{"id":265435,"date":"2025-03-11T07:53:55","date_gmt":"2025-03-10T23:53:55","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=265435"},"modified":"2025-03-11T15:57:12","modified_gmt":"2025-03-11T07:57:12","slug":"nat-commun-%ef%bc%9a%e7%94%a8%e4%ba%8e%e8%87%aa%e4%be%9b%e7%94%b5%e6%99%ba%e8%83%bd%e7%aa%97%e5%92%8c%e6%98%be%e7%a4%ba%e7%9a%84%e5%8f%91%e5%85%89%e5%a4%aa%e9%98%b3%e8%83%bd%e8%81%9a%e5%85%89-2","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=265435","title":{"rendered":"Nat. Commun.\uff1a\u7528\u4e8e\u81ea\u4f9b\u7535\u667a\u80fd\u7a97\u548c\u663e\u793a\u7684\u53d1\u5149\u592a\u9633\u80fd\u805a\u5149\u5668\u548c\u7535\u81f4\u53d8\u8272\u8d85\u7ea7\u7535\u5bb9\u5668\u96c6\u6210\u5668\u4ef6"},"content":{"rendered":"<p><strong>\u4e00\u3001<\/strong><strong>\u00a0<\/strong><strong>\u3010\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p>\u5efa\u7b51\u7269\u80fd\u8017\u5728\u5168\u7403\u603b\u80fd\u8017\u4e2d\u5360\u6bd4\u8fbe30%-40%\uff0c\u63d0\u9ad8\u5efa\u7b51\u7269\u80fd\u6e90\u81ea\u7ed9\u80fd\u529b\u5df2\u6210\u4e3a\u56fd\u9645\u793e\u4f1a\u7684\u666e\u904d\u5171\u8bc6\u3002\u9664\u4e86\u5728\u5c4b\u9876\u94fa\u8bbe\u4e0d\u900f\u660e\u7684\u592a\u9633\u80fd\u7535\u6c60\u677f\u5916\uff0c\u5229\u7528\u5efa\u7b51\u7269\u4fa7\u7acb\u9762\u7684\u73bb\u7483\u5e55\u5899\u8fdb\u884c\u5149\u4f0f\u8f6c\u6362\u5df2\u6210\u4e3a\u5f53\u524d\u7684\u7814\u7a76\u70ed\u70b9\u3002\u4f5c\u4e3a\u4e00\u79cd\u534a\u900f\u660e\u5149\u4f0f\u5668\u4ef6\uff0c\u53d1\u5149\u592a\u9633\u80fd\u805a\u5149\u5668\uff08Luminescent Solar Concentrators\uff0cLSCs\uff09\u4e0d\u4ec5\u80fd\u6536\u96c6\u76f4\u5c04\u592a\u9633\u5149\uff0c\u8fd8\u80fd\u5728\u9634\u5929\u7b49\u6563\u5c04\u5149\u73af\u5883\u4ee5\u53ca\u9634\u5f71\u73af\u5883\u4e2d\u6709\u6548\u5229\u7528\u6f2b\u53cd\u5c04\u592a\u9633\u5149\u8fdb\u884c\u5149\u4f0f\u8f6c\u6362\uff0c\u4ece\u800c\u4e3a\u9634\u5f71\u6548\u5e94\u4e25\u91cd\u7684\u57ce\u5e02\u5efa\u7b51\u4e2d\u4fa7\u7acb\u9762\u5149\u4f0f\u73bb\u7483\u5e55\u5899\u5e94\u7528\u63d0\u4f9b\u4e86\u65b0\u65b9\u6848\u3002\u7136\u800c\uff0c\u4e3a\u4e86\u5b58\u50a8LSCs\u4ea7\u751f\u7684\u5149\u4f0f\u7535\u80fd\u9700\u8981\u8fde\u63a5\u50a8\u80fd\u6a21\u5757\u548c\u7535\u538b\u8c03\u8282\u6a21\u5757\uff0c\u8fd9\u4e9b\u9644\u52a0\u6a21\u5757\u4e0d\u4ec5\u964d\u4f4e\u4e86LSCs\u7684\u6709\u6548\u5de5\u4f5c\u9762\u79ef\uff0c\u8fd8\u589e\u52a0\u4e86\u5b89\u88c5\u7a7a\u95f4\uff0c\u4e0d\u5229\u4e8e\u5728\u5149\u4f0f\u73bb\u7483\u5e55\u5899\u573a\u666f\u4e2d\u7684\u5e94\u7528\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong>\u4e8c\u3001\u3010\u6210\u679c\u63a0\u5f71\u3011<\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c\u4e1c\u5357\u5927\u5b66\u738b\u6625\u96f7\u7814\u7a76\u5458\u3001\u5f90\u6dd1\u5b8f\u526f\u7814\u7a76\u5458\u5728\u56fd\u9645\u5b66\u672f\u671f\u520a\u300aNature Communications\u300b\uff08\u81ea\u7136\u901a\u8baf\uff09\u53d1\u8868\u4e86\u9898\u4e3a\u201cIntegrated Device of Luminescent Solar Concentrators and Electrochromic Supercapacitors for Self-powered Smart Window and Display\uff08\u7528\u4e8e\u81ea\u4f9b\u7535\u667a\u80fd\u7a97\u548c\u663e\u793a\u7684\u53d1\u5149\u592a\u9633\u80fd\u805a\u5149\u5668\u548c\u7535\u81f4\u53d8\u8272\u8d85\u7ea7\u7535\u5bb9\u5668\u96c6\u6210\u5668\u4ef6\uff09\u201d\u7684\u7814\u7a76\u8bba\u6587\u3002\u8be5\u8bba\u6587\u63d0\u51fa\u4e86\u4e00\u79cd\u5177\u5907\u5149\u4f0f\u8f6c\u6362\u3001\u80fd\u91cf\u5b58\u50a8\u548c\u7535\u81f4\u53d8\u8272\u4e09\u79cd\u529f\u80fd\u7684\u65b0\u578b\u96c6\u6210\u5668\u4ef6\uff0c\u5e76\u5c06\u5176\u7528\u4e8e\u81ea\u4f9b\u7535\u667a\u80fd\u7a97\u548c\u4fe1\u606f\u663e\u793a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265436\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72471-13.png\" alt=\"\" width=\"746\" height=\"448\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72471-13.png 746w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72471-13-300x180.png 300w\" sizes=\"(max-width: 746px) 100vw, 746px\" \/>\u00a0\u00a0\u00a0\u00a0<\/p>\n<p><strong>\u4e09\u3001\u3010\u6838\u5fc3\u521b\u65b0\u70b9\u3011<\/strong><\/p>\n<p><strong>\u00a0<\/strong><\/p>\n<p>\u8be5\u5de5\u4f5c\u5f00\u53d1\u4e86\u4e00\u79cd\u57fa\u4e8eLSCs\u548c\u7535\u81f4\u53d8\u8272\u8d85\u7ea7\u7535\u5bb9\u5668\uff08Electrochromic Supercapacitors, ECSs\uff09\u7684\u201c\u9762\u5bf9\u9762\u201d\u96c6\u6210\u5668\u4ef6\u3002\u901a\u8fc7\u9009\u62e9\u7535\u538b\u7a97\u53e3\u5339\u914d\u7684\u7535\u6781\u7ec4\u5408\uff0cLSCs\u4ea7\u751f\u7684\u5149\u4f0f\u7535\u80fd\u53ef\u4ee5\u76f4\u63a5\u5b58\u50a8\u5728ECSs\u4e2d\uff0c\u65e0\u9700\u989d\u5916\u914d\u5907\u50a8\u80fd\u6a21\u5757\u548c\u7535\u538b\u8c03\u8282\u6a21\u5757\uff0c\u4ece\u800c\u663e\u8457\u63d0\u9ad8\u4e86\u5668\u4ef6\u7684\u6709\u6548\u5de5\u4f5c\u9762\u79ef\u5e76\u964d\u4f4e\u4e86\u6210\u672c\u3002ECSs\u4e0d\u4ec5\u5177\u5907\u50a8\u80fd\u529f\u80fd\uff0c\u8fd8\u8868\u73b0\u51fa\u53ef\u9006\u7684\u7535\u81f4\u53d8\u8272\u7279\u6027\uff0c\u5176\u53ef\u89c1\u5149\u4e0e\u8fd1\u7ea2\u5916\u5149\u900f\u8fc7\u7387\u80fd\u591f\u6839\u636e\u5b58\u50a8\u7684\u7535\u91cf\u52a8\u6001\u8c03\u8282\u3002\u901a\u8fc7\u63a7\u5236ECSs\u7684\u5145\u653e\u7535\u8fc7\u7a0b\uff0c\u8fd9\u79cd\u96c6\u6210\u5668\u4ef6\u8fd8\u53ef\u7528\u4f5c\u81ea\u4f9b\u7535\u7684\u7535\u81f4\u53d8\u8272\u667a\u80fd\u7a97\u6216\u4fe1\u606f\u6307\u4ee4\u663e\u793a\u5668\u3002\u8fd9\u79cd\u96c6\u5149\u4f0f\u8f6c\u6362\u3001\u80fd\u91cf\u5b58\u50a8\u548c\u7535\u81f4\u53d8\u8272\u4e09\u79cd\u529f\u80fd\u4e8e\u4e00\u4f53\u7684\u521b\u65b0\u5668\u4ef6\uff0c\u4e3a\u5efa\u7b51\u667a\u80fd\u7a97\u6237\u63d0\u4f9b\u4e86\u4e00\u79cd\u9ad8\u6548\u4e14\u591a\u529f\u80fd\u7684\u66ff\u4ee3\u65b9\u6848\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong>\u56db\u3001\u3010\u6570\u636e\u6982\u89c8\u3011<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265437\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72472-14.png\" alt=\"\" width=\"1351\" height=\"817\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72472-14.png 1351w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72472-14-300x181.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72472-14-768x464.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72472-14-1024x619.png 1024w\" sizes=\"(max-width: 1351px) 100vw, 1351px\" \/><\/p>\n<p><strong><b>\u56fe1\u3001LSCs-ECSs\u96c6\u6210\u5668\u4ef6\u7684\u7ed3\u6784\u548c\u8c03\u5236\u673a\u7406\u793a\u610f\u56fe\u3002<\/b><\/strong>\u5728\u592a\u9633\u7167\u5c04\u4e0b\uff0cLSCs\u4ea7\u751f\u7684\u7535\u80fd\u4f1a\u88ab\u50a8\u5b58\u5728ECSs\u4e2d\uff0c\u540c\u65f6\u4f7fECSs\u7684\u900f\u8fc7\u7387\u964d\u4f4e\u4ee5\u963b\u6321\u5149\u7ebf\u7684\u5165\u5c04\u3002<\/p>\n<p><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265438\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72473-11.png\" alt=\"\" width=\"1269\" height=\"662\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72473-11.png 1269w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72473-11-300x157.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72473-11-768x401.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72473-11-1024x534.png 1024w\" sizes=\"(max-width: 1269px) 100vw, 1269px\" \/><\/b><\/strong><\/p>\n<p><strong><b>\u56fe2<\/b><\/strong><strong><b>\u3001<\/b><\/strong><strong><b>PANI-600\/WO<\/b><\/strong><strong><sub><b>3<\/b><\/sub><\/strong><strong><b>-45 ECSs\u7684<\/b><\/strong><strong><b>\u80fd\u91cf\u5b58\u50a8\u548c\u7535\u81f4\u53d8\u8272<\/b><\/strong><strong><b>\u6027\u80fd\u3002<\/b><\/strong>a\u57280 ~ 1.4 V\u7535\u538b\u7a97\u4e2d\u4e0d\u540c\u626b\u63cf\u901f\u7387\u4e0b\u7684\u5faa\u73af\u4f0f\u5b89\u66f2\u7ebf\uff1bb\u4e0d\u540c\u7535\u6d41\u5bc6\u5ea6\u4e0b\u7684\u6052\u7535\u6d41\u5145\u653e\u7535\u66f2\u7ebf\uff1bc Ragone\u56fe\u548c\u4e0d\u540c\u7535\u6d41\u5bc6\u5ea6\u4e0b\u7684\u9762\u79ef\u7535\u5bb9\u3002\u63d2\u56fe\uff1a\u5149\u5b66\u56fe\u50cf\u663e\u793a\u4e00\u4e2aECSs\u8db3\u4ee5\u70b9\u4eae\u4e00\u4e2a\u8ba1\u65f6\u5668\u3002d 0 V\u30010.4 V\u30010.8 V\u30011.2 V\u30011.4 V\u65f6\u5668\u4ef6\u7684\u900f\u5c04\u5149\u8c31\uff1be\u5728550nm\u6d4b\u91cf\u53ef\u9006\u5f00\u5173\u65f6\u7684\u5b9e\u65f6\u900f\u5c04\u7387\u53d8\u5316\uff1bf\u57281mA\u00a0cm<sup>\u22122<\/sup>\u7535\u6d41\u5bc6\u5ea6\u4e0b\u7ecf\u8fc71200\u6b21\u5faa\u73af\uff0c\u5668\u4ef6\u7684\u7535\u5bb9\u548c\u7535\u81f4\u53d8\u8272\u7a33\u5b9a\u6027\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265439\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72474-11.png\" alt=\"\" width=\"1269\" height=\"635\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72474-11.png 1269w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72474-11-300x150.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72474-11-768x384.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72474-11-1024x512.png 1024w\" sizes=\"(max-width: 1269px) 100vw, 1269px\" \/><\/p>\n<p><strong><b>\u56fe3<\/b><\/strong><strong><b>\u3001<\/b><\/strong><strong><b>LSCs\u7684<\/b><\/strong><strong><b>\u5149\u7535<\/b><\/strong><strong><b>\u6027\u80fd<\/b><\/strong><strong><b>\u3002<\/b><\/strong>a CsPbI<sub>3<\/sub>\/PMMA\u590d\u5408\u8584\u819c\u7684\u900f\u5149\u7387\u3002\u63d2\u56fe\uff1a\u73af\u5883\u5149\u4e0b\u5e26\u6709\u73bb\u7483\u57fa\u677f\u7684CsPbI<sub>3<\/sub>\/PMMA\u590d\u5408\u8584\u819c\u7684\u7167\u7247\uff1bb CsPbI<sub>3<\/sub>\/PMMA\u590d\u5408\u819c\u7684\u5149\u81f4\u53d1\u5149\uff08PL\uff09\u548c\u5149\u81f4\u53d1\u5149\u6fc0\u53d1\uff08PLE\uff09\u5149\u8c31\u3002\u4f7f\u7528\u900f\u660e\u73bb\u7483\u6d4b\u91cf\u57fa\u7ebf\uff1bc CsPbI<sub>3<\/sub>\/PMMA\u590d\u5408\u819c\u7684\u5438\u6536\u66f2\u7ebf\uff0c\u4ee5\u53ca\u6807\u51c6\u592a\u9633\u5149\u8c31AM 1.5 G\uff1bd LSCs\u7684\u6b63\u9762\u548c\u4fa7\u9762\u53d1\u5c04\uff1be 1\u592a\u9633\u6761\u4ef6\u4e0bPV\u7535\u6c60\u4e0eLSCs\u8fb9\u7f18\u8026\u5408\u7684J-V\u66f2\u7ebf\u3002\u5176\u4e2d\uff0cV<sub>oc<\/sub>\u4e3a\u5f00\u8def\u7535\u538b\uff0cI<sub>sc<\/sub>\u4e3a\u77ed\u8def\u7535\u6d41\uff0cFF\u4e3a\u586b\u5145\u7cfb\u6570\uff0cJ<sub>sc<\/sub>\u4e3a\u77ed\u8def\u7535\u6d41\u5bc6\u5ea6\uff1bf\u4e0d\u540c\u5149\u8defCsPbI<sub>3<\/sub>\/PMMA LSCs\u7684PL\u5f3a\u5ea6\u3002\u63d2\u56fe\uff1a\u4e0d\u540c\u5149\u8def\u7684\u5149\u5f3a\u6d4b\u91cf\u539f\u7406\u56fe\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265440\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72475-10.png\" alt=\"\" width=\"1268\" height=\"618\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72475-10.png 1268w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72475-10-300x146.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72475-10-768x374.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72475-10-1024x499.png 1024w\" sizes=\"(max-width: 1268px) 100vw, 1268px\" \/><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>4\u3001<\/b><\/strong><strong><b>LSCs-ECSs<\/b><\/strong><strong><b>\u96c6\u6210\u5668\u4ef6<\/b><\/strong><strong><b>\u7684<\/b><\/strong><strong><b>\u5149\u7535<\/b><\/strong><strong><b>\u6027\u80fd<\/b><\/strong><strong><b>\u3002<\/b><\/strong>a\u8bbe\u5907\u7684\u7535\u8def\u56fe\uff1bb\u96c6\u6210\u5668\u4ef6\u57281\u4e2a\u592a\u9633\u5149\u7167\u6761\u4ef6\u4e0b\u5145\u7535\u8fc7\u7a0b\u548c\u5728\u9ed1\u6697\u73af\u5883\u4e0d\u540c\u7535\u6d41\u5bc6\u5ea6\u4e0b\u653e\u7535\u8fc7\u7a0b\u7684V-t\u66f2\u7ebf\uff1bc 1\u4e2a\u592a\u9633\u6761\u4ef6\u4e0b\uff0c\u4e0d\u540c\u5145\u7535\u65f6\u95f4\u7684\u96c6\u6210\u5668\u4ef6\u7684\u900f\u5c04\u5149\u8c31\uff1bd\u96c6\u6210\u5668\u4ef6\u5728\u5b8c\u5168\u653e\u7535\u548c\u5b8c\u5168\u5145\u7535\u72b6\u6001\u4e0b\u7684\u7167\u7247\uff1be 1\u4e2a\u592a\u9633\u6761\u4ef6\u4e0b\u4e0d\u540c\u5145\u7535\u72b6\u6001\u7684\u96c6\u6210\u5668\u4ef6\u7684J-V\u66f2\u7ebf\uff1bf\u96c6\u6210\u5668\u4ef6\u5728\u5145\u7535\/\u653e\u7535\u72b6\u6001\u4e0b\u7684\u592a\u9633\u8f90\u7167\u5149\u8c31\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265441\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72476-10.png\" alt=\"\" width=\"1268\" height=\"719\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72476-10.png 1268w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72476-10-300x170.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72476-10-768x435.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72476-10-1024x581.png 1024w\" sizes=\"(max-width: 1268px) 100vw, 1268px\" \/><\/p>\n<p><strong><b>\u56fe5<\/b><\/strong><strong><b>\u3001<\/b><\/strong><strong><b>\u57fa\u4e8eLSCs-ECSs\u96c6\u6210\u5668\u4ef6\u7684\u81ea\u4f9b\u7535\u663e\u793a\u5668<\/b><\/strong><strong><b>\u3002<\/b><\/strong>a\u7535\u81f4\u53d8\u8272\u663e\u793a\u5668\u7684\u5236\u5907\u793a\u610f\u56fe\u3002\u805a\u6c2f\u4e59\u70ef\uff08PVC\uff09\u8d34\u7eb8\u7528\u4f5c\u6a21\u677f\uff1bb\u81ea\u4f9b\u7535\u663e\u793a\u5668\u7684\u7b49\u6548\u7535\u8def\u3002\u5c06S1\u548cS2\u540c\u65f6\u63a5\u5728\u7ea2\u8272\u6216\u7eff\u8272\u7ebf\u4e0a\uff0c\u5206\u522b\u5b9e\u73b0I\u6863\u548cII\u6863\u7684\u63a5\u901a\u3002\u5f53S3\u5355\u72ec\u6253\u5f00\u65f6\uff0c\u8bbe\u5907\u5904\u4e8e\u6863\u4f4d\u201c0\u201d\uff1bc\u81ea\u4f9b\u7535\u663e\u793a\u5668\u5728\u4e09\u79cd\u4e0d\u540c\u5f00\u5173\u72b6\u6001\u4e0b\u7684\u5149\u5b66\u7167\u7247\uff1bd\u81ea\u4f9b\u7535\u663e\u793a\u5668\u57281\u4e2a\u592a\u9633\u6761\u4ef6\u4e0b\u7684V-t\u66f2\u7ebf\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong>\u4e94\u3001\u3010\u6210\u679c\u542f\u793a\u3011<\/strong><\/p>\n<p>&nbsp;<\/p>\n<p>\u8be5\u5de5\u4f5c\u901a\u8fc7\u7b80\u5355\u7684\u201c\u9762\u5bf9\u9762\u201d\u7ec4\u88c5\u7684\u65b9\u5f0f\u5c06\u53d1\u5149\u592a\u9633\u80fd\u805a\u5149\u5668\u548c\u7535\u81f4\u53d8\u8272\u8d85\u7ea7\u7535\u5bb9\u5668\u96c6\u6210\uff0c\u5f97\u5230\u4e86\u96c6\u5149\u4f0f\u8f6c\u6362\u3001\u80fd\u91cf\u5b58\u50a8\u548c\u7535\u81f4\u53d8\u8272\u4e09\u79cd\u529f\u80fd\u4e8e\u4e00\u4f53\u7684\u521b\u65b0\u5668\u4ef6\u3002\u8fd9\u63a8\u52a8\u4e86\u53d1\u5149\u592a\u9633\u80fd\u805a\u5149\u5668\u5728\u900f\u660e\u5149\u4f0f\u9886\u57df\u7684\u5b9e\u9645\u5e94\u7528\uff0c\u4e5f\u4e3a\u5efa\u7b51\u667a\u80fd\u7a97\u6237\u63d0\u4f9b\u4e86\u4e00\u79cd\u9ad8\u6548\u4e14\u591a\u529f\u80fd\u7684\u66ff\u4ee3\u65b9\u6848\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong>\u539f\u6587\u8be6\u60c5\uff1a<\/strong><\/p>\n<p>&nbsp;<\/p>\n<p>\u9898\u76ee\uff1aIntegrated device of luminescent solar concentrators and electrochromic supercapacitors for self-powered smart window and display<\/p>\n<p>&nbsp;<\/p>\n<p>\u4f5c\u8005\uff1aShichao Huang, Haotian Guo, Pengfei Xia, Hongcan Sun, Changgui Lu, Yuge Feng, Jing Zhu, Cai Liang, Shuhong Xu*\u00a0&amp; Chunlei Wang*<\/p>\n<p>&nbsp;<\/p>\n<p>\u6587\u7ae0\u94fe\u63a5\uff1a<a href=\"https:\/\/doi.org\/10.1038\/s41467-025-57369-6\">https:\/\/doi.org\/10.1038\/s41467-025-57369-6<\/a><\/p>\n<p>&nbsp;<\/p>\n<p>\u672c\u6587\u7531\u6587\u7ae0\u56e2\u961f\u4f9b\u7a3f<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4e00\u3001\u00a0\u3010\u5bfc\u8bfb\u3011 \u5efa\u7b51\u7269\u80fd\u8017\u5728\u5168\u7403\u603b\u80fd\u8017\u4e2d\u5360\u6bd4\u8fbe30%-40%\uff0c\u63d0\u9ad8\u5efa\u7b51\u7269\u80fd\u6e90\u81ea\u7ed9\u80fd\u529b\u5df2\u6210\u4e3a\u56fd\u9645\u793e\u4f1a\u7684\u666e\u904d\u5171\u8bc6\u3002\u9664\u4e86\u5728\u5c4b\u9876\u94fa\u8bbe\u4e0d\u900f\u660e\u7684\u592a\u9633\u80fd\u7535\u6c60\u677f\u5916\uff0c\u5229\u7528\u5efa\u7b51\u7269\u4fa7&#8230;<\/p>\n","protected":false},"author":14360,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-265435","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/265435"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/14360"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=265435"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/265435\/revisions"}],"predecessor-version":[{"id":265444,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/265435\/revisions\/265444"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=265435"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=265435"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=265435"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}