{"id":265166,"date":"2025-02-24T06:16:19","date_gmt":"2025-02-23T22:16:19","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=265166"},"modified":"2025-02-23T18:28:17","modified_gmt":"2025-02-23T10:28:17","slug":"%e8%a5%bf%e5%ae%89%e4%ba%a4%e5%a4%a7%e4%b8%81%e4%b9%a6%e6%b1%9fjoule%ef%bc%9a%e6%ba%b6%e5%89%82%e8%a1%8d%e7%94%9f%e7%9a%84%e5%af%8c%e6%9c%89%e6%9c%basei%e6%9c%89%e6%95%88%e6%8f%90%e5%8d%87%e4%bd%8e","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=265166","title":{"rendered":"\u897f\u5b89\u4ea4\u5927\u4e01\u4e66\u6c5fJoule\uff1a\u6eb6\u5242\u884d\u751f\u7684\u5bcc\u6709\u673aSEI\u6709\u6548\u63d0\u5347\u4f4e\u6e29\u9502\u91d1\u5c5e\u7535\u6c60\u5bb9\u91cf"},"content":{"rendered":"<p>\u9502\u91d1\u5c5e\u7535\u6c60\u56e0\u5176\u8d85\u8fc7500 Wh kg\u207b\u00b9\u7684\u9ad8\u80fd\u91cf\u5bc6\u5ea6\u800c\u5907\u53d7\u5173\u6ce8\uff0c\u7136\u800c\u5728\u4f4e\u6e29\uff08\u5c24\u5176\u662f\u4f4e\u4e8e-20\u00b0C\uff09\u73af\u5883\u4e0b\u9762\u4e34\u663e\u8457\u7684\u6027\u80fd\u9000\u5316\u95ee\u9898\uff0c\u5176\u6838\u5fc3\u74f6\u9888\u4e3b\u8981\u6e90\u4e8e\u754c\u9762\u52a8\u529b\u5b66\u8fdf\u6ede\u548c\u6750\u6599\/\u7ed3\u6784\u5931\u6548\u3002\u4e3a\u4e86\u63d0\u5347\u9502\u91d1\u5c5e\u7535\u6c60\u7684\u4f4e\u6e29\u6027\u80fd\uff0c\u8fd1\u5e74\u6765\u7814\u7a76\u4eba\u5458\u4e3b\u8981\u89e3\u51b3\u65b9\u6848\u4ee5\u7535\u89e3\u6db2\u9769\u65b0\u548cSEI\u8c03\u63a7\u4e3a\u6838\u5fc3\uff0c\u7ed3\u5408\u7535\u6781\u7ed3\u6784\u4f18\u5316\u4e0e\u70ed\u7ba1\u7406\u6280\u672f\uff0c\u9010\u6b65\u7a81\u7834\u4f4e\u6e29\u74f6\u9888\u3002<\/p>\n<p>\u897f\u5b89\u4ea4\u901a\u5927\u5b66\u5316\u5b66\u5b66\u9662\u4e01\u4e66\u6c5f\u6559\u6388\u56e2\u961f\u9488\u5bf9\u4f4e\u6e29\u9502\u91d1\u5c5e\u7535\u6c60\uff08LT-LMBs\uff09\u4e2d\u56fa\u4f53\u7535\u89e3\u8d28\u754c\u9762\uff08SEI\uff09\u7684\u4f20\u7edf\u8ba4\u77e5\u63d0\u51fa\u4e86\u7a81\u7834\u6027\u89c2\u70b9\uff0c\u5e76\u901a\u8fc7\u5b9e\u9a8c\u9a8c\u8bc1\u4e86\u6eb6\u5242\u884d\u751f\u5bcc\u6709\u673aSEI\u7684\u72ec\u7279\u4f18\u52bf\u3002\u8be5\u7814\u7a76\u6210\u679c\u4ee5\u201cSolvent-derived organic-rich SEI enables capacity enhancement for low-temperature lithium metal batteries\u201d\uff08\u6eb6\u5242\u884d\u751f\u7684\u5bcc\u6709\u673aSEI\u6709\u6548\u63d0\u5347\u4f4e\u6e29\u9502\u91d1\u5c5e\u7535\u6c60\u5bb9\u91cf\uff09\u4e3a\u9898\u53d1\u8868\u5728\u56fd\u9645\u80fd\u6e90\u9886\u57df\u9876\u7ea7\u671f\u520a\u201cJoule\u201d\uff08\u300a\u7126\u8033\u300b\uff09\u4e0a\uff0c\u897f\u5b89\u4ea4\u901a\u5927\u5b66\u5316\u5b66\u5b66\u9662\u4e3a\u7b2c\u4e00\u901a\u8baf\u5355\u4f4d\u3002\u8bba\u6587\u7b2c\u4e00\u4f5c\u8005\u4e3a\u897f\u5b89\u4ea4\u5927\u535a\u58eb\u751f\u9634\u7965\u51ef\uff0c\u901a\u8baf\u4f5c\u8005\u4e3a\u897f\u5b89\u4ea4\u5927\u5316\u5b66\u5b66\u9662\u4e01\u4e66\u6c5f\u6559\u6388\u3001\u9ad8\u56fd\u65b0\u526f\u6559\u6388\u548c\u4e8e\u4f1f\u526f\u6559\u6388\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-265167\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u5fae\u4fe1\u622a\u56fe_20250223182444.jpg\" alt=\"\" width=\"948\" height=\"318\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u5fae\u4fe1\u622a\u56fe_20250223182444.jpg 948w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u5fae\u4fe1\u622a\u56fe_20250223182444-300x101.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/\u5fae\u4fe1\u622a\u56fe_20250223182444-768x258.jpg 768w\" sizes=\"(max-width: 948px) 100vw, 948px\" \/><\/p>\n<p>\u8be5\u7814\u7a76\u6210\u679c\u6838\u5fc3\u521b\u65b0\u70b9\u53ef\u5f52\u7eb3\u5982\u4e0b\uff1a<\/p>\n<p><strong>1. \u7406\u8bba\u7a81\u7834\uff1a\u6311\u6218\u4f20\u7edfSEI\u8bbe\u8ba1\u8303\u5f0f<\/strong><\/p>\n<p>\u4f20\u7edf\u89c2\u70b9\u98a0\u8986\uff1a\u9996\u6b21\u63ed\u793a\u4f4e\u6e29\u6761\u4ef6\u4e0b\u9634\u79bb\u5b50\u884d\u751f\u7684\u5bcc\u65e0\u673aSEI\u56e0\u754c\u9762\u4f20\u8f93\u52a8\u529b\u5b66\u7f13\u6162\u5bfc\u81f4\u5bb9\u91cf\u8870\u51cf\uff0c\u800c\u6eb6\u5242\u884d\u751f\u7684\u5bcc\u6709\u673aSEI\u53cd\u800c\u8868\u73b0\u51fa\u66f4\u4f18\u6027\u80fd\u3002\u8fd9\u4e00\u53d1\u73b0\u6253\u7834\u4e86\u201c\u65e0\u673aSEI\u66f4\u4f18\u201d\u7684\u56fa\u6709\u8ba4\u77e5\uff0c\u4e3a\u4f4e\u6e29\u7535\u6c60\u8bbe\u8ba1\u63d0\u4f9b\u4e86\u65b0\u65b9\u5411\u3002<\/p>\n<p>\u4f4e\u6e29\u9002\u914d\u6027\u7406\u8bba\uff1a\u63d0\u51fa\u4f4e\u6e29\u73af\u5883\u4f1a\u653e\u5927SEI\u7684\u52a8\u529b\u5b66\u5dee\u5f02\uff0c\u5f3a\u8c03\u9700\u9488\u5bf9\u4f4e\u6e29\u9700\u6c42\u5b9a\u5236SEI\uff08\u800c\u975e\u76f4\u63a5\u6cbf\u7528\u5ba4\u6e29\u4f18\u5316\u7b56\u7565\uff09\uff0c\u63a8\u52a8\u4f4e\u6e29\u7535\u6c60\u754c\u9762\u7814\u7a76\u7684\u8303\u5f0f\u8f6c\u53d8\u3002<\/p>\n<p><strong>2. \u6750\u6599\u4e0e\u7ed3\u6784\u521b\u65b0\uff1a\u6709\u673a\u7845\u7535\u89e3\u6db2\u6784\u5efa\u7a33\u5b9aSEI<\/strong><\/p>\n<p><strong>\u65b0\u578b\u7535\u89e3\u6db2\u8bbe\u8ba1<\/strong>\uff1a\u5f00\u53d1\u542b<strong>Si\u2013O\u952e\u7684\u6709\u673a\u7845\u7535\u89e3\u6db2<\/strong>\uff0c\u5176\u6eb6\u5242\u5206\u5b50\u53c2\u4e0e\u5f62\u6210SEI\uff0c\u663e\u8457\u63d0\u5347\u6709\u673a\u6210\u5206\u6bd4\u4f8b\uff08<strong>16.51\u500d\u589e\u52a0<\/strong>\uff09\u3002<\/p>\n<p><strong>SEI\u7ed3\u6784\u4f18\u5316<\/strong>\uff1a\u6240\u6784\u5efa\u7684\u5bcc\u6709\u673aSEI\u517c\u5177<strong>\u5feb\u901f\u79bb\u5b50\u4f20\u8f93<\/strong>\uff08\u5f31\u754c\u9762\u4f5c\u7528\u529b\u4e0e\u5b54\u6269\u6563\u673a\u5236\uff09\u4e0e<strong>\u589e\u5f3a\u7a33\u5b9a\u6027<\/strong>\uff08Si\u2013O\u952e\u8d21\u732e\uff09\uff0c\u89e3\u51b3\u4e86\u4f20\u7edf\u6709\u673aSEI\u673a\u68b0\u6027\u80fd\u5dee\u7684\u95ee\u9898\u3002<\/p>\n<p><strong>3. \u673a\u5236\u63ed\u793a\uff1a\u754c\u9762\u6eb6\u5242\u5316\u7ed3\u6784\u4e0eSEI\u6027\u80fd\u5173\u8054<\/strong><\/p>\n<p><strong>\u8fd1\u754c\u9762\u6eb6\u5242\u5316\u7ed3\u6784\u8c03\u63a7<\/strong>\uff1a\u53d1\u73b0\u7535\u89e3\u6db2\u6eb6\u5242\u5316\u7ed3\u6784\u4e0eSEI\u7ec4\u5206\u95f4\u7684\u76f4\u63a5\u5173\u8054\uff0c\u63d0\u51fa\u901a\u8fc7\u8c03\u63a7\u6eb6\u5242\u5316\u73af\u5883\uff08\u5982\u4f4e\u6e29\u5faa\u73af\u5de5\u827a\uff09\u5b9a\u5411\u8bbe\u8ba1SEI\u5316\u5b66\u7ec4\u6210\uff0c\u4e3a\u754c\u9762\u5de5\u7a0b\u63d0\u4f9b\u7406\u8bba\u4f9d\u636e\u3002<\/p>\n<p><strong>\u52a8\u529b\u5b66\u673a\u5236\u9610\u660e<\/strong>\uff1a\u63ed\u793a\u5bcc\u6709\u673aSEI\u7684<strong>\u4f4e\u754c\u9762\u963b\u6297<\/strong>\u6e90\u4e8e\u66f4\u5feb\u7684\u5b54\u6269\u6563\u673a\u5236\uff0c\u800c\u4f20\u7edf\u65e0\u673aSEI\u7684\u81f4\u5bc6\u7ed3\u6784\u5728\u4f4e\u6e29\u4e0b\u963b\u788d\u79bb\u5b50\u8fc1\u79fb\u3002<\/p>\n<p><strong>4. \u5de5\u827a\u521b\u65b0\uff1a\u4f4e\u6e29\u6210\u819c\u5faa\u73af\u6280\u672f<\/strong><\/p>\n<p>\u5f00\u53d1<strong>\u4f4e\u6e29\u5f62\u6210\u5faa\u73af\uff08LT formation cycling\uff09\u5de5\u827a<\/strong>\uff0c\u5229\u7528\u4f4e\u6e29\u6761\u4ef6\u4fc3\u8fdb\u6eb6\u5242\u5206\u5b50\u4f18\u5148\u5206\u89e3\uff0c\u5b9e\u73b0SEI\u4e2d\u6709\u673a\u7ec4\u5206\u7684\u5b9a\u5411\u5bcc\u96c6\uff0c\u4e3a\u4f4e\u6e29\u7535\u6c60\u5236\u9020\u63d0\u4f9b\u65b0\u65b9\u6cd5\u3002<\/p>\n<p><strong>5. \u6027\u80fd\u7a81\u7834\uff1a\u521b\u7eaa\u5f55\u7684\u4f4e\u6e29\u7535\u6c60\u8868\u73b0<\/strong><\/p>\n<p><strong>\u6781\u7aef\u4f4e\u6e29\u6027\u80fd<\/strong>\uff1aLi||NCM811\u7535\u6c60\u5728**-114.05\u00b0C**\u4ecd\u4fdd\u6301\u653e\u7535\u529f\u80fd\uff0c\u5237\u65b0\u4f4e\u6e29\u5de5\u4f5c\u6781\u9650\u3002<\/p>\n<p><strong>\u9ad8\u5bb9\u91cf\u4e0e\u5faa\u73af\u7a33\u5b9a\u6027<\/strong>\uff1a\u5728**-40\u00b0C<strong>\u4e0b\u653e\u7535\u5bb9\u91cf\u63d0\u534722.5%\uff1b1.2 Ah\u8f6f\u5305\u7535\u6c60\u5728<\/strong>-20\u00b0C**\u3001\u8d2b\u7535\u89e3\u6db2\u6761\u4ef6\uff082.5 mL Ah\u207b\u00b9\uff09\u4e0b\u5faa\u73af50\u6b21\u540e\u5bb9\u91cf\u4fdd\u6301\u7387\u8fbe92.1%\uff0c\u5c55\u73b0\u5b9e\u9645\u5e94\u7528\u6f5c\u529b\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-265168\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/1C361A47FD4D910FC6C0793012C_BFE8ED98_AC21.png\" alt=\"\" width=\"338\" height=\"311\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/1C361A47FD4D910FC6C0793012C_BFE8ED98_AC21.png 338w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/1C361A47FD4D910FC6C0793012C_BFE8ED98_AC21-300x276.png 300w\" sizes=\"(max-width: 338px) 100vw, 338px\" \/><\/p>\n<p>\u8bba\u6587\u94fe\u63a5\uff1ahttps:\/\/www.cell.com\/joule\/fulltext\/S2542-4351(25)00004-2<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u9502\u91d1\u5c5e\u7535\u6c60\u56e0\u5176\u8d85\u8fc7500 Wh kg\u207b\u00b9\u7684\u9ad8\u80fd\u91cf\u5bc6\u5ea6\u800c\u5907\u53d7\u5173\u6ce8\uff0c\u7136\u800c\u5728\u4f4e\u6e29\uff08\u5c24\u5176\u662f\u4f4e\u4e8e-20\u00b0C\uff09\u73af\u5883\u4e0b\u9762\u4e34\u663e\u8457\u7684\u6027\u80fd\u9000\u5316\u95ee\u9898\uff0c\u5176\u6838\u5fc3\u74f6\u9888\u4e3b\u8981\u6e90\u4e8e\u754c\u9762\u52a8\u529b\u5b66\u8fdf\u6ede&#8230;<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-265166","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/265166"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=265166"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/265166\/revisions"}],"predecessor-version":[{"id":265169,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/265166\/revisions\/265169"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=265166"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=265166"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=265166"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}