{"id":244183,"date":"2022-11-18T08:41:35","date_gmt":"2022-11-18T00:41:35","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=244183"},"modified":"2022-11-18T08:41:35","modified_gmt":"2022-11-18T00:41:35","slug":"%e9%92%99%e9%92%9b%e7%9f%bf%e5%a4%aa%e9%98%b3%e8%83%bd%e7%94%b5%e6%b1%a0%e5%8f%88%e5%8f%91science","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=244183","title":{"rendered":"\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u53c8\u53d1science"},"content":{"rendered":"<p>\u4e00\u3001 \u5bfc\u8bfb<\/p>\n<p>\u5364\u5316\u7269\u9499\u949b\u77ff\u6750\u6599\u5177\u6709\u65e0\u9650\u7684\u7ec4\u6210\u7a7a\u95f4\uff0c\u5177\u6709\u53ef\u8c03\u7684\u7535\u5b50\u548c\u5149\u5b66\u6027\u80fd\u3002\u5c3d\u7ba1\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u5177\u6709\u5f88\u9ad8\u7684\u529f\u7387\u8f6c\u6362\u6548\u7387(PCE)\uff0c\u4f46\u5176\u6709\u9650\u7684\u5668\u4ef6\u5bff\u547d\u4ecd\u7136\u662f\u5546\u4e1a\u5316\u7684\u4e00\u4e2a\u91cd\u5927\u6311\u6218\u3002\u6df7\u5408\u9633\u79bb\u5b50\u548c\u9634\u79bb\u5b50\u7684\u4f7f\u7528\u4f7f\u5f97\u6676\u4f53\u7684\u5bb9\u5dee\u7cfb\u6570\u66f4\u5408\u9002\uff0c\u4ece\u800c\u63d0\u9ad8\u4e86\u7ed3\u6784\u7a33\u5b9a\u6027\uff0c\u5e76\u589e\u52a0\u4e86\u5408\u6210\u5438\u6536\u819c\u7684\u5316\u5b66\u7a33\u5b9a\u6027\u3002\u7136\u800c\uff0c\u6df7\u5408\u9499\u949b\u77ff\u5438\u6536\u5242\u7ecf\u5e38\u53d1\u751f\u5143\u7d20\u548c\u76f8\u504f\u6790\uff0c\u8fd9\u53ef\u80fd\u4f1a\u964d\u4f4e\u5668\u4ef6\u6548\u7387\u548c\u4f7f\u7528\u5bff\u547d\u3002\u5927\u591a\u6570\u5173\u4e8e\u6df7\u5408\u9499\u949b\u77ff\u76f8\u5206\u79bb\u7684\u7814\u7a76\u90fd\u96c6\u4e2d\u5728\u8584\u819c\u8001\u5316\u65b9\u9762\uff0c\u4ee5\u4e86\u89e3\u9633\u79bb\u5b50\u548c\u9634\u79bb\u5b50\u7684\u8fc1\u79fb\u3001\u7eb3\u7c73\u7c07\u7684\u5f62\u6210\u548c\u53d1\u5c55\u3001\u70ed\u529b\u5b66\u9a71\u52a8\u529b\u4ee5\u53ca\u5b83\u4eec\u5bf9\u8584\u819c\u6027\u80fd\u548c\u5668\u4ef6\u6027\u80fd\u7684\u5f71\u54cd\u3002\u7136\u800c\uff0c\u76f8\u5173\u7684\u5355\u4e2a\u79bb\u5b50\u7684\u539f\u5b50\u805a\u96c6\u4ee5\u53ca\u5173\u8054\u5b83\u4eec\u5bfc\u81f4\u8584\u819c\u964d\u89e3\u7684\u96c6\u4f53\u884c\u4e3a\u7684\u7814\u7a76\u76f8\u5bf9\u532e\u4e4f\u3002\u8c22\u6797\u6a21\u578b\u8fde\u63a5\u4e86\u9499\u949b\u77ff\u4e2d\u9633\u79bb\u5b50\u805a\u96c6\u7684\u5fae\u89c2\u5206\u6790\u548c\u5176\u76f8\u5206\u79bb\u548c\u819c\u964d\u89e3\u7684\u5b8f\u89c2\u89c2\u5bdf\uff0c\u9002\u7528\u4e8e\u6df7\u5408\u5364\u5316\u7269\u9499\u949b\u77ff\u7b49\u591a\u79cd\u9499\u949b\u77ff\u3002\u5c06\u5176\u5e94\u7528\u4e8e\u9ad8\u6027\u80fd\u592a\u9633\u80fd\u7535\u6c60\u6742\u5316\u5364\u5316\u7269\u9499\u949b\u77ff\u4e2d\u4f7f\u7528\u9633\u79bb\u5b50\u548c\u9634\u79bb\u5b50\u6df7\u5408\u7269\u7684\u5143\u7d20\u548c\u76f8\u5206\u79bb\u7684\u7814\u7a76\uff0c\u53ef\u4e3a\u63d0\u9ad8\u7535\u6c60\u5bff\u547d\u63d0\u4f9b\u4e86\u65b0\u7684\u79d1\u5b66\u7406\u89e3\u548c\u601d\u8def\u3002<\/p>\n<p>\u4e8c\u3001\u6210\u679c\u63a0\u5f71<\/p>\n<p>\u8fd1\u65e5\uff0c\u6765\u81ea\u5317\u4eac\u7406\u5de5\u5927\u5b66\u6750\u6599\u79d1\u5b66\u4e0e\u5de5\u7a0b\u5b66\u9662\u5148\u8fdb\u6750\u6599\u5b9e\u9a8c\u4e2d\u5fc3\u7684\u9648\u68cb\u6559\u6388\u56e2\u961f\u91c7\u7528\u8c22\u6797\u7684\u504f\u6790\u6a21\u578b\u6765\u7814\u7a76\u5355\u4e2a\u9633\u79bb\u5b50\u7684\u8fc1\u79fb\uff0c\u53d1\u73b0\u521d\u59cb\u819c\u7684\u4e0d\u5747\u5300\u6027\u52a0\u901f\u4e86\u6750\u6599\u7684\u964d\u89e3\u3002\u672c\u5de5\u4f5c\u5236\u5907\u4e86\u9499\u949b\u77ff\u819c(FA<sub>1-x<\/sub>Cs<sub>x<\/sub>PbI<sub>3<\/sub>;\u5176\u4e2dFA\u4e3a\u7532\u9170\u80fa)\uff0c\u901a\u8fc7\u6dfb\u52a0\u7852\u5429\uff0c\u5bfc\u81f4\u5747\u5300\u7684\u9633\u79bb\u5b50\u5206\u5e03\uff0c\u963b\u788d\u4e86\u6750\u6599\u52a0\u5de5\u548c\u8bbe\u5907\u8fd0\u884c\u4e2d\u7684\u9633\u79bb\u5b50\u805a\u96c6\u3002\u57281\u6b21\u592a\u9633\u5149\u7167\u4e0b\uff0c\u57283190\u5c0f\u65f6\u7684\u6700\u5927\u529f\u7387\u8f93\u51fa\u540e\uff0c\u5408\u6210\u7684\u88c5\u7f6e\u5f88\u597d\u7684\u63d0\u9ad8\u4e86\u7684\u8f6c\u5316\u6548\u7387\uff0c\u5e76\u4fdd\u6301\u4e86\u521d\u59cb\u6548\u7387\u768491%\u3002\u5176\u4e3b\u8981\u539f\u56e0\u4e3a\u521d\u59cbFACsPb(Br<sub>0.13<\/sub>I<sub>0.87<\/sub>)<sub>3<\/sub>\u5438\u6536\u5242\u5ef6\u957f\u4e86\u5668\u4ef6\u7684\u4f7f\u7528\u5bff\u547d\u3002\u76f8\u5173\u6210\u679c\u4ee5\u201c<em>Initializing film homogeneity to retard phase segregation for stable perovskite solar cells<\/em>\u201d\u4e3a\u9898\u53d1\u8868\u5728\u56fd\u9645\u9876\u7ea7\u7efc\u5408\u671f\u520aScience\u4e0a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-244184\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/\u6355\u83b7.png\" alt=\"\" width=\"1106\" height=\"477\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/\u6355\u83b7.png 1106w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/\u6355\u83b7-300x129.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/\u6355\u83b7-768x331.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/\u6355\u83b7-1024x442.png 1024w\" sizes=\"(max-width: 1106px) 100vw, 1106px\" \/><\/p>\n<p>\u4e09\u3001\u6838\u5fc3\u521b\u65b0\u70b9<\/p>\n<p>(1) \u91c7\u7528\u8c22\u6797\u504f\u6790\u6a21\u578b\u53d1\u73b0\u521d\u59cb\u8584\u819c\u7684\u4e0d\u5747\u5300\u6027\u52a0\u901f\u4e86\u6750\u6599\u7684\u964d\u89e3\uff1b<\/p>\n<p>(2) \u5728\u9499\u949b\u77ff\u8584\u819c\uff08FA<sub>1\u2013x<\/sub>Cs<sub>x<\/sub>PbI<sub>3<\/sub>\uff1b\u5176\u4e2d FA \u662f\u7532\u8112\uff09\u4e2d\u6dfb\u52a0\u7852\u5429\uff0c\u4f7f\u5668\u4ef6\u5b9e\u73b0\u4e86\u66f4\u9ad8\u7684\u6548\u7387\u5e76\u4fdd\u6301\u4e86\u5176\u5927\u4e8e91%\u521d\u59cb\u6548\u7387\uff1b<\/p>\n<p>\u56db\u3001\u6570\u636e\u6982\u89c8<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-244185\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/1-8.jpg\" alt=\"\" width=\"1268\" height=\"1279\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/1-8.jpg 1268w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/1-8-150x150.jpg 150w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/1-8-297x300.jpg 297w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/1-8-768x775.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/1-8-1015x1024.jpg 1015w\" sizes=\"(max-width: 1268px) 100vw, 1268px\" \/><\/p>\n<p>\u56fe1 \u4e8c\u5143FACs\u9499\u949b\u77ff\u7684\u964d\u89e3\u673a\u7406<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-244186\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/2-10.jpg\" alt=\"\" width=\"1269\" height=\"1076\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/2-10.jpg 1269w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/2-10-300x254.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/2-10-768x651.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/2-10-1024x868.jpg 1024w\" sizes=\"(max-width: 1269px) 100vw, 1269px\" \/><\/p>\n<p>\u56fe2 \u9633\u79bb\u5b50\u504f\u6790\u52a8\u529b\u5b66\u7684\u8c22\u6797\u6a21\u578b\u6a21\u62df<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-244187\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/3-10.jpg\" alt=\"\" width=\"1268\" height=\"1302\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/3-10.jpg 1268w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/3-10-292x300.jpg 292w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/3-10-768x789.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/3-10-997x1024.jpg 997w\" sizes=\"(max-width: 1268px) 100vw, 1268px\" \/><\/p>\n<p>\u56fe3 \u6df7\u5408\u9633\u79bb\u5b50\u9499\u949b\u77ff\u819c\u7684\u5747\u5300\u6027\u53ca\u5176\u5f71\u54cd<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-244188\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/4-10.jpg\" alt=\"\" width=\"1268\" height=\"1078\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/4-10.jpg 1268w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/4-10-300x255.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/4-10-768x653.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/11\/4-10-1024x871.jpg 1024w\" sizes=\"(max-width: 1268px) 100vw, 1268px\" \/><\/p>\n<p>\u56fe4 \u6df7\u5408\u5364\u5316\u7269\u9499\u949b\u77ff\u819c\u7684\u5747\u5300\u6027\u53ca\u5176\u5f71\u54cd<\/p>\n<p>\u4e94\u3001\u6210\u679c\u542f\u8fea<\/p>\n<p>\u57fa\u4e8e\u8c22\u6797\u6a21\u578b\u7406\u8bba\u5206\u6790\uff0c\u53ef\u4ee5\u5728\u539f\u5b50\u5c3a\u5ea6\u4e0a\u89c2\u5bdf\u8fde\u63a5\u8fc7\u6c27\u5316\u7269\u7684\u76f8\u5206\u79bb\u548c\u8584\u819c\u964d\u89e3\u3002\u7531\u6b64\u672c\u6587\u89c2\u5bdf\u5230\u521d\u59cb\u8584\u819c\u7684\u5747\u5300\u6027\u5bf9\u8584\u819c\u548c\u5668\u4ef6\u7684\u7a33\u5b9a\u6027\u6709\u5f88\u5927\u5f71\u54cd\u3002\u901a\u8fc7\u8c03\u6574\u524d\u4f53\u5316\u5b66\u4e0e\u7852\u7684\u5173\u7cfb\uff0c\u672c\u6587\u5f00\u53d1\u4e86\u9ad8\u6e29\u80fd\u591f\u5728\u9ad8\u6e29\u4e0b\u5177\u6709\u4f18\u5f02\u7a33\u5b9a\u6027\u7684\u4f18\u5f02\u9499\u949b\u77ff\u592a\u9633\u80fd\u5668\u4ef6\u3002<\/p>\n<p>\u8bba\u6587\u94fe\u63a5\uff1ahttps:\/\/www.science.org\/doi\/10.1126\/science.abn3148<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4e00\u3001 \u5bfc\u8bfb \u5364\u5316\u7269\u9499\u949b\u77ff\u6750\u6599\u5177\u6709\u65e0\u9650\u7684\u7ec4\u6210\u7a7a\u95f4\uff0c\u5177\u6709\u53ef\u8c03\u7684\u7535\u5b50\u548c\u5149\u5b66\u6027\u80fd\u3002\u5c3d\u7ba1\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u5177\u6709\u5f88\u9ad8\u7684\u529f\u7387\u8f6c\u6362\u6548\u7387(PCE)\uff0c\u4f46\u5176\u6709\u9650\u7684\u5668\u4ef6\u5bff\u547d\u4ecd\u7136\u662f\u5546\u4e1a\u5316\u7684&#8230;<\/p>\n","protected":false},"author":34569,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-244183","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/244183"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/34569"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=244183"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/244183\/revisions"}],"predecessor-version":[{"id":244189,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/244183\/revisions\/244189"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=244183"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=244183"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=244183"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}