{"id":243798,"date":"2022-11-03T08:42:28","date_gmt":"2022-11-03T00:42:28","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=243798"},"modified":"2022-11-03T08:52:53","modified_gmt":"2022-11-03T00:52:53","slug":"nature%e6%96%b0%e8%bf%9b%e5%b1%95","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=243798","title":{"rendered":"\u6d59\u6c5f\u5927\u5b66\u6700\u65b0Nature"},"content":{"rendered":"<p><strong>\u4e00\u3001\u7814\u7a76\u80cc\u666f<\/strong><\/p>\n<p>\u5728\u63d2\u5165\u5316\u5b66\u8fc7\u7a0b\u4e2d\u4ea7\u751f\u7684\u5404\u5411\u5f02\u6027\u6676\u683c\u5e94\u53d8\u548c\u5e94\u529b\u901a\u5e38\u5f15\u8d77\u6676\u4f53\u7ed3\u6784\u4e0d\u7a33\u5b9a\uff0c\u5305\u62ec\u88c2\u7eb9\u7684\u5f62\u6210\u3002\u56e0\u6b64\uff0c\u96f6\u5e94\u53d8\u63d2\u5165\u6750\u6599\u7684\u53d1\u5c55\u51b3\u5b9a\u4e86\u4f18\u8d8a\u7684\u7535\u5316\u5b66\u80fd\u529b\uff0c\u5982\u9502\u949b\u6c27\u5316\u7269\u3002\u7136\u800c\uff0c\u5f53\u4f7f\u7528\u5408\u6210\u548c\u6676\u4f53\u5316\u5b66\u6765\u7ef4\u6301\u96f6\u7f3a\u9677\u548c\u76f8\u7eaf\u5ea6\u7684\u7406\u60f3\u60c5\u51b5\u65f6\uff0c\u5b58\u5728\u673a\u68b0\u5316\u5b66\u964d\u89e3\u95ee\u9898\u3002<\/p>\n<p>\u4f7f\u7528\u6700\u5148\u8fdb\u7684\u5bcc\u954d\u5c42\u72b6\u6c27\u5316\u7269(LiNi<sub>x<\/sub>Co<sub>y<\/sub>Mn<sub>1\u2212x\u2212y<\/sub>O<sub>2<\/sub>, x &gt;0.5)\u4f5c\u4e3a\u9502\u79bb\u5b50\u7535\u6c60\u6b63\u6781\u6750\u6599\uff0c\u53ef\u4ee5\u5c06\u80fd\u91cf\u548c\u529f\u7387\u5bc6\u5ea6\u8fbe\u5230\u66f4\u9ad8\u7684\u6c34\u5e73\u3002\u7136\u800c\uff0c\u5728\u9502(\u8131)\u63d2\u5c42\u8fc7\u7a0b\u4e2d\u4ea7\u751f\u5404\u5411\u5f02\u6027\u6676\u683c\u5e94\u53d8\u548c\u5e94\u529b\u76f8\u5173\u7684\u4f53\u79ef\u53d8\u5316\uff0c\u4f1a\u5bfc\u81f4\u6b63\u6781\u6750\u6599\u7ed3\u6784\u4e25\u91cd\u4e0d\u7a33\u5b9a\u548c\u7535\u5316\u5b66\u8870\u53d8\uff0c\u5f53\u7535\u6c60\u5728\u9ad8\u7535\u538b(\u9ad8\u4e8e4.5 V)\u4e0b\u5de5\u4f5c\u65f6\uff0c\u8fd9\u79cd\u60c5\u51b5\u4f1a\u8fdb\u4e00\u6b65\u653e\u5927\uff0c\u8fd9\u4e25\u91cd\u5f71\u54cd\u4e86\u7535\u6c60\u7684\u9ad8\u80fd\u91ca\u653e\u3002\u5373\u4f7f\u7ecf\u8fc7\u4e86\u5927\u91cf\u7684\u52aa\u529b\uff0c\u76f4\u63a5\u51cf\u8f7b\u6676\u683c\u5e94\u53d8\u6301\u7eed\u7d2f\u79ef\u7684\u672c\u5f81\u5e94\u53d8\u6291\u5236\u65b9\u6cd5\u4ecd\u7136\u96be\u4ee5\u627e\u5230\u3002<\/p>\n<p><strong>\u4e8c\u3001\u6210\u679c\u63a0\u5f71<\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c\u6d59\u6c5f\u5927\u5b66\u9646\u4fca\u548c\u5434\u5929\u54c1\u6559\u6388\u63d0\u51fa\u4e86\u901a\u8fc7\u5728\u5c42\u72b6\u7ed3\u6784\u4e2d\u5f15\u5165\u76f8\u5e72\u9499\u949b\u77ff\u76f8\u4f5c\u4e3a\u201c\u94c6\u9489\u201d\uff0c\u901a\u8fc7\u9489\u4f4f\u6548\u5e94\u663e\u8457\u5730\u7f13\u89e3\u4e86\u6709\u5bb3\u7684\u7ed3\u6784\u6f14\u53d8\u3002\u4e0e\u4f20\u7edf\u6750\u6599\u76f8\u6bd4\uff0c\u6bcf\u4e00\u6b21\u5faa\u73af\u7684\u6676\u683c\u5e94\u53d8\u6f14\u5316\u663e\u8457\u964d\u4f4e\u4e86\u8fd170%\uff0c\u589e\u5f3a\u4e86\u5f62\u6001\u5b8c\u6574\u6027\uff0c\u4ece\u800c\u663e\u8457\u63d0\u9ad8\u4e86\u7535\u6c60\u7684\u5faa\u73af\u6027\u80fd\u3002<\/p>\n<p>\u76f8\u5173\u6210\u679c\u4ee5<strong>\u201cStrain-retardant coherent perovskite phase stabilized Ni-rich cathode\u201d<\/strong>\u4e3a\u9898\u53d1\u8868\u5728\u56fd\u9645\u9876\u7ea7\u671f\u520a<em>Nature<\/em>\u4e0a\uff0c\u8bba\u6587\u7b2c\u4e00\u5355\u4f4d\u4e3a\u6d59\u6c5f\u5927\u5b66\u3002<img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-243799\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/1-1.png\" alt=\"\" width=\"993\" height=\"524\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/1-1.png 993w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/1-1-300x158.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/1-1-768x405.png 768w\" sizes=\"(max-width: 993px) 100vw, 993px\" \/><\/p>\n<p><strong>\u4e09\u3001\u56fe\u6587\u5bfc\u8bfb<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-243800\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/2-1.png\" alt=\"\" width=\"573\" height=\"812\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/2-1.png 573w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/2-1-212x300.png 212w\" sizes=\"(max-width: 573px) 100vw, 573px\" \/><\/p>\n<p>\u56fe1 |\u5e94\u53d8\u6291\u5236\u7b56\u7565\u548c\u5b9e\u73b0\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-243801\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/3-1.png\" alt=\"\" width=\"873\" height=\"610\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/3-1.png 873w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/3-1-300x210.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/3-1-768x537.png 768w\" sizes=\"(max-width: 873px) 100vw, 873px\" \/><\/p>\n<p>\u56fe2 |\u7528operando\u540c\u6b65XRD\u8868\u5f81\u7684\u5e94\u53d8\u7f13\u53d8\u884c\u4e3a<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-243802\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/4-1.png\" alt=\"\" width=\"569\" height=\"728\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/4-1.png 569w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/4-1-234x300.png 234w\" sizes=\"(max-width: 569px) 100vw, 569px\" \/><\/p>\n<p>\u56fe3 |\u534a\u7535\u6c60\u7684\u7535\u5316\u5b66\u6027\u80fd\u8868\u5f81\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-243803\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/5.png\" alt=\"\" width=\"560\" height=\"475\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/5.png 560w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/5-300x254.png 300w\" sizes=\"(max-width: 560px) 100vw, 560px\" \/><\/p>\n<p>\u56fe4 |\u5316\u5b66\u76f8\u5206\u5e03\u53ca\u4e09\u7ef4\u5f62\u6001\u53d8\u5316<\/p>\n<p><strong>\u56db\u3001\u7ed3\u8bba\u5c55\u671b<\/strong><\/p>\n<p>\u7814\u7a76\u63d0\u51fa\u4e86\u901a\u8fc7\u5728\u5bcc\u954d\u5c42\u72b6\u7ed3\u6784\u4e2d\u5f15\u5165\u9499\u949b\u77ff\u76f8\u7684\u5e94\u53d8\u6291\u5236\u7b56\u7565\u3002\u7531\u4e8e\u5176\u7ed3\u6784\u76f8\u5bb9\u6027\uff0c\u9499\u949b\u77ff\u76f8\u53ef\u4ee5\u76f8\u5e72\u751f\u957f\u6210\u5c42\u72b6\u7ed3\u6784\u3002\u7531\u4e8e\u7535\u5316\u5b66\u4e0d\u6d3b\u8dc3\u7684\u5e94\u53d8\u6291\u5236\u76f8\u7684\u5927\u7684\u76f8\u53d8\u80fd\u5792\uff0c\u8fd9\u79cd\u76f8\u5e72\u7ed3\u6784\u7a33\u5065\u7684\u57fa\u4f53\u53ef\u4ee5\u7ef4\u6301\u673a\u68b0\u5316\u5b66\u7a33\u5b9a\u6027\u3002\u901a\u8fc7\u8fd9\u79cd\u65b9\u6cd5\uff0c\u53ef\u4ee5\u6781\u5927\u5730\u6291\u5236\u5c42\u72b6\u6c27\u5316\u7269\u4e2d\u56fa\u6709\u7684\u6676\u683c\u5e94\u53d8\uff0c\u83b7\u5f97\u6301\u4e45\u7684\u7ed3\u6784\u548c\u5f62\u6001\u7a33\u5b9a\u6027\uff0c\u9632\u6b62\u526f\u53cd\u5e94\u548c\u4e0d\u53ef\u9006\u76f8\u53d8\u6269\u5c55\u5230\u4f53\u76f8\u7c92\u5b50\u4e2d\u3002\u56e0\u6b64\uff0c\u8fd9\u79cd\u7a33\u5b9a\u7684\u6750\u6599\u8868\u73b0\u51fa\u4f18\u8d8a\u7684\u7535\u5316\u5b66\u6027\u80fd\uff0c\u7279\u522b\u662f\u957f\u671f\u5faa\u73af\u7a33\u5b9a\u6027\uff0c\u5373\u4f7f\u57284.6 V\u7684\u975e\u5e38\u9ad8\u7684\u622a\u6b62\u7535\u538b\u4e0b(\u57281C\u7535\u6d41\u4e0b\uff0c\u8d85\u8fc7200\u4e2a\u5468\u671f\u4fdd\u630194.7%\u7684\u5bb9\u91cf\u4fdd\u6301\u7387)\u3002\u8fd9\u79cd\u65b0\u7684\u5e94\u53d8\u6291\u5236\u65b9\u6cd5\u62d3\u5bbd\u4e86\u6676\u683c\u5de5\u7a0b\u91ca\u653e\u9502(\u8131)\u63d2\u5c42\u4ea7\u751f\u7684\u5e94\u53d8\u7684\u524d\u666f\uff0c\u4e3a\u53d1\u5c55\u5177\u6709\u957f\u5bff\u547d\u7684\u9ad8\u80fd\u91cf\u5bc6\u5ea6\u9634\u6781\u94fa\u5e73\u4e86\u9053\u8def\uff0c\u540c\u65f6\u4e5f\u62d3\u5bbd\u9ad8\u5ea6\u7a33\u5b9a\u7684\u6676\u4f53\u7ed3\u6784\u5e94\u7528\u4e8e\u5148\u8fdb\u9ad8\u80fd\u7535\u6c60\u7cfb\u7edf\u7684\u524d\u666f\u3002<\/p>\n<p>\u539f\u6587\u8be6\u60c5\uff1ahttps:\/\/www.nature.com\/articles\/s41586-022-05238-3<\/p>\n<p>\u672c\u6587\u7531\u5f20\u7199\u7199\u4f9b\u7a3f\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4e00\u3001\u7814\u7a76\u80cc\u666f \u5728\u63d2\u5165\u5316\u5b66\u8fc7\u7a0b\u4e2d\u4ea7\u751f\u7684\u5404\u5411\u5f02\u6027\u6676\u683c\u5e94\u53d8\u548c\u5e94\u529b\u901a\u5e38\u5f15\u8d77\u6676\u4f53\u7ed3\u6784\u4e0d\u7a33\u5b9a\uff0c\u5305\u62ec\u88c2\u7eb9\u7684\u5f62\u6210\u3002\u56e0\u6b64\uff0c\u96f6\u5e94\u53d8\u63d2\u5165\u6750\u6599\u7684\u53d1\u5c55\u51b3\u5b9a\u4e86\u4f18\u8d8a\u7684\u7535\u5316\u5b66\u80fd\u529b\uff0c\u5982\u9502\u949b\u6c27\u5316\u7269&#8230;<\/p>\n","protected":false},"author":39557,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-243798","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/243798"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/39557"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=243798"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/243798\/revisions"}],"predecessor-version":[{"id":243807,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/243798\/revisions\/243807"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=243798"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=243798"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=243798"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}