{"id":252677,"date":"2023-07-08T07:56:59","date_gmt":"2023-07-07T23:56:59","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=252677"},"modified":"2023-07-08T07:56:59","modified_gmt":"2023-07-07T23:56:59","slug":"%e6%9c%80%e6%96%b0nature-catalysis%ef%bc%9a%e7%87%83%e6%96%99%e7%94%b5%e6%b1%a0%e5%82%ac%e5%8c%96%e5%89%82%e5%b1%82%e7%9a%84%e4%b8%89%e7%bb%b4%e7%ba%b3%e7%b1%b3%e8%8d%a7%e5%85%89%e6%88%90%e5%83%8f","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=252677","title":{"rendered":"\u6700\u65b0Nature Catalysis\uff1a\u71c3\u6599\u7535\u6c60\u50ac\u5316\u5242\u5c42\u7684\u4e09\u7ef4\u7eb3\u7c73\u8367\u5149\u6210\u50cf"},"content":{"rendered":"<p style=\"text-align: center;\">\u00a0<\/p>\n<p style=\"text-align: center;\"><strong><b>\u4e00\u3001<\/b><\/strong><strong><b>[\u5bfc\u8bfb]<\/b><\/strong><\/p>\n<p style=\"text-align: center;\">\u00a0<\/p>\n<p>\u8d28\u5b50\u4ea4\u6362\u819c\u71c3\u6599\u7535\u6c60\u4e2d\u7684\u50ac\u5316\u5242\u5c42\u7531\u8d1f\u8f7d\u5728\u78b3\u805a\u96c6\u4f53\u4e0a\u7684\u94c2\u65cf\u91d1\u5c5e\u7eb3\u7c73\u50ac\u5316\u5242\u7ec4\u6210\uff0c\u5e76\u901a\u8fc7\u79bb\u5b50\u805a\u5408\u7269\u7f51\u7edc\u7684\u6e17\u900f\u5f62\u6210\u591a\u5b54\u7ed3\u6784\u3002\u8fd9\u4e9b\u5f02\u8d28\u7ec4\u88c5\u4f53\u7684\u5c40\u90e8\u7ed3\u6784\u7279\u5f81\u4e0e\u4f20\u8d28\u963b\u788d\u548c\u968f\u540e\u7684\u7535\u6c60\u6027\u80fd\u635f\u5931\u76f4\u63a5\u76f8\u5173\uff1b\u56e0\u6b64\uff0c\u5b83\u7684\u4e09\u7ef4\u53ef\u89c6\u5316\u662f\u6709\u610f\u4e49\u7684\u3002<\/p>\n<p><strong><b>\u00a0<\/b><\/strong><\/p>\n<p style=\"text-align: center;\"><strong><b>\u4e8c\u3001<\/b><\/strong><strong><b>[\u6210\u679c\u63a0\u5f71]<\/b><\/strong><\/p>\n<p><strong><b>\u00a0<\/b><\/strong><\/p>\n<p><strong><b>\u8fd1\u65e5\uff0c<\/b><\/strong><strong><b>\u745e\u58eb\u6d1b\u6851\u8054\u90a6\u7406\u5de5\u5b66\u9662Vasiliki Tileli\u8bfe\u9898\u7ec4\u5b9e\u73b0\u4e86\u6df1\u5ea6\u5b66\u4e60\u8f85\u52a9\u7684\u4f4e\u6e29\u900f\u5c04\u7535\u5b50\u65ad\u5c42\u6210\u50cf\u56fe\u50cf\u590d\u539f\uff0c\u5e76\u5728\u5c40\u90e8\u53cd\u5e94\u4f4d\u70b9\u5c3a\u5ea6\u4e0a\u5b9a\u91cf\u7814\u7a76\u4e86\u5404\u79cd\u50ac\u5316\u5242\u5c42\u7684\u5b8c\u6574\u5f62\u8c8c<\/b><\/strong>\u3002\u901a\u8fc7\u5206\u6790\uff0c\u53ef\u4ee5\u8ba1\u7b97\u79bb\u805a\u4f53\u5f62\u8c8c\u3001\u8986\u76d6\u7387\u548c\u5747\u5300\u6027\u3001\u94c2\u5728\u78b3\u8f7d\u4f53\u4e0a\u7684\u4f4d\u7f6e\u4ee5\u53ca\u94c2\u5bf9\u79bb\u805a\u4f53\u7f51\u7edc\u7684\u53ef\u63a5\u8fd1\u6027\u7b49\u6307\u6807\uff0c\u5e76\u5c06\u7ed3\u679c\u4e0e\u5b9e\u9a8c\u6d4b\u91cf\u7ed3\u679c\u8fdb\u884c\u76f4\u63a5\u6bd4\u8f83\u548c\u9a8c\u8bc1\u3002\u672c\u5de5\u4f5c\u671f\u671b\u8be5\u7814\u7a76\u7ed3\u679c\u548c\u8bc4\u4f30\u50ac\u5316\u5242\u5c42\u7ed3\u6784\u7684\u65b9\u6cd5\u5c06\u6709\u52a9\u4e8e\u5c06\u5f62\u8c8c\u4e0e\u4f20\u8f93\u7279\u6027\u548c\u6574\u4f53\u71c3\u6599\u7535\u6c60\u6027\u80fd\u8054\u7cfb\u8d77\u6765\u3002\u76f8\u5173\u8bba\u6587\u4ee5\u9898\u4e3a\u201c<strong>Three-dimensional nanoimaging of fuel cell catalyst layers<\/strong>\u201d\u7684\u8bba\u6587\u53d1\u8868\u5728<strong><em>Nature Catalysis<\/em><\/strong>\u4e0a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-252678\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/07\/\u56fe\u72471-2.png\" alt=\"\" width=\"726\" height=\"238\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/07\/\u56fe\u72471-2.png 726w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/07\/\u56fe\u72471-2-300x98.png 300w\" sizes=\"(max-width: 726px) 100vw, 726px\" \/><\/p>\n<p>&nbsp;<\/p>\n<p style=\"text-align: center;\"><strong><b>\u4e09\u3001<\/b><\/strong><strong><b>[\u6838\u5fc3\u521b\u65b0\u70b9]<\/b><\/strong><\/p>\n<p>\u5bf9\u5206\u6563\u6216\u663e\u5fae\u5207\u5272\u7684\u6837\u54c1\u8fdb\u884c\u4f4e\u6e29\u7535\u5b50\u65ad\u5c42\u626b\u63cf(Cryo-ET)\uff0c\u540c\u65f6\u5229\u7528\u6df1\u5ea6\u5b66\u4e60\u65b9\u6cd5\u8fdb\u884c\u53bb\u566a\u548c\u5206\u5272\u4ee5\u83b7\u5f97\u5b9a\u91cf\u4fe1\u606f\uff0c\u4ece\u800c\u5b9e\u73b0\u50ac\u5316\u5242\u5c42\u7684\u4e09\u7ef4\u7eb3\u7c73\u8367\u5149\u6210\u50cf\u3002<\/p>\n<p><strong><b>\u00a0<\/b><\/strong><\/p>\n<p style=\"text-align: center;\"><strong><b>\u56db\u3001<\/b><\/strong><strong><b>[\u6570\u636e\u6982\u89c8]<\/b><\/strong><\/p>\n<ul>\n<li><b><\/b><strong><b>\u50ac\u5316\u5242\u5c42\u805a\u96c6\u4f53\u7684\u4f4e\u6e29\u7535\u5b50\u5c42\u6790\u6210\u50cf<\/b><\/strong><\/li>\n<\/ul>\n<p>&nbsp;<\/p>\n<p>\u5305\u62ec\u79bb\u805a\u7269\u5728\u5185\u7684\u6709\u673a\u6837\u54c1\u7684\u7535\u5b50\u6210\u50cf\u901a\u5e38\u5728\u4f4e\u6e29\u4e0b\u8fdb\u884c\uff0c\u56e0\u4e3a\u5b83\u964d\u4f4e\u4e86\u8f90\u89e3\u7684\u901f\u7387\uff0c\u800c\u8f90\u89e3\u662f\u8fd9\u7c7b\u6750\u6599\u4e2d\u7535\u5b50\u675f\u8bf1\u5bfc\u635f\u4f24\u7684\u4e3b\u8981\u6765\u6e90\u3002\u4e3a\u4e86\u83b7\u5f97\u4f53\u79ef\u4fe1\u606f\uff0c\u672c\u5de5\u4f5c\u5c06\u8fd9\u79cd\u65b9\u6cd5\u4e0e\u7535\u5b50\u5c42\u6790\u6210\u50cf\u76f8\u7ed3\u5408\uff0c\u5176\u4e2d\u4e00\u7cfb\u5217\u6295\u5f71\u56fe\u50cf\u662f\u901a\u8fc7\u589e\u52a0\u6837\u54c1\u503e\u659c\u89d2\u5ea6\u83b7\u5f97\u7684\uff0c\u5e76\u7528\u4e8e\u8ba1\u7b97\u6837\u54c1\u7684\u4e09\u7ef4\u91cd\u5efa\u3002\u5728\u6b64\u6761\u4ef6\u4e0b\u8fd0\u884c\u7684\u663e\u5fae\u955c\u7ed3\u6784\u793a\u610f\u56fe\u5982<strong><b>\u56fe1a<\/b><\/strong>\u6240\u793a\uff0cNafion-\u4f4e\u8868\u9762\u78b3(LSC)-\u94c2\u805a\u96c6\u4f53\u7684\u660e\u573aTEM\u7167\u7247\u5982<strong><b>\u56fe1b<\/b><\/strong>\u6240\u793a\u3002\u5982<strong><b>\u56fe1c<\/b><\/strong>\u6240\u793a\uff0c\u572898\u2009K\u4e0b\uff0c\u7d2f\u79ef\u7535\u5b50\u66b4\u9732\u4e3a80\u2009e<sup>&#8211;<\/sup>\u00c5<sup>-2<\/sup>\u65f6\uff0c\u50ac\u5316\u5242\u5c42\u4e2d\u53d1\u73b0\u7684\u7eb3\u7c73\u539a\u5ea6\u5c42\u7684\u539a\u5ea6\u635f\u5931\u4e3a10-40%\u3002\u5728<strong><b>\u56fe1d<\/b><\/strong>\u4e2d\uff0c\u672c\u5de5\u4f5c\u5c55\u793a\u4e86\u7531Nafion\u79bb\u805a\u7269\u3001LSC\u8f7d\u4f53\u548c\u94c2\u7eb3\u7c73\u9897\u7c92\u5236\u5907\u7684\u50ac\u5316\u5242\u5c42\u805a\u96c6\u4f53\u7684\u91cd\u5efa\u548c\u53bb\u566a\u8fc7\u7a0b\u7684\u7ed3\u679c\u3002\u901a\u8fc7\u5bf9\u91cd\u5efa\u7ed3\u679c\u7684\u4ed4\u7ec6\u68c0\u67e5\u53ef\u4ee5\u53d1\u73b0\uff0c\u5728\u5bf9\u6bd4\u5ea6\u548c\u7eb9\u7406\u53d8\u5316\u7684\u590d\u6742\u7ec4\u5408\u7684\u57fa\u7840\u4e0a\uff0c\u53ef\u4ee5\u8bc6\u522b\u603b\u91cf\u4e2d\u7684\u6240\u6709\u4e09\u4e2a\u9636\u6bb5\u3002\u5982<strong>\u56fe1e<\/strong>\u4e2d\u7684X\u5c04\u7ebf\u65ad\u5c42\u7167\u7247\u548c\u7ebf\u8f6e\u5ed3\u6240\u793a\uff0c\u78b3\u9897\u7c92\u7684\u81f4\u5bc6\u548c\u9ad8\u5ea6\u77f3\u58a8\u5316\u7684\u5916\u58f3\u5bfc\u81f4\u4e86\u4e00\u4e2a\u5178\u578b\u7684\u4e2d\u7a7a\u548c\u660e\u4eae\u7684\u591a\u5b54\u6838\u5fc3\u5468\u56f4\u7684\u9ed1\u6697\u5bf9\u6bd4\u3002\u53d1\u73b0\u8fd9\u79cd\u58f3\u5c42\u4ece\u51e0\u4e2a\u78b3\u5c42\u5230\u51e0\u5341\u7eb3\u7c73\u4e0d\u7b49\uff0c\u5e76\u901a\u8fc7\u9ad8\u5206\u8fa8TEM\u56fe\u50cf\u8fdb\u4e00\u6b65\u8bc1\u5b9e\u4e86\u8fd9\u4e00\u70b9\u3002\u94c2\u7eb3\u7c73\u9897\u7c92\u7684\u5bf9\u6bd4\u5ea6\u6700\u6697\uff0c\u5176\u7279\u5f81\u5c3a\u5bf8\u4e3a2~5\u2009nm\u3002\u901a\u8fc7\u6392\u963b\u6cd5\u786e\u5b9a\u79bb\u805a\u7269\u4e3a\u78b3\u548c\u94c2\u9897\u7c92\u5468\u56f4\u6216\u4e4b\u95f4\u7684\u5149\u6ed1\u3001\u5178\u578b\u7684\u8fde\u7eed\u548c\u7a0d\u8f7b\u7684\u7ed3\u5408\u76f8\u3002<\/p>\n<p>\u5728<strong>\u56fe1h<\/strong>\u4e2d\uff0c\u672c\u5de5\u4f5c\u901a\u8fc7\u7814\u7a76\u4e09\u79cd\u4e0d\u540c\u79bb\u805a\u7269\u4e0e\u78b3(I\/C)\u91cd\u91cf\u6bd4\u7684\u6a21\u578b\u50ac\u5316\u5242\u5c42\u7684\u5e72\u71e5\u5206\u6563\u5f97\u5230\u7684\u805a\u96c6\u4f53\uff0c\u8bc1\u660e\u7ecf\u8fc7\u5904\u7406\u7684\u91cd\u5efa\u53ef\u4ee5\u63d0\u4f9b\u5b9a\u6027\u548c\u5b9a\u91cf\u7684\u4fe1\u606f\u3002\u968f\u7740LSC\u7535\u6781\u7684I\/C\u6bd4\u7684\u589e\u52a0\uff0c\u5c40\u90e8I\/C\u91cd\u91cf\u6bd4\u548c\u8ba1\u7b97\u7684\u78b3\u8986\u76d6\u7387\u5448\u5355\u8c03\u4e0a\u5347\u8d8b\u52bf(<strong>\u56fe1h<\/strong>)\uff1b\u7136\u800c\uff0c\u8ba1\u7b97\u7684I\/C\u6bd4\u7cfb\u7edf\u6027\u5730\u4f4e\u4e8e\u9884\u671f\uff0c\u672c\u5de5\u4f5c\u4e3b\u8981\u5f52\u56e0\u4e8e\u5206\u6563\u6837\u54c1\u5236\u5907\u7684\u7834\u574f\u6027\u5f71\u54cd\u3002\u4e3a\u4e86\u51cf\u8f7b\u8fd9\u4e9b\u5f71\u54cd\uff0c\u4e0b\u9762\u91c7\u7528\u90e8\u5206\u5305\u57cb\u548c\u8d85\u8584\u5207\u7247\u7684\u65b9\u6cd5\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-252679\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/07\/\u56fe\u72472-2.png\" alt=\"\" width=\"1076\" height=\"452\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/07\/\u56fe\u72472-2.png 1076w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/07\/\u56fe\u72472-2-300x126.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/07\/\u56fe\u72472-2-768x323.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/07\/\u56fe\u72472-2-1024x430.png 1024w\" sizes=\"(max-width: 1076px) 100vw, 1076px\" \/><\/p>\n<p><strong>\u56fe1<\/strong>\u00a0\u00a0Nafion-LSC-\u94c2\u805a\u96c6\u4f53\u7684Cryo-ET\u5de5\u4f5c\u6d41\u7a0b\u53ca\u5206\u6790\u00a0\u00a9 2023 The Authors<\/p>\n<p>&nbsp;<\/p>\n<ul>\n<li><b><\/b><strong><b>\u50ac\u5316\u5242\u5c42\u7684\u7ed3\u6784<\/b><\/strong><\/li>\n<\/ul>\n<p><strong><b>\u00a0<\/b><\/strong><\/p>\n<p>\u4e3a\u4e86\u6df1\u5165\u4e86\u89e3\u5178\u578b\u8d28\u5b50\u4ea4\u6362\u819c\u71c3\u6599\u7535\u6c60\u9634\u6781\u7684\u5f62\u8c8c\uff0c\u672c\u5de5\u4f5c\u7814\u7a76\u4e8619.8\u2009wt%\u94c2\u8d1f\u8f7d\u5728\u9ad8\u6bd4\u8868\u9762\u79ef\u78b3(HSC)\u4e0a\u7684\u50ac\u5316\u5c42\uff0c\u5e76\u57280.7 w\/w\u7684I\/C\u6bd4\u4e0b\u75283M 800 EW\u79bb\u805a\u7269\u5236\u5907\u3002\u5206\u5272\u91cd\u5efa\u7684\u9762\u7ed8\u5236\u5982<strong>\u56fe2a<\/strong>\u6240\u793a\u3002\u89c2\u5bdf\u5230\u76f8\u5bf9\u8f83\u5c0f\u4e14\u53d6\u5411\u7684\u78b3\u805a\u96c6\u4f53- -\u76f4\u5f84\u4e3a20~40\u2009nm\u7684\u521d\u7ea7\u73e0\u5b50- -\u7c7b\u4f3c\u4e8ePt\/C\u50ac\u5316\u5242\u5206\u6563\u4f53\u7684TEM\u7167\u7247\u4e2d\u770b\u5230\u7684\u7ed3\u6784\u3002\u5728<strong>\u56fe2c<\/strong>\u4e2d\u7ed9\u51fa\u4e86\u5c40\u90e8\u539a\u5ea6\u7684\u5f69\u8272\u7f16\u78013D\u56fe\uff0c\u4ee5\u53ca\u4ece\u4f53\u79ef\u4e2d\u63d0\u53d6\u7684\u653e\u5927\u622a\u9762\uff0c\u5e76\u8bf4\u660e\u4e86\u4e24\u79cd\u8ba1\u7b97\u7b56\u7565\u4e4b\u95f4\u7684\u5dee\u5f02\u3002\u76f8\u5e94\u7684\u5206\u5e03\u56fe\u5982<strong>\u56fe2d<\/strong>\u6240\u793a\u3002\u672c\u5de5\u4f5c\u53d1\u73b0\u4e86\u5e7f\u6cdb\u7684\u79bb\u805a\u4f53\u539a\u5ea6\uff0c\u6b63\u5982\u4ee5\u524d\u4ece2D\u663e\u5fae\u7167\u7247\u548c\u6df7\u5408\u6a21\u62df\u89c2\u5bdf\u65b9\u6cd5\u4e2d\u89c2\u5bdf\u5230\u7684\uff0c\u7f51\u7edc\u7684\u5e73\u5747\u539a\u5ea6\u4e3a9.2\u2009nm\u3002\u56fe\u8c31\u548c\u5206\u5e03\u4e5f\u8868\u660e\u5b58\u5728\u8f83\u5927\u7684\u79bb\u805a\u4f53\u533a\u57df\uff0c\u539a\u5ea6\u53ef\u8fbe24\u2009nm\u3002<strong><b>\u6709\u8da3\u7684\u662f\uff0c\u901a\u8fc7\u79bb\u5b50\u4ea4\u6362\u5f97\u5230\u7684\u4e92\u8865\u7ed3\u679c\u8868\u660e\uff0c\u7eaf\u79bb\u805a\u7269\u7684\u8fd9\u4e9b\u5927\u56e2\u805a\u4f53\u5185\u53ef\u80fd\u5b58\u5728\u76f8\u5206\u79bb<\/b><\/strong>\u3002\u76f8\u6bd4\u4e4b\u4e0b\uff0c\u94c2\u548c\u78b3\u8986\u76d6\u7387\u63d0\u53d6\u7684\u6570\u636e\u663e\u793a\u51fa\u66f4\u7a84\u548c\u63a5\u8fd1\u7684\u5206\u5e03\uff0c\u5e73\u5747\u539a\u5ea6\u5206\u522b\u4e3a4.9\u548c5.7\u2009nm\uff0c\u5e76\u4e14\u5728\u4e24\u79cd\u60c5\u51b5\u4e0b\u90fd\u96c6\u4e2d\u57283\u2009nm\u9644\u8fd1\u3002<\/p>\n<p>\u4e0e\u5176\u4ed6\u8868\u5f81\u50ac\u5316\u5242\u5c42\u4e2d\u79bb\u805a\u7269\u819c\u539a\u5ea6\u7684\u5c1d\u8bd5\u76f8\u6bd4\uff0c\u672c\u5de5\u4f5c\u53d1\u73b0\u5728\u8be5\u79bb\u805a\u7269\u542b\u91cf\u4e0b\u7684\u7ed3\u679c\u4e0eCetinbas\u7684\u7814\u7a76\u7ed3\u679c\u4e00\u81f4\uff0c\u4f46\u6570\u503c\u8fdc\u5c0f\u4e8e\u5148\u524d\u4eceSTEM\u65ad\u5c42\u626b\u63cf\u548c\u539f\u4f4d\u539f\u5b50\u529b\u663e\u5fae\u955c\u4e2d\u62a5\u9053\u7684\u7ed3\u679c\u3002\u8fd9\u4e9b\u4e0e\u4ee5\u524d\u7814\u7a76\u7684\u5dee\u5f02\u53ef\u80fd\u662f\u7531\u4e8e\u6837\u54c1\u5236\u5907\u7684\u5dee\u5f02\uff0c\u4ee5\u53ca\u7531\u4e8e\u79bb\u805a\u7269\u7684\u6c34\u5408\u72b6\u6001\u548c\u53ef\u80fd\u8f83\u9ad8\u7684\u79bb\u805a\u7269\u542b\u91cf\u3002<strong><b>\u5c3d\u7ba1\u5982\u6b64\uff0c<\/b><\/strong><strong><b>\u672c\u5de5\u4f5c<\/b><\/strong><strong><b>\u7684\u6d4b\u91cf\u7ed3\u679c\u4e0e\u79bb\u805a\u7269\u5206\u6563\u4f53\u7684\u5f62\u8c8c\u5f62\u6210\u4e86\u4e00\u81f4\u7684\u56fe\u50cf<\/b><\/strong>\uff0c\u5df2\u77e5\u79bb\u805a\u7269\u5206\u6563\u4f53\u7684\u521d\u7ea7\u68d2\u72b6\u805a\u96c6\u4f53\u7684\u534a\u5f84\u4e3a1.5~2.5\u2009nm\uff0c\u53d6\u51b3\u4e8e\u7b49\u6548\u91cd\u91cf\u548c\u4fa7\u94fe\u957f\u5ea6\uff0c\u800c\u6b21\u7ea7\u805a\u96c6\u4f53\u5219\u4e3b\u8981\u53d6\u51b3\u4e8e\u5206\u6563\u73af\u5883\uff0c\u53ef\u8fbe\u6570\u767e\u7eb3\u7c73\u3002<strong><b>\u8be5<\/b><\/strong><strong><b>\u4e00\u81f4\u6027\u8868\u660e\uff0c\u5728\u8fd9\u79cd\u79bb\u805a\u7269\u542b\u91cf\u4e0b\uff0c\u78b3\u548c\u94c2\u8868\u9762\u5c06\u6700\u9891\u7e41\u5730\u88ab\u5355\u4e2a\u521d\u7ea7\u79bb\u805a\u7269\u805a\u96c6\u4f53\u8986\u76d6\uff0c\u56e0\u6b64\uff0c\u79bb\u805a\u7269\u5728\u5206\u6563\u4e2d\u7684\u72b6\u6001\u5c06\u4e0e\u50ac\u5316\u5242\u5c42\u4e2d\u7684\u6700\u7ec8\u5f62\u6001\u5bc6\u5207\u76f8\u5173<\/b><\/strong>\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-252680\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/07\/\u56fe\u72473-2.png\" alt=\"\" width=\"520\" height=\"740\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/07\/\u56fe\u72473-2.png 520w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/07\/\u56fe\u72473-2-211x300.png 211w\" sizes=\"(max-width: 520px) 100vw, 520px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>2<\/strong>\u00a0\u00a03M\u79bb\u805a\u4f53-HSC-\u94c2\u50ac\u5316\u5c42\u7684Cryo-ET\u91cd\u5efa\u53ca\u79bb\u805a\u4f53\u7f51\u7edc\u5206\u6790\u00a9 2023 The Authors<\/p>\n<p>&nbsp;<\/p>\n<ul>\n<li><b><\/b><strong><b>\u5f62\u8c8c\u53ca\u76f8\u4e92\u4f5c\u7528<\/b><\/strong><\/li>\n<\/ul>\n<p>&nbsp;<\/p>\n<p>\u91cd\u5efa\u7684\u4f53\u79ef\u8fdb\u4e00\u6b65\u5141\u8bb8\u7814\u7a76\u94c2\u7eb3\u7c73\u7c92\u5b50\u4e0e\u78b3\u8f7d\u4f53\u548c\u79bb\u805a\u7269\u7f51\u7edc\u7684\u5f62\u8c8c\u548c\u76f8\u4e92\u4f5c\u7528\u3002<strong>\u56fe3a<\/strong>\u5c55\u793a\u4e86\u4ece<strong>\u56fe2<\/strong>\u4e2d\u91cd\u5efa\u5f97\u5230\u7684\u4e00\u4e2a\u5b50\u4f53\u7684\u4e09\u7ef4\u53ef\u89c6\u5316\u548c\u7279\u5199\u8d34\u56fe\u3002\u6709\u76f8\u5f53\u4e00\u90e8\u5206(46%)\u7684\u7eb3\u7c73\u9897\u7c92\u9a7b\u7559\u5728\u78b3\u521d\u7ea7\u9897\u7c92\u5185\u7684\u7eb3\u7c73\u5b54\u4e2d\uff0c\u8fd9\u4e0e\u5148\u524d\u5bf9\u8fd9\u7c7b\u9ad8\u6bd4\u8868\u9762\u79ef\u78b3\u7684\u7814\u7a76\u7ed3\u679c\u4e00\u81f4\u3002\u5185\u90e8\u548c\u5916\u90e8\u94c2\u91d1\u5c3a\u5bf8\u5206\u5e03\u5982<strong>\u56fe3b<\/strong>\u6240\u793a\u3002\u4e24\u79cd\u7c92\u5b50\u5177\u6709\u76f8\u4f3c\u7684\u5f62\u8c8c\uff0c\u5185\u90e8\u548c\u5916\u90e8\u7c92\u5b50\u7684\u5e73\u5747\u76f4\u5f84\u5206\u522b\u4e3a2.7\u548c3.0\u2009nm\uff0c\u5916\u90e8\u7c92\u5b50(<em><i>\u03c3<\/i><\/em>\u5185=0.7\u2009nm,<em><i>\u03c3<\/i><\/em>\u5916=\u2009.0\u2009nm)\u7684\u5206\u5e03\u7565\u5bbd\uff0c\u8fd9\u53ef\u80fd\u662f\u7531\u4e8e\u5408\u6210\u8fc7\u7a0b\u4e2d\u78b3\u8f7d\u4f53\u7684\u5185\u90e8\u5b54\u9699\u9650\u5236\u4e86\u7c92\u5b50\u7684\u751f\u957f\u3002<\/p>\n<p>\u805a\u7126\u4e8e\u5916\u90e8\u94c2\u9897\u7c92\u53ca\u5176\u4e0e\u79bb\u805a\u7269\u7f51\u7edc\u7684\u8fde\u901a\u6027\uff0c\u672c\u5de5\u4f5c\u6bd4\u8f83\u4e86\u4ece\u65ad\u5c42\u56fe\u50cf\u8ba1\u7b97\u7684\u8868\u9762\u79ef\u548c\u4f53\u6d4b\u91cf\u7684\u8868\u9762\u79ef\u3002\u4ece<strong>\u56fe3c<\/strong>\u53ef\u4ee5\u770b\u51fa\uff0c\u5c42\u6790\u6210\u50cf\u53ef\u4ee5\u5f97\u5230\u4e0d\u540c\u7684\u91cf\u3002\u5982<strong>\u56fe3c<\/strong>\u4e2d\u653e\u5927\u5207\u7247\u6240\u793a\uff0c\u8fde\u901a\u8868\u9762\u5b9a\u4e49\u4e3a\u4e0e\u79bb\u805a\u4f53\u76f4\u63a5\u63a5\u89e6\u7684\u94c2\u91d1\u8868\u9762\uff0c\u5728\u91cd\u5efa\u4e2d\u5360\u603b\u94c2\u91d1\u8868\u9762\u768415\u00b18%\u3002\u76f8\u6bd4\u4e4b\u4e0b\uff0c\u8fde\u63a5\u9897\u7c92\u7684\u8868\u9762\u662f\u8861\u91cf\u4e0e\u79bb\u5b50\u819c\u63a5\u89e6\u7684\u6240\u6709\u9897\u7c92\u7684\u603b\u8868\u9762\uff0c\u662f\u91cd\u5efa\u4e2d\u94c2\u91d1\u603b\u8868\u9762\u768452\u00b113%\u3002\u8fd9\u4e9b\u91cf\u4e4b\u95f4\u7684\u5dee\u5f02\u53ef\u4ee5\u90e8\u5206\u5f52\u56e0\u4e8e\u5206\u5272\u7ed3\u679c\u4e2d\u7684\u4e00\u79cd\u503e\u5411\uff0c\u5373\u5d4c\u5165\u94c2\u91d1\u7684\u6df1\u5ea6\u6bd4\u5b9e\u9645\u60c5\u51b5\u66f4\u6df1\uff0c\u8fd9\u662f\u901a\u8fc7\u672c\u5de5\u4f5c\u5728\u8bc4\u4f30\u6570\u636e\u96c6\u7684\u5e73\u5747\u7edd\u5bf9\u8bef\u5dee\u8ba1\u7b97\u4e2d\u7684\u8bef\u5dee\u4f30\u8ba1\u6765\u6355\u6349\u7684\u3002<\/p>\n<p>\u572810%\u76f8\u5bf9\u6e7f\u5ea6\u4e0b\uff0cCO\u5265\u79bb\u6d4b\u91cf\u8868\u660e\u94c2\u7684\u5229\u7528\u7387\u4e3a31%\uff0c\u4ecb\u4e8e\u8fde\u901a\u8868\u9762\u548c\u5c42\u6790\u6210\u50cf\u8ba1\u7b97\u7684\u8fde\u901a\u9897\u7c92\u8868\u9762\u4e4b\u95f4\u3002<strong><b>\u8fd9\u8868\u660e\uff0c\u5373\u4f7f\u5728\u4f4e\u76f8\u5bf9\u6e7f\u5ea6\u4e0b\uff0c\u4e0e\u79bb\u805a\u4f53\u76f4\u63a5\u63a5\u89e6\u7684\u533a\u57df\u4e5f\u6709\u66f4\u5927\u7684\u9762\u79ef\u53c2\u4e0eECSA\u6d4b\u91cf<\/b><\/strong>\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-252681\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/07\/\u56fe\u72474-2.png\" alt=\"\" width=\"769\" height=\"516\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/07\/\u56fe\u72474-2.png 769w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/07\/\u56fe\u72474-2-300x201.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/07\/\u56fe\u72474-2-768x515.png 768w\" sizes=\"(max-width: 769px) 100vw, 769px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>3<\/strong>\u00a0\u00a0\u663e\u5fae\u5207\u52723M\u79bb\u805a\u7269-HSC-\u94c2\u50ac\u5316\u5c42\u4e2d\u94c2\u76f8\u5173\u5f62\u8c8c\u5206\u6790\u00a9 2023 The Authors<\/p>\n<p>&nbsp;<\/p>\n<p style=\"text-align: center;\"><strong><b>\u4e94\u3001<\/b><\/strong><strong><b>[\u6210\u679c\u542f\u793a]<\/b><\/strong><\/p>\n<p><strong><b>\u00a0<\/b><\/strong><\/p>\n<p><strong><b>\u603b\u4e4b\uff0c<\/b><\/strong><strong><b>\u672c\u5de5\u4f5c<\/b><\/strong><strong><b>\u8be6\u7ec6\u9610\u8ff0\u4e86\u4e00\u79cd\u5728\u7eb3\u7c73\u7ea7\u5206\u8fa8\u7387\u4e0b\u63d0\u4f9b\u5b9a\u91cf\u4e09\u7ef4\u6570\u636e\u7684\u65b9\u6cd5\uff0c<\/b><\/strong><strong><b>\u901a\u8fc7\u8be5\u65b9\u6cd5<\/b><\/strong><strong><b>\u53ef\u4ee5\u8be6\u7ec6\u89c2\u5bdf\u8d28\u5b50\u4ea4\u6362\u819c\u71c3\u6599\u7535\u6c60\u50ac\u5316\u5242\u5c42\u7ed3\u6784\u53ca\u5176\u6240\u6709\u7ec4\u4ef6<\/b><\/strong>\u3002\u7814\u7a76\u8868\u660e\uff0c\u5c3d\u7ba1\u4e0d\u80fd\u5b8c\u5168\u6291\u5236\u7535\u5b50\u675f\u5bf9\u79bb\u805a\u4f53\u7684\u635f\u4f24\uff0c\u4f46\u4f4e\u6e29\u7535\u5b50\u65ad\u5c42\u626b\u63cf\u53ef\u4ee5\u5145\u5206\u51cf\u8f7b\u8fd9\u4e9b\u5f71\u54cd\uff0c\u5e76\u5141\u8bb8\u8fdb\u884c\u4f53\u79ef\u91cd\u5efa\u3002\u6b64\u5916\uff0c\u5148\u8fdb\u7684\u56fe\u50cf\u5904\u7406\u65b9\u6cd5\u5b9e\u73b0\u4e86\u6240\u6709\u6210\u5206\u7684\u5b9a\u91cf\u6d4b\u91cf\uff0c\u800c\u8d85\u8584\u5207\u7247\u673a\u7684\u6837\u54c1\u5236\u5907\u5141\u8bb8\u89c2\u5bdf\u9ad8\u5ea6\u8fde\u7eed\u7684\u7f51\u7edc\u5e76\u7814\u7a76\u5176\u7279\u6027\u3002\u672c\u5de5\u4f5c\u8bc1\u5b9e\u5728(\u9ad8\u8fbe20~24\u2009nm)\u5c42\u5185\u5b58\u5728\u5e7f\u6cdb\u7684\u79bb\u805a\u7269\u539a\u5ea6\uff0c\u78b3\u8f7d\u4f53\u5916\u90e8\u7684\u94c2\u9897\u7c92\u5927\u90e8\u5206\u88ab\u5355\u4e2a\u79bb\u805a\u7269\u805a\u96c6\u4f53\u8986\u76d6\uff0c\u539a\u5ea6\u4e3a3-4\u2009nm\u3002\u6b64\u5916\uff0c\u5916\u90e8\u78b3\u8868\u9762\u7684\u9ad8\u8986\u76d6\u7387\u5bfc\u81f4\u79bb\u805a\u7269\u7f51\u7edc\u8fde\u63a5\u4e86\u591a\u5b54\u9ad8\u6bd4\u8868\u9762\u79ef\u78b3\u8f7d\u4f53\u4e0a\u7684\u5927\u90e8\u5206\u5916\u90e8\u94c2\u7eb3\u7c73\u9897\u7c92\u3002<\/p>\n<p><strong><b>\u672c\u5de5\u4f5c\u8868\u660e<\/b><\/strong><strong><b>\uff0c\u7528\u4f4e\u6e29ET\u5bf9\u50ac\u5316\u5242\u5c42\u8fdb\u884c\u5e38\u89c4\u7814\u7a76\u9700\u8981\u8fdb\u4e00\u6b65\u7684\u6280\u672f\u8fdb\u6b65<\/b><\/strong>\u3002\u5728\u8fd9\u9879\u5de5\u4f5c\u4e2d\uff0c\u672c\u5de5\u4f5c\u5e7f\u6cdb\u4f9d\u8d56\u4e8e\u4eba\u5de5\u7684\u64cd\u4f5c\uff0c\u540c\u65f6\u5229\u7528\u673a\u5668\u5b66\u4e60\u4f5c\u4e3a\u624b\u52a8\u5206\u5272\u7684\u6269\u5c55\u3002\u8fd9\u662f\u4e00\u4e2a\u8270\u82e6\u7684\u8fc7\u7a0b\uff0c\u53ef\u80fd\u4f1a\u5e26\u6765\u4e00\u5b9a\u7a0b\u5ea6\u7684\u4e0d\u786e\u5b9a\u6027\u3002\u5c3d\u7ba1\u5982\u6b64\uff0c\u672c\u5de5\u4f5c\u7684\u7ed3\u679c\u5f97\u5230\u4e86\u5927\u91cf\u6837\u54c1\u6d4b\u91cf\u548c\u6027\u8d28\u7684\u7cfb\u7edf\u8bc1\u5b9e\uff0c\u5305\u62ecI\/C\u6bd4\u3001\u79bb\u805a\u4f53\u5e73\u5747\u539a\u5ea6\u548c\u94c2\u6bd4\u8868\u9762\u79ef\u3002\u5c55\u671b\u672a\u6765\uff0c\u4e3a\u4e86\u9650\u5236\u4e0d\u786e\u5b9a\u6027\u548c\u7b80\u5316\u56fe\u50cf\u5904\u7406\u5de5\u4f5c\u6d41\u7a0b\uff0c\u63d0\u9ad8\u91c7\u96c6\u4e2d\u4fe1\u566a\u6bd4\u7684\u65b9\u6cd5\u52bf\u5728\u5fc5\u884c\u3002\u6b64\u5916\uff0c\u5728\u5206\u5272\u8fc7\u7a0b\u4e2d\u51cf\u5c11\u624b\u52a8\u8f93\u5165\u7684\u7b56\u7565\u53ef\u4ee5\u5efa\u7acb\u5728\u5728\u5408\u6210\u56fe\u50cf\u4e0a\u8bad\u7ec3\u7684\u901a\u7528\u6a21\u578b\u4e0a\uff0c\u8be5\u6a21\u578b\u5c06\u88ab\u5fae\u8c03\u5230\u53ea\u9700\u8981\u5c11\u91cf\u6ce8\u91ca\u7684\u6bcf\u4e2a\u91cd\u5efa\u4e2d\u3002<\/p>\n<p><strong><b>\u56e0\u6b64\uff0c<\/b><\/strong><strong><b>\u672c\u5de5\u4f5c<\/b><\/strong><strong><b>\u7684<\/b><\/strong><strong><b>\u7814\u7a76\u6210\u679c<\/b><\/strong><strong><b>\u4e3a\u7eb3\u7c73\u5c3a\u5ea6\u4e0b\u4e0d\u540c\u50ac\u5316\u5242\u5c42\u5f62\u8c8c\u7684\u6bd4\u8f83\u5960\u5b9a\u4e86\u57fa\u7840<\/b><\/strong>\u3002\u57fa\u4e8e\u8fd9\u79cd\u65b9\u6cd5\u7684\u8fdb\u4e00\u6b65\u7814\u7a76\u53ef\u4ee5\u4e3a\u78b3-\u79bb\u805a\u7269\u754c\u9762\u5de5\u7a0b\u7684\u5f71\u54cd\u63d0\u4f9b\u6709\u4ef7\u503c\u7684\u89c1\u89e3\uff0c\u8fd9\u4e9b\u754c\u9762\u5de5\u7a0b\u6700\u8fd1\u88ab\u7528\u4e8e\u63d0\u9ad8\u78b3\u8986\u76d6\u7387\uff0c\u5e76\u6709\u52a9\u4e8e\u63ed\u793a\u79bb\u805a\u7269\u5728\u5206\u6563\u4f53\u548c\u50ac\u5316\u5242\u6d46\u6599\u4e2d\u7684\u72b6\u6001\u4e0e\u5176\u5728\u50ac\u5316\u5242\u5c42\u4e2d\u7684\u6700\u7ec8\u8584\u819c\u548c\u7f51\u7edc\u5f62\u8c8c\u4e4b\u95f4\u7684\u5173\u7cfb\u3002<\/p>\n<p>&nbsp;<\/p>\n<p>\u7b2c\u4e00\u4f5c\u8005\uff1aRobin Girod<\/p>\n<p>\u901a\u8baf\u4f5c\u8005\uff1aVasiliki Tileli<\/p>\n<p>\u901a\u8baf\u5355\u4f4d\uff1a\u745e\u58eb\u6d1b\u6851\u8054\u90a6\u7406\u5de5\u5b66\u9662<\/p>\n<p>\u8bba\u6587doi\uff1ahttps:\/\/doi.org\/10.1038\/s41929-023-00947-y<\/p>\n<p>&nbsp;<\/p>\n<p>\u672c\u6587\u7531\u6e29\u534e\u4f9b\u7a3f\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u00a0 \u4e00\u3001[\u5bfc\u8bfb] \u00a0 \u8d28\u5b50\u4ea4\u6362\u819c\u71c3\u6599\u7535\u6c60\u4e2d\u7684\u50ac\u5316\u5242\u5c42\u7531\u8d1f\u8f7d\u5728\u78b3\u805a\u96c6\u4f53\u4e0a\u7684\u94c2\u65cf\u91d1\u5c5e\u7eb3\u7c73\u50ac\u5316\u5242\u7ec4\u6210\uff0c\u5e76\u901a\u8fc7\u79bb\u5b50\u805a\u5408\u7269\u7f51\u7edc\u7684\u6e17\u900f\u5f62\u6210\u591a\u5b54\u7ed3\u6784\u3002\u8fd9\u4e9b\u5f02\u8d28\u7ec4\u88c5\u4f53\u7684\u5c40\u90e8\u7ed3\u6784&#8230;<\/p>\n","protected":false},"author":34419,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[4848,27],"class_list":["post-252677","post","type-post","status-publish","format-standard","hentry","category-jiedu","tag-3d","tag-cell"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/252677"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/34419"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=252677"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/252677\/revisions"}],"predecessor-version":[{"id":252715,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/252677\/revisions\/252715"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=252677"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=252677"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=252677"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}