{"id":261074,"date":"2024-06-27T07:28:18","date_gmt":"2024-06-26T23:28:18","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=261074"},"modified":"2024-06-26T22:29:58","modified_gmt":"2024-06-26T14:29:58","slug":"%e6%ad%a6%e5%a4%b7%e5%ad%a6%e9%99%a2%e9%97%bd%e6%b1%9f%e5%ad%a6%e9%99%a2%e4%b8%ad%e5%9b%bd%e7%a7%91%e5%ad%a6%e9%99%a2%e7%a6%8f%e5%bb%ba%e7%89%a9%e8%b4%a8%e7%bb%93%e6%9e%84%e7%a0%94%e7%a9%b6%e6%89%80","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=261074","title":{"rendered":"\u6b66\u5937\u5b66\u9662&#038;\u95fd\u6c5f\u5b66\u9662&#038;\u4e2d\u56fd\u79d1\u5b66\u9662\u798f\u5efa\u7269\u8d28\u7ed3\u6784\u7814\u7a76\u6240&#038;\u5bbe\u5915\u6cd5\u5c3c\u4e9a\u5dde\u7acb\u5927\u5b66\uff1aACS Sensors"},"content":{"rendered":"<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-261075 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/\u56fe\u72471-17.png\" alt=\"\" width=\"1184\" height=\"464\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/\u56fe\u72471-17.png 1184w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/\u56fe\u72471-17-300x118.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/\u56fe\u72471-17-768x301.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/\u56fe\u72471-17-1024x401.png 1024w\" sizes=\"(max-width: 1184px) 100vw, 1184px\" \/> \u00a0<\/p>\n<p>\u76ae\u80a4\u63a5\u89e6\u5f0f\u53ef\u7a7f\u6234\u4f20\u611f\u5668\u53ef\u4ee5\u8fde\u7eed\u76d1\u6d4b\u5404\u79cd\u751f\u7269\u7269\u7406\u548c\u751f\u7269\u5316\u5b66\u4fe1\u53f7\uff0c\u4ee5\u8fdb\u884c\u5065\u5eb7\u76d1\u6d4b\u548c\u75be\u75c5\u8bca\u65ad\u3002\u7136\u800c\uff0c\u8fd9\u7c7b\u8bbe\u5907\u901a\u5e38\u53d7\u9650\u4e8e\u5728\u673a\u68b0\u53d8\u5f62\u548c\u4eba\u4f53\u8fd0\u52a8\u4e0b\u7535\u6e90\u8f93\u51fa\u6027\u80fd\u4e0d\u4f73\u548c\u4e0d\u7a33\u5b9a\u3002\u6b64\u5916\uff0c\u8fd8\u7f3a\u4e4f\u4e00\u79cd\u7b80\u5355\u4e14\u6210\u672c\u6548\u76ca\u9ad8\u7684\u5236\u9020\u6280\u672f\u6765\u5728\u8bbe\u5907\u7cfb\u7edf\u4e2d\u5236\u9020\u548c\u96c6\u6210\u4e0d\u540c\u6750\u6599\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-261076 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/\u56fe\u72472-15.png\" alt=\"\" width=\"972\" height=\"407\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/\u56fe\u72472-15.png 972w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/\u56fe\u72472-15-300x126.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/\u56fe\u72472-15-768x322.png 768w\" sizes=\"(max-width: 972px) 100vw, 972px\" \/><\/p>\n<p>\u56fe1. \u81ea\u5145\u7535\u53ef\u7a7f\u6234\u4f20\u611f\u7cfb\u7edf\u793a\u610f\u56fe\u53ca\u8fd0\u52a8\u548c\u5fc3\u7387\u76d1\u6d4b\u793a\u610f\u56fe<\/p>\n<p>&nbsp;<\/p>\n<p>\u9274\u4e8e\u6b64\uff0c\u6b66\u5937\u5b66\u9662\/\u4e2d\u56fd\u79d1\u5b66\u9662\u798f\u5efa\u7269\u8d28\u7ed3\u6784\u7814\u7a76\u6240\u7684\u4e01\u6653\u7ea2\u535a\u58eb\u540e\u3001\u95fd\u6c5f\u5b66\u9662\u7684\u5f20\u8bda\u7814\u7a76\u5458\u3001\u5bbe\u5915\u6cd5\u5c3c\u4e9a\u5dde\u7acb\u5927\u5b66\u7684\u7a0b\u5bf0\u5b87\u6559\u6388\u548c\u4e2d\u56fd\u79d1\u5b66\u9662\u798f\u5efa\u7269\u8d28\u7ed3\u6784\u7814\u7a76\u6240\u5434\u7acb\u65b0\u7814\u7a76\u5458\u7b49\u8054\u5408\u62a5\u9053\u4e86\u4e00\u79cd\u5b8c\u5168\u96c6\u6210\u7684\u72ec\u7acb\u53ef\u62c9\u4f38\u751f\u7269\u7269\u7406\u4f20\u611f\u7cfb\u7edf\u3002\u8be5\u7cfb\u7edf\u7ed3\u5408\u4e86\u53ef\u7a7f\u6234\u751f\u7269\u7269\u7406\u4f20\u611f\u5668\u3001\u6469\u64e6\u7535\u7eb3\u7c73\u53d1\u7535\u673a\uff08TENG\uff09\u3001\u5fae\u578b\u8d85\u7ea7\u7535\u5bb9\u5668\u9635\u5217\uff08MSCA\uff09\u3001\u7535\u6e90\u7ba1\u7406\u7535\u8def\u548c\u65e0\u7ebf\u4f20\u8f93\u6a21\u5757\u3002<\/p>\n<p>\u5728\u6750\u6599\u8bbe\u8ba1\u4e2d\uff0c\u6240\u6709\u57fa\u4e8e3D\u7f51\u7edc\u77f3\u58a8\u70ef\/Co<sub>3<\/sub>O<sub>4<\/sub>\u7eb3\u7c73\u590d\u5408\u6750\u6599\u7684\u8bbe\u5907\u7ec4\u4ef6\u548c\u8fde\u63a5\u90fd\u662f\u901a\u8fc7\u4f4e\u6210\u672c\u548c\u53ef\u6269\u5c55\u7684\u76f4\u63a5\u6fc0\u5149\u5199\u5165\u6280\u672f\u5236\u9020\u7684\u3002\u81ea\u5145\u7535\u7535\u6e90\u5355\u5143\u53ef\u4ee5\u6709\u6548\u5730\u5c06\u8eab\u4f53\u8fd0\u52a8\u7684\u80fd\u91cf\u8f6c\u5316\u4e3a\u7a33\u5b9a\u548c\u53ef\u8c03\u7684\u7535\u538b\/\u7535\u6d41\u8f93\u51fa\uff0c\u4ee5\u9a71\u52a8\u5404\u79cd\u751f\u7269\u7269\u7406\u4f20\u611f\u5668\u548c\u65e0\u7ebf\u4f20\u8f93\u6a21\u5757\uff0c\u4ece\u800c\u8fde\u7eed\u6355\u83b7\u3001\u5904\u7406\u548c\u5b9e\u65f6\u65e0\u7ebf\u4f20\u8f93\u5404\u79cd\u4fe1\u53f7\u3002\u65b0\u9896\u7684\u6750\u6599\u6539\u6027\u3001\u8bbe\u5907\u914d\u7f6e\u548c\u7cfb\u7edf\u96c6\u6210\u7b56\u7565\u4e3a\u4e0b\u4e00\u4ee3\u72ec\u7acb\u53ef\u62c9\u4f38\u4f20\u611f\u7cfb\u7edf\u5728\u5065\u5eb7\u76d1\u6d4b\u548c\u4eba\u673a\u754c\u9762\u4e2d\u7684\u8bbe\u8ba1\u548c\u5e94\u7528\u63d0\u4f9b\u4e86\u4e00\u6761\u5feb\u901f\u4e14\u53ef\u6269\u5c55\u7684\u9014\u5f84\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-261077 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/\u56fe\u72473-14.png\" alt=\"\" width=\"1269\" height=\"906\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/\u56fe\u72473-14.png 1269w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/\u56fe\u72473-14-300x214.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/\u56fe\u72473-14-768x548.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/06\/\u56fe\u72473-14-1024x731.png 1024w\" sizes=\"(max-width: 1269px) 100vw, 1269px\" \/><\/p>\n<p>\u56fe2. \u7528\u4e8e\u65e0\u521b\u548c\u6301\u7eed\u5065\u5eb7\u76d1\u6d4b\u7684\u5168\u96c6\u6210\u72ec\u7acb\u751f\u7269\u7269\u7406\u4f20\u611f\u7cfb\u7edf\u7684\u8d34\u8eab\u8bc4\u4f30\u3002<\/p>\n<p>&nbsp;<\/p>\n<p>\u8be5\u6210\u679c\u4ee5\u300aStandalone stretchable biophysical sensing system based on\u00a0laser direct write of patterned porous graphene\/Co<sub>3<\/sub>O<sub>4<\/sub>\u00a0nanocomposites\u300b\u4e3a\u9898\u53d1\u8868\u4e8e\u7f8e\u56fd\u5316\u5b66\u5b66\u4f1a\u65d7\u4e0b\u5b66\u672f\u671f\u520aACS Sensors\uff0cDOI:10.1021\/acssensors.4c00916\u00a0(\u4e2d\u79d1\u96621\u533atop, IF=8.9)\u3002<\/p>\n<p>\u8fd9\u9879\u5de5\u4f5c\u5f97\u5230\u4e86\u4e2d\u56fd\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\uff0852002162\uff0c12174172\uff09\u3001\u798f\u5efa\u7701\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\uff082021J011040\uff0c2021J05249\uff0c2023J011396\uff09\u3001\u6b66\u5937\u5b66\u9662\u5f15\u8fdb\u4eba\u624d\u79d1\u7814\u542f\u52a8\u57fa\u91d1\uff08YJ202101\uff09\uff0c\u798f\u5dde\u79d1\u6280\u9879\u76ee\uff082021-SG-273\uff09\uff0c\u7f8e\u56fd\u56fd\u7acb\u536b\u751f\u7814\u7a76\u9662\uff08R21EB030140\uff09\u3001\u7f8e\u56fd\u56fd\u5bb6\u79d1\u5b66\u57fa\u91d1\u4f1a\uff08NSF\uff09\uff082309323\uff0c2243979\uff0c2319139\uff0c2222654\uff09\u4ee5\u53ca\u5bbe\u5915\u6cd5\u5c3c\u4e9a\u5dde\u7acb\u5927\u5b66\u7684\u652f\u6301\u3002<\/p>\n<p>\u8bba\u6587\u94fe\u63a5\uff1ahttps:\/\/pubs.acs.org\/doi\/10.1021\/acssensors.4c00916<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u00a0 \u76ae\u80a4\u63a5\u89e6\u5f0f\u53ef\u7a7f\u6234\u4f20\u611f\u5668\u53ef\u4ee5\u8fde\u7eed\u76d1\u6d4b\u5404\u79cd\u751f\u7269\u7269\u7406\u548c\u751f\u7269\u5316\u5b66\u4fe1\u53f7\uff0c\u4ee5\u8fdb\u884c\u5065\u5eb7\u76d1\u6d4b\u548c\u75be\u75c5\u8bca\u65ad\u3002\u7136\u800c\uff0c\u8fd9\u7c7b\u8bbe\u5907\u901a\u5e38\u53d7\u9650\u4e8e\u5728\u673a\u68b0\u53d8\u5f62\u548c\u4eba\u4f53\u8fd0\u52a8\u4e0b\u7535\u6e90\u8f93\u51fa\u6027\u80fd\u4e0d\u4f73\u548c\u4e0d\u7a33&#8230;<\/p>\n","protected":false},"author":14360,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-261074","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/261074"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/14360"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=261074"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/261074\/revisions"}],"predecessor-version":[{"id":261078,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/261074\/revisions\/261078"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=261074"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=261074"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=261074"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}