{"id":244588,"date":"2022-12-05T06:44:29","date_gmt":"2022-12-04T22:44:29","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=244588"},"modified":"2022-12-04T20:44:42","modified_gmt":"2022-12-04T12:44:42","slug":"%e9%a6%99%e6%b8%af%e5%9f%8e%e5%b8%82%e5%a4%a7%e5%ad%a6nature-energy%ef%bc%9a%e9%87%87%e7%94%a8%e5%b9%b3%e9%9d%a2%e6%b7%b7%e5%90%88%e5%bc%82%e8%b4%a8%e7%bb%93%e7%bb%93%e6%9e%84%e7%9a%84%e6%9c%89","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=244588","title":{"rendered":"\u9999\u6e2f\u57ce\u5e02\u5927\u5b66Nature Energy\uff1a\u91c7\u7528\u5e73\u9762\u6df7\u5408\u5f02\u8d28\u7ed3\u7ed3\u6784\u7684\u6709\u673a\u5149\u4f0f\u5668\u4ef6\u4e2d\u53d7\u6291\u5236\u7684\u590d\u5408\u635f\u5931"},"content":{"rendered":"<p style=\"text-align: center;\">\u3010\u5bfc\u8bfb\u3011<\/p>\n<p>\u00a0\u6709\u673a\u5149\u4f0f\uff08OPV\uff09\u56e0\u5176\u5728\u5149\u6d3b\u6027\u6750\u6599\u4e2d\u7684\u5de8\u5927\u5206\u5b50\u53ef\u8c03\u8c10\u6027\u800c\u6709\u671b\u6210\u4e3a\u6e05\u6d01\u80fd\u6e90\u3002\u76ee\u524d\uff0c\u9ad8\u6027\u80fd\u7684\u6709\u673a\u5149\u4f0f\u5668\u4ef6\u5927\u591a\u91c7\u7528\u4f53\u5f02\u8d28\u7ed3\u7ed3\u6784\uff0c\u5728\u8fd9\u79cd\u7ed3\u6784\u4e2d\uff0c\u5927\u91cf\u7684\u4f9b\u4f53-\u53d7\u4f53(D-A)\u5f02\u8d28\u7ed3\u5904\u5f62\u6210\u7684\u7535\u8377\u8f6c\u79fb\u6001\u6709\u52a9\u4e8e\u6fc0\u5b50\u89e3\u79bb\u3002\u7136\u800c\uff0c\u6765\u81ea\u4e8e\u5149\u8f7d\u6d41\u5b50\u91cd\u7ec4\u7684\u7535\u8377\u8f6c\u79fb\u6001\u7684\u81ea\u65cb\u7279\u6027\u5141\u8bb8\u5728\u8fd9\u4e9b\u5f02\u8d28\u7ed3\u5904\u5f1b\u8c6b\u5230\u80fd\u91cf\u6700\u4f4e\u7684\u4e09\u6001\u6fc0\u5b50(T<sub>1<\/sub>)\uff0c\u5bfc\u81f4\u5149\u7535\u6d41\u635f\u5931\u3002\u76ee\u524d\u6700\u9ad8\u7684\u7535\u80fd\u8f6c\u6362\u6548\u7387(PCEs)\u4e3a18%\uff0c\u4e0d\u65ad\u63d0\u9ad8OPV\u6027\u80fd\u4ee5\u8fbe\u5230\u7406\u8bba\u4e0a\u53ef\u5b9e\u73b0\u7684\u503c\u4ecd\u7136\u662f\u4e00\u4e2a\u91cd\u5927\u6311\u6218\u3002<\/p>\n<p style=\"text-align: center;\">\u3010\u6210\u679c\u63a0\u5f71\u3011<\/p>\n<p>\u8fd1\u65e5\uff0c\u9999\u6e2f\u57ce\u5e02\u5927\u5b66Francis R. Lin\u6559\u6388\u548cAlex K.-Y. Jen\u6559\u6388\u548c\u5357\u4eac\u5927\u5b66\u5f20\u6625\u5cf0\u6559\u6388\u8054\u5408\u53d1\u73b0\u8fd9\u79cd\u635f\u5931\u9014\u5f84\u53ef\u4ee5\u5728\u987a\u5e8f\u5904\u7406\u7684\u5e73\u9762\u6df7\u5408\u5f02\u8d28\u7ed3\uff08PMHJ\uff09\u88c5\u7f6e\u4e2d\u5f97\u5230\u7f13\u89e3\uff0c\u8be5\u88c5\u7f6e\u91c7\u7528\u5177\u6709\u5185\u5728\u8f83\u5f31\u6fc0\u5b50\u7ed3\u5408\u5f3a\u5ea6\u7684\u7ed9\u4f53\u548c\u53d7\u4f53\u3002PMHJ\u4e2d\u51cf\u5c11\u7684D-A\u6df7\u5408\u51cf\u8f7b\u4e86D-A\u63a5\u89e6\u5904\u7684\u975e\u53cc\u5143\u590d\u5408\uff0c\u9650\u5236\u4e86\u5f1b\u8c6b\u7684\u673a\u4f1a\uff0c\u4ece\u800c\u5728\u4e0d\u727a\u7272\u6fc0\u5b50\u89e3\u79bb\u6548\u7387\u7684\u60c5\u51b5\u4e0b\u6291\u5236\u4e86T<sub>1<\/sub>\u7684\u5f62\u6210\u3002\u8fd9\u4f7f\u5f97\u88c5\u7f6e\u5177\u6709&gt;19%\u7684\u9ad8\u529f\u7387\u8f6c\u6362\u6548\u7387\u3002\u76f8\u5173\u6210\u679c\u4ee5\u201c<strong>Suppressed recombination loss in organic photovoltaics adopting a planar\u2013mixed heterojunction architecture<\/strong>\u201d\u53d1\u8868\u5728<strong><em>Nature Energy<\/em><\/strong>\u4e0a\u3002\u9999\u6e2f\u57ce\u5e02\u5927\u5b66Francis R. Lin\u548cAlex K.-Y. Jen\u548c\u5357\u4eac\u5927\u5b66\u5f20\u6625\u5cf0\u6559\u6388\u4e3a\u8bba\u6587\u7684\u5171\u540c\u901a\u8baf\u4f5c\u8005\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-244596\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/0-1.png\" alt=\"\" width=\"1539\" height=\"786\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/0-1.png 1539w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/0-1-300x153.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/0-1-768x392.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/0-1-1024x523.png 1024w\" sizes=\"(max-width: 1539px) 100vw, 1539px\" \/><\/p>\n<p style=\"text-align: center;\">\u3010\u6838\u5fc3\u521b\u65b0\u70b9\u3011<\/p>\n<p>\u672c\u5de5\u4f5c\u9610\u660e\u4e86PMHJ\u7684\u5de5\u4f5c\u673a\u5236\uff0c\u5e76\u8ba8\u8bba\u4e86\u5bf9\u6750\u6599\u8bbe\u8ba1\uff0c\u5668\u4ef6\u5de5\u7a0b\u548c\u5149\u7269\u7406\u5b66\u7684\u5f71\u54cd\uff0c\u4ece\u800c\u4e3a\u672a\u6765\u7684\u6709\u673a\u5149\u4f0f\u53d1\u7535\u63d0\u4f9b\u5168\u9762\u7684\u57fa\u7840\u3002<\/p>\n<p style=\"text-align: center;\">\u3010\u6570\u636e\u6982\u51b5\u3011<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-244595\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/1-1.png\" alt=\"\" width=\"995\" height=\"841\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/1-1.png 995w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/1-1-300x254.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/1-1-768x649.png 768w\" sizes=\"(max-width: 995px) 100vw, 995px\" \/><\/p>\n<p>\u56fe1|Jablonski\u56fe\u548c\u7528\u4e8eOPV\u5236\u9020\u7684\u6d3b\u6027\u6750\u6599\u3002<\/p>\n<p>a\u3001OPV\u4e2d\u6fc0\u53d1\u6001\u52a8\u529b\u5b66\u7684\u56fe\u89e3\uff1a\uff081\uff09\u5355\u7ebf\u6001\u6fc0\u5b50\u7684\u5149\u6fc0\u53d1\uff1aS<sub>0<\/sub>\u2192LE\uff1b\uff082\uff0c4\uff09\u5149\u6fc0\u53d1\u5355\u7ebf\u6001\u6fc0\u5b50\u7684\u8f6c\u79fb\u9014\u5f84\uff1aLE\u2192<sup>1<\/sup>CT\uff082\uff09\u548cLE\u2192DSE\uff084\uff09\uff1b\uff083\uff0c5\uff09\u677e\u6563\u675f\u7f1a\u7684\u5355\u7ebf\u6001\u6fc0\u5b50\u89e3\u79bb\u6210\u81ea\u7531\u7535\u8377\uff1a<sup>1<\/sup>CT\u2192CS\uff083\uff09\u6216DSE\u2192CS\uff085\uff09\uff1b\uff086\uff0c7\uff09\u901a\u8fc7\u975e\u53cc\u5b50\u590d\u5408\u5f62\u6210CT\u72b6\u6001\uff1aCS\u2192<sup>1<\/sup>CT\/<sup>3<\/sup>CT\uff0c\u53ef\u80fd\u5e26\u6709<sup>1<\/sup>CT\/<sup>3<\/sup>CT\u2192CS\u518d\u586b\u5145\u548c\u65cb\u8f6c\u5141\u8bb8<sup>1<\/sup>CT\u2192S<sub>0<\/sub>\u5f1b\u8c6b\uff1b\uff088\uff09 <sup>3<\/sup>CT\u2192T<sub>1<\/sub>\u5f1b\u8c6b\uff0c\u5176\u4e2d\u8fdb\u4e00\u6b65\u7684T<sub>1<\/sub>\u2192S<sub>0<\/sub>\u5f1b\u8c6b\u53ef\u4ee5\u901a\u8fc7\u4e09\u91cd\u6001\u7535\u8377\u6e6e\u706d\u53d1\u751f\uff0c\u5bfc\u81f4\u5149\u8f7d\u6d41\u5b50\u7684\u6c38\u4e45\u635f\u5931\u3002b\u3001\u672c\u7814\u7a76\u4e2d\u4f7f\u7528\u7684D18\u548c\u4e24\u79cd\u4e3b\u8981NFA\u7684\u5206\u5b50\u7ed3\u6784\u3002c\u3001D18\u3001NFAs\u548cD18\/NFA PMHJ\u5171\u6df7\u7269\u7684\u8584\u819c\u5149\u5b66\u5438\u6536\u3002d\u3001\u6750\u6599\u80fd\u7ea7\u56fe\uff08IP\uff1a\u5bf9\u5e94\u4e8e\u6700\u9ad8\u5360\u636e\u5206\u5b50\u8f68\u9053\u80fd\u7ea7\u7684\u7535\u79bb\u52bf\uff1bEA\uff1a\u5bf9\u5e94\u4e8e\u6700\u4f4e\u672a\u5360\u636e\u5206\u5b50\u8f68\u9053\u80fd\u91cf\u80fd\u7ea7\u7684\u7535\u5b50\u4eb2\u548c\u529b\u3002\uff09\u3002e\u3001ToF SIMS Se<sup>2\u2212<\/sup> D18\/T9SBN-F PMHJ\u548cD18:T9SBN-F-BHJ\u5171\u6df7\u7269\u7684\u79bb\u5b50\u4ea7\u7387\u968f\u6e85\u5c04\u65f6\u95f4\u7684\u53d8\u5316\u66f2\u7ebf\u3002\u63d2\u56fe\u663e\u793a\u4e86PMHJ\u548cBHJ\u6df7\u5408\u7269\u7684\u793a\u610f\u56fe\u3002\u00a92022 Springer Nature<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-244594\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/2-1.png\" alt=\"\" width=\"1276\" height=\"806\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/2-1.png 1276w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/2-1-300x189.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/2-1-768x485.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/2-1-1024x647.png 1024w\" sizes=\"(max-width: 1276px) 100vw, 1276px\" \/><\/p>\n<p>\u56fe2 |\u5149\u4f0f\u7535\u6c60\u7279\u6027\u3002<\/p>\n<p>a\u3001\u4e8c\u5143D18\/NFA\uff08\u865a\u7ebf\uff09\u548c\u4e09\u5143D18\/NFC:Y6-O\uff08\u5b9e\u7ebf\uff09\u7684\u6700\u4f73PMHJ\u7535\u6c60\u7684<em>J\u2013V<\/em>\u7279\u6027\u3002b\u3001\u4f18\u5316\u7535\u6c60\u7684\u5916\u90e8\u91cf\u5b50\u6548\u7387\uff08EQE\uff09\u8c31\uff08\u5b9e\u7ebf\uff09\u548c\u79ef\u5206\u7535\u6d41\u5bc6\u5ea6\uff08\u865a\u7ebf\uff09\u3002c\u3001 d\uff0cD18\/T9TBO-F\uff08c\uff09\u548cD18\/T9SBN-F\uff08d\uff09\u7535\u6c60\u7684\u5f52\u4e00\u5316\u5085\u91cc\u53f6\u53d8\u6362\u5149\u7535\u6d41\u8c31EQE\uff08FTPS-EQE\uff0c\u7070\u8272\u7ebf\uff09\u548c\u7535\u81f4\u53d1\u5149\uff08\u7ea2\u8272\u7ebf\uff09\u66f2\u7ebf\u7684\u534a\u5bf9\u6570\u56fe\uff0c\u7ed8\u5236\u4e3a\u80fd\u91cf\u7684\u51fd\u6570\u3002FTPS-EQE\u7684\u4f4e\u80fd\u62d6\u5c3e\u5728\u7406\u8bba\u4e0a\u4e0e\u7535\u81f4\u53d1\u5149\u901a\u91cf\uff08<em>\u03d5<\/em><sub>EL<\/sub>\uff09\u548c\u9ed1\u4f53\u8f90\u5c04\u5149\u8c31\uff08<em>\u03d5<\/em><sub>BB<\/sub>\uff0c\u5728300\u2009K\uff09 \uff0c\u5982\u6df1\u84dd\u8272\u865a\u7ebf\u6240\u793a\u3002\u00a92022 Springer Nature<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-244597\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/3-2.png\" alt=\"\" width=\"1082\" height=\"830\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/3-2.png 1082w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/3-2-300x230.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/3-2-768x589.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/3-2-1024x786.png 1024w\" sizes=\"(max-width: 1082px) 100vw, 1082px\" \/><\/p>\n<p>\u56fe3|TA\u7ed3\u679c\u548c\u7eaf\u6750\u6599\u7684MD\u6a21\u62dfDSE\u4e8c\u805a\u4f53\u3002<\/p>\n<p>a\u2013c\uff0cD18\uff08a\uff09\u3001T9TBO-F\uff08b\uff09\u548cT9SBN-F\uff08c\uff09\u7684TA\u66f2\u7ebf\u3002GSB\/LE\/DSE\u6ce2\u6bb5\u4e3a590\/1180\/940\u2009\u7eb3\u7c73\uff08D18\uff09\uff1b825\/915\/1,550\u2009\u7eb3\u7c73\uff08T9TBO-F\uff09\uff1b840\/930\/1,600\u2009\u7eb3\u7c73\uff08T9SBN-F\uff09\u3002T9SBN-F\u819c\u4e2d~1440\u5904\u7684\u5f3aESA\u5e26\u4e0e\u901a\u8fc7\u4e09\u91cd\u654f\u5316\u9274\u5b9a\u7684NFA\u4e2dT<sub>1<\/sub>\u7684\u5149\u8c31\u7279\u5f81\u76f8\u5339\u914d\uff0c\u53ef\u80fd\u8868\u660e\u7531\u4e8e\u91cd\u539f\u5b50\u6548\u5e94\uff08\u7852\uff09\u5bfc\u81f4\u7684\u6709\u6548\u7684\u5355\u91cd\u6001-\u4e09\u91cd\u6001\u7cfb\u7edf\u95f4\u4ea4\u53c9\u3002d\u2013f\uff0c\u4fc3\u8fdbD18\uff08d\uff09\u3001T9TBO-f\uff08e\uff09\u548cT9SBN-f\uff08f\uff09\u4e2dDSE\u5f62\u6210\u7684\u4ee3\u8868\u6027\u586b\u5145\u56fe\u6848\u3002\u79bb\u57df\u7535\u5b50\u548c\u7a7a\u7a74\u7684\u5206\u5e03\u5206\u522b\u4e3a\u6a59\u8272\u548c\u84dd\u8272\u3002\u00a92022 Springer Nature<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-244598\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/4-1.png\" alt=\"\" width=\"720\" height=\"859\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/4-1.png 720w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/4-1-251x300.png 251w\" sizes=\"(max-width: 720px) 100vw, 720px\" \/><\/p>\n<p>\u56fe4 |\u4e0d\u540c\u5171\u6df7\u7269\u7684TA\u7ed3\u679c\u3002<\/p>\n<p>a\u3001b\u3001e\u3001f D18\/T9TBO-f PMHJ\uff08a\uff09\u548cD18:T9TBO-b BHJ\uff08b\uff09\u3001D18\/T9SBN-f PMHJ\uff08e\uff09\u548cD18:T9SBN-C BHJ\uff08f\uff09\u7684TA\u5256\u9762\u56fe\u3002D18:590 nm\u7684GSB\u6ce2\u6bb5\u2009\u3002\u5171\u6df7\u7269\u7684CS\u5e26\uff1a765\u2009nm\uff08D18\/T9TBO-F\u3001D18:T9TBO-F\uff09\uff1b790\u2009nm\uff08D18\/T9SBN-F\u3001D18:T9SBN-F\uff09\u3002\u5171\u6df7\u7269\u7684T<sub>1<\/sub>\u4fe1\u53f7\uff1a~1440\u2009nm\u3002c\u3001 g\uff0c\u5728D18\/T9TBO-F\u548cD18:T9TBO-F\uff08c\uff09\u4ee5\u53caD18\/T9SBN-F\u548cD18:T9SBN-F\uff08g\uff09\u76841440nm\u5904\u63a2\u6d4bESA\u4fe1\u53f7\u7684TA\u52a8\u529b\u5b66\u3002d\u3001 h\uff0cTA\u5149\u8c31\u57281000\u2009ps D18\/T9TBO-F\u548cD18:T9TBO-F\u7684\u5ef6\u65f6\u3002\uff08d\uff09 \u4ee5\u53caD18\/T9SBN-F\u548cD18:T9SBN-F\uff08h\uff09\u3002\u7bad\u5934\u663e\u793a\u4e86PMHJ\u5171\u6df7\u7269\u4e0eBHJ\u5171\u6df7\u7269\u76f8\u6bd4T<sub>1<\/sub>\u6291\u5236\u7684\u8d8b\u52bf\u3002c\u3001d\u3001g\u548ch\u4e2d\u7684\u6240\u6709\u75d5\u8ff9\u5206\u522b\u5f52\u4e00\u5316\u4e3a\u6bcf\u4e2a\u6837\u672c\u4e2d\u76f8\u5e94CS\u5e26\u7684\u6700\u5c0f\u503c\u3002\u00a92022 Springer Nature<\/p>\n<p style=\"text-align: center;\">\u3010\u6210\u679c\u542f\u793a\u3011<\/p>\n<p>\u603b\u4e4b\uff0c\u4f5c\u8005\u62a5\u544a\u4e86\u4e00\u79cd\u901a\u8fc7\u5728\u5177\u6709\u672c\u8d28\u4e0a\u51cf\u5c11\u7684D-A\u5f02\u8d28\u7ed3\u7684\u987a\u5e8f\u6c89\u79efPMHJ OPVs\u4e2d\u53bb\u9664\u91cd\u7ec4\u7684CT\u72b6\u6001\u6765\u7f13\u89e3\u975e\u53cc\u5b50\u91cd\u7ec4\u7684\u7b56\u7565\uff0c\u5176\u4e2d\u6291\u5236\u7684T<sub>1<\/sub>\u5f62\u6210\u53ef\u4ee5\u88ab\u89c2\u5bdf\u4e3a\u7279\u5f81\u3002\u901a\u8fc7\u4f7f\u7528\u5177\u6709\u8f83\u4f4e\u6fc0\u5b50\u7ed3\u5408\u5f3a\u5ea6\u7684\u5149\u6d3b\u6027\u6750\u6599\uff0c\u786e\u4fdd\u4e86PMHJ\u7535\u6c60\u4e2d\u7684\u6709\u6548\u6fc0\u5b50\u89e3\u79bb\u3002PMHJ\u4e2d\u7684\u5de5\u4f5c\u673a\u5236\u4e5f\u88ab\u9610\u660e\uff0c\u4ee5\u66f4\u597d\u5730\u7406\u89e3OPV\u7684\u6027\u80fd\u3002\u672a\u6765\u4e3a\u63d0\u9ad8\u8fd9\u4e9bPMHJ\u7535\u6c60\u7684\u7a33\u5b9a\u6027\u548c\u63ed\u793a\u8fd9\u4e9b\u9ad8\u6027\u80fd\u5668\u4ef6\u4e2d<em>V<\/em><sub>OC<\/sub>\u635f\u5931\u7684\u57fa\u672c\u673a\u5236\u6240\u505a\u7684\u52aa\u529b\u5c06\u8fdb\u4e00\u6b65\u51cf\u5c11\u5149\u7535\u538b-\u5149\u7535\u6d41\u7684\u6743\u8861\uff0c\u4f7fPCEs\u8d85\u8fc720%\uff0c\u4ece\u800c\u8fbe\u5230OPV\u7684\u7406\u8bba\u6781\u9650\u3002<\/p>\n<p>&nbsp;<\/p>\n<p>\u53c2\u8003\u6587\u732e\uff1aJiang, K., Zhang, J., Zhong, C. et al. Suppressed recombination loss in organic photovoltaics adopting a planar\u2013mixed heterojunction architecture. Nat Energy 7, 1076\u20131086 (2022).<\/p>\n<p>https:\/\/doi.org\/10.1038\/s41560-022-01138-y<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5bfc\u8bfb\u3011 \u00a0\u6709\u673a\u5149\u4f0f\uff08OPV\uff09\u56e0\u5176\u5728\u5149\u6d3b\u6027\u6750\u6599\u4e2d\u7684\u5de8\u5927\u5206\u5b50\u53ef\u8c03\u8c10\u6027\u800c\u6709\u671b\u6210\u4e3a\u6e05\u6d01\u80fd\u6e90\u3002\u76ee\u524d\uff0c\u9ad8\u6027\u80fd\u7684\u6709\u673a\u5149\u4f0f\u5668\u4ef6\u5927\u591a\u91c7\u7528\u4f53\u5f02\u8d28\u7ed3\u7ed3\u6784\uff0c\u5728\u8fd9\u79cd\u7ed3\u6784\u4e2d\uff0c\u5927\u91cf\u7684\u4f9b\u4f53-&#8230;<\/p>\n","protected":false},"author":34544,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-244588","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/244588"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/34544"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=244588"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/244588\/revisions"}],"predecessor-version":[{"id":244635,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/244588\/revisions\/244635"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=244588"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=244588"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=244588"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}