{"id":256616,"date":"2023-12-19T06:52:05","date_gmt":"2023-12-18T22:52:05","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=256616"},"modified":"2023-12-18T17:00:44","modified_gmt":"2023-12-18T09:00:44","slug":"%e6%b7%b1%e5%9c%b3%e5%9b%bd%e9%99%85%e7%a0%94%e7%a9%b6%e7%94%9f%e9%99%a2%e5%bc%a0%e7%92%87%e3%80%81%e5%91%a8%e5%85%89%e6%95%8f%e5%9b%a2%e9%98%9f%e5%9c%a8%e8%81%94%e9%82%a6%e5%ad%a6%e4%b9%a0%e5%ae%9e","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=256616","title":{"rendered":"\u6e05\u534e\u6df1\u5733\u56fd\u9645\u7814\u7a76\u751f\u9662\u5f20\u7487\u3001\u5468\u5149\u654fNat. Commun.\uff1a\u8054\u90a6\u673a\u5668\u5b66\u4e60\u5b9e\u73b0\u9000\u5f79\u7535\u6c60\u534f\u540c\u5206\u7c7b\u56de\u6536"},"content":{"rendered":"<p class=\"vsbcontent_start\"><strong>\u6e05\u534e\u65b0\u95fb\u7f5112\u670815\u65e5\u7535<\/strong>\u00a0\u5728\u9000\u5f79\u7535\u6c60\u56de\u6536\u884c\u4e1a\u4e2d\uff0c\u6b63\u6781\u6750\u6599\u7684\u56de\u6536\u4ef7\u503c\u6781\u9ad8\u3002\u4f20\u7edf\u7684\u5904\u7406\u65b9\u5f0f\uff08\u4f8b\u5982\u706b\u6cd5\u3001\u6e7f\u6cd5\uff09\u901a\u5e38\u4e0d\u5bf9\u6b63\u6781\u6750\u6599\u8fdb\u884c\u5206\u7c7b\uff0c\u800c\u4ee5\u6df7\u5408\u5f62\u5f0f\u56de\u6536\uff0c\u8d44\u6e90\u5229\u7528\u6548\u7387\u4f4e\u4e14\u5229\u6da6\u6709\u9650\u3002\u76f8\u8f83\u4e4b\u4e0b\uff0c\u76f4\u63a5\u56de\u6536\uff08\u4fee\u590d\uff09\u65b9\u6cd5\u53ef\u4ee5\u663e\u8457\u63d0\u5347\u7ecf\u6d4e\u4ef7\u503c\uff0c\u5177\u6709\u5de5\u827a\u6d41\u7a0b\u77ed\u3001\u4e8c\u6b21\u80fd\u6e90\u6d88\u8017\u548c\u6c61\u67d3\u4f4e\u3001\u7ecf\u6d4e\u6548\u76ca\u9ad8\u7684\u4f18\u70b9\uff0c\u4f46\u9700\u8981\u4e8b\u5148\u83b7\u53d6\u7535\u6c60\u7684\u6b63\u6781\u6750\u6599\u4fe1\u606f\u3002\u8fd9\u4e9b\u4fe1\u606f\u6d89\u53ca\u5236\u9020\u5546\u3001\u7528\u6237\u3001\u79d1\u7814\u673a\u6784\u7b49\u654f\u611f\u6570\u636e\uff0c\u96be\u4ee5\u83b7\u53d6\u548c\u96c6\u4e2d\u5229\u7528\u3002\u6b64\u5916\uff0c\u7535\u6c60\u5236\u9020\u6807\u51c6\u591a\u6837\u6027\u3001\u5386\u53f2\u8fd0\u884c\u6761\u4ef6\u5dee\u5f02\u548c\u591a\u65b9\uff08\u56de\u6536\u5408\u4f5c\u8005\uff09\u534f\u4f5c\u65f6\u7684\u6570\u636e\u9690\u79c1\u95ee\u9898\u52a0\u5267\u4e86\u9000\u5f79\u7535\u6c60\u5206\u7c7b\u7684\u96be\u5ea6\uff0c\u5236\u7ea6\u4e86\u56de\u6536\u6548\u7387\u7684\u63d0\u5347\u548c\u56de\u6536\u4ea7\u4e1a\u7684\u89c4\u6a21\u5316\u53d1\u5c55\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u6e05\u534e\u5927\u5b66\u6df1\u5733\u56fd\u9645\u7814\u7a76\u751f\u9662\u5f20\u7487\u3001\u5468\u5149\u654f\u56e2\u961f\u5efa\u7acb\u4e86\u57fa\u4e8e\u8054\u90a6\u5b66\u4e60\u7684\u9000\u5f79\u7535\u6c60\u5feb\u901f\u5206\u7c7b\u6a21\u578b\uff0c\u65e0\u9700\u5386\u53f2\u8fd0\u884c\u6570\u636e\uff0c\u4ec5\u7528\u5c11\u91cf\u73b0\u573a\u6d4b\u8bd5\u4fe1\u606f\u5373\u53ef\u5b9e\u73b0\u9000\u5f79\u7535\u6c60\u6b63\u6781\u6750\u6599\u7684\u7cbe\u786e\u5206\u7c7b\u3002<\/p>\n<p>\u56e2\u961f\u6536\u96c6\u4e86\u6765\u81ea7\u4e2a\u5236\u9020\u5546\u3001\u5305\u542b5\u79cd\u6b63\u6781\u6750\u6599\u3001\u5177\u6709\u4e0d\u540c\u5386\u53f2\u4f7f\u7528\u60c5\u51b5\uff08\u5982\u6765\u81ea\u5b9e\u9a8c\u5ba4\u6d4b\u8bd5\u3001\u7535\u52a8\u6c7d\u8f66\u8fd0\u884c\u7b49\uff09\u7684130\u4e2a\u9000\u5f79\u7535\u6c60\u7684\u6570\u636e\uff08\u56fe1\uff09\uff0c\u4ec5\u5229\u7528\u56de\u6536\u73b0\u573a\u6d4b\u8bd5\u7684\u4e00\u6b21\u5faa\u73af\u5145\u653e\u7535\u6570\u636e\uff0c\u901a\u8fc7\u6570\u636e\u6e05\u6d17\u548c\u566a\u58f0\u5904\u7406\uff08\u4fdd\u7559\u4e86\u4eba\u4e3a\u548c\u6b63\u6781\u8d28\u5f02\u6027\u5f15\u8d77\u7684\u566a\u58f0\uff09\uff0c\u5f62\u6210\u4e86\u9002\u7528\u4e8e\u7279\u5f81\u5de5\u7a0b\u7684\u6807\u51c6\u5316\u53c2\u6570\u66f2\u7ebf\u3002\u7279\u5f81\u5de5\u7a0b\u91cd\u70b9\u5173\u6ce8\u9000\u5f79\u7535\u6c60\u5728\u6700\u540e\u4e00\u4e2a\u5468\u671f\u7684\u5145\u653e\u7535\u4fe1\u606f\uff0c\u4ece\u7535\u538b-\u5bb9\u91cf\u548cdQ\/dV\u66f2\u7ebf\u4e2d\u63d0\u53d6\u4e8630\u4e2a\u7279\u5f81\uff0c\u7528\u4e8e\u6307\u5bfc\u7535\u6c60\u5206\u7c7b\u3002<\/p>\n<p><img decoding=\"async\" class=\"img_vsb_content aligncenter\" title=\"20231212-\u56fe1 \u7279\u5f81\u5de5\u7a0b\u7ed3\u679c-\u5f20\u7487\u56e2\u961f-\u56fd\u9645\u7814\u7a76\u751f\u9662.jpg\" src=\"https:\/\/www.tsinghua.edu.cn\/__local\/4\/71\/C1\/DAEEB8DC1B059189C3008292965_7EFA503D_1C1D08.jpg\" alt=\"undefined\" width=\"554\" height=\"\" border=\"0\" vspace=\"0\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe1.\u7279\u5f81\u5de5\u7a0b\u7ed3\u679c<\/strong><\/p>\n<p>\u7814\u7a76\u4eba\u5458\u91c7\u7528\u8054\u90a6\u5b66\u4e60\u6846\u67b6\u8fdb\u884c\u9000\u5f79\u7535\u6c60\u6b63\u6781\u6750\u6599\u5206\u7c7b\uff08\u56fe2\uff09\uff1a\u9996\u5148\u4f7f\u7528\u5404\u53c2\u4e0e\u65b9\uff08\u56de\u6536\u5408\u4f5c\u8005\uff09\u7684\u672c\u5730\u6570\u636e\u3001\u4ee5\u5e76\u884c\u65b9\u5f0f\u8bad\u7ec3\u672c\u5730\u968f\u673a\u68ee\u6797\u6a21\u578b\uff0c\u518d\u901a\u8fc7Wasserstein-Distance\u6295\u7968\uff08WDV\uff09\u7b56\u7565\u5c06\u53c2\u4e0e\u65b9\u672c\u5730\u6a21\u578b\u805a\u5408\u6210\u5168\u5c40\u6a21\u578b\u3002\u8054\u90a6\u5b66\u4e60\u6709\u6548\u5229\u7528\u4e86\u6765\u81ea\u591a\u65b9\u7684\u672c\u5730\u5927\u89c4\u6a21\u7535\u6c60\u6570\u636e\uff0c\u4e14\u6570\u636e\u65e0\u9700\u5728\u53c2\u4e0e\u65b9\u4e4b\u95f4\u5171\u4eab\uff0c\u5145\u5206\u4fdd\u62a4\u4e86\u591a\u65b9\u534f\u4f5c\u65f6\u7684\u6570\u636e\u9690\u79c1\u3002<\/p>\n<p><img decoding=\"async\" class=\"img_vsb_content aligncenter\" title=\"20231212-\u56fe2 \u57fa\u4e8e\u8054\u90a6\u5b66\u4e60\u7684\u7535\u6c60\u56de\u6536\u5206\u7c7b\u6846\u67b6-\u5f20\u7487\u56e2\u961f-\u56fd\u9645\u7814\u7a76\u751f\u9662.jpg\" src=\"https:\/\/www.tsinghua.edu.cn\/__local\/6\/21\/81\/6E3E29C245AE567478378EBF3D5_D67B3A5D_CCEE9.jpg\" alt=\"undefined\" width=\"554\" height=\"\" border=\"0\" vspace=\"0\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe2. \u57fa\u4e8e\u8054\u90a6\u5b66\u4e60\u7684\u7535\u6c60\u56de\u6536\u5206\u7c7b\u6846\u67b6<\/strong><\/p>\n<p>\u540c\u65f6\uff0c\u56e2\u961f\u8003\u8651\u4e86\u540c\u8d28\u6027\uff08\u56fe3\uff09\u548c\u8d28\u5f02\u6027\uff08\u56fe4\uff09\u9000\u5f79\u573a\u666f\uff0c\u5728\u4e24\u79cd\u573a\u666f\u4e0b\u5747\u5b9e\u73b0\u4e86\u9ad8\u7cbe\u5ea6\u5206\u7c7b\u3002\u5176\u4e2d\uff0c\u91c7\u7528WDV\u7b56\u7565\u7684\u8054\u90a6\u5b66\u4e60\u65b9\u6cd5\u76f8\u8f83\u4e8e\u5176\u5b83\u65b9\u6cd5\u5206\u7c7b\u7cbe\u5ea6\u9ad8\u3001\u9690\u79c1\u9884\u7b97\uff08PB\uff09\u9ad8\uff0c\u5728\u5b9e\u73b0\u9ad8\u7cbe\u5ea6\u5206\u7c7b\u7684\u540c\u65f6\uff0c\u6781\u5927\u964d\u4f4e\u4e86\u6570\u636e\u6cc4\u9732\u98ce\u9669\u3002<\/p>\n<p><img decoding=\"async\" class=\"img_vsb_content aligncenter\" title=\"20231212-\u56fe3 \u540c\u8d28\u6027\u9000\u5f79\u7535\u6c60\u5206\u7c7b\u7ed3\u679c-\u5f20\u7487\u56e2\u961f-\u56fd\u9645\u7814\u7a76\u751f\u9662.jpg\" src=\"https:\/\/www.tsinghua.edu.cn\/__local\/A\/DC\/94\/E82FFE8A09910C85CCCE80391CC_F4781A78_15D6C1.jpg\" alt=\"undefined\" width=\"554\" height=\"\" border=\"0\" vspace=\"0\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe3.\u540c\u8d28\u6027\u9000\u5f79\u7535\u6c60\u5206\u7c7b\u7ed3\u679c<\/strong><\/p>\n<p><img decoding=\"async\" class=\"img_vsb_content aligncenter\" title=\"20231212-\u56fe4 \u8d28\u5f02\u6027\u9000\u5f79\u7535\u6c60\u5206\u7c7b\u7ed3\u679c-\u5f20\u7487\u56e2\u961f-\u56fd\u9645\u7814\u7a76\u751f\u9662.jpg\" src=\"https:\/\/www.tsinghua.edu.cn\/__local\/4\/05\/41\/26C826BC24C9336D48003105FFF_945A18E5_140F56.jpg\" alt=\"undefined\" width=\"554\" height=\"\" border=\"0\" vspace=\"0\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe4. \u8d28\u5f02\u6027\u9000\u5f79\u7535\u6c60\u5206\u7c7b\u7ed3\u679c<\/strong><\/p>\n<p>\u56e2\u961f\u8fd8\u57fa\u4e8e\u4e0d\u540cLFP\/NMC\u6bd4\u4f8b\u7684\u7535\u6c60\u6570\u636e\uff0c\u5bf9\u4e09\u79cd\u673a\u5668\u5b66\u4e60\u5206\u7c7b\u65b9\u6cd5\uff08\u91c7\u7528\u591a\u6570\u6295\u7968MV\u3001Wasserstein-Distance\u6295\u7968WDV\u7684\u8054\u90a6\u5b66\u4e60\u65b9\u6cd5\u548c\u975e\u8054\u90a6\u5b66\u4e60\u65b9\u6cd5\uff09\u548c\u4e09\u79cd\u7535\u6c60\u56de\u6536\u65b9\u6cd5\uff08\u706b\u6cd5\u3001\u6e7f\u6cd5\u548c\u76f4\u63a5\u56de\u6536\u65b9\u6cd5\uff09\u8fdb\u884c\u4e86\u7ecf\u6d4e\u6027\u8bc4\u4f30\uff08\u56fe5\uff09\u3002\u7814\u7a76\u53d1\u73b0\uff0c\u57fa\u4e8e\u8054\u90a6\u5b66\u4e60\u7684\u7535\u6c60\u5206\u7c7b\u80fd\u9ad8\u6548\u534f\u540c\u56de\u6536\u5408\u4f5c\u8005\uff0c\u4fdd\u969c\u5927\u89c4\u6a21\u5206\u5e03\u5f0f\u7684\u7535\u6c60\u6570\u636e\u9690\u79c1\uff0c\u5e76\u5b9e\u73b0\u9000\u5f79\u7535\u6c60\u7684\u76c8\u5229\u6027\u76f4\u63a5\u56de\u6536\u3002<\/p>\n<p><img decoding=\"async\" class=\"img_vsb_content aligncenter\" title=\"20231212-\u56fe5 \u9000\u5f79\u7535\u6c60\u56de\u6536\u7684\u7ecf\u6d4e\u6027\u8bc4\u4f30-\u5f20\u7487\u56e2\u961f-\u56fd\u9645\u7814\u7a76\u751f\u9662.jpg\" src=\"https:\/\/www.tsinghua.edu.cn\/__local\/5\/79\/C8\/49AA68B659130E50BFD63A3A0B1_5B1F8770_FBF47.jpg\" alt=\"undefined\" width=\"554\" height=\"\" border=\"0\" vspace=\"0\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe5.\u9000\u5f79\u7535\u6c60\u56de\u6536\u7684\u7ecf\u6d4e\u6027\u8bc4\u4f30<\/strong><\/p>\n<p>\u76f8\u5173\u7814\u7a76\u6210\u679c\u4ee5\u201c\u901a\u8fc7\u8054\u90a6\u673a\u5668\u5b66\u4e60\u5b9e\u73b0\u9690\u79c1\u4fdd\u62a4\u7684\u9000\u5f79\u7535\u6c60\u534f\u540c\u5206\u7c7b\u548c\u76c8\u5229\u6027\u76f4\u63a5\u56de\u6536\u201d\uff08Collaborative and privacy-preserving retired battery sorting for profitable direct recycling via federated machine learning\uff09\u4e3a\u9898\u53d1\u8868\u5728\u300a\u81ea\u7136\u00b7\u901a\u8baf\u300b\uff08<em>Nature Communications<\/em>\uff09\u4e0a\u3002<\/p>\n<p>\u6e05\u534e\u5927\u5b66\u6df1\u5733\u56fd\u9645\u7814\u7a76\u751f\u96622022\u7ea7\u535a\u58eb\u7814\u7a76\u751f\u9676\u665f\u5b87\u4e3a\u8bba\u6587\u7b2c\u4e00\u4f5c\u8005\uff0c2022\u7ea7\u535a\u58eb\u7814\u7a76\u751f\u5218\u6d77\u821f\u548c2023\u7ea7\u535a\u58eb\u7814\u7a76\u751f\u5b59\u5d07\u535a\u4e3a\u8bba\u6587\u5171\u540c\u7b2c\u4e00\u4f5c\u8005\uff0c2023\u7ea7\u535a\u58eb\u7814\u7a76\u751f\u5b63\u660a\u94d6\u4e3a\u8bba\u6587\u7b2c\u4e8c\u4f5c\u8005\u3002\u6e05\u534e\u5927\u5b66\u6df1\u5733\u56fd\u9645\u7814\u7a76\u751f\u9662\u526f\u6559\u6388\u5f20\u7487\u3001\u5468\u5149\u654f\u548c\u6e05\u534e\u5927\u5b66\u3001\u592a\u539f\u7406\u5de5\u5927\u5b66\u6559\u6388\u5b59\u5b8f\u658c\u4e3a\u5171\u540c\u901a\u8baf\u4f5c\u8005\u3002\u5408\u4f5c\u8005\u5305\u62ec\u590d\u65e6\u5927\u5b66\u4fe1\u606f\u79d1\u5b66\u4e0e\u5de5\u7a0b\u5b66\u9662\u667a\u6167\u80fd\u6e90\u63a7\u5236\u4e0e\u4eff\u771f\u5b9e\u9a8c\u5ba4\u6559\u6388\u5b59\u8000\u6770\u3001\u526f\u7814\u7a76\u5458\u738b\u745c\uff0c2022\u7ea7\u535a\u58eb\u7814\u7a76\u751f\u4ed8\u8bd7\u610f\u548c\u817e\u8baf\u4eba\u5de5\u667a\u80fd\u5b9e\u9a8c\u5ba4\u4e13\u5bb6\u7814\u7a76\u5458\u8363\u94b0\u7b49\u3002\u8be5\u7814\u7a76\u5f97\u5230\u4e86\u6df1\u5733\u5e02\u79d1\u6280\u521b\u65b0\u59d4\u5458\u4f1a\u3001\u5c71\u897f\u7701\u80fd\u6e90\u4e92\u8054\u7f51\u7814\u7a76\u9662\u3001\u6e05\u534e\u5927\u5b66\u6df1\u5733\u56fd\u9645\u7814\u7a76\u751f\u9662\u3001\u6df1\u5733\u5e02\u9e4f\u745e\u57fa\u91d1\u4f1a\u7b49\u79d1\u7814\u7ecf\u8d39\u652f\u6301\u3002<\/p>\n<p>\u8bba\u6587\u94fe\u63a5\uff1a<a href=\"https:\/\/doi.org\/10.1038\/s41467-023-43883-y\">https:\/\/doi.org\/10.1038\/s41467-023-43883-y<\/a><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6e05\u534e\u65b0\u95fb\u7f5112\u670815\u65e5\u7535\u00a0\u5728\u9000\u5f79\u7535\u6c60\u56de\u6536\u884c\u4e1a\u4e2d\uff0c\u6b63\u6781\u6750\u6599\u7684\u56de\u6536\u4ef7\u503c\u6781\u9ad8\u3002\u4f20\u7edf\u7684\u5904\u7406\u65b9\u5f0f\uff08\u4f8b\u5982\u706b\u6cd5\u3001\u6e7f\u6cd5\uff09\u901a\u5e38\u4e0d\u5bf9\u6b63\u6781\u6750\u6599\u8fdb\u884c\u5206\u7c7b\uff0c\u800c\u4ee5\u6df7\u5408\u5f62\u5f0f\u56de\u6536\uff0c\u8d44\u6e90\u5229\u7528\u6548\u7387&#8230;<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-256616","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/256616"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=256616"}],"version-history":[{"count":5,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/256616\/revisions"}],"predecessor-version":[{"id":256622,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/256616\/revisions\/256622"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=256616"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=256616"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=256616"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}