{"id":252284,"date":"2023-06-24T06:54:27","date_gmt":"2023-06-23T22:54:27","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=252284"},"modified":"2023-06-23T21:58:22","modified_gmt":"2023-06-23T13:58:22","slug":"%e5%9b%9b%e5%b7%9d%e5%a4%a7%e5%ad%a6%e5%90%b4%e6%99%93%e4%b8%9cacs-sensors%ef%bc%9a%e5%9c%a8%e5%ae%b6%e4%b9%9f%e8%83%bd%e5%81%9a%e7%a0%94%e7%a9%b6%ef%bc%9f-%e5%ae%b6%e5%88%b6%e5%a4%9a","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=252284","title":{"rendered":"\u56db\u5ddd\u5927\u5b66\u5434\u6653\u4e1cACS Sensors\uff1a\u5728\u5bb6\u4e5f\u80fd\u505a\u7814\u7a76\uff1f \u2014 \u5bb6\u5236\u591a\u529f\u80fd\u5065\u5eb7\u76d1\u6d4b\u5e73\u53f0"},"content":{"rendered":"<p><strong>\u3010\u7814\u7a76\u80cc\u666f\u3011<\/strong><\/p>\n<p>\u67d4\u6027\u53ef\u7a7f\u6234\u667a\u80fd\u4f20\u611f\u5668\u5728\u4eba\u4f53\u751f\u547d\u4f53\u5f81\uff08\u5982\u4f53\u6e29\u3001\u5fc3\u7387\u3001\u547c\u5438\u9891\u7387\u7b49\uff09\u7684\u8fde\u7eed\u6027\u76d1\u6d4b\u65b9\u9762\u5177\u6709\u5de8\u5927\u7684\u5e94\u7528\u6f5c\u529b\u3002\u8fd1\u5e74\u6765\uff0c\u7528\u4e8e\u53ef\u7a7f\u6234\u5065\u5eb7\u76d1\u6d4b\u7684\u67d4\u6027\u4f20\u611f\u5668\u53d6\u5f97\u4e86\u663e\u8457\u8fdb\u5c55\uff0c\u7136\u800c\u7edd\u5927\u90e8\u5206\u62a5\u9053\u7684\u67d4\u6027\u4f20\u611f\u5668\u90fd\u6d89\u53ca\u590d\u6742\u7684\u5b9e\u9a8c\u5ba4\u5236\u5907\u6d41\u7a0b\uff08\u5982\u66dd\u5149\u3001\u8680\u523b\u3001\u771f\u7a7a\u9540\u819c\u3001\u4e8c\u7ef4\/\u4e09\u7ef4\u6253\u5370\u3001\u5408\u6210\/\u6539\u6027\/\u52a0\u5de5\u7b49\u5de5\u827a\uff09\uff0c\u4e14\u9700\u8981\u7528\u5230\u7279\u6b8a\u7684\u5fae\u7c73\/\u7eb3\u7c73\u6750\u6599\uff08\u5982\u91d1\u5c5e\u7eb3\u7c73\u5bfc\u7535\u6750\u6599\u3001\u78b3\u57fa\u7eb3\u7c73\u5bfc\u7535\u6750\u6599\u3001\u805a\u5408\u7269\u5bfc\u4f53\/\u534a\u5bfc\u4f53\u3001\u4e8c\u7ef4\u6750\u6599\u7b49\uff09\uff0c\u4e0a\u8ff0\u56e0\u7d20\u5728\u4e00\u5b9a\u7a0b\u5ea6\u4e0a\u9650\u5236\u4e86\u67d4\u6027\u4f20\u611f\u5668\u7684\u89c4\u6a21\u5316\u5236\u5907\u548c\u5927\u9762\u79ef\u90e8\u7f72\uff08\u5c24\u5176\u5728\u8d44\u6e90\u76f8\u5bf9\u532e\u4e4f\u7684\u573a\u666f\u6216\u5730\u533a\uff09\u3002\u5982\u4f55\u5229\u7528\u89e6\u624b\u53ef\u53ca\u7684\u751f\u6d3b\u7528\u54c1\u5728\u5c45\u5bb6\u6761\u4ef6\u4e0b\u5b9e\u73b0\u67d4\u6027\u667a\u80fd\u4f20\u611f\u5668\u4ef6\u7684\u7b80\u4fbf\u5316\u6784\u7b51\u4e0e\u6309\u9700\u8c03\u63a7\uff0c\u5bf9\u4e8e\u5bb6\u5ead\u5f0f\u5065\u5eb7\u76d1\u6d4b\u548c\u672a\u6765\u667a\u6167\u533b\u7597\u7684\u63a8\u5e7f\u548c\u666e\u53ca\u5177\u6709\u91cd\u8981\u7684\u73b0\u5b9e\u610f\u4e49\u3002<\/p>\n<p><strong>\u3010\u6587\u7ae0\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c<strong>\u56db\u5ddd\u5927\u5b66\u673a\u68b0\u5de5\u7a0b\u5b66\u9662\u5434\u6653\u4e1c\u7814\u7a76\u5458<\/strong><strong>\u7b49\u4eba<\/strong>\u63d0\u51fa\u4e00\u79cd\u5728\u5c45\u5bb6\u6761\u4ef6\u4e0b\u5229\u7528\u65e5\u5e38\u751f\u6d3b\u7528\u54c1\u6765\u6784\u5efa\u9ad8\u6027\u80fd\u3001\u591a\u529f\u80fd\u67d4\u6027\u4f20\u611f\u5668\u7684\u65b0\u65b9\u6cd5\u3002\u5177\u4f53\u5730\u8bb2\uff0c\u4f7f\u7528\u94c5\u7b14\u6d82\u5236\u5bfc\u7535\u77f3\u58a8\u6b63\u7535\u6781\uff0c\u4f7f\u7528\u5bb6\u7528\u94dd\u7b94\u4f5c\u4e3a\u8d1f\u7535\u6781\uff0c\u4f7f\u7528\u529e\u516c\u80f6\u6c34\u3001\u62a4\u80a4\u4fdd\u6e7f\u5242\u548c\u70f9\u996a\u98df\u76d0\u6765\u6784\u5efa\u56fa\u6001\u79bb\u5b50\u7535\u89e3\u8d28\u3002\u901a\u8fc7\u4e0a\u8ff0\u5bb6\u5236\u7535\u6781\u4e0e\u7535\u89e3\u8d28\u7684\u5408\u7406\u7ec4\u5408\uff0c\u53ef\u6784\u7b51\u4e00\u7cfb\u5217\u65b0\u578b\u7535\u4f4d\u5f0f\u529b\u5b66\u4f20\u611f\u5668\u3001\u7535\u4f4d\u5f0f\u6e29\u5ea6\u4f20\u611f\u5668\u53ca\u529b\/\u70ed\u591a\u529f\u80fd\u4f20\u611f\u5e73\u53f0\u3002\u57fa\u4e8e\u8be5\u7cfb\u5217\u5bb6\u5236\u4f20\u611f\u5668\u548c\u4f20\u611f\u5e73\u53f0\uff0c\u53ef\u5b9e\u73b0\u591a\u79cd\u4eba\u4f53\u5173\u952e\u751f\u547d\u4f53\u5f81\uff08\u5982\u4f53\u6e29\u3001\u5fc3\u7387\u3001\u547c\u5438\u9891\u7387\u3001\u54b3\u55fd\u3001\u4eba\u4f53\u6d3b\u52a8\u7b49\uff09\u7684\u53ef\u9760\u68c0\u6d4b\u4e0e\u8fde\u7eed\u76d1\u6d4b\uff0c\u4e14\u4f20\u611f\u5668\u53ef\u9760\u6027\u548c\u7a33\u5b9a\u6027\u53ef\u4e0e\u5546\u7528\u4f20\u611f\u5668\u76f8\u5ab2\u7f8e\u3002\u4e0a\u8ff0\u5de5\u4f5c\u4e3a\u5bb6\u5ead\u5f0f\u8fde\u7eed\u5065\u5eb7\u76d1\u6d4b\u63d0\u4f9b\u4e86\u4e00\u79cd\u4fbf\u6377\u800c\u6709\u6548\u7684\u65b0\u65b9\u6cd5\uff0c\u4e5f\u4e3a\u8d44\u6e90\u532e\u4e4f\u56fd\u5bb6\u548c\u5730\u533a\u7684\u6570\u5b57\u5316\u533b\u7597\u666e\u53ca\u63d0\u4f9b\u4e86\u4e00\u6761\u65b0\u9014\u5f84\u3002\u76f8\u5173\u7814\u7a76\u6210\u679c\u4ee5 \u201cHome-Made, Self-Powered, Skin-Attachable Sensing Platform for Diverse Vital Signs Monitoring\u201d \u4e3a\u9898\uff0c\u53d1\u8868\u5728\u4f20\u611f\u5668\u9886\u57df\u56fd\u9645\u8457\u540d\u671f\u520a\u300a<strong>ACS Sensors<\/strong>\u300b\u4e0a\uff08\u4e2d\u79d1\u96621\u533aTop\u671f\u520a\uff0c\u5f71\u54cd\u56e0\u5b50\uff1a9.618\uff09\uff0c<strong>\u8bba\u6587\u7b2c\u4e00\u4f5c\u8005\u548c\u901a\u8baf\u4f5c\u8005\u4e3a\u56db\u5ddd\u5927\u5b66\u5434\u6653\u4e1c\u7814\u7a76\u5458\uff0c\u52a0\u5dde\u5927\u5b66\u4f2f\u514b\u5229\u5206\u6821<\/strong><strong>Ana Arias<\/strong><strong>\u6559\u6388\u4e3a\u5171\u540c\u901a\u8baf\u4f5c\u8005\u3002<\/strong><\/p>\n<p><strong>\u00a0\u3010\u7814\u7a76\u5185\u5bb9\u3011<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-252291\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/1-3.jpg\" alt=\"\" width=\"1269\" height=\"1149\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/1-3.jpg 1269w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/1-3-300x272.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/1-3-768x695.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/1-3-1024x927.jpg 1024w\" sizes=\"(max-width: 1269px) 100vw, 1269px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>1. <\/strong>\u5bb6\u5236\u4f20\u611f\u5668\u53ca\u4f20\u611f\u5e73\u53f0\u7684\u5236\u5907\u539f\u6599\uff08\u59822B\u94c5\u7b14\u3001A4\u7eb8\u3001\u5bb6\u7528\u94dd\u7b94\u3001\u529e\u516c\u80f6\u6c34\u3001\u62a4\u80a4\u4fdd\u6e7f\u5242\u3001\u70f9\u996a\u98df\u76d0\u3001\u7802\u7eb8\u7b49\uff09\u3001\u5de5\u4f5c\u673a\u7406\u3001\u5668\u4ef6\u6784\u578b\u53ca\u5176\u5728\u4e0d\u540c\u4eba\u4f53\u5173\u952e\u751f\u547d\u4f53\u5f81\u76d1\u6d4b\uff08\u5305\u62ec\u4f53\u6e29\u3001\u5fc3\u7387\u3001\u547c\u5438\u9891\u7387\u3001\u54b3\u55fd\u7b49\uff09\u65b9\u9762\u7684\u5e94\u7528\u573a\u666f\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-252292\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/2-4.jpg\" alt=\"\" width=\"1269\" height=\"905\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/2-4.jpg 1269w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/2-4-300x214.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/2-4-768x548.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/2-4-1024x730.jpg 1024w\" sizes=\"(max-width: 1269px) 100vw, 1269px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>2. <\/strong>\u5bb6\u5236\u4f20\u611f\u5668\u53ca\u4f20\u611f\u5e73\u53f0\u4e0d\u540c\u7ec4\u5206\uff08\u5305\u62ec\u57fa\u4e8e\u80f6\u6c34\/\u4fdd\u6e7f\u5242\/\u98df\u76d0\u6240\u6784\u5efa\u7684\u56fa\u6001\u79bb\u5b50\u7535\u89e3\u8d28\u3001\u4f7f\u7528\u94c5\u7b14\u6d82\u5236\u7684\u5bfc\u7535\u77f3\u58a8\u7535\u6781\u7b49\uff09\u7684\u5236\u5907\u6d41\u7a0b\u3001\u6027\u80fd\u8868\u5f81\u53ca\u6700\u7ec8\u5668\u4ef6\u5c55\u793a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-252293\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/3-3.jpg\" alt=\"\" width=\"692\" height=\"554\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/3-3.jpg 692w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/3-3-300x240.jpg 300w\" sizes=\"(max-width: 692px) 100vw, 692px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>3. <\/strong>\u5bb6\u5236\u7535\u4f4d\u5f0f\u529b\u5b66\u4f20\u611f\u5668\u548c\u7535\u4f4d\u5f0f\u70ed\u5b66\u4f20\u611f\u5668\u7684\u7efc\u5408\u6027\u80fd\u8868\u5f81\u4e0e\u8bc4\u4f30\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-252294\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/4-2.jpg\" alt=\"\" width=\"1269\" height=\"721\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/4-2.jpg 1269w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/4-2-300x170.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/4-2-768x436.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/4-2-1024x582.jpg 1024w\" sizes=\"(max-width: 1269px) 100vw, 1269px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>4. <\/strong>\u5229\u7528\u5bb6\u5236\u7535\u4f4d\u5f0f\u529b\u5b66\u4f20\u611f\u5668\u76d1\u6d4b\u4eba\u4f53\u8109\u640f\u4fe1\u53f7\u3001\u4eba\u4f53\u5fc3\u7387\u53ca\u5176\u53d8\u5316\u60c5\u51b5\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-252295\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/5-1.jpg\" alt=\"\" width=\"1269\" height=\"590\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/5-1.jpg 1269w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/5-1-300x139.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/5-1-768x357.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/5-1-1024x476.jpg 1024w\" sizes=\"(max-width: 1269px) 100vw, 1269px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>5. <\/strong>\u57fa\u4e8e\u5bb6\u5236\u7535\u4f4d\u5f0f\u70ed\u5b66\u4f20\u611f\u5668\u76d1\u6d4b\u4eba\u4f53\u4e0d\u540c\u90e8\u4f4d\u4f53\u8868\u6e29\u5ea6\u53ca\u6e29\u5ea6\u53d8\u5316\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-252296\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/6-1.jpg\" alt=\"\" width=\"692\" height=\"456\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/6-1.jpg 692w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/6-1-300x198.jpg 300w\" sizes=\"(max-width: 692px) 100vw, 692px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>6.<\/strong> \u5229\u7528\u5bb6\u5236\u7535\u4f4d\u5f0f\u70ed\u5b66\u4f20\u611f\u5668\u76d1\u6d4b\u4eba\u4f53\u5b9e\u65f6\u547c\u5438\u72b6\u6001\uff08\u5305\u62ec\u6b63\u5e38\u547c\u5438\u548c\u5404\u79cd\u5f02\u5e38\u547c\u5438\u60c5\u51b5\uff09\u53ca\u5176\u547c\u5438\u901f\u7387\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-252297\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/7-1.jpg\" alt=\"\" width=\"692\" height=\"577\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/7-1.jpg 692w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/06\/7-1-300x250.jpg 300w\" sizes=\"(max-width: 692px) 100vw, 692px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>7<\/strong>. \u5229\u7528\u5bb6\u5236\u7535\u4f4d\u5f0f\u529b\u5b66\u4f20\u611f\u5668\u76d1\u6d4b\u4eba\u4f53\u547c\u5438\u72b6\u6001\u3001\u547c\u5438\u901f\u7387\u53ca\u54b3\u55fd\u8fc7\u7a0b\u3002\u00a0<\/p>\n<p><strong>\u3010\u7ed3\u8bba\u548c\u5c55\u671b\u3011<\/strong><\/p>\n<p>\u4e0a\u8ff0\u5de5\u4f5c\u8868\u660e\uff0c\u901a\u5e38\u5728\u5b9e\u9a8c\u5ba4\u4e2d\u8fdb\u884c\u7684\u57fa\u4e8e\u590d\u6742\u5de5\u827a\u548c\u7279\u6b8a\u6750\u6599\u6784\u5efa\u7684\u67d4\u6027\u53ef\u7a7f\u6234\u4f20\u611f\u5668\u4e5f\u53ef\u4ee5\u4f7f\u7528\u65e5\u5e38\u751f\u6d3b\u7528\u54c1\u5728\u5c45\u5bb6\u73af\u5883\u4e0b\u8fdb\u884c\u5236\u9020\u3002\u5b9e\u9a8c\u7ed3\u679c\u8868\u660e\uff0c\u8be5\u79cd\u5bb6\u5236\u591a\u529f\u80fd\u4f20\u611f\u5e73\u53f0\u80fd\u591f\u51c6\u786e\u3001\u8fde\u7eed\u5730\u76d1\u6d4b\u591a\u79cd\u5173\u952e\u4eba\u4f53\u751f\u547d\u4f53\u5f81\uff0c\u5305\u62ec\u4f53\u6e29\u3001\u5fc3\u8df3\/\u8109\u640f\u3001\u547c\u5438\u9891\u7387\u3001\u54b3\u55fd\u548c\u5404\u79cd\u8eab\u4f53\u8fd0\u52a8\u3002\u4e0e\u5b9e\u9a8c\u5ba4\u5236\u5907\u7684\u6602\u8d35\u4e14\u590d\u6742\u7684\u4f20\u611f\u5668\u4ef6\u76f8\u6bd4\uff0c\u8be5\u79cd\u5bb6\u5236\u591a\u529f\u80fd\u4f20\u611f\u5e73\u53f0\u5177\u6709\u53ef\u6bd4\u62df\u7684\u7efc\u5408\u6027\u80fd\uff0c\u4f46\u5728\u4fbf\u6377\u6027\u3001\u7ecf\u6d4e\u6027\u3001\u53ef\u63a8\u5e7f\u6027\u7b49\u65b9\u9762\u5177\u6709\u663e\u8457\u4f18\u52bf\uff0c\u5728\u4ee5\u5bb6\u5ead\u4e3a\u4e2d\u5fc3\u6216\u8d44\u6e90\u532e\u4e4f\u5730\u533a\u7684\u6570\u5b57\u5316\u533b\u7597\u65b9\u9762\u5177\u6709\u5f88\u597d\u7684\u5b9e\u7528\u4ef7\u503c\uff1b\u6b64\u5916\uff0c\u8be5\u79cd\u5bb6\u5236\u591a\u529f\u80fd\u4f20\u611f\u5e73\u53f0\u4e5f\u53ef\u4ee5\u4e3a\u8bfe\u5802\u6559\u5b66\u548c\u4e34\u5e8a\u57f9\u8bad\u63d0\u4f9b\u65b0\u7684\u8303\u4f8b\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1ahttps:\/\/doi.org\/10.1021\/acssensors.3c00630\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u7814\u7a76\u80cc\u666f\u3011 \u67d4\u6027\u53ef\u7a7f\u6234\u667a\u80fd\u4f20\u611f\u5668\u5728\u4eba\u4f53\u751f\u547d\u4f53\u5f81\uff08\u5982\u4f53\u6e29\u3001\u5fc3\u7387\u3001\u547c\u5438\u9891\u7387\u7b49\uff09\u7684\u8fde\u7eed\u6027\u76d1\u6d4b\u65b9\u9762\u5177\u6709\u5de8\u5927\u7684\u5e94\u7528\u6f5c\u529b\u3002\u8fd1\u5e74\u6765\uff0c\u7528\u4e8e\u53ef\u7a7f\u6234\u5065\u5eb7\u76d1\u6d4b\u7684\u67d4\u6027\u4f20\u611f\u5668\u53d6\u5f97\u4e86\u663e\u8457&#8230;<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-252284","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/252284"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=252284"}],"version-history":[{"count":4,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/252284\/revisions"}],"predecessor-version":[{"id":252298,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/252284\/revisions\/252298"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=252284"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=252284"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=252284"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}