{"id":261041,"date":"2024-07-02T06:45:56","date_gmt":"2024-07-01T22:45:56","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=261041"},"modified":"2024-07-01T21:46:12","modified_gmt":"2024-07-01T13:46:12","slug":"%e6%9c%80%e6%96%b0nature%ef%bc%9a%e5%8f%8c%e9%97%a8%e6%8e%a7%e7%9f%b3%e5%a2%a8%e7%83%af%e4%b8%ad%e8%b4%a8%e5%ad%90%e4%bc%a0%e8%be%93%e5%92%8c%e6%b0%a2%e5%8c%96%e7%9a%84%e7%b2%be%e7%a1%ae%e6%8e%a7","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=261041","title":{"rendered":"\u6700\u65b0Nature\uff1a\u53cc\u95e8\u63a7\u77f3\u58a8\u70ef\u4e2d\u8d28\u5b50\u4f20\u8f93\u548c\u6c22\u5316\u7684\u7cbe\u786e\u63a7\u5236"},"content":{"rendered":"<p><strong>\u4e00\u3001\u3010\u79d1\u5b66\u80cc\u666f\u3011<\/strong><\/p>\n<p>\u77f3\u58a8\u70ef\u5728\u73af\u5883\u6761\u4ef6\u4e0b\u6240\u6709\u539f\u5b50\u548c\u5206\u5b50\u90fd\u662f\u65e0\u6cd5\u6e17\u900f\u7684\uff0c\u4f46\u70ed\u8d28\u5b50\u5728\u5782\u76f4\u4e8e\u5176\u57fa\u9762\u65b9\u5411\u4e0a\u662f\u53ef\u6e17\u900f\u7684\u3002\u4e4b\u524d\u7684\u7814\u7a76\u8ba4\u4e3a\u9700\u8981\u6676\u683c\u4e2d\u7684\u9488\u5b54\u624d\u80fd\u5b9e\u73b0\u8d28\u5b50\u4f20\u8f93\uff0c\u4f46\u6700\u65b0\u7814\u7a76\u8868\u660e\uff0c\u539f\u59cb\u6676\u683c\u5bf9\u8d28\u5b50\u662f\u53ef\u6e17\u900f\u7684\uff0c\u800c\u6676\u683c\u4e2d\u7684\u5e94\u53d8\u7b49\u7f3a\u9677\u4f1a\u964d\u4f4e\u4f20\u8f93\u7684\u80fd\u5792\u3002\u8d28\u5b50\u53ef\u4ee5\u5316\u5b66\u5438\u9644\u5728\u77f3\u58a8\u70ef\u4e0a\u5e76\u5bf9\u5176\u8fdb\u884c\u6c22\u5316\uff0c\u8fd9\u4e2a\u8fc7\u7a0b\u4f1a\u5bfc\u81f4\u77f3\u58a8\u70ef\u7684\u5bfc\u4f53-\u7edd\u7f18\u4f53\u8f6c\u53d8\u3002\u8d28\u5b50\u4f20\u8f93\u4e0e\u77f3\u58a8\u70ef\u6c22\u5316\u8fc7\u7a0b\u662f\u4e24\u4e2a\u590d\u6742\u7684\u76f8\u5173\u8054\u7684\u7535\u5316\u5b66\u8fc7\u7a0b\u3002\u5e38\u7528\u7684\u6539\u6027\u65b9\u6cd5\u53ef\u4ee5\u52a0\u901f\u8d28\u5b50\u4f20\u8f93\uff0c\u4f46\u662f\u4f1a\u5bf9\u77f3\u58a8\u70ef\u7684\u5176\u4ed6\u6027\u8d28\u4ea7\u751f\u5f71\u54cd\u3002\u56e0\u6b64\uff0c\u5982\u4f55\u5728\u4e0d\u5f71\u54cd\u5176\u4ed6\u6027\u8d28\u7684\u60c5\u51b5\u4e0b\u63a7\u5236\u6c22\u5316\u8fc7\u7a0b\uff0c\u4ee5\u53ca\u907f\u514d\u6c22\u5316\u5bf9\u77f3\u58a8\u70ef\u6027\u80fd\u7684\u8d1f\u9762\u5f71\u54cd\u4e5f\u662f\u4e00\u4e2a\u5173\u952e\u95ee\u9898\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261049\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/0-9.png\" alt=\"\" width=\"986\" height=\"514\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/0-9.png 986w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/0-9-300x156.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/0-9-768x400.png 768w\" sizes=\"(max-width: 986px) 100vw, 986px\" \/><br \/>\n <strong>\u4e8c\u3001\u3010\u521b\u65b0\u6210\u679c\u3011<\/strong><\/p>\n<p>\u4e3a\u4e86\u89e3\u51b3\u8fd9\u4e00\u95ee\u9898\uff0c<strong>\u82f1\u56fd\u66fc\u5f7b\u65af\u7279\u5927\u5b66<\/strong>\u7684<strong>M. Lozada-Hidalgo<\/strong>\u6559\u6388\u548c<strong>J. Tong<\/strong>\u535a\u58eb\u5728\u7535\u89e3\u8d28\u53cc\u95e8\u63a7\u77f3\u58a8\u70ef\u5668\u4ef6\u4e2d\u901a\u8fc7\u72ec\u7acb\u63a7\u5236\u7535\u573a\u548c\u8f7d\u6d41\u5b50\u5bc6\u5ea6\uff0c\u5b9e\u73b0\u5bf9\u8d28\u5b50\u4f20\u8f93\u548c\u6c22\u5316\u8fc7\u7a0b\u7684\u7cbe\u786e\u63a7\u5236\uff0c\u4ece\u800c\u52a0\u901f\u8d28\u5b50\u4f20\u8f93\u5e76\u5b9e\u73b0\u5bf9\u8fd9\u4e9b\u8fc7\u7a0b\u7684\u9009\u62e9\u6027\u9a71\u52a8\u3002\u8fd9\u4e3a\u57fa\u4e8e\u8d28\u5b50\u7684\u903b\u8f91\u548c\u5b58\u50a8\u77f3\u58a8\u70ef\u5668\u4ef6\u63d0\u4f9b\u4e86\u53ef\u80fd\u6027\u3002\u9996\u6b21\u540c\u65f6\u5b9e\u73b0\u4e86\u903b\u8f91\u8fd0\u7b97\u4e0e\u8bb0\u5fc6\u5b58\u50a8\u8fd9\u4e24\u4e2a\u8ba1\u7b97\u673a\u7684\u57fa\u672c\u529f\u80fd\uff0c\u4e3a\u57fa\u4e8e\u77f3\u58a8\u70ef\u7684\u5668\u4ef6\u5f00\u53d1\u4e0e\u5e94\u7528\u63d0\u4f9b\u4e86\u65b0\u7684\u65b9\u5411\u3002\u76f8\u5173\u6210\u679c\u201c<strong>Control of proton transport and hydrogenation in double-gated graphene<\/strong>\u201d\u53d1\u8868\u5728<strong>Nature<\/strong>\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261051\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/1-13.png\" alt=\"\" width=\"1269\" height=\"628\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/1-13.png 1269w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/1-13-300x148.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/1-13-768x380.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/1-13-1024x507.png 1024w\" sizes=\"(max-width: 1269px) 100vw, 1269px\" \/> <img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261052\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/1-14.png\" alt=\"\" width=\"1269\" height=\"628\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/1-14.png 1269w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/1-14-300x148.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/1-14-768x380.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/1-14-1024x507.png 1024w\" sizes=\"(max-width: 1269px) 100vw, 1269px\" \/><\/p>\n<p><strong>\u56fe1\u53cc\u95e8\u63a7\u77f3\u58a8\u70ef\u5668\u4ef6\u4e2d\u7684\u8d28\u5b50\u4f20\u8f93\u548c\u6c22\u5316\u7684\u9009\u62e9\u6027\u63a7\u5236 \u00a9 2024 Springer Nature Limited<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261053\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/2-13.png\" alt=\"\" width=\"1386\" height=\"1519\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/2-13.png 1386w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/2-13-274x300.png 274w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/2-13-768x842.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/2-13-934x1024.png 934w\" sizes=\"(max-width: 1386px) 100vw, 1386px\" \/><\/p>\n<p><strong>\u56fe2\u53cc\u95e8\u63a7\u77f3\u58a8\u70ef\u4e2d\u72ec\u7acb\u63a7\u5236\u7535\u573aE\u548c\u7535\u8377\u5bc6\u5ea6n\u5bf9\u8d28\u5b50\u548c\u7535\u5b50\u8f93\u8fd0\u7684\u5f71\u54cd \u00a9 2024 Springer Nature Limited<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261054\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/3-14.png\" alt=\"\" width=\"1413\" height=\"1759\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/3-14.png 1413w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/3-14-241x300.png 241w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/3-14-768x956.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/3-14-823x1024.png 823w\" sizes=\"(max-width: 1413px) 100vw, 1413px\" \/><\/p>\n<p><strong>\u56fe3\u53cc\u95e8\u63a7\u77f3\u58a8\u70ef\u4e2d\u8d28\u5b50\u4f20\u8f93\u548c\u6c22\u5316\u7684\u7a33\u5065\u800c\u7cbe\u786e\u7684\u5207\u6362\uff0c\u5b9e\u73b0\u4e86\u57fa\u4e8e\u8d28\u5b50\u7684\u903b\u8f91\u548c\u5b58\u50a8\u5668\u4ef6 \u00a9 2024 Springer Nature Limited<\/strong><\/p>\n<p><strong>\u4e09\u3001\u3010\u79d1\u5b66\u542f\u8fea\u3011<\/strong><\/p>\n<p>\u5728\u8fd9\u9879\u5de5\u4f5c\u4e2d\uff0c\u53cc\u95e8\u63a7\u77f3\u58a8\u70ef\u5668\u4ef6\u901a\u8fc7\u5bf9E\u548cn\u7684\u72ec\u7acb\u63a7\u5236\u5b9e\u73b0\u4e86\u7cbe\u786e\u7684\u8d28\u5b50\u8f93\u8fd0\u548c\u6c22\u5316\u63a7\u5236\u3002\u5728\u53cc\u95e8\u63a7\u77f3\u58a8\u70ef\u4e2d\uff0c\u8d28\u5b50\u7535\u6d41\u53ef\u4ee5\u7528\u4e8e\u6267\u884c\u903b\u8f91\u64cd\u4f5c\uff0c\u4e3a\u4e8c\u7ef4\u7535\u5316\u5b66\u6750\u6599\u7684\u7814\u7a76\u63d0\u4f9b\u4e86\u65b0\u7684\u65b9\u6cd5\u548c\u601d\u8def\u3002\u8fd9\u9879\u5de5\u4f5c\u62a5\u544a\u7684\u8d28\u5b50\u8f93\u8fd0\u548c\u6c22\u5316\u7684\u9009\u62e9\u6027\u52a0\u901f\u8868\u660e\uff0c\u7c7b\u4f3c\u7684\u4e8c\u7ef4\u6676\u4f53\u5668\u4ef6\u53ef\u80fd\u6709\u9009\u62e9\u6027\u5730\u9a71\u52a8\u5176\u4ed6\u8026\u5408\u7684\u754c\u9762\u8fc7\u7a0b\u3002\u4ece\u6839\u672c\u4e0a\u8bb2\uff0c\u8fd9\u9879\u5de5\u4f5c\u6269\u5c55\u4e86\u7814\u7a76\u4e8c\u7ef4\u6676\u4f53\u4e2d\u7535\u5316\u5b66\u8fc7\u7a0b\u7684\u53c2\u6570\u7a7a\u95f4\u3002<\/p>\n<p>\u539f\u6587\u8be6\u60c5\uff1aTong, J., Fu, Y., Domaretskiy, D. et al. Control of proton transport and hydrogenation in double-gated graphene. Nature 630, 619\u2013624 (2024).<\/p>\n<p>https:\/\/doi.org\/10.1038\/s41586-024-07435-8<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4e00\u3001\u3010\u79d1\u5b66\u80cc\u666f\u3011 \u77f3\u58a8\u70ef\u5728\u73af\u5883\u6761\u4ef6\u4e0b\u6240\u6709\u539f\u5b50\u548c\u5206\u5b50\u90fd\u662f\u65e0\u6cd5\u6e17\u900f\u7684\uff0c\u4f46\u70ed\u8d28\u5b50\u5728\u5782\u76f4\u4e8e\u5176\u57fa\u9762\u65b9\u5411\u4e0a\u662f\u53ef\u6e17\u900f\u7684\u3002\u4e4b\u524d\u7684\u7814\u7a76\u8ba4\u4e3a\u9700\u8981\u6676\u683c\u4e2d\u7684\u9488\u5b54\u624d\u80fd\u5b9e\u73b0\u8d28\u5b50\u4f20\u8f93\uff0c\u4f46\u6700\u65b0&#8230;<\/p>\n","protected":false},"author":36633,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-261041","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/261041"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/36633"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=261041"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/261041\/revisions"}],"predecessor-version":[{"id":261056,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/261041\/revisions\/261056"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=261041"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=261041"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=261041"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}