{"id":255151,"date":"2023-10-17T06:39:34","date_gmt":"2023-10-16T22:39:34","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=255151"},"modified":"2023-10-16T16:43:28","modified_gmt":"2023-10-16T08:43:28","slug":"%e7%b1%bb%e9%87%91%e5%88%9a%e7%9f%b3%e8%96%84%e8%86%9c%e7%bb%84%e5%88%86%e4%b8%8e%e7%bb%93%e6%9e%84%e5%92%8c%e6%91%a9%e6%93%a6%e7%95%8c%e9%9d%a2%e7%9a%84%e8%87%aa%e5%8c%b9%e9%85%8d%e8%b0%83%e6%8e%a7","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=255151","title":{"rendered":"\u7c7b\u91d1\u521a\u77f3\u8584\u819c\u7ec4\u5206\u4e0e\u7ed3\u6784\u548c\u6469\u64e6\u754c\u9762\u7684\u81ea\u5339\u914d\u8c03\u63a7\u5fae\u52a8\u8fd0\u884c\u5fae\u52a8\u72b6\u6001\u548c\u8f6c\u79fb\u819c\u7684\u6f14\u5316\u673a\u5236"},"content":{"rendered":"<p>\u5fae\u52a8\uff08fretting\uff09\u662f\u6307\u5728\u673a\u68b0\u632f\u52a8\u3001\u75b2\u52b3\u8f7d\u8377\u3001\u7535\u78c1\u632f\u52a8\u3001\u6216\u70ed\u5faa\u73af\u7b49\u4ea4\u53d8\u8f7d\u8377\u4f5c\u7528\u4e0b\uff0c\u63a5\u89e6\u8868\u9762\u95f4\u53d1\u751f\u7684\u632f\u5e45\u6781\u5c0f\uff08\u901a\u5e38\u4e3a\u5fae\u7c73\u91cf\u7ea7\uff09\u7684\u76f8\u5bf9\u8fd0\u52a8\u3002\u5fae\u52a8\u662f\u4e00\u79cd\u4e0d\u540c\u4e8e\u6ed1\u52a8\u548c\u6eda\u52a8\u7684\u6469\u64e6\u8fd0\u52a8\u65b9\u5f0f\uff0c\u7531\u4e8e\u5176\u76f8\u5bf9\u8fd0\u52a8\u7684\u5e45\u5ea6\u5f88\u5c0f\uff0c\u6240\u4ee5\u5177\u6709\u5f88\u9ad8\u7684\u9690\u853d\u6027\u3002\u5fae\u52a8\u4f1a\u9020\u6210\u63a5\u89e6\u8868\u9762\u95f4\u7684\u78e8\u635f\uff0c\u4ea7\u751f\u6750\u6599\u635f\u5931\u548c\u6784\u4ef6\u5c3a\u5bf8\u53d8\u5316\uff0c\u5f15\u8d77\u6784\u4ef6\u54ac\u5408\u3001\u677e\u52a8\u3001\u529f\u7387\u635f\u5931\u3001\u632f\u52a8\u566a\u58f0\u589e\u52a0\u7b49\u5931\u6548\u73b0\u8c61\uff1b\u4e5f\u4f1a\u4ea7\u751f\u75b2\u52b3\uff0c\u8bf1\u5bfc\u96f6\u90e8\u4ef6\u5c40\u90e8\u840c\u751f\u88c2\u7eb9\u5e76\u6269\u5c55\uff0c\u4e25\u91cd\u7f29\u77ed\u6784\u4ef6\u7684\u4f7f\u7528\u5bff\u547d\u3002\u8868\u9762\u5de5\u7a0b\u6280\u672f\u5bf9\u51cf\u7f13\u548c\u9884\u9632\u5fae\u52a8\u635f\u4f24\u975e\u5e38\u6709\u6548\uff0c\u4f46\u8868\u9762\u5de5\u7a0b\u6280\u672f\u79cd\u7c7b\u7e41\u591a\uff0c\u5728\u5fae\u52a8\u6469\u64e6\u6761\u4ef6\u4e0b\u7684\u635f\u4f24\u673a\u7406\u5dee\u5f02\u5f88\u5927\uff0c\u6240\u4ee5\u7cfb\u7edf\u5730\u7814\u7a76\u5fae\u52a8\u5de5\u51b5\u6761\u4ef6\u4e0e\u635f\u4f24\u673a\u7406\u95f4\u7684\u5173\u8054\u662f\u5341\u5206\u5fc5\u8981\u7684\u3002<\/p>\n<p>\u5fae\u52a8\u6469\u64e6\u7531\u4e8e\u4f4d\u79fb\u5e45\u503c\u6781\u5c0f\uff0c\u5728\u6469\u64e6\u8fc7\u7a0b\u4e2d\u4ea7\u751f\u7684\u78e8\u5c51\u5f88\u96be\u53ca\u65f6\u6392\u51fa\uff0c\u4f1a\u5728\u63a5\u89e6\u754c\u9762\u95f4\u5f62\u6210\u7b2c\u4e09\u4f53\u5c42\u52a0\u901f\u5bf9\u57fa\u5e95\u6750\u6599\u7684\u78e8\u635f\u3002\u7c7b\u91d1\u521a\u77f3\u78b3\uff08DLC\uff09\u8584\u819c\u662f\u4e00\u79cd\u7531\u91d1\u521a\u77f3\u7ed3\u6784\u7684sp<sup>3<\/sup>\u6742\u5316\u78b3\u539f\u5b50\u548c\u77f3\u58a8\u7ed3\u6784\u7684sp<sup>2<\/sup>\u6742\u5316\u78b3\u539f\u5b50\u7ec4\u6210\u7684\u975e\u6676\u6001\u7ed3\u6784\u6750\u6599\uff0c\u5177\u6709\u7c7b\u91d1\u521a\u77f3\u78b3\u4f18\u5f02\u7684\u673a\u68b0\u5f3a\u5ea6\u548c\u7c7b\u77f3\u58a8\u826f\u597d\u7684\u6469\u64e6\u6027\u80fd\u3002\u6700\u91cd\u8981\u7684\u662fDLC\u8584\u819c\u4f5c\u4e3a\u4e00\u79cd\u81ea\u6da6\u6ed1\u6750\u6599\uff0c\u5728\u6469\u64e6\u8fc7\u7a0b\u4e2d\u4ea7\u751f\u7684\u78e8\u5c51\u6b63\u597d\u53ef\u4ee5\u6210\u4e3a\u56fa\u4f53\u6da6\u6ed1\u5242\uff0c\u5bf9\u57fa\u5e95\u8d77\u5230\u51cf\u6469\u6297\u78e8\u7684\u4fdd\u62a4\u4f5c\u7528\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c<strong><b>\u897f\u5357\u4ea4\u901a\u5927\u5b66\u6750\u6599\u670d\u5f79\u884c\u4e3a<\/b><\/strong><strong><b>\u4e0e\u5b89\u5168\u8bc4\u4ef7<\/b><\/strong><strong><b>\u56e2\u961f<\/b><\/strong>\u7814\u7a76\u4e86\u901a\u8fc7\u81ea\u914d\u5bf9\u542b\u6c22DLC\u8584\u819c\u4e0eCr\u63ba\u6742DLC\u8584\u819c\u3001\u901a\u8fc7\u70ed\u5904\u7406\u8c03\u63a7DLC\u7684\u7ec4\u5206\u4e0e\u7ed3\u6784\u540e\uff0c\u7cfb\u7edf\u63a2\u7a76\u4e86DLC\u8584\u819c\u5728\u4e0d\u540c\u6cd5\u5411\u8d1f\u8377\u548c\u4f4d\u79fb\u5e45\u503c\u5de5\u51b5\u4e0b\u7684\u5fae\u52a8\u884c\u4e3a\u3002\u901a\u8fc7DLC\u8584\u819c\u914d\u5bf9\u548c\u7ec4\u5206\u4e0e\u7ed3\u6784\u6f14\u53d8\u63a7\u5236\u6469\u64e6\u63a5\u89e6\u754c\u9762\u72b6\u6001\uff0c\u9610\u660e\u4e86\u8f6c\u79fb\u819c\u964d\u4f4e\u6469\u64e6\u7684\u673a\u7406\u548c\u5f15\u8d77\u6469\u64e6\u884c\u4e3a\u5dee\u5f02\u7684\u539f\u56e0\u3002\u7ed3\u679c\u8868\u660e\uff0c\u968f\u7740\u65bd\u52a0\u8f7d\u8377\u7684\u589e\u52a0\uff0c\u76f8\u5bf9\u6ed1\u79fb\u51cf\u5c0f\uff0c\u5f39\u6027\u53d8\u5f62\u589e\u5927\uff0c\u5fae\u52a8\u533a\u57df\u5411\u7740\u90e8\u5206\u6ed1\u79fb\u533a\u53d1\u5c55\uff0c\u800c\u632f\u5e45\u7684\u589e\u52a0\u4f7f\u5fae\u52a8\u533a\u57df\u5411\u6ed1\u79fb\u533a\u79fb\u52a8\uff1b\u5728\u5fae\u52a8\u8fc7\u7a0b\u4e2d\uff0c\u7b2c\u4e09\u4f53\u5c42\u8f6c\u79fb\u5230\u5bf9\u5076\u7403\u8868\u9762\uff0c\u5f62\u6210\u5747\u5300\u81f4\u5bc6\u7684\u77f3\u58a8\u5316\u7684\u8f6c\u79fb\u819c\uff1bDLC\u8584\u819csp<sup>2<\/sup>\/sp<sup>3<\/sup>\u6742\u5316\u78b3\u542b\u91cf\u3001\u5fae\u89c2\u7ec4\u7ec7\u7ed3\u6784\uff08\u7279\u522b\u662f\u77ed\u7a0b\u6709\u5e8f\u7ed3\u6784\uff09\u548c\u5b8f\u89c2\u529b\u5b66\u6027\u80fd\u7684\u5dee\u5f02\u4e0d\u4ec5\u5f71\u54cd\u4e86\u8dd1\u5408\u671f\u957f\u77ed\uff0c\u66f4\u5f71\u54cd\u4e86\u8f6c\u79fb\u819c\u7684\u5f62\u6210\u901f\u7387\u548c\u77f3\u58a8\u5316\u7a0b\u5ea6\uff0c\u4ece\u800c\u5bfc\u81f4\u4e86\u9540\u8584\u819c\u7684\u6469\u64e6\u7cfb\u7edf\u5fae\u52a8\u884c\u4e3a\u5dee\u5f02\uff0c\u5b9e\u73b0\u4e86DLC\u8584\u819c\u5bf9\u5fae\u52a8\u8fd0\u884c\u72b6\u6001\u7684\u53ef\u8c03\u63a7\u6027\uff0c\u5bf9\u89e3\u51b3\u5de5\u4e1a\u754c\u5fae\u52a8\u78e8\u635f\u5177\u6709\u4e00\u5b9a\u7684\u6307\u5bfc\u610f\u4e49\u3002<\/p>\n<p>\u8be5\u7814\u7a76\u8fd1\u65e5\u4ee5\u9898\u4e3a\u201cFretting behaviors of self-mated diamond-like carbon films: The evolution of fretting regime and transfer film\u201d\u548c\u201cRegulating the fretting behavior of diamond-like carbon films by changing the composition and structure\u201d\u53d1\u8868\u5728\u77e5\u540d\u671f\u520aCarbon\u4e0a(Carbon 203 (2023) 695-705\u548cCarbon (2023) 118097)\u3002\u8bba\u6587\u7684\u7b2c\u4e00\u4f5c\u8005\u4e3a\u897f\u5357\u4ea4\u901a\u5927\u5b66<strong><b>\u535a\u58eb\u751f<\/b><\/strong><strong><b>\u5cb3\u7167\u51e1<\/b><\/strong>\uff0c\u901a\u8baf\u4f5c\u8005\u4e3a<strong><b>\u6a0a\u5c0f\u5f3a\u6559\u6388<\/b><\/strong>\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-255153\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/10\/\u56fe\u7247-1-10.png\" alt=\"\" width=\"800\" height=\"760\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/10\/\u56fe\u7247-1-10.png 800w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/10\/\u56fe\u7247-1-10-300x285.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/10\/\u56fe\u7247-1-10-768x730.png 768w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>1<\/b><\/strong><strong><b>.<\/b><\/strong>\u00a0DLC\u8584\u819c\u590d\u914d\u8c03\u63a7\u5fae\u52a8\u6469\u64e6\u884c\u4e3a\u548c\u5fae\u52a8\u8fd0\u884c\u72b6\u6001\u6f14\u53d8.<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-255154\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/10\/\u56fe\u7247-2-10.png\" alt=\"\" width=\"800\" height=\"555\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/10\/\u56fe\u7247-2-10.png 800w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/10\/\u56fe\u7247-2-10-300x208.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/10\/\u56fe\u7247-2-10-768x533.png 768w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>2<\/b><\/strong><strong><b>.<\/b><\/strong>\u00a0DLC\u8584\u819c\u7ec4\u5206\u4e0e\u7ed3\u6784\u53d8\u5316\u8c03\u63a7\u5fae\u52a8\u6469\u64e6\u884c\u4e3a\u548c\u5fae\u52a8\u8fd0\u884c\u72b6\u6001\u6f14\u53d8<\/p>\n<p><strong>\u539f\u6587\u94fe\u63a5\uff1a<\/strong><\/p>\n<p><a href=\"https:\/\/doi.org\/10.1016\/j.carbon.2022.12.032\"><u>https:\/\/doi.org\/10.1016\/j.carbon.2022.12.032<\/u><\/a><\/p>\n<p><a href=\"https:\/\/doi.org\/10.1016\/j.carbon.2023.118097\"><u>https:\/\/doi.org\/10.1016\/j.carbon.2023.118097<\/u><\/a><\/p>\n<p><strong><b>\u56e2\u961f<\/b><\/strong><strong><b>\u4ecb\u7ecd<\/b><\/strong><\/p>\n<p>\u6750\u6599\u670d\u5f79\u884c\u4e3a\u4e0e\u5b89\u5168\u8bc4\u4ef7\u56e2\u961f\u4f9d\u6258\u8f68\u9053\u4ea4\u901a\u8fd0\u8f7d\u7cfb\u7edf\u5168\u56fd\u91cd\u70b9\u5b9e\u9a8c\u5ba4\u3001\u6750\u6599\u5148\u8fdb\u6280\u672f\u6559\u80b2\u90e8\u91cd\u70b9\u5b9e\u9a8c\u5ba4\u7b49\u56fd\u5bb6\u7ea7\u79d1\u7814\u5e73\u53f0\uff0c\u96c6\u57fa\u7840\u7406\u8bba\u7814\u7a76\u3001\u524d\u6cbf\u6280\u672f\u7814\u7a76\u4e0e\u5f00\u53d1\u4e8e\u4e00\u4f53\uff0c\u4ece\u4e8b\u5fae\u52a8\u78e8\u635f\u4e0e\u5fae\u52a8\u75b2\u52b3\u673a\u7406\u53ca\u5176\u9632\u62a4\u3001\u94c1\u8def\u6469\u64e6\u5b66\uff08\u8f6e\u8f68\u3001\u5f13\u7f51\u3001\u5236\u52a8\u7b49\u6469\u64e6\u78e8\u635f\u673a\u7406\uff09\u3001\u87ba\u6813\u8fde\u63a5\u5931\u6548\uff08\u677e\u52a8\u4e0e\u65ad\u88c2\uff09\u673a\u7406\u53ca\u9632\u62a4\u3001\u8010\u78e8\u51cf\u6469\u6750\u6599\u53ca\u5176\u8868\u9762\u5de5\u7a0b\u6280\u672f\u3001\u76f8\u5173\u68c0\u6d4b\u8bbe\u5907\u7814\u53d1\u7b49\u9886\u57df\u7684\u6559\u5b66\u4e0e\u79d1\u7814\u5de5\u4f5c\u3002\u56e2\u961f\u73b0\u6709\u6559\u63882\u540d\u3001\u526f\u6559\u63885\u540d\u3001\u526f\u7814\u7a76\u54581\u540d\u3001\u52a9\u7406\u6559\u63881\u540d\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-255155\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/10\/\u56fe\u7247-3-9.png\" alt=\"\" width=\"216\" height=\"324\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/10\/\u56fe\u7247-3-9.png 216w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/10\/\u56fe\u7247-3-9-200x300.png 200w\" sizes=\"(max-width: 216px) 100vw, 216px\" \/><\/p>\n<p><strong><b>\u56e2\u961f\u8d1f\u8d23\u4eba\uff1a<\/b><\/strong><strong><b>\u6731\u65fb\u660a<\/b><\/strong><strong><b>\u00a0\u6559\u6388<\/b><\/strong>\uff0c\u897f\u5357\u4ea4\u901a\u5927\u5b66\u9996\u5e2d\u6559\u6388\uff0c\u56fd\u5bb6\u6770\u9752\u3001\u201c\u957f\u6c5f\u5b66\u8005\u201d\u7279\u8058\u6559\u6388\u3001\u201c\u4e07\u4eba\u8ba1\u5212\u201d\u9886\u519b\u4eba\u624d\u3001\u6559\u80b2\u90e8\u521b\u65b0\u56e2\u961f\u5e26\u5934\u4eba\u3001\u5168\u56fd\u4f18\u79c0\u535a\u58eb\u8bba\u6587\u83b7\u5f97\u8005\u3002\u8f68\u9053\u4ea4\u901a\u5b89\u5168\u7814\u7a76\u9662\u9662\u957f\u3002<\/p>\n<p>\u4e3b\u8981\u4ece\u4e8b\u6469\u64e6\u5b66\uff08\u5fae\u52a8\u6469\u64e6\u5b66\u3001\u94c1\u8def\u6469\u64e6\u5b66\u7b49\uff09\u3001\u8868\u9762\u5de5\u7a0b\u3001\u6750\u6599\u670d\u5f79\u884c\u4e3a\u7814\u7a76\u7b49\u3002\u66fe\u8363\u83b7\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u4e8c\u7b49\u5956\u3001\u6559\u80b2\u90e8\u81ea\u7136\u79d1\u5b66\u4e00\u7b49\u5956\u3001\u56db\u5ddd\u7701\u79d1\u6280\u8fdb\u6b65\u4e8c\u7b49\u5956\u3001\u6cd5\u56fd\u822a\u7a7a\u822a\u5929\u96c6\u56e2SNECMA\u79d1\u6280\u5956\uff08\u4e8c\u7b49\uff09\u3001\u8305\u4ee5\u5347\u94c1\u9053\u79d1\u5b66\u6280\u672f\u5956\u3002\u5df2\u51fa\u7248\u4e13\u84575\u90e8\u3001\u6388\u6743\u56fd\u5bb6\u53d1\u660e\u4e13\u522950\u4f59\u9879\uff1b\u5728\u56fd\u5185\u5916\u5b66\u672f\u671f\u520a\u4e0a\u53d1\u8868\u8bba\u6587550\u4f59\u7bc7\uff08SCI\u6536\u5f55300\u4f59\u7bc7\uff09\uff0c2009\u5e74\u4ee5\u6765\u6709\u5173\u201c\u5fae\u52a8\uff08fretting\uff09\u201d\u7684SCI\u8bba\u6587\u5728\u56fd\u9645\u4e0a\u6392\u540d\u7b2c1\uff1b\u62c5\u4efb\u56fd\u9645\u5fae\u52a8\u75b2\u52b3\u4f1a\u8bae\uff08ISFF\uff09\u56fd\u9645\u6267\u59d4\uff0c\u4e3b\u529e\u56fd\u9645\u4f1a\u8bae3\u6b21\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-255156\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/10\/\u56fe\u7247-4-8.png\" alt=\"\" width=\"216\" height=\"216\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/10\/\u56fe\u7247-4-8.png 216w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2023\/10\/\u56fe\u7247-4-8-150x150.png 150w\" sizes=\"(max-width: 216px) 100vw, 216px\" \/><\/p>\n<p>\u6a0a\u5c0f\u5f3a\u00a0\u6559\u6388\uff0c\u56db\u5ddd\u7701\u6770\u9752\u3001\u7701\u7279\u8058\u4e13\u5bb6\u3002\u8363\u83b7\u6e29\u8bd7\u94f8\u67ab\u53f6\u5956\u3001\u5e7f\u897f\u79d1\u6280\u8fdb\u6b65\u4e00\u7b49\u5956\u3001\u5168\u56fd\u94c1\u8def\u9752\u5e74\u79d1\u6280\u521b\u65b0\u5956\u3001\u4e2d\u56fd\u79d1\u5b66\u9662\u9662\u957f\u4f18\u79c0\u5956\u3001\u7b2c\u4e03\u5c4aIFAM\u4f18\u79c0\u9752\u5e74\u79d1\u5b66\u5bb6\u5956\u7b49\u8363\u8a89\uff0c\u5165\u9009\u65af\u5766\u798f\u5168\u7403\u524d2%\u79d1\u5b66\u5bb6\u699c\u5355\u3002\u4e3b\u8981\u4ece\u4e8b\u78e8\u8680\u8026\u5408\u5931\u6548\u673a\u5236\u548c\u9632\u62a4\u6280\u672f\u65b9\u9762\u7684\u7814\u7a76\uff0c\u4ee5\u7b2c\u4e00\u6216\u901a\u8baf\u4f5c\u8005\u5df2\u5728\u56fd\u9645\u6743\u5a01\u671f\u520a\u53d1\u8868SCI\u4e00\u533a\u6587\u7ae080\u4f59\u7bc7\uff08\u4ed6\u5f152600\u4f59\u6b21\uff09\uff0c\u6388\u6743\u56fd\u5bb6\u53d1\u660e\u4e13\u522920\u4ef6\uff0c\u83b7\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\uff08\u9752\u5e74\u3001\u9762\u4e0a\u3001\u8054\u5408\u57fa\u91d1\uff09\u7b49\u8d44\u52a9\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u5fae\u52a8\uff08fretting\uff09\u662f\u6307\u5728\u673a\u68b0\u632f\u52a8\u3001\u75b2\u52b3\u8f7d\u8377\u3001\u7535\u78c1\u632f\u52a8\u3001\u6216\u70ed\u5faa\u73af\u7b49\u4ea4\u53d8\u8f7d\u8377\u4f5c\u7528\u4e0b\uff0c\u63a5\u89e6\u8868\u9762\u95f4\u53d1\u751f\u7684\u632f\u5e45\u6781\u5c0f\uff08\u901a\u5e38\u4e3a\u5fae\u7c73\u91cf\u7ea7\uff09\u7684\u76f8\u5bf9\u8fd0\u52a8\u3002\u5fae\u52a8\u662f\u4e00\u79cd\u4e0d\u540c\u4e8e\u6ed1\u52a8&#8230;<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-255151","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/255151"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=255151"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/255151\/revisions"}],"predecessor-version":[{"id":255157,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/255151\/revisions\/255157"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=255151"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=255151"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=255151"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}