{"id":251425,"date":"2023-05-28T07:48:05","date_gmt":"2023-05-27T23:48:05","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=251425"},"modified":"2023-05-28T07:52:33","modified_gmt":"2023-05-27T23:52:33","slug":"%e6%9a%a8%e5%8d%97%e5%a4%a7%e5%ad%a6%e5%ad%9f%e7%8e%89%e8%8b%b1small%ef%bc%9a%e5%a4%9a%e5%ad%94%e7%a2%b3%e8%b4%9f%e8%bd%bd%e9%ab%98%e5%af%86%e5%ba%a6%e9%93%81%e5%8d%95%e5%8e%9f%e5%ad%90%e5%82%ac-2","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=251425","title":{"rendered":"\u66a8\u5357\u5927\u5b66\u5b5f\u7389\u82f1Small\uff1a\u591a\u5b54\u78b3\u8d1f\u8f7d\u9ad8\u5bc6\u5ea6\u94c1\u5355\u539f\u5b50\u50ac\u5316\u5242\u5b9e\u73b0\u9ad8\u6548\u6c27\u8fd8\u539f"},"content":{"rendered":"<p><strong>\u4e00\u3001<\/strong><strong>\u00a0<\/strong><strong>\u3010\u5bfc\u8bfb\u3011 \u00a0<\/strong><\/p>\n<p>\u8d28\u5b50\u4ea4\u6362\u819c\u71c3\u6599\u7535\u6c60\uff08PEMFC\uff09\u548c\u91d1\u5c5e-\u7a7a\u6c14\u7535\u6c60\u7531\u4e8e\u6c27\u8fd8\u539f\u53cd\u5e94\uff08ORR\uff09\u590d\u6742\u7684\u56db\u7535\u5b50\u8f6c\u79fb\u3001\u7f13\u6162\u7684\u52a8\u529b\u5b66\u53ca\u6240\u9700\u4ef7\u683c\u6602\u8d35\u7684\u8d35\u91d1\u5c5e\u50ac\u5316\u5242\u6210\u4e3a\u5236\u7ea6\u8be5\u7c7b\u5668\u4ef6\u53d1\u5c55\u7684\u74f6\u9888\u4e4b\u4e00\u3002\u8fc7\u6e21\u91d1\u5c5e\u5355\u539f\u5b50\u50ac\u5316\u5242\uff08SACs\uff09\u7531\u4e8e\u5176100%\u7684\u539f\u5b50\u5229\u7528\u7387\uff0c\u4f18\u5f02\u7684\u50ac\u5316\u6d3b\u6027\u548c\u9009\u62e9\u6027\uff0c\u88ab\u8ba4\u4e3a\u6700\u6709\u524d\u666f\u7684ORR\u50ac\u5316\u5242\u3002\u4f46\u5355\u539f\u5b50\u7ed3\u6784\u6613\u53d1\u751f\u805a\u96c6\u800c\u5f62\u6210\u56e2\u7c07\u6216\u7eb3\u7c73\u9897\u7c92\uff0c\u83b7\u5f97\u9ad8\u8d28\u91cf\u5bc6\u5ea6\u5355\u539f\u5b50\u4ecd\u5177\u6709\u5de8\u5927\u6311\u6218\u3002<\/p>\n<p><strong>\u4e8c\u3001\u3010\u6210\u679c\u63a0\u5f71\u3011<\/strong><\/p>\n<p>\u57fa\u4e8e\u6b64\uff0c\u66a8\u5357\u5927\u5b66\u5b5f\u7389\u82f1\u526f\u6559\u6388\u548c\u7f8e\u56fd\u65b0\u6cfd\u897f\u5dde\u7acb\u5927\u5b66Tewodros Asefa\u6559\u6388\uff08\u5171\u540c\u901a\u8baf\uff09\u7b49\u4eba\u901a\u8fc7\u9ad8\u6e29\u70ed\u89e3\u805a\u5421\u54af\u7edc\u5408\u94c1\u524d\u9a71\u4f53\uff08PPY-Fe\uff09\u53ca\u76d0\u9178\u523b\u8680\u5904\u7406\uff0c\u8bbe\u8ba1\u51fa\u4e00\u79cd\u6c2e\u63ba\u6742\u591a\u5b54\u78b3\u8d1f\u8f7d\u9ad8\u5bc6\u5ea6\u94c1\u5355\u539f\u5b50\u50ac\u5316\u5242\uff08Fe<sub>SA<\/sub>\/NMCs\uff09\u3002\u7814\u7a76\u53d1\u73b0\uff0c\u94c1\u5355\u539f\u5b50Fe<sub>SA<\/sub>\/NMC-800\u8d28\u91cf\u5bc6\u5ea6\u53ef\u9ad8\u8fbe4.05 wt.\u00a0%\uff0c\u6ca1\u6709\u751f\u6210\u94c1\u884d\u751f\u6676\u4f53\u7eb3\u7c73\u9897\u7c92\u6216\u94c1\u56e2\u7c07\uff0c\u663e\u793a\u51fa\u9ad8\u5bc6\u5ea6\u5b64\u7acb\u7684\u94c1\u5355\u539f\u5b50\u3002\u540c\u6b65\u8f90\u5c04\u6d4b\u8bd5\u7ed3\u679c\u8868\u660e\u5927\u91cf\u5b64\u7acb\u7684\u94c1\u5355\u539f\u5b50\u4ee5Fe-N<sub>4<\/sub>\u7684\u914d\u4f4d\u7ed3\u6784\u951a\u5b9a\u5728\u591a\u5b54\u6c2e\u63ba\u6742\u78b3\u8f7d\u4f53\u4e0a\u3002\u7535\u5316\u5b66\u7ed3\u679c\u8868\u660e\uff0c\u5f53\u70ed\u89e3\u6e29\u5ea6\u4e3a800 \u2103\u65f6\uff0c\u6240\u5f97\u6750\u6599Fe<sub>SA<\/sub>\/NMC-800\u5728\u9178\u6027\u548c\u78b1\u6027\u4ecb\u8d28\u4e2d\u5747\u8868\u73b0\u51fa\u4f18\u5f02\u7684ORR\u6d3b\u6027\uff0c\u5176\u6d3b\u6027\u4e0e\u5546\u4e1a\u7684Pt\/C\uff0820 wt. %\uff09\u50ac\u5316\u5242\u76f8\u5ab2\u7f8e\u3002\u57280.1 M HClO<sub>4<\/sub>\u548c0.1 M KOH\u6eb6\u6db2\u4e2d\uff0cORR\u5177\u6709\u8f83\u6b63\u7684\u8d77\u59cb\u7535\u4f4d\uff0c\u5206\u522b\u4e3a0.93\u548c0.98 V\u3002\u540c\u65f6\uff0c\u8be5\u50ac\u5316\u5242\u5728\u4e24\u79cd\u7535\u89e3\u8d28\u4e2d\u5747\u5177\u6709\u8f83\u9ad8\u7684\u7535\u5b50\u8f6c\u79fb\u6570\uff08~ 4\uff09\u3001\u4f18\u5f02\u7684\u8010\u4e45\u6027\u548c\u8010\u7532\u9187\u6027\u3002\u6b64\u5916\uff0cFe<sub>SA<\/sub>\/NMC-800\u4f5c\u4e3a\u9634\u6781\u7535\u50ac\u5316\u5242\uff0c\u5728PEMFC\u548c\u950c-\u7a7a\u6c14\u7535\u6c60\u4e2d\u8868\u73b0\u51fa\u4f18\u5f02\u7684\u50ac\u5316\u6027\u80fd\uff0c\u6700\u9ad8\u529f\u7387\u5bc6\u5ea6\u53ef\u5206\u522b\u9ad8\u8fbe320\u548c91 mW cm<sup>-2<\/sup>\u3002\u76f8\u5173\u7814\u7a76\u6210\u679c\u4ee5\u201c<strong>High Density <\/strong><strong>Single <\/strong><strong>Fe<\/strong><strong>\u00a0Atoms <\/strong><strong>on<\/strong><strong>\u00a0Mesoporous N<\/strong><strong>&#8211;<\/strong><strong>D<\/strong><strong>oped <\/strong><strong>C<\/strong><strong>arbons: <\/strong><strong>Noble M<\/strong><strong>etal-<\/strong><strong>F<\/strong><strong>ree <\/strong><strong>E<\/strong><strong>lectrocatalyst<\/strong><strong>s<\/strong><strong>\u00a0for <\/strong><strong>O<\/strong><strong>xygen <\/strong><strong>R<\/strong><strong>eduction <\/strong><strong>R<\/strong><strong>eaction in <\/strong><strong>A<\/strong><strong>cidic<\/strong><strong>\u00a0<\/strong><strong>and<\/strong><strong>\u00a0A<\/strong><strong>lkaline <\/strong><strong>M<\/strong><strong>edia<\/strong>\u201d\u4e3a\u9898\u53d1\u8868\u5728\u56fd\u9645\u8457\u540d\u671f\u520a<strong><b>S<\/b><\/strong><strong><b>mall<\/b><\/strong>\u4e0a\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-1-1.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-251427\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-1-1.png\" alt=\"\" width=\"600\" height=\"277\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-1-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-1-1-300x139.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p><strong>\u00a0\u4e09\u3001\u3010\u6838\u5fc3\u521b\u65b0\u70b9\u3011<\/strong><\/p>\n<p>\u901a\u8fc7\u7403\u5dee\u7535\u955c\u3001\u540c\u6b65\u8f90\u5c04\u7b49\u8868\u5f81\u5206\u6790\u8bc1\u660e\u8be5\u6750\u6599\u4ee5\u5355\u539f\u5b50\u7ea7\u522b\u7684\u5f62\u5f0f\u5b58\u5728\u3002\u5e76\u901a\u8fc7\u7535\u5316\u5b66\u6d4b\u8bd5\u7684\u65b9\u6cd5\u63a2\u7d22\u94c1\u5355\u539f\u5b50ORR\u7684\u7535\u50ac\u5316\u6027\u80fd\uff0c\u8bc1\u660e\u5176\u50ac\u5316\u6d3b\u6027\u662f\u6765\u81ea\u5355\u539f\u5b50\u3002\u5e76\u5c06\u5355\u539f\u5b50\u6750\u6599\u8fdb\u884c\u4e86\u950c-\u7a7a\u7535\u6c60\u548cH<sub>2<\/sub>-O<sub>2<\/sub>\u9178\u6027\u8d28\u5b50\u4ea4\u6362\u819c\u71c3\u6599\u7535\u6c60\uff08PEMFC\uff09\u6d4b\u8bd5\uff0c\u5728\u7535\u6c60\u6d4b\u8bd5\u4e2d\u5747\u8868\u5148\u51fa\u4f18\u826f\u7684\u6027\u80fd\uff0c\u8fd9\u4f53\u73b0\u4e86\u8be5\u6750\u6599\u5728\u5b9e\u9645\u5e94\u7528\u4e2d\u5177\u6709\u4e00\u5b9a\u7684\u4ef7\u503c\u548c\u610f\u4e49\u3002\u5728\u9178\u6027\u4ecb\u8d28\u4e2d\u8fdb\u884c\u5bc6\u5ea6\u6cdb\u51fd\u7406\u8bba\u8ba1\u7b97\uff0c\u63ed\u793a\u50ac\u5316\u53cd\u5e94\u7684\u901f\u63a7\u6b65\u9aa4\u662f\u5438\u9644O<sub>2<\/sub>\u751f\u6210*OOH\uff0c\u8ba1\u7b97\u7ed3\u679c\u8868\u660e\uff0c\u77f3\u58a8\u70ef\u4e0a\u7684Fe-N<sub>4<\/sub>\u5177\u6709\u66f4\u6709\u7684ORR\u50ac\u5316\u6027\u80fd\u3002<\/p>\n<p><strong>\u00a0\u56db\u3001\u3010\u6570\u636e\u6982\u89c8\u3011<\/strong><\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-2-1.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-251428\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-2-1.png\" alt=\"\" width=\"600\" height=\"165\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-2-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-2-1-300x83.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p><strong>\u56fe1<\/strong>\u00a0N\u63ba\u6742\u4ecb\u5b54\u78b3\u8d1f\u8f7d\u94c1\u5355\u539f\u5b50\u50ac\u5316\u5242\uff08Fe<sub>SA<\/sub>\/NMCs\uff09\u5408\u6210\u8fc7\u7a0b\u793a\u610f\u56fe\u3002<strong>\u00a9<\/strong><strong>\u00a02023 Wiley<\/strong><\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-4-2.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-251429\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-4-2.png\" alt=\"\" width=\"600\" height=\"515\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-4-2.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-4-2-300x258.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p><strong>\u56fe2 <\/strong>a\uff09Fe<sub>SA<\/sub>\/NMC-800\u3001Fe<sub>3<\/sub>C\/NC-800\u548cNCB\u6750\u6599\u7684XRD\u56fe\uff1bb\uff09Fe<sub>3<\/sub>C\/NC-800 \u548cc\uff09Fe<sub>SA<\/sub>\/NMC-800\u7684TEM\u56fe\u50cf\uff1bd\uff09HR-TEM\u56fe\u50cf\uff1be-f\uff09AC HAADF-STEM\u56fe\u50cf\uff08\u5176\u4e2d\u5b64\u7acb\u7684 Fe \u6d3b\u6027\u4f4d\u70b9\u7528\u9ec4\u8272\u5706\u5708\u7a81\u51fa\u663e\u793a\uff09\uff1bg\uff09Fe<sub>SA<\/sub>\/NMC-800\u7684STEM\u56fe\u50cf\u548ch-k\uff09Fe\u3001N\u3001O \u548cC\u7684\u76f8\u5e94\u5143\u7d20\u6620\u5c04\u56fe\u50cf\u3002<strong>\u00a9<\/strong><strong>\u00a02023 Wiley<\/strong><\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-3-3.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-251430\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-3-3.png\" alt=\"\" width=\"600\" height=\"450\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-3-3.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-3-3-300x225.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p><strong>\u56fe3 <\/strong>a\uff09Fe<sub>3<\/sub>C\/NC-800\u3001Fe<sub>SA<\/sub>\/NMC-800 \u548cNCB\u7684\u62c9\u66fc\u5149\u8c31\uff1bb\uff09Fe<sub>3<\/sub>C\/NC-800\u3001Fe<sub>SA<\/sub>\/NMC-800 \u548c NCB\u7684XPS\u6d4b\u91cf\u5149\u8c31\uff1bc\uff09Fe<sub>SA<\/sub>\/NMC-T\u6750\u6599\u4e2dN:C\u548cFe:C\u7684\u539f\u5b50\u6bd4\u4e0e\u70ed\u89e3\u6e29\u5ea6\u7684\u51fd\u6570\u5173\u7cfb\uff1bFe<sub>SA<\/sub>\/NMC-800\u7684 d\uff09N 1s\u548ce\uff09C 1s\u5cf0\u7684\u9ad8\u5206\u8fa8\u7387XPS\u5149\u8c31\uff1bf\uff09\u5f52\u4e00\u5316\u7684 Fe-K\u8fb9\u7f18XANES\u5149\u8c31\uff1bg\uff09Fe<sub>SA<\/sub>\/NMC-800\u3001Fe \u7b94\u548cFe<sub>2<\/sub>O<sub>3<\/sub>\u7684k3\u52a0\u6743EXAFS\u5149\u8c31\u7684FT \uff1bh\uff09Fe K\u8fb9\u7684EXAFS\u5149\u8c31\uff0c\u63d2\u56fe\u4e3a\u6750\u6599\u4e0aFe\u914d\u4f4d\u73af\u5883\u7684\u793a\u610f\u56fe\uff0c\u5176\u4e2d\u989c\u8272\u8868\u793a\u4e3a\uff1a\u7ea2\u8272\u4ee3\u8868Fe\uff0c\u84dd\u8272\u4ee3\u8868N\uff0c\u7070\u8272\u4ee3\u8868C\uff1bi\uff09Fe<sub>SA<\/sub>\/NMC-800\u7684WT EXAFS\u5149\u8c31\u3002<strong>\u00a9<\/strong><strong>\u00a02023 Wiley<\/strong><\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-5-1.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-251431\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-5-1.png\" alt=\"\" width=\"600\" height=\"460\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-5-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-5-1-300x230.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p><strong>\u56fe4 <\/strong>a\uff09Fe<sub>SA<\/sub>\/NMC-800\u3001Fe<sub>3<\/sub>C\/NC-800 \u548c NCB\u7535\u50ac\u5316\u5242\u5728\u9971\u548cO<sub>2<\/sub>\u76840.1 M\u00a0HClO<sub>4<\/sub>\u6eb6\u6db2\u4e2d\u7535\u50ac\u5316ORR \u7684LSV\u66f2\u7ebf\uff1bb\uff09\u76f8\u5e94 \u7684Tafel \u56fe\uff1bc\uff09Fe<sub>SA<\/sub>\u00a0\/NMC-800 \u5728\u4e0d\u540c\u901f\u5ea6\u4e0b\u7535\u50ac\u5316ORR\u7684LSV\u66f2\u7ebf\u548c\uff1bd\uff09\u76f8\u5e94\u7684K\u00a0&#8211;\u00a0L\u56fe\uff1be\uff09J<sub>L<\/sub>\u7684\u503c\u4e0e\u70ed\u89e3\u6e29\u5ea6\u7684\u51fd\u6570\u5173\u7cfb\uff1bf\uff09Fe<sub>SA<\/sub>\/NMC-800 \u548c\u5546\u7528 Pt\/C\uff0820\u00a0wt%\uff09\u7535\u50ac\u5316\u5242\u8ba1\u65f6\u7535\u6d41\u66f2\u7ebf\uff1b\u00a0g\uff09\u8010\u7532\u9187\u4ea4\u53c9\u53cd\u5e94\u56fe\uff1bh\uff09\u50ac\u5316\u5242\u6bd2\u5316\u5b9e\u9a8c\uff1bi\uff09\u4f7f\u7528Fe<sub>SA<\/sub>\u00a0\/NMC-800 \u548c 40 wt. % Pt\/C \u4f5c\u4e3a\u7535\u6781\u4e0a\u7684\u7535\u50ac\u5316\u5242\u7ec4\u88c5\u7684 PEMFC \u7684\u6781\u5316\u548c\u529f\u7387\u5bc6\u5ea6\u4e0e\u7535\u6d41\u5bc6\u5ea6\u66f2\u7ebf\u3002<strong>\u00a9<\/strong><strong>\u00a02023 Wiley<\/strong><\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-7-1.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-251433\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-7-1.png\" alt=\"\" width=\"600\" height=\"279\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-7-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-7-1-300x140.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p><strong>\u56fe5<\/strong><strong>\u00a0<\/strong>a\uff09Fe<sub>SA<\/sub>\/NMC-800\u3001Fe<sub>3<\/sub>C\/NC-800 \u548c NCB\u5728\u9971\u548cO<sub>2<\/sub>\u7684 0.1\u00a0M\u00a0KOH \u6eb6\u6db2\u4e2d\u7535\u50ac\u5316ORR\u7684LSV \u66f2\u7ebf\uff1bb\uff09Fe<sub>SA<\/sub>\/NMC-800 \u7535\u50ac\u5316\u5728\u4e0d\u540c\u8f6c\u901f\u4e0b\u7528 RDE \u83b7\u5f97\u7684 ORR \u7684 LSV \u66f2\u7ebf\uff1bc\uff09\u76f8\u5e94\u7684<em><i>K<\/i><\/em>\u00a0&#8211;\u00a0<em><i>L<\/i><\/em>\u56fe\uff1bd\uff09\u5728 Fe<sub>SA<\/sub>\/NMC-800, Fe<sub>3<\/sub>C\/NC-800 \u548c NCB \u50ac\u5316\u5242\u4e0a\u7684\u7535\u50ac\u5316ORR \u8fc7\u7a0b\u4e2dn\u503c\u548cH<sub>2<\/sub>O<sub>2<\/sub>\u7684\u4ea7\u7387\u4e0e\u7535\u538b\u7684\u5173\u7cfb\u56fe\uff1be\uff09Fe<sub>SA<\/sub>\/NMC-800\u548cPt\/C\uff0840 <em><i>wt.<\/i><\/em>\u00a0%\uff09\u50ac\u5316\u7684\u81ea\u5236\u950c-\u7a7a\u6c14\u7535\u6c60\u653e\u7535\u6781\u5316\u53ca\u529f\u7387\u66f2\u7ebf\u3002F\uff09Fe<sub>SA<\/sub>\/NMC-800\u548cPt\/C\uff0840<em><i>\u00a0wt.<\/i><\/em>\u00a0%\uff09+\u00a0RuO<sub>2<\/sub>\u5206\u522b\u4f5c\u4e3a\u9634\u6781\u7aef\u548c\u9633\u6781\u7aef\u50ac\u5316\u5242\u7ec4\u88c5\u7684\u950c-\u7a7a\u6c14\u7535\u6c60\u5728\u7535\u6d41\u5bc6\u5ea6\u4e3a5 mA cm<sup>-2<\/sup>\u65f6\u7684\u6052\u6d41\u653e\u7535-\u5145\u7535\u5faa\u73af\u66f2\u7ebf.<strong>\u00a0\u00a9<\/strong><strong>\u00a02023 Wiley<\/strong><\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-6-2.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-251434\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-6-2.png\" alt=\"\" width=\"600\" height=\"228\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-6-2.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/05\/\u56fe\u7247-6-2-300x114.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p><strong>\u56fe6<\/strong><strong>\u00a0<\/strong>a\uff09\u6c2e\u63ba\u6742\u77f3\u58a8\u70ef\u548c\u77f3\u58a8\u70ef\u4e0a\u5355\u539f\u5b50Fe-N<sub>4<\/sub>\uff0cb\uff09Fe<sub>3<\/sub>C \uff08002\uff09\u00a0\u53cd\u5e94\u81ea\u7531\u80fd\u53d8\u5316\u3002<strong>\u00a9<\/strong><strong>\u00a02023 Wiley<\/strong><\/p>\n<p><strong>\u4e94\u3001\u3010\u6210\u679c\u542f\u793a\u3011<\/strong><\/p>\n<p>\u7efc\u4e0a\u6240\u8ff0\uff0c\u4f5c\u8005\u901a\u8fc7\u70ed\u89e3Fe-PPY\uff0c\u7136\u540e\u8680\u523b\u6210\u529f\u5408\u6210\u4e86\u4ee5Fe-N\u00a0<sub>4<\/sub>\u5f62\u5f0f\u5206\u6563\u5728N\u63ba\u6742\u4ecb\u5b54\u78b3\u4e0a\u7684\u9ad8\u5bc6\u5ea6Fe\u5355\u539f\u5b50\u6750\u6599\u3002\u6750\u6599\u4e2dFe-N<sub>4<\/sub>\u7684\u9ad8\u5bc6\u5ea6\u4f4d\u70b9\u548c\u4ecb\u5b54\u7ed3\u6784\u4f7f\u5b83\u4eec\u80fd\u591f\u5728\u9178\u6027\u548c\u78b1\u6027\u4ecb\u8d28\u4e2d\u5bf9 ORR \u8868\u73b0\u51fa\u826f\u597d\u7684\u4f20\u8d28\u548c\u7535\u50ac\u5316\u6d3b\u6027\u3002\u5b83\u8fd8\u5728 PEMFC \u548c\u950c-\u7a7a\u6c14\u7535\u6c60\u4e2d\u4f5c\u4e3a\u7535\u50ac\u5316\u5242\u8868\u73b0\u51fa\u826f\u597d\u7684\u6027\u80fd\uff0c\u8868\u660e\u5176\u5728\u80fd\u91cf\u8f6c\u6362\u548c\u5b58\u50a8\u7cfb\u7edf\u7684\u5b9e\u9645\u5e94\u7528\u4e2d\u5177\u6709\u53ef\u884c\u6027\u3002\u8fd9\u9879\u5de5\u4f5c\u4e3a\u5355\u539f\u5b50\u50ac\u5316\u5242\u4f5c\u4e3a\u9ad8\u6d3b\u6027\u3001\u9ad8\u7a33\u5b9a\u6027\u7684ORR\u7535\u50ac\u5316\u5242\u63d0\u4f9b\u65b0\u9896\u3001\u6709\u6548\u7684\u8bbe\u8ba1\u9014\u5f84\u3002<\/p>\n<p><strong>\u539f\u6587\u8be6\u60c5<\/strong>\uff1aHigh Density Single Fe\u00a0Atoms on\u00a0Mesoporous N-Doped Carbons: Noble Metal-Free Electrocatalysts\u00a0for Oxygen Reduction Reaction in Acidic\u00a0and\u00a0Alkaline Media.\u00a0<em><i>Small<\/i><\/em>, 2023,\u00a0https:\/\/doi.org\/10.1002\/smll.202303214.<\/p>\n<p>\u672c\u6587\u7531\u4f5c\u8005\u4f9b\u7a3f<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4e00\u3001\u00a0\u3010\u5bfc\u8bfb\u3011 \u00a0 \u8d28\u5b50\u4ea4\u6362\u819c\u71c3\u6599\u7535\u6c60\uff08PEMFC\uff09\u548c\u91d1\u5c5e-\u7a7a\u6c14\u7535\u6c60\u7531\u4e8e\u6c27\u8fd8\u539f\u53cd\u5e94\uff08ORR\uff09\u590d\u6742\u7684\u56db\u7535\u5b50\u8f6c\u79fb\u3001\u7f13\u6162\u7684\u52a8\u529b\u5b66\u53ca\u6240\u9700\u4ef7\u683c\u6602\u8d35\u7684\u8d35\u91d1\u5c5e\u50ac\u5316\u5242\u6210\u4e3a\u5236\u7ea6\u8be5&#8230;<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-251425","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/251425"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=251425"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/251425\/revisions"}],"predecessor-version":[{"id":251436,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/251425\/revisions\/251436"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=251425"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=251425"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=251425"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}