{"id":243443,"date":"2022-10-20T06:38:22","date_gmt":"2022-10-19T22:38:22","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=243443"},"modified":"2022-10-19T21:39:06","modified_gmt":"2022-10-19T13:39:06","slug":"%e6%b8%85%e5%8d%8e%e4%ba%8e%e6%b5%a6%e5%9b%a2%e9%98%9f%e5%ae%9e%e7%8e%b0%e7%ba%b3%e7%b1%b3%e5%b0%ba%e5%ba%a6%e4%b8%8a%e7%bb%9d%e7%bc%98%e4%bd%93-%e9%87%91%e5%b1%9e%e7%9b%b8%e5%8f%98%e7%9a%84","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=243443","title":{"rendered":"\u6e05\u534e\u4e8e\u6d66\u56e2\u961f\u5b9e\u73b0\u7eb3\u7c73\u5c3a\u5ea6\u4e0a\u7edd\u7f18\u4f53\u2014\u91d1\u5c5e\u76f8\u53d8\u7684\u8c03\u63a7"},"content":{"rendered":"<p><strong>\u3010\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p>\u5f3a\u5173\u8054\u6c27\u5316\u7269\u6750\u6599\u5177\u6709\u4f17\u591a\u6709\u8da3\u7684\u7269\u7406\u6027\u8d28\uff0c\u7edd\u7f18\u4f53-\u91d1\u5c5e\u76f8\u53d8\u5c31\u662f\u5176\u4e2d\u4e4b\u4e00\u3002\u5728\u7edd\u7f18\u4f53-\u91d1\u5c5e\u76f8\u53d8\uff08IMT\uff09\u4e2d\uff0c\u7535\u5bfc\u7387\u4f1a\u56e0\u4e3a\u5916\u754c\u523a\u6fc0\u800c\u53d1\u751f\u7edd\u7f18\u4f53-\u91d1\u5c5e\u8f6c\u53d8\u6025\u5267\u53d8\u5316\uff0c\u8fd9\u4e00\u73b0\u8c61\u5728\u8fc7\u53bb\u51e0\u5341\u5e74\u91cc\u5907\u53d7\u5173\u6ce8\u3002\u901a\u8fc7\u7535\u573a\u64cd\u7eb5IMT\u5728\u591a\u529f\u80fd\u5668\u4ef6\u4e2d\u6709\u7740\u5e7f\u9614\u7684\u5e94\u7528\u524d\u666f\uff0c\u4f8b\u5982\u5b58\u50a8\u5668\u3001\u667a\u80fd\u7a97\u53e3\u3001\u5149\u5b66\u8c03\u5236\u5668\u3001\u963b\u53d8\u5668\u4ef6\u7b49\u3002\u6700\u8fd1\u7684\u7814\u7a76\u8868\u660e\uff0c\u7535\u573a\u63a7\u5236\u7684\u79bb\u5b50\u6f14\u53d8\u53ef\u4f5c\u4e3a\u5b9e\u73b0IMT\u7684\u7b80\u5355\u4e14\u6709\u6548\u7684\u9014\u5f84\u3002\u800c\u5728\u8fd9\u4e9b\u7814\u7a76\u4e2d\uff0c\u6c22\u4f5c\u4e3a\u6700\u5c0f\u548c\u6700\u8f7b\u7684\u63ba\u6742\u5143\u7d20\uff0c\u8868\u73b0\u51fa\u4e86\u7535\u573a\u9a71\u52a8\u4e0b\u8fc1\u79fb\u5feb\u3001\u8c03\u63a7\u80fd\u529b\u5f3a\u7b49\u7279\u70b9\uff0c\u88ab\u5e7f\u6cdb\u5e94\u7528\u4e8e\u7535\u573a\u8bf1\u5bfc\u7684\u6750\u6599\u7269\u6027\u8c03\u63a7\u5f53\u4e2d\u3002\u901a\u8fc7\u7535\u573a\u9a71\u52a8\u4e0b\u6750\u6599\u4e2d\u6c22\u79bb\u5b50\u7684\u5d4c\u5165\u548c\u6790\u51fa\uff0c\u83b7\u5f97\u4e86\u78c1\u6027\u8c03\u63a7\u3001\u8d85\u5bfc\u589e\u5f3a\u548c\u7edd\u7f18\u4f53\u2014\u91d1\u5c5e\u76f8\u53d8\u7b49\u4e00\u7cfb\u5217\u6709\u8da3\u7269\u6027\u3002\u4e3a\u4e86\u4fc3\u8fdb\u6837\u54c1\u6c22\u5316\uff0c\u901a\u5e38\u9700\u8981\u4f7f\u7528\u6db2\u4f53\u6216\u56fa\u4f53\u7535\u89e3\u8d28\u7684\u7535\u573a\u95e8\u63a7\uff08gating\uff09\u6280\u672f\uff0c\u4ee5\u5c06\u8d28\u5b50\u5f15\u5165\u6837\u54c1\u6765\u89e6\u53d1\u7ed3\u6784\u8f6c\u53d8\u548cIMT\u3002\u7136\u800c\uff0c\u8fd9\u79cd\u65b9\u6cd5\u901a\u5e38\u6d89\u53ca\u590d\u6742\u7684\u5668\u4ef6\u7ed3\u6784\u548c\u96be\u4ee5\u6349\u6478\u7684\u7535\u5316\u5b66\u53cd\u5e94\uff0c\u8fd9\u7ed9\u5177\u6709\u7eb3\u7c73\u5c3a\u5ea6\u53ef\u8c03\u8c10\u529f\u80fd\u7684\u5668\u4ef6\u5fae\u578b\u5316\u5e26\u6765\u4e86\u6781\u5927\u7684\u6280\u672f\u6311\u6218\u3002\u800c\u6709\u6548\u5b9e\u73b0\u6c22\u5316\u7684\u53e6\u4e00\u79cd\u9014\u5f84\u5219\u662f\u4f7f\u7528\u94c2\u50ac\u5316\u5242\u8f85\u52a9\u7684\u6c22\u5316\u4f5c\u7528\u3002\u5c3d\u7ba1\u8fd9\u79cd\u65b9\u6cd5\u53ef\u4ee5\u7528\u4e8e\u7eb3\u7c73\u7ea7\u7684\u6c22\u5316\u5de5\u7a0b\uff0c\u4f46\u5728\u5b9e\u8df5\u4e2d\u7f3a\u4e4f\u53ef\u63a7\u6027\u3002\u603b\u7684\u6765\u8bf4\uff0c\u4f20\u7edf\u79bb\u5b50\u8c03\u63a7\u7b56\u7565\u9762\u4e34\u7740\u96be\u4ee5\u5728\u7eb3\u7c73\u5c3a\u5ea6\u5b9e\u73b0\u6709\u6548\u64cd\u63a7\u548c\u8c03\u63a7\u65f6\u95f4\u957f\u7b49\u56f0\u5883\uff0c\u5236\u7ea6\u4e86\u76f8\u5e94\u7684\u529f\u80fd\u5e94\u7528\u63a2\u7d22\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u63a0\u5f71\u3011<\/strong><\/p>\n<p>\u8fd1\u671f\uff0c<strong>\u6e05\u534e\u5927\u5b66\u4e8e\u6d66\u6559\u6388<\/strong>\uff08\u901a\u8baf\u4f5c\u8005\uff09\u7b49\u4eba\u4f7f\u7528\u626b\u63cf\u63a2\u9488\u663e\u5fae\u6280\u672f\uff0c\u5b9e\u73b0\u4e86\u7eb3\u7c73\u5c3a\u5ea6\u6c22\u5316\u7684\u53ef\u9006\u7535\u573a\u8c03\u63a7\u3002\u5728\u8fd9\u4e00\u8fc7\u7a0b\u4e2d\uff0c\u9540\u94c2\u7eb3\u7c73\u63a2\u9488\u4f5c\u4e3a\u5177\u6709\u6c22\u50ac\u5316\u6d3b\u6027\u7684\u50ac\u5316\u5242\u53ef\u5206\u89e3\u6c14\u4f53\u6c1b\u56f4\u4e2d\u7684\u6c22\u5206\u5b50\u5f62\u6210\u6c22\u79bb\u5b50\uff0c\u968f\u4e4b\u65bd\u52a0\u7684\u6b63\u5411\u504f\u538b\u5219\u53ef\u5728\u9488\u5c16\u548c\u6837\u54c1\u8868\u9762\u4e4b\u95f4\u52a0\u901f\u6c22\u79bb\u5b50\uff0c\u4f7f\u5176\u6ce8\u5165VO<sub>2<\/sub>\u8584\u819c\uff0c\u4ece\u800c\u4f7f\u5f97\u7edd\u7f18VO<sub>2<\/sub>\u8f6c\u53d8\u4e3a\u975e\u6613\u5931\u5bfc\u7535\u7684H<em><sub>x<\/sub><\/em>VO<sub>2<\/sub>\uff1b\u800c\u5f53\u65bd\u52a0\u8d1f\u5411\u504f\u538b\u65f6\u5219\u53ef\u4ee5\u89e6\u53d1\u8131\u6c22\u53cd\u5e94\uff0c\u4f7f\u6837\u54c1\u91cd\u65b0\u6062\u590d\u7edd\u7f18\u6001\uff0c\u8fdb\u800c\u5b8c\u6574\u5730\u5b9e\u73b0\u4e86\u7535\u573a\u4f5c\u7528\u4e0b\u7684\u53ef\u9006\u6c22\u5316\u548c\u7edd\u7f18\u4f53\u2014\u91d1\u5c5e\u76f8\u53d8\u3002\u8fd9\u9879\u5de5\u4f5c\u901a\u8fc7\u6c22\u6f14\u5316\u5c55\u793a\u4e86\u7535\u573a\u63a7\u5236\u4e0b\u5c40\u90e8\u3001\u53ef\u9006\u7684\u7edd\u7f18\u4f53-\u91d1\u5c5e\u76f8\u53d8\uff0c\u6709\u671b\u4e3a\u5728\u7eb3\u7c73\u5c3a\u5ea6\u5f00\u53d1\u591a\u529f\u80fd\u5668\u4ef6\u63d0\u4f9b\u5f3a\u5927\u7684\u591a\u6837\u5316\u5e73\u53f0\u3002\u8be5\u6587\u7b2c\u4e00\u4f5c\u8005\u4e3a\u6e05\u534e\u5927\u5b66\u7269\u7406\u7cfb\u535a\u58eb\u540e\u674e\u73b2\u9f99\uff08\u5165\u9009\u201c\u535a\u58eb\u540e\u521b\u65b0\u4eba\u624d\u652f\u6301\u8ba1\u5212\u201d\uff0c\u73b0\u5165\u804c\u4e1c\u5357\u5927\u5b66\u7269\u7406\u5b66\u9662\uff09\uff0c\u6587\u7ae0\u4ee5\u9898\u4e3a<strong>\u201cManipulating the insulator\u2013metal transition through tip-induced hydrogenation\u201d<\/strong>\u53d1\u5e03\u5728\u56fd\u9645\u8457\u540d\u671f\u520a<strong><em>Nature Materials<\/em><\/strong>\u4e0a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-243448\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/10\/\u9898\u56fe-1.jpg\" alt=\"\" width=\"600\" height=\"265\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/10\/\u9898\u56fe-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/10\/\u9898\u56fe-1-300x133.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u3010\u6838\u5fc3\u521b\u65b0\u70b9\u3011<\/strong><\/p>\n<p>1.\u5229\u7528\u63a2\u9488\u504f\u538b\uff0c\u6709\u6548\u5730\u964d\u4f4e\u4e86\u8d28\u5b50\u4e0e\u6c27\u5316\u7269\u95f4\u7684\u8868\u9762\u5d4c\u5165\u52bf\u5792\uff0c\u5c06\u76f8\u53d8\u901f\u5ea6\u4ece\u5b8f\u89c2\u5668\u4ef6\u7684\u5206\u949f\u91cf\u7ea7\u63d0\u9ad8\u5230\u4e86\u6beb\u79d2\u91cf\u7ea7\u3002<\/p>\n<p>2.\u5728\u7535\u573a\u4f5c\u7528\u4e0b\uff0c\u5b9e\u73b0\u4e86\u7eb3\u7c73\u5c3a\u5ea6\u7684\u6c22\u79bb\u5b50\u53ef\u9006\u8c03\u63a7\uff0c\u5e76\u6709\u671b\u5c06\u79bb\u5b50\u8c03\u63a7\u6269\u5c55\u5230\u4f17\u591a\u7684\u6c27\u5316\u7269\u3001\u4e8c\u7ef4\u6750\u6599\u3001\u8d85\u5bfc\u6750\u6599\u7b49\u4f53\u7cfb\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u89e3\u8bfb\u3011<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-243444\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/10\/1-7.jpg\" alt=\"\" width=\"600\" height=\"500\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/10\/1-7.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/10\/1-7-300x250.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>1.<\/strong> <strong>\u901a\u8fc7\u6c22\u5316\u4f5c\u7528\u5b9e\u73b0<\/strong><strong>VO<sub>2<\/sub><\/strong><strong>\u8584\u819c\u7684<\/strong><strong>IMT<\/strong><strong>\u3002<\/strong><strong>\u00a9 2022 Springer Nature Limited<\/strong><\/p>\n<p>\uff08a\uff09\u5b64\u7acb\u94c2\u9897\u7c92\u534f\u52a9\u7684\u6c22\u5316\u4f5c\u7528\u793a\u610f\u56fe\uff1b<\/p>\n<p>\uff08b\uff09\u5728Al<sub>2<\/sub>O<sub>3<\/sub>\u886c\u5e95\u884d\u5c04\u5cf0\u9644\u8fd1\u5bf9VO<sub>2<\/sub>\uff08\u84dd\u7ebf\uff09\u548c\u6c22\u5316H<em><sub>x<\/sub><\/em>VO<sub>2<\/sub>\uff08\u7ea2\u7ebf\uff09\u8fdb\u884cX\u5c04\u7ebf\u884d\u5c04\u626b\u63cf\uff1b<\/p>\n<p>\uff08c\uff09\u70ed\u5904\u7406\u524d\u540eVO<sub>2<\/sub>\u8584\u819c\u7684\u6e29\u5ea6\u4f9d\u8d56\u6027\u8868\u9762\u7535\u963b\uff1b<\/p>\n<p>\uff08d\uff09\u5728\u5ba4\u6e29\u4e0b\u5bf9\u6d4b\u5f97\u7684VO<sub>2<\/sub>\u548c\u6c22\u5316H<em><sub>x<\/sub><\/em>VO<sub>2<\/sub>\u62c9\u66fc\u5149\u8c31\u8fdb\u884c\u6bd4\u8f83\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-243445\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/10\/2-9.jpg\" alt=\"\" width=\"600\" height=\"376\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/10\/2-9.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/10\/2-9-300x188.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>2. <\/strong><strong>\u5229\u7528\u626b\u63cf\u63a2\u9488\u5728<\/strong><strong>VO<sub>2<\/sub><\/strong><strong>\u4e2d\u8fdb\u884c\u6c22\u5316\u64cd\u7eb5<\/strong><strong>\u3002<\/strong><strong>\u00a92022 Springer Nature Limited<\/strong><\/p>\n<p>\uff08a\uff09\u9488\u5c16\u8bf1\u5bfc\u6c22\u5316\u793a\u610f\u56fe\uff1b<\/p>\n<p>\uff08b\uff09\u9488\u5c16\u8bf1\u5bfc\u56fe\u6848\u5316\u7684\u6c22\u5316H<em><sub>x<\/sub><\/em>VO<sub>2<\/sub>\u533a\u57df\uff1b<\/p>\n<p>\uff08c\uff09\u9488\u5c16\u8bf1\u5bfc\u6c22\u5316\u4e2d\u6e29\u5ea6\u548c\u9488\u5c16\u7535\u538b\u7684\u4f9d\u8d56\u6027\uff1b<\/p>\n<p>\uff08d\uff09\u4e0d\u540c\u626b\u63cf\u9488\u5c16\u548c\u6c14\u6c1b\u4e2d\u7684\u9488\u5c16\u8bf1\u5bfc\u6c22\u5316\uff1b<\/p>\n<p>\uff08e\uff09\u6539\u53d8\u63a2\u9488\u7684\u626b\u63cf\u9891\u7387\u540e\u5f97\u5230\u7684\u9488\u5c16\u8bf1\u5bfc\u6c22\u5316\u7684\u8f6c\u53d8\u901f\u5ea6\u3002<\/p>\n<p><strong>\u00a0<img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-243446\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/10\/3-7.jpg\" alt=\"\" width=\"600\" height=\"456\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/10\/3-7.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/10\/3-7-300x228.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/strong><\/p>\n<p><strong>\u56fe<\/strong><strong>3. <\/strong><strong>\u9488\u5c16\u8bf1\u5bfc\u6c22\u5316\u64cd\u7eb5<\/strong><strong>IMT<\/strong><strong>\u3002<\/strong><strong>\u00a9 2022 Springer Nature Limited<\/strong><\/p>\n<p>\uff08a\uff09\u9488\u5c16\u626b\u63cf\u533a\u57df\u7684\u6c22\u6d53\u5ea6SIMS\u5206\u5e03\uff1b<\/p>\n<p>\uff08b\uff09\u9492\u79bb\u5b50\u7684\u4ef7\u6001\u6f14\u53d8\uff1b<\/p>\n<p>\uff08c\uff09\u00a0\u9488\u5c16\u5199\u5165\u533a\u57df\u7684\u7535\u6d41\u5206\u5e03\uff1b<\/p>\n<p>\uff08d\uff09\u63a2\u9488\u8bf1\u5bfc\u6c22\u5316\u524d\u540e\u6e29\u5ea6\u4f9d\u8d56\u7684\u7535\u963b\u53d8\u5316\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-243447\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/10\/4-8.jpg\" alt=\"\" width=\"600\" height=\"500\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/10\/4-8.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/10\/4-8-300x250.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>4. <\/strong><strong>\u9488\u5c16\u8bf1\u5bfc\u6c22\u5316\u7684\u53ef\u9006\u6027\u4ee5\u53ca\u7a7a\u95f4\u5206\u8fa8\u6d4b\u8bd5<\/strong><strong>\u00a0<\/strong><strong>\u3002<\/strong><strong>\u00a9 2022 Springer Nature Limited<\/strong><\/p>\n<p>\uff08a\uff09\u5229\u7528\u4e24\u79cd\u76f8\u53cd\u504f\u538b\u8fdb\u884c\u53ef\u9006\u6c22\u5316\u548c\u8131\u6c22\u8fc7\u7a0b\u540e\u7684\u7535\u6d41\u5206\u5e03\uff1b<\/p>\n<p>\uff08b\uff09\u5229\u7528AFM\u63a2\u9488\u4f5c\u4e3a\u9876\u7535\u6781\uff0c\u5728\u4e0d\u540c\u533a\u57df\u6d4b\u91cf\u5c40\u90e8<em>I<\/em>\u2013<em>V<\/em>\u66f2\u7ebf\uff1b<\/p>\n<p>\uff08c\uff09\u00a0\u5199\u5165\u7535\u538b\u4e3a10V\u65f6\uff0c\u9a6c\u8d5b\u514b\u56fe\u6848\u7684\u7535\u6d41\u5206\u5e03\uff1b<\/p>\n<p>\uff08d\uff09\u6cbf\u7740\uff08c\uff09\u4e2d\u767d\u7ebf\u7684\u7535\u6d41\u5206\u5e03\u5206\u6790\u3002<\/p>\n<p><strong>\u3010\u7ed3\u8bba\u4e0e\u5c55\u671b\u3011<\/strong><\/p>\n<p>\u672c\u9879\u7814\u7a76\u5229\u7528\u4e8c\u5143\u6c27\u5316\u7269VO<sub>2<\/sub>\u6765\u8bc1\u660e\u901a\u8fc7\u6c22\u5316\u4f5c\u7528\u53ef\u5b9e\u73b0\u63a2\u9488\u8bf1\u5bfc\u7684IMT\u3002VO<sub>2<\/sub>\u5177\u6709\u4ece\u4f4e\u6e29\u5355\u659c\u76f8\u5230\u9ad8\u6e29\u91d1\u7ea2\u77f3\u76f8\u7684\u8fd1\u5ba4\u6e29IMT\u884c\u4e3a\uff0c\u8be5\u884c\u4e3a\u4f34\u968f\u7740\u9ad8\u8fbe\u51e0\u4e2a\u6570\u91cf\u7ea7\u7684\u5267\u70c8\u7535\u963b\u7387\u53d8\u5316\u3002\u7531\u4e8e\u5176IMT\u53ef\u901a\u8fc7\u5916\u90e8\u523a\u6fc0\u8fdb\u884c\u63a7\u5236\uff0cVO<sub>2<\/sub>\u5df2\u5e7f\u6cdb\u5e94\u7528\u4e8e\u5b58\u50a8\u5668\u3001\u8d85\u6750\u6599\u3001\u667a\u80fd\u7a97\u53e3\u7b49\u8bb8\u591a\u5176\u4ed6\u9886\u57df\u3002\u800c\u5728\u672c\u5de5\u4f5c\u4e2d\uff0c\u4f5c\u8005\u5728VO<sub>2<\/sub>\u4e0a\u5b9e\u73b0\u4e86\u626b\u63cf\u63a2\u9488\u8bf1\u5bfc\u7684IMT\u3002\u5728\u504f\u538b\u9488\u5c16\u626b\u63cf\u671f\u95f4\uff0c\u6c22\u79bb\u5b50\u901a\u8fc7\u9488\u5c16-\u8868\u9762\u7ed3\u88ab\u5f15\u5165\u6837\u54c1\uff0c\u4ece\u800c\u901a\u8fc7\u6c22\u5316\u4f5c\u7528\u5c06VO<sub>2<\/sub>\u8f6c\u53d8\u4e3aH<em><sub>x<\/sub><\/em>VO<sub>2<\/sub>\u3002\u8fd9\u9879\u5de5\u4f5c\u9610\u91ca\u4e86\u57fa\u4e8e\u626b\u63cf\u63a2\u9488\u663e\u5fae\u6280\u672f\u6240\u5177\u6709\u7684\u7eb3\u7c73\u7ea7\u7a7a\u95f4\u5206\u8fa8\u7387\u53ef\u5bf9VO<sub>2<\/sub>\u7684IMT\u8fdb\u884c\u7eb3\u7c73\u7ea7\u64cd\u4f5c\u3002\u66f4\u91cd\u8981\u7684\u662f\uff0c\u8fd9\u9879\u7814\u7a76\u4e3a\u5b9e\u73b0\u6c22\u6f14\u53d8\u7684\u5c40\u90e8\u63a7\u5236\u5f00\u8f9f\u4e86\u4e00\u6761\u4fbf\u6377\u6709\u6548\u7684\u9014\u5f84\uff0c\u4e3a\u64cd\u7eb5\u5fae\u89c2\u73b0\u8c61\uff08\u76f8\u5206\u79bb\u3001\u7574\u7ed3\u6784\u3001\u76f8\u8fb9\u754c\u7b49\uff09\u63d0\u4f9b\u4e86\u5de8\u5927\u7684\u53ef\u80fd\u6027\uff0c\u4e5f\u4e3a\u5f00\u53d1\u63a2\u9488\u76f4\u5199\u529f\u80fd\u5668\u4ef6\u63d0\u4f9b\u4e86\u5e7f\u9614\u7684\u5e94\u7528\u524d\u666f\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong>https:\/\/www.nature.com\/articles\/s41563-022-01373-4<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5bfc\u8bfb\u3011 \u5f3a\u5173\u8054\u6c27\u5316\u7269\u6750\u6599\u5177\u6709\u4f17\u591a\u6709\u8da3\u7684\u7269\u7406\u6027\u8d28\uff0c\u7edd\u7f18\u4f53-\u91d1\u5c5e\u76f8\u53d8\u5c31\u662f\u5176\u4e2d\u4e4b\u4e00\u3002\u5728\u7edd\u7f18\u4f53-\u91d1\u5c5e\u76f8\u53d8\uff08IMT\uff09\u4e2d\uff0c\u7535\u5bfc\u7387\u4f1a\u56e0\u4e3a\u5916\u754c\u523a\u6fc0\u800c\u53d1\u751f\u7edd\u7f18\u4f53-\u91d1\u5c5e\u8f6c\u53d8\u6025\u5267\u53d8&#8230;<\/p>\n","protected":false},"author":1076,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-243443","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/243443"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/1076"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=243443"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/243443\/revisions"}],"predecessor-version":[{"id":243450,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/243443\/revisions\/243450"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=243443"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=243443"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=243443"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}