4f4e\u4e86CO<sub>2<\/sub>RR\u7684\u6574\u4f53\u80fd\u6e90\u6548\u7387\u3002\u7531\u4e8eCO<sub>2<\/sub>\u6d41\u548c\u7535\u89e3\u8d28\u4e4b\u95f4\u7684\u6301\u7eed\u5316\u5b66\u53cd\u5e94\uff0c\u5f53\u4f7f\u7528\u5f3a\u78b1\u6027\u6eb6\u6db2\u65f6\uff0c\u78b3\u635f\u5931\u95ee\u9898\u66f4\u52a0\u4e25\u91cd\u3002<br \/>\n <img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-236214\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/8-1.jpg\" alt=\"\" width=\"1068\" height=\"545\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/8-1.jpg 1068w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/8-1-300x153.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/8-1-768x392.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/8-1-1024x523.jpg 1024w\" sizes=\"(max-width: 1068px) 100vw, 1068px\" \/><\/p>\n<p><strong>\u3010\u6210\u679c\u63a0\u5f71\u3011<\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c<strong>\u7f8e\u56fd\u83b1\u65af\u5927\u5b66\u6c6a\u6dcf\u7530\u6559\u6388\uff08\u901a\u8baf\u4f5c\u8005\uff09\u7b49\u4eba<\/strong>\u62a5\u9053\u4e86\u4e00\u79cd\u591a\u5b54\u56fa\u4f53\u7535\u89e3\u8d28\uff08porous solid electrolyte, PSE\uff09\u53cd\u5e94\u5668\uff0c\u4ee5\u6709\u6548\u7684\u5b9e\u73b0\u4e86\u5728CO<sub>2<\/sub>RR\u7535\u89e3\u8fc7\u7a0b\u4e2d\u4ea4\u53c9CO<sub>2<\/sub>\u7684\u9ad8\u6548\u56de\u6536\u3002\u901a\u8fc7\u5728\u9634\u6781\u548c\u9633\u6781\u4e4b\u95f4\u5f62\u6210\u53ef\u6e17\u900f\u7684\u79bb\u5b50\u4f20\u5bfc\u78fa\u5316\u805a\u5408\u7269\u7535\u89e3\u8d28\u4f5c\u4e3a\u7f13\u51b2\u5c42\uff0c\u4ea4\u53c9\u78b3\u9178\u76d0\uff08CO<sub>3<\/sub><sup>2-<\/sup>\uff09\u53ef\u4ee5\u4e0e\u9633\u6781OER\u4ea7\u751f\u7684\u8d28\u5b50\uff08H<sup>+<\/sup>\uff09\u7ed3\u5408\uff0c\u91cd\u65b0\u5f62\u6210CO<sub>2<\/sub>\u6c14\u4f53\uff0c\u540c\u65f6\u5229\u7528\u53bb\u79bb\u5b50\u6c34\u8fde\u7eed\u51b2\u6d17PSE\u7f13\u51b2\u5c42\uff0c\u53ef\u4ee5\u5f88\u5bb9\u6613\u5730\u91cd\u65b0\u6355\u83b7CO<sub>2<\/sub>\u6c14\u4f53\u4ee5\u91cd\u590d\u4f7f\u7528\uff0c\u800c\u65e0\u9700\u4e0e\u9633\u6781O2\u6df7\u5408\u3002\u6b64\u5916\uff0c\u4f5c\u8005\u4f7f\u7528\u94f6\u7eb3\u7c73\u7ebf\uff08Ag NWs\uff09\u50ac\u5316\u5242\u4f5c\u4e3a\u6a21\u578b\uff0c\u5c06CO<sub>2<\/sub>\u8fd8\u539f\u4e3aCO\uff0c\u80fd\u591f\u4ee5\u8d85\u9ad8\u7eaf\u5ea6\u5f62\u5f0f\uff08\u6c14\u4f53\u7eaf\u5ea6\u8d85\u8fc799%\uff09\u5b9e\u73b0\u56de\u6536\u7387\u9ad8\u8fbe90%\u7684\u4ea4\u53c9CO<sub>2<\/sub>\u6c14\u4f53\uff0c\u540c\u65f6\u5728200 mA cm<sup>-2<\/sup>\u7535\u6d41\u5bc6\u5ea6\u4e0b\u53ef\u4ee5\u63d0\u4f9b\u8d85\u8fc790%\u7684CO\u6cd5\u62c9\u7b2c\u6548\u7387\uff08FE\uff09\u3002\u6b64\u5916\uff0c\u4f5c\u8005\u8fd8\u8bc1\u660e\u4e86\u7528\u4e8e\u4ea4\u53c9CO2\u56de\u6536\u7684PSE\u53cd\u5e94\u5668\u53ef\u4ee5\u6210\u529f\u5730\u6269\u5c55\u5230\u4e0d\u540c\u7684CO2RR\u50ac\u5316\u5242\u548c\u4ea7\u54c1\u3002\u5c06\u8fd9\u4e9b\u56de\u6536\u7684CO<sub>2<\/sub>\u518d\u5faa\u73af\u56de\u8f93\u5165\u6d41\u4e2d\uff0c\u5728100 mA cm<sup>-2<\/sup>\u7535\u6d41\u5bc6\u5ea6\u4e0b\u83b7\u5f97\u8d85\u8fc790%\u7684\u8fde\u7eedCO<sub>2<\/sub>\u8f6c\u5316\u6548\u7387\u3002\u7814\u7a76\u6210\u679c\u4ee5\u9898\u4e3a<strong>\u201cRecovering carbon losses in CO<sub>2<\/sub> electrolysis using a solid electrolyte reactor\u201d<\/strong>\u53d1\u5e03\u5728\u56fd\u9645\u8457\u540d\u671f\u520a<em>Nature Catalysis<\/em>\u4e0a\u3002<\/p>\n<p>\u672c\u6587\u6240\u6709\u56fe\u6765\u6e90\u4e8e\u00a9 2022 Springer Nature Limited\u3002<br \/>\n <img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-236215\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/TOC.webp_.jpg\" alt=\"\" width=\"685\" height=\"367\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/TOC.webp_.jpg 685w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/TOC.webp_-300x161.jpg 300w\" sizes=\"(max-width: 685px) 100vw, 685px\" \/><br \/>\n <strong>\u3010\u6838\u5fc3\u521b\u65b0\u3011<\/strong><\/p>\n<p>1\u3001\u5229\u7528PSE\u53cd\u5e94\u5668\uff0c\u5b9e\u73b0\u4e86\u5728CO<sub>2<\/sub>RR\u7535\u89e3\u8fc7\u7a0b\u4e2d\u4ea4\u53c9CO<sub>2<\/sub>\u7684\u9ad8\u6548\u56de\u6536\uff0c\u800c\u65e0\u9700\u4e0e\u9633\u6781O<sub>2<\/sub>\u6df7\u5408\u3002<\/p>\n<p>2\u3001\u5229\u7528Ag NWs\u50ac\u5316\u5242\u5c06CO<sub>2<\/sub>\u8fd8\u539f\u4e3aCO\uff0c\u4ee5\u6c14\u4f53\u7eaf\u5ea6\u8d85\u8fc799%\u5f62\u5f0f\u5b9e\u73b0\u56de\u6536\u7387\u9ad8\u8fbe90%\u7684\u4ea4\u53c9CO<sub>2<\/sub>\u6c14\u4f53\uff0c\u540c\u65f6\u5728200 mA cm<sup>-2<\/sup>\u4e0b\u53ef\u63d0\u4f9b\u8d85\u8fc790%\u7684CO\u6cd5\u62c9\u7b2c\u6548\u7387\uff08FE\uff09\u3002<\/p>\n<p>3\u3001\u5c06\u56de\u6536\u7684CO<sub>2<\/sub>\u518d\u5faa\u73af\u56de\u8f93\u5165\u6d41\u4e2d\uff0c\u5728100 mA cm<sup>-2<\/sup>\u4e0b\u5b9e\u73b0\u4e86\u8d85\u8fc790%\u7684\u8fde\u7eedCO<sub>2<\/sub>\u8f6c\u5316\u6548\u7387<\/p>\n<p><strong>\u3010\u6570\u636e\u6982\u89c8\u3011<\/strong><\/p>\n<p><strong>\u56fe\u4e00\u3001\u9634\u79bb\u5b50MEA\u7535\u6c60\u4e2dCO<sub>2<\/sub>\u4ea4\u53c9\u73b0\u8c61\u7684\u793a\u610f\u56fe<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-236216\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/1.webp_-3.jpg\" alt=\"\" width=\"800\" height=\"449\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/1.webp_-3.jpg 800w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/1.webp_-3-300x168.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/1.webp_-3-768x431.jpg 768w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/p>\n<p><strong>\u56fe\u4e8c\u3001\u4f20\u7edfCO<sub>2<\/sub> MEA\u7535\u89e3\u69fd\u4e2d\u7684\u5927\u91cf\u78b3\u635f\u5931<\/strong><br \/>\n <img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-236217\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/2.webp_-3.jpg\" alt=\"\" width=\"800\" height=\"712\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/2.webp_-3.jpg 800w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/2.webp_-3-300x267.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/2.webp_-3-768x684.jpg 768w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/>\uff08a\uff09\u9634\u6781\u4fa7CO<sub>2<\/sub>\u6d41\u91cf\u5206\u6790\uff0c\u5176\u4e2d\u5b9eCO<sub>2<\/sub>\u6d41\u51fa\u8fdc\u5c0f\u4e8eCO<sub>2<\/sub>\u6d41\u91cf\uff0c\u4ec5\u8003\u8651CO<sub>2<\/sub>RR\u6d88\u8017\uff1b<\/p>\n<p>\uff08b\uff09\u9633\u6781\u4fa7\u7684\u603b\u6c14\u4f53\u6d41\u91cf\u5206\u6790\uff0c\u5176\u4e2d\u7535\u5316\u5b66\u8ba1\u7b97\u7684O<sub>2<\/sub>\u6d41\u91cf\u548c\u6d4b\u91cf\u7684O<sub>2<\/sub>\u6d41\u51fa\u91cf\u8fdc\u8fdc\u8d85\u8fc7\u4ea4\u53c9CO<sub>2<\/sub>\u6c14\u4f53\u6d41\u91cf\uff1b<\/p>\n<p>\uff08c\uff09CO2\u6d41\u91cf\u5206\u6790\uff0c\u663e\u793a\u4ea4\u53c9CO<sub>2<\/sub>\u548c\u8f6c\u5316\u7684CO<sub>2<\/sub>\uff0c\u52a0\u8d77\u6765\u5339\u914d\u9634\u6781\u4fa7\u7684\u603bCO<sub>2<\/sub>\u6d41\u91cf\u53d8\u5316\uff1b<\/p>\n<p>\uff08d\uff09\u4e0d\u540cCO<sub>2<\/sub>RR\u4ea7\u7269\u7684\u4ea4\u53c9CO<sub>2<\/sub>\u4e0e\u8f6c\u5316CO<sub>2<\/sub>\u7684\u6bd4\u7387\u3002<\/p>\n<p><strong>\u56fe\u4e09\u3001PSE\u53cd\u5e94\u5668\u53ca\u5176\u6c14\u4f53\u5206\u6790\u7cfb\u7edf<\/strong><br \/>\n <img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-236218\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/3.webp_-3.jpg\" alt=\"\" width=\"800\" height=\"958\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/3.webp_-3.jpg 800w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/3.webp_-3-251x300.jpg 251w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/3.webp_-3-768x920.jpg 768w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/>\uff08a\uff09PSE\u53cd\u5e94\u5668\u4e2dCO<sub>2<\/sub>RR\u7684\u793a\u610f\u56fe\u4ee5\u53ca\u901a\u8fc7\u4e0ePSE\u7f13\u51b2\u5c42\u4e2d\u7684\u8d28\u5b50\u590d\u5408\u6765\u56de\u6536\u4ea4\u53c9CO<sub>3<\/sub><sup>2-<\/sup>\u79bb\u5b50\u7684\u8fc7\u7a0b\uff1b<\/p>\n<p>\uff08b\uff09PSE\u53cd\u5e94\u5668\u4e2dCO<sub>2<\/sub>RR\u8fc7\u7a0b\u4e2dCO2\u56de\u6536\u7387\u6d4b\u91cf\u7684\u793a\u610f\u56fe\u3002<\/p>\n<p><strong>\u56fe\u56db\u3001Ag NW\u56fa\u4f53\u7535\u89e3\u8d28\u53cd\u5e94\u5668\u4e2d\u7684\u4ea4\u53c9CO<sub>2<\/sub>\u56de\u6536\u6027\u80fd<\/strong><br \/>\n <img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-236219\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/4.webp_-3.jpg\" alt=\"\" width=\"800\" height=\"1013\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/4.webp_-3.jpg 800w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/4.webp_-3-237x300.jpg 237w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/4.webp_-3-768x972.jpg 768w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/>\uff08a\uff09Ag NW\u7684SEM\u548cHRTEM\u56fe\u50cf\uff1b<\/p>\n<p>\uff08b\uff09\u56fa\u4f53\u7535\u89e3\u8d28\u53cd\u5e94\u5668\u4e2d\uff0cAg NW\u50ac\u5316\u5242\u4e0aCO<sub>2<\/sub>RR\u7684IV\u66f2\u7ebf\uff1b<\/p>\n<p>\uff08c\uff09\u56fa\u4f53\u7535\u89e3\u8d28\u53cd\u5e94\u5668\u4e2d\uff0c\u4e0d\u540c\u5de5\u4f5c\u7535\u6d41\u4e0bAg NW\u7684CO FE\uff1b<\/p>\n<p>\uff08d\uff09\u4f7f\u7528Ag NW\u7684\u56fa\u4f53\u7535\u89e3\u8d28\u53cd\u5e94\u5668\u7684CO<sub>2<\/sub>\u56de\u6536\u6027\u80fd\uff1b<\/p>\n<p>\uff08e\uff09\u4e0eGC\u6d4b\u91cf\u7684\u4ea4\u53c9CO<sub>2<\/sub>\u6216\u7406\u8bba\u8ba1\u7b97\u7684\u4ea4\u53c9CO<sub>2<\/sub>\u76f8\u6bd4\uff0c\u5728\u4e2d\u95f4\u5c42\u56de\u6536\u7684CO<sub>2<\/sub>\u7684\u6bd4\u4f8b\uff1b<\/p>\n<p>\uff08f\uff09\u6765\u81eaGC\u7684\u70ed\u5bfc\u68c0\u6d4b\u5668\u54cd\u5e94\u663e\u793aH<sub>2<\/sub>\u5cf0\u3001O<sub>2<\/sub>\u5cf0\u548cCO<sub>2<\/sub>\u5cf0\uff0c\u5176\u4e2dCO<sub>2<\/sub>\u5bf9\u5e94\u4e8e\u4e00\u7cfb\u5217\u7535\u6d41\u7684\u56de\u6536\u6c14\u4f53\u7eaf\u5ea6\u3002<\/p>\n<p><strong>\u56fe\u4e94\u3001PSE\u53cd\u5e94\u5668\u56de\u6536\u4ea4\u53c9CO<sub>2<\/sub>\u7684\u5e7f\u6cdb\u9002\u7528\u6027<\/strong><br \/>\n <img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-236220\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/5.webp_-3.jpg\" alt=\"\" width=\"800\" height=\"796\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/5.webp_-3.jpg 800w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/5.webp_-3-150x150.jpg 150w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/5.webp_-3-300x300.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/5.webp_-3-768x764.jpg 768w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/>\uff08a-c\uff09Ni-SAC\u30012D-Bi\u548cCu NPs\u7684TEM;<\/p>\n<p>\uff08d-f\uff09PSE\u53cd\u5e94\u5668\u4e0eNi-SAC\u30012D-Bi\u548cCu NPs\u7684\u7535\u6d41\u548c\u7535\u6d41\u5bc6\u5ea6\u4e0e\u7535\u6c60\u7535\u538b\uff08IV\u66f2\u7ebf\uff09\u7684\u5173\u7cfb\uff1b<\/p>\n<p>\uff08g-i\uff09CO\u3001\u7532\u9178\u76d0\u548c\u4e03\u79cd\u4e0d\u540c\u7684CO<sub>2<\/sub>RR\u4ea7\u7269FE\u5206\u522b\u5728Ni-SAC\u30012D-Bi\u548cCu NPs\u7684\u56fa\u4f53\u7535\u89e3\u8d28\u53cd\u5e94\u5668\u4e2d\u8fdb\u884c\u7535\u5316\u5b66\u6d4b\u8bd5\uff1b<\/p>\n<p>\uff08j-l\uff09\u5177\u6709Ni-SAC\u30012D-Bi\u548cCu NPs\u7684PSE\u53cd\u5e94\u5668\u7684CO<sub>2<\/sub>\u56de\u6536\u6027\u80fd\u3002<\/p>\n<p><strong>\u56fe\u516d\u3001\u8fde\u7eedCO<sub>2<\/sub>\u6c14\u4f53\u56de\u6536\u7684DI\u6c34\u5faa\u73af\u548c\u7a33\u5b9a\u6027\u6d4b\u8bd5<\/strong><br \/>\n <img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-236221\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/6.webp_-1.jpg\" alt=\"\" width=\"800\" height=\"755\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/6.webp_-1.jpg 800w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/6.webp_-1-300x283.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/6.webp_-1-768x725.jpg 768w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/>\uff08a\uff09\u7528\u4e8eCO2\u6c14\u4f53\u56de\u6536\u7684\u56fa\u4f53\u7535\u89e3\u8d28\u53cd\u5e94\u5668\u7cfb\u7edf\u7684\u56fe\u50cf\u548c\u7535\u6c60\u8fd0\u884c\u524dAg NW\u50ac\u5316\u5242\u7684SEM\u56fe\u50cf\uff1b<\/p>\n<p>\uff08b\uff09\u7535\u6c60\u5728250\u2009 mA\uff08100\u2009mA\u2009cm<sup>-2<\/sup>\uff09\u4e0b\u8fd0\u884c90\u2009 min\u540e\uff0c\u56de\u6536\u7684CO<sub>2<\/sub>\u586b\u5145\u4e86\u4e00\u4e2a100 ml\u7684\u6c14\u7403\uff1b<\/p>\n<p>\uff08c\uff09250 mA\u2009cm<sup>-2<\/sup>\u6216100\u2009mA\u2009cm<sup>-2<\/sup>\u4e0b750\u2009 h\u7684CO<sub>2<\/sub>\u56de\u6536\u7a33\u5b9a\u6027\u6d4b\u8bd5\u3002<\/p>\n<p><strong>\u56fe\u4e03\u3001\u5229\u7528\u56de\u6536\u4ea4\u53c9CO<sub>2<\/sub>\u63d0\u9ad8CO<sub>2<\/sub>\u8f6c\u5316\u7387<\/strong><br \/>\n <img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-236222\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/7.webp_.jpg\" alt=\"\" width=\"800\" height=\"591\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/7.webp_.jpg 800w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/7.webp_-300x222.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/04\/7.webp_-768x567.jpg 768w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/>\uff08a\uff09\u4f7f\u7528PSE\u53cd\u5e94\u5668CO<sub>2<\/sub>\u56de\u6536\u6280\u672f\u7684\u5b9e\u7528CO2RR\u5de5\u827a\u793a\u610f\u56fe\uff0c\u53ef\u786e\u4fdd\u6574\u4e2a\u64cd\u4f5c\u8fc7\u7a0b\u4e2d\u7684\u9ad8\u78b3\u6548\u7387\uff1b<\/p>\n<p>\uff08b\uff09\u968f\u7740\u5165\u53e3CO<sub>2<\/sub>\u6d41\u91cf\u7684\u53d8\u5316\uff0c\u56fa\u4f53\u7535\u89e3\u8d28\u7535\u6c60\u9634\u6781\u4fa7\u548c\u4e2d\u95f4\u5c42\u7684\u78b3\u5e73\u8861\u5206\u6790\uff1b<\/p>\n<p>\uff08c\uff09CO FE\u548cAg NW\u5728\u5177\u6709CO<sub>2<\/sub>\u56de\u6536\u7cfb\u7edf\u7684\u56fa\u4f53\u7535\u89e3\u8d28\u4e2d\u7684\u8fde\u7eed\u8f6c\u5316\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u542f\u793a\u3011<\/strong><\/p>\n<p>\u7efc\u4e0a\u6240\u8ff0\uff0c\u4f5c\u8005\u5c55\u793a\u4e86\u4f7f\u7528PSE\u53cd\u5e94\u5668\u8bbe\u8ba1\u6210\u529f\u56de\u6536CO<sub>2<\/sub>RR\u7535\u89e3\u8fc7\u7a0b\u4e2d\u635f\u5931\u7684CO<sub>2<\/sub>\u6c14\u4f53\uff0c\u540c\u65f6\u4fdd\u6301\u9ad8\u50ac\u5316\u6027\u80fd\u3002\u8be5\u5de5\u4f5c\u8868\u660e\u4f20\u7edf\u7535\u89e3\u69fd\u7684CO<sub>2<\/sub>\u5229\u7528\u6548\u7387\u8f83\u5dee\uff0c\u8fd9\u4f7f\u5f97\u8be5\u8fc7\u7a0b\u4e0d\u53ef\u6301\u7eed\u3002\u6dfb\u52a0\u591a\u5b54\u548c\u79bb\u5b50\u4f20\u5bfc\u56fa\u4f53\u7535\u89e3\u8d28\u7f13\u51b2\u5c42\u8bc1\u660e\u4e86\u53ef\u4ee5\u6709\u6548\u5730\u6062\u590d\u8fd9\u4e9b\u78b3\u635f\u5931\uff0c\u4ee5\u786e\u4fdd\u9ad8CO<sub>2<\/sub>\u4f7f\u7528\u6548\u7387\u3002\u8fd9\u79cd\u7b56\u7565\u907f\u514d\u4e86\u4f7f\u7528\u989d\u5916\u7684\u6c14\u4f53\u5206\u79bb\u8bbe\u5907\u6216\u5c06\u4ea4\u53c9CO<sub>2<\/sub>\u4e0e\u6742\u8d28\uff08\u5c24\u5176\u662fO<sub>2<\/sub>\uff09\u5206\u79bb\u6240\u9700\u7684\u80fd\u91cf\u3002\u672a\u6765\u7684\u7814\u7a76\u53ef\u4ee5\u8fdb\u4e00\u6b65\u6539\u8fdbPSE\u53cd\u5e94\u5668\u4e2d\u7684\u6bcf\u4e2a\u7ec4\u4ef6\uff0c\u4f7f\u5176\u5728CO<sub>2<\/sub>RR\u7535\u89e3\u8fc7\u7a0b\u4e2d\u66f4\u9002\u7528\u4e8e\u5b9e\u9645\u7684CO<sub>2<\/sub>\u56de\u6536\uff0c\u5305\u62ec\u4f18\u5316\u56fa\u4f53\u7535\u89e3\u8d28\u5c42\u7684\u539a\u5ea6\u4ee5\u6700\u5c0f\u5316ohmic\u4e0b\u964d\uff0c\u6539\u5584\u79bb\u5b50\u9634\u6781\u548c\u9633\u6781\u95f4\u6761\u4ef6\u901a\u8fc7\u8bbe\u8ba1\u4e0d\u540c\u7684\u56fa\u6001\u79bb\u5b50\u5bfc\u4f53\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"https:\/\/doi.org\/10.1038\/s41929-022-00763-w\" target=\"_blank\" rel=\"noopener\">Recovering carbon losses in CO<sub>2<\/sub> electrolysis using a solid electrolyte reactor<\/a><\/strong>. <em>Nature Catalysis<\/em>, <strong>2022<\/strong>, DOI: 10.1038\/s41929-022-00763-w.<\/p>\n<p><strong>\u56e2\u961f\u4ecb\u7ecd\uff1a<\/strong><\/p>\n<p><strong>\u83b1\u65af\u5927\u5b66\u6c6a\u6dcf\u7530\u56e2\u961f<\/strong>\u81f4\u529b\u4e8e\u5f00\u53d1\u65b0\u578b\u7535\u89e3\u6c60\u548c\u7535\u5316\u5b66\u50ac\u5316\u5242\uff0c\u4ee5\u5229\u7528\u53ef\u518d\u751f\u7535\u80fd\u5b9e\u73b0\u57fa\u7840\u71c3\u6599\u548c\u5316\u5de5\u54c1\u7684\u7eff\u8272\u5408\u6210\uff0c\u52a9\u529b\u78b3\u4e2d\u548c\u3002\u8bfe\u9898\u7ec4\u65b9\u5411\u5305\u62ec\u7535\u5316\u5b66\u4e8c\u6c27\u5316\u78b3\u5438\u6536\u548c\u8f6c\u5316\uff0c\u7535\u5316\u5b66\u5408\u6210\u9ad8\u7eaf\u5ea6\u9ad8\u6d53\u5ea6\u53cc\u6c27\u6c34\uff0c\u7eff\u8272\u6c22\u80fd\uff0c\u9502\u79bb\u5b50\u7535\u6c60\u56de\u6536\u53ca\u6c34\u5904\u7406\u3002\u81ea\u5f00\u53d1\u51fa\u7b2c\u4e00\u4ee3\u56fa\u6001\u7535\u89e3\u8d28\u53cd\u5e94\u5668\u4ee5\u6765\uff0c\u8bfe\u9898\u7ec4\u5728\u8be5\u6280\u672f\u4e0a\u5df2\u53d1\u8868\u4e00\u7bc7<em>Science<\/em>\uff0c\u4e00\u7bc7<em>Nature Energy<\/em>\uff0c\u4e24\u7bc7<em>Nature Catalysis<\/em>\uff0c\u4e00\u7bc7<em>PNAS<\/em>\u548c\u4e24\u7bc7<em>Nature Communications<\/em>\uff0c\u5f62\u6210\u4e00\u6574\u5957\u56fa\u6001\u7535\u89e3\u6c60\u6280\u672f\u4f53\u7cfb\uff0c\u5df2\u6210\u529f\u5e94\u7528\u5230\u4e8c\u6c27\u5316\u78b3\u8fd8\u539f\u5236\u5907\u9ad8\u7eaf\u5ea6\u7532\u9178\u3001\u4e59\u9178\u71c3\u6599\uff0c\u6c27\u6c14\u8fd8\u539f\u5236\u5907\u9ad8\u7eaf\u5ea6\u53cc\u6c27\u6c34\uff0c\u4e8c\u6c27\u5316\u78b3\u56de\u6536\u5229\u7528\u7b49\u3002\u8be5\u6280\u672f\u4e5f\u5f97\u5230\u9886\u57df\u5185\u5e7f\u6cdb\u5173\u6ce8\uff0c\u5df2\u6709\u4e0d\u5c11\u8bfe\u9898\u7ec4\u6210\u529f\u5c06\u5176\u5e94\u7528\u81f3\u4e0d\u540c\u53cd\u5e94\u3002<\/p>\n<p><strong>\u60f3\u4e86\u89e3\u66f4\u591a\u6c6a\u6dcf\u7530\u8bfe\u9898\u7ec4\u8bf7\u8bbf\u95eehttp:\/\/wang.rice.edu\/<\/strong><\/p>\n<p>\u672c\u6587\u7531CQR\u7f16\u8bd1\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1\uff1atougao@cailiaoren.com.<\/p>\n<p>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaokefu.<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5bfc\u8bfb\u3011 \u5229\u7528\u4e8c\u6c27\u5316\u78b3\u8fd8\u539f\u53cd\u5e94\uff08CO2RR\uff09\u5c06CO2\u7535\u5316\u5b66\u8f6c\u5316\u6210\u57fa\u672c\u7684\u5316\u5b66\u539f\u6599\u662f\u4e00\u79cd\u5728\u7f13\u89e3\u6c14\u5019\u53d8\u5316\u7684\u65b9\u6cd5\uff0c\u540c\u65f6\u50a8\u5b58\u548c\u4f7f\u7528\u53ef\u518d\u751f\u7535\u529b\u3002\u5176\u4e2d\uff0c\u50ac\u5316\u6750\u6599\u8bbe\u8ba1\u548c\u53cd\u5e94\u5668\u5de5&#8230;<\/p>\n","protected":false},"author":7770,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215,2],"tags":[3527],"class_list":["post-236213","post","type-post","status-publish","format-standard","hentry","category-jiedu","category-keji","tag-co2rr"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/236213"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/7770"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=236213"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/236213\/revisions"}],"predecessor-version":[{"id":236230,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/236213\/revisions\/236230"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=236213"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=236213"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=236213"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}