{"id":241318,"date":"2022-08-21T05:02:30","date_gmt":"2022-08-20T21:02:30","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=241318"},"modified":"2022-08-20T22:06:26","modified_gmt":"2022-08-20T14:06:26","slug":"%e5%8c%97%e5%b7%a5%e5%a4%a7%e9%83%91%e5%9d%a4%e7%a0%94%e7%a9%b6%e5%91%98%e5%9b%a2%e9%98%9f%e5%b7%9d%e5%a4%a7%e6%9d%a8%e7%a3%8a%e5%89%af%e6%95%99%e6%8e%88%e5%90%88%e4%bd%9c%e5%9c%a8adv-mater","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=241318","title":{"rendered":"\u5317\u5de5\u5927\u90d1\u5764\u7814\u7a76\u5458\u56e2\u961f&#038;\u5ddd\u5927\u6768\u78ca\u526f\u6559\u6388\u5408\u4f5c\u5728Adv. Mater.\uff1a\u53d1\u73b0\u5728\u591a\u6676Cu2Se\u6750\u6599\u4e2d\u7531\u6676\u754c\u7ed3\u6784\u4e3b\u5bfc\u7684\u975e\u540c\u6b65\u4e8c\u6b21\u76f8\u53d8\u884c\u4e3a"},"content":{"rendered":"<p><strong>\u5bfc\u8bfb\uff1a<\/strong><\/p>\n<p>\u56fa\u6001\u76f8\u53d8\u662f\u6750\u6599\u4e2d\u666e\u904d\u5b58\u5728\u7684\u4e00\u79cd\u7269\u7406\u73b0\u8c61\uff0c\u5176\u5728\u529f\u80fd\u6750\u6599\u9886\u57df\u4e2d\u7684\u5e94\u7528\u5341\u5206\u5e7f\u6cdb\u3002\u867d\u7136\u56fa\u6001\u76f8\u53d8\u7684\u7406\u8bba\u65e9\u5df2\u5efa\u7acb\u3002\u4f46\u662f\uff0c\u968f\u7740\u7eb3\u7c73\u6280\u672f\u548c\u7f3a\u9677\u5de5\u7a0b\u5728\u6750\u6599\u79d1\u5b66\u4e2d\u7684\u5e94\u7528\u800c\u51fa\u73b0\u4e86\u4f17\u591a\u65b0\u578b\u76f8\u53d8\u6750\u6599\uff0c\u8fd9\u4e9b\u6750\u6599\u4e2d\u5f80\u5f80\u5305\u542b\u4f17\u591a\u7684\u7f3a\u9677\u7ed3\u6784\uff0c\u5e76\u4e14\u8fd9\u4e9b\u7f3a\u9677\u7ed3\u6784\u4f1a\u5bf9\u76f8\u53d8\u4ea7\u751f\u5f71\u54cd\uff0c\u5bfc\u81f4\u5176\u53d1\u751f\u76f8\u53d8\u7684\u673a\u7406\u53d1\u751f\u6539\u53d8\u3002\u6240\u4ee5\uff0c\u7ecf\u5178\u7684\u76f8\u53d8\u7406\u8bba\u5728\u8fd9\u4e9b\u6750\u6599\u4e2d\u4e0d\u518d\u9002\u7528\u3002\u4e3a\u4e86\u80fd\u591f\u89e3\u91ca\u5176\u76f8\u53d8\u673a\u7406\u6211\u4eec\u5c31\u5fc5\u987b\u6e05\u695a\u7684\u4e86\u89e3\u5176\u76f8\u53d8\u7684\u5177\u4f53\u53d1\u751f\u8fc7\u7a0b\u3002\u7136\u800c\uff0c\u7531\u4e8e\u5176\u7ed3\u6784\u7684\u590d\u6742\u6027\uff0c\u5728\u8fc7\u53bb\u4f20\u7edf\u7684\u6d4b\u8bd5\u624b\u6bb5\uff0c\u4f8b\u5982XRD\u3001DSC\u7b49\u90fd\u53ea\u80fd\u7ed9\u51fa\u4e00\u4e2a\u5e73\u5747\u7684\u7ed3\u679c\uff0c\u90fd\u5f88\u96be\u6df1\u5165\u5230\u539f\u5b50\u5c3a\u5ea6\u6765\u8868\u5f81\u8fd9\u4e9b\u7f3a\u9677\u5468\u8fb9\u7ed3\u6784\u53d1\u751f\u76f8\u53d8\u7684\u5177\u4f53\u52a8\u6001\u8fc7\u7a0b\u3002\u6240\u4ee5\uff0c\u5982\u4f55\u7cbe\u786e\u5730\u8868\u5f81\u7f3a\u9677\u7ed3\u6784\u76f8\u53d8\u7684\u52a8\u6001\u6f14\u5316\u8fc7\u7a0b\u4ecd\u662f\u4e00\u4e2a\u96be\u9898\u3002<\/p>\n<p><strong>\u6210\u679c\u63a0\u5f71\uff1a<\/strong><\/p>\n<p>\u5728\u672c\u6587\u4e2d\uff0c\u4f5c\u8005\u4f7f\u7528\u7403\u5dee\u77eb\u6b63\u7684\u7535\u5b50\u663e\u5fae\u955c\u7ed3\u5408\u539f\u4f4d\u6280\u672f\uff0c\u5728\u539f\u5b50\u5c3a\u5ea6\u4e0a\u63a2\u7a76\u4e86\u591a\u6676Cu<sub>2<\/sub>Se\u4e2d\u7531\u4e0d\u540c\u5c3a\u5ea6\u6676\u754c\u7f3a\u9677\u7ed3\u6784\u4e3b\u5bfc\u7684\u975e\u540c\u6b65\u76f8\u53d8\u8fc7\u7a0b\u3002\u5176\u4e3b\u8981\u5b9e\u9a8c\u6570\u636e\uff1a<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-241319\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image002-9.jpg\" alt=\"\" width=\"692\" height=\"567\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image002-9.jpg 692w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image002-9-300x246.jpg 300w\" sizes=\"(max-width: 692px) 100vw, 692px\" \/> <\/p>\n<p>\u56fe1.\u5fae\u7c73\u6676\u548c\u7eb3\u7c73\u6676Cu<sub>2<\/sub>Se\u7684\u7ed3\u6784\u8868\u5f81\u548c\u76f8\u53d8\u8fc7\u7a0b\u4e2d\u7684\u539f\u4f4d\u7535\u5b66\u6d4b\u8bd5 a) \u5fae\u7c73\u6676Cu<sub>2<\/sub>Se\u7684\u6697\u573aTEM\u50cf\uff1bb)\u56fea\u4e2d\u7684\u9009\u533a\u7535\u5b50\u884d\u5c04\uff1bc)\u7eb3\u7c73\u6676Cu<sub>2<\/sub>Se\u7684\u6697\u573aTEM\u50cf\u3002d) c\u4e2d\u7eb3\u7c73\u6676\u7c92\u7684\u9ad8\u5206\u8fa8HAADF-STEM\u56fe\uff1be)\u56fed\u4e2d\u6807\u8bb0\u533a\u57df\u7684iDPC-STEM\u56fe\u50cf\uff1bf)\u539f\u4f4d\u70ed\u7535\u82af\u7247\u7684SEM\u56fe\u50cf\uff0c\u63d2\u56fe\u662f\u6d4b\u8bd5\u6837\u54c1\u3002g)\u539f\u4f4d\u6d4b\u8bd5\u76f8\u53d8\u8fc7\u7a0b\u4e2d\u5fae\u7c73\u6676\u548c\u7eb3\u7c73\u6676Cu<sub>2<\/sub>Se\u7535\u6d41\u968f\u6e29\u5ea6\u53d8\u5316\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-241320\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image004-10.jpg\" alt=\"\" width=\"692\" height=\"591\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image004-10.jpg 692w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image004-10-300x256.jpg 300w\" sizes=\"(max-width: 692px) 100vw, 692px\" \/><\/p>\n<p>\u56fe2.\u5fae\u7c73\u6676Cu<sub>2<\/sub>Se\u6676\u754c\u5904\u7684\u76f8\u53d8\u8fc7\u7a0b\u3002\u5728a) 397 K. b) 398 K. c) 399 K\u65f6Cu<sub>2<\/sub>Se\u6676\u754c\u7684HRTEM\u56fe\uff0c\u63d2\u56fe\u662f\u4e0e\u4e4b\u76f8\u5173\u7684FFT\u56fe\u50cf\uff1bd) \u5728398.4 \u76f8\u754c\u7684\u6ce2\u52a8\u8fc7\u7a0b\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-241321\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image006-11.jpg\" alt=\"\" width=\"692\" height=\"713\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image006-11.jpg 692w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image006-11-291x300.jpg 291w\" sizes=\"(max-width: 692px) 100vw, 692px\" \/><\/p>\n<p>\u56fe3. a) \u5ba4\u6e29\u4e0bCu<sub>2<\/sub>Se\u7eb3\u7c73\u591a\u6676\u7684HRTEM\u56fe\u50cf\u3002 b) a\u4e2d\u6807\u8bb0\u7684\u03b1-Cu<sub>2<\/sub>Se\u7684\u6676\u754cb1\u3001b2\u3001b3\u3001b4\u7684\u6676\u754c\uff08GB\uff09\u80fd\u91cf\u3002c-e\uff09\u5728\u52a0\u70ed\u8fc7\u7a0b\u4e2d\uff0c\u5206\u522b\u5728394 K\u3001395 K\u3001397 K\u62cd\u6444\u7684HRTEM\u56fe\u50cf\u3002 f-h\uff09\u5728\u51b7\u5374\u8fc7\u7a0b\u4e2d\uff0c\u5206\u522b\u5728392 K\u3001390 K\u3001386 K\u62cd\u6444\u7684HRTEM\u56fe\u50cf\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-241322\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image008-7.jpg\" alt=\"\" width=\"692\" height=\"638\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image008-7.jpg 692w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image008-7-300x277.jpg 300w\" sizes=\"(max-width: 692px) 100vw, 692px\" \/><\/p>\n<p>\u56fe4. a)392K\u65f6\u7eb3\u7c73\u6676Cu<sub>2<\/sub>Se\u7684HRTEM\u56fe\u50cf\u3002b-e)\u5206\u522b\u4e3aA-\u03b1\u3001A-\u03b2\u3001B-\u03b1\u3001B-\u03b2\u6807\u8bb0\u533a\u57df\u7684FFT\u56fe\u3002f)\u5728400K\u65f6Cu<sub>2<\/sub>Se\u7684HRTEM\u56fe\u50cf\uff1bg)\u56fef\u4e2d\u6807\u8bb0\u533a\u57df\u7684HRTEM\u56fe\uff1b\u5728h)xx\uff0ci)yy\uff0cj)xy\u65b9\u5411\u7684\u5e94\u529b\u5206\u6790\u3002<\/p>\n<p><strong>\u7ed3\u8bba\u548c\u610f\u4e49\uff1a<\/strong><\/p>\n<p>\u7efc\u4e0a\u6240\u8ff0\uff0c\u6211\u4eec\u7814\u7a76\u4e86\u591a\u6676Cu<sub>2<\/sub>Se\u7684\u4e8c\u6b21\u76f8\u53d8\u884c\u4e3a\uff0c\u5728\u539f\u5b50\u5c3a\u5ea6\u4e0a\u89c2\u5bdf\u4e86\u6676\u754c\u9644\u8fd1\u4e0d\u540c\u6b65\u76f8\u53d8\u7684\u52a8\u6001\u53d8\u5316\u3002\u5fae\u6676\u548c\u7eb3\u7c73Cu<sub>2<\/sub>Se\u7684\u76f8\u53d8\u884c\u4e3a\u4e0d\u540c\u7684\u539f\u56e0\u662f\u6676\u754c\u5bc6\u5ea6\u548c\u6676\u754c\u6210\u6838\u673a\u5236\u7684\u4e0d\u540c\u3002\u76f8\u53d8\u603b\u662f\u4ece\u6676\u754c\u5f00\u59cb\u53d1\u751f\u5e76\u5ef6\u4f38\u5230\u6676\u7c92\u5185\u90e8\u3002\u7531\u4e8e\u5fae\u6676Cu<sub>2<\/sub>Se\u4e2d\u7684\u6676\u754c\u5bc6\u5ea6\u76f8\u5bf9\u8f83\u4f4e\uff0c\u5b83\u4eec\u5e76\u4e0d\u5f71\u54cd\u6837\u54c1\u6574\u4f53\u7684\u76f8\u53d8\u7279\u6027\u3002\u4f46\u662f\uff0c\u5728\u5177\u6709\u9ad8\u6676\u754c\u6d53\u5ea6\u548c\u5c0f\u6676\u7c92\u5c3a\u5bf8\u7684\u7eb3\u7c73\u6676Cu<sub>2<\/sub>Se\u7cfb\u7edf\u4e2d\uff0c\u6676\u754c\u7ed3\u6784\u5728\u76f8\u53d8\u7684\u8fc7\u7a0b\u4e2d\u6709\u5341\u5206\u91cd\u8981\u7684\u4f5c\u7528\u3002\u539f\u5b50\u5c3a\u5ea6\u7684\u89c2\u6d4b\u7ed3\u5408\u7406\u8bba\u8ba1\u7b97\u8868\u660e\uff0c\u6676\u754c\u9644\u8fd1\u7684\u65b0\u76f8\u5f62\u6210\u7684\u6e29\u5ea6\u4e0e\u6676\u754c\u80fd\u91cf\u6709\u5173\u3002\u6676\u754c\u80fd\u91cf\u7684\u5dee\u5f02\u4f1a\u9020\u6210\u7eb3\u7c73\u6676\u6750\u6599\u4e2d\u9ad8\u6e29\u548c\u4f4e\u6e29\u76f8\u7684\u5171\u5b58\uff0c\u4ee5\u53ca\u5728\u6676\u7c92\u5185\u90e8\u5f62\u6210\u975e\u5747\u5300\u7684\u5e94\u53d8\u5206\u5e03\u3002\u6211\u4eec\u7684\u53d1\u73b0\u4e0d\u4ec5\u9002\u7528Cu<sub>2<\/sub>Se\u6750\u6599\uff0c\u5bf9\u7406\u89e3\u6240\u6709\u7eb3\u7c73\u591a\u6676\u4f53\u7cfb\u76f8\u53d8\u6750\u6599\u7684\u76f8\u53d8\u7269\u7406\u673a\u5236\u4e5f\u6709\u91cd\u8981\u610f\u4e49\u3002<\/p>\n<p><strong>\u6587\u7ae0\u5728\u7f51\u7ad9\u4e0a\u7684\u94fe\u63a5\u548c\u622a\u56fe\uff1a<\/strong>https:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adma.202205715<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-241323\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image010-4.jpg\" alt=\"\" width=\"619\" height=\"252\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image010-4.jpg 619w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image010-4-300x122.jpg 300w\" sizes=\"(max-width: 619px) 100vw, 619px\" \/><\/p>\n<p><strong>\u672c\u6587\u901a\u8baf\u4f5c\u8005\u7b80\u4ecb<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-241324\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image012-1.png\" alt=\"\" width=\"182\" height=\"254\" \/> <\/p>\n<p>\u90d1\u5764\uff0c\u5317\u4eac\u5de5\u4e1a\u5927\u5b66\u6750\u6599\u4e0e\u5236\u9020\u5b66\u90e8\u526f\u4e3b\u4efb\uff0c\u6559\u6388\u3001\u535a\u58eb\u751f\u5bfc\u5e08\u3002\u4ece\u4e8b\u6750\u6599\u7ed3\u6784\u7535\u5b50\u663e\u5fae\u5b66\u8868\u5f81\u65b9\u5411\u7684\u7814\u7a76\uff0c\u4ece\u5fae\u89c2\u751a\u81f3\u539f\u5b50\u5c3a\u5ea6\u7406\u89e3\u6750\u6599\u7ed3\u6784\u4e0e\u5b8f\u89c2\u7279\u6027\u7684\u5173\u8054\uff0c\u9610\u660e\u5176\u5185\u5728\u7684\u7269\u7406\u673a\u7406\u3002\u66fe\u83b72011\u5e74\u5168\u56fd\u767e\u7bc7\u4f18\u79c0\u535a\u58eb\u5b66\u4f4d\u8bba\u6587\uff0c2012\u5e74\u5165\u9009\u201c\u5317\u4eac\u5e02\u79d1\u6280\u65b0\u661f\u8ba1\u5212\u201d\uff0c2015\u5165\u9009\u5317\u4eac\u5e02\u9ad8\u5c42\u6b21\u4eba\u624d\u652f\u6301\u8ba1\u5212\u9752\u5e74\u62d4\u5c16\u4eba\u624d\uff0c2018\u5e74\u5165\u9009\u5317\u4eac\u5e02\u957f\u57ce\u5b66\u8005\uff1b\u4f5c\u4e3a\u4e3b\u8981\u5b8c\u6210\u4eba\u83b7\u5f972020\u5e74\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u4e8c\u7b49\u5956\uff0c2016\u5e74\u5317\u4eac\u5e02\u79d1\u5b66\u6280\u672f\u4e00\u7b49\u5956\uff0c2007\u5e74\u5168\u56fd\u9ad8\u7b49\u9662\u6821\u5341\u5927\u79d1\u6280\u8fdb\u5c55\u3002\u4ee5\u7b2c\u4e00\/\u901a\u8baf\u5728Nature Energy, Advanced Materials, Energy &amp; Environmental Science, Nature Communications\uff0cNano Letters\uff0cAdvanced Functional Materials, Applied Catalysis B: Environmental\u7b49\u56fd\u9645\u91cd\u8981SCI\u5b66\u672f\u671f\u520a\u53d1\u8868\u5b66\u672f\u8bba\u6587\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-241325\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/08\/image014-1.jpg\" alt=\"\" width=\"180\" height=\"212\" \/><\/p>\n<p>\u6768\u78ca\uff0c\u56db\u5ddd\u5927\u5b66\u6750\u6599\u79d1\u5b66\u4e0e\u5de5\u7a0b\u5b66\u9662\u526f\u6559\u6388\uff0c\u535a\u58eb\u751f\u5bfc\u5e08\uff0c\u56db\u5ddd\u7701\u7279\u8058\u4e13\u5bb6\u30022016\u5e748\u6708\u83b7\u6fb3\u5927\u5229\u4e9a\u6606\u58eb\u5170\u5927\u5b66\u535a\u58eb\u5b66\u4f4d\uff1b 2017\u5e749\u6708\u81f32020\u5e749\u6708\u56db\u5ddd\u5927\u5b66\u6750\u6599\u5b66\u9662\u7279\u8058\u526f\u7814\u7a76\u5458\uff0c2020\u5e7410\u6708\u81f3\u4eca\u56db\u5ddd\u5927\u5b66\u6750\u6599\u79d1\u5b66\u4e0e\u5de5\u7a0b\u5b66\u9662\u526f\u6559\u6388\u3002\u4e3b\u8981\u7814\u7a76\u9ad8\u6027\u80fd\u70ed\u7535\u6750\u6599\u7684\u7eb3\u7c73\u5316\u5408\u6210\u53ca\u8868\u5f81\u3001\u9ad8\u6027\u80fd\u5ba4\u6e29\u70ed\u7535\u6750\u6599\u548c\u67d4\u6027\u70ed\u7535\u5668\u4ef6\u3002\u81f3\u4eca\u5728Advanced Materials, Advanced Energy Materials\uff0cNano Today, Nano Energy\uff0cChemical Engineering Journal, Acta Materialia\uff0c\u7b49\u9ad8\u6c34\u5e73\u671f\u520a\u4e0a\u53d1\u8868\u8bba\u658790\u7bc7\uff0c\u5f15\u7528\u8fd15000\u6b21\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u5bfc\u8bfb\uff1a \u56fa\u6001\u76f8\u53d8\u662f\u6750\u6599\u4e2d\u666e\u904d\u5b58\u5728\u7684\u4e00\u79cd\u7269\u7406\u73b0\u8c61\uff0c\u5176\u5728\u529f\u80fd\u6750\u6599\u9886\u57df\u4e2d\u7684\u5e94\u7528\u5341\u5206\u5e7f\u6cdb\u3002\u867d\u7136\u56fa\u6001\u76f8\u53d8\u7684\u7406\u8bba\u65e9\u5df2\u5efa\u7acb\u3002\u4f46\u662f\uff0c\u968f\u7740\u7eb3\u7c73\u6280\u672f\u548c\u7f3a\u9677\u5de5\u7a0b\u5728\u6750\u6599\u79d1\u5b66\u4e2d\u7684\u5e94\u7528\u800c\u51fa&#8230;<\/p>\n","protected":false},"author":35234,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-241318","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/241318"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/35234"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=241318"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/241318\/revisions"}],"predecessor-version":[{"id":241326,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/241318\/revisions\/241326"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=241318"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=241318"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=241318"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}