{"id":265714,"date":"2025-03-26T07:31:12","date_gmt":"2025-03-25T23:31:12","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=265714"},"modified":"2025-03-25T23:42:25","modified_gmt":"2025-03-25T15:42:25","slug":"ku-leuven-monash-university-%e5%8d%8e%e4%b8%ad%e7%a7%91%e6%8a%80%e5%a4%a7%e5%ad%a6%e8%81%94%e5%90%88%e5%9b%a2%e9%98%9f%e5%9c%a8advanced-functional-materials%e5%8f%91%e8%a1%a8%e7%95%8c%e9%9d%a2","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=265714","title":{"rendered":"KU Leuven &#038; Monash University &#038; \u534e\u4e2d\u79d1\u6280\u5927\u5b66\u8054\u5408\u56e2\u961f\u5728Advanced Functional Materials\u53d1\u8868\u754c\u9762\u805a\u5408\u6784\u7b51\u6e17\u900f\u6c7d\u5316\u819c\u7814\u7a76\u8fdb\u5c55\u7efc\u8ff0"},"content":{"rendered":"<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265715\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72471-37.png\" alt=\"\" width=\"600\" height=\"263\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72471-37.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72471-37-300x132.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u521b\u65b0\u6210\u679c\uff1a<\/p>\n<p>\u8fd1\u5e74\u6765\uff0c\u754c\u9762\u805a\u5408\uff08Interfacial Polymerization, IP\uff09\u4f5c\u4e3a\u6784\u5efa\u8d85\u8584\u9009\u62e9\u6027\u5c42\u7684\u9ad8\u6548\u6280\u672f\uff0c\u5728\u819c\u5206\u79bb\u9886\u57df\u4e2d\u5c55\u73b0\u51fa\u5de8\u5927\u6f5c\u529b\u3002\u8fd1\u65e5\uff0c\u6bd4\u5229\u65f6\u8377\u8bed\u9c81\u6c76\u5927\u5b66\uff08KU Leuven\uff09\u9773\u9e4f\u745e\u535a\u58eb\uff0cBart. Van der Bruggen \u6559\u6388&amp;\u534e\u4e2d\u79d1\u6280\u5927\u5b66\u8881\u672f\u73ca\u6559\u6388&amp;\u6fb3\u6d32\u83ab\u7eb3\u4ec0\u5927\u5b66\uff08Monash University\uff09\u738b\u7115\u5ead\u6559\u6388\u56e2\u961f\u5728Advanced Functional Materials\u5408\u4f5c\u64b0\u5199\u4e86\u9898\u4e3a\u201d<em><i>Recent Advances in Membrane Synthesis by Interfacial Polymerization for Pervaporation<\/i><\/em>\u201d\u00a0\u7684\u7efc\u8ff0\u8bba\u6587\u5e76\u53d1\u8868\u4e8eAdv. Funct. Mater.\u3002\u8be5\u6587\u7cfb\u7edf\u68b3\u7406\u4e86\u754c\u9762\u805a\u5408\uff08Interfacial Polymerization, IP\uff09\u6784\u5efa\u6e17\u900f\u6c7d\u5316\uff08Pervaporation, PV\uff09\u819c\u6750\u6599\u7684\u6700\u65b0\u7814\u7a76\u8fdb\u5c55\u3001\u5173\u952e\u6311\u6218\u4e0e\u672a\u6765\u53d1\u5c55\u8d8b\u52bf\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong><b>\u7814\u7a76\u80cc\u666f<\/b><\/strong>\uff1a\u80fd\u6e90\u4e0e\u6c34\u8d44\u6e90\u53cc\u91cd\u5371\u673a\u9a71\u52a8\u4e0b\u7684\u819c\u5206\u79bb\u9769\u65b0<\/p>\n<p>\u5728\u201c\u53cc\u78b3\u76ee\u6807\u201d\u9a71\u52a8\u4e0b\uff0c\u5982\u4f55\u63d0\u5347\u5206\u79bb\u6548\u7387\u3001\u964d\u4f4e\u80fd\u8017\u5df2\u6210\u4e3a\u5316\u5de5\u8fc7\u7a0b\u6280\u672f\u7684\u6838\u5fc3\u8bae\u9898\u3002\u6e17\u900f\u6c7d\u5316\u4f5c\u4e3a\u4e00\u79cd\u80fd\u5b9e\u73b0\u201c\u6db2\u4f53\u2192\u6c14\u4f53\u201d\u8de8\u76f8\u9ad8\u6548\u5206\u79bb\u7684\u819c\u8fc7\u7a0b\u6280\u672f\uff0c\u56e0\u5176\u9002\u7528\u4e8e\u6709\u673a\u6eb6\u5242\u8131\u6c34\u3001\u751f\u7269\u71c3\u6599\u63d0\u7eaf\u3001\u6d77\u6c34\u8131\u76d0\u53ca\u9ad8\u76d0\u5e9f\u6c34\u6d53\u7f29\u7b49\u573a\u666f\uff0c\u6210\u4e3a\u8fd1\u5e74\u6765\u56fd\u9645\u7814\u7a76\u70ed\u70b9\u3002\u4e0e\u4f20\u7edf\u84b8\u998f\u76f8\u6bd4\uff0cPV\u8fc7\u7a0b\u65e0\u9700\u6c7d\u5316\u5168\u90e8\u7269\u6599\uff0c\u80fd\u8017\u66f4\u4f4e\uff1b\u800c\u76f8\u6bd4\u53cd\u6e17\u900f\u3001\u819c\u84b8\u998f\u7b49\u538b\u529b\/\u70ed\u9a71\u52a8\u8fc7\u7a0b\uff0cPV\u5bf9\u8fdb\u6599\u6761\u4ef6\u9002\u5e94\u6027\u66f4\u5f3a\uff0c\u5c24\u5176\u5728\u9187\u7c7b\u6df7\u5408\u7269\u8131\u6c34\u3001\u542b\u76d0\u6eb6\u6db2\u6d53\u7f29\u7b49\u9ad8\u6311\u6218\u4f53\u7cfb\u4e2d\u8868\u73b0\u51fa\u663e\u8457\u4f18\u52bf\u3002\u7136\u800c\uff0cPV\u819c\u5728\u5b9e\u9645\u5e94\u7528\u4e2d\u4ecd\u9762\u4e34\u201c\u901a\u91cf-\u9009\u62e9\u6027\u201d\u96be\u4ee5\u517c\u987e\u7684\u95ee\u9898\u3002\u5982\u4f55\u6784\u5efa\u8d85\u8584\u3001\u7f3a\u9677\u5c11\u3001\u754c\u9762\u7a33\u5b9a\u7684\u9009\u62e9\u6027\u5c42\u7ed3\u6784\u6210\u4e3a\u7a81\u7834\u74f6\u9888\u7684\u5173\u952e\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong><b>\u6587\u7ae0\u4eae\u70b9<\/b><\/strong>\uff1a\u805a\u7126\u754c\u9762\u805a\u5408\u6784\u5efa\u9ad8\u6027\u80fdPV\u819c\u7684\u5168\u666f\u5f0f\u5206\u6790<\/p>\n<p>\u672c\u7efc\u8ff0\u56f4\u7ed5\u201c\u754c\u9762\u805a\u5408\u201d\u5728PV\u819c\u5236\u5907\u4e2d\u7684\u5e94\u7528\uff0c\u5168\u9762\u603b\u7ed3\u4e86\u8fc7\u53bb\u4e94\u5e74\u5185\u7684\u7814\u7a76\u8fdb\u5c55\uff0c\u6db5\u76d6\u4ee5\u4e0b\u51e0\u4e2a\u65b9\u9762\uff1a<\/p>\n<ol>\n<li>\u6e17\u900f\u6c7d\u5316\u57fa\u7840\u4e0e\u819c\u5206\u79bb\u673a\u5236<\/li>\n<\/ol>\n<p>\u7cfb\u7edf\u4ecb\u7ecdPV\u819c\u4e2d\u8d28\u91cf\u4f20\u8f93\u7684\u201c\u6eb6\u89e3-\u6269\u6563\u201d\u673a\u5236\uff1b\u68b3\u7406PV\u819c\u6027\u80fd\u8bc4\u4ef7\u6307\u6807\uff08\u5982\u6e17\u900f\u901a\u91cf\u3001\u5206\u79bb\u56e0\u5b50\u3001PSI\u6307\u6570\u7b49\uff09\uff1b\u5bf9\u6bd4\u4f20\u7edf\u84b8\u998f\u3001\u53cd\u6e17\u900f\u3001\u819c\u84b8\u998f\u4e0ePV\u7684\u80fd\u8017\u4e0e\u9002\u7528\u8303\u56f4\u3002<\/p>\n<ol start=\"2\">\n<li>\u754c\u9762\u805a\u5408\u6784\u5efa\u9009\u62e9\u6027\u5c42\u7684\u5173\u952e\u7b56\u7565<\/li>\n<\/ol>\n<p>\u603b\u7ed3\u4e0d\u540c\u5355\u4f53\uff08\u80fa\u7c7b\u4e0e\u9170\u6c2f\u7c7b\uff09\u5728\u53cd\u5e94\u901f\u7387\u3001\u4ea4\u8054\u7a0b\u5ea6\u3001\u819c\u7ed3\u6784\u65b9\u9762\u7684\u5f71\u54cd\uff1b\u6bd4\u8f83\u4e0d\u540c\u5b98\u80fd\u56e2\uff08\u4f8b\u5982\u4e59\u9187\u80fa\u3001\u82b3\u9999\u80fa\uff09\u5bf9\u819c\u6027\u80fd\u8c03\u63a7\u673a\u5236\uff1b\u5206\u6790IP\u8fc7\u7a0b\u53c2\u6570\uff08\u6d53\u5ea6\u3001\u65f6\u95f4\u3001\u6e29\u5ea6\uff09\u7684\u7ed3\u6784-\u6027\u80fd\u5173\u8054\u6027\u3002<\/p>\n<ol start=\"3\">\n<li>\u4e2d\u95f4\u5c42\u4e0e\u652f\u6491\u5c42\u7684\u534f\u540c\u4f18\u5316<\/li>\n<\/ol>\n<p>\u63a2\u8ba8\u591a\u79cd\u4e2d\u95f4\u5c42\u6750\u6599\uff08\u5982eGO\u3001MOFs\u3001COFs\u3001TiO\u2082\u3001MXene\uff09\u5bf9\u819c\u7ed3\u6784\u8c03\u63a7\u4f5c\u7528\uff1b\u5206\u6790\u805a\u5408\u7269\u652f\u6491\uff08\u5982PAN\u3001PES\uff09\u4e0e\u9676\u74f7\u652f\u6491\uff08\u5982AAO\u3001Al\u2082O\u2083\uff09\u5728\u6297\u6eb6\u80c0\u4e0e\u673a\u68b0\u7a33\u5b9a\u6027\u65b9\u9762\u7684\u4f18\u52a3\uff1b\u9610\u8ff0\u4e2d\u95f4\u5c42\u7684\u201cgutter mechanism\u201d\u5728\u63d0\u5347\u6c34\u901a\u91cf\u4e0e\u754c\u9762\u517c\u5bb9\u6027\u65b9\u9762\u7684\u91cd\u8981\u6027\u3002<\/p>\n<ol start=\"4\">\n<li>\u65b0\u5174\u6750\u6599\u5f15\u9886\u819c\u6027\u80fd\u7a81\u7834<\/li>\n<\/ol>\n<p>\u4ecb\u7ecdMOFs\u3001COFs\u3001POCs\u7b49\u65b0\u578b\u591a\u5b54\u6750\u6599\u5728IP\u9009\u62e9\u6027\u5c42\u4e2d\u7684\u5e94\u7528\uff1b\u63a2\u8ba8\u5176\u5728\u8c03\u63a7\u5b54\u5f84\u3001\u8868\u9762\u5316\u5b66\u6027\u8d28\u3001\u4eb2\u6c34\u6027\u53ca\u7a33\u5b9a\u6027\u65b9\u9762\u7684\u4f18\u52bf\uff1b\u5c55\u671b\u4ee5COF\u9aa8\u67b6\u3001\u5c42\u72b62D\u6750\u6599\u4e3a\u6838\u5fc3\u6784\u7b51\u4e0b\u4e00\u4ee3\u8d85\u8584\u9ad8\u901a\u91cf\u819c\u7684\u7814\u7a76\u8d8b\u52bf\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong><b>\u5e94\u7528\u5c55\u671b<\/b><\/strong>\uff1a\u4e3a\u53ef\u6301\u7eed\u5206\u79bb\u63d0\u4f9b\u6750\u6599\u652f\u6491<\/p>\n<p>\u672c\u7efc\u8ff0\u6307\u51fa\uff0c\u672a\u6765PV\u819c\u6280\u672f\u7684\u53d1\u5c55\u65b9\u5411\u5c06\u96c6\u4e2d\u5728\uff1a\u5355\u4f53\u7ed3\u6784\u4e0e\u53cd\u5e94\u754c\u9762\u534f\u540c\u8c03\u63a7\uff1b\u591a\u5c3a\u5ea6\u819c\u7ed3\u6784\u7684\u6784\u5efa\uff08\u81ea\u7ec4\u88c5\u3001\u4e2d\u95f4\u5c42\u6784\u578b\uff09\uff1b\u9ad8\u6027\u80fd\u3001\u4f4e\u80fd\u8017\u3001\u53ef\u89c4\u6a21\u5316\u5236\u5907\u7684\u590d\u5408\u819c\u4f53\u7cfb\uff1b<\/p>\n<p>\u9762\u5411\u5de5\u4e1a\u6eb6\u5242\u56de\u6536\u3001\u6d77\u6c34\u6de1\u5316\u7b49\u590d\u6742\u573a\u666f\u7684\u6297\u6c61\u67d3\u4e0e\u7a33\u5b9a\u6027\u589e\u5f3a\u8bbe\u8ba1\u3002<\/p>\n<p>\u6587\u7ae0\u5f3a\u8c03\uff0c\u6784\u7b51\u9ad8\u6027\u80fd\u6e17\u900f\u6c7d\u5316\u819c\u7684\u6838\u5fc3\uff0c\u662f\u6750\u6599\u8bbe\u8ba1\u3001\u754c\u9762\u8c03\u63a7\u4e0e\u591a\u5c42\u7ed3\u6784\u534f\u540c\u6784\u5efa\u7684\u7edf\u4e00\uff0c\u754c\u9762\u805a\u5408\u6280\u672f\u4e3a\u8fd9\u4e00\u76ee\u6807\u63d0\u4f9b\u4e86\u5f3a\u6709\u529b\u7684\u624b\u6bb5\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265728\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72472-2.jpg\" alt=\"\" width=\"1000\" height=\"1109\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72472-2.jpg 1000w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72472-2-271x300.jpg 271w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72472-2-768x852.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72472-2-923x1024.jpg 923w\" sizes=\"(max-width: 1000px) 100vw, 1000px\" \/><\/p>\n<p>\u56fe1\u5c55\u793a\u4e86\u5178\u578b\u819c\u5206\u79bb\u6280\u672f\u7684\u57fa\u672c\u8fc7\u7a0b\u4e0e\u673a\u5236\uff1a(a-b)\u4e3a\u53cd\u6e17\u900f\u8fc7\u7a0b\u4e2d\u6c34\u5206\u5b50\u901a\u8fc7\u534a\u900f\u819c\u4ee5\u53ca\u819c\u8868\u9762\u751f\u7269\u819c\u5f62\u6210\u7684\u793a\u610f\uff1b(c)\u5c55\u793a\u4e86\u4f20\u7edf\u819c\u84b8\u998f\u5de5\u827a\u7684\u4e0d\u540c\u5b9e\u73b0\u8def\u5f84\uff0c\u5e76\u6807\u793a\u4e86\u819c\u6c61\u67d3\u7684\u5178\u578b\u90e8\u4f4d\uff1b(d)\u4e3a\u6e17\u900f\u6c7d\u5316\u8fc7\u7a0b\u53ca\u5176\u5de5\u4f5c\u673a\u5236\uff1b(e)\u5219\u4e3a\u6e17\u900f\u6c7d\u5316\u4e2d\u57fa\u4e8e\u6eb6\u89e3-\u6269\u6563\u6a21\u578b\u7684\u4f20\u8d28\u673a\u5236\u56fe\u793a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265729\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72473-3.jpg\" alt=\"\" width=\"1000\" height=\"1183\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72473-3.jpg 1000w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72473-3-254x300.jpg 254w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72473-3-768x909.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72473-3-866x1024.jpg 866w\" sizes=\"(max-width: 1000px) 100vw, 1000px\" \/><\/p>\n<p>\u56fe2\u5c55\u793a\u4e86\u754c\u9762\u805a\u5408\uff08IP\uff09\u76f8\u5173\u7814\u7a76\u7684\u5173\u952e\u53d1\u5c55\u4e0e\u819c\u7ed3\u6784\u7279\u5f81\uff1a(a)\u4e3aIP\u6280\u672f\u7684\u91cd\u8981\u53d1\u5c55\u5386\u7a0b\u65f6\u95f4\u8f74\uff1b(b)\u5c55\u793a\u4e86\u4e09\u7fa7\u6c2f\uff08TMC\uff09\u4e0e\u95f4\u82ef\u4e8c\u80fa\uff08MPD\uff09\u4e4b\u95f4\u7684\u5178\u578bIP\u53cd\u5e94\u8fc7\u7a0b\uff0c\u63d2\u56fe\u8fdb\u4e00\u6b65\u8bf4\u660e\u4e86\u819c\u7684\u5f62\u6210\u673a\u5236\u4e0e\u6e17\u900f\u6027\u80fd\uff1b(c)\u4e3a\u4e0d\u540c\u5f62\u8c8c\u7684\u7eb3\u7c73\u819c\u622a\u9762\u626b\u63cf\u7535\u955c\uff08SEM\uff09\u56fe\u50cf\uff0c\u5de6\u4e3a\u5e73\u6574\u819c\uff0c\u53f3\u4e3a\u8936\u76b1\u819c\uff1b(d)\u4e3a\u5728\u4e0d\u540c\u5355\u4f53\u6d53\u5ea6\u4e0b\uff0c\u819c\u539a\u5ea6\u968fIP\u53cd\u5e94\u65f6\u95f4\u53d8\u5316\u7684\u5173\u7cfb\u56fe\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265730\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72474-2.jpg\" alt=\"\" width=\"1000\" height=\"1139\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72474-2.jpg 1000w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72474-2-263x300.jpg 263w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72474-2-768x875.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72474-2-899x1024.jpg 899w\" sizes=\"(max-width: 1000px) 100vw, 1000px\" \/><\/p>\n<p>\u56fe3\u5c55\u793a\u4e86\u5178\u578bTFC\u819c\u7ed3\u6784\u53ca\u5176\u5728\u6e17\u900f\u6c7d\u5316\u4e2d\u7684\u5e94\u7528\u8868\u73b0\uff1a(a)\u4e3a\u4f20\u7edfTFC\u819c\u7684\u7ed3\u6784\u793a\u610f\u56fe\uff0c\u6807\u793a\u51fa\u5404\u529f\u80fd\u5c42\u7684\u5178\u578b\u7279\u5f81\uff1b(b)\u4e3a\u9996\u6b21\u5e94\u7528\u4e8e\u6e17\u900f\u6c7d\u5316\u7684IP\u819c\uff0c\u5c55\u793a\u4e86\u4e2d\u7a7a\u7ea4\u7ef4\u819c\u6a2a\u622a\u9762\u7684\u626b\u63cf\u7535\u955c\u56fe\u50cf\uff0c\u4e0a\u56fe\u4e3a\u805a\u82ef\u80fa\u6d82\u5c42\u819c\uff0c\u4e0b\u56fe\u4e3a\u805a\u4e8c\u4e59\u70ef\u82ef\u6d82\u5c42\u819c\uff1b(c)\u4e3a\u5bf9\u6bd4TFC\u819c\u4e0e\u63ba\u94f6\uff08Ag\uff09TFC\u819c\u7684SEM\u53caTEM\u622a\u9762\u56fe\u50cf\uff1b(d)\u4e3a\u4e0d\u540c\u7c7b\u578bTFC\u819c\u7684\u5206\u79bb\u6027\u80fd\u6d4b\u8bd5\u7ed3\u679c<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265731\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72475-2.jpg\" alt=\"\" width=\"1000\" height=\"875\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72475-2.jpg 1000w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72475-2-300x263.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72475-2-768x672.jpg 768w\" sizes=\"(max-width: 1000px) 100vw, 1000px\" \/><\/p>\n<p>\u56fe4\u5c55\u793a\u4e86\u4e0d\u540cIP\u819c\u7684\u7ed3\u6784\u7279\u5f81\u53ca\u6027\u80fd\u8bc4\u4ef7\u65b9\u6cd5\uff1a(a)\u4e3aNBDC\/mPAN\u590d\u5408\u819c\u7684\u7ed3\u6784\u56fe\uff1b(b)\u901a\u8fc7\u5149\u900f\u8fc7\u7387\u53d8\u5316\u53cd\u6620\u805a\u9170\u80fa\u53cd\u5e94\u901f\u7387\uff1b(c)\u4e3a\u4e09\u79cd\u4e0d\u540c\u5355\u4f53\u4f53\u7cfb\u5236\u5907\u7684TFC\u819c\u7684SEM\u56fe\u50cf\uff0c\u5206\u522b\u4e3a(c1) TFCBAE\u3001(c2) TFCBATO \u548c (c3) TFCODA\uff1b(d)\u4e3aMPD\/BDSC\u4e0eTETA\/BDSC\u4e24\u79cd\u5355\u4f53\u4f53\u7cfb\u5728IP\u8fc7\u7a0b\u4e2d\u7684\u805a\u5408\u4ea7\u7269\u793a\u610f\u56fe\uff1b(e)\u4e3a\u57fa\u4e8e\u6b63\u7535\u5b50\u6e6e\u6ca1\u5bff\u547d\u8c31\uff08PALS\uff09\u6d4b\u8bd5\u7684\u819c\u6750\u6599\u53c2\u6570\u4e0e\u6b63\u7535\u5b50\u5165\u5c04\u80fd\u91cf\u7684\u5173\u7cfb\u56fe.<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265732\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72476-2.jpg\" alt=\"\" width=\"1000\" height=\"1060\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72476-2.jpg 1000w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72476-2-283x300.jpg 283w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72476-2-768x814.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72476-2-966x1024.jpg 966w\" sizes=\"(max-width: 1000px) 100vw, 1000px\" \/><\/p>\n<p>\u56fe5\u5c55\u793a\u4e86\u9009\u62e9\u6027\u5c42\u7ed3\u6784\u8c03\u63a7\u4e0e\u590d\u5408\u819c\u6784\u5efa\u7b56\u7565\uff1a(a)\u4e3a\u539f\u5b50\u529b\u663e\u5fae\u955c\u56fe\u50cf\uff0c\u5206\u522b\u663e\u793a\u4e86\u5e73\u6574\u7eb3\u7c73\u819c(a1)\u4e0e\u8936\u76b1\u7eb3\u7c73\u819c(a2)\u7684\u5b9e\u9645\u957f\u5ea6\u4e0e\u8868\u89c2\u957f\u5ea6\u5bf9\u6bd4\uff1b(b)\u4e3a\u4e0d\u540ceGO\u6c89\u79ef\u91cf\uff080\u300140\u300180 \u548c 120 mg\u00b7m\u00b2\uff09\u4e0bPAN\u7eb3\u7c73\u7ea4\u7ef4\u652f\u6491\u5c42\u7684\u8868\u9762\u5f62\u8c8c\uff1b(c)\u4e3a\u901a\u8fc7\u53cc\u9009\u62e9\u6027\u5c42\u8def\u5f84\u6784\u5efa\u590d\u5408\u819c\u7684\u5236\u5907\u6d41\u7a0b\u56fe\uff1b(d)\u4e3a\u91c7\u7528\u4e0d\u540c\u591a\u5b54\u652f\u6491\u5c42\u6784\u5efa\u7684PVA\u57faTFC\u819c\u7ed3\u6784\u793a\u610f\u56fe\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265733\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72477-1.jpg\" alt=\"\" width=\"1000\" height=\"1006\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72477-1.jpg 1000w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72477-1-150x150.jpg 150w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72477-1-298x300.jpg 298w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72477-1-768x773.jpg 768w\" sizes=\"(max-width: 1000px) 100vw, 1000px\" \/><\/p>\n<p>\u56fe6\u5c55\u793a\u4e86\u57fa\u4e8e\u65b0\u578b\u529f\u80fd\u6750\u6599\u6784\u5efa\u7684IP\u819c\u7ed3\u6784\u4e0e\u8868\u5f81\u7ed3\u679c\uff1a(a)\u4e3aTpHZ\/AAO\u819c\u7684\u5b9e\u7269\u56fe\u50cf\uff0c\u5176\u4e2d(a1)\u4e3a\u6574\u4f53\u819c\uff0c(a2)\u4e0e(a3)\u5206\u522b\u4e3a\u4e0d\u540cTpHZ\u542b\u91cf\uff080.5\u548c1.5\uff09\u4e0b\u7684\u819c\u5916\u89c2\uff1b(b)\u4e3aCHF\u652f\u6491\u5c42(b1)\u53ca\u901a\u8fc7IP\u8fc7\u7a0b\u5f15\u5165\u6c2e\u63ba\u6742\u78b3\u91cf\u5b50\u70b9\uff08N-CDs\uff09\u540e\u7684\u9009\u62e9\u6027\u5c42(b2)\u7684\u622a\u9762SEM\u56fe\uff1b(c)\u4e3aAEL\u7eb3\u7c73\u7247\/\u805a\u9170\u80fa\u590d\u5408\u819c\u7684\u622a\u9762\u7ed3\u6784(c)\uff0c\u5176(c1\u2013c2)\u4e3aEDS\u5143\u7d20\u5206\u5e03\u56fe\uff0c(c3\u2013c4)\u4e3a\u5265\u79bb\u6001AEL\u7eb3\u7c73\u7247\u7684TEM\u56fe\u50cf\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265734\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72478.jpg\" alt=\"\" width=\"1000\" height=\"730\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72478.jpg 1000w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72478-300x219.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72478-768x561.jpg 768w\" sizes=\"(max-width: 1000px) 100vw, 1000px\" \/><\/p>\n<p>\u56fe7\u5c55\u793a\u4e86\u591a\u79cd\u4e2d\u95f4\u5c42\u6750\u6599\u5728\u4e0d\u540c\u652f\u6491\u5c42\u4e0a\u7684\u6784\u7b51\u4e0e\u819c\u6027\u80fd\u8868\u5f81\uff1a(a)\u4e3aTiO\u2082\u4e2d\u95f4\u5c42\u5728CHF\u652f\u6491\u5c42\u4e0a\u7684\u5206\u5e03\u60c5\u51b5\uff1b(b)\u4e3aMoS\u2082\u4e2d\u95f4\u5c42\u5728CHF\u652f\u6491\u5c42\u4e0a\u7684\u5f62\u8c8c\uff1b(c)\u4e3aCOF\u4e2d\u95f4\u5c42\u5728PES\u652f\u6491\u5c42\u4e0a\u7684\u7ed3\u6784\u793a\u610f\uff1b(d)\u5305\u542b\u4e0d\u540c\u819c\u7684(d1-d2) ATR-FTIR\u5149\u8c31\u4e0eZeta\u7535\u4f4d\u6d4b\u8bd5\u7ed3\u679c\uff0c\u4ee5\u53ca(d3-d4) \u805a\u9170\u80fa\u590d\u5408\u819c\u7684\u622a\u9762\u7ed3\u6784\u56fe\u50cf\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265735\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72479.jpg\" alt=\"\" width=\"1000\" height=\"1037\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72479.jpg 1000w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72479-289x300.jpg 289w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72479-768x796.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u72479-987x1024.jpg 987w\" sizes=\"(max-width: 1000px) 100vw, 1000px\" \/><\/p>\n<p>\u56fe8\u5c55\u793a\u4e86\u57fa\u4e8eMOF\u6750\u6599\u7684\u754c\u9762\u805a\u5408\u8fc7\u7a0b\u4e0e\u819c\u6784\u7b51\u7b56\u7565\uff1a(a1)\u4e3a\u4e2d\u7a7aZIF-8\u7eb3\u7c73\u7403\u7684\u7ed3\u6784\u56fe\uff0c(a2)\u4e3a\u5728\u4e0d\u540cIP\u5355\u4f53\u6d53\u5ea6\u4e0b\u7684\u5bf9\u5e94TEM\u56fe\u50cf\uff1b(b)\u4e3aMOF\u819c\u5408\u6210\u7684\u591a\u79cd\u7b56\u7565\uff0c\u5176\u4e2d(b1)\u4e3aMOF\u5c42\u5728\u57fa\u5e95\u4e0a\u7684\u6c89\u79ef\u8fc7\u7a0b\uff0c(b2)\u5c55\u793a\u4e86MOF\u5c42\u53c2\u4e0e\u7684\u754c\u9762\u805a\u5408\u8fc7\u7a0b\uff0c\u56fe\u4e2d\u6a59\u8272\u7403\u8868\u793a\u91d1\u5c5e\u79bb\u5b50\uff0c\u84dd\u8272\u516b\u9762\u4f53\u4ee3\u8868MOF\u6676\u4f53\uff0c\u6df1\u84dd\u8272\u516b\u9762\u4f53\u4e3a\u5df2\u5f62\u6210\u7ed3\u6784\uff1b(c)\u4e3a\u4e8c\u7ef4MOF\u7247\u5c42\u7684\u751f\u957f\u793a\u610f\u56fe\uff1b(d)\u5c55\u793a\u4e86\u4e2d\u7a7a\u7ea4\u7ef4\u4e2dMOF\u819c\u7684\u754c\u9762\u5fae\u6d41\u63a7\u6784\u5efa\u65b9\u6cd5\uff1b(e)\u4e3aZIF-8@MMM\u819c\u7684\u591a\u79cd\u5408\u6210\u7b56\u7565\u793a\u610f\u56fe\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265736\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724710.jpg\" alt=\"\" width=\"1000\" height=\"778\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724710.jpg 1000w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724710-300x233.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724710-768x598.jpg 768w\" sizes=\"(max-width: 1000px) 100vw, 1000px\" \/><\/p>\n<p>\u56fe9\u5c55\u793a\u4e86\u57fa\u4e8eCOF\u6750\u6599\u7684\u754c\u9762\u805a\u5408\u8fc7\u7a0b\u4e0e\u819c\u7ed3\u6784\u8868\u5f81\uff1a(a)\u4e3aTp-PaHzx\u819c\u7684\u5236\u5907\u8fc7\u7a0b\u793a\u610f\u56fe\uff0c(a1)\u663e\u793a\u5408\u6210\u8def\u5f84\uff0c(a2)\u4e3a\u4e0d\u540cHz\u6d53\u5ea6\u6761\u4ef6\u4e0b\u7684\u5bf9\u5e94SEM\u56fe\u50cf\uff1b(b)\u4e3a\u7ecf\u6c27\u7b49\u79bb\u5b50\u4f53\u523b\u8680\u5904\u7406\u540e\u7684TpPa\/PAN\u819c\u5236\u5907\u8fc7\u7a0b\uff1b(c)\u4e3a\u901a\u8fc7\u6c14-\u6db2\u754c\u9762\u805a\u5408\u6cd5\u6784\u5efa\u7684TpHZ\/PAN\u819c\uff1b(d)\u4e3a\u91c7\u7528\u6c34\u89e3PAN\uff08HPAN\uff09\u4e3a\u57fa\u5e95\u6784\u5efa\u7684TpPa\/HPAN\u819c\uff1b(e)\u4e3aTp-PaHzx\uff08x=0, 4\uff09\u819c\u7684\u6c2e\u6c14\u5438\u9644-\u8131\u9644\u7b49\u6e29\u7ebf\u53ca\u5bf9\u5e94\u7684\u5b54\u5f84\u5206\u5e03\uff08\u63d2\u56fe\uff09\uff1b(f)\u4e3a\u901a\u8fc7Br\u00f8nsted\u9178\u4ecb\u5bfc\u5408\u6210\u7684COFs-JLU2\u819c\u7ed3\u6784\u793a\u610f\u56fe\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265737\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724711.jpg\" alt=\"\" width=\"1000\" height=\"1021\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724711.jpg 1000w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724711-294x300.jpg 294w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724711-768x784.jpg 768w\" sizes=\"(max-width: 1000px) 100vw, 1000px\" \/><\/p>\n<p>\u56fe10\u5c55\u793a\u4e86\u57fa\u4e8e\u591a\u5b54\u6709\u673a\u7b3c\u4f53\uff08POCs\uff09\u6750\u6599\u7684\u819c\u6784\u5efa\u53ca\u5176\u5206\u79bb\u6027\u80fd\uff1a(a)\u4e3a\u8131\u76d0\u7cfb\u7edf\u7684\u6574\u4f53\u793a\u610f\u56fe\uff1b(b)\u4e3a\u4e0d\u540c\u819c\u6750\u6599\u6e17\u900f\u6027\u80fd\u7684\u5bf9\u6bd4\u7ed3\u679c\uff1b(c)\u4e3aPOC\u819c\u7684\u5f62\u8c8c\u4e0e\u7ed3\u6784\u56fe\u50cf\uff1b(d)\u4e3a\u57fa\u4e8ePOC\u6750\u6599\u7684\u754c\u9762\u805a\u5408\u8fc7\u7a0b\u793a\u610f\uff1b(e)\u4e3aCC3\u819c\u7684\u5206\u79bb\u673a\u5236\u56fe\uff0c\u5c55\u793a\u4e86\u5176\u5bf9\u6eb6\u8d28\u7684\u622a\u7559\u8fc7\u7a0b\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265738\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724712.jpg\" alt=\"\" width=\"1000\" height=\"818\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724712.jpg 1000w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724712-300x245.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724712-768x628.jpg 768w\" sizes=\"(max-width: 1000px) 100vw, 1000px\" \/><\/p>\n<p>\u56fe11\u5c55\u793a\u4e86\u8fd1\u4e94\u5e74\u57fa\u4e8e\u754c\u9762\u805a\u5408\uff08IP\uff09\u7684\u6e17\u900f\u6c7d\u5316\uff08PV\uff09\u819c\u7814\u7a76\u7684\u7edf\u8ba1\u4e0e\u6027\u80fd\u5206\u6790\uff1a(a)\u4e3aIP\u819c\u5728PV\u9886\u57df\u5e94\u7528\u7684\u7edf\u8ba1\u7ed3\u679c\uff0c\u6db5\u76d6\u4e0d\u540c\u7684\u6c34\u76f8\/\u6709\u673a\u76f8\u5355\u4f53\u7ec4\u5408\uff08\u5982\u95f4\u4e8c\u5f02\u6c30\u9178\u4e8c\u7532\u82ef m-xd \u548c\u53cd\u5f0f-5-\u964d\u51b0\u7247\u70ef-2,3-\u4e8c\u7fa7\u9170\u6c2f TC\uff09\uff1b(b)\u4e3a\u57fa\u4e8eIP\u7684PV\u819c\u5728\u6c34\/\u9187\u9009\u62e9\u6027\u4e0e\u901a\u91cf\u4e4b\u95f4\u7684\u6027\u80fd\u6743\u8861\u5173\u7cfb\u56fe\uff0c\u865a\u7ebf\u6240\u793a\u7684\u4e0a\u9650\u4e3b\u8981\u7531\u4f20\u7edf\u5355\u4f53\uff08\u5982BAPP\u3001DEPA\u3001TETA\/TMC\uff09\u6784\u6210\uff0c\u5b9e\u7ebf\u6240\u793a\u7684\u6027\u80fd\u4e0a\u9650\u5219\u57fa\u4e8e\u65b0\u578b\u5355\u4f53\uff08\u5982Pa\u548cHh\uff09\uff0c\u63d2\u56fe\u4e3a\u57fa\u4e8eIP\u819c\u5bf9\u4e59\u9178\u3001\u56db\u6c22\u544b\u5583\u548c\u8fc7\u6c27\u5316\u6c22\u7684\u8131\u6c34\u8868\u73b0\uff1b(c)\u4e3a\u91c7\u7528\u4e0d\u540c\u6784\u7b51\u7b56\u7565\u5236\u5907\u7684IP\u819c\u5728\u9009\u62e9\u6027\u4e0e\u6e17\u900f\u6027\u4e4b\u95f4\u7684\u6743\u8861\u5206\u6790\uff0c\u865a\u7ebf\u4ee3\u8868\u4f20\u7edf\u624b\u6bb5\uff08\u5982\u63a7\u5236IP\u8fc7\u7a0b\u3001\u5f15\u5165\u4e2d\u95f4\u5c42\u7b49\uff09\u6784\u5efa\u7684\u6027\u80fd\u4e0a\u9650\uff0c\u5b9e\u7ebf\u5219\u4ee3\u8868\u91c7\u7528\u65b0\u6280\u672f\uff08\u5982TFN\u819c\uff09\u6784\u5efa\u7684\u6027\u80fd\u8fb9\u754c\uff0c\u63d2\u56fe\u5c55\u793a\u4e86\u4e0d\u540c\u65b9\u6cd5\u4e0b\u7528\u4e8e\u8131\u76d0\u7684IP\u819c\u7ed3\u6784\u793a\u610f\u56fe\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265739\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724713.jpg\" alt=\"\" width=\"1000\" height=\"522\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724713.jpg 1000w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724713-300x157.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724713-768x401.jpg 768w\" sizes=\"(max-width: 1000px) 100vw, 1000px\" \/><\/p>\n<p>\u56fe12\u5c55\u793a\u4e86\u64cd\u4f5c\u6761\u4ef6\u4e0e\u819c\u7ed3\u6784\u5bf9\u6e17\u900f\u6c7d\u5316\u6027\u80fd\u7684\u5f71\u54cd\uff1a(a)\u4e3a\u4e0d\u540c\u58f3\u805a\u7cd6\uff08CS\uff09\u6d53\u5ea6\u4e0b\u590d\u5408\u819c\u572840\u201370\u202f\u00b0C\u64cd\u4f5c\u6e29\u5ea6\u8303\u56f4\u5185\u7684PV\u6027\u80fd\uff1b(b)\u4e3a\u8fdb\u6599\u4e2d\u5f02\u4e19\u9187\uff08IPA\uff09\u542b\u91cf\u5bf9343\u202fK\u4e0bPV\u6d4b\u8bd5\u6027\u80fd\u7684\u5f71\u54cd\uff1b(c-d)\u4e3a\u5265\u79bb\u6001MoS\u2082\u7eb3\u7c73\u7247\uff08\u539a\u5ea6\u7ea61.1\u202fnm\uff09\u6784\u5efa\u7684TFC\u819c\u539a\u5ea6\u8868\u5f81\uff1b(e)\u4e3a\u64cd\u4f5c\u6e29\u5ea6\u5bf9PV\u819c\u5206\u79bb\u6027\u80fd\u7684\u5f71\u54cd\uff1b(f)\u4e3a\u5206\u5b50\u52a8\u529b\u5b66\u6a21\u62df\u7ed3\u679c\uff0c\u5c55\u793aEDA\u5728\u4e09\u79cd\u4e0d\u540c\u819c\u4e2d\u7684\u6269\u6563\u7cfb\u6570\u5bf9\u6bd4\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-265740\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724714-1.jpg\" alt=\"\" width=\"1000\" height=\"683\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724714-1.jpg 1000w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724714-1-300x205.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/03\/\u56fe\u724714-1-768x525.jpg 768w\" sizes=\"(max-width: 1000px) 100vw, 1000px\" \/><\/p>\n<p>\u56fe13\u5c55\u793a\u4e86\u53cd\u6e17\u900f\u4e0e\u6e17\u900f\u6c7d\u5316\u8131\u76d0\u8fc7\u7a0b\u4e2d\u7684\u8d28\u91cf\u4f20\u8f93\u884c\u4e3a\u53ca\u819c\u6027\u80fd\uff1a(a)\u4e3a\u53cd\u6e17\u900f\uff08RO\uff09\u8fc7\u7a0b\u4e2d\u6c34\u5206\u5b50\u7a7f\u8fc7\u819c\u7684\u8d28\u91cf\u4f20\u8f93\u8def\u5f84\uff1b(b)\u4e3a\u6e17\u900f\u6c7d\u5316\uff08PV\uff09\u8131\u76d0\u8fc7\u7a0b\u7684\u4f20\u8d28\u673a\u5236\u793a\u610f\u56fe\uff1b(c)\u4e3a\u572810 wt% NaCl\u6761\u4ef6\u4e0b\uff0cACQD-TFN\uff0850 wt%\uff09\u819c\u4e0ePA-eGO\u590d\u5408\u819c\u7684PV\u957f\u671f\u8131\u76d0\u6027\u80fd\u5bf9\u6bd4\uff1b(d)\u4e3a\u57283.5 wt% NaCl\u300170\u202f\u00b0C\u64cd\u4f5c\u6761\u4ef6\u4e0b\u7684PV\u8131\u76d0\u6027\u80fd\u6d4b\u8bd5\u7ed3\u679c\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u521b\u65b0\u6210\u679c\uff1a \u8fd1\u5e74\u6765\uff0c\u754c\u9762\u805a\u5408\uff08Interfacial Polymerization, IP\uff09\u4f5c\u4e3a\u6784\u5efa\u8d85\u8584\u9009\u62e9\u6027\u5c42\u7684\u9ad8\u6548\u6280\u672f\uff0c\u5728\u819c\u5206\u79bb\u9886\u57df\u4e2d\u5c55\u73b0\u51fa\u5de8\u5927\u6f5c\u529b\u3002\u8fd1\u65e5\uff0c&#8230;<\/p>\n","protected":false},"author":14360,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-265714","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/265714"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/14360"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=265714"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/265714\/revisions"}],"predecessor-version":[{"id":265741,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/265714\/revisions\/265741"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=265714"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=265714"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=265714"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}