{"id":257616,"date":"2024-02-01T07:26:33","date_gmt":"2024-01-31T23:26:33","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=257616"},"modified":"2024-01-31T21:29:46","modified_gmt":"2024-01-31T13:29:46","slug":"%e9%ab%98%e8%b4%a8%e9%87%8f%e5%8d%8a%e5%af%bc%e4%bd%93%e7%ba%a4%e7%bb%b4%ef%bc%81%e5%8d%97%e6%b4%8b%e7%90%86%e5%b7%a5%e5%a4%a7%e5%ad%a6%e6%b7%b1%e5%9c%b3%e5%85%88%e8%bf%9b%e9%99%a2%e8%8b%8f%e5%b7%9e","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=257616","title":{"rendered":"\u9ad8\u8d28\u91cf\u534a\u5bfc\u4f53\u7ea4\u7ef4\uff01\u5357\u6d0b\u7406\u5de5\u5927\u5b66&#038;\u6df1\u5733\u5148\u8fdb\u9662&#038;\u82cf\u5dde\u7eb3\u7c73\u6240\u4e09\u6821\u8054\u53d1Nature\uff01"},"content":{"rendered":"<p>\u4ee5\u7845\u9517\u4e3a\u4ee3\u8868\u7684\u534a\u5bfc\u4f53\u662f\u73b0\u4ee3\u7535\u5b50\u4ea7\u4e1a\u7684\u201c\u5927\u8111\u201d\u2014\u82af\u7247\u4e0d\u53ef\u6216\u7f3a\u7684\u5173\u952e\u6750\u6599\u3002\u8fd9\u4e9b\u65e0\u673a\u534a\u5bfc\u4f53\u5728\u5316\u5b66\u53ca\u70ed\u7a33\u5b9a\u6027\uff0c\u7535\u5b66\u6027\u80fd\uff0c\u89c4\u6a21\u5316\u751f\u4ea7\u7b49\u65b9\u9762\u5177\u6709\u4e0d\u53ef\u6bd4\u62df\u7684\u4f18\u52bf\u3002\u7136\u800c\u5728\u7535\u5b50\u4ea7\u4e1a\u62e5\u62b1\u67d4\u6027\u5316\u7684\u65b0\u8d8b\u52bf\u4e0b\uff0c\u8fd9\u4e9b\u534a\u5bfc\u4f53\u7684\u672c\u5f81\u8106\u6027\u7ed9\u79d1\u5b66\u5bb6\u5e26\u6765\u4e86\u4e0d\u5c0f\u7684\u6311\u6218\u3002\u5982\u4f55\u7528\u8fd9\u4e9b\u534a\u5bfc\u4f53\u53d1\u6325\u67d4\u6027\uff1f\u8fd1\u4e9b\u5e74\u56fd\u9645\u5b66\u672f\u754c\u76f8\u7ee7\u63d0\u51fa\u4e86\u4e00\u4e9b\u964d\u4f4e\u7ef4\u5ea6\u7684\u89e3\u51b3\u65b9\u6848\u3002\u4f8b\u5982\u91c7\u7528\u4e09\u7ef4\u5c3a\u5bf8\u6781\u5c0f\uff0c\u53ef\u4ee5\u8ba4\u4e3a\u662f\u96f6\u7ef4\u5f62\u6001\u7684\u7845\u201c\u70b9\u201d\uff0c\u4ee5\u9635\u5217\u5f62\u5f0f\u5206\u5e03\u5728\u67d4\u6027\u57fa\u5e95\u4e0a\uff0c\u5f62\u6210\u4e00\u4e2a\u8f6f\u786c\u4ea4\u8054\u7684\u7f51\u7edc\u6765\u5b9e\u73b0\u5bf9\u8106\u786c\u6750\u6599\u7684\u67d4\u6027\u5316\uff1b\u6216\u662f\u51cf\u5c0f\u6676\u5706\u7684\u539a\u5ea6\uff0c\u5e76\u949d\u5316\u673a\u68b0\u635f\u4f24\uff0c\u4ece\u800c\u5f97\u5230\u4e00\u5f20\u4e8c\u7ef4\u5f62\u6001\u53ef\u4ee5\u5f2f\u66f2\u7684\u7845\u8584\u819c\u3002\u7136\u800c\uff0c\u5bf9\u4e00\u7ef4\u5f62\u6001\u7684\u534a\u5bfc\u4f53\u7ea4\u7ef4\u7814\u7a76\u76f8\u5bf9\u8f83\u5c11\uff0c\u4e3b\u8981\u539f\u56e0\u662f\u5236\u5907\u5f02\u5e38\u56f0\u96be\u3002\u5728\u8fd9\u65b9\u9762\uff0c\u5c3d\u7ba1\u6709\u5fae\u4e0b\u62c9\u6cd5\u7b49\u4ece\u7194\u4f53\u51fa\u53d1\u7684\u6676\u4f53\u751f\u957f\u6cd5\u7684\u793a\u4f8b\uff0c\u4f46\u534a\u5bfc\u4f53\u7ea4\u7ef4\u7684\u5236\u5907\u4ecd\u7136\u9762\u4e34\u4e00\u4e9b\u91cd\u5927\u96be\u9898\u3002\u5176\u5173\u952e\u6311\u6218\u5728\u4e8e\uff1a\u5982\u4f55\u5927\u89c4\u6a21\u8fde\u7eed\u5236\u9020\u5177\u6709\u76f8\u5f53\u8d85\u957f\u548c\u65e0\u88c2\u7eb9\u7684\u534a\u5bfc\u4f53\u7ea4\u7ef4\u3002<\/p>\n<p>\u7194\u82af\u70ed\u62c9\u6cd5\u662f\u751f\u4ea7\u591a\u6750\u6599\u7ea4\u7ef4\u901a\u7528\u7684\u5927\u89c4\u6a21\u5236\u5907\u6280\u672f\uff0c\u8fd9\u79cd\u65b9\u6cd5\u5177\u6709\u4f4e\u6210\u672c\u3001\u9ad8\u4ea7\u7387\u548c\u8d85\u957f\u8fde\u7eed\u7b49\u4f18\u70b9\u3002\u7136\u800c\uff0c\u7194\u82af\u70ed\u62c9\u6cd5\u5236\u9020\u51fa\u7684\u534a\u5bfc\u4f53\u7ea4\u7ef4\u5f80\u5f80\u5177\u6709\u5f62\u72b6\u4e0d\u5747\u5300\uff0c\u7ea4\u82af\u65ad\u88c2\u591a\u53d1\u7b49\u7f3a\u9677\uff0c\u9650\u5236\u4e86\u5176\u5e7f\u6cdb\u7684\u5b9e\u9645\u5e94\u7528\u3002\u8981\u89e3\u51b3\u534a\u5bfc\u4f53\u7ea4\u7ef4\u7684\u751f\u4ea7\u96be\u9898\uff0c\u7194\u82af\u70ed\u62c9\u6cd5\u662f\u4e00\u4e2a\u6709\u6f5c\u529b\u7684\u529e\u6cd5\uff0c\u4f46\u9700\u8981\u4ece\u6839\u672c\u4e0a\u68b3\u7406\u6e05\u695a\u7f3a\u9677\u53d1\u751f\u673a\u5236\uff0c\u4ece\u6e90\u5934\u4e0a\u89e3\u51b3\u95ee\u9898\u3002\u5357\u6d0b\u7406\u5de5\u5927\u5b66\u9b4f\u78ca\u526f\u6559\u6388\u56e2\u961f\u8054\u5408\u5357\u6d0b\u7406\u5de5\u5927\u5b66\u9ad8\u534e\u5065\u9662\u58eb\u56e2\u961f\u3001\u6df1\u5733\u5148\u8fdb\u9662\u9648\u660e\u526f\u7814\u7a76\u5458\u56e2\u961f\u548c\u82cf\u5dde\u7eb3\u7c73\u6240\u5f20\u5176\u51b2\u7814\u7a76\u5458\u56e2\u961f\uff0c\u7a81\u7834\u4f20\u7edf\u601d\u7ef4\uff0c\u901a\u8fc7\u591a\u5b66\u79d1\u4ea4\u53c9\uff0c\u4ece\u57fa\u7840\u79d1\u5b66\u51fa\u53d1\u5e76\u7ed3\u5408\u5b9e\u9a8c\u9a8c\u8bc1\uff0c\u5206\u9636\u6bb5\u5730\u628a\u7194\u82af\u70ed\u62c9\u6cd5\u4e2d\u4e0d\u540c\u7684\u7269\u7406\u548c\u5316\u5b66\u8fc7\u7a0b\u6e05\u6670\u7684\u5f52\u7eb3\u603b\u7ed3\uff0c\u660e\u786e\u4e86\u7ea4\u7ef4\u5236\u5907\u4e2d\u5173\u952e\u7684\u6d41\u4f53\u548c\u56fa\u4f53\u529b\u5b66\u95ee\u9898\u3002\u5efa\u7acb\u4e86\u7194\u82af\u70ed\u62c9\u6cd5\u7684\u591a\u9636\u6bb5\u529b\u5b66\u6a21\u578b\uff0c\u5229\u7528\u8be5\u7406\u8bba\u6a21\u578b\u6307\u5bfc\u5de5\u827a\u4f18\u5316\uff0c\u53d1\u5c55\u4e86\u6838\u5fc3\u534a\u5bfc\u4f53\u6750\u6599\u548c\u58f3\u4f53\u6750\u6599\u7684\u673a\u68b0\u5339\u914d\u539f\u5219\uff0c\u6709\u6548\u89e3\u51b3\u4e86\u7ea4\u7ef4\u62c9\u5236\u8fc7\u7a0b\u4e2d\u7684\u6d41\u4f53\u4e0d\u7a33\u5b9a\u6027\u53ca\u673a\u68b0\u5931\u5339\u5bfc\u81f4\u7684\u88c2\u7eb9\u6269\u5c55\u96be\u9898\uff0c\u7a81\u7834\u8106\u6027\u65e0\u673a\u534a\u5bfc\u4f53\u6750\u6599\u7684\u7ea4\u7ef4\u67d4\u6027\u5316\u6280\u672f\uff0c\u5b9e\u73b0\u8d85\u957f\u3001\u65e0\u65ad\u88c2\u548c\u65e0\u6270\u52a8\u65e0\u673a\u534a\u5bfc\u4f53\u7ea4\u7ef4\u7684\u8fde\u7eed\u5316\u5236\u5907\u3002\u76f8\u5173\u6210\u679c\u4ee5\u300aHigh-quality semiconductor fibres via mechanical design\u300b\u4e3a\u9898\uff0c\u4e8e\u5317\u4eac\u65f6\u95f42\u67081\u65e5\u53d1\u8868\u5728Nature\u4e0a\u3002\u5357\u6d0b\u7406\u5de5\u5927\u5b66\u535a\u58eb\u540e\u6c6a\u5fd7\u52cb\u3001\u674e\u680b\u548c\u5409\u6797\u5927\u5b66\u6559\u6388\u738b\u54f2\u4e3a\u5171\u540c\u7b2c\u4e00\u4f5c\u8005\uff0c\u5357\u6d0b\u7406\u5de5\u5927\u5b66\u9b4f\u78ca\u526f\u6559\u6388\/\u9ad8\u534e\u5065\u9662\u58eb\uff0c\u6df1\u5733\u5148\u8fdb\u9662\u9648\u660e\u526f\u7814\u7a76\u5458\u548c\u82cf\u5dde\u7eb3\u7c73\u5f20\u5176\u51b2\u7814\u7a76\u5458\u4e3a\u5171\u540c\u901a\u8baf\u4f5c\u8005\u3002\u8fd9\u9879\u5de5\u4f5c\u83b7\u5f97\u4e86\u5ba1\u7a3f\u4eba\u7684\u9ad8\u5ea6\u8bc4\u4ef7\uff1a\u201c\u4f5c\u8005\u4eec\u5c55\u793a\u4e86\u4ee4\u4eba\u5370\u8c61\u6df1\u523b\u7684\u4e00\u7cfb\u5217\u5bf9\u4e8e\u5149\u7535\u7ea4\u7ef4\u53ca\u5176\u5e94\u7528\u4e8e\u53ef\u7a7f\u6234\u5668\u4ef6\u7684\u91cd\u8981\u521b\u65b0\u548c\u8fdb\u5c55\u201d\uff08\u201cWang and collaborators presents an impressively broad range of important innovations and advancements in optoelectronic fibres and their development into functional wearable devices\u201d\uff1b\u201c\u91cd\u8981\u4e14\u6253\u7834\u4e86\u4f20\u7edf\u601d\u7ef4\u201d\uff08\u201cimportant and breaks with conventional thinking\u201d\uff09\u4ee5\u53ca\u201c\u8fc7\u53bb\u5341\u5e74\u4e2d\u53ef\u7a7f\u6234\u7535\u5b50\u7a81\u98de\u731b\u8fdb\uff0c\u800c\u8fd9\u9879\u5de5\u4f5c\u662f\u8be5\u9886\u57df\u91cd\u5927\u6210\u5c31\u7684\u4ee3\u8868\u4e4b\u4e00\u201d\uff08\u201cthis field of wearable electronics has grown substantially over the past decade and this work represents one\u00a0of the most important series of multiple contributions\u201d\uff09<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-257617\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/01\/\u56fe\u72471-9.png\" alt=\"\" width=\"744\" height=\"775\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/01\/\u56fe\u72471-9.png 744w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/01\/\u56fe\u72471-9-288x300.png 288w\" sizes=\"(max-width: 744px) 100vw, 744px\" \/>\u00a0<\/p>\n<p>\u56fe1. \u534a\u5bfc\u4f53\u5149\u7535\u7ea4\u7ef4\u7684\u8bbe\u8ba1\u4e0e\u5236\u5907<\/p>\n<p>\u7ea4\u82af\u6750\u6599\u4e2d\u7684\u5e94\u529b\u4e3b\u8981\u662f\u7531\u7ea4\u82af\u548c\u5305\u5c42\u4e4b\u95f4\u7684\u4f53\u79ef\u53d8\u5316\u5dee\u5f02\u5f15\u8d77\u7684\uff0c\u8fd9\u79cd\u5dee\u5f02\u6e90\u81ea\u7ea4\u82af\u51dd\u56fa\u548c\u4e0d\u5339\u914d\u7684\u70ed\u81a8\u80c0\u3002\u7ea4\u82af\u51dd\u56fa\u524d\u7684\u6270\u52a8\u662f\u7531\u6bdb\u7ec6\u7ba1\u4e0d\u7a33\u5b9a\u6027\u5f15\u8d77\u7684\u3002\u8fd9\u4e9b\u673a\u5236\u5f97\u5230\u5efa\u6a21\u548c\u6709\u9650\u5143\u6a21\u62df\u7684\u8fdb\u4e00\u6b65\u652f\u6301\uff0c\u901a\u8fc7\u6750\u6599\u9009\u62e9\u548c\u5de5\u827a\u4f18\u5316\u8fdb\u884c\u5408\u7406\u7684\u529b\u5b66\u8bbe\u8ba1\u53ef\u4ee5\u7f13\u89e3\u548c\u6291\u5236\u6b64\u7c7b\u5e94\u529b\u548c\u4e0d\u7a33\u5b9a\u6027\u3002\u7194\u82af\u6cd5\u7684\u529b\u5b66\u8bbe\u8ba1\u4e3a\u9ad8\u8d28\u91cf\u534a\u5bfc\u4f53\u7ea4\u7ef4\u7684\u53d1\u5c55\u63d0\u4f9b\u4e86\u65b0\u7684\u7814\u7a76\u65b9\u5411\uff0c\u5e76\u6709\u671b\u6269\u5c55\u5230\u66f4\u5e7f\u6cdb\u7684\u6750\u6599\u8303\u56f4\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-257618\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/01\/\u56fe\u72472-9.png\" alt=\"\" width=\"606\" height=\"753\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/01\/\u56fe\u72472-9.png 606w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/01\/\u56fe\u72472-9-241x300.png 241w\" sizes=\"(max-width: 606px) 100vw, 606px\" \/><\/p>\n<p>\u56fe2. \u7194\u82af\u70ed\u62c9\u6cd5\u4e2d\u7684\u5e94\u529b\u548c\u6bdb\u7ec6\u7ba1\u4e0d\u7a33\u5b9a\u6027\u5206\u6790<\/p>\n<p>\u91c7\u7528\u65b0\u5f00\u53d1\u7684\u6536\u655b\u70ed\u62c9\u6cd5\u5c06\u534a\u5bfc\u4f53\u7ea4\u7ef4\u96c6\u6210\u5230\u5177\u6709\u4e0d\u540c\u8bbe\u8ba1\u7684\u5bfc\u4f53\u3001\u534a\u5bfc\u4f53\u548c\u7edd\u7f18\u4f53\u590d\u5408\u7ed3\u6784\u4e2d\uff0c\u7531\u6b64\u83b7\u5f97\u7684\u5149\u7535\u7ea4\u7ef4\u5728 2 V \u504f\u538b\u4e0b\u8868\u73b0\u51fa\u9ad8\u8fbe 0.55 A W<sup>-1<\/sup>\u00a0\u7684\u54cd\u5e94\u5ea6\u548c\u77ed\u81f3 900 ns \u7684\u54cd\u5e94\u65f6\u95f4\uff0c\u4e0e\u5546\u7528\u5e73\u9762\u578b\u5149\u7535\u63a2\u6d4b\u5668\u76f8\u5f53\uff0c\u89e3\u51b3\u4e86\u9ad8\u6027\u80fd\u7684\u65e0\u673a\u534a\u5bfc\u4f53\u6750\u6599\u4e0e\u70ed\u62c9\u6cd5\u5236\u5907\u7ea4\u7ef4\u7684\u517c\u5bb9\u6027\u95ee\u9898\u3002\u66f4\u91cd\u8981\u7684\u662f\uff0c\u8fd9\u4e9b\u7ea4\u7ef4\u7684\u67d4\u8f6f\u8f7b\u4fbf\u548c\u51fa\u8272\u7684\u673a\u68b0\u6027\u80fd\u4f7f\u5176\u7279\u522b\u9002\u5408\u6784\u5efa\u5927\u9762\u79ef\u5149\u7535\u7ec7\u7269\uff0c\u540c\u65f6\u4fdd\u6301\u8f7b\u8d28\u3001\u8212\u9002\u6027\u3001\u53ef\u673a\u6d17\u548c\u900f\u6c14\u6027\u7b49\u6709\u5229\u7279\u6027\u3002\u7814\u7a76\u56e2\u961f\u8fdb\u4e00\u6b65\u5c55\u793a\u4e86\u5149\u7535\u7ec7\u7269\u7684\u5e7f\u6cdb\u5e94\u7528\uff0c\u5305\u62ec\u4e2a\u4eba\u8f85\u52a9\u8bbe\u5907\u3001\u7528\u4e8e\u7ec7\u7269\u95f4\u901a\u4fe1\u7684\u53ef\u7a7f\u6234Li-Fi\u7cfb\u7edf\u3001\u7528\u4e8e\u4e2a\u4eba\u5065\u5eb7\u76d1\u6d4b\u7684\u667a\u80fd\u624b\u8868\u5e26\u4ee5\u53ca\u6c34\u4e0b\u53ef\u89c1\u5149\u901a\u4fe1\u7cfb\u7edf\u3002\u8fd9\u9879\u5de5\u4f5c\u4e3a\u4ece\u4f20\u7edf\u6750\u6599\u548c\u5668\u4ef6\u5f62\u6001\u4e2d\u65e0\u6cd5\u4f01\u53ca\u7684\u6781\u7aef\u529b\u5b66\u548c\u6d41\u4f53\u52a8\u529b\u5b66\u63d0\u4f9b\u4e86\u65b0\u7684\u89c1\u89e3\uff0c\u6709\u671b\u4fc3\u8fdb\u89e3\u51b3\u5bf9\u9ad8\u6027\u80fd\u67d4\u6027\u534a\u5bfc\u4f53\u6750\u6599\u548c\u53ef\u7a7f\u6234\u7535\u5b50\u5668\u4ef6\u65e5\u76ca\u589e\u957f\u7684\u9700\u6c42\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-257619\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/01\/\u56fe\u72473-7.png\" alt=\"\" width=\"813\" height=\"655\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/01\/\u56fe\u72473-7.png 813w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/01\/\u56fe\u72473-7-300x242.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/01\/\u56fe\u72473-7-768x619.png 768w\" sizes=\"(max-width: 813px) 100vw, 813px\" \/><\/p>\n<p>\u56fe3. \u5149\u7535\u7ea4\u7ef4\u548c\u5927\u9762\u79ef\u5149\u7535\u7ec7\u7269<\/p>\n<p>\u534a\u5bfc\u4f53\u662f\u51b3\u5b9a\u7535\u5b50\u5668\u4ef6\u6027\u80fd\u7684\u5173\u952e\u6750\u6599\uff0c\u9ad8\u8d28\u91cf\u7684\u534a\u5bfc\u4f53\u7ea4\u7ef4\u53ef\u80fd\u4f1a\u4f7f\u5177\u6709\u4f20\u611f\u3001\u6570\u636e\u50a8\u5b58\uff0c\u751a\u81f3\u662f\u96c6\u6210\u7535\u8def\u548c\u5fae\u5904\u7406\u5668\u7b49\u529f\u80fd\u7684\u7ea4\u7ef4\u5668\u4ef6\u5feb\u901f\u53d1\u5c55\uff0c\u4ece\u800c\u63d0\u4f9b\u5177\u6709\u7ecf\u6d4e\u548c\u793e\u4f1a\u6548\u76ca\u7684\u521b\u65b0\u3002\u9ad8\u8d28\u91cf\u534a\u5bfc\u4f53\u7ea4\u7ef4\u7684\u89c4\u6a21\u5316\u751f\u4ea7\u5df2\u7ecf\u5b9e\u73b0\u7a81\u7834\uff0c\u4f46\u8981\u5b9e\u73b0\u5e7f\u6cdb\u7684\u5e94\u7528\uff0c\u8fd8\u9762\u4e34\u4e00\u4e9b\u673a\u9047\u548c\u6311\u6218\u3002\u4ece\u7ea4\u7ef4\u5f62\u6001\u51fa\u53d1\uff0c\u76ee\u524d\u7684\u5f62\u72b6\u5355\u4e00\uff0c\u800c\u4e0d\u540c\u7684\u5668\u4ef6\u53ef\u80fd\u8981\u6c42\u4e0d\u540c\u5f62\u72b6\u6216\u662f\u5177\u6709\u5185\u90e8\u7ed3\u6784\u7684\u7ea4\u7ef4\uff1b\u4ece\u6750\u6599\u6765\u8bf4\uff0c\u4e5f\u9700\u8981\u63a2\u7d22\u7b2c\u4e09\u4ee3\u53ca\u7b2c\u56db\u4ee3\u534a\u5bfc\u4f53\u6750\u6599\u7684\u7ea4\u7ef4\u5316\u5236\u5907\u3002\u81f4\u529b\u4e8e\u591a\u529f\u80fd\u7ea4\u7ef4\u7684\u53d1\u5c55\uff0c\u5171\u540c\u89e3\u51b3\u751f\u4ea7\u5236\u5907\u8fc7\u7a0b\u4e2d\u91cd\u5927\u96be\u9898\uff0c\u4ece\u800c\u53d1\u6325\u529f\u80fd\u7ea4\u7ef4\u5de8\u5927\u7684\u5e94\u7528\u6f5c\u529b\u3002<\/p>\n<p>\u8bba\u6587\u94fe\u63a5\uff1a\u00a0https:\/\/www.nature.com\/articles\/s41586-023-06946-0<\/p>\n<p>&nbsp;<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4ee5\u7845\u9517\u4e3a\u4ee3\u8868\u7684\u534a\u5bfc\u4f53\u662f\u73b0\u4ee3\u7535\u5b50\u4ea7\u4e1a\u7684\u201c\u5927\u8111\u201d\u2014\u82af\u7247\u4e0d\u53ef\u6216\u7f3a\u7684\u5173\u952e\u6750\u6599\u3002\u8fd9\u4e9b\u65e0\u673a\u534a\u5bfc\u4f53\u5728\u5316\u5b66\u53ca\u70ed\u7a33\u5b9a\u6027\uff0c\u7535\u5b66\u6027\u80fd\uff0c\u89c4\u6a21\u5316\u751f\u4ea7\u7b49\u65b9\u9762\u5177\u6709\u4e0d\u53ef\u6bd4\u62df\u7684\u4f18\u52bf\u3002\u7136\u800c\u5728\u7535\u5b50\u4ea7&#8230;<\/p>\n","protected":false},"author":14360,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-257616","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/257616"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/14360"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=257616"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/257616\/revisions"}],"predecessor-version":[{"id":257620,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/257616\/revisions\/257620"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=257616"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=257616"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=257616"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}