{"id":264570,"date":"2025-01-22T10:13:40","date_gmt":"2025-01-22T02:13:40","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=264570"},"modified":"2025-01-22T10:13:40","modified_gmt":"2025-01-22T02:13:40","slug":"nature-materials%ef%bc%9a%e6%97%a0%e9%98%b3%e6%9e%81%e5%9b%ba%e6%80%81%e7%94%b5%e6%b1%a0%e7%9a%84%e7%94%b5%e5%8c%96%e5%ad%a6%e5%8a%9b%e5%ad%a6","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=264570","title":{"rendered":"Nature Materials\uff1a\u65e0\u9633\u6781\u56fa\u6001\u7535\u6c60\u7684\u7535\u5316\u5b66\u529b\u5b66"},"content":{"rendered":"<p>\u5f20\u7199\u7199<\/p>\n<p>\u4e00\u3001 \u3010\u79d1\u5b66\u80cc\u666f\u3011 <strong>\u00a0\u00a0<\/strong><\/p>\n<p>\u9502\u79bb\u5b50\u7535\u6c60\u63a8\u52a8\u4e86\u6d88\u8d39\u7535\u5b50\u4ea7\u54c1\u7684\u53d1\u5c55\uff0c\u52a0\u901f\u4e86\u7535\u52a8\u6c7d\u8f66\u7684\u666e\u53ca\u3002\u4f46\u662f\u76ee\u524d\u7684\u9502\u79bb\u5b50\u7535\u6c60\u6280\u672f\u4ecd\u96be\u4ee5\u6ee1\u8db3\u91cd\u578b\u8f66\u8f86\u548c\u7535\u52a8\u98de\u884c\u5668\u7b49\u9886\u57df\u7684\u8981\u6c42\u3002\u56fa\u6001\u7535\u6c60\uff08SSBs\uff09\u4f7f\u7528\u56fa\u6001\u7535\u89e3\u8d28\uff08SSE\uff09\u53d6\u4ee3\u6db2\u4f53\u7535\u89e3\u8d28\uff0c\u53ef\u4ee5\u4f7f\u7528\u66f4\u5b89\u5168\u66f4\u9ad8\u5bb9\u91cf\u7684\u7535\u6781\uff08\u5982\u9502\u91d1\u5c5e\uff09\uff0c\u4ece\u800c\u5c55\u73b0\u51fa\u80fd\u91cf\u5bc6\u5ea6\u6bd4\u73b0\u6709\u7684\u9502\u79bb\u5b50\u7535\u6c60\u9ad8\u51fa50%\u7684\u5de8\u5927\u4f18\u52bf\u3002\u6b64\u5916\uff0cSSBs\u5728\u907f\u514d\u6613\u71c3\u65b9\u9762\uff0c\u5373\u6539\u8fdb\u5b89\u5168\u6027\u65b9\u9762\uff0c\u4e5f\u5177\u6709\u6781\u5927\u7684\u4f18\u52bf\u3002\u7136\u800c\uff0c\u9502\u91d1\u5c5e\u9633\u6781\u63d0\u4f9b\u4e86\u5353\u8d8a\u7684\u80fd\u91cf\u5bc6\u5ea6\u7684\u540c\u65f6\uff0c\u9502\u7b94\u4e25\u683c\u7684\u5236\u5907\u73af\u5883\uff0c\u9700\u8981\u9ad8\u6602\u7684\u6210\u672c\u3002\u65e0\u9633\u6781SSB\u4e3a\u8fd9\u4e00\u95ee\u9898\u63d0\u4f9b\u4e86\u4e00\u4e2a\u6f5c\u5728\u7684\u89e3\u51b3\u65b9\u6848\uff0c\u540c\u65f6\u5b9e\u73b0\u4e86\u66f4\u9ad8\u7684\u80fd\u91cf\u5bc6\u5ea6\u3002\u201c\u65e0\u9633\u6781\u201d\u8fd9\u4e00\u672f\u8bed\u6307\u7684\u662f\u5728\u7535\u6c60\u7ec4\u88c5\u65f6\u8d1f\u6781\u6ca1\u6709\u989d\u5916\u7684\u9502\u91d1\u5c5e\u5b58\u5728\u3002 \u8fd9\u79cd\u67b6\u6784\u4e5f\u88ab\u79f0\u4e3a\u201c\u65e0\u8d1f\u6781\u201d\u3001\u201c\u65e0\u50a8\u9502\u201d\u6216\u201c\u96f6\u9502\u201d\u3002\u3002<\/p>\n<p>\u5728\u65e0\u9633\u6781SSB\u4e2d\uff0c\u5b8c\u5168\u9502\u5316\uff08\u653e\u7535\uff09\u7684\u9634\u6781\u6d3b\u6027\u6750\u6599\uff0c\u5982LiNi<sub>0.8<\/sub>Co<sub>0.1<\/sub>Mn<sub>0.1<\/sub>O<sub>2<\/sub>\uff0c\u4e0e\u8d1f\u6781SSE\u754c\u9762\u5904\u4e0d\u5b58\u5728\u8fc7\u91cf\u9502\u91d1\u5c5e\u7684\u96c6\u6d41\u4f53\u914d\u5bf9\u3002\u91d1\u5c5e\u9502\u5728\u5145\u7535\u65f6\u88ab\u9540\u5728\u96c6\u6d41\u4f53\u4e0a\uff0c\u653e\u7535\u65f6\u88ab\u5265\u79bb\u3002\u7531\u4e8e\u67d0\u4e9b\u56fa\u6001\u7535\u6c60\u4e0e\u9502\u91d1\u5c5e\u5177\u6709\u826f\u597d\u7684\u754c\u9762\u7a33\u5b9a\u6027\uff0c\u5e76\u4e14\u56fa\u4f53-\u7535\u89e3\u8d28\u754c\u9762\u76f8\uff08SEI\uff09\u7684\u5f62\u6210\u5728\u7a7a\u95f4\u4e0a\u4ecd\u7136\u5c40\u9650\u4e8e\u8be5\u5e73\u9762\u754c\u9762\uff0c\u56e0\u6b64\u65e0\u9633\u6781SSB\u53ef\u4ee5\u8bf4\u6bd4\u65e0\u9633\u6781\u6db2\u6001\u7535\u6c60\u66f4\u6709\u524d\u9014\uff0c\u56e0\u4e3a\u65e0\u9633\u6781\u6db2\u6001\u7535\u6c60\u5728\u6bcf\u4e2a\u5145\u653e\u7535\u5468\u671f\u4e2d\u90fd\u503e\u5411\u4e8e\u6301\u7eed\u5f62\u6210SEI\u3002<\/p>\n<p>\u5e38\u89c4\u9502\u8fc7\u91cfSSBs\u7684\u6027\u80fd\u5728\u5f88\u5927\u7a0b\u5ea6\u4e0a\u53d6\u51b3\u4e8e\u9502SSE\u754c\u9762\u7684\u52a8\u6001\u6f14\u53d8\u3002\u5728\u7535\u6c60\u653e\u7535\u8fc7\u7a0b\u4e2d\uff0c\u9502\u4ece\u754c\u9762\u4e0a\u88ab\u79fb\u9664\uff08\u5265\u79bb\uff09\uff0c\u5982\u679c\u8fd9\u4e2a\u8fc7\u7a0b\u53d1\u751f\u5f97\u592a\u5feb\uff0c\u65e0\u6cd5\u8865\u5145\u8017\u5c3d\u7684\u9502\uff0c\u5c31\u4f1a\u5f62\u6210\u7a7a\u9699\uff0c\u5bfc\u81f4\u754c\u9762\u63a5\u89e6\u635f\u5931\u548c\u9ad8\u963b\u6297\u3002\u8fd9\u79cd\u5f62\u5f0f\u7684\u754c\u9762\u63a5\u89e6\u635f\u5931\u53d1\u751f\u5728\u56fa\u6001\u7535\u6c60\u4e2d\uff0c\u800c\u4e0d\u5728\u6db2\u6001\u7535\u89e3\u8d28\u7535\u6c60\u4e2d\u53d1\u751f\uff0c\u5b83\u4f1a\u5f3a\u70c8\u5f71\u54cd\u5faa\u73af\u884c\u4e3a\u3002\u5728\u968f\u540e\u7684\u5145\u7535\u4e2d\uff0c\u4e0d\u5b8c\u7f8e\u7684\u63a5\u89e6\u4f1a\u5bfc\u81f4\u4e0d\u5747\u5300\u7684\u9502\u6c89\u79ef\uff0c\u5728\u7a7a\u9699\u5468\u56f4\u7684\u7535\u6d41\u6d53\u5ea6\u4f1a\u5bfc\u81f4\u679d\u6676\u548c\u4e1d\u72b6\u751f\u957f\uff0c\u4ece\u800c\u7a7f\u900fSSE\u5e76\u5bfc\u81f4\u77ed\u8def\u3002<\/p>\n<p>\u4e0e\u9502\u8fc7\u91cfSSBs\u4e00\u6837\uff0c\u65e0\u9633\u6781SSBs\u7684\u884c\u4e3a\u5728\u5f88\u5927\u7a0b\u5ea6\u4e0a\u53d6\u51b3\u4e8e\u754c\u9762\u6f14\u5316\u548c\u964d\u89e3\u73b0\u8c61\u3002\u7136\u800c\uff0c\u4e0e\u9502\u8fc7\u91cf\u7684\u60c5\u51b5\u76f8\u53cd\uff0c\u65e0\u9633\u6781\u7cfb\u7edf\u5bf9\u5176\u4ed6\u56e0\u7d20\u654f\u611f\u3002\u7a7a\u95f4\u5747\u5300\u7684\u9540\u9502\u548c\u5265\u79bb\u9502\u662f\u9632\u6b62\u5faa\u73af\u8fc7\u7a0b\u4e2d\u7535\u6d41\u6d53\u5ea6\u7684\u7406\u60f3\u9009\u62e9\u3002\u4e3a\u4e86\u5b9e\u73b0\u9ad8\u80fd\u91cf\u5bc6\u5ea6\u548c\u957f\u5faa\u73af\u5bff\u547d\uff0c\u65e0\u9633\u6781\u7535\u6c60\u7684\u5e93\u4ed1\u6548\u7387\uff08CE\uff09\u5e94\u8be5\u975e\u5e38\u9ad8\uff08&gt;99.95%\uff09\uff0c\u56e0\u4e3a\u7cfb\u7edf\u4e2d\u6ca1\u6709\u591a\u4f59\u7684\u9502\u6765\u8865\u5145\u4efb\u4f55\u56e0\u526f\u53cd\u5e94\u800c\u635f\u5931\u7684\u9502\u3002\u8fd9\u4e9b\u56e0\u7d20\u90fd\u4e0e\u65e0\u9633\u6781SSBs\u7684\u57fa\u672c\u7535\u5316\u5b66\u529b\u5b66\u73b0\u8c61\u6709\u5173\u3002<\/p>\n<p><strong>\u4e8c\u3001\u3010<\/strong>\u521b\u65b0\u6210\u679c<strong>\u3011<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-264571\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/1-8.png\" alt=\"\" width=\"1001\" height=\"590\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/1-8.png 1001w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/1-8-300x177.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/1-8-768x453.png 768w\" sizes=\"(max-width: 1001px) 100vw, 1001px\" \/>\u8fd1\u65e5\uff0c\u6765\u81ea\u4f50\u6cbb\u4e9a\u7406\u5de5\u5b66\u9662\u7684Matthew T. McDowell\u2009\u7b49\u7814\u7a76\u8005\u5728<em>Nature Materials<\/em>\u671f\u520a\u53d1\u8868\u4e86\u9898\u4e3a\u201c<strong>Electro-chemo-mechanics of anode-free <\/strong><strong>solid-state batteries<\/strong>\u201d\u7684\u8bba\u6587\uff0c\u8be5\u9879\u7814\u7a76\u6982\u8ff0\u4e86\u5728\u65e0\u9633\u6781\u56fa\u6001\u7535\u6c60\u4e2d\u63a7\u5236\u9502\u6210\u6838\u3001\u751f\u957f\u3001\u5265\u79bb\u548c\u5faa\u73af\u7684\u56e0\u7d20\uff0c\u5305\u62ec\u9502\u7684\u673a\u68b0\u53d8\u5f62\u3001\u96c6\u6d41\u4f53\u7684\u5316\u5b66\u548c\u673a\u68b0\u6027\u80fd\u3001\u5fae\u89c2\u7ed3\u6784\u6548\u5e94\u548c\u5265\u79bb\u52a8\u529b\u5b66\u3002\u8ba8\u8bba\u4e86\u5de5\u7a0b\u63a5\u53e3\u6700\u5927\u5316\u6027\u80fd\u548c\u5ef6\u957f\u7535\u6c60\u5bff\u547d\u7684\u9014\u5f84\u3002\u6700\u540e\uff0c\u4f5c\u8005\u63d0\u51fa\u4e86\u4e00\u4e9b\u5173\u952e\u7684\u7814\u7a76\u95ee\u9898\uff0c\u5305\u62ec\u4e86\u89e3\u4f4e\u5806\u53e0\u538b\u529b\u4e0b\u7684\u884c\u4e3a\uff0c\u8c03\u6574\u754c\u9762\u751f\u957f\uff0c\u4ee5\u53ca\u8bbe\u8ba1\u7535\u6d41\u6536\u96c6\u5668\u548c\u4e2d\u95f4\u5c42\u3002<\/p>\n<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-264572\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/2-8.png\" alt=\"\" width=\"428\" height=\"167\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/2-8.png 428w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/2-8-300x117.png 300w\" sizes=\"(max-width: 428px) 100vw, 428px\" \/><\/strong><\/p>\n<p><strong>\u56fe<\/strong><strong>1\u00a0 SSBs<\/strong><strong>\u7684\u7ed3\u6784\u3002<\/strong><strong>\u00a9 2025 Springer Nature Limited<\/strong><\/p>\n<p><strong>\u00a0<img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-264573\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/3-8.png\" alt=\"\" width=\"791\" height=\"590\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/3-8.png 791w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/3-8-300x224.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/3-8-768x573.png 768w\" sizes=\"(max-width: 791px) 100vw, 791px\" \/><\/strong><\/p>\n<p><strong>\u56fe<\/strong><strong>2\u00a0 <\/strong><strong>\u5f71\u54cd\u65e0\u9633\u6781\u56fa\u6001\u7535\u6c60\u4e2d\u9502\u521d\u59cb\u6c89\u79ef\u7684\u56e0\u7d20\u3002<\/strong><strong>\u00a9 2025 Springer Nature Limited<\/strong><\/p>\n<p><strong>\u00a0<img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-264574\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/4-8.png\" alt=\"\" width=\"875\" height=\"467\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/4-8.png 875w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/4-8-300x160.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/4-8-768x410.png 768w\" sizes=\"(max-width: 875px) 100vw, 875px\" \/><\/strong><\/p>\n<p><strong>\u56fe<\/strong><strong>3\u00a0 <\/strong><strong>\u5f71\u54cd\u65e0\u9633\u6781\u56fa\u6001\u7535\u6c60\u5145\u653e\u7535\u5faa\u73af\u884c\u4e3a\u7684\u56e0\u7d20\u3002<\/strong><strong>\u00a9 2025 Springer Nature Limited<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-264575\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/5-7.png\" alt=\"\" width=\"876\" height=\"202\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/5-7.png 876w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/5-7-300x69.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/01\/5-7-768x177.png 768w\" sizes=\"(max-width: 876px) 100vw, 876px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>4<\/strong><strong>\u65e0\u9633\u6781\u56fa\u6001\u7535\u6c60\u4e2d\u6c89\u79ef\u9502\u7684\u8868\u5f81\u3002<\/strong><strong>\u00a9 2025 Springer Nature Limited<\/strong><\/p>\n<p><strong>\u00a0<\/strong><\/p>\n<p><strong>\u00a0<\/strong><strong>\u4e09\u3001\u3010<\/strong>\u79d1\u5b66\u542f\u8fea<strong>\u3011<\/strong><\/p>\n<p>\u4e0e\u9502\u7535\u6c60\u76f8\u6bd4\uff0c\u65e0\u9633\u6781\u56fa\u6001\u7535\u6c60\u5728\u63a8\u8fdb\u50a8\u80fd\u6280\u672f\u65b9\u9762\u5177\u6709\u5de8\u5927\u7684\u6f5c\u529b\uff0c\u5177\u6709\u4f18\u8d8a\u7684\u80fd\u91cf\u5bc6\u5ea6\u548c\u6613\u4e8e\u5236\u9020\u7684\u7279\u70b9\u3002\u5c3d\u7ba1\u8fd1\u5e74\u6765\u5728\u7406\u89e3\u884c\u4e3a\u65b9\u9762\u53d6\u5f97\u4e86\u8fdb\u5c55\uff0c\u4f46\u65e0\u9633\u6781SSBs\u7684\u79d1\u5b66\u548c\u6280\u672f\u4ecd\u5904\u4e8e\u53d1\u5c55\u7684\u65e9\u671f\u9636\u6bb5\u3002<\/p>\n<p>\u8be5\u9879\u6210\u679c\u6982\u8ff0\u4e86\u63a7\u5236\u65e0\u9633\u6781\u56fa\u6001\u7535\u6c60\u4e2d\u9502\u6c89\u79ef\u3001\u5265\u79bb\u548c\u5faa\u73af\u7684\u56e0\u7d20\uff0c\u5f3a\u8c03\u7535\u5316\u5b66\u548c\u529b\u5b66\u4e4b\u95f4\u7684\u76f8\u4e92\u4f5c\u7528\u5982\u4f55\u5728\u51b3\u5b9a\u884c\u4e3a\u4e2d\u8d77\u5173\u952e\u4f5c\u7528\u3002\u4f7f\u7528\u9ad8\u5806\u53e0\u538b\u529b\u548c\u6e29\u5ea6\u6765\u63d0\u9ad8\u6027\u80fd\u76f8\u5bf9\u5bb9\u6613\uff0c\u4f46\u662f\u4e5f\u9700\u8981\u5173\u6ce8\u4f4e\u5806\u538b\uff08&lt; 1mpa\uff09\u5bf9\u6750\u6599\u6f14\u53d8\u7684\u5f71\u54cd\u3002\u6b64\u5916\uff0c\u7531\u4e8e\u8815\u53d8\u53ef\u4ee5\u4f9d\u8d56\u4e8e\u6cbf\u5fae\u89c2\u7ed3\u6784\u7279\u5f81\u7684\u6269\u6563\uff0c\u56e0\u6b64\u5bf9\u9502\u7684\u5fae\u89c2\u7ed3\u6784\u63a7\u5236\u53ef\u4ee5\u63d0\u9ad8\u8815\u53d8\u901f\u7387\u3002\u5e76\u4e14\uff0c\u9502\u4e2d\u7684\u6742\u8d28\u53ef\u80fd\u5728\u5265\u79bb\u8fc7\u7a0b\u4e2d\u79ef\u805a\u5728\u754c\u9762\u4e0a\u6216\u5f71\u54cd\u9502\u7684\u5fae\u89c2\u7ed3\u6784\u3002\u9700\u8981\u8fdb\u4e00\u6b65\u4e86\u89e3\u9502\u539f\u5b50\u6742\u8d28\u5bf9\u65e0\u9633\u6781\u56fa\u6001\u7535\u6c60\u5faa\u73af\u884c\u4e3a\u7684\u5f71\u54cd\u3002\u7531\u4e8e\u754c\u9762\u8d28\u91cf\u7684\u91cd\u8981\u6027\uff0c\u7535\u6c60\u7ec4\u88c5\u65b9\u6cd5\u5728\u51b3\u5b9a\u7535\u6c60\u6027\u80fd\u65b9\u9762\u4e5f\u8d77\u7740\u81f3\u5173\u91cd\u8981\u7684\u4f5c\u7528\u3002<\/p>\n<p>\u672a\u6765\u7684\u7b56\u7565\u53ef\u80fd\u4fa7\u91cd\u4e8e\u8c03\u6574\u76f8\u95f4\u5c42\uff0c\u4ee5\u6700\u5927\u9650\u5ea6\u5730\u51cf\u5c11\u9502\u7684\u6d88\u8017\u3002\u8fd9\u53ef\u4ee5\u901a\u8fc7\u5728\u9502\u6c89\u79ef\u524d\u5c06\u96c6\u6d41\u4f53\u4fdd\u6301\u5728\u53ef\u63a7\u7535\u4f4d\u6765\u6539\u53d8\u754c\u9762\u5f62\u6210\uff0c\u901a\u8fc7\u4fee\u6539SSE\u8868\u9762\u6210\u5206\u6216\u6dfb\u52a0\u8584\u7684\u201c\u4eba\u5de5SEI\u201d\u5c42\u6765\u5b9e\u73b0\u3002\u53e6\u4e00\u4e2a\u63d0\u9ad8\u6027\u80fd\u7684\u7b56\u7565\u662f\u5728\u5265\u79bb\u7ed3\u675f\u65f6\u5bf9\u7535\u6d41\u548c\u7535\u538b\u8fdb\u884c\u95ed\u73af\u53cd\u9988\u63a7\u5236\uff0c\u4ee5\u7cbe\u786e\u63a7\u5236\u6750\u6599\u7684\u6f14\u53d8\u3002\u8bbe\u8ba1\u8d1f\u6781\u96c6\u6d41\u4f53\u6216SSE\u7684\u754c\u9762\u5fae\u89c2\u7ed3\u6784\u6765\u4fc3\u8fdb\u6709\u6548\u7684\u9502\u5faa\u73af\u4e5f\u662f\u6709\u6548\u7684\u3002\u6700\u540e\uff0c\u5e94\u7528\u539f\u4f4doperando\u8868\u5f81\u6765\u63d0\u9ad8\u5bf9\u64cd\u4f5c\u548c\u964d\u89e3\u6a21\u5f0f\u7684\u7406\u89e3\u5c06\u7ee7\u7eed\u5bf9\u8be5\u6280\u672f\u7684\u53d1\u5c55\u81f3\u5173\u91cd\u8981\u3002<\/p>\n<p><strong>\u539f\u6587\u8be6\u60c5<\/strong>\uff1ahttps:\/\/doi.org\/10.1038\/s41563-024-02055-z<\/p>\n<p>&nbsp;<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u5f20\u7199\u7199 \u4e00\u3001 \u3010\u79d1\u5b66\u80cc\u666f\u3011 \u00a0\u00a0 \u9502\u79bb\u5b50\u7535\u6c60\u63a8\u52a8\u4e86\u6d88\u8d39\u7535\u5b50\u4ea7\u54c1\u7684\u53d1\u5c55\uff0c\u52a0\u901f\u4e86\u7535\u52a8\u6c7d\u8f66\u7684\u666e\u53ca\u3002\u4f46\u662f\u76ee\u524d\u7684\u9502\u79bb\u5b50\u7535\u6c60\u6280\u672f\u4ecd\u96be\u4ee5\u6ee1\u8db3\u91cd\u578b\u8f66\u8f86\u548c\u7535\u52a8\u98de\u884c\u5668\u7b49\u9886\u57df\u7684\u8981\u6c42\u3002&#8230;<\/p>\n","protected":false},"author":39557,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-264570","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/264570"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/39557"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=264570"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/264570\/revisions"}],"predecessor-version":[{"id":264576,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/264570\/revisions\/264576"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=264570"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=264570"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=264570"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}