{"id":262829,"date":"2024-09-27T08:30:04","date_gmt":"2024-09-27T00:30:04","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=262829"},"modified":"2024-09-27T08:30:04","modified_gmt":"2024-09-27T00:30:04","slug":"%e5%8d%97%e4%ba%ac%e5%a4%a7%e5%ad%a6%e6%9c%b1%e5%98%89%e5%9b%a2%e9%98%9f%e6%9c%80%e6%96%b0science%ef%bc%9a%e5%88%a9%e7%94%a8%e8%87%aa%e7%84%b6%e9%98%b3%e5%85%89%e4%bb%8e%e7%9b%90%e6%b0%b4%e4%b8%ad","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=262829","title":{"rendered":"\u5357\u4eac\u5927\u5b66\u6731\u5609\u56e2\u961f\u6700\u65b0Science\uff1a\u5229\u7528\u81ea\u7136\u9633\u5149\u4ece\u76d0\u6c34\u4e2d\u63d0\u53d6\u548c\u50a8\u5b58\u9502"},"content":{"rendered":"<p>\u9502\u7535\u6c60\u5728\u53ef\u518d\u751f\u80fd\u6e90\u57fa\u7840\u8bbe\u65bd\u4e2d\u7684\u6838\u5fc3\u5730\u4f4d\u6fc0\u53d1\u4e86\u4eba\u4eec\u5bf9\u66f4\u9ad8\u6548\u7684\u9502\u8d44\u6e90\u83b7\u53d6\u65b9\u6cd5\u7684\u7814\u7a76\u3002\u6d77\u6d0b\u4e2d\u542b\u6709\u5927\u91cf\u7684\u9502\u76d0\uff0c\u4f46\u7531\u4e8e\u6d53\u5ea6\u76f8\u5bf9\u8f83\u4f4e\uff0c\u5f88\u96be\u4ece\u94a0\u548c\u9541\u4e2d\u5206\u79bb\u51fa\u6765\u3002\u968f\u7740\u53ef\u518d\u751f\u6280\u672f\u5bf9\u9502\u7684\u9700\u6c42\u4e0d\u65ad\u589e\u52a0\uff0c\u9502\u63d0\u53d6\u5fc5\u987b\u5bf9\u73af\u5883\u548c\u793e\u4f1a\u8d1f\u8d23\uff0c\u4ee5\u786e\u4fdd\u53ef\u6301\u7eed\u53d1\u5c55\u3002\u76ee\u524d\uff0c\u9502\u4e3b\u8981\u901a\u8fc7\u70ed\u5316\u5b66\u9014\u5f84\u4ece\u786c\u5ca9\u77ff\u77f3\u6216\u901a\u8fc7\u84b8\u53d1\u8fc7\u7a0b\u4ece\u76d0\u6c34\u4e2d\u83b7\u53d6\u300287%\u7684\u9502\u5f00\u91c7\u8bbe\u65bd\u91c7\u7528\u84b8\u53d1\u6cd5\uff0c\u5176\u52a8\u529b\u5b66\u6709\u9650\uff0c\u7528\u6c34\u91cf\u5927\uff0c\u4ec5\u9002\u7528\u4e8e\u9ad8\u6863\u76d0\u6c34\u3002\u4ece\u5404\u79cd\u76d0\u6c34\u4e2d\u63d0\u53d6\u9502\u7684\u53ef\u6301\u7eed\u6280\u672f\u5bf9\u4e8e\u786e\u4fdd\u6e05\u6d01\u53ef\u9760\u7684\u9502\u4f9b\u5e94\u81f3\u5173\u91cd\u8981\u3002<\/p>\n<p>\u5728\u81ea\u7136\u754c\u4e2d\uff0c\u8bb8\u591a\u751f\u547d\u7cfb\u7edf\u5df2\u7ecf\u8fdb\u5316\u5230\u80fd\u591f\u6709\u6548\u5730\u63d0\u53d6\u7279\u5b9a\u7269\u79cd\u3002\u7279\u522b\u662f\u76d0\u751f\u690d\u7269\uff0c\u4e00\u79cd\u5728\u76d0\u78b1\u73af\u5883\u4e2d\u751f\u957f\u7684\u690d\u7269\uff0c\u5df2\u7ecf\u53d1\u5c55\u51fa\u4e00\u79cd\u63d0\u53d6-\u50a8\u5b58-\u91ca\u653e(ESR)\u673a\u5236\uff0c\u53ef\u4ee5\u5728\u4e0d\u53d7\u4f24\u5bb3\u7684\u60c5\u51b5\u4e0b\u4ece\u9ad8\u76d0\u5ea6\u7684\u571f\u58e4\u6216\u6c34\u4e2d\u5438\u6536\u517b\u5206\u3002\u5b83\u4eec\u50cf\u5176\u4ed6\u690d\u7269\u4e00\u6837\u5229\u7528\u84b8\u817e\u4f5c\u7528\u6765\u63d0\u53d6\u8425\u517b\uff0c\u4f46\u5b83\u4eec\u4e5f\u6709\u4e13\u95e8\u7684\u5668\u5b98\u6765\u50a8\u5b58\u548c\u6392\u51fa\u4f53\u5185\u591a\u4f59\u7684\u76d0\u3002\u8fd9\u79cd\u989d\u5916\u7684\u76d0\u50a8\u5b58\u548c\u91ca\u653e\u673a\u5236\u5bf9\u76d0\u751f\u690d\u7269\u5728\u76d0\u6c34\u4e2d\u751f\u5b58\u81f3\u5173\u91cd\u8981\uff0c\u4f7f\u5f97\u76d0\u751f\u690d\u7269\u4e0d\u4f1a\u56e0\u5e72\u65f1\u800c\u6b7b\u4ea1\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-262830\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/0-10.png\" alt=\"\" width=\"1329\" height=\"569\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/0-10.png 1329w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/0-10-300x128.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/0-10-768x329.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/0-10-1024x438.png 1024w\" sizes=\"(max-width: 1329px) 100vw, 1329px\" \/><\/p>\n<p>\u53d7\u5927\u81ea\u7136\u5728\u84b8\u817e\u4f5c\u7528\u4e2d\u9009\u62e9\u6027\u63d0\u53d6\u7269\u79cd\u7684\u80fd\u529b\u7684\u542f\u53d1\uff0c\u8fd1\u65e5\uff0c\u5357\u4eac\u5927\u5b66\u56fa\u4f53\u5fae\u7ed3\u6784\u56fd\u5bb6\u91cd\u70b9\u5b9e\u9a8c\u5ba4\u6731\u5609\u6559\u6388\u4e0e\u7f8e\u56fd\u52a0\u5dde\u5927\u5b66\u4f2f\u514b\u5229\u5206\u6821\u571f\u6728\u4e0e\u73af\u5883\u5de5\u7a0b\u7cfb\u7c73\u5b9d\u971e\u6559\u6388\u56e2\u961f\u5728<strong><em>Science<\/em><\/strong>\u671f\u520a\u4e0a\u53d1\u8868\u9898\u4e3a\u201cSolar transpiration\u2013powered lithium extraction and storage\u201d\u7684\u6587\u7ae0\uff0c\u62a5\u9053\u4e86\u4e00\u79cd\u592a\u9633\u80fd\u84b8\u817e\u9a71\u52a8\u7684\u9502\u63d0\u53d6\u548c\u50a8\u5b58(STLES)\u88c5\u7f6e\uff0c\u8be5\u88c5\u7f6e\u53ef\u4ee5\u5229\u7528\u81ea\u7136\u9633\u5149\u4ece\u76d0\u6c34\u4e2d\u63d0\u53d6\u548c\u50a8\u5b58\u9502\uff0c\u4e0d\u9700\u8981\u8015\u5730\u6216\u8005\u989d\u5916\u7684\u80fd\u6e90\u8f93\u5165\u3002\u5177\u4f53\u6765\u8bf4\uff0c\u8be5\u88c5\u7f6e\u4f7f\u7528\u5206\u5c42\u7ed3\u6784\u7684\u592a\u9633\u80fd\u84b8\u53d1\u5668\u6765\u4ea7\u751f\u538b\u529b\u68af\u5ea6\uff0c\u4ece\u800c\u5141\u8bb8\u4ece\u76d0\u6c34\u4e2d\u63d0\u53d6\u9502\uff0c\u5e76\u5c06\u5176\u50a8\u5b58\u5728\u8840\u7ba1\u50a8\u5b58\u5c42\u4e2d\u3002\u957f\u671f\u5b9e\u9a8c\u3001\u5404\u79cd\u819c\u6d4b\u8bd5\u548c\u4e0d\u540c\u5c3a\u5bf8\u8bc4\u4f30\u8bc1\u660e\u4e86\u8be5\u6750\u6599\u7684\u7a33\u5b9a\u6027\u3001\u517c\u5bb9\u6027\u548c\u53ef\u6269\u5c55\u6027\u3002\u8fd9\u79cd\u592a\u9633\u80fd\u91c7\u77ff\u6280\u672f\u4e3a\u5173\u952e\u8d44\u6e90\u7684\u53ef\u6301\u7eed\u5f00\u91c7\u63d0\u4f9b\u4e86\u53e6\u4e00\u79cd\u53d1\u5c55\u9014\u5f84\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-262831\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/1-5.jpg\" alt=\"\" width=\"4276\" height=\"2957\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/1-5.jpg 4276w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/1-5-300x207.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/1-5-768x531.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/1-5-1024x708.jpg 1024w\" sizes=\"(max-width: 4276px) 100vw, 4276px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe1.\u592a\u9633\u80fd\u84b8\u817e\u9a71\u52a8\u7684\u9502\u63d0\u53d6\u548c\u50a8\u5b58(STLES)\u88c5\u7f6e\u7684\u6982\u5ff5\u4e0e\u8bbe\u8ba1\u00a9 2024 AAAS<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-262832\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/2-5.jpg\" alt=\"\" width=\"4291\" height=\"2673\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/2-5.jpg 4291w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/2-5-300x187.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/2-5-768x478.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/2-5-1024x638.jpg 1024w\" sizes=\"(max-width: 4291px) 100vw, 4291px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe2. \u592a\u9633\u80fd\u84b8\u53d1\u5668\u53ca\u9502\u50a8\u5c42\u7684\u8bbe\u8ba1\u4e0e\u8868\u5f81\u00a9 2024 AAAS<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-262834\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/3-4.jpg\" alt=\"\" width=\"4324\" height=\"3804\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/3-4.jpg 4324w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/3-4-300x264.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/3-4-768x676.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/3-4-1024x901.jpg 1024w\" sizes=\"(max-width: 4324px) 100vw, 4324px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe3. \u5668\u4ef6\u5236\u9020\u53ca\u9502\u63d0\u53d6\u6027\u80fd\u00a9 2024 AAAS<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-262835\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/4-5.jpg\" alt=\"\" width=\"4323\" height=\"2488\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/4-5.jpg 4323w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/4-5-300x173.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/4-5-768x442.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/09\/4-5-1024x589.jpg 1024w\" sizes=\"(max-width: 4323px) 100vw, 4323px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe4. STLES\u7684\u517c\u5bb9\u6027\u548c\u53ef\u6269\u5c55\u6027\u00a9 2024 AAAS<\/p>\n<p>\u8be5\u9879\u5de5\u4f5c\u62a5\u9053\u4e86\u4e00\u79cd STLES \u88c5\u7f6e\u7684\u8bbe\u8ba1\u53ca\u6f14\u793a\uff0c\u8be5\u88c5\u7f6e\u80fd\u591f\u5728\u73af\u5883\u6761\u4ef6\u4e0b\u5229\u7528\u81ea\u7136\u9633\u5149\u4ece\u76d0\u6c34\u4e2d\u63d0\u53d6\u9502\uff0c\u65e0\u9700\u8015\u5730\uff0c\u4e14\u4ea7\u751f\u7684\u6e29\u5ba4\u6c14\u4f53\u8fd1\u4e4e\u4e3a\u96f6\u3002STLES \u76f8\u8f83\u4e8e\u5f53\u524d\u53ca\u65b0\u5174\u7684\u9502\u63d0\u53d6\u65b9\u6cd5\u5177\u6709\u82e5\u5e72\u4f18\u52bf\u3002\u9996\u5148\uff0c\u4e00\u7ecf\u5b89\u88c5\uff0c\u5176\u88ab\u52a8\u6a21\u5f0f\u80fd\u591f\u5b9e\u73b0\u5177\u6709\u6210\u672c\u6548\u76ca\u3001\u80fd\u6e90\u6548\u76ca\u548c\u78b3\u6548\u76ca\u7684\u9502\u5f00\u91c7\u3002\u8fd9\u79cd\u88ab\u52a8\u5de5\u4f5c\u6a21\u5f0f\u4e0d\u4ec5\u964d\u4f4e\u4e86\u8fd0\u8425\u6210\u672c\uff0c\u8fd8\u51cf\u5c11\u4e86\u5bf9\u5916\u90e8\u80fd\u6e90\u4f9b\u5e94\u7684\u4f9d\u8d56\uff0c\u4f7f\u5f97\u6574\u4e2a\u8fc7\u7a0b\u66f4\u52a0\u9ad8\u6548\u548c\u73af\u4fdd\u3002\u5176\u6b21\uff0c\u5b83\u80fd\u591f\u4e0e\u73b0\u6709\u7684\u84b8\u53d1\u6c60\u65e0\u7f1d\u96c6\u6210\uff0c\u800c\u73b0\u6709\u84b8\u53d1\u6c60\u5728 87%\u7684\u9502\u5f00\u91c7\u8bbe\u65bd\u4e2d\u5747\u6709\u5e94\u7528\uff0c\u4ece\u800c\u964d\u4f4e\u4e86\u5b89\u88c5\u6210\u672c\u3002\u8fd9\u4e00\u6574\u5408\u80fd\u529b\u5927\u5e45\u5ea6\u964d\u4f4e\u4e86\u65b0\u7684\u8bbe\u5907\u5b89\u88c5\u6210\u672c\uff0c\u540c\u65f6\u4e5f\u63d0\u9ad8\u4e86\u8d44\u6e90\u5229\u7528\u6548\u7387\uff0c\u6709\u52a9\u4e8e\u52a0\u901f\u6280\u672f\u63a8\u5e7f\u3002\u5176\u4e09\uff0c\u5b83\u80fd\u591f\u6f02\u6d6e\u5728\u76d0\u6c34\u4e0a\uff0c\u51cf\u5c11\u4e86\u571f\u5730\u5360\u7528\u3002\u5728\u5168\u7403\u65e5\u76ca\u7d27\u5f20\u7684\u4eba\u53e3\u538b\u529b\u53ca\u571f\u5730\u8d44\u6e90\u7ade\u4e89\u80cc\u666f\u4e0b\uff0c\u8fd9\u4e00\u70b9\u5c24\u4e3a\u91cd\u8981\u3002\u6b64\u5916\uff0c\u6f02\u6d6e\u5f0f\u7ed3\u6784\u8fd8\u53ef\u80fd\u5e26\u6765\u66f4\u597d\u7684\u70ed\u91cf\u5438\u6536\u6548\u679c\uff0c\u63d0\u9ad8\u6574\u4f53\u80fd\u91cf\u8f6c\u5316\u6548\u7387\u3002\u6700\u540e\uff0c\u9884\u8ba1\u5728 STLES \u4e2d\u4f7f\u7528\u9ad8\u84b8\u817e\u538b\u84b8\u53d1\u5668\uff08\u4f8b\u5982\u6c34\u51dd\u80f6\u819c\uff09\u5c06\u6709\u52a9\u4e8e\u5904\u7406\u6e17\u900f\u538b\u9ad8\u8fbe 400 bar\u7684\u9ad8\u76d0\u76d0\u6c34\uff0c\u8fd9\u4e00\u538b\u529b\u662f\u5f53\u524d\u819c\u8fc7\u6ee4\u7cfb\u7edf\u538b\u529b\u6781\u9650\u7684\u4e94\u500d\u3002\u8fd9\u610f\u5473\u7740\uff0c\u901a\u8fc7\u5f15\u5165\u5148\u8fdb\u6750\u6599\u548c\u6280\u672f\uff0c\u53ef\u4ee5\u663e\u8457\u62d3\u5bbd\u9002\u7528\u4e8e\u4e0d\u540c\u7c7b\u578b\u76d0\u6c34\u6e90\u8fdb\u884c\u9502\u63d0\u53d6\u7684\u65b9\u6cd5\uff0c\u4e3a\u672a\u6765\u5f00\u53d1\u66f4\u591a\u9ad8\u6548\u3001\u7ecf\u6d4e\u4e14\u73af\u4fdd\u7684\u65b0\u578b\u9502\u83b7\u53d6\u9014\u5f84\u5960\u5b9a\u57fa\u7840\u3002\u7efc\u4e0a\u6240\u8ff0\uff0c\u672c\u7814\u7a76\u5c55\u793a\u4e86\u4e00\u79cd\u521b\u65b0\u6027\u7684\u89e3\u51b3\u65b9\u6848\uff0c\u4e0d\u4ec5\u63a8\u52a8\u4e86\u6e05\u6d01\u80fd\u6e90\u6750\u6599\u7684\u53d1\u5c55\uff0c\u4e5f\u4e3a\u5e94\u5bf9\u5168\u7403\u65e5\u76ca\u589e\u957f\u7684\u7535\u52a8\u8f66\u53ca\u50a8\u80fd\u9700\u6c42\u63d0\u4f9b\u4e86\u4e00\u6761\u5207\u5b9e\u53ef\u884c\u4e4b\u8def\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1ahttps:\/\/www.science.org\/doi\/10.1126\/science.adm7034<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u9502\u7535\u6c60\u5728\u53ef\u518d\u751f\u80fd\u6e90\u57fa\u7840\u8bbe\u65bd\u4e2d\u7684\u6838\u5fc3\u5730\u4f4d\u6fc0\u53d1\u4e86\u4eba\u4eec\u5bf9\u66f4\u9ad8\u6548\u7684\u9502\u8d44\u6e90\u83b7\u53d6\u65b9\u6cd5\u7684\u7814\u7a76\u3002\u6d77\u6d0b\u4e2d\u542b\u6709\u5927\u91cf\u7684\u9502\u76d0\uff0c\u4f46\u7531\u4e8e\u6d53\u5ea6\u76f8\u5bf9\u8f83\u4f4e\uff0c\u5f88\u96be\u4ece\u94a0\u548c\u9541\u4e2d\u5206\u79bb\u51fa\u6765\u3002\u968f\u7740\u53ef\u518d\u751f\u6280\u672f&#8230;<\/p>\n","protected":false},"author":35295,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-262829","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/262829"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/35295"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=262829"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/262829\/revisions"}],"predecessor-version":[{"id":262839,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/262829\/revisions\/262839"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=262829"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=262829"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=262829"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}