{"id":261315,"date":"2024-07-12T06:01:33","date_gmt":"2024-07-11T22:01:33","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=261315"},"modified":"2024-07-11T23:01:52","modified_gmt":"2024-07-11T15:01:52","slug":"%e9%92%99%e9%92%9b%e7%9f%bf%e8%8e%ab%e5%b0%94%e8%b6%85%e6%99%b6%e6%a0%bc%ef%bc%8c%e6%9c%80%e6%96%b0nature-materials","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=261315","title":{"rendered":"\u9499\u949b\u77ff\u83ab\u5c14\u8d85\u6676\u683c\uff0c\u6700\u65b0Nature Materials!"},"content":{"rendered":"<p><strong>1.<\/strong><strong>\u3010\u79d1\u5b66\u80cc\u666f\u3011<\/strong><\/p>\n<p><strong>\u83ab\u5c14\u8d85\u6676\u683c<\/strong>\u901a\u8fc7\u5229\u7528\u7a7a\u95f4\u53d8\u5316\u7684\u5c42\u95f4\u76f8\u4e92\u4f5c\u7528\u6765\u6539\u53d8\u7535\u5b50\u80fd\u5e26\u7ed3\u6784\uff0c\u5df2\u7ecf\u6210\u4e3a\u7814\u7a76\u5f3a\u76f8\u5173\u91cf\u5b50\u73b0\u8c61\u7684\u65b0\u5e73\u53f0\u3002\u5305\u62ec\u8d85\u5bfc\u548c\u83ab\u7279\u7edd\u7f18\u4f53\u5728\u5185\u7684\u5927\u91cf\u91cf\u5b50\u73b0\u8c61\u5df2\u7ecf\u5728\u9b54\u89d2\u77f3\u58a8\u70ef\u548c\u626d\u8f6c\u53cc\u5c42\u8fc7\u6e21\u91d1\u5c5e\u4e8c\u786b\u5316\u7269\uff08TMDCs\uff09\u4e2d\u5b9e\u73b0\u3002\u7136\u800c\uff0c\u5c42\u95f4\u76f8\u4e92\u4f5c\u7528\u4ec5\u9650\u4e8e\u5c42\u72b6\u77f3\u58a8\u70ef\u548cTMDCs\u4e2d\u76f8\u5bf9\u8f83\u5f31\u7684\u8303\u5fb7\u534e\u529b\uff0c\u56e0\u6b64\u83ab\u5c14\u6761\u7eb9\u5f15\u5165\u7684\u80fd\u91cf\u8c03\u5236\u76f8\u5bf9\u8f83\u5c0f\uff0c\u76ee\u524d\u4e3a\u6b62\uff0c\u83ab\u5c14\u5e73\u5766\u5e26\u51e0\u4e4e\u53ea\u80fd\u5728\u4f4e\u6e29\u4e0b\u88ab\u89c2\u5bdf\u5230\u3002\u4e3a\u4e86\u589e\u52a0\u80fd\u91cf\u8c03\u5236\u7684\u6df1\u5ea6\u5b9e\u73b0\u5ba4\u6e29\u83ab\u5c14\u6750\u6599\uff0c\u9700\u8981\u8d85\u8d8a\u8303\u5fb7\u534e\u529b\u7684\u5c42\u95f4\u76f8\u4e92\u4f5c\u7528\u3002\u7136\u800c\uff0c\u5236\u9020\u539a\u5ea6\u53ef\u63a7\u7684\u5927\u578b\u4e8c\u7ef4\u975e\u8303\u5fb7\u534e\u6750\u6599\u5177\u6709\u5f88\u5927\u6311\u6218\u3002\u9499\u949b\u77ff\u6676\u4f53\u7ed3\u6784\u4e5f\u53ef\u4ee5\u6784\u9020\u5177\u6709\u72ec\u7279\u83ab\u5c14\u6027\u8d28\u7684\u6709\u8da3\u51e0\u4f55\u5f62\u72b6\uff0c<strong>\u4f46\u662f\u76ee\u524d\u7684\u65b9\u6cd5\u96be\u4ee5\u5236\u5907\u5177\u6709\u6784\u5efa\u83ab\u5c14\u8d85\u6676\u683c\u6240\u5fc5\u987b\u7684\u3001\u53ef\u826f\u597d\u63a7\u5236\u626d\u8f6c\u89d2\u7684\u539f\u5b50\u7ea7\u5149\u6ed1\u3001\u8d85\u8584\u3001\u65e0\u914d\u4f53\u7684\u5927\u9762\u79ef\u4e8c\u7ef4\u9499\u949b\u77ff\u6676\u4f53\u3002<\/strong><\/p>\n<p><strong>2.<\/strong><strong>\u3010\u521b\u65b0\u6210\u679c\u3011<\/strong><\/p>\n<p>\u57fa\u4e8e\u4ee5\u4e0a\u7814\u7a76\u80cc\u666f\uff0c<strong>\u7f8e\u56fd\u666e\u6e21\u5927\u5b66\u9ec4\u4e3d\u767d\u6559\u6388\u3001\u7aa6\u4e50\u6dfb\u6559\u6388\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\u7b49\u4eba\u5f00\u53d1\u4e86\u4e00\u79cd\u65e0\u914d\u4f53APbX<sub>3<\/sub>\u4e8c\u7ef4\u9499\u949b\u77ff\u7684\u65b9\u6cd5\uff0c\u5176\u539a\u5ea6\u53ef\u4ee5\u4f4e\u81f3~2-5 nm\uff0c\u4efb\u610f\u57fa\u6750\u4e0a\u7684\u5c3a\u5bf8\u53ef\u8fbe10 \u03bcm\u4ee5\u4e0a\u3002\u65f6\u95f4\u5206\u8fa8\u5149\u5b66\u663e\u5fae\u955c\u663e\u793a\uff0c\u4eba\u4e3a\u626d\u66f2\u7684\u7ed3\u6784\u5177\u6709\u65b9\u5f62\u83ab\u5c14\u6761\u7eb9\u548c10\u00b0\u626d\u8f6c\u89d2\u9644\u8fd1\u7684\u5c40\u57df\u6fc0\u5b50\u548c\u7535\u8377\u3002<strong>\u8fd9\u9879\u5de5\u4f5c\u5c55\u793a\u4e86\u4e8c\u7ef4\u9499\u949b\u77ff\u4f5c\u4e3a\u72ec\u7279\u5ba4\u6e29\u83ab\u5c14\u6750\u6599\u7684\u524d\u666f\u3002<\/strong>\u76f8\u5173\u7814\u7a76\u6210\u679c\u4ee5\u201cMoir\u00e9 superlattices in twisted two-dimensional halide perovskites\u201d\u4e3a\u9898\u53d1\u8868\u5728\u6700\u65b0<strong><em>Nature Materials<\/em><\/strong>\u671f\u520a\u4e0a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261316\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/\u5c01\u9762.png\" alt=\"\" width=\"885\" height=\"475\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/\u5c01\u9762.png 885w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/\u5c01\u9762-300x161.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/\u5c01\u9762-768x412.png 768w\" sizes=\"(max-width: 885px) 100vw, 885px\" \/><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261317\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/1-8.png\" alt=\"\" width=\"1779\" height=\"1338\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/1-8.png 1779w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/1-8-300x226.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/1-8-768x578.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/1-8-1024x770.png 1024w\" sizes=\"(max-width: 1779px) 100vw, 1779px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>1.<\/strong><strong>\u5e73\u8861\u6eb6\u6db2\u6cd5\u5c06<\/strong><strong>RP<\/strong><strong>\u76f8\u4e8c\u7ef4\u9499\u949b\u77ff\u8f6c\u5316\u4e3a<\/strong><strong>APbX<sub>3<\/sub><\/strong><strong>\u76f8\u7684\u5236\u5907\u53ca\u8868\u5f81<\/strong><strong>\u3002<\/strong>\u00a9 2024 Springer Nature<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261318\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/2-9.png\" alt=\"\" width=\"1798\" height=\"1176\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/2-9.png 1798w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/2-9-300x196.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/2-9-768x502.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/2-9-1024x670.png 1024w\" sizes=\"(max-width: 1798px) 100vw, 1798px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>2. <\/strong><strong>\u626d\u8f6c\u9499\u949b\u77ff\u5c42\u4e2d\u7684\u65b9\u5f62\u83ab\u5c14\u56fe\u6848<\/strong><strong>\u3002<\/strong>\u00a9 2024 Springer Nature<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261319\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/3-9.png\" alt=\"\" width=\"1824\" height=\"1793\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/3-9.png 1824w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/3-9-300x295.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/3-9-768x755.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/3-9-1024x1007.png 1024w\" sizes=\"(max-width: 1824px) 100vw, 1824px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>3.<\/strong><strong> MAPbI<sub>3<\/sub><\/strong><strong>\u626d\u8f6c\u9499\u949b\u77ff\u5c42\u4e2d\u4e0e\u626d\u8f6c\u89d2\u76f8\u5173\u7684\u6fc0\u5b50\u8f93\u8fd0\u548c\u6e6e\u706d<\/strong><strong>\u3002<\/strong>\u00a9 2024 Springer Nature<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-261320\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/4-9.png\" alt=\"\" width=\"1803\" height=\"1336\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/4-9.png 1803w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/4-9-300x222.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/4-9-768x569.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/07\/4-9-1024x759.png 1024w\" sizes=\"(max-width: 1803px) 100vw, 1803px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>4.<\/strong> <strong>MAPbI<sub>3<\/sub><\/strong><strong>\u626d\u8f6c\u9499\u949b\u77ff\u5c42\u4e2d\u4e0e\u626d\u8f6c\u89d2\u76f8\u5173\u7684\u5149\u81f4\u53d1\u5149\u3002<\/strong>\u00a9 2024 Springer Nature<\/p>\n<p><strong>3.<\/strong><strong>\u3010\u79d1\u5b66\u542f\u8fea\u3011<\/strong><\/p>\n<p>\u8be5\u7814\u7a76\u7ed3\u679c\u8868\u660e\uff0c\u626d\u8f6c\u7684\u4e8c\u7ef4APbX<sub>3<\/sub>\u9499\u949b\u77ff\u8d85\u6676\u683c\u662f\u7814\u7a76\u5ba4\u6e29\u83ab\u5c14\u6fc0\u5b50\u6750\u6599\u7684\u4e00\u4e2a\u65b0\u5e73\u53f0\u3002<strong>\u8fd9\u4e9b\u7ed3\u6784\u5f15\u5165\u7684\u79bb\u5b50\u5c42\u95f4\u76f8\u4e92\u4f5c\u7528\u8d85\u8d8a\u4e86\u4f20\u7edf\u4e8c\u7ef4\u6750\u6599\u4e2d\u7684\u8303\u5fb7\u534e\u76f8\u4e92\u4f5c\u7528\uff0c\u4ece\u800c\u62d3\u5bbd\u4e86\u83ab\u5c14\u6750\u6599\u53ef\u7528\u7684\u9009\u62e9\u8303\u56f4\u3002<\/strong>\u5364\u5316\u7269\u9499\u949b\u77ff\u4e2d\u660e\u4eae\u7684\u76f4\u63a5\u83ab\u5c14\u6fc0\u5b50\u4e5f\u4e3a\u8bbe\u8ba1\u80fd\u91cf\u548c\u7535\u8377\u8f6c\u79fb\u6cdb\u51fd\u63d0\u4f9b\u4e86\u66f4\u591a\u673a\u4f1a\u3002\u5728\u6b64\u7814\u7a76\u57fa\u7840\u4e0a\uff0c\u8fd8\u9700\u8981\u8fdb\u4e00\u6b65\u7814\u7a76\u6676\u683c\u5f1b\u8c6b\u6548\u5e94\u5bf9\u83ab\u5c14\u7535\u52bf\u7684\u5f71\u54cd\u3002\u53e6\u5916\uff0c\u7531\u4e8e\u9499\u949b\u77ff\u6676\u683c\u4e0d\u8010\u53d7\u7535\u5b50\u675f\u7167\u5c04\uff0c\u9700\u8981\u6539\u8fdbTEM\u6280\u672f\u6765\u5e2e\u52a9\u76f4\u63a5\u6210\u50cf\u89c2\u5bdf\u754c\u9762\u6676\u683c\u7684\u5f1b\u8c6b\u548c\u91cd\u5efa\uff0c\u63ed\u793a10\u00b0\u9b54\u89d2\u7684\u6f5c\u5728\u539f\u56e0\u3002<\/p>\n<p><strong>\u539f\u6587\u8be6\u60c5<\/strong>\uff1aZhang, S., Jin, L., Lu, Y. et al. Moir\u00e9 superlattices in twisted two-dimensional halide perovskites. Nat. Mater. (2024). https:\/\/doi.org\/10.1038\/s41563-024-01921-0\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>1.\u3010\u79d1\u5b66\u80cc\u666f\u3011 \u83ab\u5c14\u8d85\u6676\u683c\u901a\u8fc7\u5229\u7528\u7a7a\u95f4\u53d8\u5316\u7684\u5c42\u95f4\u76f8\u4e92\u4f5c\u7528\u6765\u6539\u53d8\u7535\u5b50\u80fd\u5e26\u7ed3\u6784\uff0c\u5df2\u7ecf\u6210\u4e3a\u7814\u7a76\u5f3a\u76f8\u5173\u91cf\u5b50\u73b0\u8c61\u7684\u65b0\u5e73\u53f0\u3002\u5305\u62ec\u8d85\u5bfc\u548c\u83ab\u7279\u7edd\u7f18\u4f53\u5728\u5185\u7684\u5927\u91cf\u91cf\u5b50\u73b0\u8c61\u5df2\u7ecf\u5728\u9b54&#8230;<\/p>\n","protected":false},"author":35692,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-261315","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/261315"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/35692"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=261315"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/261315\/revisions"}],"predecessor-version":[{"id":261323,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/261315\/revisions\/261323"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=261315"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=261315"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=261315"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}