{"id":265238,"date":"2025-02-28T08:51:35","date_gmt":"2025-02-28T00:51:35","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=265238"},"modified":"2025-02-28T08:51:35","modified_gmt":"2025-02-28T00:51:35","slug":"%e4%bb%8a%e6%97%a5science%ef%bc%8c%e6%b5%99%e5%a4%a7%e5%86%8d%e5%87%ba%e5%9c%88%ef%bc%8c%e5%bc%80%e5%8f%91%e6%9e%81%e7%ab%af%e6%9d%a1%e4%bb%b6%e4%b8%8b%e6%b0%b4%e5%87%9d%e8%83%b6","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=265238","title":{"rendered":"\u4eca\u65e5Science\uff0c\u6d59\u5927\u518d\u201c\u51fa\u5708\u201d\uff0c\u5f00\u53d1\u6781\u7aef\u6761\u4ef6\u4e0b\u6c34\u51dd\u80f6\uff01"},"content":{"rendered":"<p><strong>\u4e00\u3001\u3010\u79d1\u5b66\u80cc\u666f\u3011<\/strong><\/p>\n<p>\u6c34\u51dd\u80f6\u56e0\u5176\u5bcc\u542b\u6c34\u7684\u4ea4\u8054\u7f51\u7edc\uff0c\u88ab\u5e7f\u6cdb\u5e94\u7528\u4e8e\u7ec4\u7ec7\u5de5\u7a0b\u3001\u67d4\u6027\u7535\u5b50\u548c\u8f6f\u4f53\u673a\u5668\u4eba\u7b49\u9886\u57df\u3002\u5c3d\u7ba1\u901a\u8fc7\u589e\u5f3a\u805a\u5408\u7269\u7f51\u7edc\u63d0\u5347\u4e86\u6c34\u51dd\u80f6\u7684\u5ef6\u5c55\u6027\u548c\u97e7\u6027\uff0c\u4f46\u5176\u67d4\u97e7\u6027\u4ecd\u4f9d\u8d56\u4e8e\u53ef\u79fb\u52a8\u7684\u6c34\u5206\u5b50\u3002\u56e0\u6b64\uff0c\u8fd9\u79cd\u4f9d\u8d56\u6027\u5bfc\u81f4\u6c34\u51dd\u80f6\u5728\u6e29\u5ea6\u53d8\u5316\u8fc7\u7a0b\u4e2d\u56e0\u84b8\u53d1\u6216\u51bb\u7ed3\u800c\u5931\u6c34\u65f6\u53d8\u5f97\u575a\u786c\u548c\u6613\u788e\u3002\u73b0\u6709\u65b9\u6cd5\u901a\u8fc7\u7528\u79bb\u5b50\u6db2\u4f53\u3001\u65e0\u673a\u76d0\u6eb6\u6db2\u7b49\u66ff\u4ee3\u6c34\u5206\u5b50\u4ee5\u63d0\u9ad8\u76f8\u53d8\u6e29\u5ea6\uff0c\u4f46\u8fd9\u4e9b\u6eb6\u5242\u5b58\u5728\u5438\u6e7f\u6027\u3001\u6e29\u5ea6\u8303\u56f4\u6709\u9650\uff08\u901a\u5e38\u4f4e\u4e8e-80 \u2103\u621680 \u2103\uff09\u7b49\u95ee\u9898\u3002\u6c34\u5206\u5b50\u5728\u66ff\u4ee3\u6eb6\u5242\u4e2d\u4ecd\u53ef\u80fd\u51bb\u7ed3\u6216\u9038\u51fa\uff0c\u5bfc\u81f4\u7f51\u7edc\u8106\u5f31\u3002\u56e0\u6b64\uff0c\u5982\u4f55\u56fa\u5b9a\u6c34\u5206\u5b50\u5e76\u7ef4\u6301\u5176\u6d41\u52a8\u6027\uff0c\u6210\u4e3a\u62d3\u5bbd\u6c34\u51dd\u80f6\u6781\u7aef\u6e29\u5ea6\u9002\u5e94\u6027\u7684\u5173\u952e\u6311\u6218\u3002<\/p>\n<p><strong>\u4e8c\u3001\u3010\u521b\u65b0\u6210\u679c\u3011<\/strong><\/p>\n<p>\u4e3a\u89e3\u51b3\u4ee5\u4e0a\u96be\u9898\uff0c<strong>\u6d59\u6c5f\u5927\u5b66\u7f57\u81ea\u751f\u6559\u6388\u3001\u674e\u94c1\u98ce\u6559\u6388\u548c\u6768\u6829\u65ed\u535a\u58eb\u7b49\u4eba<\/strong>\u5728<strong><em>Science<\/em><\/strong>\u4e0a\u53d1\u8868\u4e86\u9898\u4e3a\u201c<strong>Hydro-locking in hydrogel for extreme temperature tolerance<\/strong>\u201d\u7684\u8bba\u6587\uff0c\u62a5\u9053\u5f00\u53d1\u4e86\u4e00\u79cd\u201c\u6c34\u9501\u201d\u7b56\u7565\uff0c\u901a\u8fc7\u786b\u9178\u5728\u805a\u5408\u7269\u7f51\u7edc\u4e2d\u5efa\u7acb\u6c34\u5206\u5b50\u4e0e\u805a\u5408\u7269\u7684\u5f3a\u8fde\u63a5\uff0c\u9501\u5b9a\u6c34\u5206\u5b50\uff0c\u5e76\u5f15\u5165\u727a\u7272\u7f51\u7edc\u4fdd\u62a4\u805a\u5408\u7269\u4e3b\u7f51\u7edc\u514d\u4e8e\u574d\u584c\u3002\u5728\u201c\u6c34\u9501\u201d\u7b56\u7565\u4e0b\u5236\u5907\u7684\u6d77\u85fb\u9178\u94a0-\u805a\u4e19\u70ef\u9170\u80fa\u53cc\u7f51\u7edc\u6c34\u51dd\u80f6\u5728-115 \u2103\u81f3143 \u2103\u7684\u5bbd\u6e29\u57df\u5185\u4fdd\u6301\u67d4\u8f6f\u548c\u53ef\u62c9\u4f38\u6027\u3002\u8be5\u7b56\u7565\u9002\u7528\u4e8e\u591a\u79cd\u6c34\u51dd\u80f6\u548c\u6eb6\u6db2\uff0c\u6709\u671b\u5b9e\u73b0\u6781\u7aef\u6e29\u5ea6\u4e0b\u6750\u6599\u751a\u81f3\u751f\u7269\u6837\u672c\u7684\u4fdd\u5b58\u4e0e\u89c2\u6d4b\u3002<\/p>\n<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-265239\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/0-4.png\" alt=\"\" width=\"600\" height=\"274\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/0-4.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/0-4-300x137.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>\u00a0<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-265240\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/1-7.jpg\" alt=\"\" width=\"600\" height=\"661\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/1-7.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/1-7-272x300.jpg 272w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>1\u00a0 S-<\/strong><strong>\u51dd\u80f6\u7684\u201c\u6c34\u9501\u201d\u7b56\u7565\u548c\u76f8\u53d8\u6e29\u5ea6<\/strong><strong> \u00a9 2025 AAAS<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-265241\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/2-7.jpg\" alt=\"\" width=\"600\" height=\"436\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/2-7.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/2-7-300x218.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>2\u00a0 <\/strong><strong>S-<\/strong><strong>\u51dd\u80f6\u4e2d\u7684\u53cd\u5e94\u53ca\u76f8\u4e92\u4f5c\u7528<\/strong> <strong>\u00a9 2025 AAAS<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-265242\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/3-8.jpg\" alt=\"\" width=\"600\" height=\"452\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/3-8.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/3-8-300x226.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>3\u00a0 S-<\/strong><strong>\u51dd\u80f6\u548c\u539f\u4f4d\u78b3\u70b9\u7684\u7ed3\u6784\u7279\u6027<\/strong><strong> \u00a9 2025 AAAS<\/strong><\/p>\n<p><strong>\u00a0<img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-265243\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/4-7.jpg\" alt=\"\" width=\"600\" height=\"702\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/4-7.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/02\/4-7-256x300.jpg 256w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/strong><\/p>\n<p><strong>\u56fe<\/strong><strong>4\u00a0 CS-<\/strong><strong>\u51dd\u80f6\u5728\u6781\u7aef\u6e29\u5ea6\u4e0b\u7684\u673a\u68b0\u6027\u80fd<\/strong><strong> \u00a9 2025 AAAS<\/strong><\/p>\n<p>&nbsp;<\/p>\n<p><strong>\u4e09\u3001\u3010\u79d1\u5b66\u542f\u8fea\u3011<\/strong><\/p>\n<p>\u7efc\u4e0a\uff0c\u672c\u7814\u7a76\u901a\u8fc7\u201c\u6c34\u9501\u201d\u7b56\u7565\u5c06\u6c34\u5206\u5b50\u7262\u56fa\u56fa\u5b9a\u5728\u805a\u5408\u7269\u7f51\u7edc\u4e2d\uff0c\u4f7f\u6c34\u51dd\u80f6\u5728-115 \u2103\u81f3143 \u2103\u7684\u6781\u7aef\u6e29\u5ea6\u8303\u56f4\u5185\u4fdd\u6301\u67d4\u8f6f\u548c\u53ef\u62c9\u4f38\u6027\u3002\u8be5\u7b56\u7565\u9002\u7528\u4e8e\u591a\u79cd\u6c34\u51dd\u80f6\uff08\u5982PVP\u6c34\u51dd\u80f6\uff09\u548c\u6eb6\u5242\uff08\u5982DMSO\uff09\uff0c\u5e76\u901a\u8fc7\u78b3\u5316\u5f62\u6210\u4fdd\u62a4\u5c42\u9632\u6b62\u7f51\u7edc\u574d\u584c\u3002\u201c\u6c34\u9501\u201d\u6c34\u51dd\u80f6\uff08\u5982CS-gel\uff09\u5728\u4f4e\u6e29\uff08-100 \u2103\uff09\u548c\u9ad8\u6e29\uff08140 \u2103\uff09\u4e0b\u4ecd\u5177\u5907\u5bfc\u7535\u6027\u548c\u4f20\u611f\u529f\u80fd\uff0c\u5c55\u793a\u4e86\u5728\u67d4\u6027\u7535\u5b50\u548c\u6781\u7aef\u73af\u5883\u751f\u7269\u4fdd\u5b58\u4e2d\u7684\u6f5c\u5728\u5e94\u7528\u4ef7\u503c\u3002<\/p>\n<p>\u539f\u6587\u8be6\u60c5\uff1a<a href=\"https:\/\/www.science.org\/doi\/10.1126\/science.adq2711\" target=\"_blank\" rel=\"noopener\">Hydro-locking in hydrogel for extreme temperature tolerance<\/a> (<em>Science<\/em> <strong>2025<\/strong>, 387, 967-973)<\/p>\n<p>\u672c\u6587\u7531\u5927\u5175\u54e5\u4f9b\u7a3f\u3002<\/p>\n<p>&nbsp;<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4e00\u3001\u3010\u79d1\u5b66\u80cc\u666f\u3011 \u6c34\u51dd\u80f6\u56e0\u5176\u5bcc\u542b\u6c34\u7684\u4ea4\u8054\u7f51\u7edc\uff0c\u88ab\u5e7f\u6cdb\u5e94\u7528\u4e8e\u7ec4\u7ec7\u5de5\u7a0b\u3001\u67d4\u6027\u7535\u5b50\u548c\u8f6f\u4f53\u673a\u5668\u4eba\u7b49\u9886\u57df\u3002\u5c3d\u7ba1\u901a\u8fc7\u589e\u5f3a\u805a\u5408\u7269\u7f51\u7edc\u63d0\u5347\u4e86\u6c34\u51dd\u80f6\u7684\u5ef6\u5c55\u6027\u548c\u97e7\u6027\uff0c\u4f46\u5176\u67d4\u97e7\u6027\u4ecd\u4f9d&#8230;<\/p>\n","protected":false},"author":1004,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[67],"tags":[5147],"class_list":["post-265238","post","type-post","status-publish","format-standard","hentry","category-zhoubao","tag-5147"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/265238"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/1004"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=265238"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/265238\/revisions"}],"predecessor-version":[{"id":265246,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/265238\/revisions\/265246"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=265238"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=265238"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=265238"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}