{"id":264916,"date":"2025-02-10T06:46:59","date_gmt":"2025-02-09T22:46:59","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=264916"},"modified":"2025-02-09T18:51:36","modified_gmt":"2025-02-09T10:51:36","slug":"%e9%bb%84%e8%8c%b9%e5%a9%b7applied-catalysis-b-environment-and-energy%ef%bc%9a%e9%87%91%e5%b1%9e%e6%9c%89%e6%9c%ba%e6%a1%86%e6%9e%b6%e6%9d%90%e6%96%99%e5%a4%8d%e5%90%88%e5%be%ae%e8%97%bb%e5%8d%8f","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=264916","title":{"rendered":"\u9ec4\u8339\u5a77Applied Catalysis B: Environment and Energy\uff1a\u91d1\u5c5e\u6709\u673a\u6846\u67b6\u6750\u6599\u590d\u5408\u5fae\u85fb\u534f\u540c\u50ac\u5316\u8fd8\u539fCO2"},"content":{"rendered":"<p>\u4e00\u3001 \u3010\u5bfc\u8bfb\u3011<\/p>\n<p>\u76ee\u524d\uff0cCO2\u5149\u50ac\u5316\u8f6c\u5316\u8fc7\u7a0b\u4e2d\u4ecd\u9700\u6210\u672c\u9ad8\u6602\u7684\u5149\u654f\u5242\u6765\u5b9e\u73b0\u9ad8\u6548\u50ac\u5316\u8fd8\u539f\uff0c\u800c\u5fae\u85fb\u4f18\u8d8a\u7684 CO2\u6355\u96c6\u80fd\u529b\u80fd\u591f\u5728\u50ac\u5316\u8fd8\u539f\u4e2d\u5145\u5f53\u7406\u60f3\u7684\u5438\u9644\u5242\u548c\u5149\u654f\u5242\uff0c\u6070\u597d\u5f25\u8865\u4e86\u5149\u50ac\u5316\u5242\u6750\u6599\u5bf9 CO2 \u6355\u96c6\u548c\u5149\u5438\u6536\u80fd\u529b\u6709\u9650\u7684\u95ee\u9898\u3002\u5b89\u5fbd\u5927\u5b66\u8d44\u6e90\u4e0e\u73af\u5883\u5de5\u7a0b\u5b66\u9662\u6c61\u67d3\u63a7\u5236\u4e0e\u8d44\u6e90\u5316\u56e2\u961f\u9ec4\u8339\u5a77\u526f\u6559\u6388\u603b\u7ed3\u76f8\u5173\u6280\u672f\uff0c\u5728\u73af\u5883\u79d1\u5b66-\u5de5\u7a0b\u9886\u57df\u9876\u7ea7\u671f\u520a\u300aApplied Catalysis B: Environment and Energy\u300b\u4e0a\u4ee5\u201cCatalytic Activity of Microcystis aeruginosa in Fe-Co-MOFs System for Efficient CO2 Fixation and High-Value Conversion\u201d\u4e3a\u9898\u53d1\u8868\u8bba\u6587\uff08DOI: 10.1016\/j.apcatb.2025.125120\uff09\uff0c\u5b89\u5fbd\u5927\u5b66\u4e3a\u7b2c\u4e00\u901a\u8baf\u5355\u4f4d\u3002<\/p>\n<p>\n\u4e8c\u3001\u3010\u6210\u679c\u63a0\u5f71\u3011<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-264917\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u56fe\u72471-7.png\" alt=\"\" width=\"371\" height=\"282\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u56fe\u72471-7.png 371w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u56fe\u72471-7-300x228.png 300w\" sizes=\"(max-width: 371px) 100vw, 371px\" \/><\/p>\n<p>&nbsp;<\/p>\n<p>\u4e09\u3001\u3010\u6838\u5fc3\u521b\u65b0\u70b9\u3011<\/p>\n<p>\u57fa\u4e8e\u524d\u671f\u7814\u7a76\u57fa\u7840\uff0c\u56e2\u961f\u521b\u65b0\u6027\u5730\u5c06\u5fae\u85fb\uff08\u5fae\u56ca\u85fb\uff09\u4e0e\u91d1\u5c5e\u6709\u673a\u6846\u67b6\uff08Fe-Co-MOFs\uff09\u6750\u6599\u6709\u6548\u7ec4\u88c5\uff0c\u5229\u7528\u5149\u50ac\u5316\u4f53\u7cfb\u5b9e\u73b0\u4e86\u4e8c\u6c27\u5316\u78b3\uff08CO2\uff09\u5411\u7532\u70f7\uff08CH4\uff09\u7684\u9ad8\u9009\u62e9\u6027\u5b9a\u5411\u8f6c\u5316\u3002\u8be5\u590d\u5408\u4f53\u7cfb\u7531\u4e8eCo\u539f\u5b50\u4e2d\u5fc3\u7684\u52a0\u5165\uff0c\u4f7f\u5f97CO2\u66f4\u4e3a\u6709\u6548\u5f97\u5438\u9644\u5728\u6d3b\u6027\u4f4d\u70b9\u9644\u8fd1\uff0c\u5e76\u4e0e\u5fae\u56ca\u85fb\u4ea7\u751f\u534f\u540c\u4f5c\u7528\uff0c\u4ece\u800c\u8868\u73b0\u51fa\u4f18\u5f02\u7684CH4\u4ea7\u7387\uff0892.6 \u03bcmol g\u207b\u00b9 h\u207b\u00b9\uff09\uff0c\u6bd4Fe-Co-MOFs\u7684\u50ac\u5316\u6548\u7387\u9ad81.46\u500d\uff0c\u540c\u65f6\u5b9e\u73b0\u4e86\u9ad8\u8fbe96.1%\u7684\u8f6c\u5316\u9009\u62e9\u6027\u3002\u6b64\u5916\uff0c\u901a\u8fc7\u8f6c\u5f55\u7ec4\u5206\u5206\u6790\uff0c\u63ed\u793a\u4e86Fe-Co-MOFs\u80fd\u591f\u6709\u6548\u63d0\u5347\u5fae\u56ca\u85fb\u5149\u5408\u4f5c\u7528\u6697\u53cd\u5e94\u8fc7\u7a0b\u4e2d\u7684CO2\u6d53\u5ea6\uff0c\u4ece\u800c\u4fc3\u8fdb\u7535\u5b50\u8f6c\u79fb\u8fc7\u7a0b\uff0c\u589e\u5f3a\u4e8c\u6c27\u5316\u78b3\u7684\u56fa\u5b9a\u80fd\u529b\uff0c\u4e3a\u4e8c\u6c27\u5316\u78b3\u7684\u5bcc\u96c6\u548c\u9ad8\u503c\u8f6c\u5316\u3001\u5fae\u85fb\u8d44\u6e90\u5316\u5229\u7528\u63d0\u4f9b\u4e86\u7406\u8bba\u548c\u5b9e\u9a8c\u652f\u6301\u3002<\/p>\n<p>\u56db\u3001\u3010\u6570\u636e\u6982\u89c8\u3011<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-264918\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u56fe\u72472-7.png\" alt=\"\" width=\"700\" height=\"393\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u56fe\u72472-7.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u56fe\u72472-7-300x168.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/> <br \/>\n \u56fe1 \u5fae\u56ca\u85fb-MOFs\u590d\u5408\u4f53\u7cfb\uff08Microcystis aeruginosa-NDC-T130\uff09\u5149\u50ac\u5316\u8fd8\u539fCO2\u6027\u80fd<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-264919\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u56fe\u72473-1.jpg\" alt=\"\" width=\"700\" height=\"775\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u56fe\u72473-1.jpg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u56fe\u72473-1-271x300.jpg 271w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u56fe2 \u7406\u8bba\u8ba1\u7b97\uff1aFe-Co-MOFs\u5149\u50ac\u5316\u8fd8\u539fCO2\u8fc7\u7a0b\u793a\u610f\u56fe\u548c\u5409\u5e03\u65af\u81ea\u7531\u80fd\u5206\u6790<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-264920\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u56fe\u72474-7.png\" alt=\"\" width=\"700\" height=\"440\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u56fe\u72474-7.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u56fe\u72474-7-300x189.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u56fe3 Microcystis aeruginosa-NDC-T130\u53cd\u5e94\u524d\u540e\u5fae\u85fb\u57fa\u56e0\u4fe1\u606f<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-264921\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u56fe\u72475.jpg\" alt=\"\" width=\"700\" height=\"480\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u56fe\u72475.jpg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u56fe\u72475-300x206.jpg 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u56fe4 Microcystis aeruginosa-NDC-T130\u5149\u50ac\u5316\u8fd8\u539fCO2\u53cd\u5e94\u673a\u7406<\/p>\n<p>\u539f\u6587\u8be6\u60c5\uff1a<\/p>\n<p>https:\/\/www.sciencedirect.com\/science\/article\/pii\/S0926337325001031<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4e00\u3001 \u3010\u5bfc\u8bfb\u3011 \u76ee\u524d\uff0cCO2\u5149\u50ac\u5316\u8f6c\u5316\u8fc7\u7a0b\u4e2d\u4ecd\u9700\u6210\u672c\u9ad8\u6602\u7684\u5149\u654f\u5242\u6765\u5b9e\u73b0\u9ad8\u6548\u50ac\u5316\u8fd8\u539f\uff0c\u800c\u5fae\u85fb\u4f18\u8d8a\u7684 CO2\u6355\u96c6\u80fd\u529b\u80fd\u591f\u5728\u50ac\u5316\u8fd8\u539f\u4e2d\u5145\u5f53\u7406\u60f3\u7684\u5438\u9644\u5242\u548c\u5149\u654f\u5242\uff0c\u6070\u597d\u5f25&#8230;<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-264916","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/264916"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=264916"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/264916\/revisions"}],"predecessor-version":[{"id":264922,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/264916\/revisions\/264922"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=264916"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=264916"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=264916"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}