{"id":264165,"date":"2025-01-20T09:27:47","date_gmt":"2025-01-20T01:27:47","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=264165"},"modified":"2025-01-20T09:27:47","modified_gmt":"2025-01-20T01:27:47","slug":"%e6%9c%80%e6%96%b0nature-catalysis%ef%bc%9a%e8%81%9a%e5%90%88%e7%89%a9%e4%bf%ae%e9%a5%b0%e6%b4%bb%e7%bb%86%e8%83%9e%e5%ae%9e%e7%8e%b0%e5%8f%af%e5%9b%9e%e6%94%b6%e5%85%89%e9%85%b6%e5%82%ac%e5%8c%96","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=264165","title":{"rendered":"\u6700\u65b0Nature Catalysis\uff1a\u805a\u5408\u7269\u4fee\u9970\u6d3b\u7ec6\u80de\u5b9e\u73b0\u53ef\u56de\u6536\u5149\u9176\u50ac\u5316"},"content":{"rendered":"<p style=\"text-align: center;\">01\u3010\u79d1\u5b66\u80cc\u666f\u3011<\/p>\n<p>\u5728\u81ea\u7136\u754c\u4e2d\uff0c\u7ec6\u80de\u5df2\u7ecf\u8fdb\u5316\u5230\u80fd\u591f\u5728\u5176\u819c\u5185\u7ec4\u88c5\u5177\u6709\u50ac\u5316\u6d3b\u6027\u7684\u751f\u7269\u5927\u5206\u5b50\uff0c\u4fc3\u8fdb\u591a\u79cd\u9176\u4ecb\u5bfc\u7684\u53cd\u5e94\uff0c\u4f7f\u5e95\u7269\u53ef\u4ee5\u76f4\u63a5\u63a5\u89e6\u50ac\u5316\u5242\uff0c\u7ed5\u8fc7\u8de8\u7ec6\u80de\u819c\u7684\u4f20\u8d28\u963b\u529b\uff0c\u5bf9\u4e8e\u52a0\u901f\u5236\u836f\u548c\u53d1\u9175\u5de5\u4e1a\u7684\u751f\u7269\u8f6c\u5316\u5177\u6709\u91cd\u5927\u610f\u4e49\u3002\u4f8b\u5982\uff0c\u54fa\u4e73\u52a8\u7269\u7684\u7ec6\u80de\u819c\u542b\u6709\u5929\u51ac\u6c28\u9178N-\u4e59\u9170\u8f6c\u79fb\u9176\u3001\u5f17\u6797\u86cb\u767d\u9176\u548c\u4eba\u916a\u6c28\u9178\u9176\uff0c\u5b83\u4eec\u50ac\u5316\u5408\u6210\u529f\u80fd\u86cb\u767d\u6240\u9700\u7684\u91cd\u8981\u6c28\u57fa\u9178\u3002\u53e6\u4e00\u65b9\u9762\uff0c\u7ec6\u83cc\u7ec6\u80de\u819c\u4e2d\u542b\u6709\u8102\u8d28A\u4e8c\u7cd6\u8131\u6c22\u9176\u3001\u9187\u8131\u6c22\u9176 (ADH) \u548c\u919b\u8131\u6c22\u9176 (ALDH)\uff0c\u5b83\u4eec\u8d1f\u8d23\u5c06\u5404\u79cd\u8425\u517b\u7269\u8d28\u8f6c\u5316\u4e3a\u652f\u6301\u751f\u547d\u8fc7\u7a0b\u7684\u5173\u952e\u5316\u5408\u7269\u3002\u8fd9\u4e9b\u81ea\u7136\u8fdb\u5316\u7684\u7cfb\u7edf\u5141\u8bb8\u5e95\u7269\u76f4\u63a5\u63a5\u89e6\u50ac\u5316\u5242\uff0c\u7ed5\u8fc7\u8de8\u7ec6\u80de\u819c\u7684\u4f20\u8d28\u963b\u529b\uff0c\u8fd9\u4e00\u4f18\u52bf\u5bf9\u52a0\u901f\u5236\u836f\u548c\u53d1\u9175\u884c\u4e1a\u7684\u751f\u7269\u8f6c\u5316\u5177\u6709\u91cd\u8981\u610f\u4e49\u3002\u7136\u800c, \u5929\u7136\u751f\u7269\u50ac\u5316\u5242\u5df2\u7ecf\u8fdb\u5316\u7528\u4e8e\u7279\u5b9a\u7684\u751f\u7269\u76ee\u7684, \u56e0\u6b64\u8868\u73b0\u51fa\u6709\u9650\u7684\u79cd\u7c7b\u548c\u529f\u80fd, \u4f7f\u5f97\u5b83\u4eec\u4e0d\u9002\u5408\u4e8e\u5e7f\u6cdb\u7684\u5de5\u4e1a\u5e94\u7528\u3002\u4e3a\u4e86\u89e3\u51b3\u8fd9\u4e9b\u9650\u5236, \u7814\u7a76\u4eba\u5458\u5df2\u7ecf\u5f00\u53d1\u4e86\u9057\u4f20\u548c\u5316\u5b66\u5de5\u7a0b\u7b56\u7565, \u7528\u4e8e\u5c06\u611f\u5174\u8da3\u7684\u751f\u7269\u5927\u5206\u5b50\uff08\u4ece\u5929\u7136\u5230\u4eba\u5de5\u9176\uff09\u7ed3\u5408\u5230\u7ec6\u80de\u8868\u9762\u4ee5\u8fbe\u5230\u50ac\u5316\u76ee\u7684, \u4f8b\u5982\u6709\u673a\u78f7\u519c\u836f\u964d\u89e3, \u751f\u7269\u67f4\u6cb9\u7684\u5408\u6210\u7b49\u3002\u5c3d\u7ba1\u53d6\u5f97\u4e86\u76f8\u5f53\u5927\u7684\u8fdb\u5c55, \u4f46\u4e0e\u7ec6\u80de\u5185\u7684\u91cd\u7ec4\u9176\u76f8\u6bd4, \u5de5\u7a0b\u819c\u76f8\u5173\u751f\u7269\u5927\u5206\u5b50\u901a\u5e38\u8868\u73b0\u51fa\u8f83\u4f4e\u7684\u8868\u8fbe\u6c34\u5e73\uff0c\u5bfc\u81f4\u50ac\u5316\u5242\u4f9b\u5e94\u4e0d\u8db3\u3002\u6b64\u5916, \u7531\u4e8e\u76f4\u63a5\u66b4\u9732\u4e8e\u73af\u5883\u5e94\u529b, \u5982\u7d2b\u5916\u7ebf\u8f90\u5c04\u3001 \u6709\u673a\u6eb6\u5242\u548c\u9ad8\u6e29, \u5b83\u4eec\u7684\u7a33\u5b9a\u6027\u5f80\u5f80\u53d7\u5230\u635f\u5bb3, \u8fd9\u5728\u5de5\u4e1a\u8fc7\u7a0b\u4e2d\u662f\u5e38\u89c1\u7684\u3002\u56e0\u6b64, \u63d0\u9ad8\u8fd9\u4e9b\u751f\u7269\u5927\u5206\u5b50\u7684\u53cd\u5e94\u6027\u4ee5\u5b9e\u73b0\u7a33\u5065\u4e14\u65b0\u9896\u7684\u5316\u5b66\u8f6c\u5316\u4ecd\u7136\u662f\u4e00\u4e2a\u7d27\u8feb\u7684\u6311\u6218\u3002\u6700\u8fd1\uff0c\u591a\u529f\u80fd\u805a\u5408\u7269\u7ed3\u5408\u4e86\u63a5\u679d\u548c\u63a5\u679d\u7684\u65b9\u6cd5\uff0c\u4f7f\u514d\u75ab\u4fdd\u62a4\u548c\u9009\u62e9\u6027\u5fae\u751f\u7269\u7ed3\u5408\u7b49\u5e94\u7528\u6210\u4e3a\u53ef\u80fd\u3002\u7136\u800c\uff0c\u5c3d\u7ba1\u6d3b\u6027\u5408\u6210\u5927\u5206\u5b50\u5728\u4fc3\u8fdb\u751f\u7269\u8f6c\u5316\u65b9\u9762\u5177\u6709\u6f5c\u529b\uff0c\u4f46\u5b83\u4eec\u5728\u7ec6\u80de\u819c\u4e0a\u4e0e\u7ec6\u80de\u4e2d\u7684\u91cd\u7ec4\u9176\u7ed3\u5408\u7528\u4e8e\u50ac\u5316\u76ee\u7684\u7684\u5e94\u7528\u4ecd\u672a\u5f97\u5230\u5145\u5206\u7684\u63a2\u7d22\u3002\u7f3a\u4e4f\u8fdb\u5c55\u7684\u4e00\u4e2a\u4e3b\u8981\u539f\u56e0\u662f\uff0c\u5728\u4fdd\u6301\u751f\u7269\u76f8\u5bb9\u6027\u548c\u7ec6\u80de\u529f\u80fd\u7684\u540c\u65f6\uff0c\u5982\u4f55\u6709\u6548\u5730\u5c06\u5408\u6210\u5927\u5206\u5b50\u5ac1\u63a5\u5230\u7ec6\u80de\u819c\u4e0a\u5b58\u5728\u6311\u6218\u3002<\/p>\n<p style=\"text-align: center;\">02\u3010\u521b\u65b0\u6210\u679c\u3011<\/p>\n<p>\u9488\u5bf9\u4ee5\u4e0a\u95ee\u9898\uff0c\u8fd1\u65e5\uff0c\u5357\u4e39\u9ea6\u5927\u5b66\u5434\u660c\u67f1\u6559\u6388\u56e2\u961f\u5728\u300aNature Catalysis\u300b\u4e0a\u53d1\u8868\u4e86\u9898\u4e3a\u201cEngineering living cells with polymers for recyclable photoenzymatic catalysis\u201d\u7684\u6587\u7ae0\uff0c\u8be5\u9879\u7814\u7a76\u63d0\u51fa\u4e86\u4e00\u79cd\u901a\u8fc7\u5408\u6210\u50ac\u5316\u805a\u5408\u7269\u5de5\u7a0b\u5316\u7ec6\u80de\u819c\u7684\u6982\u5ff5\u9a8c\u8bc1\uff0c\u5728\u7ec6\u80de\u819c\u4e0a\u4fee\u9970\u50ac\u5316\u805a\u5408\u7269\uff0c\u4ece\u800c\u5b9e\u73b0\u5149\u9176\u50ac\u5316\uff0c\u514b\u670d\u7ec6\u80de\u819c\u5de5\u7a0b\u5316\u7684\u56f0\u96be\u548c\u6311\u6218\uff0c\u5f97\u5230\u7a33\u5065\u3001\u53ef\u5faa\u73af\u5229\u7528\u7684\u5149\u9176\u50ac\u5316\u5242\u3002\u8be5\u9879\u5de5\u4f5c\u5728\u5927\u80a0\u6746\u83cc\u4e0a\u901a\u8fc7\u4e00\u6b65\u539f\u4f4d\u539f\u5b50\u8f6c\u79fb\u81ea\u7531\u57fa\u805a\u5408\uff0c\u5728\u7ec6\u80de\u5f62\u6210\u5177\u6709\u4fdd\u62a4\u80fd\u529b\u7684\u805a\u5408\u7269\u5c42\uff0c\u4fdd\u62a4\u7ec6\u80de\u514d\u53d7\u73af\u5883\u538b\u529b\u7684\u5f71\u54cd\uff0c\u4fc3\u8fdb\u9176\u50ac\u5316\u53cd\u5e94\u3002\u4f5c\u4e3a\u6982\u5ff5\u9a8c\u8bc1\uff0c\u8be5\u9879\u7814\u7a76\u5c55\u793a\u4e86\u4e00\u79cd\u57fa\u4e8e\u84bd\u918c\u805a\u5408\u7269\u548c\u82ef\u7532\u919b\u88c2\u89e3\u9176\u7684\u5149\u9176\u7ea7\u8054\u53cd\u5e94\uff0c\u5c06\u82ef\u7532\u9187\u8f6c\u5316\u4e3a\u82ef\u5076\u59fb\uff0c\u5e76\u5b9e\u73b0\u4e86\u6bd4\u5bf9\u7167\u7ec4\u9ad815\u500d\u7684\u751f\u7269\u8f6c\u5316\u7387\u3002\u6b64\u5916\uff0c\u7ec6\u80de\u4f5c\u4e3a\u805a\u5408\u7269\u7684\u5de8\u5927\u751f\u7269\u652f\u67b6\uff0c\u4f7f\u5927\u5206\u5b50\u50ac\u5316\u5242\u80fd\u591f\u5faa\u73af\u5229\u7528\u3002\u8fd9\u4e00\u6210\u679c\u5728\u5408\u6210\u5316\u5b66\u3001\u805a\u5408\u7269\u5316\u5b66\u548c\u751f\u7269\u6280\u672f\u9886\u57df\u6253\u5f00\u4e86\u65b0\u7684\u524d\u666f\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-264166\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/0-8.png\" alt=\"\" width=\"1090\" height=\"672\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/0-8.png 1090w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/0-8-300x185.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/0-8-768x473.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/0-8-1024x631.png 1024w\" sizes=\"(max-width: 1090px) 100vw, 1090px\" \/><\/p>\n<p style=\"text-align: center;\">03\u3010\u6570\u636e\u6982\u89c8\u3011<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-264167\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/1-10.png\" alt=\"\" width=\"1268\" height=\"1378\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/1-10.png 1268w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/1-10-276x300.png 276w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/1-10-768x835.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/1-10-942x1024.png 942w\" sizes=\"(max-width: 1268px) 100vw, 1268px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe1.\u00a0\u805a\u5408\u7269\u63a5\u679d\u7ec6\u80de\u7684\u5236\u5907\u53ca\u5176\u5728\u5316\u5b66\u9176\u7ea7\u8054\u53cd\u5e94\u4e2d\u7684\u5e94\u7528\u00a9 2024 Springer Nature<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-264168\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/2-10.png\" alt=\"\" width=\"1267\" height=\"1999\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/2-10.png 1267w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/2-10-190x300.png 190w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/2-10-768x1212.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/2-10-649x1024.png 649w\" sizes=\"(max-width: 1267px) 100vw, 1267px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe2.\u00a0\u63a5\u679d\u805a\u5408\u7269\u7684\u7279\u6027\u53ca\u5176\u5728\u7ec6\u80de\u8868\u9762\u7684\u5206\u5e03\u00a9 2024 Springer Nature<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-264169\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/3-10.png\" alt=\"\" width=\"1268\" height=\"1578\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/3-10.png 1268w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/3-10-241x300.png 241w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/3-10-768x956.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/3-10-823x1024.png 823w\" sizes=\"(max-width: 1268px) 100vw, 1268px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe3.\u00a0\u805a\u5408\u7269\u63a5\u679d\u5927\u80a0\u6746\u83cc\u7ec6\u80de\u7684\u6d3b\u529b\u548c\u589e\u6b96\u7814\u7a76\u00a9 2024 Springer Nature<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-264170\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/4-9.png\" alt=\"\" width=\"1267\" height=\"1185\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/4-9.png 1267w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/4-9-300x281.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/4-9-768x718.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/4-9-1024x958.png 1024w\" sizes=\"(max-width: 1267px) 100vw, 1267px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe4.\u00a0\u63a5\u679d\u805a\u5408\u7269\u5927\u80a0\u6746\u83cc\u7ec6\u80de\u7684\u76f8\u5bb9\u6027\u8bc4\u4ef7\u00a9 2024 Springer Nature<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-264171\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/5-7.png\" alt=\"\" width=\"1270\" height=\"614\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/5-7.png 1270w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/5-7-300x145.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/5-7-768x371.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/5-7-1024x495.png 1024w\" sizes=\"(max-width: 1270px) 100vw, 1270px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe5.\u00a0\u805a\u5408\u7269\u5bf9\u5916\u90e8\u5e94\u529b\u73af\u5883\u7684\u4fdd\u62a4\u00a9 2024 Springer Nature<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-264172\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/6-2.png\" alt=\"\" width=\"1270\" height=\"1635\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/6-2.png 1270w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/6-2-233x300.png 233w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/6-2-768x989.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/6-2-795x1024.png 795w\" sizes=\"(max-width: 1270px) 100vw, 1270px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe6.\u00a0\u805a\u5408\u7269\u63a5\u679d\u5927\u80a0\u6746\u83cc\u7ec6\u80de\u7684\u5149\u9176\u7ea7\u8054\u53cd\u5e94\u00a9 2024 Springer Nature<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-264173\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/7-1.png\" alt=\"\" width=\"1267\" height=\"1301\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/7-1.png 1267w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/7-1-292x300.png 292w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/7-1-768x789.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2024\/12\/7-1-997x1024.png 997w\" sizes=\"(max-width: 1267px) 100vw, 1267px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe7.\u00a0\u805a\u5408\u7269\u79fb\u690d\u7684\u5927\u80a0\u6746\u83cc\u7ec6\u80de\u7684\u5316\u5b66\u9176\u7ea7\u8054\u7814\u7a76\u00a9 2024 Springer Nature<\/p>\n<p style=\"text-align: center;\">04\u3010\u79d1\u5b66\u542f\u8fea\u3011<\/p>\n<p>\u8be5\u9879\u5de5\u4f5c\u901a\u8fc7\u5c06\u5408\u6210\u5927\u5206\u5b50\u6574\u5408\u5230\u7ec6\u80de\u819c\u4e0a\uff0c\u8bbe\u8ba1\u4e86\u4e00\u79cd\u5316\u5b66\u5de5\u7a0b\u5927\u80a0\u6746\u83cc\u7ec6\u80de\u7684\u539f\u7406\u9a8c\u8bc1\u7b56\u7565\uff0c\u4e3a\u5316\u5b66\u5de5\u7a0b\u7ec6\u80de\u63d0\u4f9b\u4e86\u4e00\u4e2a\u7b80\u5355\u7684\u5e73\u53f0\u6280\u672f\uff0c\u5141\u8bb8\u5176\u4ed6\u7ec6\u80de\u548c\u805a\u5408\u7269\u7684\u7ec4\u5408\u6765\u89e3\u51b3\u751f\u7269\u533b\u5b66\u548c\u751f\u7269\u8f6c\u5316\u9886\u57df\u7684\u6311\u6218\uff0c\u4e3a\u65b0\u7684\u81ea\u7136\u5e94\u7528\u94fa\u5e73\u4e86\u9053\u8def\u3002\u8fd9\u9879\u539f\u7406\u9a8c\u8bc1\u7814\u7a76\u5229\u7528\u8be5\u65b9\u6cd5\u7684\u7b80\u4fbf\u6027\u548c\u4fdd\u62a4\u6027\uff0c\u63a2\u7d22\u4e86\u805a\u5408\u7269\u63a5\u679d\u7ec6\u80de\u5728\u5316\u5b66\u9176\u4fc3\u7ea7\u8054\u53cd\u5e94\u4e2d\u7684\u5e94\u7528\uff0c\u5c06\u4e24\u79cd\u805a\u5408\u7269\u50ac\u5316\u5242\u4e0e\u7ec6\u80de\u4e2d\u4e09\u79cd\u8fc7\u8868\u8fbe\u7684\u9176\u7ed3\u5408\u8d77\u6765\uff0c\u5b9e\u73b0\u4e86\u589e\u503c\u4e0d\u5bf9\u79f0\u5408\u6210\uff0c\u6db5\u76d6\u4e86\u4ece\u5355\u6b65\u53cd\u5e94\u5230\u591a\u6b65\u7ea7\u8054\u53cd\u5e94\u7684\u8303\u56f4\u3002\u6b64\u5916\uff0c\u8fd9\u4e9b\u7ec6\u80de\u4f5c\u4e3a\u805a\u5408\u7269\u50ac\u5316\u5242\u7684\u751f\u7269\u8f7d\u4f53\uff0c\u4fc3\u8fdb\u4e86\u50ac\u5316\u5242\u7684\u6709\u6548\u5faa\u73af\u5229\u7528\u3002\u805a\u5408\u7269\u5de5\u7a0b\u7b56\u7565\u53ef\u4ee5\u8fdb\u4e00\u6b65\u5b8c\u5584\u6210\u4e3a\u4e00\u79cd\u901a\u7528\u7684\u53ef\u56de\u6536\u5316\u5b66\u9176\u50ac\u5316\u65b9\u6cd5\uff0c\u4e3a\u53ef\u6301\u7eed\u5316\u5b66\u7684\u672a\u6765\u505a\u51fa\u8d21\u732e\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<\/p>\n<p>https:\/\/www.nature.com\/articles\/s41929-024-01259-5<\/p>\n","protected":false},"excerpt":{"rendered":"<p>01\u3010\u79d1\u5b66\u80cc\u666f\u3011 \u5728\u81ea\u7136\u754c\u4e2d\uff0c\u7ec6\u80de\u5df2\u7ecf\u8fdb\u5316\u5230\u80fd\u591f\u5728\u5176\u819c\u5185\u7ec4\u88c5\u5177\u6709\u50ac\u5316\u6d3b\u6027\u7684\u751f\u7269\u5927\u5206\u5b50\uff0c\u4fc3\u8fdb\u591a\u79cd\u9176\u4ecb\u5bfc\u7684\u53cd\u5e94\uff0c\u4f7f\u5e95\u7269\u53ef\u4ee5\u76f4\u63a5\u63a5\u89e6\u50ac\u5316\u5242\uff0c\u7ed5\u8fc7\u8de8\u7ec6\u80de\u819c\u7684\u4f20\u8d28\u963b\u529b\uff0c\u5bf9&#8230;<\/p>\n","protected":false},"author":35295,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-264165","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/264165"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/35295"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=264165"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/264165\/revisions"}],"predecessor-version":[{"id":264554,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/264165\/revisions\/264554"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=264165"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=264165"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=264165"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}