{"id":261263,"date":"2024-07-06T06:25:02","date_gmt":"2024-07-05T22:25:02","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=261263"},"modified":"2024-07-05T21:38:23","modified_gmt":"2024-07-05T13:38:23","slug":"%e6%b1%9f%e8%8b%8f%e7%a7%91%e6%8a%80%e5%a4%a7%e5%ad%a6%e9%83%ad%e5%b3%b0-%e6%96%bd%e4%bc%9f%e9%be%99%e5%9b%a2%e9%98%9ffuel%ef%bc%9a%e7%a3%81%e5%9c%ba%e8%af%b1%e5%af%bc%e6%b4%bb%e5%8c%96%e5%85%b7","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=261263","title":{"rendered":"\u6c5f\u82cf\u79d1\u6280\u5927\u5b66\u90ed\u5cf0\/\u65bd\u4f1f\u9f99\u56e2\u961fFuel\uff1a\u78c1\u573a\u8bf1\u5bfc\u6d3b\u5316\u5177\u6709\u6838\u58f3\u7ed3\u6784\u7684S\u578b\u5f02\u8d28\u7ed3\u4fc3\u8fdb\u5149\u70ed\u8f85\u52a9-\u5149\u50ac\u5316\u5236\u6c22"},"content":{"rendered":"<p><strong>01<\/strong><strong>\u3001\u3010\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p>\u957f\u671f\u4ee5\u6765\uff0c\u4eba\u7c7b\u793e\u4f1a\u7684\u52a8\u6001\u53d1\u5c55\u4e00\u76f4\u4f9d\u8d56\u4e8e\u4f20\u7edf\u7684\u3001\u4e0d\u53ef\u518d\u751f\u7684\u5316\u77f3\u71c3\u6599\u3002\u7136\u800c\uff0c\u5316\u77f3\u71c3\u6599\u7684\u7316\u7357\u6d88\u8d39\u52a0\u5267\u4e86\u80fd\u6e90\u77ed\u7f3a\u548c\u73af\u5883\u6c61\u67d3\uff0c\u8feb\u5207\u9700\u8981\u5f00\u53d1\u7eff\u8272\u548c\u66f4\u65b0\u80fd\u6e90\u3002\u6c22\u6c14\u662f\u4e00\u79cd\u53ef\u518d\u751f\u7684\u9ad8\u5bc6\u5ea6\u6e05\u6d01\u71c3\u6599\uff0c\u53ef\u4f5c\u4e3a\u4f20\u7edf\u5316\u77f3\u71c3\u6599\u7684\u66ff\u4ee3\u54c1\u3002\u5728\u5404\u79cd\u5236\u6c22\u9014\u5f84\u4e2d\uff0c\u592a\u9633\u80fd\u9a71\u52a8\u7684\u5149\u50ac\u5316\u6c34\u88c2\u89e3\u4f5c\u4e3a\u4e00\u79cd\u516c\u8ba4\u7684\u7f13\u89e3\u8fd9\u4e00\u5371\u673a\u7684\u6709\u6548\u7b56\u7565\u800c\u53d7\u5230\u5e7f\u6cdb\u5173\u6ce8\u3002\u4ece\u6839\u672c\u4e0a\u8bf4\uff0c\u8be5\u8fc7\u7a0b\u7684\u6709\u6548\u6027\u53d6\u51b3\u4e8e\u8bbe\u8ba1\u826f\u597d\u7684\u5149\u50ac\u5316\u5242\u3002\u4e0d\u5e78\u7684\u662f\uff0c\u73b0\u6709\u7684\u534a\u5bfc\u4f53\u5149\u50ac\u5316\u5242\u5bf9\u9633\u5149\u7684\u5438\u6536\u80fd\u529b\u5dee\uff0c\u5bb9\u6613\u4e0e\u5149\u751f\u6210\u7684\u8f7d\u6d41\u5b50\u7edc\u5408\uff0c\u6c27\u5316\u8fd8\u539f\u80fd\u529b\u6709\u9650\uff0c\u5e26\u4f4d\u4e0d\u8db3\uff0c\u963b\u788d\u4e86\u5176\u5149\u50ac\u5316\u5e94\u7528\u3002\u56e0\u6b64\uff0c\u8bbe\u8ba1\u9ad8\u6548\u3001\u7a33\u5b9a\u7684\u5149\u50ac\u5316\u5242\u662f\u7814\u7a76\u4eba\u5458\u5de5\u4f5c\u7684\u65b9\u5411\uff0c\u4e5f\u662f\u8be5\u9886\u57df\u9762\u4e34\u7684\u91cd\u8981\u6311\u6218\u3002<\/p>\n<p>\u5149\u70ed\u6548\u5e94\u80fd\u591f\u663e\u8457\u63d0\u9ad8\u8f90\u7167\u671f\u95f4\u7684\u5c40\u90e8\u6e29\u5ea6\uff0c\u4f46\u5728\u4f20\u7edf\u7684\u5149\u50ac\u5316\u4f53\u7cfb\u4e2d\uff0c\u5149\u70ed\u6548\u5e94\u5f80\u5f80\u88ab\u5ffd\u7565\u3002\u5927\u91cf\u7814\u7a76\u5df2\u7ecf\u8bc1\u5b9e\u4e86\u5149\u50ac\u5316\u8fc7\u7a0b\u4e2d\u7684\u5149\u70ed\u6548\u5e94\u4fc3\u8fdb\u4e86\u5149\u751f\u6210\u8f7d\u4f53\u7684\u5206\u79bb\uff0c\u4ece\u800c\u4f18\u5316\u4e86\u6c27\u5316\u8fd8\u539f\u53cd\u5e94\uff0c\u4ece\u800c\u63d0\u9ad8\u4e86\u5149\u50ac\u5316\u6d3b\u6027\u3002\u9664\u4e86\u4f9d\u8d56\u4e8e\u5149\u50ac\u5316\u53cd\u5e94\u672c\u8eab\u7684\u5149\u70ed\u9a71\u52a8\u529b\u5916\uff0c\u5916\u573a\u7684\u5f15\u5165\u8fd8\u53ef\u4ee5\u4e3a\u5149\u50ac\u5316\u7cfb\u7edf\u63d0\u4f9b\u989d\u5916\u7684\u80fd\u91cf\uff0c\u4ece\u800c\u63d0\u9ad8\u5149\u50ac\u5316\u7cfb\u7edf\u7684\u6574\u4f53\u6548\u7387\u3002\u6b64\u5916\uff0c\u901a\u8fc7\u5f15\u5165\u78c1\u573a\uff0c\u53ef\u4ee5\u5229\u7528\u7531\u7535\u8377\u7684\u76f8\u5bf9\u8fd0\u52a8\u800c\u4ea7\u751f\u7684\u6d1b\u4f26\u5179\u529b\uff0c\u8fdb\u4e00\u6b65\u5bfc\u81f4\u7535\u8377\u8fd0\u52a8\u7684\u504f\u5dee\u3002\u5927\u91cf\u7814\u7a76\u8868\u660e\uff0c\u5916\u90e8\u78c1\u573a\u4ea7\u751f\u7684\u6d1b\u4f26\u5179\u529b\u53ef\u4ee5\u9a71\u52a8\u53cd\u5e94\u7269\u5728\u5149\u50ac\u5316\u5242\u4e0a\u7684\u8868\u9762\u5438\u9644\u8d85\u8fc7\u7c92\u5b50\u5185\u6269\u6563\u6240\u65bd\u52a0\u7684\u5438\u9644\u6781\u9650\uff0c\u4fc3\u8fdb\u5149\u8bf1\u5bfc\u7535\u5b50\u548c\u7a7a\u7a74\u5411\u76f8\u53cd\u65b9\u5411\u8fc1\u79fb\uff0c\u6291\u5236\u5149\u751f\u8f7d\u6d41\u5b50\u7684\u91cd\u7ec4\uff0c\u4f7f\u66f4\u591a\u7684\u6d3b\u6027\u7535\u8377\u53c2\u4e0e\u5149\u50ac\u5316\u53cd\u5e94\uff0c\u5e76\u53ef\u4ee5\u901a\u8fc7\u591a\u573a\u8026\u5408\u89e3\u51b3\u5355\u4e00\u5149\u70ed\u573a\u7684\u5c40\u9650\u3002\u4ece\u8fd9\u4e2a\u89d2\u5ea6\u6765\u770b\uff0c\u7ed3\u5408\u78c1\u573a\u8bf1\u5bfc\u5149\u70ed\u5206\u6790\u7684\u5149\u50ac\u5316\u5236\u6c22\u7cfb\u7edf\u53ef\u80fd\u662f\u4e00\u79cd\u6709\u6548\u7684\u9ad8\u6d3b\u6027\u5149\u50ac\u5316\u5242\u7684\u8bbe\u8ba1\u3002\u9664\u4e86\u573a\u6548\u5e94\u5916\uff0c\u5f02\u8d28\u7ed3\u7684\u6784\u5efa\u4e5f\u53ef\u4ee5\u6709\u6548\u5730\u52a0\u901f\u7535\u8377\u5206\u79bb\u3002\u57fa\u4e8e\u6b64\u5206\u6790\uff0c\u5f00\u53d1\u4e00\u79cd\u5229\u7528\u78c1\u573a\u8bf1\u5bfc\u4fc3\u8fdb\u5149\u70ed\u8f85\u52a9\u5149\u50ac\u5316\u5236\u6c22\u7684S\u578b\u5f02\u8d28\u7ed3\u4f53\u7cfb\u662f\u4e00\u4e2a\u8feb\u5207\u9700\u8981\u7684\u95ee\u9898\uff0c\u4e5f\u662f\u4e00\u4e2a\u7d27\u8feb\u7684\u6311\u6218\u3002<\/p>\n<p><strong>02<\/strong><strong>\u3001\u3010\u6210\u679c\u63a0\u5f71\u3011<\/strong><\/p>\n<p>\u8fd1\u671f\uff0c\u6c5f\u82cf\u79d1\u6280\u5927\u5b66\u65bd\u4f1f\u9f99\/\u90ed\u5cf0\u56e2\u961f\u63d0\u51fa\u4e00\u79cd\u9ad8\u6548\u7684\u7531\u78c1\u573a\u8bf1\u5bfc\u7684\u5149\u70ed\u8f85\u52a9\u5149\u50ac\u5316\u5236\u6c22\u7cfb\u7edf\u3002Mn<sub>3<\/sub>O<sub>4<\/sub>@ZnIn<sub>2<\/sub>S<sub>4<\/sub>\uff08MO@ZIS\uff09\u7cfb\u7edf\u7684\u5149\u50ac\u5316\u6d3b\u6027\u7684\u663e\u8457\u589e\u5f3a\u662f\u7531\u4e8e\u78c1\u573a\u5f15\u8d77\u7684\u78c1\u70ed\u6548\u5e94\u548cMO\u6240\u8868\u73b0\u51fa\u7684\u5f3a\u5149\u70ed\u6548\u5e94\u7684\u534f\u540c\u6548\u5e94\uff0c\u663e\u8457\u63d0\u9ad8\u4e86\u5149\u50ac\u5316\u5242\u7684\u5f02\u8d28\u7ed3\u8868\u9762\u6e29\u5ea6\uff0c\u4fc3\u8fdb\u4e86\u5149\u8bf1\u5bfc\u7535\u5b50\u7a7a\u7a74\u5bf9\u7684\u5206\u79bb\u548c\u8f6c\u79fb\uff0c\u4ece\u800c\u52a0\u901f\u4e86\u8868\u9762\u6790\u6c22\u52a8\u529b\u5b66\uff0c\u8be5\u7814\u7a76\u62d3\u5bbd\u4e86\u591a\u573a\u534f\u540c\u5728\u63d0\u9ad8\u5149\u50ac\u5316\u6027\u80fd\u65b9\u9762\u7684\u5e94\u7528\u3002\u76f8\u5173\u6210\u679c\u4ee5\u201cMagnetic-field-induced activation of S-scheme heterojunction with core-shell structure for boosted photothermal-assisted photocatalytic\u201d \u4e3a\u9898\u53d1\u8868\u4e8e\u56fd\u9645\u77e5\u540d\u5b66\u672f\u671f\u520a\u300aFuel\u300b\u4e0a(https:\/\/doi.org\/10.1016\/j.fuel.2024.132394)\u3002\u6c5f\u82cf\u79d1\u6280\u5927\u5b66\u65bd\u4f1f\u9f99\u548c\u90ed\u5cf0\u526f\u6559\u6388\u4e3a\u672c\u6587\u901a\u8baf\u4f5c\u8005\uff0c2022\u7ea7\u5728\u8bfb\u7855\u58eb\u7814\u7a76\u751f\u84bf\u9e4f\u5b87\u4e3a\u672c\u6587\u7b2c\u4e00\u4f5c\u8005\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261265\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/1-6.png\" alt=\"\" width=\"554\" height=\"271\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/1-6.png 554w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/1-6-300x147.png 300w\" sizes=\"(max-width: 554px) 100vw, 554px\" \/><\/p>\n<p><strong>03<\/strong><strong>\u3001\u3010\u6570\u636e\u6982\u89c8\u3011<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261266\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/2-7.png\" alt=\"\" width=\"700\" height=\"804\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/2-7.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/2-7-261x300.png 261w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u56fe1. (a) MO@ZIS\u6838\u58f3\u5f02\u8d28\u7ed3\u7684\u5408\u6210\u793a\u610f\u56fe\u3002(b) ZIS\uff0c(c) MO\u548c(d) MO@ZIS-30\u7684SEM\u56fe\u50cf\u3002MO@ZIS-30\u5f02\u8d28\u7ed3\u7684\uff08e\uff0cf\uff09TEM\uff0c(g) HRTEM\uff0c(h) HAADF-STEM\u56fe\u50cf\u53ca\u76f8\u5e94\u5143\u7d20\u6620\u5c04\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261267\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/3-7.png\" alt=\"\" width=\"700\" height=\"581\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/3-7.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/3-7-300x249.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u56fe2. \u5236\u5907\u6837\u54c1\u7684 (a) XRD\u56fe\u8c31\u3002ZIS\u3001MO\u548cMO@ZIS-30\u7684 (b) N<sub>2<\/sub>\u5438\u9644-\u89e3\u5438\u7b49\u6e29\u7ebf\u548c (c) \u5b54\u5f84\u5206\u5e03\uff0c(d) XPS\u5168\u8c31\uff0c (e) Mn 2p\uff1b(f) O 1 s\uff1b(g) Zn 2p\uff1b(h) In 3d\u548c (i) S 2p\u7684XPS\u9ad8\u5206\u8fa8\u5149\u8c31\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261268\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/4-7.png\" alt=\"\" width=\"700\" height=\"588\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/4-7.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/4-7-300x252.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u56fe3. (a) \u5168\u5149\u8c31\u5149\u7167\u5c04\u4e0bZIS\u3001MO\u548cMO@ZIS\u7684\u5149\u50ac\u5316\u5236\u6c22\u66f2\u7ebf\u548c (b) \u5236\u6c22\u901f\u7387\u3002(c) MO@ZIS-30\u7684\u5149\u50ac\u5316\u5236\u6c22\u901f\u7387\u4e0e\u673a\u68b0\u6df7\u5408\u65f6\u5bf9\u6bd4\u3002ZIS\u548cMO@ZIS-30\u7684 (d) \u77ac\u6001\u5149\u7535\u6d41\u54cd\u5e94\uff0c(e) EIS\u548c (f) LSV\u66f2\u7ebf\u3002(g) MO@ZIS-30\u5728\u9ed1\u6697\u548c\u5149\u7167\u4e0b\u7684SPV\u5149\u8c31\uff08\u63d2\u56fe\u4e3aKPFM\u56fe\u50cf\uff09\u3002(h) \u5236\u5907\u6837\u54c1\u7684PL\u5149\u8c31\u548c (i) TRPL\u8367\u5149\u53d1\u5c04\u5149\u8c31\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261269\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/5-3.png\" alt=\"\" width=\"700\" height=\"714\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/5-3.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/5-3-294x300.png 294w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u56fe4. \u6240\u6709\u5149\u50ac\u5316\u5242\u7684 (a) \u7d2b\u5916-\u53ef\u89c1-\u8fd1\u7ea2\u5916\u5438\u6536\u5149\u8c31\u3002(b) \u5728MO\u4e2d\u7684\u975e\u5f1b\u8c6b\u8f90\u5c04\u8fc7\u7a0b\u7684\u793a\u610f\u56fe\u3002(c) MO@ZIS\u6838\u58f3\u5f02\u8d28\u7ed3\u7684\u4f20\u70ed\u6548\u5e94\u3002(d) \u5df2\u5236\u5907\u6750\u6599\u5728\u5149\u7167\u4e0b\u7684\u6e29\u5ea6\u6620\u5c04\u56fe\u50cf\u548c (e) \u76f8\u5e94\u7684\u6e29\u5ea6\u53d8\u5316\u66f2\u7ebf\u3002MO@ZIS-30\u7684 (f) \u5149\u70ed\u8f6c\u6362\u6548\u7387\u3002(g)\u5149\u50ac\u5316\u5236\u6c22\u8fc7\u7a0b\u4e2d\u7684\u5149\u70ed\u7ea2\u5916\u56fe\u50cf\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261270\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/6-3.png\" alt=\"\" width=\"700\" height=\"547\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/6-3.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/6-3-300x234.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u56fe5. ZIS\u548cMO@ZIS-30\u5728\u4e0d\u540c\u53cd\u5e94\u6e29\u5ea6\u4e0b\u7684 (a) \u5236\u6c22\u6d3b\u6027\u548c (b) \u5236\u6c22\u901f\u7387\u3002MO@ZIS-30 (c)\u5728\u4e0d\u540c\u6e29\u5ea6\u4e0b\u5149\u50ac\u5316\u5236\u6c22\u901f\u7387\u4e0e\u53cd\u5e94\u6e29\u5ea6\u7684\u5173\u7cfb\u53ca (d) \u6d3b\u5316\u80fd\u7684\u8ba1\u7b97\u3002MO@ZIS-30\u5728\u4e0d\u540c\u6e29\u5ea6\u6761\u4ef6\u4e0b\u7684 (e) \u77ac\u6001\u5149\u7535\u6d41\u54cd\u5e94\u66f2\u7ebf\uff0c(f) EIS\u56fe\u8c31\u548c (g) PL\u5149\u8c31\u3002ZIS\u548cMO@ZIS-30\u5728\u5149\u7167\u548c\u9ed1\u6697\u6761\u4ef6\u4e0b\u7684 (h) \u83ab\u7279\u8096\u7279\u57fa\u548c (i) \u8ba1\u7b97\u7684N<sub>D<\/sub>\u503c\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261271\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/7-2.png\" alt=\"\" width=\"700\" height=\"513\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/7-2.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/7-2-300x220.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u56fe6. (a) MO\u548cMO@ZIS-30\u7684\u78c1\u6ede\u56de\u7ebf\u3002MO@ZIS-30\u5728\u78c1\u573a\u4e0b\u76f8\u5e94\u7684 (b) \u5149\u50ac\u5316\u5236\u6c22\u6d3b\u6027\u548c (c) \u5236\u6c22\u901f\u7387\u3002(d) MO@ZIS-30\u5728420, 550\u548c650 nm\u6ce2\u957f\u5904\u7684AQE\u3002(e) MO@ZIS-30\u4e0e\u6700\u8fd1\u62a5\u9053\u7684\u5149\u70ed\u548c\u78c1\u573a\u8bf1\u5bfc\u5149\u50ac\u5316\u5242\u5236\u6c22\u6027\u80fd\u5bf9\u6bd4\u3002(f) \u5faa\u73af\u5236\u6c22\u5b9e\u9a8c\u3002(g) \u53cd\u5e94\u524d\u540e\u7684XRD\u8c31\u56fe\u3002(h) MO@ZIS-30\u7684\u78c1\u6027\u53ef\u56de\u6536\u7387\u548c\u78c1\u6027\u5206\u79bb\u7279\u6027\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261272\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/8.png\" alt=\"\" width=\"700\" height=\"559\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/8.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/8-300x240.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u56fe7. \u5728\u4e0d\u540c\u6761\u4ef6\u4e0b\u7684 (a) \u77ac\u6001\u5149\u7535\u6d41\u54cd\u5e94\u3001(b) EIS\u56fe\u3001(c) LSV\u3001(d) \u83ab\u7279\u8096\u7279\u57fa\u548c (e) \u8f7d\u6d41\u5b50\u6d53\u5ea6\u503c\u3002(f) MO@ZIS-30\u5728\u6709\u65e0\u78c1\u573a\u548c\u5149\u7167\u4f5c\u7528\u4e0b\u7684\u6e29\u5ea6\u53d8\u5316\u3002(g) MO@ZIS-30\u5728\u78c1\u573a\u4f5c\u7528\u4e0b\u5236\u6c22\u8fc7\u7a0b\u7684\u5149\u70ed\u6620\u5c04\u56fe\u50cf\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261273\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/9.png\" alt=\"\" width=\"709\" height=\"1012\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/9.png 709w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/9-210x300.png 210w\" sizes=\"(max-width: 709px) 100vw, 709px\" \/><\/p>\n<p>\u56fe8. MO\u548cZIS\u7684 (a) \u5e26\u9699\u503c\uff0c(b) \u83ab\u7279\u8096\u7279\u57fa\u548c (c) \u7d2b\u5916\u5149\u7535\u5b50\u80fd\u8c31\u3002(d) S\u578bMO@ZIS\u5f02\u8d28\u7ed3\u5149\u50ac\u5316\u5236\u6c22\u7684\u53cd\u5e94\u673a\u7406\u548c (e) \u78c1\u573a\u8bf1\u5bfc\u5149\u70ed\u8f85\u52a9\u5149\u50ac\u5316\u673a\u7406\u793a\u610f\u56fe\u3002<\/p>\n<p><strong>04<\/strong><strong>\u3001\u3010\u6210\u679c\u542f\u793a\u3011<\/strong><\/p>\n<p>\u7efc\u4e0a\u6240\u8ff0\uff0c\u901a\u8fc7\u4f4e\u6e29\u6c34\u6d74\u6cd5\u6210\u529f\u5408\u6210\u4e86\u5177\u6709S\u578b\u5f02\u8d28\u7ed3\u7535\u8377\u8f6c\u79fb\u9014\u5f84\u7684\u6838\u58f3MO@ZIS\u5149\u50ac\u5316\u4f53\u7cfb\uff0c\u7528\u4e8e\u78c1\u573a\u8bf1\u5bfc\u7684\u5149\u70ed\u8f85\u52a9\u5149\u50ac\u5316\u5236\u6c22\u3002\u6700\u4f73MO@ZIS-30\u7684\u5149\u50ac\u5316\u5236\u6c22\u6027\u80fd\u4e3a33.29 mmol h<sup>-1<\/sup> g<sup>-1<\/sup>\uff0c\u663e\u8457\u9ad8\u4e8e\u65e0\u78c1\u573a\u65f6\u3002\u8fd9\u79cd\u6027\u80fd\u7684\u6539\u5584\u662f\u7531\u4e8e\uff1a(i) \u78c1\u573a\u4ea7\u751f\u7684\u6d1b\u4f26\u5179\u529b\u6709\u6548\u5730\u6291\u5236\u5149\u4ea7\u751f\u7535\u8377\u7684\u91cd\u7ec4\uff0c\u4fc3\u8fdb\u7535\u5b50\u7a7a\u7a74\u5bf9\u7684\u5206\u79bb\uff0c\u4f7f\u66f4\u591a\u7684\u7535\u5b50\u53c2\u4e0e\u5236\u6c22\u53cd\u5e94\uff1b\uff08ii\uff09\u6838\u58f3\u5f02\u8d28\u7ed3\u5185\u7684\u6838\u5fc3MO\u8868\u73b0\u51fa\u5f3a\u70c8\u7684\u5149\u70ed\u6548\u5e94\uff0c\u5c06\u6709\u6548\u7684\u70ed\u4f20\u5230ZIS\u58f3\uff1b\uff08iii\uff09\u78c1\u573a\u5f15\u8d77\u7684\u78c1\u70ed\u6548\u5e94\u53ef\u4ee5\u8fdb\u4e00\u6b65\u63d0\u9ad8\u5149\u50ac\u5316\u4f53\u7cfb\u7684\u6574\u4f53\u6e29\u5ea6\uff0c\u4ece\u800c\u964d\u4f4e\u53cd\u5e94\u7684\u6d3b\u5316\u80fd\uff0c\u63d0\u9ad8\u6790\u6c22\u53cd\u5e94\u52a8\u529b\u5b66\uff1b\uff08iv\uff09S\u578b\u5f02\u8d28\u7ed3\u7684\u6784\u5efa\u663e\u8457\u4fc3\u8fdb\u4e86\u5149\u751f\u7535\u8377\u7684\u7a7a\u95f4\u5206\u79bb\uff0c\u4fdd\u8bc1\u4e86\u4fdd\u7559\u5177\u6709\u5f3a\u8fd8\u539f\u80fd\u529b\u7684\u7535\u5b50\uff0c\u4fc3\u8fdb\u5149\u50ac\u5316\u5236\u6c22\u53cd\u5e94\u3002\u672c\u7814\u7a76\u4e3a\u78c1\u573a\u8bf1\u5bfc\u7684\u5149\u70ed\u8f85\u52a9\u5149\u50ac\u5316\u5242\u7684\u8bbe\u8ba1\u63d0\u4f9b\u4e86\u6df1\u523b\u7684\u76d1\u7763\u548c\u7cfb\u7edf\u7684\u65b9\u6cd5\uff0c\u4e3a\u591a\u573a\u8026\u5408\u5149\u50ac\u5316\u53cd\u5e94\u4f53\u7cfb\u7684\u5e94\u7528\u5f00\u8f9f\u4e86\u65b0\u7684\u53ef\u80fd\u6027\u3002<\/p>\n<p>\u5168\u6587\u94fe\u63a5\uff1a<\/p>\n<p><a href=\"https:\/\/doi.org\/10.1016\/j.fuel.2024.132394\">https:\/\/doi.org\/10.1016\/j.fuel.2024.132394<\/a><\/p>\n<p><strong>\u3010\u4f5c\u8005\u4fe1\u606f\u3011<\/strong><\/p>\n<p><strong>\u84bf\u9e4f\u5b87\uff08\u7b2c\u4e00\u4f5c\u8005\uff09<\/strong>\uff0c\u6c5f\u82cf\u79d1\u6280\u5927\u5b66\u80fd\u6e90\u4e0e\u52a8\u529b\u5b66\u96622022\u7ea7\u5728\u8bfb\u7855\u58eb\u7814\u7a76\u751f\u3002\u4e3b\u8981\u4ece\u4e8b\u80fd\u6e90\u5149\u50ac\u5316(\u5149\u70ed\u8f85\u52a9-\u5149\u50ac\u5316\u5236\u6c22)\uff0c\u73af\u5883\u5149\u50ac\u5316\u7b49\u9886\u57df\u7684\u7814\u7a76\uff0c\u4ee5\u7b2c\u4e00\u4f5c\u8005\u5728\u8457\u540d\u56fd\u9645\u671f\u520a\u300aSeparation and Purification Technology\u300b\u3001\u300aFuel\u300b\u4e0a\u53d1\u8868SCI\u8bba\u65872\u7bc7\u3002<\/p>\n<p><strong>\u90ed\u5cf0\uff08\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\uff0c\u6c11\u76df\u76df\u5458, \u73b0\u4efb\u6c5f\u82cf\u79d1\u6280\u5927\u5b66\u526f\u6559\u6388\uff0c\u7855\u58eb\u751f\u5bfc\u5e08\uff0c\u65b0\u80fd\u6e90\u7cfb\u4e13\u4e1a\u8d1f\u8d23\u4eba\uff0c\u4e2d\u56fd\u611f\u5149\u5b66\u4f1a\u5149\u50ac\u5316\u4e13\u4e1a\u59d4\u5458\u4f1a\u4f1a\u5458\uff0c\u6c5f\u82cf\u7701\u73af\u5883\u79d1\u5b66\u5b66\u4f1a\u4f1a\u5458, \u65b0\u52a0\u5761\u7ef4\u6cfd\u4e13\u5bb6\u5e93\uff08VE\uff09\u6750\u6599\u79d1\u5b66\u4e13\u5bb6\u59d4\u5458\u4f1a\u4f1a\u5458\u3002\u957f\u5b89\u5927\u5b66\u5e02\u653f\u5de5\u7a0b\u4e13\u4e1a\u535a\u58eb\u6bd5\u4e1a\uff0c\u83b7\u5de5\u5b66\u535a\u58eb\u5b66\u4f4d\u3002\u4e3b\u8981\u4ece\u4e8bg-C3N4\u57fa\u590d\u5408\u5149\u50ac\u5316\u6750\u6599\u7684\u8bbe\u8ba1\u3001\u6784\u7b51\u4ee5\u53ca\u5149\u50ac\u5316\u6027\u80fd\u7b49\u65b9\u9762\u7684\u7814\u7a76\u5de5\u4f5c\u3002\u4e3b\u6301\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u9879\u76ee\uff0c\u6c5f\u82cf\u7701\u9752\u5e74\u57fa\u91d1\u9879\u76ee\uff0c\u6c5f\u82cf\u7701\u201c\u9752\u84dd\u5de5\u7a0b\u201d\u4f18\u79c0\u9aa8\u5e72\u6559\u5e08\u4eba\u624d\u9879\u76ee\uff0c\u6821\u7ea7\u6df1\u84dd\u6770\u51fa\u4eba\u624d\u9879\u76ee, \u6cb3\u5317\u7701\u6c34\u8d44\u6e90\u53ef\u6301\u7eed\u5229\u7528\u4e0e\u5f00\u53d1\u5b9e\u9a8c\u5ba4\u5f00\u53d1\u57fa\u91d1\uff0c\u6c5f\u82cf\u7701\u4ea7\u5b66\u7814\u9879\u76ee\u7b4910\u4f59\u9879\u3002\u8fd1\u5e74\u6765\uff0c\u5171\u8ba1\u4ee5\u7b2c\u4e00\u4f5c\u8005\u6216\u901a\u8baf\u4f5c\u8005\u53d1\u8868110\u4f59\u7bc7SCI\u6536\u5f55\u8bba\u6587\uff0cESI\u9ad8\u88ab\u5f15\u8bba\u658730\u4f59\u7bc7\uff0cESI\u70ed\u70b9\u8bba\u65879\u7bc7\uff0c\u5f15\u752811500\u4f59\u6b21\uff0cH-index 65\u30021\u7bc7\u83b7\u5f97Inorganic Chemistry Frontiers\u671f\u520a2020\u5e74\u5ea6\u6700\u4f73\u8bba\u6587\u5956\uff0c2023\u5e74\u5ea6\u6c5f\u82cf\u7701\u9ad8\u7b49\u5b66\u6821\u79d1\u5b66\u6280\u672f\u7814\u7a76\u6210\u679c\u5956\u4e8c\u7b49\u5956\uff0c2023\u5e74\u5ea6\u6c5f\u82cf\u7701\u590d\u5408\u6750\u6599\u5b66\u4f1a\u79d1\u6280\u8fdb\u6b65\u4e8c\u7b49\u5956\uff0c\u5165\u90092023\u5e74\u6c5f\u82cf\u7701\u81ea\u7136\u79d1\u5b66\u767e\u7bc7\u4f18\u79c0\u5b66\u672f\u6210\u679c\u8bba\u6587\uff0c\u8363\u83b7\u56fd\u9645\u5b66\u672f\u5956\u201c\u6700\u4f73\u7814\u7a76\u8005\u201d\u5956\uff0c\u56fd\u5bb6\u6388\u6743\u53d1\u660e\u4e13\u52295\u9879\uff0c\u6307\u5bfc\u672c\u79d1\u751f\u83b7\u5f97\u6c5f\u82cf\u7701\u4f18\u79c0\u672c\u79d1\u6bd5\u8bbe\u4e00\u7b49\u59561\u6b21\uff0c\u6559\u80b2\u90e8\u80fd\u6e90\u4e0e\u52a8\u529b\u5168\u56fd\u4f18\u79c0\u767e\u7bc7\u6bd5\u4e1a\u8bbe\u8ba1\u8bba\u65872\u6b21\u3002\u5165\u90092022\/2023\u5e74\u5168\u7403\u524d2%\u9876\u5c16\u79d1\u5b66\u5bb6\u699c\u5355\uff08World\u2019s Top 2% Scientists 2022\/2023\uff09\u3001\u6c5f\u82cf\u7701\u201c\u79d1\u6280\u526f\u603b\u201d\u3001\u9547\u6c5f\u5e02\u201c\u51fa\u5f69\u6559\u80b2\u4eba\u201d\u3001\u6821\u201c\u4f18\u79c0\u6559\u5e08\u201d\u3001\u672c\u521b\u201c\u4f18\u79c0\u6307\u5bfc\u6559\u5e08\u201d\u3001\u7701\u7ea7\u7ade\u8d5b\u201c\u4f18\u79c0\u6307\u5bfc\u6559\u5e08\u201d\u7b49\u79f0\u53f7\uff0c\u76f8\u5173\u5de5\u4f5c\u53d1\u8868\u5728\u300aApplied Catalysis B: Environmental\u300b\u3001\u300aChemical Engineering Journal\u300b\u3001\u300aJournal of Hazardous Materials\u300b\u3001\u300aSmall\u300b\u3001\u300aAdvanced Powder Materials\u300b\u3001\u300aJournal of Catalysis\u300b\u3001\u300aSeparation and Purification Technology\u300b\u7b49\u9ad8\u6c34\u5e73\u6742\u5fd7\u3002<\/p>\n<p><strong>\u65bd\u4f1f\u9f99\uff08\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\uff0c\u65e0\u515a\u6d3e\u4eba\u58eb\uff0c\u534e\u4e2d\u79d1\u6280\u5927\u5b66\u535a\u58eb\uff0c\u90d1\u5dde\u5927\u5b66\u535a\u58eb\u540e\uff0c\u73b0\u4efb\u6c5f\u82cf\u79d1\u6280\u5927\u5b66\u526f\u6559\u6388\uff0c\u7855\u58eb\u751f\u5bfc\u5e08\uff0c\u4e2d\u56fd\u611f\u5149\u5b66\u4f1a\u5149\u50ac\u5316\u4e13\u4e1a\u59d4\u5458\u4f1a\u4f1a\u5458\uff0c\u6c5f\u82cf\u7701\u590d\u5408\u6750\u6599\u5b66\u4f1a\u4f1a\u5458\uff0c\u6c5f\u82cf\u7701\u73af\u5883\u79d1\u5b66\u5b66\u4f1a\u4f1a\u5458\uff0c\u6c5f\u82cf\u7701\u6750\u6599\u5b66\u4f1a\u4f1a\u5458\u3002\u4e3b\u8981\u4ece\u4e8b\u78b3\u57fa\uff08\u78b3\u70b9\u3001\u6c2e\u5316\u78b3\uff09\u590d\u5408\u5149\u50ac\u5316\u6750\u6599\u7684\u8bbe\u8ba1\u3001\u6784\u7b51\u4ee5\u53ca\u5149\u50ac\u5316\u6027\u80fd\uff08\u964d\u89e3\u3001\u5206\u89e3\u6c34\u5236\u6c22\u3001\u6d77\u6c34\u6de1\u5316\u53ca\u9632\u8150\uff09\u7b49\u65b9\u9762\u7684\u7814\u7a76\u5de5\u4f5c\u3002\u76f8\u5173\u5de5\u4f5c\u53d1\u8868\u5728Appl. Catal. B: Environ., Adv. Powder Mater., J. Mater. Chem. A, Chem. Eng. J., J. Cat. ACS Appl. Mater. Inter., Small, J. Hazard. Mater., Sep. Purif. Technol., Inorg. Chem. Front.,\u7b49\u9ad8\u6c34\u5e73\u6742\u5fd7\u3002\u622a\u6b62\u76ee\u524d\uff0c\u5171\u8ba1\u4ee5\u7b2c\u4e00\u4f5c\u8005\u6216\u901a\u8baf\u4f5c\u8005\u53d1\u8868120\u4f59\u7bc7SCI\u6536\u5f55\u8bba\u6587\uff0cESI\u9ad8\u88ab\u5f15\u8bba\u658740\u4f59\u7bc7\uff0cESI\u70ed\u70b9\u8bba\u658717\u7bc7\uff0c\u5f15\u752812000\u4f59\u6b21\uff0cH-index 66\uff0c\u51fa\u7248\u5b66\u672f\u4e13\u84571\u672c\uff0c1\u7bc7\u83b7\u5f97Inorganic Chemistry Frontiers\u671f\u520a2020\u5e74\u5ea6\u6700\u4f73\u8bba\u6587\uff0c\u5165\u90092024\u5e74\u6c5f\u82cf\u7701\u201c\u9752\u84dd\u5de5\u7a0b\u201d\u4f18\u79c0\u9aa8\u5e72\u6559\u5e08\uff0c2023\u5e74\u5ea6\u6c5f\u82cf\u7701\u9ad8\u7b49\u5b66\u6821\u79d1\u5b66\u6280\u672f\u7814\u7a76\u6210\u679c\u5956\u4e8c\u7b49\u5956\uff0c2023\u5e74\u5ea6\u6c5f\u82cf\u7701\u590d\u5408\u6750\u6599\u5b66\u4f1a\u79d1\u6280\u8fdb\u6b65\u4e8c\u7b49\u5956\uff0c2023\u5e74\u6c5f\u82cf\u7701\u81ea\u7136\u79d1\u5b66\u767e\u7bc7\u4f18\u79c0\u5b66\u672f\u6210\u679c\u8bba\u6587\uff0c2023\u5e74\u6c5f\u82cf\u7701\u4f18\u79c0\u7855\u58eb\u8bba\u65871\u7bc7\u3002\u8363\u83b7\u56fd\u9645\u590d\u5408\u6750\u6599\u201c\u6700\u4f73\u7814\u7a76\u8005\u201d\u5956\uff0c\u6388\u6743\u56fd\u5185\u53d1\u660e\u4e13\u52292\u9879\u3002\u5165\u90092022\/2023\u5e74\u5168\u7403\u524d2%\u9876\u5c16\u79d1\u5b66\u5bb6\u699c\u5355\uff08World\u2019s Top 2% Scientists 2022\/2023\uff09\uff0c\u4e3b\u6301\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u9752\u5e74\u3001\u4e2d\u56fd\u535a\u58eb\u540e\u9762\u4e0a\u57fa\u91d1\u3001\u6c5f\u82cf\u7701\u201c\u53cc\u521b\u535a\u58eb\u201d\u3001\u201c\u79d1\u6280\u526f\u603b\u201d\u4eba\u624d\u9879\u76ee\u3001\u6cb3\u5357\u7701\u535a\u58eb\u540e\u79d1\u7814\u9879\u76ee\u542f\u52a8\u8d44\u52a9\u3001\u6cb3\u5317\u7701\u6c34\u8d44\u6e90\u53ef\u6301\u7eed\u5229\u7528\u4e0e\u5f00\u53d1\u5b9e\u9a8c\u5ba4\u5f00\u53d1\u57fa\u91d1\u3001\u4e2d\u56fd\u77f3\u6cb9\u548c\u5316\u5de5\u884c\u4e1a\u592a\u9633\u80fd\u7535\u6c60\u7535\u6781\u6750\u6599\u91cd\u70b9\u5b9e\u9a8c\u5ba4\u5f00\u653e\u57fa\u91d1\u3001\u529f\u80fd\u65e0\u673a\u6750\u6599\u5316\u5b66\u6559\u80b2\u90e8\u91cd\u70b9\u5b9e\u9a8c\u5ba4\u5f00\u653e\u57fa\u91d1\u3001\u6c5f\u82cf\u7701\u4ea7\u5b66\u7814\u9879\u76ee\u3001\u6821\u7ea7\u6df1\u84dd\u6770\u51fa\u4eba\u624d\u7b4910\u4f59\u9879\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>01\u3001\u3010\u5bfc\u8bfb\u3011 \u957f\u671f\u4ee5\u6765\uff0c\u4eba\u7c7b\u793e\u4f1a\u7684\u52a8\u6001\u53d1\u5c55\u4e00\u76f4\u4f9d\u8d56\u4e8e\u4f20\u7edf\u7684\u3001\u4e0d\u53ef\u518d\u751f\u7684\u5316\u77f3\u71c3\u6599\u3002\u7136\u800c\uff0c\u5316\u77f3\u71c3\u6599\u7684\u7316\u7357\u6d88\u8d39\u52a0\u5267\u4e86\u80fd\u6e90\u77ed\u7f3a\u548c\u73af\u5883\u6c61\u67d3\uff0c\u8feb\u5207\u9700\u8981\u5f00\u53d1\u7eff\u8272\u548c\u66f4\u65b0\u80fd\u6e90\u3002&#8230;<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-261263","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/261263"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=261263"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/261263\/revisions"}],"predecessor-version":[{"id":261274,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/261263\/revisions\/261274"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=261263"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=261263"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=261263"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}