{"id":24445,"date":"2016-07-05T08:00:08","date_gmt":"2016-07-05T00:00:08","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=24445"},"modified":"2016-07-04T20:49:05","modified_gmt":"2016-07-04T12:49:05","slug":"%e8%b6%85%e9%ab%98%e6%b8%a9%e7%a6%bb%e5%ad%90%e6%b3%a8%e5%85%a5%e6%b3%95%e6%9c%89%e6%95%88%e5%90%88%e6%88%90%e4%bd%8e%e7%bc%ba%e9%99%b7%e8%83%bd%e5%b8%a6%e7%bb%93%e6%9e%84%e5%8f%af%e8%b0%83%e7%9a%84","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=24445","title":{"rendered":"\u8d85\u9ad8\u6e29\u79bb\u5b50\u6ce8\u5165\u6cd5\u6709\u6548\u5408\u6210\u4f4e\u7f3a\u9677\u80fd\u5e26\u7ed3\u6784\u53ef\u8c03\u7684\u77f3\u58a8\u70ef\u819c"},"content":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u8ba9\u6211\u4eec\u804a\u804a\u88ab\u79f0\u4e3a\u201c\u9ed1\u91d1\u201d\u201c\u65b0\u6750\u6599\u4e4b\u738b\u201d\u7684\u77f3\u58a8\u70ef\u7684\u65b0\u9c9c\u4e8b\u5427\uff01\u636e\u8bf4\u79d1\u5b66\u5bb6\u5df2\u8bc1\u5b9e\u8d85\u9ad8\u6e29\u79bb\u5b50\u6ce8\u5165\u6cd5\uff08HyTII\uff09\u80fd\u6709\u6548\u5730\u5408\u6210\u4f4e\u7f3a\u9677\uff0c\u80fd\u5e26\u7ed3\u6784\u53ef\u8c03\u7684\u77f3\u58a8\u70ef\u819c\uff0c\u53ef\u9002\u5408\u4e8e\u591a\u79cd\u8bbe\u5907\u5e73\u53f0\u548c\u5e94\u7528\u3002\u90a3\u4e48\u8fd9\u5230\u5e95\u662f\u600e\u4e48\u5b9e\u73b0\u7684\u5462\uff1f<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-24446\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/@JP6WP4H4BMSPI_L9ULDR.png\" alt=\"_@JP6WP4H4BMSP{I_L9ULDR\" width=\"558\" height=\"240\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/@JP6WP4H4BMSPI_L9ULDR.png 558w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/@JP6WP4H4BMSPI_L9ULDR-300x129.png 300w\" sizes=\"(max-width: 558px) 100vw, 558px\" \/><\/p>\n<p>\u7f8e\u56fd\u6d77\u519b\u7814\u7a76\u5b9e\u9a8c\u5ba4\uff08NRL\uff09\uff0c\u7535\u5b50\u79d1\u5b66\u4e0e\u6280\u672f\u548c\u6750\u6599\u79d1\u5b66\u4e0e\u6280\u672f\u90e8\u95e8\u7684\u79d1\u5b66\u5bb6\u7ec4\u6210\u7684\u8de8\u5b66\u79d1\u56e2\u961f\u5df2\u7ecf\u8bc1\u660e\u4e86\u8d85\u9ad8\u6e29\u79bb\u5b50\u6ce8\u5165\uff08HyTII\uff09\u53ef\u4f5c\u4e3a\u66ff\u4f4d\u63ba\u6742\u77f3\u58a8\u70ef\u2014\u2014\u4e00\u79cd\u516d\u8fb9\u5f62\u6392\u5217\u7684\u5355\u5c42\u78b3\u539f\u5b50\u5c42\u2014\u2014\u7684\u6709\u6548\u65b9\u6cd5\u3002\u8be5\u65b9\u6cd5\u5236\u5907\u7684\u8584\u819c\u7f3a\u9677\u5c11\uff0c\u80fd\u5e26\u7ed3\u6784\u53ef\u8c03\uff0c\u9002\u7528\u4e8e\u591a\u79cd\u8bbe\u5907\u5e73\u53f0\u548c\u5e94\u7528\u7a0b\u5e8f\u3002<\/p>\n<p>\u7814\u7a76\u8bc1\u660e\uff0cHyTII\u6cd5\u80fd\u591f\u5bf9\u63ba\u6742\u6d53\u5ea6\u8fdb\u884c\u7cbe\u786e\u5730\u8c03\u63a7\uff0c\u5e76\u901a\u8fc7\u63ba\u6742\u53cc\u5c42\u77f3\u58a8\u70ef\u4e2d\u7684\u4e00\u5c42\uff0c\u9996\u6b21\u5b9e\u73b0\u4e86\u5bf9\u6ce8\u5165\u6df1\u5ea6\u7684\u7cbe\u786e\u8c03\u63a7\u3002\u8be5\u65b9\u6cd5\u5236\u5f97\u7684\u8584\u819c\uff0c\u7535\u5b50\u4f20\u8f93\u6027\u80fd\u826f\u597d\u3002\u4e0e\u5176\u5b83\u7684\u63ba\u6742\u6216\u4fee\u9970\u7b49\u6539\u53d8\u7f3a\u9677\u7684\u65b9\u6cd5\u4e0d\u540c\u7684\u662f\uff0c\u672c\u5b9e\u9a8c\u901a\u8fc7\u76f4\u63a5\u8c03\u8282\u80fd\u5e26\u7ed3\u6784\uff0c\u6539\u5584\u4e86\u8584\u819c\u7684\u7535\u5b50\u4f20\u8f93\u6027\u80fd\u3002<\/p>\n<p>NRL\u7684\u6750\u6599\u7814\u7a76\u5de5\u7a0b\u5e08Cory Cress\u535a\u58eb\u8bf4\uff1a\u201c\u78b3\u539f\u5b50SP2\u6742\u5316\u7ed3\u5408\u5f62\u6210\u7684\u5355\u539f\u5b50\u5c42\uff0c\u4e5f\u5c31\u662f\u77f3\u58a8\u70ef\uff0c\u53ef\u4ee5\u4ece\u5757\u72b6\u77f3\u58a8\u4e2d\u5206\u79bb\uff0c\u5177\u6709\u4f18\u5f02\u7684\u7535\u5b50\u548c\u7535\u5b50\u81ea\u65cb\u6027\u8d28\u3002\u4e0d\u8fc7\uff0c\u5e94\u7528\u53d7\u9650\uff0c\u56e0\u4e3a\u77f3\u58a8\u70ef\u6ca1\u6709\u5e26\u9699\u5e76\u4e14\u63ba\u6742\u96be\u4ee5\u63a7\u5236\uff0c\u56e0\u6b64\u77f3\u58a8\u70ef\u5668\u4ef6\u53ea\u80fd\u7528\u4e8e\u7279\u6b8a\u7684\u8bbe\u5907\u6280\u672f\u4e2d\u201d\u3002<\/p>\n<p>\u63ba\u6742\u6216\u5316\u5b66\u4fee\u9970\u6cd5\u53ef\u80fd\u4f1a\u589e\u52a0\u4e00\u4e2a\u53ef\u7528\u7684\u95f4\u9699\u3002\u4f46\u662f\uff0c\u8fd9\u4e9b\u65b9\u6cd5\u5f80\u5f80\u4f1a\u4e0d\u53ef\u907f\u514d\u5730\u4f7f\u8584\u819c\u4ea7\u751f\u7f3a\u9677\uff0c\u964d\u4f4e\u4e86\u5b83\u7684\u7a33\u5b9a\u6027\uff0c\u63ba\u6742\u5242\u548c\u5b98\u80fd\u56e2\u7684\u4e0d\u5747\u5300\u8986\u76d6\u4e5f\u4f1a\u5927\u5927\u9650\u5236\u5b83\u4eec\u7684\u4f5c\u7528\uff0c\u964d\u4f4e\u77f3\u58a8\u70ef\u8584\u819c\u56fa\u6709\u7684\u6027\u80fd\u3002<\/p>\n<p>\u4e3a\u89e3\u51b3\u8fd9\u4e2a\u95ee\u9898\uff0cNRL\u79d1\u5b66\u5bb6\u5229\u7528\u5176\u8f90\u5c04\u6548\u5e94\u5f00\u53d1\u4e86\u4e00\u79cd\u5177\u6709\u76f8\u5f53\u7684\u7cbe\u5ea6\u548c\u63a7\u5236\u80fd\u529b\u7684\u8d85\u9ad8\u6e29\u79bb\u5b50\u6ce8\u5165\u7cfb\u7edf\uff0c\u76f4\u63a5\u5411\u77f3\u58a8\u70ef\u4e2d\u6ce8\u5165\u6c2e\u79bb\u5b50\uff08N +\uff09\u6765\u8fdb\u884c\u66ff\u4f4d\u63ba\u6742\u3002<\/p>\n<p>Cress \u8868\u793a\uff1a\u201c\u5f00\u53d1\u7cfb\u7edf\u7684\u51e0\u4e2a\u6708\u540e\uff0c\u6211\u4eec\u53d1\u73b0\u8be5\u6280\u672f\u7684\u53ef\u884c\u6027\u53d6\u51b3\u4e8e\u7b2c\u4e00\u6b21\u5b9e\u9a8c\u3002\u5728\u6211\u4eec\u7684\u7814\u7a76\u4e2d\uff0c\u6211\u4eec\u786e\u5b9a\u4e86\u4f7f\u77f3\u58a8\u70ef\u7684\u6c2e\u63ba\u6742\u91cf\u6700\u9ad8\uff0c\u4e14\u7f3a\u9677\u6700\u5c11\u7684\u9ad8\u6e29\u79bb\u5b50\u80fd\u91cf\u8303\u56f4\uff0c\u540c\u65f6\u4e5f\u8bc1\u5b9e\u4e86HyTII\u65b9\u6cd5\u80fd\u591f\u63a7\u5236\u63ba\u6742\u7684\u6df1\u5ea6\u3002<\/p>\n<p>\u4e3a\u5b9e\u73b0\u540e\u8005\uff0c\u79d1\u5b66\u5bb6\u5f00\u53d1\u4e86\u53cc\u5c42\u77f3\u58a8\u70ef\u6750\u6599\u7cfb\u7edf\uff0c\u4e00\u5c42\u4e3a\u5929\u7136\u77f3\u58a8\u70ef\uff0c99%\u7684\u78b3\u539f\u5b50\u4e3a12C\uff1b\u4e00\u5c42\u4e3a\u5408\u6210\u77f3\u58a8\u70ef\uff0c99%\u7684\u78b3\u539f\u5b50\u4e3a13C\u3002\u62c9\u66fc\u5149\u8c31\u6cd5\u53ef\u4ee5\u5206\u6790\u8fd9\u79cd\u53cc\u5c42\u6750\u6599\u6bcf\u4e00\u5c42\u7684\u53d8\u5316\u60c5\u51b5\u3002<\/p>\n<p>\u5728\u6700\u4f18\u9ad8\u6e29\u79bb\u5b50\u7684\u80fd\u91cf\u8303\u56f4\u5185\uff0c\u6c2e\u63ba\u6742\u7684\u77f3\u58a8\u70ef\u8584\u819c\u7684\u6027\u80fd\u53d6\u51b3\u4e8eN+\u6ce8\u5165\u7684\u5242\u91cf\uff0c\u8868\u660e\u4e86\u6c2e\u5728\u6539\u53d8\u8584\u819c\u6027\u80fd\u4e2d\u53d1\u6325\u4e86\u91cd\u8981\u4f5c\u7528\u3002\u76f8\u5bf9\u4e8e\u539f\u5b50\u63ba\u6742\uff0c\u79bb\u5b50\u63ba\u6742\u5236\u5907\u7684\u5668\u4ef6\u6709\u7740\u66f4\u597d\u7684\u7535\u5b66\u6027\u8d28\uff0c\u79d1\u5b66\u5bb6\u53d1\u73b0\u8fd9\u79cd\u73b0\u8c61\u4f53\u73b0\u51fa\u7684\u6e29\u5ea6\u4f9d\u8d56\u6027\u53d6\u51b3\u4e8e\u4e24\u4e2a\u65b9\u9762\uff1a\u4e00\u662f\u66ff\u4f4d\u63ba\u6742\u5bfc\u81f4\u7684\u80fd\u5e26\u6548\u5e94\uff0c\u4e8c\u662f\u7f3a\u9677\u5bfc\u81f4\u7684\u7c7b\u7edd\u7f18\u4f53\u6548\u5e94\u3002<\/p>\n<p>\u51fa\u4eba\u610f\u6599\u7684\u662f\uff0c\u7814\u7a76\u4eba\u5458\u53d1\u73b0\uff0c\u6c2e\u63ba\u6742\u542b\u91cf\u8fc7\u9ad8\uff0c\u7535\u4e2d\u6027\u4f4d\u70b9\u5904\u7684\u5e26\u9699\u4e0d\u4f1a\u7ee7\u7eed\u52a0\u5bbd\u3002\u53ea\u6709\u5728\u6ce8\u5165\u79bb\u5b50\u7684\u80fd\u91cf\u5f88\u9ad8\u65f6\uff0c\u7f3a\u9677\u624d\u5f00\u59cb\u5360\u636e\u4e3b\u5bfc\u4f5c\u7528\uff0c\u56e0\u4e3a\u6b64\u65f6\u7f3a\u9677\u6570\u91cf\u5927\u5927\u589e\u52a0\u3002\u8fd9\u4e5f\u8fdb\u4e00\u6b65\u8868\u660e\u4e86\u771f\u6b63\u63ba\u6742\u7684\u8584\u819c\u548c\u7f3a\u9677\/\u63ba\u6742\u8584\u819c\u7684\u533a\u522b\u3002<\/p>\n<p>NRL\u7814\u7a76\u7269\u7406\u5b66\u5bb6Adam L. Friedman \u8bf4\uff1a\u201c\u6211\u4eec\u7684\u8fd9\u4e9b\u5668\u4ef6\u7684\u6d4b\u8bd5\u7ed3\u679c\u6709\u529b\u8868\u660e\uff0c\u6211\u4eec\u7ec8\u4e8e\u5236\u6210\u4e86\u5e26\u9699\u53ef\u8c03\u3001\u7f3a\u9677\u5bc6\u5ea6\u4f4e\u548c\u7a33\u5b9a\u6027\u9ad8\u7684\u77f3\u58a8\u70ef\u8584\u819c\u3002\u56e0HyTII\u77f3\u58a8\u70ef\u8584\u819c\u4f20\u8f93\u6027\u80fd\u597d\uff0c\u5e26\u9699\u53ef\u8c03\uff0c\u8f7d\u6d41\u5b50\u5bc6\u5ea6\u5927\uff0c\u6211\u4eec\u63a8\u6d4b\u5176\u5728\u7535\u5b50\u6216\u81ea\u65cb\u7535\u5b50\u5e94\u7528\u4e0a\u6709\u7740\u5177\u6709\u5de8\u5927\u6f5c\u529b\u3002<\/p>\n<p>\u53c2\u8003\u6587\u7ae0\uff1a<a href=\"https:\/\/www.sciencedaily.com\/releases\/2016\/06\/160606111313.htm\" target=\"_blank\">New low-defect method to nitrogen dope graphene resulting in tunable bandstructure<\/a><\/p>\n<p>\u611f\u8c22\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u738b\u5b87\u63d0\u4f9b\u7d20\u6750\uff0c\u4fdd\u6301\u5b66\u4e60\u7684\u4e60\u60ef\uff0c\u70b9\u6211\u52a0\u5165<a href=\"http:\/\/cailiaoren.mikecrm.com\/6qSdMU\" target=\"_blank\">\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u8ba9\u6211\u4eec\u804a\u804a\u88ab\u79f0\u4e3a\u201c\u9ed1\u91d1\u201d\u201c\u65b0\u6750\u6599\u4e4b\u738b\u201d\u7684\u77f3\u58a8\u70ef\u7684\u65b0\u9c9c\u4e8b\u5427\uff01\u636e\u8bf4\u79d1\u5b66\u5bb6\u5df2\u8bc1\u5b9e\u8d85\u9ad8\u6e29\u79bb\u5b50\u6ce8\u5165\u6cd5\uff08HyTII\uff09\u80fd\u6709\u6548\u5730\u5408\u6210\u4f4e\u7f3a\u9677\uff0c\u80fd\u5e26\u7ed3\u6784\u53ef\u8c03\u7684\u77f3\u58a8\u70ef\u819c\uff0c\u53ef&#8230;<\/p>\n","protected":false},"author":284,"featured_media":24446,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[54,46,76],"class_list":["post-24445","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-keji","tag-making","tag-graphene","tag-carbon"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/24445"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/284"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=24445"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/24445\/revisions"}],"predecessor-version":[{"id":24654,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/24445\/revisions\/24654"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/24446"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=24445"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=24445"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=24445"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}