{"id":266991,"date":"2025-05-22T07:59:05","date_gmt":"2025-05-21T23:59:05","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=266991"},"modified":"2025-05-21T22:13:45","modified_gmt":"2025-05-21T14:13:45","slug":"%e5%a4%a9%e6%b4%a5%e4%b8%ad%e5%8c%bb%e8%8d%af%e5%a4%a7%e5%ad%a6%e6%9d%8e%e9%81%87%e4%bc%af%e6%95%99%e6%8e%88%e5%8d%97%e5%bc%80%e5%a4%a7%e5%ad%a6%e5%bc%a0%e6%8c%af%e6%9d%b0%e6%95%99%e6%8e%88%e3%80%81","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=266991","title":{"rendered":"\u5929\u6d25\u4e2d\u533b\u836f\u5927\u5b66\u674e\u9047\u4f2f\u6559\u6388&#038;\u5357\u5f00\u5927\u5b66\u5f20\u632f\u6770\u6559\u6388\u3001\u9648\u7476\u6559\u6388\u5408\u4f5c\u53d1\u8868Chem Soc Rev\uff08IF=40.4\uff09\u5c01\u9762\u6587\u7ae0\uff1a\u5171\u4ef7\u6709\u673a\u6846\u67b6\uff08COFs\uff09\u4f5c\u4e3a\u6709\u6bd2\u7269\u8d28\u53bb\u9664\u7684\u4f18\u826f\u5438\u9644\u5242"},"content":{"rendered":"<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-266992\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/05\/\u56fe\u72471-21.png\" alt=\"\" width=\"1268\" height=\"1792\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/05\/\u56fe\u72471-21.png 1268w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/05\/\u56fe\u72471-21-212x300.png 212w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/05\/\u56fe\u72471-21-768x1085.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/05\/\u56fe\u72471-21-725x1024.png 725w\" sizes=\"(max-width: 1268px) 100vw, 1268px\" \/>\u00a0<\/p>\n<p>\u3010\u521b\u65b0\u6210\u679c\u3011<\/p>\n<p>\u8fd1\u65e5\uff0c<strong><b>\u5929\u6d25\u4e2d\u533b\u836f\u5927\u5b66\u4e2d\u836f\u5b66\u9662\u674e\u9047\u4f2f\u6559\u6388\u4e0e\u5357\u5f00\u5927\u5b66\u5316\u5b66\u5b66\u9662\u5f20\u632f\u6770\u6559\u6388\u3001\u5357\u5f00\u5927\u5b66\u836f\u5b66\u9662\u9648\u7476\u6559\u6388\u5408\u4f5c<\/b><\/strong>\uff0c\u5728\u5316\u5b66\u9886\u57df\u56fd\u9645\u9876\u7ea7\u7efc\u8ff0\u671f\u520a<strong><b>Chemical Society Reviews\uff08<\/b><\/strong><strong><b>IF=40.4<\/b><\/strong><strong><b>\uff09<\/b><\/strong>\u4e0a\u53d1\u8868\u9898\u4e3a\u201c<strong><b>Covalent organic frameworks as superior adsorbents for the removal of toxic substances<\/b><\/strong>\u201d\u7684\u7efc\u8ff0\u8bba\u6587\u3002\u6587\u7ae0\u7cfb\u7edf\u603b\u7ed3\u4e86\u5171\u4ef7\u6709\u673a\u6846\u67b6\uff08COFs\uff09\u6750\u6599\u5728\u6709\u6bd2\u7269\u8d28\u5438\u9644\u9886\u57df\u7684\u6700\u65b0\u7814\u7a76\u8fdb\u5c55\uff0c\u6df1\u5165\u63a2\u8ba8\u4e86\u6750\u6599\u8bbe\u8ba1\u7b56\u7565\u3001\u5438\u9644\u673a\u5236\u53ca\u672a\u6765\u5e94\u7528\u524d\u666f\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-266993\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/05\/\u56fe\u72472-20.png\" alt=\"\" width=\"1005\" height=\"616\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/05\/\u56fe\u72472-20.png 1005w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/05\/\u56fe\u72472-20-300x184.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/05\/\u56fe\u72472-20-768x471.png 768w\" sizes=\"(max-width: 1005px) 100vw, 1005px\" \/><\/p>\n<p><strong><b>\u3010\u7814\u7a76\u80cc\u666f\u3011<\/b><\/strong><\/p>\n<p>\u968f\u7740\u4eba\u4eec\u5bf9\u4e8e\u5065\u5eb7\u7684\u91cd\u89c6\u7a0b\u5ea6\u65e5\u76ca\u52a0\u6df1\uff0c\u7814\u7a76\u6bd2\u6027\u7269\u8d28\u7684\u53bb\u9664\u6280\u672f\u5e76\u63a8\u52a8\u5176\u5e94\u7528\u5177\u6709\u91cd\u8981\u7684\u79d1\u5b66\u4ef7\u503c\u548c\u793e\u4f1a\u610f\u4e49\u3002\u4e00\u4e9b\u836f\u7528\u690d\u7269\uff08\u5982\u9a6c\u515c\u94c3\u79d1\u7684\u9a6c\u515c\u94c3\u3001\u7ec6\u8f9b\u7b49\uff09\u7531\u4e8e\u542b\u6709\u690d\u7269\u6bd2\u7d20\uff0c\u5e38\u5bfc\u81f4\u4e2d\u6bd2\u4e8b\u4ef6\u548c\u4e34\u5e8a\u6bd2\u526f\u4f5c\u7528\uff0c\u9650\u5236\u4e86\u5b83\u4eec\u7684\u4e34\u5e8a\u5e94\u7528\u3002\u56e0\u6b64\uff0c\u6709\u6548\u3001\u9009\u62e9\u6027\u5730\u53bb\u9664\u836f\u7528\u690d\u7269\u4e2d\u7684\u6709\u6bd2\u6210\u5206\u5bf9\u4e8e\u51cf\u8f7b\u6bd2\u6027\u3001\u4fdd\u7559\u836f\u6548\u4ee5\u786e\u4fdd\u5176\u4e34\u5e8a\u5b89\u5168\u5e94\u7528\u81f3\u5173\u91cd\u8981\u3002\u4f20\u7edf\u5438\u9644\u6750\u6599\uff08\u5982\u6d3b\u6027\u70ad\u3001\u5206\u5b50\u7b5b\uff09\u5b58\u5728\u5438\u9644\u53bb\u9664\u5bb9\u91cf\u4f4e\u3001\u9009\u62e9\u6027\u5dee\u3001\u4e8c\u6b21\u6c61\u67d3\u7b49\u95ee\u9898\uff0c\u5f00\u53d1\u9ad8\u6548\u3001\u5b89\u5168\u7684\u65b0\u578b\u5438\u9644\u5242\u6210\u4e3a\u6750\u6599\u79d1\u5b66\u9886\u57df\u7684\u7814\u7a76\u70ed\u70b9\u3002\u5171\u4ef7\u6709\u673a\u6846\u67b6\uff08COFs\uff09\u4f5c\u4e3a\u4e00\u7c7b\u65b0\u5174\u7ed3\u6676\u591a\u5b54\u6750\u6599\uff0c\u51ed\u501f\u5176\u9ad8\u5ea6\u6709\u5e8f\u7684\u7ed3\u6784\u3001\u9ad8\u6bd4\u8868\u9762\u79ef\u3001\u70ed\u5316\u5b66\u7a33\u5b9a\u6027\u3001\u6c38\u4e45\u5b54\u9699\u3001\u9ad8\u7ed3\u6676\u5ea6\u3001\u53ef\u8c03\u5b54\u5f84\u548c\u62d3\u6251\u591a\u6837\u6027\u7b49\u4f18\u826f\u7279\u6027\uff0c\u5728\u6bd2\u6027\u7269\u8d28\u53bb\u9664\u9886\u57df\u5c55\u73b0\u51fa\u5de8\u5927\u6f5c\u529b\u3002\u7136\u800c\uff0cCOFs\u7684\u89c4\u6a21\u5316\u5236\u5907\u3001\u590d\u6742\u4f53\u7cfb\u9009\u62e9\u6027\u5438\u9644\u53ca\u5e94\u7528\u7a33\u5b9a\u6027\u4ecd\u9762\u4e34\u91cd\u5927\u6311\u6218\u3002<\/p>\n<p><strong><b>\u3010\u6587\u7ae0\u6982\u8ff0\u3011<\/b><\/strong><\/p>\n<p>\u8be5\u7efc\u8ff0\u4ece<strong><b>\u6750\u6599\u8bbe\u8ba1\u7b56\u7565\u3001\u591a\u573a\u666f\u5e94\u7528\u3001\u5438\u9644\u673a\u5236\u53ca\u672a\u6765\u6311\u6218<\/b><\/strong>\u56db\u4e2a\u65b9\u9762\u7cfb\u7edf\u68b3\u7406\u4e86COFs\u5728\u6709\u6bd2\u7269\u8d28\u53bb\u9664\u4e2d\u7684\u7814\u7a76\u8fdb\u5c55\u3002\u9996\u5148\uff0c\u805a\u7126COFs\u7684\u5408\u6210\u4e0e\u529f\u80fd\u5316\u8bbe\u8ba1\uff0c\u8be6\u7ec6\u9610\u8ff0\u4e86\u901a\u8fc7\u62d3\u6251\u8c03\u63a7\u3001\u529f\u80fd\u57fa\u56e2\u5f15\u5165\u53ca\u590d\u5408\u7b56\u7565\u4f18\u5316\u6750\u6599\u6027\u80fd\u7684\u8def\u5f84\uff0c\u63a2\u8ba8\u5982\u4f55\u901a\u8fc7\u7ed3\u6784\u8bbe\u8ba1\u4e0e\u5316\u5b66\u4fee\u9970\u63d0\u5347\u5438\u9644\u9009\u62e9\u6027\u548c\u7a33\u5b9a\u6027\u3002\u5176\u6b21\uff0c\u91cd\u70b9\u5206\u6790\u4e86COFs\u5728\u751f\u7269\u6bd2\u7d20\uff0c\u5c24\u5176\u662f\u4e2d\u836f\/\u5929\u7136\u690d\u7269\u6709\u6bd2\u6210\u5206\uff08\u5982\u9a6c\u515c\u94c3\u9178\u7c7b\u6210\u5206\uff09\u548c\u4f53\u5185\u6bd2\u7d20\u53bb\u9664\u9886\u57df\u7684\u5e94\u7528\u6f5c\u529b\uff0c\u4ece\u5206\u5b50\u7b5b\u5206\u6548\u5e94\u5230\u5316\u5b66\u534f\u540c\u4f5c\u7528\uff0c\u8bba\u8bc1\u5176\u5728\u4e0d\u540c\u573a\u666f\u4e0b\u7684\u6280\u672f\u4f18\u52bf\u3002\u6b64\u5916\uff0c\u7cfb\u7edf\u89e3\u6790\u4e86COFs\u5438\u9644\u6709\u6bd2\u7269\u8d28\u7684\u5fae\u89c2\u673a\u5236\uff0c\u9610\u660e\u5b54\u5f84\u5339\u914d\u3001\u9759\u7535\u4f5c\u7528\u3001\u6c22\u952e\u53ca\u758f\u6c34\u6548\u5e94\u7b49\u591a\u56e0\u7d20\u8026\u5408\u7684\u5438\u9644\u673a\u7406\u3002\u6700\u540e\uff0c\u603b\u7ed3\u4e86\u5f53\u524d\u7814\u7a76\u5728\u6709\u6bd2\u7269\u8d28\u53bb\u9664\u9886\u57df\u9762\u4e34\u7684\u5173\u952e\u6311\u6218\uff0c\u5305\u62ec\u7eff\u8272\u89c4\u6a21\u5316\u5236\u5907\u5de5\u827a\u7684\u7f3a\u5931\u3001\u590d\u6742\u4f53\u7cfb\u52a8\u6001\u8c03\u63a7\u9700\u6c42\u53ca\u751f\u7269\u5b89\u5168\u6027\u9a8c\u8bc1\u4e0d\u8db3\uff0c\u5e76\u63d0\u51fa\u901a\u8fc7\u5de5\u827a\u521b\u65b0\u3001\u667a\u80fd\u6750\u6599\u5f00\u53d1\u53ca\u8de8\u5b66\u79d1\u5408\u4f5c\u63a8\u52a8\u6280\u672f\u843d\u5730\u7684\u672a\u6765\u65b9\u5411\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-266994\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/05\/\u56fe\u72473-19.png\" alt=\"\" width=\"734\" height=\"823\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/05\/\u56fe\u72473-19.png 734w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/05\/\u56fe\u72473-19-268x300.png 268w\" sizes=\"(max-width: 734px) 100vw, 734px\" \/><\/p>\n<p>COFs\u6750\u6599\u5728\u4e2d\u836f\u9a6c\u515c\u94c3\u9178\u7c7b\u6210\u5206\u9009\u62e9\u6027\u53bb\u9664\u4e2d\u7684\u5e94\u7528<\/p>\n<p><strong><b>\u3010\u57fa\u91d1\u8d44\u52a9\u3011<\/b><\/strong><\/p>\n<p>\u8be5\u7814\u7a76\u5de5\u4f5c\u5f97\u5230\u4e86\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\uff08\u9879\u76ee\u7f16\u53f7\uff1a82374300\u300182474182\u300182141209)\u7684\u652f\u6301\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><strong><b>\u3010\u8bba\u6587\u4fe1\u606f\u3011<\/b><\/strong><\/p>\n<p>Covalent organic frameworks as superior adsorbents for the removal of toxic substances<\/p>\n<p>Yubo Li,<sup>\u2020*<\/sup>\u00a0Jinxia Wei,<sup>\u2020<\/sup>\u00a0Jian Wang,<sup>\u2020<\/sup>\u00a0Yuanyuan Wang, Peishuang Yu, Yao Chen<sup>*<\/sup>,\u00a0Zhenjie Zhang<sup>*<\/sup><\/p>\n<p>Chem Soc Rev.,\u00a02025;\u00a054(6):\u00a02693-2725. DOI:\u00a010.1039\/d4cs00591k<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u00a0 \u3010\u521b\u65b0\u6210\u679c\u3011 \u8fd1\u65e5\uff0c\u5929\u6d25\u4e2d\u533b\u836f\u5927\u5b66\u4e2d\u836f\u5b66\u9662\u674e\u9047\u4f2f\u6559\u6388\u4e0e\u5357\u5f00\u5927\u5b66\u5316\u5b66\u5b66\u9662\u5f20\u632f\u6770\u6559\u6388\u3001\u5357\u5f00\u5927\u5b66\u836f\u5b66\u9662\u9648\u7476\u6559\u6388\u5408\u4f5c\uff0c\u5728\u5316\u5b66\u9886\u57df\u56fd\u9645\u9876\u7ea7\u7efc\u8ff0\u671f\u520aChemical S&#8230;<\/p>\n","protected":false},"author":14360,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-266991","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/266991"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/14360"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=266991"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/266991\/revisions"}],"predecessor-version":[{"id":266995,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/266991\/revisions\/266995"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=266991"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=266991"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=266991"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}