{"id":24744,"date":"2016-07-07T08:00:01","date_gmt":"2016-07-07T00:00:01","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=24744"},"modified":"2016-07-06T13:55:35","modified_gmt":"2016-07-06T05:55:35","slug":"%e6%96%b0%e5%9e%8b%e7%bb%9d%e7%bc%98%e7%8e%af%e8%a1%a8%e9%9d%a2%e5%b1%95%e7%8e%b0%e5%87%ba%e4%bb%a4%e4%ba%ba%e6%83%8a%e5%8f%b9%e7%9a%84%e6%80%a7%e8%83%bd","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=24744","title":{"rendered":"\u65b0\u578b\u7edd\u7f18\u73af\u8868\u9762\u5c55\u73b0\u51fa\u4ee4\u4eba\u60ca\u53f9\u7684\u6027\u80fd"},"content":{"rendered":"<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-25162 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/21-26-76835.jpg\" alt=\"21-26-76835\" width=\"600\" height=\"514\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/21-26-76835.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/21-26-76835-300x257.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: justify;\"><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>\u6765\u81ea\u7c73\u7eb3\u65af\u5409\u62c9\u65af\u5dde\u7ef4\u7d22\u8428\u548c\u5df4\u897f\u7684\u8054\u90a6\u5927\u5b66\u7684\u7814\u7a76\u8005\u4eec\u53d1\u73b0\u4e86\u7edd\u7f18\u73af\u8868\u9762\u4ee4\u4eba\u60ca\u53f9\u7684\u6027\u80fd\uff0c\u8868\u660e\u5176\u5728\u7535\u5b50\u5668\u4ef6\u65b9\u9762\u6709\u6f5c\u5728\u7684\u5e94\u7528\uff0c\u5e76\u5c06\u8fdb\u4e00\u6b65\u7814\u7a76\u5982\u4f55\u66f4\u597d\u7684\u63a7\u5236\u5176\u673a\u5236\u3002<\/p>\n<p style=\"text-align: justify;\">\u62d3\u6251\u7edd\u7f18\u4f53\u8868\u73b0\u4e3a\u5185\u90e8\u7edd\u7f18\u800c\u8868\u9762\u6709\u5f88\u597d\u7684\u5bfc\u7535\u6027\u3002\u8fd9\u4e9b\u7279\u70b9\u5f52\u529f\u4e8e\u5206\u522b\u57282007\u5e74\u548c2009\u5e74\u57282D\u548c3D\u6750\u6599\u4e2d\u53d1\u73b0\u7684\u65b0\u7684\u91cf\u5b50\u6001\u3002\u79d1\u5b66\u5bb6\u4eec\u7814\u7a76\u73af\u72b6\u6216\u73af\u5f62\u5706\u7eb9\u66f2\u9762\u3001\u62d3\u6251\u7edd\u7f18\u4f53\uff0c\u53d1\u73b0\u4e86\u5148\u524d\u5728\u7403\u5f62\u7edd\u7f18\u4f53\u4e2d\u8bc1\u5b9e\u7684\u7279\u5f81\u3002\u6765\u81ea\u7c73\u7eb3\u65af\u5409\u62c9\u65af\u5dde\u7ef4\u7d22\u8428\u548c\u5df4\u897f\u7684\u8054\u90a6\u5927\u5b66\u7684Jakson Fonseca\uff0c\u4e0e\u540c\u4e8b\u4eec\u4e00\u8d77\u5728\u4e00\u7bc7\u6587\u7ae0\u4e2d\u63cf\u8ff0\u4e86\u4ed6\u4eec\u7684\u53d1\u73b0\uff0c\u8be5\u6587\u7ae0\u53d1\u8868\u5728EPJ B\u4e0a\u3002\u8fd9\u4e9b\u7814\u7a76\u7ed3\u679c\u8868\u660e\u5176\u5728\u7535\u5b50\u5668\u4ef6\u65b9\u9762\u6709\u6f5c\u5728\u7684\u5e94\u7528\u3002\u786e\u5b9e\uff0c\u8fd9\u9879\u53d1\u73b0\u610f\u5473\u7740\u66f2\u9762\u5f15\u8d77\u5185\u90e8\u573a\uff0c\u79f0\u4e3a\u8ba1\u91cf\u573a\uff0c\u643a\u5e26\u7535\u8377\u7684\u7535\u5b50\u4f4d\u4e8e\u8868\u9762\u3002\u4e0e\u6b64\u76f8\u53cd\uff0c\u5728\u77f3\u58a8\u70ef\u4e2d\uff0c\u7c7b\u4f3c\u7684\u573a\u7531\u673a\u68b0\u5f20\u529b\u6216\u78b3\u539f\u5b50\u6392\u5217\u4e8e\u5355\u539f\u5b50\u539a\u5ea6\u8702\u7a9d\u72b6\u6676\u683c\u4e2d\u7684\u7f3a\u9677\u5f15\u8d77\u7684\u3002\u4f5c\u8005\u4eec\u8c03\u67e5\u4e86\u5728\u73af\u72b6\u8868\u9762\u5e26\u4e00\u4e2a\u7535\u8377\u7684\u9897\u7c92\u662f\u5426\u5177\u6709\u8be5\u7279\u5f81\uff0c\u88ab\u79f0\u4e3a\u76f8\u5bf9\u8bba\u8d28\u91cf\u7ebf\u6027\u8c31\u3002\u57282012\u5e74\uff0c\u4e00\u4e2a\u65e5\u672c\u7684\u56e2\u961f\u901a\u8fc7\u5728\u4e00\u4e2a\u7403\u4f53\u4e0a\u7684\u7814\u7a76\uff0c\u5bf9\u6b64\u505a\u4e86\u90e8\u5206\u56de\u5e94\u3002\u4e3a\u4e86\u660e\u767d\u7edd\u7f18\u4f53\u8868\u9762\u4e0a\u53d1\u751f\u4e86\u4ec0\u4e48\uff0c\u4ed6\u4eec\u4f7f\u7528\u4e86\u4e00\u4e2a\u57fa\u4e8e\u5fae\u5206\u51e0\u4f55\u5b66\u7684\u6570\u5b66\u65b9\u6cd5\u3002<\/p>\n<p style=\"text-align: justify;\">\u5728\u8fd9\u9879\u5de5\u4f5c\u4e2d\uff0c\u4f5c\u8005\u4eec\u8868\u660e\u5728\u73af\u72b6\u6750\u6599\u4e2d\u76f8\u5bf9\u8bba\u8c31\u4ecd\u4e0e\u7403\u72b6\u6750\u6599\u4e2d\u7684\u76f8\u540c\u3002\u5177\u4f53\u6765\u8bf4\uff0c\u4f5c\u8005\u4eec\u8868\u660e\u4e86\u5728\u73af\u72b6\u62d3\u6251\u7edd\u7f18\u4f53\u8868\u9762\u6709\u4e00\u4e2a\u96f6\u80fd\u91cf\u72b6\u6001\u3002\u4ed6\u4eec\u4e5f\u53d1\u73b0\u4e86\u66f2\u7387\u6548\u5e94\u5f15\u8d77\u4e86\u7535\u8377\u8f7d\u4f53\u548c\u53d8\u5316\u7684\u9ad8\u65af\u66f2\u7387\u95f4\u7684\u8026\u5408\uff0c\u7c7b\u4f3c\u4e8e\u540c\u8ba1\u91cf\u573a\u7684\u8026\u5408\u3002\u8fd9\u79cd\u8026\u5408\u8d1f\u8d23\u7535\u5b50\u81ea\u65cb\u7684\u4e24\u79cd\u4e0d\u540c\u7c7b\u578b\u91cf\u5b50\u529b\u5b66\u884c\u4e3a\uff08\u79f0\u4e3aBerry\u76f8\u4f4d\uff09\u548c\u5728\u5706\u73af\u4e2d\u5fc3\u5f15\u8d77\u7684\u4e00\u7cfb\u5217\u78c1\u5355\u6781\u3002<\/p>\n<p style=\"text-align: justify;\">\u63a5\u4e0b\u6765\u7684\u5de5\u4f5c\u662f\u8fdb\u4e00\u6b65\u7814\u7a76\u5982\u4f55\u66f4\u597d\u7684\u63a7\u5236\u8fd9\u4e9b\u5728\u62d3\u6251\u7edd\u7f18\u4f53\u4e2d\u5f15\u8d77\u8868\u9762\u8f7d\u4f53\u7684\u8ba1\u91cf\u573a\u7684\u673a\u5236\u3002<\/p>\n<p style=\"text-align: justify;\">\u539f\u6587\u53c2\u8003\u5730\u5740\uff1a<a href=\"http:\/\/esciencenews.com\/articles\/2016\/06\/29\/surprising.qualities.insulator.ring.surfaces\">http:\/\/esciencenews.com\/articles\/2016\/06\/29\/surprising.qualities.insulator.ring.surfaces<\/a><\/p>\n<p style=\"text-align: justify;\">\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u987e\u73a5\u63d0\u4f9b\u7d20\u6750\uff0c\u6731\u661f\u70e8\u7f16\u8bd1\u3002<\/p>\n<p style=\"text-align: justify;\">\u6750\u6599\u725b\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u8fd9\u91cc\u6c47\u96c6\u4e86\u5404\u5927\u9ad8\u6821\u7855\u535a\u751f\u3001\u4e00\u7ebf\u79d1\u7814\u4eba\u5458\u4ee5\u53ca\u884c\u4e1a\u4ece\u4e1a\u8005\uff0c\u5982\u679c\u60a8\u5bf9\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u8fdb\u5c55\uff0c\u89e3\u8bfb\u9ad8\u6c34\u5e73\u6587\u7ae0\u6216\u662f\u8bc4\u8ff0\u884c\u4e1a\u6709\u5174\u8da3\uff0c<a href=\"http:\/\/cailiaoren.mikecrm.com\/6qSdMU\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u6765\u81ea\u7c73\u7eb3\u65af\u5409\u62c9\u65af\u5dde\u7ef4\u7d22\u8428\u548c\u5df4\u897f\u7684\u8054\u90a6\u5927\u5b66\u7684\u7814\u7a76\u8005\u4eec\u53d1\u73b0\u4e86\u7edd\u7f18\u73af\u8868\u9762\u4ee4\u4eba\u60ca\u53f9\u7684\u6027\u80fd\uff0c\u8868\u660e\u5176\u5728\u7535\u5b50\u5668\u4ef6\u65b9\u9762\u6709\u6f5c\u5728\u7684\u5e94\u7528\uff0c\u5e76\u5c06\u8fdb\u4e00\u6b65\u7814\u7a76\u5982\u4f55\u66f4\u597d\u7684\u63a7\u5236\u5176\u673a\u5236&#8230;<\/p>\n","protected":false},"author":60,"featured_media":24746,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[31],"class_list":["post-24744","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-keji","tag-dianzi"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/24744"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/60"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=24744"}],"version-history":[{"count":5,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/24744\/revisions"}],"predecessor-version":[{"id":25163,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/24744\/revisions\/25163"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/24746"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=24744"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=24744"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=24744"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}