{"id":268004,"date":"2025-08-20T07:59:00","date_gmt":"2025-08-19T23:59:00","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=268004"},"modified":"2025-08-20T22:01:51","modified_gmt":"2025-08-20T14:01:51","slug":"%e6%b8%af%e5%9f%8e%e5%a4%a7-%e7%90%86%e5%a4%a7%e3%80%8aadvanced-materials%e3%80%8b%ef%bc%9a%e8%b6%85%e5%86%b7%e8%b4%b4%e7%89%87%e5%ae%9e%e7%8e%b0%e5%85%89%e4%bc%8f%e9%ab%98%e6%95%88%e9%99%8d%e6%b8%a9","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=268004","title":{"rendered":"\u6e2f\u57ce\u5927\/\u7406\u5927\u300aAdvanced Materials\u300b\uff1a\u8d85\u51b7\u8d34\u7247\u5b9e\u73b0\u5149\u4f0f\u9ad8\u6548\u964d\u6e29\u589e\u4ea7"},"content":{"rendered":"\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"281\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/08\/2382c315a6ba396-17.png\" alt=\"\" class=\"wp-image-268005\"\/><\/figure>\n\n\n\n<p>\u7b2c\u4e00\u4f5c\u8005\uff1a\u6bdb\u6b63\u4e49 \u9999\u6e2f\u57ce\u5e02\u5927\u5b66\u535a\u58eb\u540e\u7814\u7a76\u5458<\/p>\n\n\n\n<p>\u901a\u8baf\u4f5c\u8005\uff1a\u6768\u6d2a\u5174&nbsp;\u9999\u6e2f\u7406\u5de5\u5927\u5b66\u6559\u6388\uff1b&nbsp;\u738b\u5176\u6881&nbsp;\u82f1\u56fd\u8bfa\u4e01\u6c49\u5927\u5b66\u6b27\u76df\u201c\u739b\u4e3d\u00b7\u5c45\u91cc\u201d\u5b66\u8005\uff1b\u5415\u575a&nbsp;\u9999\u6e2f\u57ce\u5e02\u5927\u5b66\u8bb2\u5e2d\u6559\u6388<\/p>\n\n\n\n<p><strong>\u5f15\u8a00<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u5149\u4f0f\u53d1\u7535\u5728\u5168\u7403\u53ef\u518d\u751f\u80fd\u6e90\u5360\u6bd4\u5de8\u5927\u3002\u4f46\u5149\u4f0f\u677f\u8fc7\u70ed\u95ee\u9898\u4e0d\u4ec5\u4e25\u91cd\u635f\u5bb3\u5149\u4f0f\u53d1\u7535\u6548\u7387\u8fd8\u4f1a\u635f\u5bb3\u5149\u4f0f\u677f\u4f7f\u7528\u5bff\u547d\u3002\u6e2f\u57ce\u5927\u5415\u575a\u9662\u58eb\/\u6e2f\u7406\u5de5\u6768\u6d2a\u5174\u6559\u6388\/\u8bfa\u4e01\u6c49\u738b\u5176\u6881\u535a\u58eb\u5408\u4f5c\uff0c\u5728\u524d\u671fNat. Water, 2024, 2, 93-100\u5de5\u4f5c\u7684\u57fa\u7840\u4e0a\uff0c\u63d0\u51fa\u4e86\u4e00\u79cd\u88ab\u52a8\u51b7\u5374\u7b56\u7565\uff0c\u4f7f\u7528\u8d85\u51b7\u5374\u8d34\u7247\uff08UCP\uff09\uff0c\u80fd\u591f\u6709\u6548\u964d\u4f4e\u5149\u4f0f\u9762\u677f\u7684\u6e29\u5ea6\uff0c\u5b9e\u73b0\u8fd1700 W m\u207b\u00b2\u7684\u5353\u8d8a\u51b7\u5374\u80fd\u529b\uff0c\u5e76\u56de\u6536\u8d85\u8fc770%\u7684\u5e9f\u70ed\u7528\u4e8e\u6de1\u6c34\u751f\u4ea7\u3002UCP\u7684\u7075\u6d3b\u6027\u548c\u7c98\u9644\u7279\u6027\u4f7f\u5176\u80fd\u591f\u4e0e\u5404\u79cd\u5149\u4f0f\u914d\u7f6e\uff08\u5305\u62ec\u67d4\u6027\u9762\u677f\uff09\u8f7b\u677e\u96c6\u6210\u3002\u6b64\u5916\uff0cUCP\u8fd8\u53ef\u4ee5\u91cd\u6784\u4e3a\u5404\u79cd\u6563\u70ed\u7ed3\u6784\uff0c\u4ece\u800c\u8c03\u6574\u70ed\u4f20\u5bfc\u8def\u5f84\u3002\u8fd9\u79cd\u88ab\u52a8\u5f0f\u8bbe\u8ba1\u589e\u5f3a\u4e86\u5149\u4f0f\u9762\u677f\u7684\u6563\u70ed\u6027\u80fd\uff0c\u8fdb\u4e00\u6b65\u63d0\u5347\u4e86\u51b7\u5374\u6548\u679c\u3002\u56e0\u6b64\uff0c\u5149\u4f0f\u9762\u677f\u7684\u6e29\u5ea6\u964d\u4f4e\u4e8629\u2103\uff0c\u4ece\u800c\u4f7f\u6700\u5927\u529f\u7387\u5bc6\u5ea6\u663e\u8457\u63d0\u9ad8\u3002\u6b64\u5916\uff0c\u5bf9\u7ea61 m\u00b2\u5149\u4f0f\u9762\u677f\u7684\u6237\u5916\u5b9e\u9a8c\u9a8c\u8bc1\u4e86\u5176\u51b7\u5374\u6027\u80fd\u548c\u5b9e\u9645\u5e94\u7528\u6027\u3002\u8fd9\u9879\u7814\u7a76\u63d0\u4f9b\u4e86\u4e00\u79cd\u5177\u6709\u5546\u4e1a\u6f5c\u529b\u7684\u89e3\u51b3\u65b9\u6848\uff0c\u4ee5\u5e94\u5bf9\u80fd\u6e90\u4e0e\u6c34\u8d44\u6e90\u5371\u673a\uff0c\u56e0\u5176\u9ad8\u6548\u7387\u3001\u53ef\u6269\u5c55\u6027\u548c\u6210\u672c\u6548\u76ca\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"516\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/08\/ce6e2814f207c93-17.png\" alt=\"\" class=\"wp-image-268006\"\/><\/figure>\n\n\n\n<p><strong>\u56fe1.<\/strong><strong>&nbsp;<\/strong><strong>UCP\u7ed3\u6784\u793a\u610f\u56fe\u3002<\/strong><strong><\/strong><\/p>\n\n\n\n<p>UCP\u7531\u4e09\u5c42\u7ed3\u6784\u7ec4\u6210\uff1a\u5927\u6c14\u6c34\u6536\u96c6\u5668\uff08AWH\uff09\u3001\u70ed\u8c03\u8282\u5c42\u548c\u7c98\u5408\u5c42\uff08\u89c1\u56fe1a\uff09\u3002AWH\u91c7\u7528\u5177\u6709\u5bf9\u9f50\u901a\u9053\u548c\u76f8\u4e92\u8fde\u63a5\u5b54\u9699\u7684\u6c34\u51dd\u80f6\u5236\u6210\u3002\u7ecf\u8fc7\u5438\u6e7f\u6750\u6599\u7684\u52a0\u8f7d\uff0cAWH\u80fd\u591f\u901a\u8fc7\u8fd9\u4e9b\u4f4e\u66f2\u6298\u5ea6\u901a\u9053\u5feb\u901f\u5438\u6536\u7a7a\u6c14\u4e2d\u7684\u6c34\u5206\u3002\u70ed\u8c03\u8282\u5c42\u8d1f\u8d23\u8c03\u6574\u5feb\u901f\u70ed\u4f20\u5bfc\u8def\u5f84\u3002\u5e95\u90e8\u7684\u7c98\u5408\u5c42\u4f7fUCP\u80fd\u591f\u7d27\u5bc6\u53ef\u9006\u5730\u9644\u7740\u5728\u5404\u79cd\u57fa\u6750\u4e0a\u3002\u5176\u7075\u6d3b\u6027\u548c\u7c98\u5408\u7279\u6027\u663e\u8457\u7b80\u5316\u4e86UCP\u7684\u5b89\u88c5\uff0c\u4f7f\u5176\u80fd\u591f\u5e94\u7528\u4e8e\u67d4\u6027\u5149\u4f0f\u6750\u6599\uff08\u89c1\u56fe1b\uff09\u3002\u6b64\u5916\uff0cUCP\u8fd8\u53ef\u4ee5\u91cd\u65b0\u5851\u9020\u6210\u9ccd\u7247\u72b6\u51e0\u4f55\u5f62\u72b6\uff0c\u4ee5\u6269\u5927\u754c\u9762\u9762\u79ef\uff0c\u5e76\u8fdb\u4e00\u6b65\u8c03\u8282\u70ed\u4f20\u5bfc\u8def\u5f84\uff0c\u4ece\u800c\u589e\u5f3a\u88ab\u52a8\u6563\u70ed\uff08\u89c1\u56fe1c\uff09\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"478\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/08\/7f88dbbcaa77a1d-16.png\" alt=\"\" class=\"wp-image-268007\"\/><\/figure>\n\n\n\n<p><strong>\u56fe2.<\/strong><strong>&nbsp;<\/strong><strong>\u5236\u5907\u548c\u8868\u5f81\u3002<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u7ad6\u76f4\u4e92\u8054\u5b54\u7ed3\u6784\u5b9e\u73b0\u4e86\u9ad8\u6548\u4f20\u8d28\uff0c\u5229\u4e8e\u5feb\u901f\u7a7a\u6c14\u53d6\u6c34\u4e0e\u84b8\u53d1\u6563\u70ed\u3002\u9ecf\u9644\u5c42\u8868\u73b0\u51fa\u4f18\u5f02\u548c\u53ef\u91cd\u590d\u7684\u7c98\u9644\u6027\u80fd\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"333\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/08\/4e9a0ba2491dfde-18.png\" alt=\"\" class=\"wp-image-268008\"\/><\/figure>\n\n\n\n<p><strong>\u56fe3.<\/strong><strong>\u00a0<\/strong><strong>UCP\u7684\u88ab\u52a8\u51b7\u5374\u6027\u80fd\u3002<\/strong><\/p>\n\n\n\n<p>\u901a\u8fc7\u5bf9\u7167\u7ec4\u8bbe\u8ba1\uff0c\u8bc1\u660e\u51b7\u5374\u8d34\u7247\u5bf9\u5149\u4f0f\u677f\u826f\u597d\u7684\u964d\u6e29\u6548\u679c\uff0c\u5b9e\u73b0\u4e86\u957f\u4e45\u6709\u6548\u7684\u88ab\u52a8\u5149\u4f0f\u70ed\u7ba1\u7406\uff0c\u663e\u8457\u63d0\u9ad8\u4e86\u5149\u4f0f\u677f\u7684\u4ea7\u7535\u6027\u80fd\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"349\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/08\/b14210e1ee30421-16.png\" alt=\"\" class=\"wp-image-268009\"\/><\/figure>\n\n\n\n<p><strong>\u56fe4.<\/strong><strong>&nbsp;<\/strong><strong>\u91cd\u6784UCP\u589e\u5f3a\u6362\u70ed\u5b9e\u73b0\u9ad8\u6548\u5149\u4f0f\u964d\u6e29\u589e\u4ea7<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u5229\u7528\u51b7\u5374\u8d34\u7247\u7684\u67d4\u6027\u4e0e\u7c98\u9644\u6027\uff0c\u91cd\u6784\u51b7\u5374\u8d34\u7247\u7ed3\u6784\uff0c\u5b9e\u73b0\u4e86\u88ab\u52a8\u589e\u5f3a\u7684\u70ed\u4ea4\u6362\u3002\u91cd\u6784\u7ed3\u6784\u589e\u52a0\u4e86\u6563\u70ed\u4e0e\u4f20\u70ed\u9762\u79ef\uff0c\u70ed\u8c03\u8282\u5c42\u5feb\u901f\u4f20\u70ed\uff0c\u88ab\u52a8\u63d0\u9ad8\u4e86\u51b7\u5374\u8d34\u7247\u7684\u6563\u70ed\u6027\u80fd\uff0c\u8fdb\u4e00\u6b65\u589e\u5f3a\u4e86\u5149\u4f0f\u7684\u4ea7\u7535\u8868\u73b0\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"662\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/08\/de5bcf7d8eaea98-10.png\" alt=\"\" class=\"wp-image-268010\"\/><\/figure>\n\n\n\n<p><strong>\u56fe5.<\/strong><strong>&nbsp;<\/strong><strong>\u5149\u4f0f\u51b7\u5374\u8d34\u7247\u7684\u6237\u5916\u6d4b\u8bc4<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u5bf9\u51b7\u5374\u8d34\u7247\u8fdb\u884c\u653e\u5927\u4e0e\u6237\u5916\u5b9e\u9a8c\u6d4b\u8bd5\u3002\u7ed3\u679c\u8868\u660e\uff0c\u8be5\u51b7\u5374\u8d34\u7247\u5728\u5b9e\u9645\u5e94\u7528\u4e2d\u5bf9\u5149\u4f0f\u677f\u5177\u6709\u826f\u597d\u7684\u964d\u6e29\u589e\u4ea7\u6548\u679c\uff0c\u540c\u65f6\u53ef\u4ee5\u6709\u6548\u6536\u96c6\u6de1\u6c34\u3002\u57fa\u4e8e\u4e0a\u8ff0\u4f18\u52bf\uff0c\u8be5\u6280\u672f\u6b63\u5728\u8fdb\u884c\u5927\u9762\u79ef\uff0c\u5728\u9ad8\u6548\u5149\u4f0f\u70ed\u7ba1\u7406\u9886\u57df\u5c55\u73b0\u51fa\u826f\u597d\u7684\u5e94\u7528\u524d\u666f\u3002\u5c3d\u7ba1\u8be5\u7814\u7a76\u5e26\u6765\u4e00\u5b9a\u8fdb\u5c55\uff0c\u4f46\u5b9e\u9645\u5e94\u7528\u4e2d\u8fd8\u9700\u8003\u8651\u66f4\u591a\u7684\u56e0\u7d20\uff0c\u4f8b\u5982\u4ea7\u7535-\u4ea7\u6c34\u6027\u80fd\u7684\u6743\u8861\u3001\u6750\u6599\u6210\u672c\u548c\u5e94\u7528\u573a\u666f\uff08\u6e29\u5ea6\u3001\u6e7f\u5ea6\uff09\u7b49\u7684\u5f71\u54cd\u3002<\/p>\n\n\n\n<p>\u9999\u6e2f\u7814\u7a76\u8d44\u52a9\u5c40\uff08RGC\uff09\u7b56\u7565\u4e13\u9898\u7814\u7a76\uff08STG\uff09\uff08STG2\/P-705\/24-R\uff09\u4e3a\u7b2c\u4e00\u652f\u6301\u9879\u76ee\uff0c\u8be5\u6210\u679c\u8fd8\u53d7\u5230\u9999\u6e2f\u521b\u65b0\u79d1\u6280\u7f72\uff08ITS\/199\/23\uff09\u3001\u4e2d\u79d1\u9662\u9999\u6e2f\u8054\u5408\u5b9e\u9a8c\u5ba4\uff08JLFS\/E-102\/24\uff09\u548c\u5e7f\u4e1c\u7701\u79d1\u6280\u5408\u4f5c\u9879\u76ee\uff082023B1212120008\uff09\u7b49\u7684\u57fa\u91d1\u652f\u6301\u3002<\/p>\n\n\n\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong>https:\/\/doi.org\/10.1002\/adma.202505002<\/p>\n\n\n\n<p><strong>\u901a\u8baf\u4f5c\u8005\u7b80\u4ecb\uff1a<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u5415\u575a\u9662\u58eb\uff1a\u6cd5\u56fd\u56fd\u5bb6\u6280\u672f\u79d1\u5b66\u9662\uff08NATF\uff09\u9662\u58eb\u3001\u9999\u6e2f\u5de5\u7a0b\u9662\u9662\u58eb\u3001\u9999\u6e2f\u6750\u6599\u7814\u7a76\u4f1a\u7406\u4e8b\u957f\uff08HKMRS\uff09\u3001\u9999\u6e2f\u57ce\u5e02\u5927\u5b66\u673a\u68b0\u5de5\u7a0b\u7cfb\u8bb2\u5ea7\u6559\u6388\u3001\u5de5\u5b66\u9662\u9662\u957f\u3001\u56fd\u5bb6\u8d35\u91d1\u5c5e\u6750\u6599\u5de5\u7a0b\u7814\u7a76\u4e2d\u5fc3\u9999\u6e2f\u5206\u4e2d\u5fc3\u4e3b\u4efb\u3001\u5148\u8fdb\u7ed3\u6784\u6750\u6599\u4e2d\u5fc3\u4e3b\u4efb\u3002\u7814\u7a76\u65b9\u5411\u6d89\u53ca\u5148\u8fdb\u7ed3\u6784\u4e0e\u529f\u80fd\u7eb3\u7c73\u6750\u6599\u7684\u5236\u5907\u548c\u529b\u5b66\u6027\u80fd\uff0c\u7ed3\u6784\u4e0e\u529f\u80fd\u6750\u6599\u7684\u8bbe\u8ba1\u53ca\u589e\u6750\u5236\u9020\uff0c\u56fe\u7075\u53ca\u9ad8\u71b5\u5408\u91d1\u50ac\u5316\u5242\u5728\u7535\u89e3\u6c34\u5236\u7eff\u6c22\u53ca\u71c3\u6599\u7535\u6c60\u4e0e\u6c61\u6c34\u5904\u7406\uff0c\u8d85\u9ad8\u7075\u654f\u5ea6\u8868\u9762\u589e\u5f3a\u62c9\u66fc\u5149\u8c31\uff08SERS\uff09\u53ca\u5728\u5fc3\u8111\u8840\u7ba1\u75be\u75c5\u65e9\u671f\u5feb\u901f\u8bca\u65ad\uff0c\u73af\u4fdd\uff0c\u98df\u54c1\u5b89\u5168\u7b49\u9886\u57df\u7684\u5e94\u7528\u3002\u4e2d\u79d1\u9662\u9996\u6279\u6d77\u5916\u8bc4\u5ba1\u4e13\u5bb6\uff0c\u4e2d\u79d1\u9662\u6c88\u9633\u91d1\u5c5e\u6240\u5ba2\u5ea7\u9996\u5e2d\u7814\u7a76\u5458\uff0c\u897f\u5b89\u4ea4\u901a\u5927\u5b66\u3001\u4e1c\u5317\u5927\u5b66\u3001\u5317\u4eac\u79d1\u6280\u5927\u5b66\u3001\u5357\u660c\u5927\u5b66\u540d\u8a89\u6559\u6388\uff0c\u897f\u5317\u5de5\u4e1a\u5927\u5b66\u3001\u4e0a\u6d77\u4ea4\u901a\u5927\u5b66\u548c\u897f\u5357\u4ea4\u901a\u5927\u5b66\u987e\u95ee\u6559\u6388\uff0c\u4e2d\u79d1\u9662\u77e5\u540d\u5b66\u8005\u56e2\u961f\u6210\u5458\uff0c2011\u5e74\u88ab\u6cd5\u56fd\u56fd\u5bb6\u6280\u672f\u79d1\u5b66\u9662\uff08NATF\uff09\u9009\u4e3a\u9662\u58eb\uff0c\u662f\u8be5\u9662\u8fd1300\u4f4d\u9662\u58eb\u4e2d\u9996\u4f4d\u534e\u88d4\u9662\u58eb\u30022006\u5e74\u4e0e2017\u5e74\u5206\u522b\u83b7\u6cd5\u56fd\u603b\u7edf\u4efb\u547d\u83b7\u6cd5\u56fd\u56fd\u5bb6\u8363\u8a89\u9a91\u58eb\u52cb\u7ae0\u53ca\u6cd5\u56fd\u56fd\u5bb6\u8363\u8a89\u519b\u56e2\u9a91\u58eb\u52cb\u7ae0\uff0c2018\u5e74\u83b7\u4e2d\u56fd\u5de5\u7a0b\u9662\u5149\u534e\u5de5\u7a0b\u79d1\u6280\u5956\u3002\u5df2\u53d6\u5f9784\u9879\u6b27\u3001\u7f8e\uff0850\u9879\uff09\u3001\u4e2d\u53d1\u660e\u4e13\u5229\u6388\u6743\uff0c\u5728\u672c\u9886\u57df\u9876\u5c16\u6742\u5fd7Nature\uff08\u5c01\u9762\u6587\u7ae0\uff09\u3001Science\u3001Nature Materials\u3001Nature Chemistry, Nature Water\uff0c Science Advances\u3001Nature Communications\u3001Materials Today\u3001Advanced Materials\u3001Advanced Functional Materials, JACS, Angew. Chem. JMPS\uff0c Acta Materialia \u7b49\u4e13\u4e1a\u6742\u5fd7\u4e0a\u53d1\u8868\u8bba\u6587580\u4f59\u7bc7\uff0c\u5f15\u7528\u4e94\u4e07\u4f59\u6b21\u3002\u4e2a\u4eba\u4e3b\u9875\uff1ahttps:\/\/www.cityu.edu.hk\/mne\/people\/academic-staff\/prof-lu-jian<\/p>\n\n\n\n<p>\u738b\u5176\u6881\u535a\u58eb\uff0c2019\u5e74\u535a\u58eb\u6bd5\u4e1a\u4e8e\u4e2d\u56fd\u79d1\u5b66\u6280\u672f\u5927\u5b66\uff0c\u66fe\u4efb\u9999\u6e2f\u7406\u5de5\u5927\u5b66\u7814\u7a76\u52a9\u7406\u6559\u6388\uff0c\u73b0\u4e3a\u82f1\u56fd\u8bfa\u4e01\u6c49\u5927\u5b66\u6b27\u76df\u201c\u739b\u4e3d\u00b7\u5c45\u91cc\u201d\u5b66\u8005, \u5165\u9009\u56fd\u5bb6\u9ad8\u5c42\u6b21\u9752\u5e74\u4eba\u624d\u548c\u4e2d\u79d1\u9662\u9752\u5e74\u4eba\u624d\u8ba1\u5212\u3002\u4e3b\u8981\u4ece\u4e8b\u592a\u9633\u80fd\u9ad8\u6548\u8f6c\u6362\u5229\u7528\u3001\u592a\u9633\u80fd\u6d77\u6c34\u6de1\u5316\u3001\u592a\u9633\u80fd\u5efa\u7b51\u7b49\u9886\u57df\u7684\u7814\u7a76\u5de5\u4f5c\uff0c\u5728\u56fd\u9645\u77e5\u540d\u80fd\u6e90\u671f\u520a\u53d1\u8868\u5b66\u672f\u8bba\u658780\u4f59\u7bc7\uff0c\u5176\u4e2d\u5df2\u7b2c\u4e00\/\u901a\u8baf\u4f5c\u8005\u5728Nat. Water\u3001Nat. Cities\u3001Adv. Mat.\u3001ACS Nano\u3001Innovation Energ.\u3001Adv. Sci.\u3001Appl. Energy\u7b49\u80fd\u6e90\u6743\u5a01\u671f\u520a\u53d1\u8868\u8bba\u658740\u4f59\u7bc7\uff0c\u6388\u6743\u4e2d\u56fd\u548c\u7f8e\u56fd\u4e13\u5229\u517118\u9879\u3002\u83b7\u56fd\u9645\u53ef\u6301\u7eed\u80fd\u6e90\u6280\u672f\u534f\u4f1a\u521b\u65b0\u5956(WSSET Innovation Award)\u3001\u65e5\u5185\u74e6\u56fd\u9645\u53d1\u660e\u5c55\u7279\u522b\u91d1\u5956\u3001\u4e2d\u79d1\u9662\u9662\u957f\u7279\u522b\u5956\u3001Sustainable Building Energy Engineering\u5148\u950b\u9752\u5e74\u79d1\u5b66\u5bb6\u5956\u3001\u5168\u56fd\u5927\u5b66\u751f\u5e74\u5ea6\u4eba\u7269\u63d0\u540d\u5956\u7b49\u8363\u8a89\uff1b\u76ee\u524d\u62c5\u4efbAppl. Energy\u3001Innovation\u3001Nexus\u3001Carbon Neutrality\u3001Int. J. Photoenergy\u7b49\u56fd\u9645\u671f\u520a\u7f16\u59d4\u6216\u9752\u5e74\u7f16\u59d4\u804c\u52a1\u3002<\/p>\n\n\n\n<p>\u6768\u6d2a\u5174\u6559\u6388\uff0c\u9999\u6e2f\u7406\u5de5\u5927\u5b66\u5efa\u7b51\u73af\u5883\u4e0e\u80fd\u6e90\u5de5\u7a0b\u5b66\u7cfb\u6559\u6388\uff0c\u535a\u58eb\u751f\u5bfc\u5e08\uff0c\u56fd\u9645\u671f\u520a\u300aApplied Energy\u300b\u7684\u9ad8\u7ea7\u7f16\u8f91\u548c\u9999\u6e2f\u5de5\u7a0b\u5e08\u5b66\u4f1a\u7684\u8d44\u6df1\u4f1a\u5458\u3002\u4e3b\u8981\u4ece\u4e8b\u53ef\u518d\u751f\u80fd\u6e90\u5229\u7528\u548c\u5efa\u7b51\u8282\u80fd\u7684\u6559\u5b66\u548c\u524d\u6cbf\u8bfe\u9898\u7814\u53d1\uff0c\u5305\u62ec\u57ce\u5e02\u4f9b\u6c34\u7f51\u7edc\u5fae\u6c34\u7535\u6280\u672f\uff0c\u5efa\u7b51\u7ba1\u9053\u53d1\u7535\u6280\u672f\uff0c\u592a\u9633\u80fd\u5149\u4f0f\u4e00\u4f53\u5316\u6280\u672f\uff0c\u592a\u9633\u80fd\u7a7a\u8c03\u6280\u672f\uff0c\u98ce\u80fd\u5f00\u53d1\u6280\u672f\uff0c\u98ce\u5149\u4e92\u8865\u84c4\u80fd\u6280\u672f\uff0c\u5730\u6e90\u70ed\u6cf5\u7a7a\u8c03\u6280\u672f\u548c\u95f4\u63a5\u84b8\u53d1\u51b7\u5374\u6280\u672f\u7b49\u3002\u4f5c\u4e3a\u8bfe\u9898\u4e3b\u8981\u8d1f\u8d23\u4eba\u5b8c\u6210\u4e8660\u591a\u4e2a\u7814\u53d1\u9879\u76ee\uff0c\u83b7\u5f97\u8d85\u8fc74000\u4e07\u6e2f\u5e01\u8d44\u52a9\uff0c\u5305\u62ec\u56fd\u5bb6\u548c\u9999\u6e2f\u7279\u533a\u653f\u5e9c\u53ca\u5de5\u4e1a\u754c\u7684\u7814\u7a76\u7ecf\u8d39\u8d44\u52a9\uff0c\u5982\u9999\u6e2f\u7814\u7a76\u8d44\u52a9\u5c40\u3001\u9999\u6e2f\u521b\u65b0\u79d1\u6280\u7f72\u3001\u9999\u6e2f\u5efa\u9020\u4e1a\u8bae\u4f1a\u3001\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u3001\u56fd\u5bb6\u79d1\u59d4\u3001\u9999\u6e2f\u5b66\u8005\u534f\u4f1a\u7b49\u3002\u4e0e\u5de5\u4e1a\u754c\u53ca\u653f\u5e9c\u90e8\u95e8\u6709\u7d27\u5bc6\u7684\u7814\u53d1\u5408\u4f5c\uff0c\u5305\u62ec\u65b0\u9e3f\u57fa\u3001\u4fe1\u548c\u3001\u4e2d\u7535\u3001\u6e2f\u706f\u3001\u5927\u65cf\u6fc0\u5149\u3001\u4e2d\u5efa\u3001\u65e5\u65b0\u79d1\u6280\u3001\u673a\u7535\u5de5\u7a0b\u7f72\u3001\u6c34\u52a1\u7f72\u3001\u6e20\u52a1\u7f72\u548c\u623f\u5c4b\u7f72\u7b49\u3002\u53d1\u8868\u8457\u4f5c7\u90e8\uff0c\u8bba\u6587500\u591a\u7bc7\uff0c\u5305\u62ec300\u591a\u7bc7SCI\u671f\u520a\u8bba\u6587\uff0c\u662f2016\u20142020\u5e74\u79d1\u777f\u552f\u5b89\u9ad8\u88ab\u5f15\u5b66\u8005\uff0c\u4e5f\u662f\u4eca\u5e74\u65af\u5766\u798f\u5927\u5b66\u900f\u8fc7Scopus\u516c\u5e03\u7684\u201c\u80fd\u6e90\u201d\u9886\u57df\u201c\u5168\u7403\u524d&nbsp;2%&nbsp;\u9802\u5c16\u79d1\u5b78\u5bb6\u201d\u5b66\u8005\u4e4b\u4e00\u3002\u8363\u83b7\u56fd\u5bb6\u6559\u80b2\u90e8\u79d1\u5b66\u6280\u672f\u4e8c\u7b49\u5956\u548c\u591a\u4e2a\u65e5\u5185\u74e6\u53d1\u660e\u91d1\u5956\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u7b2c\u4e00\u4f5c\u8005\uff1a\u6bdb\u6b63\u4e49 \u9999\u6e2f\u57ce\u5e02\u5927\u5b66\u535a\u58eb\u540e\u7814\u7a76\u5458 \u901a\u8baf\u4f5c\u8005\uff1a\u6768\u6d2a\u5174&nbsp;\u9999\u6e2f\u7406\u5de5\u5927\u5b66\u6559\u6388\uff1b&nbsp;\u738b\u5176\u6881&nbsp;\u82f1\u56fd\u8bfa\u4e01\u6c49\u5927\u5b66\u6b27\u76df\u201c\u739b\u4e3d\u00b7\u5c45\u91cc\u201d\u5b66\u8005\uff1b\u5415&#8230;<\/p>\n","protected":false},"author":31345,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-268004","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/268004"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/31345"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=268004"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/268004\/revisions"}],"predecessor-version":[{"id":268011,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/268004\/revisions\/268011"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=268004"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=268004"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=268004"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}