{"id":252199,"date":"2023-06-20T06:27:50","date_gmt":"2023-06-19T22:27:50","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=252199"},"modified":"2023-06-19T11:46:44","modified_gmt":"2023-06-19T03:46:44","slug":"%e4%b8%ad%e7%a7%91%e9%99%a2%e7%90%86%e5%8c%96%e6%89%80%e7%8e%8b%e6%a0%91%e6%b6%9b-%e6%97%b6%e8%bf%9e%e9%91%ab%e5%9b%a2%e9%98%9f%e3%80%8aam%e3%80%8b%ef%bc%9a%e5%88%86%e5%bd%a2%e8%87%aa%e6%b3%b5","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=252199","title":{"rendered":"\u4e2d\u79d1\u9662\u7406\u5316\u6240\u738b\u6811\u6d9b\/\u65f6\u8fde\u946b\u56e2\u961f\u300aAM\u300b\uff1a\u5206\u5f62\u81ea\u6cf5\u6cb9\u6c34\u51dd\u80f6\u6577\u6599\u4fc3\u8fdb\u70e7\u70eb\u4f24\u521b\u9762\u6108\u5408"},"content":{"rendered":"<p><strong>\u4e00\u3001<\/strong><strong>\u00a0<\/strong><strong>\u3010\u5bfc\u8bfb\u3011 \u00a0<\/strong><\/p>\n<p>\u70e7\u70eb\u4f24\u4f24\u53e3\u4e2d\u6c34\u80bf\u7ec4\u7ec7\u548c\u5927\u91cf\u6c34\u6ce1\u5206\u6ccc\u7684\u8fc7\u91cf\u6e17\u51fa\u6db2\uff0c\u4e25\u91cd\u963b\u788d\u4e86\u521b\u9762\u6108\u5408\uff0c\u5bf9\u4f20\u7edf\u6577\u6599\u63d0\u51fa\u5de8\u5927\u6311\u6218\u3002<\/p>\n<p><strong>\u4e8c\u3001\u3010\u6210\u679c\u63a0\u5f71\u3011<\/strong><\/p>\n<p>\u4e3a\u6b64\uff0c<strong><b>\u4e2d\u79d1\u9662\u7406\u5316\u6240<\/b><\/strong><strong><b>\u738b\u6811\u6d9b<\/b><\/strong><strong><b>\/<\/b><\/strong><strong><b>\u65f6\u8fde\u946b<\/b><\/strong><strong><b>\u56e2\u961f\u62a5\u9053\u4e86<\/b><\/strong><strong><b>\u4e00\u79cd\u5177\u6709\u5206\u5f62\u4eb2\u6c34\u5fae\u901a\u9053\u7684\u81ea\u6cf5\u6cb9\u6c34\u51dd\u80f6\uff0c\u53ef\u4ee5\u5feb\u901f\u79fb\u9664\u8fc7\u91cf\u6e17\u51fa\u6db2\uff0c\u6548\u7387\u6bd4\u7eaf\u6c34\u51dd\u80f6\u63d0\u9ad8\u7ea630\u500d\uff0c\u5e76\u6709\u6548\u5730\u4fc3\u8fdb<\/b><\/strong><strong><b>\u70e7\u70eb\u4f24\u521b\u9762<\/b><\/strong><strong><b>\u6108\u5408<\/b><\/strong><strong><b>\u3002<\/b><\/strong>\u8be5\u7814\u7a76\u63d0\u51fa\u4e86\u4e00\u79cd\u52a8\u6001\u4e73\u5316\u8fc7\u7a0b\u8f85\u52a9\u7684\u4e73\u6db2\u754c\u9762\u805a\u5408\u65b9\u6cd5\uff0c\u501f\u52a9\u4e9a\u7a33\u6001\u4e73\u5316\u52a8\u6001\u8fc7\u7a0b\uff0c\u5236\u5907\u4e86\u5177\u6709\u5206\u5f62\u7ed3\u6784\u7684\u81ea\u6cf5\u6cb9\u6c34\u51dd\u80f6\u6577\u6599\u3002\u5728\u5927\u9f20\u70e7\u70eb\u4f24\u521b\u9762\u6a21\u578b\u4e2d\uff0c\u5206\u5f62\u81ea\u6cf5\u6cb9\u6c34\u51dd\u80f6\u6577\u6599\u53ef\u663e\u8457\u4fc3\u8fdb\u771f\u76ae\u3001\u8840\u7ba1\u3001\u6bdb\u56ca\u518d\u751f\uff0c\u76f8\u6bd4\u5546\u7528\u6577\u6599Tegaderm<sup>TM<\/sup>\uff0c\u65b0\u751f\u6bdb\u56ca\u6570\u76ee\u63d0\u9ad8\u7ea613.5\u500d\uff0c\u65b0\u751f\u8840\u7ba1\u6570\u76ee\u63d0\u9ad8\u7ea66.6\u500d\uff0c\u65b0\u751f\u771f\u76ae\u7a7a\u8154\u9762\u79ef\u51cf\u5c11\u7ea642.5%<strong><b>\u3002<\/b><\/strong>\u8be5\u7814\u7a76\u4e3a\u8bbe\u8ba1\u9ad8\u6027\u80fd\u70e7\u70eb\u4f24\u529f\u80fd\u6577\u6599\u63d0\u4f9b\u4e86\u65b0\u601d\u8def\uff0c\u8fd1\u65e5\u4ee5\u9898\u4e3a\u201cA Rapid Self-pumping Organohydrogel Dressing with Hydrophilic Fractal Microchannels to Promote Burn Wound Healing\u201d\u7684\u8bba\u6587\u53d1\u8868\u5728\u300a<strong><em><b><i>Advanced Materials<\/i><\/b><\/em><\/strong>\u300b\u4e0a\uff08<a href=\"https:\/\/doi.org\/10.1002\/adma.202301765\"><u>https:\/\/doi.org\/10.1002\/adma.202301765<\/u><\/a>\uff09\u3002\u4e2d\u56fd\u79d1\u5b66\u9662\u7406\u5316\u6280\u672f\u7814\u7a76\u6240\u5170\u664b\u6cfd\u535a\u58eb\u4e3a\u7b2c\u4e00\u4f5c\u8005\uff0c\u4e2d\u56fd\u79d1\u5b66\u9662\u7406\u5316\u6280\u672f\u7814\u7a76\u6240\u738b\u6811\u6d9b\u7814\u7a76\u5458\u548c\u65f6\u8fde\u946b\u526f\u7814\u7a76\u5458\u4e3a\u901a\u8baf\u4f5c\u8005\uff0c\u7814\u7a76\u5de5\u4f5c\u5f97\u5230\u4e86\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u548c\u4e2d\u79d1\u9662\u9752\u5e74\u521b\u65b0\u4fc3\u8fdb\u4f1a\u7684\u8d44\u52a9\u652f\u6301\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-252201\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/\u56fe\u7247-2-11.png\" alt=\"\" width=\"700\" height=\"305\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/\u56fe\u7247-2-11.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/\u56fe\u7247-2-11-300x131.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p><strong>\u4e09\u3001\u3010\u6838\u5fc3\u521b\u65b0\u70b9\u3011<\/strong><\/p>\n<p>\u901a\u8fc7\u4e00\u79cd\u4e73\u6cb9\u5316\u8fc7\u7a0b\u8f85\u52a9\u7684\u4e73\u6db2\u754c\u9762\u805a\u5408\u53cd\u5e94\u5236\u5907\u4e86\u542b\u6709\u5206\u5f62\u5fae\u901a\u9053\u7ed3\u6784\u7684\u81ea\u6cf5\u6cb9\u6c34\u51dd\u80f6\uff0c\u6781\u5927\u5730\u63d0\u5347\u4e86\u51dd\u80f6\u7684\u5438\u6536\u6027\u80fd\uff0c\u6700\u7ec8\u5728\u52a8\u7269\u6a21\u578b\u4e0a\u5b9e\u73b0\u4fc3\u8fdb\u70e7\u4f24\u4f24\u53e3\u7684\u6108\u5408\u3002<\/p>\n<p><strong>\u56db\u3001\u3010\u6570\u636e\u6982\u89c8\u3011<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-252202\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/\u56fe\u7247-1-11.png\" alt=\"\" width=\"700\" height=\"560\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/\u56fe\u7247-1-11.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/\u56fe\u7247-1-11-300x240.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u56fe1\uff1a\u5feb\u901f\u81ea\u6cf5\u5206\u5f62\u6cb9\u6c34\u51dd\u80f6\u6577\u6599\u8bbe\u8ba1\u3002a\uff09\u5206\u5f62\u81ea\u6cf5\u6cb9\u6c34\u51dd\u80f6\u5feb\u901f\u5bfc\u51fa\u4f24\u53e3\u6e17\u51fa\u6db2\u4fc3\u8fdb\u70e7\u70eb\u4f24\u6108\u5408\u793a\u610f\u56fe\uff1bb\uff0cc\uff09\u81ea\u6cf5\u6cb9\u6c34\u51dd\u80f6\uff08b\uff09\u4e2d\u5206\u5f62\u6c34\u51dd\u80f6\u5fae\u901a\u9053\uff08c\uff09\u622a\u9762\u56fe\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-252203\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/\u56fe\u7247-3-10.png\" alt=\"\" width=\"700\" height=\"411\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/\u56fe\u7247-3-10.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/\u56fe\u7247-3-10-300x176.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u56fe2\uff1a\u5206\u5f62\u81ea\u6cf5\u6cb9\u6c34\u51dd\u80f6\uff08a\uff09\u3001\u5747\u76f8\u6cb9\u6c34\u51dd\u80f6\uff08b\uff09\u4e0e\u7eaf\u6c34\u51dd\u80f6\uff08c\uff09\u7684\u7ed3\u6784\u793a\u610f\u56fe\u548c\u52a8\u6001\u63a5\u89e6\u89d2\u66f2\u7ebf\u5bf9\u6bd4\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-252204\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/\u56fe\u7247-4-8.png\" alt=\"\" width=\"700\" height=\"640\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/\u56fe\u7247-4-8.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/\u56fe\u7247-4-8-300x274.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u56fe3\uff1a\u5206\u5f62\u81ea\u6cf5\u6cb9\u6c34\u51dd\u80f6\u6577\u6599\u4fc3\u8fdb\u5927\u9f20\u70e7\u70eb\u4f24\u521b\u9762\u6108\u5408\u3002a\uff09\u4e0d\u540c\u5904\u74067\u5929\u53ca21\u5929\u540e\uff0c\u65b0\u751f\u771f\u76aeH&amp;E\u67d3\u8272\u5207\u7247\u4e2d\u7a7a\u8154\u533a\u57df\uff08*\u6807\u6ce8\uff09\u5bf9\u6bd4\uff1bb\uff09\u4e0d\u540c\u5904\u740621\u5929\u540e\uff0c\u65b0\u751f\u7ec4\u7ec7\u514d\u75ab\u7ec4\u5316\u67d3\u8272\u5207\u7247\u4e2d\u65b0\u751f\u6bdb\u56ca\uff08\u84dd\u8272\u7bad\u5934\uff09\u548c\u8840\u7ba1\uff08\u7ea2\u8272\u7bad\u5934\uff09\u5bf9\u6bd4\uff1bc-e\uff09\u65b0\u751f\u771f\u76ae\u7a7a\u8154\u9762\u79ef\uff08c\uff09\uff0c\u65b0\u751f\u6bdb\u56ca\u6570\u76ee\uff08d\uff09\u4ee5\u53ca\u8840\u7ba1\u76f4\u5f84\uff08e\uff09\u5b9a\u91cf\u7edf\u8ba1\u3002<\/p>\n<p><strong>\u4e94\u3001\u3010\u6210\u679c\u542f\u793a\u3011<\/strong><\/p>\n<p>\u76f8\u6bd4\u4e8e\u4f20\u7edf\u6c34\u51dd\u80f6\uff0c\u672c\u7814\u7a76\u6240\u62a5\u9053\u7684\u81ea\u6cf5\u6cb9\u6c34\u51dd\u80f6\u901a\u8fc7\u6784\u7b51\u5206\u5f62\u6bdb\u7ec6\u5fae\u901a\u9053\u7ed3\u6784\u6781\u5927\u5730\u63d0\u5347\u4e86\u5438\u6c34\u6548\u7387\uff0c\u5b9e\u73b0\u4e86\u9ad8\u6548\u7ba1\u7406\u4f24\u53e3\u6e17\u51fa\u6db2\u3002\u4e3a\u8bbe\u8ba1\u9ad8\u6027\u80fd\u70e7\u70eb\u4f24\u529f\u80fd\u6577\u6599\u63d0\u4f9b\u4e86\u65b0\u601d\u8def\uff0c\u6709\u52a9\u4e8e\u65b0\u4e00\u4ee3\u529f\u80fd\u5316\u6577\u6599\u7684\u7814\u7a76\u4e0e\u8bbe\u8ba1\u3002<\/p>\n<p><strong>\u539f\u6587\u8be6\u60c5<\/strong>\uff1aLan, Jinze, Shi, Lianxin, Xiao, Wuyi, Zhang, Xiaobin and Wang, Shutao, A Rapid Self-pumping Organohydrogel Dressing with Hydrophilic Fractal Microchannels to Promote Burn Wound Healing. Adv. Mater., 2023, 2301765.<\/p>\n<p>DOI\uff1a<a href=\"https:\/\/doi.org\/10.1002\/adma.202301765\"><strong><u><b>https:\/\/doi.org\/10.1002\/adma.202301765<\/b><\/u><\/strong><\/a><\/p>\n<p>\u672c\u6587\u7531\u4f5c\u8005\u5170\u664b\u6cfd\u4f9b\u7a3f<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4e00\u3001\u00a0\u3010\u5bfc\u8bfb\u3011 \u00a0 \u70e7\u70eb\u4f24\u4f24\u53e3\u4e2d\u6c34\u80bf\u7ec4\u7ec7\u548c\u5927\u91cf\u6c34\u6ce1\u5206\u6ccc\u7684\u8fc7\u91cf\u6e17\u51fa\u6db2\uff0c\u4e25\u91cd\u963b\u788d\u4e86\u521b\u9762\u6108\u5408\uff0c\u5bf9\u4f20\u7edf\u6577\u6599\u63d0\u51fa\u5de8\u5927\u6311\u6218\u3002 \u4e8c\u3001\u3010\u6210\u679c\u63a0\u5f71\u3011 \u4e3a\u6b64\uff0c\u4e2d\u79d1\u9662\u7406\u5316\u6240\u738b\u6811\u6d9b\/\u65f6&#8230;<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-252199","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/252199"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=252199"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/252199\/revisions"}],"predecessor-version":[{"id":252205,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/252199\/revisions\/252205"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=252199"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=252199"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=252199"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}