{"id":268677,"date":"2025-09-29T07:53:00","date_gmt":"2025-09-28T23:53:00","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=268677"},"modified":"2025-09-28T21:04:59","modified_gmt":"2025-09-28T13:04:59","slug":"%e9%87%8d%e5%ba%86%e5%a4%a7%e5%ad%a6%e8%89%be%e6%96%8cchemical-society-reviews%ef%bc%9a%e5%9f%ba%e4%ba%8e%e9%98%b4%e5%bd%b1%e7%90%83%e5%85%89%e5%88%bb%e3%80%81%e7%ad%89%e7%a6%bb%e5%ad%90%e4%bd%93","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=268677","title":{"rendered":"\u91cd\u5e86\u5927\u5b66\u827e\u658cChemical Society Reviews\uff1a\u57fa\u4e8e\u9634\u5f71\u7403\u5149\u523b\u3001\u7b49\u79bb\u5b50\u4f53\u4e0e\u4eba\u5de5\u667a\u80fd\u7684\u4e0b\u4e00\u4ee3\u667a\u80fd\u4f20\u611f"},"content":{"rendered":"\n<p><strong>\u4e00\u3001<\/strong><strong>&nbsp;<\/strong><strong>\u3010\u5bfc\u8bfb\u3011 &nbsp;<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u5728\u80fd\u6e90\u3001\u533b\u7597\u5065\u5eb7\u548c\u667a\u80fd\u5236\u9020\u7b49\u5feb\u901f\u53d1\u5c55\u9886\u57df\uff0c\u5bf9\u4f20\u611f\u5668\u7684\u6027\u80fd\u63d0\u51fa\u4e86\u524d\u6240\u672a\u6709\u7684\u8981\u6c42\uff1a\u4e9a\u767e\u5206\u70b9\u7cbe\u5ea6\u3001\u6beb\u79d2\u7ea7\u54cd\u5e94\u3001\u957f\u671f\u7a33\u5b9a\u6027\u548c\u6676\u5706\u7ea7\u96c6\u6210\uff0c\u800c\u4f20\u7edf\u7684\u4f20\u611f\u5668\u96be\u4ee5\u6ee1\u8db3\u8fd9\u4e9b\u9700\u6c42\u3002\u8fd1\u5e74\u6765\u5174\u8d77\u7684\u7b49\u79bb\u5b50\u4f53\u5fae\u7eb3\u5149\u5b66\u4f20\u611f\u5668\u6709\u671b\u5728\u539f\u7406\u4e0a\u652f\u6491\u8fd9\u4e9b\u6781\u9650\u6307\u6807\uff0c\u4f46\u5fc5\u987b\u4f9d\u8d56\u4e09\u4e2a\u957f\u671f\u76f8\u4e92\u72ec\u7acb\u7684\u7814\u7a76\u65b9\u5411\u7684\u6df1\u5ea6\u878d\u5408\uff1a<\/p>\n\n\n\n<ol class=\"wp-block-list\">\n<li>\u7269\u7406\u9a71\u52a8\u7684\u7eb3\u7c73\u7ed3\u6784\u8bbe\u8ba1\u00a0\u2014\u2014\u00a0\u6784\u5efa\u9ad8\u54c1\u8d28\u56e0\u5b50\uff08High-Q\uff09\u7684\u6df7\u5408\u5171\u632f\u6a21\u5f0f\uff1b<\/li>\n\n\n\n<li>\u53ef\u6269\u5c55\u4f4e\u6210\u672c\u7684\u5236\u9020\u8def\u7ebf\u00a0\u2014\u2014\u00a0\u5c06\u8bbe\u8ba1\u84dd\u56fe\u8f6c\u5316\u4e3a\u5927\u9762\u79ef\u3001\u53ef\u91cf\u4ea7\u7684\u5668\u4ef6\uff1b<\/li>\n\n\n\n<li>\u6570\u636e\u9a71\u52a8\u7684\u4fe1\u53f7\u5904\u7406\u4e0e\u9884\u6d4b\u00a0\u2014\u2014\u00a0\u4ece\u672c\u8d28\u4e0a\u5fae\u5f31\u4e14\u6f02\u79fb\u654f\u611f\u7684\u5149\u5b66\u8bfb\u51fa\u4e2d\u63d0\u53d6\u53ef\u9760\u4fe1\u606f\u3002<\/li>\n<\/ol>\n\n\n\n<p><strong>\u4e8c\u3001\u3010\u6210\u679c\u63a0\u5f71\u3011<\/strong><strong><\/strong><\/p>\n\n\n\n<p><strong>\u91cd\u5e86\u5927\u5b66\u5fae\u7535\u5b50\u4e0e\u901a\u4fe1\u5de5\u7a0b\u5b66\u9662\u827e\u658c\u56e2\u961f<\/strong>\u5728Chemical Society Reviews\u5728\u7ebf\u53d1\u8868\u4e86\u9898\u4e3a\u201cClosing the loop in next-generation sensing through shadow sphere lithography, plasmonics, and artificial intelligence\u201d\u7684\u7efc\u8ff0\u6027\u8bba\u6587\uff0c\u8be5\u7efc\u8ff0\u7cfb\u7edf\u6027\u5730\u56de\u987e\u4e862019\u20132024\u5e74\u4e0a\u8ff0\u7814\u7a76\u80cc\u666f\u4e2d\u7684\u63d0\u5230\u4e09\u6761\u7814\u7a76\u8def\u7ebf\u7684\u5168\u94fe\u6761\u878d\u5408\u8fdb\u5c55\u3002\u7814\u7a76\u56e2\u961f\u91cd\u70b9\u4ecb\u7ecd\u4e86&nbsp;\u201c<strong>\u9634\u5f71\u7403\u5149\u523b\uff08Shadow-Sphere Lithography, SSL\uff09<\/strong>\u201d\u4f5c\u4e3a\u4e00\u79cd\u53ef\u6269\u5c55\u7684\u4e9a50\u7eb3\u7c73\u56fe\u6848\u5316\u65b9\u6cd5\uff0c\u5ba1\u89c6\u4e86\u8868\u9762\u7b49\u79bb\u5b50\u4f53\u81ea\u7ec4\u88c5SSL\u7684\u73b0\u72b6\uff0c\u9610\u8ff0\u51b3\u5b9a\u7279\u5f81\u5f62\u8c8c\u7684\u81ea\u7ec4\u88c5\u7269\u7406\u539f\u7406\u53ca\u540e\u5904\u7406\u7b56\u7565\u3002\u5c06\u8fd9\u4e00\u7ed3\u6784\u5e93\u6620\u5c04\u5230\u5149\u5b66\u9886\u57df\uff0c\u89e3\u91ca\u7279\u5b9a\u51e0\u4f55\u5982\u4f55\u6fc0\u53d1\u5c40\u57df\u8868\u9762\u7b49\u79bb\u5b50\u4f53\u3001\u6676\u683c\u6216\u675f\u7f1a\u6001\u5171\u632f\uff0c\u4ee5\u53ca\u8fd9\u4e9b\u6a21\u5f0f\u5982\u4f55\u5728\u7075\u654f\u5ea6\u3001\u7279\u5f02\u6027\u548c\u5149\u8c31\u5e26\u5bbd\u65b9\u9762\u63a8\u52a8\u6700\u65b0\u8fdb\u5c55\u3002\u7cfb\u7edf\u56de\u987e\u7269\u7406\u611f\u77e5\u7684\u9884\u5904\u7406\u3001\u7279\u5f81\u5de5\u7a0b\u3001\u6709\u76d1\u7763\u4e0e\u65e0\u76d1\u7763\u5b66\u4e60\u53ca\u9006\u5411\u8bbe\u8ba1\uff0c\u5c55\u793a\u6bcf\u79cd\u6280\u672f\u5982\u4f55\u7f13\u89e3\u5236\u9020\u76f8\u5173\u9650\u5236\u6216\u89e3\u9501\u65b0\u7684\u4f20\u611f\u6a21\u5f0f\u3002\u6700\u540e\uff0c\u6211\u4eec<strong>\u6982\u8ff0\u4e86\u4e00\u4e2a\u95ed\u73af\u8def\u7ebf<\/strong>\uff0c<strong>\u94fe\u63a5SSL\u3001\u7b49\u79bb\u5b50\u4f53\u548c\u4eba\u5de5\u667a\u80fd\uff08AI\uff09\u5206\u6790<\/strong>\uff0c\u76ee\u6807\u662f\u5728\u6beb\u7c73\u8303\u56f4\u5185\u5b9e\u73b0\u9ad8\u6298\u5c04\u7387\u5206\u8fa8\u7387\uff0c\u540c\u65f6\u786e\u5b9a\u56fe\u6848\u7ed3\u6784\u9006\u5411\u8bbe\u8ba1\u548c\u81ea\u52a8\u5316\u81ea\u7ec4\u88c5\uff0c\u5728\u7ebf\u8d28\u91cf\u5206\u7ea7\uff0c\u81ea\u9002\u5e94\u4fe1\u53f7\u89e3\u91ca\u7b49\u65b9\u9762\u7684\u5f00\u653e\u6311\u6218\u3002<strong><\/strong><\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"700\" height=\"343\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/09\/2382c315a6ba396-30.png\" alt=\"\" class=\"wp-image-268681\"\/><\/figure>\n\n\n\n<p>&nbsp;\u4e09\u3001\u3010\u6838\u5fc3\u521b\u65b0\u70b9\u3011<\/p>\n\n\n\n<ol class=\"wp-block-list\">\n<li><strong>\u591a\u53c2\u6570\u534f\u540c\u7684\u201c\u5de5\u827a-\u7ed3\u6784-\u5149\u5b66\u201d\u53ef\u7f16\u7a0b\u8bbe\u8ba1<\/strong><strong>\u3002<\/strong>\u7cfb\u7edf\u63ed\u793a\u5e76\u5229\u7528\u4e86SSL\u4e2d\u7403\u5f84-\u89d2\u5ea6-\u5468\u671f-\u8680\u523b-\u6c89\u79ef\u7b49\u591a\u53c2\u6570\u7684\u534f\u540c\u5173\u7cfb\uff0c\u603b\u7ed3\u4e86\u4ece\u4e8c\u7ef4\u7eb3\u7c73\u73af\u3001\u4e09\u89d2\u7f1d\u9699\u5230\u4e09\u7ef4\u87ba\u65cb\u3001\u7eb3\u7c73\u94a9\u7b49\u590d\u6742\u975e\u5bf9\u79f0\u7ed3\u6784\u7684\u53ef\u7f16\u7a0b\u5236\u9020\u8def\u5f84\u3002<\/li>\n\n\n\n<li><strong>\u201c\u7ed3\u6784-\u5149\u8c31-\u6027\u80fd\u201d\u53ef\u9884\u6d4b\u6620\u5c04\u6a21\u578b<\/strong><strong>\u3002<\/strong>\u5b9e\u73b0\u4e86\u5bf9 SERS\u3001SEF\u3001SEIRAS \u7b49\u591a\u79cd\u7b49\u79bb\u5b50\u4f53\u589e\u5f3a\u5149\u8c31\u6280\u672f\u7684\u9ad8\u7cbe\u5ea6\u5b9a\u91cf\u4e0e\u5206\u7c7b\u9884\u6d4b<strong>\u3002<\/strong><\/li>\n\n\n\n<li><strong>AI\u95ed\u73af\u4fe1\u53f7\u5f15\u64ce<\/strong><strong>\u3002<\/strong>\u7cfb\u7edf\u603b\u7ed3\u4e86\u4eba\u5de5\u667a\u80fd\u5728\u7b49\u79bb\u5b50\u4f53\u4f20\u611f\u5668\u9006\u5411\u8bbe\u8ba1\u4e0e\u5168\u5149\u8c31\u667a\u80fd\u89e3\u6790\u4e2d\u7684\u7a81\u7834\u6027\u4f5c\u7528\uff0c\u91cd\u70b9\u63ed\u793a\u4e86AI\u5982\u4f55\u901a\u8fc7\u95ed\u73af\u4f18\u5316\u5c06\u4f20\u611f\u5668\u7814\u53d1\u4ece\u201c\u7ecf\u9a8c\u9a71\u52a8\u201d\u5347\u7ea7\u4e3a\u201c\u76ee\u6807\u9a71\u52a8\u201d\u8303\u5f0f\u3002<\/li>\n<\/ol>\n\n\n\n<p><strong>\u56db\u3001\u3010\u6570\u636e\u6982\u89c8\u3011 <\/strong><strong><\/strong><\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"1380\" height=\"1138\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/09\/ce6e2814f207c93-26.png\" alt=\"\" class=\"wp-image-268678\"\/><\/figure>\n\n\n\n<p><strong>\u56fe1 &nbsp;&nbsp;SSL<\/strong><strong>\u7684<\/strong><strong>\u6d41\u7a0b\u6a21\u5757\u5316<\/strong><strong>\u53ca\u7ed3\u6784\u5206\u7c7b\u6bd4\u8f83<\/strong><strong>\u3002\u00a9 2025 <\/strong><strong>The Royal Society of Chemistry<\/strong><strong><\/strong><\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"775\" height=\"739\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/09\/7f88dbbcaa77a1d-27.png\" alt=\"\" class=\"wp-image-268679\"\/><\/figure>\n\n\n\n<p><strong>\u56fe2 &nbsp;<\/strong>\u4e0d\u540c\u7b56\u7565\u4e0b\u7ed3\u6784\u7279\u5f81\u548c\u611f\u77e5\u4f18\u52bf\u3002<strong>\u00a9 2025<\/strong><strong>&nbsp;The Royal Society of Chemistry<\/strong><strong><\/strong><\/p>\n\n\n\n<div class=\"wp-block-group is-nowrap is-layout-flex wp-container-core-group-is-layout-1 wp-block-group-is-layout-flex\">\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"1271\" height=\"875\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/09\/4e9a0ba2491dfde-26.png\" alt=\"\" class=\"wp-image-268680\"\/><\/figure>\n\n\n\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-admin\/edit.php?post_type=post\"><\/a><\/p>\n<\/div>\n\n\n\n<p><strong>\u56fe3 \u00a0<\/strong><strong>AI<\/strong><strong>\u4e0e\u7b49\u79bb\u5b50\u4f53\u4f20\u611f\u7684\u7ed3\u5408\u3002\u00a9<\/strong><strong>\u00a0<\/strong><strong>2025 <\/strong><strong>The Royal Society of Chemistry<\/strong><\/p>\n\n\n\n<p><strong>\u4e94\u3001\u3010\u6210\u679c\u542f\u793a\u3011<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u672c\u6587\u63d0\u51fa\u4e86\u4e00\u4e2a<strong>\u95ed\u73af\u7814\u7a76\u8def\u7ebf<\/strong>\u2014\u2014\u5c06&nbsp;SSL\u3001\u5927\u9762\u79ef\u4f4e\u6210\u672c\u5236\u9020\u3001\u7b49\u79bb\u5b50\u4f53\u7eb3\u7c73\u5149\u5b66\u3001\u4ee5\u53ca&nbsp;AI&nbsp;\u9a71\u52a8\u7684\u6570\u636e\u5206\u6790\u6709\u673a\u7ed3\u5408\uff0c\u7784\u51c6\u5728\u6beb\u7c73\u7ea7\u4f20\u611f\u5668\u4e2d\u5b9e\u73b0\u9ad8\u6298\u5c04\u7387\u5206\u8fa8\u7387\uff0c\u5e76\u6307\u51fa\u4e86\u672a\u6765\u7684\u91cd\u5927\u6311\u6218\uff0c\u5305\u62ec\u6676\u5706\u7ea7\u4e09\u7ef4\u56fe\u6848\u5316\u7684\u9006\u5411\u8bbe\u8ba1\u3001\u81ea\u7ec4\u88c5\u7b56\u7565\u3001\u5728\u7ebf\u8d28\u91cf\u5206\u7ea7\u4e0e\u81ea\u9002\u5e94\u4fe1\u53f7\u89e3\u6790\u3002\u8be5\u6280\u672f\u6846\u67b6\u7684\u5e94\u7528\u610f\u4e49\u5728\u4e8e\u6253\u901a\u4e86\u201c\u7eb3\u7c73\u7ed3\u6784\u8bbe\u8ba1-\u5149\u8c31\u91c7\u96c6-AI\u89e3\u6790\u201d\u7684\u5168\u94fe\u6761\u534f\u540c\uff0c\u4f7fSSL\u7b49\u79bb\u5b50\u4f53\u4f20\u611f\u5668\u4ece\u5b9e\u9a8c\u5ba4\u5de5\u5177\u5347\u7ea7\u4e3a\u5177\u5907\u5de5\u4e1a\u90e8\u7f72\u6f5c\u529b\u7684\u667a\u80fd\u8bca\u65ad\u5e73\u53f0\uff0c\u4e0d\u4ec5\u80fd\u6ee1\u8db3\u590d\u6742\u73af\u5883\u4e2d\u9ad8\u7cbe\u5ea6\u5316\u5b66\/\u751f\u7269\u68c0\u6d4b\u9700\u6c42\uff0c\u66f4\u53ef\u80fd\u901a\u8fc7\u9006\u5411\u8bbe\u8ba1\u63a8\u52a8\u4f20\u611f\u5143\u4ef6\u7684\u6309\u9700\u5b9a\u5236\uff0c\u91cd\u65b0\u5b9a\u4e49\u4e0b\u4e00\u4ee3\u667a\u80fd\u4f20\u611f\u5668\u7684\u6027\u80fd\u8fb9\u754c\u3002\u8be5\u7814\u7a76\u7684\u7cfb\u7edf\u603b\u7ed3\u4e3a\u5b9e\u73b0\u9ad8\u6027\u80fd\u3001\u667a\u80fd\u5316\u3001\u53ef\u89c4\u6a21\u843d\u5730\u7684\u5149\u5b66\u4f20\u611f\u5668\u63d0\u4f9b\u4e86\u5168\u666f\u5f0f\u5c55\u671b\uff0c\u5bf9\u63a8\u52a8<strong>\u80fd\u6e90\u3001\u533b\u7597\u5065\u5eb7\u3001\u98df\u54c1\u4e0e\u5236\u836f\u7b49\u884c\u4e1a\u7684\u667a\u80fd\u4f20\u611f\u4e0e\u8d28\u91cf\u68c0\u6d4b<\/strong>\u5177\u6709\u91cd\u8981\u610f\u4e49\u3002<\/p>\n\n\n\n<p><strong>\u539f\u6587\u8be6\u60c5<\/strong>\uff1a<\/p>\n\n\n\n<p>Mingyu Cheng, et al. Closing the Loop in Next-generation Sensing through Shadow Sphere Lithography, Plasmonics, and Artificial Intelligence. Chem. Soc. Rev., 2025. DOI: 10.1039\/D5CS00345H<\/p>\n\n\n\n<figure class=\"wp-block-embed\"><div class=\"wp-block-embed__wrapper\">\nhttps:\/\/pubs.rsc.org\/en\/Content\/ArticleLanding\/2025\/CS\/D5CS00345H\n<\/div><\/figure>\n","protected":false},"excerpt":{"rendered":"<p>\u4e00\u3001&nbsp;\u3010\u5bfc\u8bfb\u3011 &nbsp; \u5728\u80fd\u6e90\u3001\u533b\u7597\u5065\u5eb7\u548c\u667a\u80fd\u5236\u9020\u7b49\u5feb\u901f\u53d1\u5c55\u9886\u57df\uff0c\u5bf9\u4f20\u611f\u5668\u7684\u6027\u80fd\u63d0\u51fa\u4e86\u524d\u6240\u672a\u6709\u7684\u8981\u6c42\uff1a\u4e9a\u767e\u5206\u70b9\u7cbe\u5ea6\u3001\u6beb\u79d2\u7ea7\u54cd\u5e94\u3001\u957f\u671f\u7a33\u5b9a\u6027\u548c\u6676\u5706&#8230;<\/p>\n","protected":false},"author":31345,"featured_media":0,"comment_status":"open","ping_status":"","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-268677","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/268677"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/31345"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=268677"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/268677\/revisions"}],"predecessor-version":[{"id":268682,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/268677\/revisions\/268682"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=268677"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=268677"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=268677"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}