{"id":268133,"date":"2025-08-28T10:04:53","date_gmt":"2025-08-28T02:04:53","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=268133"},"modified":"2025-08-28T10:04:54","modified_gmt":"2025-08-28T02:04:54","slug":"%e6%8a%95%e7%a8%bf870%e5%a4%a9%e7%bb%88%e6%8e%a5%e6%94%b6%ef%bc%81%e5%8d%8e%e4%b8%9c%e7%90%86%e5%b7%a5%e5%a4%a7%e5%ad%a6%ef%bc%8c2025%e5%b9%b4%e9%a6%96%e7%af%87nature%ef%bc%81","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=268133","title":{"rendered":"\u6295\u7a3f870\u5929\u7ec8\u63a5\u6536\uff01\u534e\u4e1c\u7406\u5de5\u5927\u5b66\uff0c2025\u5e74\u9996\u7bc7Nature\uff01"},"content":{"rendered":"\n<p><strong>\u4e00\u3001<\/strong><strong>\u3010\u5bfc\u8bfb\u3011<a><\/a><\/strong><a><\/a><a><\/a><\/p>\n\n\n\n<p>\u5927\u591a\u6570\u5408\u91d1\u53ca\u5176\u5fae\u89c2\u7ed3\u6784\u5728\u8fc7\u53bb\u51e0\u5341\u5e74\u4e2d\u5df2\u7ecf\u5f00\u53d1\u51fa\u6765\uff0c\u4ee5\u5728\u5ba4\u6e29\u548c\u9ad8\u6e29\u4e0b\u63d0\u4f9b\u6240\u9700\u7684\u529b\u5b66\u6027\u80fd\u3002\u7136\u800c\uff0c\u5c3d\u7ba1\u5728\u8fd9\u4e00\u9886\u57df\u6210\u672c\u9650\u5236\u4e0d\u592a\u4e25\u683c\uff0c\u4f46\u7528\u4e8e\u9ad8\u5f3a\u5ea6\u548c\u8010\u635f\u4f24\u4f4e\u6e29\u5e94\u7528\u7684\u6750\u6599\u9009\u62e9\u5374\u8f83\u5c11\u3002\u4f8b\u5982\uff0c\u6c89\u6dc0\u786c\u5316\u4e00\u76f4\u662f\u63d0\u9ad8\u5408\u91d1\u5f3a\u5ea6\u7684\u6700\u6210\u529f\u7b56\u7565\u4e4b\u4e00\uff0c\u901a\u8fc7\u963b\u788d\u4f4d\u9519\u8fd0\u52a8\uff0c\u4ece\u800c\u9700\u8981\u66f4\u9ad8\u7684\u8f7d\u8377\u6765\u7ef4\u6301\u5851\u6027\u53d8\u5f62\u3002\u7136\u800c\uff0c\u5728\u4f4e\u6e29\u6761\u4ef6\u4e0b\uff0c\u7531\u4e8e\u5728\u6c89\u6dc0\u76f8-\u57fa\u4f53\u754c\u9762\u5904\u5f62\u6210\u4f4d\u9519\u585e\u548c\u9ad8\u5e94\u529b\u96c6\u4e2d\uff0c\u8fd9\u79cd\u65b9\u6cd5\u4ee5\u727a\u7272\u5ef6\u5c55\u6027\u4e3a\u4ee3\u4ef7\uff0c\u8fd9\u4e24\u4e2a\u7279\u5f81\u90fd\u4fc3\u8fdb\u4e86\u8fd9\u4e9b\u90e8\u4f4d\u7684\u635f\u4f24\u8d77\u59cb\u3002\u5728\u67d0\u4e9b\u9762\u5fc3\u7acb\u65b9\uff08fcc\uff09\u6750\u6599\u4e2d\u5f62\u6210\u5171\u683c\u6c89\u6dc0\u7269\u53ef\u4ee5\u5728\u4e00\u5b9a\u7a0b\u5ea6\u4e0a\u51cf\u5c11\u635f\u4f24\u8d77\u59cb\u503e\u5411\uff0c\u56e0\u4e3a\u4e0e\u975e\u5171\u683c\u548c\u534a\u5171\u683c\u754c\u9762\u76f8\u6bd4\uff0c\u5176\u754c\u9762\u80fd\u8f83\u4f4e\u3002\u7136\u800c\uff0c\u7531\u4e8e\u53cd\u76f8\u8fb9\u754c\u80fd\u9ad8\u4ee5\u53ca\u56f4\u7ed5\u5b83\u4eec\u5f62\u6210\u7684\u4f4d\u9519\u73af\u963b\u788d\u4e86\u968f\u540e\u7684\u4f4d\u9519\u8fd0\u52a8\uff0c\u5f53\u8fd9\u4e9b\u6c89\u6dc0\u7269\u5728\u957f\u65f6\u95f4\u65f6\u6548\u540e\u5c3a\u5bf8\u8db3\u591f\u5927\u65f6\uff0c\u4ecd\u7136\u53ef\u4ee5\u53d1\u5c55\u51fa\u5f3a\u70c8\u7684\u5f02\u8d28\u5e94\u529b\u573a\u3002\u4e0e\u8fd9\u4e9b\u5df2\u5efa\u7acb\u7684\u786c\u5316\u673a\u5236\u53ca\u5176\u5728\u4f20\u7edf\u7a00\u8584\u5408\u91d1\u4e2d\u5df2\u77e5\u7684\u56fa\u6709\u7f3a\u70b9\u76f8\u6bd4\uff0c\u4e9a\u7eb3\u7c73\u5c3a\u5ea6\u5316\u5b66\u77ed\u7a0b\u6709\u5e8f\uff08SRO\uff09\u7279\u5f81\u5bf9\u529b\u5b66\u6027\u80fd\u7684\u5f71\u54cd\u5c1a\u672a\u88ab\u5145\u5206\u7406\u89e3\u3002\u8fd9\u4e9b\u539f\u5b50\u6392\u5e8f\u56e2\u7c07\u4f3c\u4e4e\u5728\u4e00\u4e9b\u4e2d\u71b5\u5408\u91d1\u548c\u9ad8\u71b5\u5408\u91d1\uff08MEAs\u548cHEAs\uff09\u4e2d\u5f62\u6210\uff0c\u8fd9\u662f\u7531\u4e8e\u7ec4\u6210\u5143\u7d20\u4e4b\u95f4\u7684\u5c40\u90e8\u7113\u76f8\u4e92\u4f5c\u7528\u4e0e\u8fd9\u4e9b\u5408\u91d1\u57fa\u4e8e\u7684\u71b5\u4e3b\u5bfc\u7684\u56fa\u6eb6\u4f53\u4e4b\u95f4\u7684\u5fae\u5999\u76f8\u4e92\u4f5c\u7528\u3002\u9ad8\u5ea6\u5206\u6563\u4e14\u5747\u5300\u5206\u5e03\u7684SRO\u533a\u57df\uff0c\u4ee5\u53ca\u5b83\u4eec\u5bf9\u4f4d\u9519\u6ed1\u79fb\u7684\u6291\u5236\u4f5c\u7528\u4ee5\u53ca\u76f8\u5173\u7684\u4f4e\u5e94\u529b\u548c\u5e94\u53d8\u4e0d\u5747\u5300\u6027\uff0c\u7ed3\u679c\u8bc1\u660e\u662f\u4f4e\u6e29\u4e0b\u7406\u60f3\u7684\u5f3a\u5316\u673a\u5236\uff0c\u4f46\u6f5c\u5728\u7684\u5f3a\u5316\u673a\u5236\u53ca\u5176\u53ef\u8c03\u6027\u81f3\u4eca\u4ecd\u4e0d\u6e05\u695a\u3002<\/p>\n\n\n\n<p><strong>\u4e8c\u3001<\/strong><strong>\u3010\u6210\u679c\u63a0\u5f71\u3011<\/strong><\/p>\n\n\n\n<p>\u5728\u6b64\uff0c<strong>\u534e\u4e1c\u7406\u5de5\u5927\u5b66\u5f20\u663e\u7a0b\u6559\u6388\u548c\u5fb7\u56fd\u9a6c\u514b\u601d\u666e\u6717\u514b\u53ef\u6301\u7eed\u6750\u6599\u7814\u7a76\u6240Dierk Raabe\u9662\u58eb\u7b49\u4eba<\/strong><strong>\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\u5728\u57fa\u4e8eCoNiV\u7684\u5408\u91d1\u4e2d\u5f15\u5165\u4e86\u4e00\u79cd\u53cc\u5c3a\u5ea6\u539f\u5b50\u6392\u5e8f\u7eb3\u7c73\u7ed3\u6784\uff0c\u8be5\u7ed3\u6784\u4ee5\u6781\u9ad8\u7684\u6570\u91cf\u5bc6\u5ea6\u7684\uff08\u7ea62.4\u00d710<sup>26<\/sup>&nbsp;m<sup>-3<\/sup>\uff09\u4e9a\u7eb3\u7c73\u5c3a\u5ea6\u77ed\u7a0b\u6709\u5e8f\u548c\uff08\u7ea64.5\u00d710<sup>25<\/sup>&nbsp;m<sup>-3<\/sup>\uff09\u7eb3\u7c73\u5c3a\u5ea6\u957f\u7a0b\u6709\u5e8f\u57df\u4e3a\u7279\u5f81\uff0c\u8fd9\u4e9b\u6709\u5e8f\u57df\u5171\u5b58\u4e8e\u91d1\u5c5e\u56fa\u6eb6\u4f53\u57fa\u4f53\u4e2d\uff0c\u4ee5\u6539\u5584\u4f4e\u6e29\u4e0b\u7684\u5f3a\u5ea6\u548c\u5ef6\u5c55\u6027\u7684\u534f\u540c\u4f5c\u7528\u3002\u7ed3\u679c\u663e\u793a\uff0c\u7531\u4e8e\u7eb3\u7c73\u5c3a\u5ea6\u957f\u7a0b\u6709\u5e8f\u7684\u4f4d\u9519\u963b\u6321\u6548\u5e94\u4ee5\u53ca\u7531\u6b64\u4ea7\u751f\u7684\u65b0\u4f4d\u9519\uff0c\u4f7f\u5f97\u4f4d\u9519\u526a\u5207\u5e94\u529b\u589e\u52a0\u4ee5\u53ca\u4f4d\u9519\u589e\u6b96\u901f\u5ea6\u52a0\u5feb\u3002\u540e\u4e00\u79cd\u6548\u5e94\u8fd8\u91ca\u653e\u4e86\u7eb3\u7c73\u5c3a\u5ea6\u957f\u7a0b\u6709\u5e8f\u969c\u788d\u7269\u5904\u7684\u5e94\u529b\u96c6\u4e2d\uff0c\u5426\u5219\u8fd9\u4e9b\u5e94\u529b\u96c6\u4e2d\u4f1a\u4fc3\u8fdb\u635f\u4f24\u7684\u8d77\u59cb\u548c\u5931\u6548\u3002\u56e0\u6b64\uff0c\u8be5\u5408\u91d1\u572887 K\u65f6\u5c55\u73b0\u51fa\u7ea61.2 GPa\u7684\u5c48\u670d\u5f3a\u5ea6\u548c76 GPa%\u7684\u5f3a\u5ea6-\u5ef6\u4f38\u7387\u4e58\u79ef\uff0c\u4f18\u4e8e\u7f3a\u4e4f\u8fd9\u79cd\u6709\u5e8f\u5c42\u6b21\u7ed3\u6784\u7684\u6750\u6599\uff0c\u8fd9\u4e9b\u6750\u6599\u4ec5\u5305\u542b\u77ed\u7a0b\u6709\u5e8f\u6216\u51e0\u5341\u7eb3\u7c73\u5c3a\u5bf8\u7684\u5171\u683c\u6c89\u6dc0\u7269\u3002\u672c\u6587\u7684\u7ed3\u679c\u7a81\u51fa\u4e86\u53cc\u5171\u5b58\u5316\u5b66\u6709\u5e8f\u5bf9\u590d\u6742\u5408\u91d1\u529b\u5b66\u6027\u80fd\u7684\u5f71\u54cd\uff0c\u5e76\u4e3a\u63a7\u5236\u8fd9\u4e9b\u6709\u5e8f\u72b6\u6001\u4ee5\u589e\u5f3a\u5176\u4f4e\u6e29\u5e94\u7528\u7684\u529b\u5b66\u6027\u80fd\u63d0\u4f9b\u4e86\u6307\u5bfc\u3002<\/p>\n\n\n\n<p>\u76f8\u5173\u7814\u7a76\u6210\u679c\u4ee5\u201c<strong>Dual-scale chemical ordering for cryogenic properties in CoNiV-based alloys<\/strong>\u201d\u4e3a\u9898\u53d1\u8868\u5728<strong><em>N<\/em><\/strong><strong><em>ature<\/em><\/strong>\u4e0a\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"348\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/08\/\u5c01\u9762.jpg\" alt=\"\" class=\"wp-image-268134\" \/><\/figure>\n\n\n\n<p><strong>\u4e09\u3001<\/strong><strong>\u3010\u6838\u5fc3\u521b\u65b0\u70b9\u3011<\/strong><strong><\/strong><\/p>\n\n\n\n<p>1.\u5728\u57fa\u4e8eCoNiV\u7684\u5408\u91d1\u4e2d\u5b9e\u73b0\u4e86\u7eb3\u7c73\u7ed3\u6784\u8bbe\u8ba1\u7b56\u7565\uff0c\u5176\u7ec4\u6210\u4e3aCo<sub>32<\/sub>Ni<sub>32<\/sub>V<sub>32<\/sub>Al<sub>2<\/sub>Ti<sub>2<\/sub>\uff08\u539f\u5b50\u767e\u5206\u6bd4\uff09\u3002\u9492\uff08V\uff09\u4e0e\u94b4\uff08Co\uff09\u548c\u954d\uff08Ni\uff09\u4e4b\u95f4\u7684\u7113\u76f8\u4e92\u4f5c\u7528\uff0c\u4ee5\u53ca\u5b83\u4eec\u5728\u539f\u5b50\u5c3a\u5bf8\u548c\u526a\u5207\u6a21\u91cf\u4e0a\u7684\u663e\u8457\u4e0d\u5339\u914d\uff0c\u4fc3\u8fdb\u4e86\u5c40\u90e8\u5316\u5b66\u77ed\u7a0b\u6709\u5e8f\u7684\u5f62\u6210\u3002<\/p>\n\n\n\n<p>2.\u7eb3\u7c73\u5c3a\u5ea6\u957f\u7a0b\u6709\u5e8f\u7684\u4f4d\u9519\u963b\u6321\u6548\u5e94\u4ee5\u53ca\u7531\u6b64\u4ea7\u751f\u7684\u65b0\u4f4d\u9519\uff0c\u4f7f\u5f97\u4f4d\u9519\u526a\u5207\u5e94\u529b\u589e\u52a0\u4ee5\u53ca\u4f4d\u9519\u589e\u6b96\u901f\u5ea6\u52a0\u5feb\uff0c\u4e14\u540e\u4e00\u79cd\u6548\u5e94\u8fd8\u91ca\u653e\u4e86\u7eb3\u7c73\u5c3a\u5ea6\u957f\u7a0b\u6709\u5e8f\u969c\u788d\u7269\u5904\u7684\u5e94\u529b\u96c6\u4e2d\u3002<\/p>\n\n\n\n<p><strong>\u56db\u3001<\/strong><strong>\u3010\u6570\u636e\u6982\u89c8\u3011<\/strong><strong><\/strong><\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"600\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/08\/\u56fe\u72471-1.jpg\" alt=\"\" class=\"wp-image-268135\" \/><\/figure>\n\n\n\n<p><strong>\u56fe<\/strong><strong>1 \u672c\u6587CoNiV-AlTi\u6837\u54c1\u7684\u5fae\u89c2\u7ed3\u6784\u548c\u53cc\u5c3a\u5ea6\u5316\u5b66\u6709\u5e8f\u3002<\/strong><strong><\/strong><\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"247\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/08\/\u56fe\u72472-1.jpg\" alt=\"\" class=\"wp-image-268136\" \/><\/figure>\n\n\n\n<p><strong>\u56fe<\/strong><strong>2 \u7814\u7a76\u5408\u91d1\u572887 K\u65f6\u7684\u4f4e\u6e29\u62c9\u4f38\u6027\u80fd\u3002<\/strong><strong><\/strong><\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"494\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/08\/\u56fe\u72473-1.jpg\" alt=\"\" class=\"wp-image-268137\" \/><\/figure>\n\n\n\n<p><strong>\u56fe<\/strong><strong>3 CoNiV-AlTi\u5408\u91d1\u7684\u5178\u578b\u53d8\u5f62\u4e9a\u7ed3\u6784\u3002<\/strong><strong><\/strong><\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"499\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/08\/\u56fe\u72474-1.jpg\" alt=\"\" class=\"wp-image-268138\" \/><\/figure>\n\n\n\n<p><strong>\u56fe<\/strong><strong>4 \u542b\u6709\u4e0d\u540c\u6709\u5e8f\u7ed3\u6784\u7684\u6837\u54c1\uff08CoNiV-AlTi\u3001CoNiV(SS)\u548cCoNiV(SSA)\uff09\u7684\u6e29\u5ea6\u4f9d\u8d56\u6027\u529b\u5b66\u884c\u4e3a\u3002<\/strong><strong><\/strong><\/p>\n\n\n\n<p><strong>\u4e94\u3001<\/strong><strong>\u3010\u6210\u679c\u542f\u793a\u3011<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u7efc\u4e0a\u6240\u8ff0\uff0c\u4f5c\u8005\u8868\u660e\u53cc\u5c3a\u5ea6\u77ed\u7a0b\u5230\u957f\u7a0b\u5316\u5b66\u6709\u5e8f\u7b56\u7565\u53ef\u4ee5\u663e\u8457\u6539\u5584\u91d1\u5c5e\u5408\u91d1\u5728\u4f4e\u6e29\u4e0b\u7684\u529b\u5b66\u6027\u80fd\u3002\u8fd9\u4e24\u79cd\u6709\u5e8f\u7ed3\u6784\u9650\u5236\u4e86\u4f4d\u9519\u7684\u5e73\u5747\u81ea\u7531\u7a0b\uff0c\u5e76\u5728\u4f4e\u6e29\u4e0b\u63d0\u4f9b\u66f4\u9ad8\u7684\u6469\u64e6\u5e94\u529b\uff08\u8d4b\u4e88\u5f3a\u5ea6\uff09\u548c\u66f4\u5feb\u7684\u4f4d\u9519\u589e\u6b96\u7387\uff08\u589e\u5f3a\u5e94\u53d8\u786c\u5316\u80fd\u529b\uff09\uff0c\u4e0e\u6ca1\u6709\u8fd9\u79cd\u6709\u5e8f\u5c42\u6b21\u7ed3\u6784\u7684\u53c2\u8003\u6837\u54c1\u76f8\u6bd4\u3002\u8fd9\u79cd\uff08\u4e9a\uff09\u7eb3\u7c73\u5c3a\u5ea6\u5fae\u89c2\u7ed3\u6784\u7b56\u7565\u4e0e\u5e7f\u6cdb\u91c7\u7528\u7684\u6c89\u6dc0\u786c\u5316\u65b9\u6cd5\u4e0d\u540c\uff0c\u540e\u8005\u4f1a\u4ea7\u751f\u5c40\u90e8\u5e94\u529b\u5cf0\u503c\uff0c\u53ef\u80fd\u5bfc\u81f4\u635f\u4f24\u8d77\u59cb\u3002\u8fd8\u5728\u57fa\u4e8eNiCrFe\u548cCoCrNi\u7684\u4e2d\u71b5\u5408\u91d1\uff08MEAs\uff09\u4e2d\u9a8c\u8bc1\u4e86\u53cc\u5c3a\u5ea6\u5316\u5b66\u6709\u5e8f\u65b9\u6cd5\u5728\u6539\u5584\u4f4e\u6e29\u5f3a\u5ea6-\u5ef6\u5c55\u6027\u534f\u540c\u4f5c\u7528\u65b9\u9762\u7684\u6709\u6548\u6027\uff0c\u8bc1\u660e\u4e86\u6982\u5ff5\u7684\u666e\u904d\u6027\u3002\u56e0\u6b64\uff0c\u672c\u6587\u7684\u5de5\u4f5c\u6269\u5c55\u4e86\u5fae\u89c2\u7ed3\u6784\u8bbe\u8ba1\uff0c\u5f25\u8865\u4e86\u6b64\u524d\u7f3a\u4e4f\u4f7f\u5408\u91d1\u80fd\u591f\u627f\u53d7\u6076\u52a3\u4f4e\u6e29\u73af\u5883\u7684\u6709\u6548\u624b\u6bb5\u3002<\/p>\n\n\n\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a\u201c<\/strong><a href=\"https:\/\/www.nature.com\/articles\/s41586-025-09458-1\"><strong><u>Dual-scale chemical ordering for cryogenic properties in<\/u><\/strong><strong><u>&nbsp;<\/u><\/strong><strong><u>CoNiV-based alloys<\/u><\/strong><\/a><strong>\u201d<\/strong><strong>\uff08<\/strong><strong><em>N<\/em><\/strong><strong><em>ature<\/em><\/strong><strong>\uff0c<\/strong><strong>202<\/strong><strong>4<\/strong><strong>\uff0c<\/strong><strong>10.1038\/s41586-025-09458-1<\/strong><strong>\uff09<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u672c\u6587\u7531\u6750\u6599\u4ebaCYM\u7f16\u8bd1\u4f9b\u7a3f\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4e00\u3001\u3010\u5bfc\u8bfb\u3011 \u5927\u591a\u6570\u5408\u91d1\u53ca\u5176\u5fae\u89c2\u7ed3\u6784\u5728\u8fc7\u53bb\u51e0\u5341\u5e74\u4e2d\u5df2\u7ecf\u5f00\u53d1\u51fa\u6765\uff0c\u4ee5\u5728\u5ba4\u6e29\u548c\u9ad8\u6e29\u4e0b\u63d0\u4f9b\u6240\u9700\u7684\u529b\u5b66\u6027\u80fd\u3002\u7136\u800c\uff0c\u5c3d\u7ba1\u5728\u8fd9\u4e00\u9886\u57df\u6210\u672c\u9650\u5236\u4e0d\u592a\u4e25\u683c\uff0c\u4f46\u7528\u4e8e\u9ad8\u5f3a\u5ea6\u548c\u8010\u635f\u4f24\u4f4e&#8230;<\/p>\n","protected":false},"author":9629,"featured_media":268134,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[293],"class_list":["post-268133","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu","tag-nature"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/268133"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/9629"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=268133"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/268133\/revisions"}],"predecessor-version":[{"id":268139,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/268133\/revisions\/268139"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/268134"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=268133"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=268133"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=268133"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}