{"id":238126,"date":"2022-06-06T06:39:33","date_gmt":"2022-06-05T22:39:33","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=238126"},"modified":"2022-06-11T09:59:40","modified_gmt":"2022-06-11T01:59:40","slug":"%e7%8e%8b%e8%a8%80%e5%8d%9a%e9%9f%a9%e7%a4%bc%e5%85%83nat-energy%ef%bc%9a%e7%a2%b3%e5%8c%96%e5%90%88%e9%87%91%e7%94%b5%e6%9e%81%e6%8f%90%e5%8d%87%e9%92%99%e9%92%9b%e7%9f%bf%e7%94%b5%e6%b1%a0","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=238126","title":{"rendered":"\u738b\u8a00\u535a&#038;\u97e9\u793c\u5143Nat. Energy\uff1a\u78b3\u5316\u5408\u91d1\u7535\u6781\u63d0\u5347\u9499\u949b\u77ff\u7535\u6c60\u7a33\u5b9a\u6027"},"content":{"rendered":"<p><strong>\u4e00\u3001\u3010\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p>\u91d1\u5c5e\u5364\u5316\u7269\u9499\u949b\u77ff\u578b\u592a\u9633\u80fd\u7535\u6c60\uff08PSC\uff09\u4ee5\u5176\u4f18\u5f02\u7684\u5149\u7535\u6027\u80fd\u548c\u4f4e\u5ec9\u7684\u5236\u9020\u6210\u672c\uff0c\u5f15\u8d77\u4e86\u5b66\u672f\u754c\u548c\u5de5\u4e1a\u754c\u7684\u5e7f\u6cdb\u5173\u6ce8\u3002\u7136\u800c\uff0c PSC\u8981\u5b9e\u73b0\u5546\u4e1a\u5316\uff0c\u5fc5\u987b\u7ecf\u53d7\u4f4f\u6c27\u6c14\u3001\u6c34\u5206\u3001\u5149\u548c\u70ed\u7684\u957f\u671f\u81ea\u7136\u4fb5\u8680\u3002\u7531\u4e8e\u9499\u949b\u77ff\u6750\u6599\u3001\u7535\u8377\u4f20\u8f93\u6750\u6599\u548c\u754c\u9762\u5c42\u7684\u4f18\u5316\uff0cPSC\u7684\u8fd0\u884c\u7a33\u5b9a\u6027\u6709\u4e86\u5f88\u5927\u7684\u63d0\u9ad8\uff0c\u4f46\u5173\u952e\u529f\u80fd\u5c42\u4e4b\u4e00\u7684\u80cc\u7535\u6781\u4ecd\u5bb9\u6613\u5931\u6548\uff0c\u8fd9\u9650\u5236\u4e86\u9ad8\u6548PSC\u7684\u6574\u4f53\u8010\u4e45\u6027\u3002<\/p>\n<p>\u94f6\uff08Ag\uff09\u548c\u94dd\uff08Al\uff09\u662f\u5e38\u7528\u7684\u80cc\u7535\u6781\u3002\u7136\u800c\uff0c\u5b83\u4eec\u503e\u5411\u4e8e\u4e0e\u8fc1\u79fb\u7684\u5364\u5316\u7269\u9634\u79bb\u5b50\u53cd\u5e94\uff0c\u5f62\u6210AgI\u3001AlI<sub>3<\/sub>\uff0c\u589e\u52a0\u5668\u4ef6\u4e32\u963b\u3002\u4f7f\u7528\u91d1\uff08Au\uff09\u53ef\u6539\u5584\u4e0a\u8ff0\u95ee\u9898\uff0c\u4f46Au\u539f\u5b50\u53ef\u4ee5\u6269\u6563\u5230\u9499\u949b\u77ff\u4e2d\uff0c\u5f62\u6210\u6df1\u80fd\u7ea7Au<sub>Pb<\/sub>\u53cd\u4f4d\u7f3a\u9677\uff0c\u6210\u4e3a\u9ad8\u6548\u7684\u975e\u8f90\u5c04\u590d\u5408\u4e2d\u5fc3\u3002\u6b64\u5916\uff0c\u4f7f\u7528\u8d35\u91d1\u5c5e\u7684\u4ee3\u4ef7\u5f88\u9ad8\uff0c\u5c06\u5927\u5927\u589e\u52a0\u5236\u9020\u6210\u672c\u3002\u4e3a\u4e86\u6291\u5236\u9499\u949b\u77ff\u548c\u91d1\u5c5e\u539f\u5b50\u4e4b\u95f4\u7684\u76f8\u4e92\u4f5c\u7528\uff0c\u5f15\u5165\u8584\u7684\u963b\u9694\u5c42\uff0c\u5df2\u88ab\u62a5\u9053\u4e3a\u4e00\u79cd\u6210\u529f\u7684\u7b56\u7565\u3002\u7136\u800c\uff0c\u901a\u5e38\u7531\u53ef\u6eb6\u6db2\u52a0\u5de5\u7684\u5c0f\u5206\u5b50\u6216\u805a\u5408\u7269\u5f62\u6210\u7684\u7f13\u51b2\u5c42\u5728\u5927\u9762\u79ef\u4e0a\u96be\u4ee5\u5b9e\u73b0\u8584\u800c\u5747\u5300\u7684\u8986\u76d6\uff0c\u9499\u949b\u77ff\u6216\u91d1\u5c5e\u7535\u6781\u7684\u7ec4\u5206\u5f80\u5f80\u4f1a\u5728\u4e00\u5b9a\u65f6\u95f4\u5185\u7a7f\u900f\u8be5\u7f13\u51b2\u5c42\u3002<\/p>\n<p><strong>\u4e8c\u3001\u3010\u6210\u679c\u63a0\u5f71\u3011<\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c<strong>\u4e0a\u6d77\u4ea4\u901a\u5927\u5b66\u738b\u8a00\u535a\u52a9\u7406\u6559\u6388\u3001\u97e9\u793c\u5143\u6559\u6388<\/strong>\u8bbe\u8ba1\u4e86\u4e00\u79cd\u7531\u539f\u4f4d\u751f\u957f\u7684\u53cc\u9762\u77f3\u58a8\u70ef\u589e\u5f3a\u7684\u94dc\u954d\uff08Cu-Ni\uff09\u5408\u91d1\u590d\u5408\u7535\u6781\u3002\u5408\u91d1\u5316\u4f7fCu\u7684\u529f\u51fd\u6570\u53ef\u8c03\uff0c\u53ef\u9002\u7528\u4e8e\u6b63\u5f0f\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u3002Cu-Ni\u662f\u901a\u8fc7\u5316\u5b66\u6c14\u76f8\u6c89\u79ef\u5236\u5907\u9ad8\u8d28\u91cf\u77f3\u58a8\u70ef\u7684\u7406\u60f3\u57fa\u6750\uff0c\u5bf9\u5916\u963b\u9694\u6c34\u5206\u3001\u6c27\u6c14\uff0c\u5bf9\u5185\u6291\u5236\u9499\u949b\u77ff\u4e0e\u91d1\u5c5e\u7535\u6781\u4e4b\u95f4\u7684\u5316\u5b66\u53cd\u5e94\u3002\u4e3a\u4e86\u5c06\u590d\u5408\u7535\u6781\u4e0e\u534a\u5668\u4ef6\u94c6\u5408\u5728\u4e00\u8d77\uff0c\u4e00\u79cd\u6539\u6027\u7684\u70ed\u5851\u6027\u5171\u805a\u7269\u88ab\u7528\u4f5c\u754c\u9762\u7c98\u5408\u5c42\u3002\u7531\u6b64\u5236\u5907\u7684\u5668\u4ef6\u5b9e\u73b0\u4e8624.34%\u548c20.76%\uff08\u8ba4\u8bc1\u4e3a 20.86%\uff09\u7684\u5149\u7535\u8f6c\u6362\u6548\u7387\uff0c\u5b54\u5f84\u9762\u79ef\u5206\u522b\u4e3a0.09\u548c1.02\u2009cm<sup>2<\/sup>\u3002\u8fd9\u4e9b\u5668\u4ef6\u663e\u793a\u51fa\u4f18\u826f\u7684\u7a33\u5b9a\u6027\uff1a\u572885\u2103\u3001\u76f8\u5bf9\u6e7f\u5ea6\u4e3a85%\u7684\u6e7f\u70ed\u8bd5\u9a8c\u4e2d\uff0c\u5176\u521d\u59cb\u6548\u7387\u57281440\u5c0f\u65f6\u540e\u4ecd\u4fdd\u630197%\uff1b\u5728\u8fde\u7eed1\u4e2a\u592a\u9633\u5149\u7167\u4e0b\u7684\u6700\u5927\u529f\u7387\u70b9\u8ddf\u8e2a\u4e2d\uff0c\u5176\u521d\u59cb\u6548\u7387\u57285,000\u5c0f\u65f6\u540e\u4ecd\u4fdd\u630195%\u3002\u8be5\u8bba\u6587\u4ee5\u9898\u4e3a\u201c<strong>In situ growth of graphene on both sides of a Cu\u2013Ni alloy electrode for perovskite solar cells with improved stability\u201d<\/strong>\u53d1\u8868\u5728\u77e5\u540d\u671f\u520a<strong><em>Nature Energy<\/em><\/strong>\u4e0a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-238127\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/06\/0-e1654427253941.jpg\" alt=\"\" width=\"600\" height=\"375\" \/><\/p>\n<p>\u4e09\u3001\u3010\u6838\u5fc3\u521b\u65b0\u70b9\u3011<\/p>\n<p>1\u3001\u901a\u8fc7\u5408\u91d1\u5316\uff0c\u4f7f\u94dc\u7684\u529f\u51fd\u53ef\u8c03\uff0c\u9996\u6b21\u5c06\u94dc\u4f5c\u4e3a\u4e3b\u4f53\u7535\u6781\u6750\u6599\u5e94\u7528\u4e8e\u6b63\u5f0f\u9499\u949b\u77ff\u592a\u9633\u7535\u6c60\u4e2d\u3002<\/p>\n<p>2\u3001\u5408\u91d1\u5316\u589e\u5f3a\u4e86\u94dc\u672c\u8eab\u7684\u7535\u5316\u5b66\u7a33\u5b9a\u6027\uff0c\u6b64\u5916\uff0c\u94dc\u954d\u5408\u91d1\u53ef\u4f5c\u4e3a\u539f\u4f4d\u751f\u957f\u9ad8\u8d28\u91cf\u77f3\u58a8\u70ef\u7684\u7406\u60f3\u57fa\u5e95\u3002\u78b3\u5316\u540e\u7684\u5408\u91d1\u7535\u6781\uff0c\u5bf9\u5916\u754c\u6c34\u6c27\uff0c\u5185\u90e8\u91d1\u5c5e\u539f\u5b50\u4e0e\u5364\u7d20\u79bb\u5b50\u7684\u79fb\u52a8\u8d77\u5230\u4e86\u5f3a\u6548\u7684\u963b\u9694\u4e0e\u6291\u5236\u4f5c\u7528\u3002<\/p>\n<p>3\u3001\u4e3a\u4e86\u5c06\u590d\u5408\u7535\u6781\u4e0e\u534a\u5668\u4ef6\u94c6\u5408\uff0c\u901a\u8fc7\u70ed\u5851\u6027\u5171\u805a\u7269\u4f5c\u4e3a\u7c98\u5408\u5c42\uff0c\u5e76\u901a\u8fc7\u77f3\u58a8\u70ef\u7eb3\u7c73\u7247\u5728\u70ed\u5851\u6027\u5171\u805a\u7269\u4e2d\u5f62\u6210\u5bfc\u7535\u7f51\u7edc\uff0c\u6539\u5584\u6b27\u59c6\u63a5\u89e6\uff0c\u7531\u6b64\u5236\u5907\u7684\u5668\u4ef6\u5b9e\u73b0\u4e8624.34%\u548c20.76%\uff08\u8ba4\u8bc1\u4e3a20.86%\uff09\u7684\u529f\u7387\u8f6c\u6362\u6548\u7387\uff0c\u5b54\u5f84\u9762\u79ef\u5206\u522b\u4e3a0.09\u548c1.02\u2009cm<sup>2<\/sup>\u3002<\/p>\n<p>4\u3001\u8fd9\u4e9b\u5668\u4ef6\u663e\u793a\u51fa\u66f4\u9ad8\u7684\u7a33\u5b9a\u6027\uff1a\u572885\u2103\u548c85%\u7684\u76f8\u5bf9\u6e7f\u5ea6\u4e0b\u8fdb\u884c1440\u5c0f\u65f6\u7684\u6e7f\u70ed\u6d4b\u8bd5\u540e\uff0c\u5176\u521d\u59cb\u6548\u7387\u4ecd\u4fdd\u6301\u572897%\uff1b\u5728\u8fde\u7eed\u592a\u9633\u5149\u7167\u4e0b\uff0c\u5728\u6700\u5927\u529f\u7387\u70b9\u8ddf\u8e2a5000\u5c0f\u65f6\u540e\uff0c\u5176\u521d\u59cb\u6548\u7387\u768495%\u4fdd\u6301\u4e0d\u53d8\u3002<\/p>\n<p><strong>\u56db\u3001\u3010\u6570\u636e\u6982\u89c8\u3011<\/strong><\/p>\n<p><strong>\u56fe<\/strong><strong>1 CNG<\/strong><strong>\u590d\u5408\u7535\u6781\u77f3\u58a8\u70ef\u7684\u8d28\u91cf\u548c\u5c42\u6570\u8868\u5f81<\/strong><strong> \u00a9 2022 Springer Nature<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-238128\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/06\/1-1-e1654427270340.jpg\" alt=\"\" width=\"600\" height=\"610\" \/><\/p>\n<p>\uff08a-c\uff09CNG-5\u3001CNG-10\u548cCNG-15\u4e0a\u77f3\u58a8\u70ef\u7684\u5149\u5b66\u663e\u5fae\u955c\u56fe\u50cf\u3002<\/p>\n<p>\uff08d-f\uff09CNG-5\u3001CNG-10\u548cCNG-15\u4e0a\u77f3\u58a8\u70ef\u534a\u5cf0\u5168\u5bbd\u7684\u4e8c\u7ef4\u62c9\u66fc\u56fe\u8c31\u3002<\/p>\n<p>\uff08g-i\uff09CNG-5\u3001CNG-10\u548cCNG-15\u4e0a\u77f3\u58a8\u70ef\u7684<em>I<\/em><sub>2D<\/sub>\/<em>I<\/em><sub>G<\/sub>\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong>2 <\/strong><strong>\u5b54\u5f84\u4e3a<\/strong><strong>0.09<\/strong><strong>\u548c<\/strong><strong>1.02\u2009cm<sup>2<\/sup><\/strong><strong>\u7684<\/strong><strong>PSCs<\/strong><strong>\u7684\u7ed3\u6784\u4e0e\u6027\u80fd<\/strong><strong> \u00a9 2022 Springer Nature<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-238129\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/06\/2-1-e1654427284250.jpg\" alt=\"\" width=\"600\" height=\"695\" \/><\/p>\n<p>\uff08a\uff09CNG-10\u88c5\u7f6e\u7684\u6a2a\u622a\u9762SEM\u56fe\u50cf\u3002<\/p>\n<p>\uff08b\uff09\u6b63\u5411\u626b\u63cf\u4e0b\u5b54\u5f84\u9762\u79ef\u4e3a0.09\u2009cm<sup>2<\/sup>\u7684CNG\u548cAg\u5668\u4ef6\u7684<em>J-V<\/em>\u66f2\u7ebf\u3002<\/p>\n<p>\uff08c-d\uff091.02\u2009cm<sup>2<\/sup> CNG\u5668\u4ef6\u7684<em>J-V<\/em>\u66f2\u7ebf\u548c\u76f8\u5e94\u7684\u77ac\u6001\u5149\u7535\u538b\u7ed3\u679c\uff0c\u8be5\u5668\u4ef6\u91c7\u7528\u4e86EVA\u4e2d\u4e0d\u540c\u8d28\u91cf\u6bd4\u7684GN\u7684\u6539\u6027\u7c98\u5408\u5242\u5c42\u3002<\/p>\n<p>\uff08e-f\uff09EVA\u4e2d1.6\u2009wt%\u548c2.4\u2009wt% GN\u7684G\u5cf0\u62c9\u66fc\u56fe\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong>3 CNG<\/strong><strong>\u7535\u6781\u7684\u7a33\u5b9a\u673a\u5236<\/strong><strong> \u00a9 2022 Springer Nature<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-238130\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/06\/3-1-e1654427298489.jpg\" alt=\"\" width=\"600\" height=\"315\" \/><\/p>\n<p>\uff08a\uff09\u6e7f\u70ed\u8001\u5316\u540e\u7684Ag\u548cCNG-10\u5668\u4ef6\u7684GC-MS\u5cf0\u9762\u79ef\u3002<\/p>\n<p>\uff08b\uff09Cu\u3001Cu-Ni\u548cCNG-10\u7535\u6781\u5728NaCl\u6eb6\u6db2\uff083.5\u2009wt%\uff09\u4e2d\u7684Tafel\u66f2\u7ebf\u3002<\/p>\n<p>\uff08c-d\uff09MPP\u8001\u5316\u7684Ag\u548cCNG\u5668\u4ef6\u4e2dI<sup>&#8211;<\/sup>\u7684\u7a7a\u95f4\u5206\u5e03\u3002<\/p>\n<p>\uff08e-f\uff09MPP\u8001\u5316\u7684Ag\u548cCNG\u88c5\u7f6e\u4e2dAg<sup>&#8211;<\/sup>\u548cCu<sup>&#8211;<\/sup>\u7684\u7a7a\u95f4\u5206\u5e03\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong>4 CNG<\/strong><strong>\u7535\u6781\u5bf9\u5668\u4ef6\u7684\u7a33\u5b9a\u4f5c\u7528<\/strong> <strong>\u00a9 2022 Springer Nature<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-238131\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/06\/4-1-e1654427313607.jpg\" alt=\"\" width=\"600\" height=\"165\" \/><\/p>\n<p>\u5c01\u88c5\u7684Ag\u3001Au\u3001SG\u548cCNG-10\u5668\u4ef6\u5728MPP\u4e0b\u8fd0\u884c\u7684\u7a33\u5b9a\u6027\uff08100 mW\u2009cm<sup>\u22122<\/sup>\u73af\u5883\u6761\u4ef6\u4e0b\uff09\u3002<\/p>\n<p><strong>\u4e94\u3001\u3010\u6210\u679c\u542f\u793a\u3011<\/strong><\/p>\n<p>\u672c\u7814\u7a76\u4e3aPSC\u5f00\u53d1\u4e86\u4e00\u79cd\u590d\u5408\u7535\u6781\uff0c\u786e\u4fdd\u5728\u8bbe\u5907\u957f\u671f\u8fd0\u884c\u671f\u95f4\u9ad8\u6548\u3001\u7a33\u5b9a\u5730\u6536\u96c6\u7535\u8377\u3002\u901a\u8fc7\u4f7f\u7528Cu-Ni\u5408\u91d1\u4f5c\u4e3a\u57fa\u5e95\u6765\u7b80\u5355\u8c03\u8282WF\uff0c\u5e76\u4e14\u5728\u4e24\u4fa7\u539f\u4f4d\u751f\u957f\u77f3\u58a8\u70ef\u5c4f\u969c\u3002\u5728\u534a\u5668\u4ef6\u548cCNG\u7535\u6781\u7684\u754c\u9762\u4e0a\u8fd8\u5f15\u5165\u4e86\u4e00\u5c42\u6539\u6027\u7c98\u5408\u5242\u5c42\uff0c\u4ee5\u6539\u5584\u6b27\u59c6\u63a5\u89e6\u3002\u572885\u2103\u3001\u76f8\u5bf9\u6e7f\u5ea6\u4e3a85%\u7684\u6761\u4ef6\u4e0b\u8fdb\u884c1440\u5c0f\u65f6\u7684\u6e7f\u70ed\u8bd5\u9a8c\u540e\uff0c\u76f8\u5e94\u7684\u8bbe\u5907\u4fdd\u6301\u4e8697%\u7684\u521d\u59cb\u6548\u7387\uff0c\u5728\u8fde\u7eed1\u592a\u9633\u5149\u7167\u5c04\u4e0b\uff0c\u5728MPP\u8ddf\u8e2a5000\u5c0f\u65f6\u540e\uff0c\u4fdd\u6301\u4e8695%\u7684\u521d\u59cb\u6548\u7387\u3002\u9884\u8ba1\u8fd9\u9879\u5de5\u4f5c\u5c06\u4e3a\u9499\u949b\u77ff\u592a\u9633\u7535\u6c60\u4e2d\u7535\u6781\u53ca\u76f8\u5173\u754c\u9762\u5c42\u7684\u8bbe\u8ba1\uff0c\u63d0\u9ad8PSC\u7684\u7a33\u5b9a\u6027\u5f00\u8f9f\u65b0\u7684\u9014\u5f84\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"https:\/\/www.nature.com\/articles\/s41560-022-01038-1\" target=\"_blank\" rel=\"noopener\">In situ growth of graphene on both sides of a Cu-Ni alloy electrode for perovskite solar cells with improved stability<\/a> ( <em>Nat. Energy <\/em><strong>2022<\/strong>, DOI: 10.1038\/s41560-022-01038-1)<\/p>\n<p>\u672c\u6587\u7531\u5927\u5175\u54e5\u4f9b\u7a3f\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong>\u738b\u8a00\u535a<\/strong><\/p>\n<p>2020\u5e74\u6bd5\u4e1a\u4e8e\u4e0a\u6d77\u4ea4\u901a\u5927\u5b66\uff0c\u83b7\u5f97\u535a\u58eb\u5b66\u4f4d\u30022020\u5e74\u81f3\u4eca\u5728\u4e0a\u6d77\u4ea4\u901a\u5927\u5b66\u4efb\u52a9\u7406\u6559\u6388\uff0c\u7814\u7a76\u65b9\u5411\u4e3a\u9499\u949b\u77ff\u592a\u9633\u7535\u6c60\u3002\u5728Science\uff0cNature Energy, Nature Communications\u7b49\u56fd\u9645\u9876\u5c16\u671f\u520a\u53d1\u8868\u4e09\u5341\u4f59\u7bc7\u5b66\u672f\u8bba\u6587\uff0c\u4e3b\u6301\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u9752\u5e74\u79d1\u5b66\u57fa\u91d1\u3001\u4e2d\u56fd\u79d1\u534f\u9752\u5e74\u6258\u4e3e\u5de5\u7a0b\u3001\u4e0a\u6d77\u5e02\u9752\u5e74\u82f1\u624d\u626c\u5e06\u8ba1\u5212\u7b49\u9879\u76ee\u3002<\/p>\n<p><strong>\u97e9\u793c\u5143<\/strong><\/p>\n<p>1988\u5e74\u6bd5\u4e1a\u4e8e\u65e5\u672c\u5927\u962a\u5e9c\u7acb\u5927\u5b66\u5e94\u7528\u5316\u5b66\u4e13\u4e1a\uff0c\u5de5\u5b66\u535a\u58eb\u3002\u4e0a\u6d77\u4ea4\u901a\u5927\u5b66\u6750\u6599\u79d1\u5b66\u4e0e\u5de5\u7a0b\u5b66\u9662\u8bb2\u5e2d\u6559\u6388\u3002\u97e9\u793c\u5143\u6559\u6388\u5728\u63d0\u9ad8\u592a\u9633\u80fd\u7535\u6c60\u7684\u8f6c\u6362\u6548\u7387\u548c\u6a21\u5757\u6280\u672f\u521b\u65b0\u4e0a\u6709\u5f88\u9ad8\u7684\u9020\u8be3\u3002\u5728Science\uff0cNature\uff0cNature Energy\uff0cNature Communications\uff0cJoule\uff0cEnergy&amp;Environmental Science\u7b49\u56fd\u9645\u9876\u5c16\u671f\u520a\u4e0a\u53d1\u8868\u4e86200\u591a\u7bc7\u9ad8\u6c34\u5e73\u5b66\u672f\u8bba\u6587\uff0c\u7533\u8bf7\u4e13\u5229150\u4f59\u9879\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4e00\u3001\u3010\u5bfc\u8bfb\u3011 \u91d1\u5c5e\u5364\u5316\u7269\u9499\u949b\u77ff\u578b\u592a\u9633\u80fd\u7535\u6c60\uff08PSC\uff09\u4ee5\u5176\u4f18\u5f02\u7684\u5149\u7535\u6027\u80fd\u548c\u4f4e\u5ec9\u7684\u5236\u9020\u6210\u672c\uff0c\u5f15\u8d77\u4e86\u5b66\u672f\u754c\u548c\u5de5\u4e1a\u754c\u7684\u5e7f\u6cdb\u5173\u6ce8\u3002\u7136\u800c\uff0c PSC\u8981\u5b9e\u73b0\u5546\u4e1a\u5316\uff0c\u5fc5\u987b\u7ecf\u53d7\u4f4f\u6c27&#8230;<\/p>\n","protected":false},"author":1004,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[4868],"class_list":["post-238126","post","type-post","status-publish","format-standard","hentry","category-jiedu","tag-4868"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/238126"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/1004"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=238126"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/238126\/revisions"}],"predecessor-version":[{"id":238283,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/238126\/revisions\/238283"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=238126"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=238126"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=238126"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}