{"id":246786,"date":"2023-02-15T12:10:23","date_gmt":"2023-02-15T04:10:23","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=246786"},"modified":"2023-02-21T11:00:58","modified_gmt":"2023-02-21T03:00:58","slug":"%e3%80%90%e6%96%b0%e8%83%bd%e6%ba%90%e5%89%8d%e7%ba%bf%e3%80%91appl-catal-b%ef%bc%9a%e6%97%a0%e8%86%9c%e6%97%a0%e7%bc%93%e5%86%b2%e6%b5%b7%e6%b0%b4%e7%94%b5%e8%a7%a3%e4%ba%a7%e9%ab%98%e7%ba%af","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=246786","title":{"rendered":"Appl. Catal. B\uff1a\u65e0\u819c\u65e0\u7f13\u51b2\u6d77\u6c34\u7535\u89e3\u4ea7\u9ad8\u7eaf\u6c22\u6c14"},"content":{"rendered":"<p style=\"text-align: center;\"><span style=\"color: #0000ff;\"><strong>\u4e00\u3001<\/strong><strong>\u3010\u5bfc\u8bfb\u3011<\/strong><\/span><\/p>\n<p>\u00a0 \u00a0\u8fd1\u5e74\u6765\uff0c\u6d77\u6c34\u7535\u89e3\u5236\u6c22\u88ab\u8ba4\u4e3a\u662f\u80fd\u6e90\u8f6c\u578b\u7684\u5173\u952e\u6280\u672f\uff0c\u7136\u800c\u4ee5\u5f80\u7684\u7814\u7a76\u4e3b\u8981\u5173\u6ce8\u7684\u662f\u78b1\u6027\u6d77\u6c34\u3002\u5176\u4e2d\uff0c\u819c\uff08\u5206\u79bbH<sub>2<\/sub>\u548cO<sub>2<\/sub>\uff09\u548c\u8150\u8680\u6027 KOH (\u63d0\u9ad8\u6790\u6c27\u53cd\u5e94\u7684\u9009\u62e9\u6027) \u7684\u4f7f\u7528\u663e\u8457\u589e\u52a0\u4e86H<sub>2<\/sub>\u7684\u751f\u4ea7\u6210\u672c\u3002\u4e3a\u4e86\u964d\u4f4e\u6c22\u6c14\u7684\u6210\u672c\u4ee5\u53ca\u5b9e\u73b0\u6d77\u4e0a\u5feb\u901f\u8fd0\u8f93\uff0c\u76f4\u63a5\u6d77\u6c34\u7535\u89e3\u7814\u7a76\u5f15\u8d77\u4e86\u5e7f\u6cdb\u7684\u5173\u6ce8\u3002\u76f4\u63a5\u6d77\u6c34\u7535\u89e3\u5bf9\u7535\u6781\u7684\u9009\u62e9\u6027\u8981\u6c42\u5341\u5206\u4e25\u683c\u3002\u8fd9\u5f52\u56e0\u4e8e\u9633\u6781\u7684\u6790\u6c27\u53cd\u5e94\uff08OER\uff09\u548c\u6c2f\u6c27\u5316\u53cd\u5e94\uff08ClOR\uff09\u7684\u7ade\u4e89\uff0c\u4ee5\u53ca\u9634\u6781\u7684\u6c2f\u8fd8\u539f\u53cd\u5e94\uff08ClRR\uff0c\u6765\u81ea\u4e8e\u9633\u6781\u4ea7\u751f\u7684HClO\/ClO<sup>&#8211;<\/sup>\uff09\u548c\u6790\u6c22\u53cd\u5e94\uff08HER\uff09\u7684\u7ade\u4e89\u3002ClOR\u548cClRR\u7684\u53c2\u4e0e\u6781\u5927\u9650\u5236O<sub>2<\/sub>\u548cH<sub>2<\/sub>\u7684\u751f\u4ea7\u6548\u7387\u3002\u56e0\u6b64\u8981\u60f3\u5b9e\u73b0\u76f4\u63a5\u6d77\u6c34\u7535\u89e3\u5fc5\u987b\u5f00\u53d1\u51fa\u9ad8\u9009\u62e9\u6027\u548c\u7a33\u5b9a\u6027\u7684\u7535\u50ac\u5316\u5242\u3002<\/p>\n<p style=\"text-align: center;\"><span style=\"color: #0000ff;\"><strong>\u4e8c\u3001\u3010<\/strong><strong>\u6210\u679c\u63a0\u5f71\u3011<\/strong><\/span><\/p>\n<p><strong>\u00a0 \u00a0<\/strong>\u8fd1\u65e5\uff0c\u97e9\u56fd\u5e86\u5317\u5927\u5b66Hyunwoong\u00a0Park\u6559\u6388\u548c\u5361\u5854\u5c14\u5927\u5b66DongSuk Han\u6559\u6388\u7b49\u4eba\u63d0\u51fa\u5e76\u5b9e\u73b0\u4e86\u4e00\u79cd\u65e0\u819c\u65e0\u7f13\u51b2\u6d77\u6c34\u4ea7\u9ad8\u7eaf\u6c22\u6c14\u7684\u65b9\u6848\uff0c\u8be5\u65b9\u6848\u662f\u7531\u9ad8ClOR\u9009\u62e9\u6027\u9633\u6781\u548c\u9ad8ClRR\u6291\u5236\u6027\u9634\u6781\u7ec4\u6210\uff0c\u5b8c\u5168\u5b9e\u73b0\u4e86\u6291\u5236O<sub>2<\/sub>\u7684\u751f\u6210\uff0c\u540c\u65f6\u4f7f\u9634\u6781\u751f\u4ea7H<sub>2<\/sub>\u6700\u5927\u5316\u3002\u76f8\u5173\u7684\u7814\u7a76\u6210\u679c\u4ee5\u201c<strong><em>Membraneless unbuffered seawater electrolysis for pure hydrogen production using PtRuTiOx anode and MnOx cathode pairs<\/em><\/strong>\u201d\u4e3a\u9898\u53d1\u8868\u5728<strong><em>Applied Catalysis B: Environmental<\/em><\/strong>\u4e0a\u3002\u97e9\u56fd\u5e86\u5317\u5927\u5b66\u80fd\u6e90\u5de5\u7a0b\u5b66\u9662\u535a\u58eb\u6881\u6960\u6960\u4e3a\u7b2c\u4e00\u4f5c\u8005\uff0cHyunwoong\u00a0Park\u6559\u6388\u4e3a\u7b2c\u4e00\u901a\u8baf\u4f5c\u8005\u3002<\/p>\n<p><img decoding=\"async\" class=\"aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/1-4.png\" \/><\/p>\n<p style=\"text-align: center;\"><span style=\"color: #0000ff;\"><strong>\u4e09\u3001\u3010<\/strong><strong>\u6838\u5fc3\u521b\u65b0\u70b9\u3011<\/strong><\/span><\/p>\n<p><strong>1<\/strong><strong>\u3001\u8be5\u5de5\u4f5c\u5f00\u53d1\u51fa\u4e00\u79cd\u6700\u4f4e<\/strong><strong>Pt<\/strong><strong>\u6c34\u5e73\u7684\u4e09\u5143<\/strong><strong>Pt<\/strong><strong>\u3001<\/strong><strong> Ru <\/strong><strong>\u548c<\/strong><strong> Ti (PRT<\/strong><strong>\uff0c<\/strong><strong>Pt<sub> 0.06<\/sub>Ru<sub> 0.24<\/sub>Ti<sub>0.7<\/sub>O<sub>x<\/sub>)<\/strong><strong>\u7535\u50ac\u5316\u5242\uff0c\u53ef\u4ee5\u5728\u76d0\u6c34\u4e2d\u5b9e\u73b0\u9ad8<\/strong><strong>ClOR<\/strong><strong>\u9009\u62e9\u6027\uff0c\u6cd5\u62c9\u7b2c\u6548\u7387<\/strong><strong>(FE) ~100%<\/strong><strong>\u3002\u5e76\u4e14\u5728\u5de5\u4e1a\u7ea7\u7535\u6d41\u5bc6\u5ea6\uff08<\/strong><strong>800 mA cm<sup>-2<\/sup><\/strong><strong>\uff09\u4e0b\uff0c\u8be5\u7535\u6781\u4fdd\u6301\u7740\u5de5\u4e1a\u7ea7\u7a33\u5b9a\u6027\u548c\u6052\u5b9a\u7684<\/strong><strong>ClOR<\/strong><strong>\u6d3b\u6027\uff1b<\/strong><\/p>\n<p><strong>2<\/strong><strong>\u3001\u8be5\u5de5\u4f5c\u540c\u65f6\u4e5f\u63d0\u51fa\u5e76\u5b9e\u73b0\u4e00\u79cd\u65e0\u5e72\u6270\u3001\u65e0\u819c\u3001\u65e0\u7f13\u51b2\u6d77\u6c34\u4ea7\u9ad8\u7eaf<\/strong><strong>H<sub>2<\/sub><\/strong><strong>\u65b9\u6848\u3002\u8be5\u65b9\u6848\u4ee5<\/strong><strong>PRT <\/strong><strong>\u9633\u6781<\/strong><strong>\/MnOx<\/strong><strong>\u9634\u6781\u4f5c\u4e3a\u7535\u6781\u5bf9\uff0c\u5728\u65e0\u819c\u7535\u89e3\u6c60\u3001<\/strong><strong>pH 8.2<\/strong><strong>\u7684\u6d77\u6c34\u4e2d\u7535\u89e3\u8d85<\/strong><strong>100<\/strong><strong>\u5c0f\u65f6<\/strong><strong>, HER<\/strong><strong>\u548c<\/strong><strong>ClOR<\/strong><strong>\u4ee5<\/strong><strong>~100%<\/strong><strong>\u7684<\/strong><strong>FE<\/strong><strong>\u9a71\u52a8\uff0c\u6ca1\u6709<\/strong><strong>O<sub>2<\/sub><\/strong><strong>\u751f\u6210\u3002<\/strong><\/p>\n<p style=\"text-align: center;\"><span style=\"color: #0000ff;\"><strong>\u56db\u3001<\/strong><strong>\u3010\u6570\u636e\u6982\u89c8\u3011<\/strong><\/span><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter  wp-image-246787\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/2-4.png\" alt=\"\" width=\"537\" height=\"526\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/2-4.png 464w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/2-4-300x294.png 300w\" sizes=\"(max-width: 537px) 100vw, 537px\" \/><\/p>\n<p><strong>\u65b9\u68481<\/strong>\u00a0 \u5728\u65e0\u819c\u5355\u5ba4\u7535\u6c60\u4e2d\u4f7f\u7528 PtRuTiOx\u00a0(PRT) \u9633\u6781\u548c MnOx\u9634\u6781\u5bf9\u8fdb\u884c\u6d77\u6c34\u7535\u89e3\u7684\u793a\u610f\u56fe\u3002\u4f20\u7edf\u7684\u6d77\u6c34\u7535\u89e3\u5728\u78b1\u6027\u6761\u4ef6\u4e0b\u8fdb\u884c(pH&gt;13)\u4ee5\u786e\u4fddOER\u5bf9ClOR\u7684\u9009\u62e9\u6027\u3002\u6b64\u5916\uff0c\u5b83\u901a\u5e38\u9700\u8981\u819c\u6765\u6291\u5236ClRR \u548c HER\uff0c\u540c\u65f6\u5c06 H<sub>2<\/sub>\u4e0eO<sub>2<\/sub>\u5206\u79bb\u3002\u7136\u800c\uff0c\u5982\u679c\u7535\u89e3\u4ea7\u7269\u53ea\u6709\u6eb6\u6db2\u4e2d\u7684 HClO\uff08\u548c\/\u6216 ClO<sup>\u00a0&#8211;<\/sup>\uff09\u548c\u9876\u90e8\u7a7a\u95f4\u4e2d\u7684H<sub>\u00a02<\/sub>\uff0cClOR \u548c HER \u7684\u6cd5\u62c9\u7b2c\u6548\u7387\u5206\u522b\u4e3a ~100%\uff0c\u5219\u5206\u79bb\u6c14\u4f53\uff08H<sub>2<\/sub>\u548cO<sub>2<\/sub>) \u548c\u6291\u5236\u9634\u6781\u6c2f\u8fd8\u539f\u5c31\u6ca1\u6709\u5fc5\u8981\u3002\u00a9 2022 Elsevier B.V.<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-246788\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/3-4.png\" alt=\"\" width=\"860\" height=\"657\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/3-4.png 860w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/3-4-300x229.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/3-4-768x587.png 768w\" sizes=\"(max-width: 860px) 100vw, 860px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>1<\/strong> \u00a0\u5728500 \u00b0C \u4e0b\u9000\u706b\u7684\u5408\u6210\u4e8c\u5143 PR (Pt<sub>0.2<\/sub>Ru<sub>0.8<\/sub>O<sub>y<\/sub> ) \u548c\u4e09\u5143 PRT (Pt<sub>0.06<\/sub>Ru<sub>0.24<\/sub>Ti<sub>0.7<\/sub>O<sub>y<\/sub> ) \u9897\u7c92\u7684\u8868\u5f81\u3002(a) XRD \u5149\u8c31\u3002(b-d) XPS \u5149\u8c31\uff08b\uff1aRu 3d\uff0cc\uff1aPt 4f\uff0cd\uff1aTi 2p \u548c O 1s\uff09 <strong>\u00a9 2022 Elsevier B.V.<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-246789\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/4-4.png\" alt=\"\" width=\"927\" height=\"623\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/4-4.png 927w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/4-4-300x202.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/4-4-768x516.png 768w\" sizes=\"(max-width: 927px) 100vw, 927px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>2<\/strong> (a\u548cb)\u5206\u522b\u662f\u5408\u6210\u7684PR\u548cPRT\u9897\u7c92\u7684SEM\u56fe\u3002(c)\u5408\u6210Pt\u3001RuO<sub>2<\/sub>\u3001PR\u548cPRT\u6837\u54c1\u7684N<sub>2<\/sub>\u5438\u9644-\u89e3\u5438\u7b49\u6e29\u7ebf\u66f2\u7ebf\u3002\u63d2\u56fe\u663e\u793aBET\u8868\u9762\u79ef\u3002(d\u548ce) PRT\u6837\u54c1\u7684HR-TEM\u56fe\u50cf\u548cSAED\u6a21\u5f0f\u3002(f-j) PRT\u6837\u54c1\u7684EDS\u548c\u5143\u7d20\u6620\u5c04 <strong>\u00a9 2022 Elsevier B.V.<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-246790\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/5-2.png\" alt=\"\" width=\"927\" height=\"430\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/5-2.png 927w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/5-2-300x139.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/5-2-768x356.png 768w\" sizes=\"(max-width: 927px) 100vw, 927px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>3<\/strong> \u00a0(a) Pt, Ru, PR\u548cPRT\u7535\u6781\u57280.5 M NaCl\u6eb6\u6db2(pH 6)\u4e2d\u7684LSV\u3002\u4f5c\u4e3a\u6bd4\u8f83\uff0c\u4e5f\u4f7f\u75280.137 M NaCl\u62160.5 M NaClO<sub>4<\/sub> (pH 6)\u3002PRT(1\/4)\u662f\u6307\u8d1f\u8f7d\u8d28\u91cf\u4e3a0.83 mg cm<sup>\u22122<\/sup>\u7684PRT\u3002\u63d2\u56fe\u663e\u793a\u4e86PRT\u7535\u6781\u57280.5 M NaCl<strong>\u3001<\/strong><em>J<\/em> = 80 mA cm<sup>\u22122<\/sup>\u4e0b\u7684O<sub>2<\/sub>\u6790\u51fa\u53caFE\u3002(b) <em>J<\/em> = 80 mA cm<sup>\u22122<\/sup>\u65f6ClOR\u7684FE\u503c\u3002\u63d2\u56fe\u663e\u793a\u4e86\u5728J = 80 mA cm<sup>\u22122<\/sup>\u65f6\u81ea\u7531\u6c2f\u7684\u4ea7\u751f\u3002(c) C<sub>dl<\/sub>\u548cR<sub>ct<\/sub>\u503c\u3002(d)\u5728<em>J <\/em>= 800 mA cm<sup>\u22122<\/sup>\u6761\u4ef6\u4e0b\uff0c\u57280.941 M NaCl\u6eb6\u6db2\u4e2d\uff0c\u5bf9\u55b7\u6d82\u540e\u548c\u9000\u706b\u540e\u7684PRT\u9633\u6781\u8fdb\u884c\u957f\u65f6\u95f4\u7535\u89e3\u3002\u63d2\u56fe\u663e\u793a\u4e86\u57280.5 M NaCl\u6eb6\u6db2\u4e2d\u55b7\u6d82\u3001\u9000\u706b\u548c500 h\u4f7f\u7528\u7684PRT\u7535\u6781\u7684\u4f0f\u5b89\u56fe\u548cFE\u503c(<em>J<\/em> = 80 mA cm<sup>\u22122<\/sup>)\u3002\u8fd8\u663e\u793a\u4e86XRD\u5149\u8c31\u548cSEM\u56fe\u50cf(\u5de6:\u9000\u706b\u65f6\uff0c\u53f3:\u4f7f\u7528500 h) <strong>\u00a9 2022 Elsevier B.V.<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-246791\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/6-2.png\" alt=\"\" width=\"787\" height=\"597\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/6-2.png 787w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/6-2-300x228.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/6-2-768x583.png 768w\" sizes=\"(max-width: 787px) 100vw, 787px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>4<\/strong> \u5728\u4e0d\u540c\u6e29\u5ea6(200-500\u00b0C)\u4e0b\u9000\u706b\u7684MnOx\u7535\u6781(\u6c89\u79ef\u5728\u949b\u677f\u4e0a)\u7684\u8868\u5f81\u548c\u7535\u5316\u5b66\u5206\u6790\u3002\u9664\u975e\u53e6\u6709\u8bf4\u660e\uff0cMnOx\u4ee3\u8868MnOx-400(400\u00b0C\u9000\u706b)\u3002(a) XRD\u5149\u8c31\uff0c(b) HR-TEM\u548cSEM\u56fe\u50cf(\u5206\u522b\u4e3a\u9876\u90e8\u548c\u5e95\u90e8)\uff0c(c\u548cd) XPS\u5149\u8c31(\u5206\u522b\u4e3aMn 2p\u548cMn 3s)\uff0c (e) C<sub>dl<\/sub>\u548cR<sub>ct<\/sub>\u3002\u7535\u89e3100 h\u540e\uff0c\u7528XRD\u3001SEM\u3001XPS\u5bf9MnOx\u6837\u54c1\u8fdb\u884c\u4e86\u8868\u5f81 <strong>\u00a9 2022 Elsevier B.V.<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-246792\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/7-1.jpg\" alt=\"\" width=\"658\" height=\"489\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/7-1.jpg 658w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/7-1-300x223.jpg 300w\" sizes=\"(max-width: 658px) 100vw, 658px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>5<\/strong> \u00a0\u4f7f\u7528 Pt\u3001Ti \u548c MnOx\u7535\u6781\u5728pH 6\u7684 0.5 M NaCl\u30010.5 M NaCl \u548c 5 mM NaClO \u6216 0.4 M NaCl \u548c 0.1 M NaClO\u6eb6\u6db2\u4e2d\u5bf9ClRR \u548c HER \u7684\u7535\u5316\u5b66\u884c\u4e3a\u548c\u6d3b\u6027\u8fdb\u884c\u7814\u7a76\u3002\u9664\u975e\u53e6\u6709\u8bf4\u660e\uff0cMnOx\u4ee3\u8868MnOx-400(400\u00b0C\u9000\u706b)\u3002(a)LSV\u3002(b)\u7528CEM\u5206\u9694\u7684\u53cc\u5ba4\u7535\u6c60\uff0c\u57280.5 M NaCl\u548c5 mM NaClO<strong>\u3001<\/strong><em>J<\/em>=\u221210 mA cm<sup>\u22122<\/sup>\u4e0b\uff0c\u4e0d\u540c\u7535\u6781\u7684\u6c2f\u79bb\u5b50\u6d53\u5ea6(C<sub>t<\/sub> \/ C<sub>0<\/sub>)\u53d8\u5316\u3002\u63d2\u56fe\u663e\u793a30\u5206\u949f\u5185\u7684ClRR-FE\u503c(c) ClRR-FE\u503c\u4f5c\u4e3a<em>J<\/em>\u548cNaOCl\u6d53\u5ea6\u7684\u51fd\u6570\u3002(d)\u57280.5 M NaCl\u548c5 mM NaClO<strong>\u3001<\/strong><em>J<\/em>=\u221210 mA cm<sup>\u22122<\/sup>\u4e0b\uff0cHER-FE\u7684\u53d8\u5316 <strong>\u00a9 2022 Elsevier B.V.<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-246793\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/8-1.jpg\" alt=\"\" width=\"658\" height=\"445\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/8-1.jpg 658w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/02\/8-1-300x203.jpg 300w\" sizes=\"(max-width: 658px) 100vw, 658px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong> 6<\/strong> \u5728\u5355\u5ba4\u7535\u6c60\u4e2d\u4f7f\u7528 PRT \u9633\u6781\u548c MnOx\u9634\u6781 (PRT\/MnO x ) \u5bf9\u8fdb\u884c\u6d77\u6c34\u7535\u89e3\u3002(a) \u6bcf\u4e2a\u7535\u6781\u5728 0.5 M NaCl \u548c\u6d77\u6c34\u6eb6\u6db2\uff08\u76d0\u5ea6 36 g L<sup>-1<\/sup>\uff09\u4e2d\u7684LSV\u3002(b) \u6c2f\u7684\u751f\u4ea7\u548cClOR-FE\uff0c\u5728<em>J<sub>cell<\/sub><\/em> = 80 mA cm<sup>-2<\/sup>\u7684\u6d77\u6c34\u6eb6\u6db2\u4e2d\uff0c\u4f7f\u7528 PRT\/Ti \u548c PRT\/MnOx\u3002 (c) H<sub>2<\/sub>\u7684\u751f\u4ea7\u548c HER-FE\uff0c\u5728<em>J<sub>cell<\/sub><\/em> = 80 mA cm<sup>-2<\/sup>\u7684\u6d77\u6c34\u6eb6\u6db2\u4e2d\uff0c\u4f7f\u7528 PRT\/Ti \u548c PRT\/MnOx\u3002(d) \u4f7f\u7528 PRT\/MnOx\u7535\u6781\u5bf9\uff0c<em>J<sub>cell<\/sub><\/em> = 80 mA cm<sup>-2<\/sup>\u7684\u6d77\u6c34\u6eb6\u6db2\u4e2d\u8fdb\u884c\u957f\u65f6\u95f4\u7535\u89e3\u3002\u653e\u51fa\u7684 H<sub>2<\/sub>\u548c O<sub>2<\/sub>\u6c14\u4f53\u5728\u539f\u4f4d\u5b9e\u65f6\u6d4b\u91cf\uff0c\u540c\u65f6\u5bf9\u6c2f\u8fdb\u884c\u95f4\u6b47\u6027\u5206\u6790 <strong>\u00a9 2022 Elsevier B.V.<\/strong><\/p>\n<p><strong>\u4e94\u3001<\/strong><strong>\u3010\u6210\u679c\u542f\u793a\u3011<\/strong><\/p>\n<p>\u00a0 \u00a0\u5728\u8be5\u5de5\u4f5c\u4e2d\uff0c\u4f5c\u8005\u9996\u5148\u5f00\u53d1\u51fa\u4e00\u79cd\u4f18\u5f02\u7684ClOR\u9009\u62e9\u6027\u50ac\u5316\u5242\uff0c\u5e76\u5b9e\u73b0\u5de5\u4e1a\u7ea7\u7684\u7a33\u5b9a\u548c\u50ac\u5316\u6d3b\u6027\u3002\u8fd9\u4e3a\u6c2f\u78b1\u5de5\u4e1a\uff0c\u6c2f\u9178\u76d0\u5de5\u4e1a\u4ee5\u53ca\u6c34\u5904\u7406\u5de5\u4e1a\u63d0\u4f9b\u66f4\u9ad8\u6548\u7684\u9633\u6781\u9009\u62e9\u6027\u50ac\u5316\u5242\u3002\u540c\u65f6\u63d0\u51fa\u4e00\u79cd\u65b0\u9896\u7684\u76f4\u63a5\u6d77\u6c34\u7535\u89e3\u5236\u6c22\u7684\u7b56\u7565\uff0c\u5c06ClOR\u9009\u62e9\u6027\u9633\u6781\u548cHER\u9009\u62e9\u6027\u9634\u6781\u76f8\u7ed3\u5408\u5b9e\u73b0\u65e0\u819c\u65e0\u7f13\u51b2\u6d77\u6c34\u7535\u89e3\u4ea7\u9ad8\u7eaf\u6c22\u6c14\u3002\u8fd9\u79cd\u7b56\u7565\u4e3a\u5de5\u4e1a\u7535\u89e3\u5236\u6c22\u63d0\u4f9b\u65b0\u9896\u7684\u601d\u8def\uff0c\u540c\u65f6\u4e5f\u8fdb\u4e00\u6b65\u52a0\u5feb\u5b9e\u73b0\u6d77\u4e0a\u5236\u6c22\u548c\u6d77\u4e0aH<sub>2<\/sub>\u5feb\u901f\u8fd0\u8f93\u7684\u6b65\u4f10\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong>\u539f\u6587\u8be6\u60c5\uff1a<\/strong>https:\/\/doi.org\/10.1016\/j.apcatb.2022.122275<\/p>\n<p>\u672c\u6587\u7531K . L\u64b0\u7a3f\u3002<\/p>\n<p>&nbsp;<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4e00\u3001\u3010\u5bfc\u8bfb\u3011 \u00a0 \u00a0\u8fd1\u5e74\u6765\uff0c\u6d77\u6c34\u7535\u89e3\u5236\u6c22\u88ab\u8ba4\u4e3a\u662f\u80fd\u6e90\u8f6c\u578b\u7684\u5173\u952e\u6280\u672f\uff0c\u7136\u800c\u4ee5\u5f80\u7684\u7814\u7a76\u4e3b\u8981\u5173\u6ce8\u7684\u662f\u78b1\u6027\u6d77\u6c34\u3002\u5176\u4e2d\uff0c\u819c\uff08\u5206\u79bbH2\u548cO2\uff09\u548c\u8150\u8680\u6027 KOH (\u63d0\u9ad8\u6790\u6c27\u53cd&#8230;<\/p>\n","protected":false},"author":48789,"featured_media":246787,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[116,3592,18,54,4990],"class_list":["post-246786","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu","tag-catalyst","tag-3592","tag-xinnengyuan","tag-making","tag-4990"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/246786"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/48789"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=246786"}],"version-history":[{"count":8,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/246786\/revisions"}],"predecessor-version":[{"id":247570,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/246786\/revisions\/247570"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/246787"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=246786"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=246786"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=246786"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}