{"id":242333,"date":"2022-09-17T07:20:21","date_gmt":"2022-09-16T23:20:21","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=242333"},"modified":"2022-09-16T14:44:40","modified_gmt":"2022-09-16T06:44:40","slug":"%e6%b2%b3%e5%8d%97%e5%a4%a7%e5%ad%a6%e4%b8%8e%e5%8d%8e%e4%be%a8%e5%a4%a7%e5%ad%a6%e5%90%88%e4%bd%9c%e6%8a%a5%e9%81%93%e4%ba%86%e5%85%89%e7%94%b5%e6%95%88%e7%8e%87%e8%b6%85%e8%bf%8729%e7%9a%84%e5%ae%a4","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=242333","title":{"rendered":"\u6cb3\u5357\u5927\u5b66\u4e0e\u534e\u4fa8\u5927\u5b66\u5408\u4f5c\u62a5\u9053\u4e86\u5149\u7535\u6548\u7387\u8d85\u8fc729%\u7684\u5ba4\u5185\u948c\u57fa\u67d3\u6599\u654f\u5316\u592a\u9633\u80fd\u7535\u6c60\uff01"},"content":{"rendered":"<p><strong>\u7814\u7a76\u80cc\u666f<\/strong><\/p>\n<p>\u968f\u7740\u4e16\u754c\u4eba\u53e3\u7206\u70b8\u5f0f\u589e\u52a0\u3001\u4f20\u7edf\u5316\u77f3\u80fd\u6e90\u4e0d\u65ad\u6d88\u8017\u4ee5\u53ca\u9020\u6210\u7684\u73af\u5883\u6c61\u67d3\u95ee\u9898\u4e0d\u65ad\u52a0\u5267\uff0c\u5f00\u53d1\u65b0\u578b\u53ef\u518d\u751f\u80fd\u6e90\u6210\u4e3a\u5168\u7403\u53ef\u6301\u7eed\u53d1\u5c55\u7684\u91cd\u8981\u65b9\u5411\uff0c\u5176\u4e2d\u592a\u9633\u80fd\u7531\u4e8e\u50a8\u91cf\u4e30\u5bcc\u3001\u5206\u5e03\u5730\u57df\u5e7f\u3001\u4f7f\u7528\u65e0\u6c61\u67d3\u7b49\u8bf1\u4eba\u4f18\u52bf\u4f7f\u5f97\u79d1\u7814\u4eba\u5458\u5bf9\u592a\u9633\u80fd\u8f6c\u5316\u7684\u7814\u7a76\u6295\u5165\u5927\u91cf\u7cbe\u529b\u3002\u8fd1\u51e0\u5341\u5e74\u6765\uff0c\u5c06\u592a\u9633\u80fd\u8f6c\u5316\u4e3a\u7535\u80fd\u7684\u5149\u4f0f\u5668\u4ef6\u7814\u7a76\u4e5f\u9010\u6e10\u6210\u4e3a\u5b66\u672f\u754c\u7684\u70ed\u70b9\u8bdd\u9898\uff0c\u5176\u4e2d\u4f5c\u4e3a\u7b2c\u4e09\u4ee3\u5149\u4f0f\u5668\u4ef6\u2014\u67d3\u6599\u654f\u5316\u592a\u9633\u80fd\u7535\u6c60\u7531\u4e8e\u5236\u5907\u5de5\u827a\u7b80\u5355\uff08\u4e0d\u9700\u8981\u624b\u5957\u7bb1\u3001\u84b8\u9540\u8bbe\u5907\uff09\u3001\u7eff\u8272\u73af\u4fdd\uff08\u6240\u9700\u6eb6\u5242\u4e3b\u8981\u4e3a\u9187\u6eb6\u6027\u7eff\u8272\u578b\u6eb6\u5242\uff09\u3001\u6210\u672c\u4f4e\u5ec9\u7b49\u4f18\u52bf\u4e00\u5ea6\u5728\u5149\u7535\u8f6c\u5316\u7814\u7a76\u524d\u6cbf\u5360\u636e\u4e86\u91cd\u8981\u7684\u5730\u4f4d\u3002<\/p>\n<p><strong>\u6210\u679c\u7b80\u4ecb<\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c\u6cb3\u5357\u5927\u5b66\u5149\u4f0f\u6750\u6599\u7701\u91cd\u70b9\u5b9e\u9a8c\u5ba4\u9ad8\u8dc3\u5cb3\u5c0f\u7ec4\u4e0e\u534e\u4fa8\u5927\u5b66\u5434\u5b63\u6000\u6559\u6388\u8bfe\u9898\u7ec4\u5408\u4f5c\u5c06\u8868\u9762\u5bcc\u7f9f\u57fa\u7684Mxene\u4e8c\u7ef4\u6750\u6599\u5f15\u5165\u948c\u57fa\u67d3\u6599\uff08Z907\uff09\u654f\u5316\u592a\u9633\u80fd\u7535\u6c60\u5149\u9633\u6781\uff0c\u534f\u540c\u5b9e\u73b0\u4e86\u5668\u4ef6\u67d3\u6599\u5438\u9644\u91cf\u589e\u52a0\u3001\u5149\u9633\u6781\u7f3a\u9677\u6001\u6291\u5236\u53ca\u8f7d\u6d41\u5b50\u8fc1\u79fb\u7387\u63d0\u5347\u7b49\u529f\u6548\u3002\u6700\u7ec8\uff0c\u901a\u8fc7\u5668\u4ef6\u6027\u80fd\u4f18\u5316\uff0c\u76ee\u6807\u5668\u4ef6\u57286000lux\u7684\u5ba4\u5185\u7167\u660e\u73af\u5883\u4e0b\u5b9e\u73b0\u4e8629.68%\u7684\u8f83\u597d\u6548\u7387\u3002\u6b64\u5916\uff0c\u8be5\u7b56\u7565\u540c\u6837\u53ef\u4ee5\u9002\u7528\u4e8e\u540c\u6e90\u578b\u7684\u5149\u7535\u63a2\u6d4b\u5668\u4ef6\uff0c\u76ee\u6807\u5668\u4ef6\u5c55\u73b0\u51fa1.69\u00d710<sup>11<\/sup>\u00a0jones\u7684\u8f83\u9ad8\u68c0\u6d4b\u7387\u548c0.26s\u7684\u8f83\u5feb\u5e73\u5747\u54cd\u5e94\u65f6\u95f4\u3002\u672c\u7814\u7a76\u5de5\u4f5c\u4e3a\u6784\u7b51\u9ad8\u6548\u7684\u67d3\u6599\u654f\u5316\u592a\u9633\u80fd\u7535\u6c60\u548c\u884d\u751f\u7684\u6709\u673a\u5149\u7535\u5668\u4ef6\u63d0\u4f9b\u4e86\u4e00\u79cd\u7b80\u5355\u4e14\u9ad8\u6548\u7684\u7b56\u7565\u3002<\/p>\n<p><strong>\u56fe\u6587\u5bfc\u8bfb<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-242339\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/09\/\u5ba3\u4f20\u7a3f\u4ef6-ACS-AMI280-1.png\" alt=\"\" width=\"383\" height=\"226\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/09\/\u5ba3\u4f20\u7a3f\u4ef6-ACS-AMI280-1.png 383w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/09\/\u5ba3\u4f20\u7a3f\u4ef6-ACS-AMI280-1-300x177.png 300w\" sizes=\"(max-width: 383px) 100vw, 383px\" \/> <\/p>\n<p>\u56fe1. \u67d3\u6599\u654f\u5316\u592a\u9633\u80fd\u7535\u6c60\u5668\u4ef6\u7684\u7ed3\u6784\u548c\u5236\u5907\u8fc7\u7a0b<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-242340\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/09\/\u5ba3\u4f20\u7a3f\u4ef6-ACS-AMI307-1.png\" alt=\"\" width=\"362\" height=\"274\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/09\/\u5ba3\u4f20\u7a3f\u4ef6-ACS-AMI307-1.png 362w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/09\/\u5ba3\u4f20\u7a3f\u4ef6-ACS-AMI307-1-300x227.png 300w\" sizes=\"(max-width: 362px) 100vw, 362px\" \/><\/p>\n<p>\u56fe2. \u67d3\u6599\u654f\u5316\u592a\u9633\u80fd\u7535\u6c60\u5668\u4ef6\u6027\u80fd<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-242341\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/09\/\u5ba3\u4f20\u7a3f\u4ef6-ACS-AMI327-1.png\" alt=\"\" width=\"378\" height=\"285\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/09\/\u5ba3\u4f20\u7a3f\u4ef6-ACS-AMI327-1.png 378w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/09\/\u5ba3\u4f20\u7a3f\u4ef6-ACS-AMI327-1-300x226.png 300w\" sizes=\"(max-width: 378px) 100vw, 378px\" \/><\/p>\n<p>\u56fe3. Z907\u540c\u6e90\u63a2\u6d4b\u5668\u5668\u4ef6\u6027\u80fd<\/p>\n<p><strong>\u6587\u732e\u4fe1\u606f<\/strong><\/p>\n<p>\u4e0a\u8ff0\u5de5\u4f5c\u4ee5&#8221;Holistically optimizing charge carrier dynamics enables high performance Z907-based dye-sensitized solar cells and photodetectors&#8221;\u4e3a\u9898\u53d1\u8868\u5728\u671f\u520a<em>ACS Applied Materials &amp; Interfaces<\/em>\uff0c\u8bba\u6587\u94fe\u63a5\u4e3a<a href=\"https:\/\/pubs.acs.org\/doi\/10.1021\/acsami.2c13009\"><u>https:\/\/pubs.acs.org\/doi\/10.1021\/acsami.2c13009<\/u><\/a>\u3002<\/p>\n<p>\u6cb3\u5357\u5927\u5b66\u7855\u58eb\u7814\u7a76\u751f\u4f55\u76db\u534e\u4e3a\u8bba\u6587\u7b2c\u4e00\u4f5c\u8005\uff0c\u6cb3\u5357\u5927\u5b66\u9ad8\u8dc3\u5cb3\u4e3a\u8be5\u8bba\u6587\u7b2c\u4e00\u901a\u8baf\u4f5c\u8005\uff0c\u6cb3\u5357\u5927\u5b66\u5cb3\u6839\u7530\u526f\u6559\u6388\u3001\u8c2d\u4ed8\u745e\u6559\u6388\u548c\u534e\u4fa8\u5927\u5b66\u5434\u5b63\u6000\u6559\u6388\u4e3a\u8bba\u6587\u5171\u540c\u901a\u8baf\u4f5c\u8005\u3002\u6b64\u5916\uff0c\u8be5\u5de5\u4f5c\u540c\u65f6\u53d7\u5230\u91cd\u5e86\u5927\u5b66\u9648\u59d7\u59d7\u8001\u5e08\u7684\u6307\u5bfc\u3002\u7814\u7a76\u5de5\u4f5c\u4e3b\u8981\u7531\u6cb3\u5357\u7701\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u7b49\u8d44\u52a9\u3001\u6cb3\u5357\u7701\u7814\u7a76\u751f\u82f1\u624d\u9879\u76ee\u8d44\u52a9\u3002<\/p>\n<p><strong>\u5ef6\u4f38\u9605\u8bfb<\/strong><\/p>\n<p>\u9ad8\u8dc3\u5cb3<\/p>\n<p>\u6cb3\u5357\u5927\u5b66\u5149\u4f0f\u6750\u6599\u7701\u91cd\u70b9\u5b9e\u9a8c\u5ba4\u7814\u7a76\u5458\uff0c\u7855\u58eb\u751f\u5bfc\u5e08\uff0c\u6bd5\u4e1a\u4e8e\u54c8\u5c14\u6ee8\u5de5\u4e1a\u5927\u5b66\uff0c\u5e08\u4ece\u5f20\u52c7\u7814\u7a76\u5458\/\u6768\u7389\u6797\u6559\u6388\uff0c\u4e3b\u8981\u7814\u7a76\u65b9\u5411\u4e3a\u6709\u673a\u592a\u9633\u80fd\u7535\u6c60\u3001\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u3001\u67d3\u6599\u654f\u5316\u592a\u9633\u80fd\u7535\u6c60\u3002\u76ee\u524d\u4ee5\u7b2c\u4e00\u6216\u901a\u8baf\u4f5c\u8005\u5728Nano Energy\uff0cSmall\uff0cJournal of Materials Chemistry A\uff0cACS Applied Materials&amp;Interfaces\uff0cSolar RRL\uff0cMacromolecules\u7b49\u56fd\u9645SCI\u671f\u520a\u53d1\u8868\u8bba\u6587\u8fd120\u7bc7\uff1b\u7533\u8bf7\u56fd\u5bb6\u53d1\u660e\u4e13\u522910\u9879\uff0c\u6388\u67438\u9879\uff1b\u4e3b\u6301\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u3001\u56fd\u5bb6\u535a\u58eb\u540e\u9762\u4e0a\u57fa\u91d1\u3001\u6cb3\u5357\u7701\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u7b49\u9879\u76ee5\u9879\u3002<\/p>\n<p>\u4f55\u76db\u534e<\/p>\n<p>\u6cb3\u5357\u5927\u5b66\u5149\u4f0f\u6750\u6599\u7701\u91cd\u70b9\u5b9e\u9a8c\u5ba4\u5b66\u751f\uff0c\u7855\u58eb\u4e09\u5e74\u7ea7\uff0c\u5e08\u4ece\u9ad8\u8dc3\u5cb3\u7814\u7a76\u5458\uff0c\u4e3b\u8981\u7814\u7a76\u65b9\u5411\u4e3a\u67d3\u6599\u654f\u5316\u592a\u9633\u80fd\u7535\u6c60\u754c\u9762\u4f18\u5316\u53ca\u67d3\u6599\u8bbe\u8ba1\u5408\u6210\u7814\u7a76\u3001\u5168\u65e0\u673a\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u6027\u80fd\u7814\u7a76\u3002\u76ee\u524d\u4ee5\u7b2c\u4e00\u4f5c\u8005\u6216\u5171\u540c\u4e00\u4f5c\u5728ACS Applied Materials&amp;Interfaces\uff0cSolar RRL\uff0cJournal of Alloys and Compounds\u53d1\u8868SCI\u671f\u520a3\u7bc7\u6587\u7ae0\uff0c\u4e3b\u6301\u6cb3\u5357\u5927\u5b66\u7814\u7a76\u751f\u82f1\u624d\u9879\u76ee\u4e00\u9879\uff0c\u6388\u6743\u53d1\u660e\u4e13\u52291\u9879\uff0c\u53c2\u52a0\u56fd\u5185\u592a\u9633\u80fd\u7535\u6c60\u4f1a\u8bae2\u6b21\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u7814\u7a76\u80cc\u666f \u968f\u7740\u4e16\u754c\u4eba\u53e3\u7206\u70b8\u5f0f\u589e\u52a0\u3001\u4f20\u7edf\u5316\u77f3\u80fd\u6e90\u4e0d\u65ad\u6d88\u8017\u4ee5\u53ca\u9020\u6210\u7684\u73af\u5883\u6c61\u67d3\u95ee\u9898\u4e0d\u65ad\u52a0\u5267\uff0c\u5f00\u53d1\u65b0\u578b\u53ef\u518d\u751f\u80fd\u6e90\u6210\u4e3a\u5168\u7403\u53ef\u6301\u7eed\u53d1\u5c55\u7684\u91cd\u8981\u65b9\u5411\uff0c\u5176\u4e2d\u592a\u9633\u80fd\u7531\u4e8e\u50a8\u91cf\u4e30\u5bcc\u3001\u5206&#8230;<\/p>\n","protected":false},"author":35234,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-242333","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/242333"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/35234"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=242333"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/242333\/revisions"}],"predecessor-version":[{"id":242342,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/242333\/revisions\/242342"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=242333"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=242333"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=242333"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}