{"id":245306,"date":"2022-12-31T06:00:13","date_gmt":"2022-12-30T22:00:13","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=245306"},"modified":"2022-12-30T17:39:22","modified_gmt":"2022-12-30T09:39:22","slug":"materials-today-energy-2022%e9%ab%98%e5%bc%95top-10","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=245306","title":{"rendered":"Materials Today Energy 2022\u9ad8\u5f15TOP 10"},"content":{"rendered":"<p><strong><b>\u671f\u520a\u4ecb\u7ecd\uff1a<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-245307\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72471-22.png\" alt=\"\" width=\"1220\" height=\"1630\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72471-22.png 1220w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72471-22-225x300.png 225w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72471-22-768x1026.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72471-22-766x1024.png 766w\" sizes=\"(max-width: 1220px) 100vw, 1220px\" \/><\/p>\n<p>Materials Today Energy\u00a0(MTE)\u00a0\u662fMaterials Today (Elsevier)\u00a0\u5bb6\u65cf\u7684\u80fd\u6e90\u65d7\u8230\u671f\u520a\uff0c\u9996\u53d1\u4e8e2017\u5e74\u3002\u5e7f\u7eb3\u5947\u601d\u5999\u60f3\uff0c\u901f\u64ad\u7cbe\u54c1\u4f73\u6587\uff01\u662f\u4e00\u672c\u4ee5\u80fd\u6e90\u6750\u6599\u4e3a\u4e3b\u7684\u4ea4\u53c9\u5b66\u79d1\u7684\u671f\u520a\uff0c\u5185\u5bb9\u5305\u62ec\u7535\u6c60\uff0c\u5149\u7535\u50ac\u5316\uff0c\u592a\u9633\u80fd\u8f6c\u5316\uff0c\u751f\u7269\u80fd\u6e90\u7b49\u4e00\u5207\u80fd\u6e90\u76f8\u5173\u7814\u7a76\u9886\u57df\u30022022\u5e74\u671f\u520a\u5f71\u54cd\u56e0\u5b50: 9.257\uff0c<strong><b>SCIE Q1<\/b><\/strong>\u3002\u5357\u6d0b\u7406\u5de5\u5927\u5b66\u7684\u8303\u7ea2\u91d1\u6559\u6388\u62c5\u4efb\u4e3b\u7f16\uff0c\u4ed6\u4eb2\u529b\u4eb2\u4e3a\uff0c\u4f18\u9009\u7cbe\u54c1\u3002\u7f16\u8f91\u90e8\u62e5\u6709\u5f3a\u5927\u4f18\u79c0\u7684\u7f16\u59d4\u548c\u9752\u5e74\u7f16\u59d4\u56e2 (ECR)\u3002\u5bf9\u7a3f\u4ef6\u8981\u6c42\u9ad8\uff0c\u5904\u7406\u901f\u5ea6\u5feb\u30027\u5929\u4e4b\u5185\u9996\u6b21\u5904\u7406\uff0c\u521d\u5ba1\u610f\u89c1\u4e0d\u8d85\u8fc77\u5468\uff0c\u63a5\u6536\u540e7\u5929\u4e0a\u7f51\u3002\u671f\u520a\u51fa\u7248\u91cf2021\u5e74\u8d85\u8fc7300\u7bc7\uff0c\u9010\u5e74\u9012\u589e\uff0c\u4ece2022\u5e74\u5f00\u59cb\u6bcf\u5e748\u671f\uff0c\u5c01\u9762\u5f69\u56fe\u90fd\u514d\u8d39\u3002\u5bf9\u6807Adv Energy Mater.\u00a0\u6210\u679c\u591a\u6e20\u9053\u5e7f\u6cdb\u5ba3\u4f20\u3002<\/p>\n<p><strong><b>\u671f\u520a\u7f51\u5740\uff1a<\/b><\/strong><a href=\"https:\/\/www.sciencedirect.com\/journal\/materials-today-energy\"><u>https:\/\/www.sciencedirect.com\/journal\/materials-today-energy<\/u><\/a><\/p>\n<p>&nbsp;<\/p>\n<p><strong><b>1\u3001\u4e2d\u5357\u5927\u5b66\u6881\u53d4\u5168\/\u5468\u6c5fMTE\u5c01\u9762\u6587\u7ae0\uff1a\u6c34\u7cfbZn\/MnO<sub>2<\/sub>\u7535\u6c60\u6eb6\u89e3-\u6c89\u79ef\u673a\u7406\u65b0\u8ba4\u77e5<\/b><\/strong><\/p>\n<p>Xun Guo, Jiang Zhou*, Chaolei Bai Xinkuo Li Guozhao Fang Shuquan Liang*, Zn\/MnO<sub>2<\/sub> battery chemistry with dissolution-deposition mechanism. <strong><em>Materials Today Energy<\/em><\/strong>\u00a0<strong>16<\/strong>\u00a0(2020) 100396.\u00a0<a href=\"https:\/\/doi.org\/10.1016\/j.mtener.2020.100396\"><u>https:\/\/doi.org\/10.1016\/j.mtener.2020.100396<\/u><\/a>\u00a0<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-245308\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72472-21.png\" alt=\"\" width=\"887\" height=\"540\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72472-21.png 887w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72472-21-300x183.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72472-21-768x468.png 768w\" sizes=\"(max-width: 887px) 100vw, 887px\" \/><\/p>\n<p><strong><b>\u6587\u7ae0\u4eae\u70b9<\/b><\/strong><\/p>\n<p>1\uff09\u63d0\u51fa\u4e86\u6c34\u76f8Zn\/MnO<sub>2<\/sub>\u7535\u6c60\u4e2d\u4e00\u79cd\u65b0\u7684\u6eb6\u89e3-\u6c89\u79ef\u673a\u7406\u3002<\/p>\n<p>2\uff09\u8fd9\u79cd\u673a\u5236\u53ef\u4ee5\u5408\u7406\u5730\u89e3\u91caZn\/MnO<sub>2<\/sub>\u7535\u6c60\u4e2d\u4e00\u4e9b\u4ee4\u4eba\u56f0\u60d1\u7684\u73b0\u8c61\u3002<\/p>\n<p>3\uff09\u63a2\u8ba8\u4e86\u53cd\u5e94\u52a8\u529b\u5b66\u7684\u4e3b\u8981\u5c40\u9650\u6027\uff0c\u4f8b\u5982 Zn<sub>4<\/sub>SO<sub>4<\/sub>(OH)<sub>6<\/sub>\u00b74H<sub>2<\/sub>O \u548c\u6d3b\u6027 H<sub>2<\/sub>O\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong><b>2\u3001Raizada\u6559\u6388<\/b><\/strong><b><\/b><strong><b>(Shoolini University) <\/b><\/strong><strong><b>\u548c<\/b><\/strong><strong><b>Nguyen\u6559\u6388<\/b><\/strong><strong><b>\u00a0(<\/b><\/strong><strong><b>Duy Tan University)<\/b><\/strong><strong><b>: <\/b><\/strong><strong><b>\u591a\u5143MOF\u7eb3\u7c73\u7ed3\u6784\u7684\u5149\u50ac\u5316\u5e94\u7528\u7684\u603b\u7ed3\u548c\u5c55\u671b<\/b><\/strong><\/p>\n<p><strong><b>S.<\/b><\/strong>Patial,P. Raizada*,V. Hasija,<sup>\u00a0<\/sup>P. Singh,<sup>\u00a0<\/sup>V. Kumar Thakur,<sup>\u00a0<\/sup>V.-H. Nguyen*.<sup>\u00a0<\/sup>Recent advances in photocatalytic multivariate metal organic frameworks-based nanostructures toward renewable energy and the removal of environmental pollutants. <strong><em>Materials Today Energy<\/em><\/strong>\u00a019 (2021) 100589. <a href=\"https:\/\/doi.org\/10.1016\/j.mtener.2020.100589\"><u>https:\/\/doi.org\/10.1016\/j.mtener.2020.100589<\/u><\/a>\u00a0<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-245309\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72473-17.png\" alt=\"\" width=\"711\" height=\"674\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72473-17.png 711w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72473-17-300x284.png 300w\" sizes=\"(max-width: 711px) 100vw, 711px\" \/><\/p>\n<p><strong><b>\u6587\u7ae0\u4eae\u70b9<\/b><\/strong><\/p>\n<p>1\uff09\u7b80\u8981\u7efc\u8ff0\u4e86\u8fd1\u5e74\u6765MOFs\u57fa\u5149\u50ac\u5316\u5242\u5728\u4e0d\u540c\u9886\u57df\u4e2d\u7684\u7814\u7a76\u8fdb\u5c55\u3002<\/p>\n<p>2\uff09\u9610\u8ff0\u4e86\u6df7\u5408\u8fde\u63a5\/\u91d1\u5c5e\u914d\u4f4d\u952eMOFs\u7684\u4e00\u6b65\u5408\u6210\u6cd5\u548c\u5408\u6210\u540e\u6539\u6027\u7b56\u7565\u3002<\/p>\n<p>3\uff09\u8be6\u7ec6\u8ba8\u8bba\u4e86\u91d1\u5c5e\u6c27\u5316\u7269\/\u78b3\u8d28\u534a\u5bfc\u4f53\u548c\u591a\u5143MOFs\u5f02\u8d28\u7ed3\u6784\u7684\u5149\u50ac\u5316\u673a\u7406\u3002<\/p>\n<p>4\uff09\u5c55\u671b\u4e86\u591a\u5143MOFs\u7684\u91d1\u5c5e\u79bb\u5b50\/\u8fde\u63a5\u5242\uff0c\u5408\u6210\u65b9\u6cd5\uff0c\u4ee5\u53ca\u5149\u50ac\u5316\u673a\u7406\u7814\u7a76\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong><b>3\u3001Ayodhya et al (Osmania University): <\/b><\/strong><strong><b>\u534a\u5bfc\u4f53\u91d1\u5c5e\u786b\u5316\u7269\u7eb3\u7c73\u7ed3\u6784\u5728\u67d3\u6599\u5149\u964d\u89e3\u65b9\u9762\u7684\u7814\u7a76\u8fdb\u5c55<\/b><\/strong><\/p>\n<p>Dasari Ayodhya*, Guttena Veerabhadram. A review on recent advances in photodegradation of dyes using doped and heterojunction based semiconductor metal sulfide nanostructures for environmental protection. <strong><em>Materials Today Energy<\/em><\/strong>\u00a09 (2018) 83-113.\u00a0<a href=\"https:\/\/doi.org\/10.1016\/j.mtener.2018.05.007,\"><u>https:\/\/doi.org\/10.1016\/j.mtener.2018.05.007,<\/u><\/a><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-245310\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72474-14.png\" alt=\"\" width=\"887\" height=\"496\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72474-14.png 887w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72474-14-300x168.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72474-14-768x429.png 768w\" sizes=\"(max-width: 887px) 100vw, 887px\" \/><\/p>\n<p><strong><b>\u6587\u7ae0\u4eae\u70b9<\/b><\/strong><\/p>\n<p>1\uff09\u7b80\u8981\u6982\u8ff0\u4e86\u67d3\u6599\u6c61\u67d3\u7269\u3001\u67d3\u6599\u5206\u7c7b\u3001\u67d3\u6599\u8131\u8272\u6216\u964d\u89e3\u7b56\u7565\u3002<\/p>\n<p>2\uff09\u91cd\u70b9\u4ecb\u7ecd\u4e86\u534a\u5bfc\u4f53\u91d1\u5c5e\u786b\u5316\u7269\u7eb3\u7c73\u7ed3\u6784\u5149\u50ac\u5316\u5242\u7684\u4f5c\u7528\u673a\u7406\u3002<\/p>\n<p>3\uff09\u8be6\u7ec6\u8ba8\u8bba\u4e86\u534a\u5bfc\u4f53\u91d1\u5c5e\u786b\u5316\u7269\u7eb3\u7c73\u7ed3\u6784\u5728\u589e\u5f3a\u6709\u6bd2\u67d3\u6599\u5149\u50ac\u5316\u964d\u89e3\u4e2d\u7684\u6700\u65b0\u8fdb\u5c55\u3002<\/p>\n<p>4\uff09\u91cd\u70b9\u5173\u6ce8\u4e86\u63ba\u6742\u5242\u3001\u5f02\u8d28\u7ed3\u3001\u5e26\u9699\u3001\u5c3a\u5bf8\u3001\u5149\u5f3a\u3001\u6bd4\u8868\u9762\u79ef\u3001\u53cd\u5e94\u65f6\u95f4\u3001\u964d\u89e3\u6548\u7387\u7b49\u53c2\u6570\u5bf9\u6709\u673a\u67d3\u6599\u7684\u5f71\u54cd\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong><b>4\u3001\u5357\u6fb3\u5927\u5b66 Hao<\/b><\/strong><strong><b>lan Xu: <\/b><\/strong><strong><b>\u5149\u70ed\u6750\u6599\u5728\u9ad8\u6548\u592a\u9633\u80fd\u9a71\u52a8\u6c34\u84b8\u53d1\u65b9\u9762\u7684\u7814\u7a76\u8fdb\u5c55<\/b><\/strong><\/p>\n<p>Xuan Wu,\u00a0George Y. Chen, Gary Owens, Dewei Chu, Haolan Xu*<sup>\u00a0<\/sup>Photothermal materials: A key platform enabling highly efficient water evaporation driven by solar energy. <strong><em>Materials Today Energy<\/em><\/strong>\u00a012 (2019) 277-296. <a href=\"https:\/\/doi.org\/10.1016\/j.mtener.2019.02.001\"><u>https:\/\/doi.org\/10.1016\/j.mtener.2019.02.001<\/u><\/a><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-245311\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72475-12.png\" alt=\"\" width=\"700\" height=\"531\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72475-12.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72475-12-300x228.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p><strong>\u6587\u7ae0\u4eae\u70b9<\/strong><\/p>\n<p>1\uff09\u6982\u8ff0\u4e86\u6700\u65b0\u7eb3\u7c73\u6750\u6599\u7684\u5149\u70ed\u6548\u5e94\u3002<\/p>\n<p>2\uff09\u91cd\u70b9\u4ecb\u7ecd\u4e86\u5149\u70ed\u6280\u672f\u5728\u592a\u9633\u80fd\u84b8\u6c7d\u53d1\u7535\u65b9\u9762\u7684\u7814\u7a76\u8fdb\u5c55\u3002<\/p>\n<p>3\uff09\u8ba8\u8bba\u4e86\u5149\u70ed\u7cfb\u7edf\u5728\u63d0\u9ad8\u592a\u9633\u80fd\u5229\u7528\u65b9\u9762\u7684\u672a\u6765\u53d1\u5c55\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><b><\/b><strong><b>5\u3001\u5317\u4eac\u7406\u5de5\u5927\u5b66\u738b\u514b\u4eae\uff1a\u950c\u679d\u6676\u7684\u751f\u957f\u548c\u6291\u5236\u7b56\u7565\u7efc\u8ff0<\/b><\/strong><\/p>\n<p><strong><b>Y.<\/b><\/strong>Zuo, K.Wang*, P. Pei, M. Wei, X. Liu, Y. Xiao, P. Zhang. Zinc dendrite growth and inhibition strategies. <strong><em>Materials Today Energy<\/em><\/strong>20 (2021) 100692 <a href=\"https:\/\/doi.org\/10.1016\/j.mtener.2021.100692\"><u>https:\/\/doi.org\/10.1016\/j.mtener.2021.100692<\/u><\/a><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-245312\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72476-5.png\" alt=\"\" width=\"681\" height=\"684\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72476-5.png 681w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72476-5-150x150.png 150w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72476-5-300x300.png 300w\" sizes=\"(max-width: 681px) 100vw, 681px\" \/><\/p>\n<p><strong>\u6587\u7ae0\u4eae\u70b9<\/strong><\/p>\n<p>1\uff09\u8be6\u7ec6\u4ecb\u7ecd\u4e86\u950c\u7684\u7269\u5316\u6027\u8d28\u57fa\u7840\u77e5\u8bc6\u3002<\/p>\n<p>2\uff09\u57fa\u4e8e\u751f\u957f\u7406\u8bba\u6a21\u578b\uff0c\u5206\u6790\u4e86\u950c\u679d\u6676\u7684\u6210\u6838\u548c\u751f\u957f\u884c\u4e3a\u548c\u5176\u5173\u952e\u5f71\u54cd\u56e0\u7d20\u3002<\/p>\n<p>3\uff09\u603b\u7ed3\u4e86\u4f18\u5316\u7535\u6781\u8868\u9762\u7535\u573a\u5206\u5e03\u3001\u4fc3\u8fdb\u950c\u79bb\u5b50\u8fc1\u79fb\u548c\u6291\u5236\u679d\u6676\u5f62\u6210\u7684\u7b56\u7565\u3002<\/p>\n<p>4\uff09\u8ba8\u8bba\u4e86\u950c\u57fa\u7535\u6c60\u5728\u672a\u6765\u53d1\u5c55\u4e2d\u9762\u4e34\u7684\u6311\u6218\u548c\u53d1\u5c55\u65b9\u5411\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong><b>6\u3001Kundu et al (CSIR-Central Electrochemical Research): <\/b><\/strong><strong><b>\u5c42\u72b6\u53cc\u6c22\u6c27\u5316\u7269(L<\/b><\/strong><strong><b>DH<\/b><\/strong><strong><b>)\u7535\u50ac\u5316O<\/b><\/strong><strong><b>ER<\/b><\/strong><strong><b>\u7684\u7814\u7a76\u8fdb\u5c55\u53ca\u5176\u7ed3\u6784\u3001\u6d3b\u6027\u548c\u673a\u7406\u5206\u6790<\/b><\/strong><\/p>\n<p>Sengeni Anantharaj,<sup>\u00a0<\/sup>Kannimuthu Karthick, Subrata Kundu*, Evolution of layered double hydroxides (LDH) as high performance water oxidation electrocatalysts: A review with insights on structure, activity and mechanism.\u00a0<strong><em>Materials Today Energy<\/em><\/strong>\u00a06 (2017) 1-26. <a href=\"https:\/\/doi.org\/10.1016\/j.mtener.2017.07.016\"><u>https:\/\/doi.org\/10.1016\/j.mtener.2017.07.016<\/u><\/a><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-245313\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72477-2.png\" alt=\"\" width=\"970\" height=\"491\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72477-2.png 970w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72477-2-300x152.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72477-2-768x389.png 768w\" sizes=\"(max-width: 970px) 100vw, 970px\" \/><\/p>\n<p><strong>\u6587\u7ae0\u4eae\u70b9<\/strong><\/p>\n<p>1\uff09\u7b80\u8981\u4ecb\u7ecd\u4e86\u7535\u50ac\u5316\u6790\u6c27\u53cd\u5e94(OER)\u7684\u57fa\u7840\u548c\u5404\u79cd\u50ac\u5316\u5242\u7684\u5e94\u7528\u524d\u666f\u3002<\/p>\n<p>2\uff09\u6df1\u5165\u63a2\u8ba8\u4e86OER\u5bf9LDH\u548c\u5c42\u72b6\u6c27\u5316\u7269\u6750\u6599\u7684\u4f5c\u7528\u673a\u7406\u3002<\/p>\n<p>3\uff09\u91cd\u70b9\u9610\u8ff0\u4e86LDH\u548c\u5c42\u72b6\u6c27\u5316\u7269\u6750\u6599\u5728\u7535\u5316\u5b66\u548c\u5149\u7535\u6c34\u6c27\u5316\u4e2d\u7684\u5e94\u7528\u3002<\/p>\n<p>4\uff09\u603b\u7ed3\u5e76\u63a2\u8ba8\u4e86LDH\u6750\u6599\u5728\u7535\u5316\u5b66\u6c34\u6c27\u5316\u4e2d\u7684\u7814\u7a76\u8d8b\u52bf\u3002<\/p>\n<p>\u00b7 \u8ba8\u8bba\u4e86\u53d1\u5c55\u65b0\u578bLDH\u6750\u6599\u5728\u5927\u89c4\u6a21\u9ad8\u6548\u4ea7\u6c22\u8fc7\u7a0b\u4e2d\u6240\u9762\u4e34\u7684\u6311\u6218\u548c\u673a\u9047\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong><b>7\u3001\u4e0a\u6d77\u7535\u529b\u5927\u5b66Rui<\/b><\/strong><strong><b>-tang Guo \u548cWei-guo Pan\u56e2\u961f\uff1a<\/b><\/strong><strong><b>\u91d1\u5c5e\u6c27\u5316\u7269\u57fa<\/b><\/strong><strong><b>Z<\/b><\/strong><strong><b>\u578b\u5f02\u8d28\u7ed3\u5149\u50ac\u5316\u5242\u7684\u7814\u7a76\u73b0\u72b6\u4e0e\u53d1\u5c55<\/b><\/strong><\/p>\n<p>Ye Yuan,<sup>\u00a0<\/sup>Rui-tang Guo*,<sup>\u00a0<\/sup>Long-fei Hong,<sup>\u00a0<\/sup>Xiang-yin Ji,<sup>\u00a0<\/sup>Zhi-dong Lin,<sup>\u00a0<\/sup>Zheng-sheng Li,<sup>\u00a0<\/sup>Wei-guo Pan*. A review of metal oxide-based Z-scheme heterojunction photocatalysts: actualities and developments.\u00a0<strong><em>Materials Today Energy<\/em><\/strong>\u00a021 (2021) 100829 <a href=\"https:\/\/doi.org\/10.1016\/j.mtener.2021.100829\">https:\/\/doi.org\/10.1016\/j.mtener.2021.100829<\/a><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-245314\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72478-2.png\" alt=\"\" width=\"1099\" height=\"401\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72478-2.png 1099w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72478-2-300x109.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72478-2-768x280.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72478-2-1024x374.png 1024w\" sizes=\"(max-width: 1099px) 100vw, 1099px\" \/><\/p>\n<p><strong>\u6587\u7ae0\u4eae\u70b9<\/strong><\/p>\n<p>1\uff09\u4ecb\u7ecd\u4e86Z\u578b\u5f02\u8d28\u7ed3\u5149\u50ac\u5316\u5242\u53ca\u5176\u50ac\u5316\u673a\u7406\u548c\u7c7b\u522b\u3002<\/p>\n<p>2\uff09\u6307\u51fa\u4e86\u5728S\u578b\u5f02\u8d28\u7ed3\u5174\u8d77\u4e0b\uff0cZ\u578b\u5f02\u8d28\u7ed3\u6240\u9762\u4e34\u7684\u57fa\u672c\u6311\u6218\u3002<\/p>\n<p>3\uff09\u603b\u7ed3\u4e86\u5168\u56fa\u6001\u3001\u76f4\u63a5Z\u578b\u548cS\u578b\u5f02\u8d28\u7ed3\u5149\u50ac\u5316\u5242\u7684\u6770\u51fa\u6210\u679c\u3002<\/p>\n<p>4\uff09\u4ecb\u7ecd\u4e86\u5236\u5907Z\u578b\u5f02\u8d28\u7ed3\u7684\u5e38\u89c1\u65b9\u6cd5\u548c\u65b0\u578b\u7b56\u7565\u3002<\/p>\n<p>5\uff09\u5bf9\u62d3\u5bbd\u91d1\u5c5e\u6c27\u5316\u7269\u57faZ\u578b\u5f02\u8d28\u7ed3\u5728\u5149\u50ac\u5316\u9886\u57df\u7684\u5e94\u7528\u63d0\u4f9b\u4e86\u542f\u53d1\u548c\u5efa\u8bae\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong><b>8\u3001\u6842\u6797\u7535\u5b50\u79d1\u6280\u5927\u5b66\u6c5f\u6c11\u7ea2\u548c\u5367\u9f99\u5c97\u5927\u5b66<\/b><\/strong><strong><b>Zhenxiang Cheng\u56e2\u961f\uff1a<\/b><\/strong><strong><b>CoFe-LDH\/ MXene\u754c\u9762\u8026\u5408\u52a9\u529b\u9ad8\u6548\u6790\u6c27\u50ac\u5316\u53cd\u5e94<\/b><\/strong><\/p>\n<p>Chongyan Hao,<sup>\u00a0<\/sup>Yang Wu,<sup>\u00a0<\/sup>Yajing An,<sup>\u00a0<\/sup>Baihua Cui,<sup>\u00a0<\/sup>Jiannan Lin,<sup>\u00a0<\/sup>Xiaoning Li,<sup>\u00a0<\/sup>Dianhui Wang,<sup>\u00a0<\/sup>Minhong Jiang*,<sup>\u00a0<\/sup>Zhenxiang Cheng*,<sup>\u00a0<\/sup>Shi Hu*. Interface-coupling of CoFe-LDH on MXene as high-performance oxygen evolution catalyst. <strong><em>Materials Today Energy<\/em><\/strong>\u00a012 (2019) 453-462.\u00a0<a href=\"https:\/\/doi.org\/10.1016\/j.mtener.2019.04.009\"><u>https:\/\/doi.org\/10.1016\/j.mtener.2019.04.009<\/u><\/a><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-245315\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72479.png\" alt=\"\" width=\"712\" height=\"665\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72479.png 712w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u72479-300x280.png 300w\" sizes=\"(max-width: 712px) 100vw, 712px\" \/><\/p>\n<p><strong>\u6587\u7ae0\u4eae\u70b9<\/strong><\/p>\n<p>1\uff09\u5728Ti<sub>3<\/sub>C<sub>2<\/sub>\u00a0MXene\u7eb3\u7c73\u7247\u8868\u9762\u751f\u957fCoFe-LDH\u5f62\u6210\u7684\u590d\u5408\u7ed3\u6784OER\u6027\u80fd\u8d85\u8fc7RuO<sub>2<\/sub>\u3002<\/p>\n<p>2\uff09CoFe-LDH\/ MXene\u7684\u9ad8\u5bfc\u7535\u6027\u548c\u7d27\u5bc6\u754c\u9762\u6709\u5229\u4e8e\u6709\u6548\u7684\u7535\u8377\u8f6c\u79fb\u548c\u6c27\u6d3b\u5316\u3002<\/p>\n<p>3\uff09\u8fd9\u9879\u5de5\u4f5c\u8bc1\u660e\u4e86MXene\u57fa\u590d\u5408\u7eb3\u7c73\u7ed3\u6784\u5728\u80fd\u91cf\u8f6c\u6362\u5e94\u7528\u4e2d\u7684\u5de8\u5927\u6f5c\u529b\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong><b>9\u3001\u5317\u4eac\u5316\u5de5\u5927\u5b66<\/b><\/strong><strong><b>\u5b59\u632f\u5b87<\/b><\/strong><strong><b>\u56e2\u961f\uff1a\u7535\u5316\u5b66\u50ac\u5316CO<sub>2<\/sub>\u8fd8\u539f\u8f6c\u5316C<sub>2+<\/sub>\u2014\u2014\u591a\u76f8\u7535\u50ac\u5316\u5242\uff0c\u53cd\u5e94\u9014\u5f84\u548c\u4f18\u5316\u7b56\u7565<\/b><\/strong><\/p>\n<p>Qun Fan, Mingli Zhang, Mingwen Jia, Shizhen Liu, Jieshan Qiu, Zhenyu Sun*. Electrochemical CO<sub>2<\/sub> reduction to C<sub>2+<\/sub> species: Heterogeneous electrocatalysts, reaction pathways, and optimization strategies. <strong><em>Materials Today Energy<\/em><\/strong>\u00a010 (2018) 280-301. <a href=\"https:\/\/doi.org\/10.1016\/j.mtener.2018.10.003\">https:\/\/doi.org\/10.1016\/j.mtener.2018.10.003<\/a>\u00a0<\/p>\n<p>&nbsp;<\/p>\n<p><strong>\u6587\u7ae0\u4eae\u70b9<\/strong><\/p>\n<p>1\uff09\u5168\u9762\u603b\u7ed3\u4e86\u57fa\u4e8e\u5404\u79cd\u6750\u6599\u7684CO<sub>2<\/sub>\u7535\u50ac\u5316\u8f6c\u5316C<sub>2+<\/sub>\u78b3\u6c22\u5316\u5408\u7269\u7684\u6700\u65b0\u8fdb\u5c55\u3002<\/p>\n<p>2\uff09\u6982\u8ff0\u4e86CO<sub>2<\/sub>\u50ac\u5316\u7684\u57fa\u672c\u539f\u7406\u548cC<sub>2+<\/sub>\u53cd\u5e94\u7684\u53ef\u80fd\u9014\u5f84\u3002<\/p>\n<p>3\uff09\u91cd\u70b9\u4ecb\u7ecd\u4e86\u63d0\u9ad8C<sub>2+<\/sub>\u5316\u5408\u7269\u4ea7\u91cf\u7684\u7b56\u7565\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong><b>10\u3001\u590f\u6c38\u59da\/\u6613\u91d1\u56e2\u961f\uff1a\u901a\u8fc7\u6291\u5236\u6c34\u7684\u6d3b\u6027\u6765\u63d0\u9ad8\u950c\u8d1f\u6781\u7684\u7535\u5316\u5b66\u53ef\u9006\u6027<\/b><\/strong><\/p>\n<p>Jin Cui, Xiaoyu Liu*, Yihua Xie, Kai Wu,\u00a0Yongqing Wang*, Yuyu Liu, Jiujun Zhang, Jin Yi*, Yongyao Xia. Improved electrochemical reversibility of Zn plating\/stripping: a promising approach to suppress water-induced issues through the formation of H-bonding. <strong><em>Materials Today Energy<\/em><\/strong>\u00a018 (2020) 100563. <a href=\"https:\/\/doi.org\/10.1016\/j.mtener.2020.100563\"><u>https:\/\/doi.org\/10.1016\/j.mtener.2020.100563<\/u><\/a><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-245316\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u724710.png\" alt=\"\" width=\"554\" height=\"266\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u724710.png 554w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u724710-300x144.png 300w\" sizes=\"(max-width: 554px) 100vw, 554px\" \/><\/p>\n<p><strong><b>\u6587\u7ae0\u4eae\u70b9<\/b><\/strong><\/p>\n<p>1\uff09\u6c22\u952e\u662f\u901a\u8fc7\u6dfb\u52a0\u4e00\u79cd\u57fa\u4e8e\u919a\u7684\u6dfb\u52a0\u5242\u800c\u5f62\u6210\u7684\u3002<\/p>\n<p>2\uff09\u901a\u8fc7\u6c22\u952e\u7684\u5f62\u6210\u53ef\u4ee5\u6291\u5236\u6790\u6c22\u53cd\u5e94\u3002<\/p>\n<p>3\uff09\u901a\u8fc7\u6c22\u952e\u5408\u53ef\u4ee5\u6291\u5236\u950c\u7684\u8150\u8680\u3002<\/p>\n<p>4\uff09\u7535\u6781\/\u7535\u89e3\u8d28\u754c\u9762\u53ef\u4ee5\u901a\u8fc7\u589e\u52a0\u6da6\u6e7f\u6027\u6765\u8c03\u6574\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong><b>\u671f\u520a\u4ecb\u7ecd\uff1a<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-245317\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u724711.png\" alt=\"\" width=\"1299\" height=\"1291\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u724711.png 1299w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u724711-150x150.png 150w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u724711-300x298.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u724711-768x763.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2022\/12\/\u56fe\u724711-1024x1018.png 1024w\" sizes=\"(max-width: 1299px) 100vw, 1299px\" \/><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u671f\u520a\u4ecb\u7ecd\uff1a Materials Today Energy\u00a0(MTE)\u00a0\u662fMaterials Today (Elsevier)\u00a0\u5bb6\u65cf\u7684\u80fd\u6e90\u65d7\u8230\u671f\u520a\uff0c\u9996\u53d1\u4e8e2017&#8230;<\/p>\n","protected":false},"author":41672,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-245306","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/245306"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/41672"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=245306"}],"version-history":[{"count":5,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/245306\/revisions"}],"predecessor-version":[{"id":245338,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/245306\/revisions\/245338"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=245306"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=245306"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=245306"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}