{"id":269605,"date":"2025-11-25T07:58:00","date_gmt":"2025-11-24T23:58:00","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=269605"},"modified":"2025-11-24T21:00:07","modified_gmt":"2025-11-24T13:00:07","slug":"%e6%ad%a6%e7%a7%91%e5%a4%a7%e7%8e%8b%e7%8e%89%e5%8d%8e%e8%af%be%e9%a2%98%e7%bb%84%e3%80%8anano-energy%e3%80%8b%ef%bc%9amofs%e8%a1%a8%e9%9d%a2%e5%8c%96%e5%ad%a6%e8%b0%83%e6%8e%a7%e5%8f%8a%e5%85%b6","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=269605","title":{"rendered":"\u6b66\u79d1\u5927\u738b\u7389\u534e\u8bfe\u9898\u7ec4\u300aNano Energy\u300b\uff1aMOFs\u8868\u9762\u5316\u5b66\u8c03\u63a7\u53ca\u5176\u5728\u50ac\u5316\u3001\u4f20\u611f\u4e0e\u50a8\u80fd\u4e2d\u7684\u5e94\u7528\u524d\u77bb"},"content":{"rendered":"\n<p>\u4e00\u3001\u7814\u7a76\u80cc\u666f<\/p>\n\n\n\n<p>&nbsp;\u9762\u5bf9\u6e05\u6d01\u80fd\u6e90\u4e0e\u9ad8\u6548\u5316\u5de5\u7684\u8feb\u5207\u9700\u6c42\uff0c\u4f20\u7edf\u7eb3\u7c73\u6750\u6599\u5728\u7ed3\u6784\u7cbe\u51c6\u8c03\u63a7\u65b9\u9762\u9762\u4e34\u74f6\u9888\u3002\u5728\u6b64\u80cc\u666f\u4e0b\uff0c\u91d1\u5c5e-\u6709\u673a\u6846\u67b6\uff08MOFs\uff09\u6750\u6599\u56e0\u5176\u6781\u9ad8\u7684\u6bd4\u8868\u9762\u79ef\u3001\u9ad8\u5ea6\u53ef\u8c03\u7684\u5b54\u9053\u7ed3\u6784\u548c\u4e30\u5bcc\u7684\u5316\u5b66\u6d3b\u6027\u800c\u8131\u9896\u800c\u51fa\uff0c\u6210\u4e3a\u4e00\u9897\u5907\u53d7\u77a9\u76ee\u7684\u660e\u661f\u3002\u5b83\u5982\u540c\u4e00\u628a\u201c\u4e07\u80fd\u94a5\u5319\u201d\uff0c\u80fd\u591f\u88ab\u7cbe\u51c6\u8bbe\u8ba1\u4ee5\u6ee1\u8db3\u4e0d\u540c\u5e94\u7528\u7684\u7279\u5b9a\u9700\u6c42\u3002\u5c24\u5176\u5728\u50ac\u5316\u3001\u4f20\u611f\u4e0e\u80fd\u6e90\u5b58\u50a8\u4e09\u5927\u5173\u952e\u9886\u57df\uff0cMOFs\u4f5c\u4e3a\u6d3b\u6027\u8f7d\u4f53\u3001\u79bb\u5b50\u901a\u9053\u548c\u4fe1\u53f7\u8f6c\u6362\u5668\u7684\u6f5c\u529b\u5de8\u5927\u3002\u800c\u8981\u7a81\u7834\u73b0\u6709\u6280\u672f\u5929\u82b1\u677f\uff0c\u6df1\u5165\u7406\u89e3\u5e76\u7cbe\u51c6\u9a7e\u9a6d\u5176\u8868\u9762\u5316\u5b66\u6027\u8d28\uff0c\u5df2\u6210\u4e3a\u5b9e\u73b0\u8fd9\u4e00\u7a81\u7834\u7684\u6838\u5fc3\u6240\u5728\u3002<\/p>\n\n\n\n<p>\u4e8c\u3001\u6587\u7ae0\u7b80\u4ecb<\/p>\n\n\n\n<p>\u8fd1\u65e5\uff0c\u6b66\u6c49\u79d1\u6280\u5927\u5b66\u738b\u7389\u534e\u56e2\u961f\u53d1\u8868\u4e86\u9898\u4e3a \u300aMOF in catalysis, sensing and energy storage applications\u300b\u7684\u7efc\u8ff0\u6587\u7ae0 \u3002\u672c\u7efc\u8ff0\u7cfb\u7edf\u9610\u660e\u4e86\u91d1\u5c5e\u6709\u673a\u6846\u67b6\uff08MOFs\uff09\u7684\u4f53\u76f8\u4e0e\u8868\u754c\u9762\u5316\u5b66\u6027\u8d28\u4e0e\u5176\u5728\u50ac\u5316\u3001\u4f20\u611f\u53ca\u50a8\u80fd\u9886\u57df\u6027\u80fd\u95f4\u7684\u6784\u6548\u5173\u7cfb\uff0c\u4e0d\u4ec5\u4e3a\u901a\u8fc7\u8868\u9762\u7ec8\u7aef\u57fa\u56e2\u8c03\u63a7\u4ee5\u4f18\u5316\u5668\u4ef6\u6027\u80fd\u63d0\u4f9b\u4e86\u5b9e\u64cd\u6307\u5357\uff0c\u4e5f\u5c55\u671b\u4e86\u8be5\u9886\u57df\u9762\u4e34\u7684\u6311\u6218\u4e0e\u672a\u6765\u673a\u9047\u3002\u76f8\u5173\u7efc\u8ff0\u53d1\u8868\u5728Nano energy\u4e0a\u3002\u7855\u58eb\u7814\u7a76\u751f\u725b\u96e8\u8587\u4e3a\u8be5\u8bba\u6587\u7b2c\u4e00\u4f5c\u8005\uff0c\u6b66\u6c49\u79d1\u6280\u5927\u5b66\u738b\u7389\u534e\u6559\u6388\u4e3a\u901a\u8baf\u4f5c\u8005\uff0c\u6b66\u6c49\u79d1\u6280\u5927\u5b66\u4e3a\u8bba\u6587\u7b2c\u4e00\u5355\u4f4d\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"700\" height=\"435\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/11\/2382c315a6ba396-34.png\" alt=\"\" class=\"wp-image-269606\"\/><\/figure>\n\n\n\n<p>\u56fe1.&nbsp;MOF\u7684\u53d1\u5c55\u6f14\u53d8\uff0c\u4ee5MOF-5\u4e3a\u4f8b<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li>\u6587\u7ae0\u7b80\u4ecb<\/li>\n<\/ul>\n\n\n\n<p>1\u3001\u4f5c\u8005\u9996\u5148\u4eceMOF\u7684\u7814\u7a76\u60c5\u51b5\u51fa\u53d1\uff0c\u5206\u6790\u4e86MOF\u6750\u6599\u8fd1\u5341\u5e74\u7684\u7814\u7a76\u60c5\u51b5\uff0c\u4ee5\u53ca\u7814\u7a76\u9886\u57df\u6bd4\u4f8b\u7684\u53d8\u5316\u8d8b\u52bf\uff08\u56fe2\uff09\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"700\" height=\"492\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/11\/ce6e2814f207c93-35.png\" alt=\"\" class=\"wp-image-269607\"\/><\/figure>\n\n\n\n<p>\u56fe2. \u968f\u7740\u65f6\u95f4\u7684\u63a8\u79fb\uff0cMOF\u5e94\u7528\u589e\u591a\u3002a|\u8fd125\u5e74\u4ee5\u201cMOF\u201d\u4e3a\u5173\u952e\u8bcd\u7d22\u5f15\u7684\u51fa\u7248\u7269\u53d1\u5c55\u60c5\u51b5\u3002b|2015-2024\u5e74\u7814\u7a76\u9886\u57df\u6bd4\u4f8b\u7684\u53d8\u5316\u8d8b\u52bf\u3002\u8be5\u56fe\u5c55\u793a\u4e86\u50ac\u5316\u3001\u4f20\u611f\u3001\u80fd\u6e90\u3001\u533b\u5b66\u548c\u98df\u54c1\u9886\u57df\u7684\u76f8\u5bf9\u7814\u7a76\u6bd4\u4f8b\uff0c\u53cd\u6620\u4e86\u79d1\u5b66\u7814\u7a76\u7684\u91cd\u70b9\u9886\u57df\u968f\u65f6\u95f4\u7684\u53d8\u5316\u3002<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li>\u4f5c\u8005\u8fd8\u7efc\u8ff0\u4e86\u4f20\u611f\u65b9\u9762\u7684\u5e94\u7528\uff0c\u8be6\u7ec6\u89e3\u91ca\u4e86\u4f20\u611f\u673a\u5236\uff0c\u5982\u56fe2\u3002<\/li>\n<\/ul>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"700\" height=\"472\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/11\/7f88dbbcaa77a1d-31.png\" alt=\"\" class=\"wp-image-269608\"\/><\/figure>\n\n\n\n<p>\u56fe2&nbsp;a| Ni-MOF@Ni-HHTP-5\u6742\u5316NSs\u7684\u5408\u6210\u793a\u610f\u56fe\u53ca\u5176\u5728\u8461\u8404\u7cd6\u68c0\u6d4b\u4e2d\u7684\u5e94\u7528\u3002b|\u8bf4\u660e\u57fa\u4e8eMOF\u5e73\u53f0\u7684\u8367\u5149\u201c\u5f00\u542f\u201d\u4f20\u611f\u673a\u5236\u3002(a)\u6dec\u706d\u8367\u5149\u56e2\u7684\u521d\u59cb\u72b6\u6001\uff08OFF\uff09\u3002(b) MOF\u5b54\u5185\u76ee\u6807\u5206\u6790\u7269\u7684\u7279\u5b9a\u6355\u83b7\u3002(c)\u5206\u6790\u7269\u7ed3\u5408\u6291\u5236\u80fd\u91cf\u8f6c\u79fb\uff0c\u5bfc\u81f4\u8367\u5149\u6062\u590d\u548c\u653e\u5927\u4fe1\u53f7\u8f93\u51fa\uff08ON\uff09\u3002<\/p>\n\n\n\n<p>3\u3001\u4f5c\u8005\u63a5\u7740\u7efc\u8ff0\u4e86\u53ef\u5145\u7535\u7535\u6c60\u7684MOF\u76f8\u5173\u6750\u6599\u793a\u610f\u56fe\uff0c\u5982\u56fe3\u3002\u4ee5\u53ca\u5728\u50a8\u80fd\u65b9\u9762\u7684\u5e94\u7528\uff0c\u5982\u56fe4\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"700\" height=\"440\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/11\/4e9a0ba2491dfde-31.png\" alt=\"\" class=\"wp-image-269609\"\/><\/figure>\n\n\n\n<p>\u56fe3. \u53ef\u5145\u7535\u7535\u6c60\u7528mof\u76f8\u5173\u6750\u6599\u793a\u610f\u56fe\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"700\" height=\"481\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/11\/b14210e1ee30421-28.png\" alt=\"\" class=\"wp-image-269610\"\/><\/figure>\n\n\n\n<p>\u56fe4. MOF\u5728\u80fd\u6e90\u5b58\u50a8\u65b9\u9762\u7684\u5e94\u7528<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li>\u7ed3\u679c\u4e0e\u5c55\u671b<\/li>\n<\/ul>\n\n\n\n<p>MOFs\u6750\u6599\u51ed\u501f\u5176\u9ad8\u6bd4\u8868\u9762\u79ef\u3001\u53ef\u8c03\u5b54\u9053\u53ca\u4e30\u5bcc\u5316\u5b66\u7279\u6027\uff0c\u5728\u50a8\u80fd\u3001\u50ac\u5316\u4e0e\u4f20\u611f\u9886\u57df\u5c55\u73b0\u51fa\u5353\u8d8a\u7684\u591a\u529f\u80fd\u6027\u3002\u7814\u7a76\u5df2\u4ece\u65e9\u671f\u5355\u4e00\u5e94\u7528\uff08\u5982CO\u2082\u8fd8\u539f\u50ac\u5316\u3001\u6c14\u4f53\u4f20\u611f\uff09\u6269\u5c55\u5230\u5668\u4ef6\u5185\u90e8\u5404\u7ec4\u4ef6\uff08\u5982\u7535\u89e3\u8d28\u3001\u96c6\u6d41\u4f53\uff09\uff0c\u5e76\u901a\u8fc7\u8868\u9762\u5316\u5b66\u7cbe\u51c6\u8c03\u63a7\uff08\u5982\u5364\u5316\u7269\u529f\u80fd\u5316\uff09\u4f18\u5316\u5176\u6027\u80fd\u3002\u7136\u800c\uff0cMOFs\u7684\u5546\u4e1a\u5316\u5e94\u7528\u4ecd\u9762\u4e34\u7a33\u5b9a\u6027\u3001\u89c4\u6a21\u5316\u7eff\u8272\u5408\u6210\u53ca\u50a8\u80fd\u673a\u5236\u7406\u89e3\u4e0d\u8db3\u7b49\u6311\u6218\u3002\u672a\u6765\u7814\u7a76\u9700\u805a\u7126\u4e8e\u5f00\u53d1\u5148\u8fdb\u539f\u4f4d\u8868\u5f81\u6280\u672f\uff0c\u7ed3\u5408\u8ba1\u7b97\u6a21\u62df\u6df1\u5165\u63ed\u793a\u201c\u7ed3\u6784-\u6027\u80fd\u201d\u5173\u7cfb\uff0c\u5e76\u63a8\u52a8\u5fae\u6d41\u63a7\u7b49\u9ad8\u6548\u5408\u6210\u65b9\u6cd5\u7684\u53d1\u5c55\uff0c\u6700\u7ec8\u5b9e\u73b0MOFs\u5728\u80fd\u6e90\u8f6c\u6362\u4e0e\u5b58\u50a8\u7cfb\u7edf\u4e2d\u7684\u9ad8\u6027\u80fd\u3001\u957f\u5bff\u547d\u5e94\u7528\u3002<\/p>\n\n\n\n<p>Authors: Yuwei Niu1,2, Yuhua Wang1,2,*, Haijun Zhang1<\/p>\n\n\n\n<p>Title: MOF in catalysis, sensing and energy storage applications<\/p>\n\n\n\n<p>Published in: Nano Energy, https:\/\/doi.org\/10.1016\/j.nanoen.2025.111598<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4e00\u3001\u7814\u7a76\u80cc\u666f &nbsp;\u9762\u5bf9\u6e05\u6d01\u80fd\u6e90\u4e0e\u9ad8\u6548\u5316\u5de5\u7684\u8feb\u5207\u9700\u6c42\uff0c\u4f20\u7edf\u7eb3\u7c73\u6750\u6599\u5728\u7ed3\u6784\u7cbe\u51c6\u8c03\u63a7\u65b9\u9762\u9762\u4e34\u74f6\u9888\u3002\u5728\u6b64\u80cc\u666f\u4e0b\uff0c\u91d1\u5c5e-\u6709\u673a\u6846\u67b6\uff08MOFs\uff09\u6750\u6599\u56e0\u5176\u6781\u9ad8\u7684\u6bd4\u8868\u9762\u79ef&#8230;<\/p>\n","protected":false},"author":31345,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-269605","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/269605"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/31345"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=269605"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/269605\/revisions"}],"predecessor-version":[{"id":269611,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/269605\/revisions\/269611"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=269605"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=269605"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=269605"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}