{"id":240320,"date":"2022-07-26T05:30:03","date_gmt":"2022-07-25T21:30:03","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=240320"},"modified":"2022-07-25T14:50:20","modified_gmt":"2022-07-25T06:50:20","slug":"%e5%9b%9b%e6%a0%a1%e8%81%94%e5%90%88nat-commun-%e4%b8%a8%e5%a4%a7%e8%a7%84%e6%a8%a1%e5%88%b6%e9%80%a0%e7%a3%81%e6%8e%a7%e6%8a%98%e7%ba%b8%e6%9c%ba%e5%99%a8%e4%ba%ba","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=240320","title":{"rendered":"\u56db\u6821\u8054\u5408Nat.Commun.\u4e28\u5927\u89c4\u6a21\u5236\u9020\u78c1\u63a7\u6298\u7eb8\u673a\u5668\u4eba"},"content":{"rendered":"<p>\u78c1\u63a7\u8f6f\u4f53\u673a\u5668\u4eba\u5728\u533b\u7597\u5065\u5eb7\uff0c\u53ef\u7a7f\u6234\u5668\u4ef6\u7b49\u9886\u57df\u62e5\u6709\u8f83\u5927\u7684\u5e94\u7528\u6f5c\u529b\u3002\u76ee\u524d\uff0c\u5236\u9020\u67d4\u6027\u78c1\u63a7\u8f6f\u4f53\u673a\u5668\u4eba\u7684\u65b9\u6cd5\uff0c\u4e3b\u8981\u5305\u62ec\u6a21\u677f\u6cd5\uff0c3D\u6253\u5370\u6cd5\uff0c\u6fc0\u5149\u7f16\u7a0b\u7b49\uff0c\u7136\u800c\uff0c\u73b0\u6709\u7684\u65b9\u6cd5\u5b58\u5728\u5236\u9020\u7cbe\u5ea6\u4f4e\uff0c\u5236\u9020\u8017\u65f6\u957f\u7b49\u95ee\u9898\u3002\u8fd1\u671f\uff0c\u4e2d\u5c71\u5927\u5b66\u751f\u7269\u533b\u5b66\u5de5\u7a0b\u5b66\u9662\u848b\u4e50\u4f26\u6559\u6388\u56e2\u961f\uff0c\u4e0e\u5357\u65b9\u79d1\u6280\u5927\u5b66\u90ed\u4f20\u98de\u6559\u6388\uff0c\u534e\u4e2d\u79d1\u6280\u5927\u5b66\u5434\u5fd7\u521a\u6559\u6388\u53ca\u4e2d\u56fd\u79d1\u5b66\u6280\u672f\u5927\u5b66\u738b\u67f3\u6559\u6388\u7b49\u8054\u5408\u62a5\u9053\u4e86\u78c1\u63a7\u6298\u7eb8\u673a\u5668\u4eba\u76842D-to-4D\u5927\u89c4\u6a21\u5236\u9020\u7b56\u7565\u3002\u8bba\u6587\u9996\u5148\u5c06\u5377\u5bf9\u5377\u78c1\u6027\u7eb8\u5236\u9020\u65b9\u6cd5\u4e0e\u4e2d\u56fd\u4f20\u7edf\u6298\u7eb8\u6280\u672f\u7ed3\u5408\uff0c\u89e3\u51b3\u4e86\u4e0d\u540c\u5f62\u72b6\u4e0e\u529f\u80fd\u78c1\u63a7\u6298\u7eb8\u673a\u5668\u4eba\u7684\u9ad8\u6548\u5927\u89c4\u6a21\u5236\u9020\u95ee\u9898\u3002\u78c1\u63a7\u6298\u7eb8\u8f6f\u4f53\u673a\u5668\u4eba\u7684\u51e0\u4f55\u5f62\u72b6\u3001\u78c1\u6781\u56fe\u6848\u548c\u5f62\u72b6\u53d8\u6362\u6a21\u5f0f\u662f\u5b8c\u5168\u53ef\u7f16\u7a0b\uff0c\u56e0\u6b64\uff0c\u78c1\u63a7\u6298\u7eb8\u673a\u5668\u4eba\u53ef\u5b9e\u73b0\u65e0\u7ebf\u78c1\u63a7\u6298\u53e0\uff0c\u5c55\u5f00\uff0c\u9501\u5b9a\uff0c\u53d8\u5f62\u4e0e\u8fd0\u52a8\u7684\u5404\u79cd\u529f\u80fd\u3002\u8be5\u7814\u7a76\u7ed3\u679c\u53d1\u8868\u5728\u300a\u81ea\u7136\u00b7\u901a\u8baf\u300b\u6742\u5fd7\u4e0a\uff0c\u9898\u4e3a\u201cHigh-throughput Fabrication of Soft Magneto-origami Machines\u201d\u3002<\/p>\n<ol>\n<li><b> <\/b><strong><b>\u5377\u5bf9\u63a5<\/b><\/strong><strong><b>\u5927\u89c4\u6a21\u5236\u9020\u78c1\u6027\u7eb8\u548c2D-to-4D<\/b><\/strong><strong><b>\u5236\u9020<\/b><\/strong><strong><b>\u78c1\u63a7\u6298\u7eb8\u673a\u5668\u4eba<\/b><\/strong><\/li>\n<\/ol>\n<p>\u78c1\u6027\u7eb8\u662f\u5728\u7eb8\u4e0a\u6d82\u8986\u4e00\u5c42\u78c1\u6027\u819c\u5e76\u56fa\u5316\u800c\u6210\u3002\u78c1\u6027\u819c\u7531\u53ef\u78c1\u5316\u7684\u9495\u94c1\u787c\u9897\u7c92\u548c\u7845\u6a61\u80f6\u6df7\u5408\u7ec4\u6210\u3002\u4e3a\u4e86\u5b9e\u73b0\u78c1\u6027\u7eb8\u7684\u5927\u89c4\u6a21\u5236\u9020\uff0c\u642d\u5efa\u4e86\u4e00\u4e2a\u5377\u5bf9\u5377\u5168\u81ea\u52a8\u8bbe\u5907\uff0c\u5982\u56fe1\u548c\u89c6\u98911\u6240\u793a\u3002\u5377\u5bf9\u5377\u5927\u89c4\u6a21\u5236\u9020\u78c1\u6027\u7eb8\u8fc7\u7a0b\u5982\u4e0b\uff1a\u522e\u5200\u5747\u5300\u5730\u5728\u7eb8\u4e0a\u522e\u6d82\u4e00\u5c42\u78c1\u6027\u819c\uff0c\u78c1\u6027\u819c\u5728\u901a\u8fc7\u52a0\u70ed\u88c5\u7f6e\u65f6\u88ab\u5feb\u901f\u52a0\u70ed\u56fa\u5316\uff0c\u6700\u540e\u901a\u8fc7\u6fc0\u5149\u8bbe\u5907\u5c06\u78c1\u6027\u7eb8\u5207\u5272\u6210\u9884\u5148\u8bbe\u8ba1\u76842D\u56fe\u6848\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-240322\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/Picture-6-1.png\" alt=\"\" width=\"1512\" height=\"439\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/Picture-6-1.png 1512w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/Picture-6-1-300x87.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/Picture-6-1-768x223.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/Picture-6-1-1024x297.png 1024w\" sizes=\"(max-width: 1512px) 100vw, 1512px\" \/> <\/p>\n<p>\u56fe1 \u5377\u5bf9\u5377\u5236\u9020\u78c1\u6027\u7eb8\uff0c\u7528\u4e8e\u6298\u53e0\u5236\u9020\u78c1\u63a7\u6298\u7eb8\u673a\u5668\u4eba<\/p>\n<p>\u5377\u5bf9\u5377\u5236\u9020\u89c6\u9891\uff1ahttps:\/\/v.qq.com\/x\/page\/z3348ysxwcg.html<\/p>\n<p>2D-to-4D\u5236\u9020\u78c1\u63a7\u6298\u7eb8\u673a\u5668\u4eba\u8fc7\u7a0b\u5982\u4e0b\uff1a\u901a\u8fc7\u6298\u7eb8\u6280\u672f\uff0c\u5c06\u7279\u5b9a\u5f62\u72b6\u76842D\u78c1\u6027\u7eb8\u6298\u53e0\u6210\u76ee\u68073D\u6298\u7eb8\u7ed3\u6784\u3002\u8fdb\u4e00\u6b65\u5730\uff0c\u901a\u8fc7\u8109\u51b2\u5f3a\u78c1\u573a\u78c1\u5316\u6298\u53e0\u540e\u76843D\u6298\u7eb8\u673a\u5668\u4eba\uff0c\u8d4b\u4e88\u6298\u7eb8\u673a\u5668\u4eba\u78c1\u54cd\u5e94\u80fd\u529b\u30022D-to-4D\u6298\u7eb8\u5236\u9020\u7684\u5404\u5f0f\u78c1\u63a7\u6298\u7eb8\u673a\u5668\u4eba\u89c1\u56fe2\u3002\u5377\u5bf9\u5377\u78c1\u6027\u7eb8\u5236\u9020\u4e0e\u4e2d\u56fd\u4f20\u7edf\u6298\u7eb8\u6280\u672f\u7ed3\u5408\uff0c\u5b9e\u73b0\u4e86\u5927\u89c4\u6a21\u78c1\u63a7\u6298\u7eb8\u673a\u5668\u4eba\u7684\u9ad8\u6548\u5236\u9020\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-240321\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/Picture-5-2.png\" alt=\"\" width=\"1527\" height=\"476\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/Picture-5-2.png 1527w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/Picture-5-2-300x94.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/Picture-5-2-768x239.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/Picture-5-2-1024x319.png 1024w\" sizes=\"(max-width: 1527px) 100vw, 1527px\" \/><\/p>\n<p>\u56fe2 \u78c1\u6027\u7eb8\u548c\u6298\u53e0\u7684\u5404\u5f0f\u78c1\u63a7\u8f6f\u4f53\u673a\u5668\u4eba<\/p>\n<ol start=\"2\">\n<li><strong><b> \u65e0\u7ebf\u5145\u7535\u7684\u78c1\u63a7\u6298\u7eb8\u673a\u5668\u4eba<\/b><\/strong><\/li>\n<\/ol>\n<p>\u8be5\u673a\u5668\u4eba\u53ef\u4ee5\u6298\u53e0\u6210\u4e00\u4e2a\u957f\u65b9\u4f53\u7ed3\u6784\uff0c\u7528\u4e8e\u901a\u8fc7\u72ed\u5c0f\u7684\u901a\u9053\uff0c\u540c\u65f6\uff0c\u8be5\u673a\u5668\u4eba\u53ef\u4ee5\u5b9e\u73b0\u65e0\u7ebf\u5145\u7535\u7684\u529f\u80fd\uff0c\u4e3a\u4f20\u611f\u8bbe\u5907\u548c\u7535\u523a\u6fc0\u63d0\u4f9b\u80fd\u91cf\uff0c\u5982\u56fe3\u3002\u7814\u7a76\u4eba\u5458\u5728\u4e00\u4e2a\u732a\u80c3\u6a21\u578b\u4e2d\u6f14\u793a\u4e86\u673a\u5668\u4eba\u7684\u8fd0\u52a8\u3001\u5c55\u5f00\u548c\u65e0\u7ebf\u5145\u7535\u7684\u80fd\u529b\u3002\u901a\u8fc7\u78c1\u94c1\u7684\u9a71\u52a8\uff0c\u8be5\u673a\u5668\u4eba\u4ee5\u7ea61 mm\/\u79d2\u7684\u901f\u5ea6\u5728\u51f9\u51f8\u4e0d\u5e73\u7684\u8868\u9762\u4e0a\u8fd0\u52a8\u3002\u7136\u540e\uff0c\u901a\u8fc7\u65bd\u52a0\u4ea4\u53d8\u78c1\u573a\uff0c\u5145\u7535\u7535\u8def\u53ef\u4ee5\u4ea7\u751f3.3 V\u7684\u7a33\u5b9a\u7535\u538b\uff0c\u70b9\u4eaeLED\u706f\u3002\u901a\u8fc7\u52a0\u5165\u7535\u5b50\u7535\u8def\uff0c\u8d4b\u4e88\u673a\u5668\u4eba\u65e0\u7ebf\u5145\u7535\u7684\u80fd\u529b\uff0c\u4e3a\u690d\u5165\u5f0f\u7535\u5b50\u88c5\u7f6e\u7684\u4f9b\u7535\u548c\u957f\u671f\u5e94\u7528\u63d0\u4f9b\u4e86\u65b0\u7684\u601d\u8def\u3002\u00a0<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-240324\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/\u56fe\u7247-3-17.png\" alt=\"\" width=\"1515\" height=\"686\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/\u56fe\u7247-3-17.png 1515w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/\u56fe\u7247-3-17-300x136.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/\u56fe\u7247-3-17-768x348.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/\u56fe\u7247-3-17-1024x464.png 1024w\" sizes=\"(max-width: 1515px) 100vw, 1515px\" \/><\/p>\n<p>\u56fe3 \u53ef\u65e0\u7ebf\u5145\u7535\u7684\u78c1\u63a7\u6298\u7eb8\u673a\u5668\u4eba<\/p>\n<ol start=\"3\">\n<li><b> <\/b><strong><b>\u78c1\u63a7\u4eff\u751f\u6298\u7eb8\u6280\u672f\uff0c\u8ba9\u827a\u672f\u54c1\u201c\u6d3b\u201d\u8d77\u6765<\/b><\/strong><\/li>\n<\/ol>\n<p>\u57fa\u4e8e\u6298\u7eb8\u827a\u672f\u7684\u521b\u9020\u6027\uff0c\u78c1\u63a7\u6298\u7eb8\u673a\u5668\u4eba\u53ef\u4ee5\u5e94\u7528\u5728\u78c1\u54cd\u5e94\u827a\u672f\/\u5de5\u827a\u54c1\u4e2d\u3002\u5982\u56fe4\u6240\u793a\uff0c\u5728\u78c1\u573a\u9a71\u52a8\u4e0b\uff0c\u78c1\u6298\u7eb8\u8774\u8776\u6247\u52a8\u7fc5\u8180\uff0c\u78c1\u82b1\u6735\u751f\u52a8\u7684\u7efd\u653e\uff0c\u8ba9\u7eb8\u52a8\u8d77\u6765\uff0c\u8ba9\u827a\u672f\u753b\u201c\u6d3b\u201d\u8d77\u6765\u3002\u5e76\u4e14\uff0c\u5728\u9a71\u52a8\u8fc7\u7a0b\u4e2d\u53ef\u64ad\u653e\u80cc\u666f\u97f3\u4e50\uff0c\u8ba9\u6574\u4e2a\u827a\u672f\u54c1\u66f4\u52a0\u5145\u6ee1\u751f\u6c14\uff0c\u66f4\u52a0\u4f18\u7f8e\u3002\u78c1\u63a7\u6298\u7eb8\u6280\u672f\u53ef\u4f5c\u4e3a\u4e00\u79cd\u4f20\u64ad\u79d1\u5b66\u548c\u827a\u672f\u7684\u8ff7\u4eba\u5a92\u4ecb\uff0c\u5728\u535a\u7269\u9986\u548c\u5b66\u6821\u5c55\u51fa\uff0c\u5bf9\u516c\u4f17\uff0c\u5c24\u5176\u662f\u513f\u7ae5\u548c\u4e2d\u5c0f\u5b66\u5b66\u751f\u4ea7\u751f\u6559\u80b2\u5f71\u54cd\u3002<\/p>\n<p><em><i>\u00a0<img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-240323\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/\u56fe\u7247-2-23.png\" alt=\"\" width=\"970\" height=\"1078\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/\u56fe\u7247-2-23.png 970w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/\u56fe\u7247-2-23-270x300.png 270w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/\u56fe\u7247-2-23-768x854.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/07\/\u56fe\u7247-2-23-921x1024.png 921w\" sizes=\"(max-width: 970px) 100vw, 970px\" \/><\/i><\/em><\/p>\n<p>\u56fe4 \u78c1\u63a7\u6298\u7eb8\u8ba9\u753b\u201c\u6d3b\u201d\u8d77\u6765<\/p>\n<p>\u78c1\u63a7\u6298\u7eb8\u827a\u672f\u89c6\u9891\uff1ahttps:\/\/v.qq.com\/x\/page\/b3348ngnnj3.html<\/p>\n<h2><strong><b>\u56e2\u961f\u4ecb\u7ecd\uff1a<\/b><\/strong><\/h2>\n<p>\u4e2d\u5c71\u5927\u5b66\u751f\u7269\u533b\u5b66\u5de5\u7a0b\u5b66\u9662\u848b\u4e50\u4f26\u6559\u6388\uff0c\u81f4\u529b\u4e8e\u78c1\u63a7\u673a\u5668\u4eba\u4e0e\u4ecb\u5165\u5f0f\u533b\u7597\u5668\u4ef6\u7b49\u7814\u7a76\u5de5\u4f5c\uff0c\u4ee5\u7b2c\u4e00\/\u901a\u8baf\u4f5c\u8005\u5728<strong><em><i>Nat Commun,<\/i><\/em><\/strong>\u00a0<strong><em><i>Adv Sci<\/i><\/em><\/strong>, <strong><em><i>Nano Energy<\/i><\/em><\/strong>\u7b49\u53d1\u8868 SCI \u8bba\u658750\u4f59\u7bc7\uff0c\u83b7\u6388\u6743\u4e13\u522930\u4f59\u9879\u3002\u76ee\u524d\u5b9e\u9a8c\u5ba4\u62db\u6536\u533b\u7597\u4eea\u5668\u65b9\u5411\u535a\u58eb\/\u535a\u540e\/\u52a9\u7406\u6559\u6388\uff0c\u5f85\u9047\u4f18\u539a\uff0c\u6709\u610f\u8005\u8bf7\u53d1\u9001\u90ae\u4ef6\u5230<em><u><i>\u00a0<\/i><\/u><\/em><a href=\"mailto:jianglel@mails.sysu.edu.cn\"><em><u><i>jianglel@mails.sysu.edu.cn<\/i><\/u><\/em><\/a>\uff0c\u8be6\u60c5\u53ef\u8bbf\u95ee\u7f51\u9875\uff1a<a href=\"https:\/\/bme.sysu.edu.cn\/bmejiangll\/\"><u>https:\/\/bme.sysu.edu.cn\/bmejiangll\/<\/u><\/a>\u3002<\/p>\n<p>\u5357\u65b9\u79d1\u6280\u5927\u5b66\u6750\u6599\u79d1\u5b66\u4e0e\u5de5\u7a0b\u7cfb\u90ed\u4f20\u98de\u6559\u6388\uff0c\u4e3b\u8981\u4ece\u4e8b\u67d4\u6027\u7535\u5b50\u76ae\u80a4\u53ca\u4eba\u673a\u878d\u5408\u7684\u7814\u7a76\u3002\u56e2\u961f\u7814\u53d1\u4e86\u8d85\u7075\u654f\u3001\u5927\u91cf\u7a0b\u3001\u9ad8\u7ebf\u6027\u5ea6\u3001\u9ad8\u7a33\u5b9a\u6027\u7684\u7535\u5b50\u76ae\u80a4\uff08<strong><em><i>Nat. Commun<\/i><\/em><\/strong>. 2022, 13, 1317; <strong><em><i>ACS Nano<\/i><\/em><\/strong><em><i>\u00a0<\/i><\/em>2022, 16, 4338\u22124347; <strong><em><i>Sci. Bull<\/i><\/em><\/strong>. 2021, 66, 1091\u20131100; <strong><em><i>Nature Commun.<\/i><\/em><\/strong>\u00a02020, 11, 209; <strong><em><b>Adv. Mater.<\/b><\/em><\/strong><strong><b>\u00a0<\/b><\/strong>2019, 31, 1902955.\uff09\uff0c\u5b9e\u73b0\u4e86\u7535\u5b50\u5668\u4ef6\u4e0e\u751f\u7269\u7ec4\u7ec7\u7684\u7a33\u5b9a\u878d\u5408\uff08<strong><em><i>Adv. Mater.<\/i><\/em><\/strong>\u00a02022, 2200262; <strong><em><i>Nat. Mater<\/i><\/em><\/strong>. 2021, 20, 229-236; <strong><em><i>Adv. Funct. Mater.<\/i><\/em><\/strong>\u00a02020, 2001518.\uff09\uff0c\u5e76\u5f00\u53d1\u4e86\u57fa\u4e8e\u751f\u7269\u7ec4\u7ec7\u7684\u67d4\u6027\u4f20\u611f\u65b0\u6a21\u5f0f\uff08<strong><em><i>Nat. Commun. <\/i><\/em><\/strong>2021, 12, 4731\uff09\u3002<\/p>\n<p>\u534e\u4e2d\u79d1\u6280\u5927\u5b66\u673a\u68b0\u79d1\u5b66\u4e0e\u5de5\u7a0b\u5b66\u9662\u5434\u5fd7\u521a\u6559\u6388\uff0c\u957f\u671f\u4ece\u4e8b\u667a\u80fd\u8f6f\u4f53\uff0c\u8f6f\u4f53\u673a\u5668\u4eba\uff0c\u8f6f\u57fa\u6750\u5148\u8fdb\u5236\u9020\u7b49\u65b9\u9762\u7684\u7814\u7a76\u3002\u5728Nature\u96c6\u56e2\u65d7\u4e0b\u5b50\u520a<strong><em><i>Sci Rep<\/i><\/em><\/strong>\u548c\u56fd\u9645\u8457\u540d\u671f\u520a<strong><em><i>J Micromech Microeng<\/i><\/em><\/strong>\u7b49\u62c5\u4efb\u7f16\u8f91\u3002\u4e3b\u6301\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u6df1\u5733\u673a\u5668\u4eba\u57fa\u7840\u7814\u7a76\u4e2d\u5fc3\u8054\u5408\u57fa\u91d1\u91cd\u70b9\u9879\u76ee\u3001\u79d1\u6280\u90e8\u667a\u80fd\u673a\u5668\u4eba\u91cd\u70b9\u4e13\u9879\u5b50\u8bfe\u9898\u7b49\u56fd\u5bb6\u3001\u7701\u90e8\u7ea7\u9879\u76ee5\u9879\u3002\u5728<strong><em><i>Sci Robot\uff0cNat Commun\uff0cAdv Mater<\/i><\/em><\/strong>\u7b49\u56fd\u9645\u9876\u7ea7\u671f\u520a\u53d1\u8868\u8bba\u658780\u4f59\u7bc7\uff0c\u83b7\u5f97\u56fd\u5185\u5916\u53d1\u660e\u4e13\u522930\u4f59\u9879\u3002<\/p>\n<p>\u4e2d\u56fd\u79d1\u5b66\u6280\u672f\u5927\u5b66\u8fd1\u4ee3\u529b\u5b66\u7cfb\u738b\u67f3\u6559\u6388\uff0c\u4e3b\u8981\u7814\u7a76\u65b9\u5411\u662f\u8f6f\u4f53\u673a\u5668\u4e0e\u67d4\u6027\u7ed3\u6784\uff0c\u5305\u62ec\u8f6f\u6750\u6599\u529b\u5b66\uff0c\u8f6f\u4f53\u673a\u5668\u4eba\uff0c3D\u6253\u5370\u7b49\u3002\u4ee5\u7b2c\u4e00\/\u901a\u8baf\u4f5c\u8005\u5728\u56fd\u9645\u9876\u5c16\u671f\u520a\u4e0a\u53d1\u8868\u5b66\u672f\u8bba\u658719\u7bc7\uff0c\u5305\u62ec <strong><em><i>Nat Biomed Eng<\/i><\/em><\/strong>,<em><i>\u00a0<\/i><\/em><strong><em><i>Nat Commun<\/i><\/em><\/strong>\u00a0(3\u7bc7), <strong><em><i>Sci Adv<\/i><\/em><\/strong>, <strong><em><i>PNAS<\/i><\/em><\/strong>, <strong><em><i>Adv Mat<\/i><\/em><\/strong>\u7b49\u3002\u76ee\u524d\u5b9e\u9a8c\u5ba4\u62db\u6536\u8f6f\u4f53\u673a\u5668\u4eba\u65b9\u5411\u535a\u58eb\/\u535a\u540e\/\u7279\u8058\u526f\u7814\u7a76\u5458\uff0c\u5f85\u9047\u4f18\u539a\uff0c\u6709\u610f\u8005\u53d1\u90ae\u4ef6\u5230<em><u>wangliu05@ustc.edu.cn<\/u><\/em>\uff0c\u8be6\u60c5\u53ef\u8bbf\u95ee\u4e3b\u9875<a href=\"https:\/\/faculty.ustc.edu.cn\/liuwang\"><u>https:\/\/faculty.ustc.edu.cn\/liuwang<\/u><\/a>\u3002<\/p>\n<h2><strong><b>\u8bba\u6587\u4fe1\u606f\uff1a<\/b><\/strong><\/h2>\n<p>\u201cHigh-throughput Fabrication of Soft Magneto-origami Machines\u201d by Shengzhu Yi<sup>#<\/sup>, Liu Wang<sup>#<\/sup>, Zhipeng Chen<sup>#<\/sup>, Jian Wang, Xingyi Song, Pengfei Liu, Yuanxi Zhang, Qingqing Luo, Lelun Peng, Zhigang Wu*, Chuan Fei Guo*, Lelun Jiang*. 19 July 2022, Nature communications.<\/p>\n<p>DOI: https:\/\/doi.org\/10.1038\/s41467-022-31900-5<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u78c1\u63a7\u8f6f\u4f53\u673a\u5668\u4eba\u5728\u533b\u7597\u5065\u5eb7\uff0c\u53ef\u7a7f\u6234\u5668\u4ef6\u7b49\u9886\u57df\u62e5\u6709\u8f83\u5927\u7684\u5e94\u7528\u6f5c\u529b\u3002\u76ee\u524d\uff0c\u5236\u9020\u67d4\u6027\u78c1\u63a7\u8f6f\u4f53\u673a\u5668\u4eba\u7684\u65b9\u6cd5\uff0c\u4e3b\u8981\u5305\u62ec\u6a21\u677f\u6cd5\uff0c3D\u6253\u5370\u6cd5\uff0c\u6fc0\u5149\u7f16\u7a0b\u7b49\uff0c\u7136\u800c\uff0c\u73b0\u6709\u7684\u65b9\u6cd5\u5b58\u5728\u5236&#8230;<\/p>\n","protected":false},"author":35234,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-240320","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/240320"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/35234"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=240320"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/240320\/revisions"}],"predecessor-version":[{"id":240325,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/240320\/revisions\/240325"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=240320"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=240320"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=240320"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}