{"id":270060,"date":"2025-12-29T08:00:00","date_gmt":"2025-12-29T00:00:00","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=270060"},"modified":"2025-12-28T22:32:21","modified_gmt":"2025-12-28T14:32:21","slug":"%e4%b8%9c%e5%8d%97%e5%a4%a7%e5%ad%a6%e6%9d%8e%e4%b9%83%e6%97%ad%e6%95%99%e6%8e%88nature-communications-%e6%b0%a7%e8%b0%83%e6%8e%a7cu0-cu%e7%95%8c%e9%9d%a2%e5%b7%a5%e7%a8%8b%e5%ae%9e%e7%8e%b0","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=270060","title":{"rendered":"\u4e1c\u5357\u5927\u5b66\u674e\u4e43\u65ed\u6559\u6388Nature Communications: \u6c27\u8c03\u63a7Cu0\u2013Cu+\u754c\u9762\u5de5\u7a0b\u5b9e\u73b0\u5149\u70ed\u50ac\u5316\u4e8c\u6c27\u5316\u78b3\u8fd8\u539f\u5236\u4e59\u70ef"},"content":{"rendered":"\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"500\" height=\"686\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/12\/2382c315a6ba396-25.png\" alt=\"\" class=\"wp-image-270061\"\/><\/figure>\n\n\n\n<p><strong>\u7b2c\u4e00\u4f5c\u8005<\/strong>\uff1a\u4efb\u5b87\u5947\uff0c\u7a0b\u6dfc\uff0c\u8d3a\u7ea2\u658c<\/p>\n\n\n\n<p><strong>\u901a\u8baf\u4f5c\u8005\uff1a<\/strong>\u674e\u4e43\u65ed<\/p>\n\n\n\n<p><strong>\u901a\u8baf\u5355\u4f4d\uff1a<\/strong>\u4e1c\u5357\u5927\u5b66<strong><\/strong><\/p>\n\n\n\n<p><strong>\u8bba\u6587DOI\uff1a<\/strong>10.1038\/s41467-025-67844-9<\/p>\n\n\n\n<p><strong>1\ufe0f<\/strong><strong>\u20e3<\/strong><strong>&nbsp;\u5168\u6587\u901f\u89c8<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u9ad8\u6c27\u5206\u538b\u5de5\u51b5\u4e2d\uff0c\u4eba\u5de5\u5149\u5408CO<sub>2<\/sub>\u70c3\u5316\u8fc7\u7a0b\u53d7\u6c27\u949d\u5316\u81f4\u50ac\u5316\u5242\u5931\u6d3b\u4e0eC<sub>2<\/sub>\u5076\u8054\u57fa\u5143\u6b65\u901f\u7387\u63a7\u5236\u7684\u53cc\u91cd\u675f\u7f1a\u3002\u672c\u7814\u7a76\u91c7\u7528\u6c27\u4ecb\u5bfc\u7684\u52a8\u6001\u754c\u9762\u91cd\u6784\u7b56\u7565\uff0c\u6210\u529f\u6784\u7b51\u5177\u6709\u81ea\u9002\u5e94\u8010\u6c27\u7279\u6027\u7684Ru<sub>0.6<\/sub>Cu<sub>1<\/sub>(Cu<sup>0<\/sup>\u2013Cu<sup>1+<\/sup>)\/CeO<sub>2<\/sub>\u50ac\u5316\u5242\u3002\u5176\u6838\u5fc3\u521b\u65b0\u5728\u4e8e\u5c06\u5355\u539f\u5b50Ru\u7cbe\u51c6\u951a\u5b9a\u4e8eCeO<sub>2<\/sub>\u6676\u683c\u4f4d\u70b9\uff0c\u5f62\u6210\u72ec\u7279\u7684\u4e09\u89d2\u68f1\u67f1\u914d\u4f4d\u6784\u578b\uff0c\u6709\u6548\u4fc3\u8fdb\u8d28\u5b50\u8026\u5408\u7535\u5b50\u8f6c\u79fb\u8fc7\u7a0b\uff0c\u4ece\u800c\u663e\u8457\u52a0\u901fH<sub>2<\/sub>O\u89e3\u79bb\u52a8\u529b\u5b66\u6548\u7387\u3002\u6b64\u5916\uff0c\u5f3a\u5149\u70ed\u8026\u5408\u6548\u5e94\u9a71\u52a8O<sub>2<\/sub>\u5728Ru\/Cu\u5408\u91d1\u7c07\u5185\u90e8\u8bf1\u53d1Cu<sup>0<\/sup>\u2013Cu<sup>+<\/sup>\u7535\u8377\u68af\u5ea6\u754c\u9762\u7684\u52a8\u6001\u81ea\u7ec4\u88c5\u3002\u8fd9\u79cd\u81ea\u9002\u5e94\u754c\u9762\u4e0d\u4ec5\u4f18\u5316\u5173\u952e\u4e2d\u95f4\u4f53<sup>*<\/sup>CHOCO\u7684\u5438\u9644\u884c\u4e3a\uff0c\u66f4\u91cd\u6784\u4e86C\u2013C\u5076\u8054\u8def\u5f84\u3002\u501f\u52a9\u539f\u4f4d\u5149\u8c31\u4e0e\u7535\u5b50\u7ed3\u6784\u5206\u6790\u8bc1\u5b9e\u754c\u9762\u7535\u8377\u7684\u7ea7\u8054\u8f6c\u79fb\u4e0e\u51e0\u4f55\u4f4d\u70b9\u7684\u534f\u540c\u4f5c\u7528\uff0c\u4ece\u70ed\u529b\u5b66\u4e0a\u5b9e\u73b0\u4e86\u4ea7\u7269\u9009\u62e9\u6027\u7531C<sub>1<\/sub>\u5411C<sub>2<\/sub>\u5316\u5408\u7269\u7684\u6839\u672c\u6027\u8f6c\u53d8\u3002\u5728\u805a\u96c6\u592a\u9633\u80fd\u8f90\u7167\u4e0b\uff0c\u8be5\u50ac\u5316\u5242\u5c55\u73b0\u51fa\u4f18\u5f02\u6027\u80fd\uff1aC<sub>2<\/sub>H<sub>4<\/sub>\u4ea7\u7387\u9ad8\u8fbe549 \u00b1 20 \u03bcmol\u00b7g<sup>\u20131<\/sup>\uff0c\u9009\u62e9\u6027\u8fbe74.3%\uff0c\u592a\u9633\u80fd\u81f3\u5316\u5b66\u80fd\uff08STC\uff09\u8f6c\u5316\u6548\u7387\u8fbe0.5%\u3002\u8be5\u7814\u7a76\u63ed\u793a\u7684\u52a8\u6001\u754c\u9762\u8c03\u63a7\u673a\u5236\uff0c\u4e3a\u5b9e\u73b0\u590d\u6742\u53cd\u5e94\u7f51\u7edc\u4e2d\u7cbe\u51c6\u7684\u78b3\u94fe\u5b9a\u5411\u5408\u6210\u63d0\u4f9b\u65b0\u601d\u8def\u3002<\/p>\n\n\n\n<p><strong>2\ufe0f<\/strong><strong>\u20e3<\/strong><strong>&nbsp;\u80cc\u666f\u4ecb\u7ecd<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u5bcc\u6c27\u73af\u5883\u4e2d\u9ad8\u6548\u78b3\u8f6c\u5316\u4f5c\u4e3a\u4eba\u5de5\u5149\u5408\u4f5c\u7528\u5b9e\u9645\u5e94\u7528\u7684\u6838\u5fc3\u74f6\u9888\uff0c\u5176\u672c\u8d28\u5728\u4e8e\u592a\u9633\u80fd\u81f3\u5316\u5b66\u80fd\u8f6c\u6362\u7684\u7ea7\u8054\u80fd\u91cf\u8017\u635f\u3002\u5f53\u524d\u4e3b\u6d41\u7684\u805a\u5149\u7b56\u7565\u867d\u501f\u52a9\u77ac\u6001\u9ad8\u6e29\u4e0e\u9ad8\u5149\u5b50\u901a\u91cf\u63d0\u5347\u80fd\u91cf\u6548\u7387\uff0c\u5374\u56e0\u6025\u5267\u52a0\u901f\u6c34\u88c2\u89e3\u800c\u5bfc\u81f4\u526f\u4ea7\u7269O<sub>2<\/sub>\u7206\u53d1\u5f0f\u79ef\u7d2f\u4e0e\u6c27\u5206\u538b\u5feb\u901f\u6500\u5347\uff0c\u5f62\u6210\u201c\u5149\u5f3a\u589e\u5f3a&nbsp;\u2194&nbsp;\u73af\u5883\u6c27\u6bd2\u5316\u201d\u7684\u8d1f\u53cd\u9988\u8026\u5408\u5faa\u73af\u3002\u8be5\u8fc7\u7a0b\u901a\u8fc7\u70ed\u529b\u5b66\uff08\u6025\u5267\u589e\u5f3a\u7684\u6c27\u8fd8\u539f\u53cd\u5e94\u7ade\u4e89\u5173\u952e\u7535\u5b50\uff09\u4e0e\u52a8\u529b\u5b66\uff08\u50ac\u5316\u5242\u8868\u9762O<sub>2<\/sub>\u5438\u9644\u9971\u548c\u963b\u788dCO<sub>2<\/sub>\u5316\u5b66\u5438\u9644\uff09\u53cc\u91cd\u8def\u5f84\uff0c\u4e25\u91cd\u6291\u5236CO<sub>2<\/sub>\u8fd8\u539f\u53cd\u5e94\uff0c\u81f4\u4f7f\u5bcc\u6c27\u78b3\u8f6c\u5316\u6548\u7387\u8fdc\u4f4e\u4e8e\u538c\u6c27\u73af\u5883\uff08\u9aa4\u964d2\u4e2a\u6570\u91cf\u7ea7\u4ee5\u4e0a\uff09\u3002\u4f20\u7edf\u88ab\u52a8\u201c\u6297\u6c27\u201d\u7b56\u7565\u5728\u5267\u70c8\u53d8\u52a8\u7684\u7cfb\u7edf\u6c27\u5206\u538b\u4e0b\u5df2\u7136\u5931\u6548\u3002\u7a81\u7834\u684e\u688f\u4e9f\u9700\u6784\u7b51\u672c\u5f81\u8010\u6c27\u4e14\u80fd\u4e3b\u52a8\u5229\u7528O<sub>2<\/sub>\u89e6\u53d1\u754c\u9762\u91cd\u6784\u7684\u52a8\u6001\u50ac\u5316\u4f53\u7cfb\uff0c\u4ee5\u5b9e\u73b0C=O\u952e\u6d3b\u5316\u4e0e\u5438\u9644\u7ade\u4e89\u7684\u65f6\u7a7a\u89e3\u8026\u3002\u57fa\u4e8e\u6b64\uff0c\u672c\u7814\u7a76\u521b\u65b0\u6027\u63d0\u51fa\u201cO\u2082\u4ecb\u5bfc\u52a8\u6001\u754c\u9762\u91cd\u6784\u201d\u673a\u5236\uff0c\u8bbe\u8ba1\u5e76\u6784\u7b51Ru<sub>0.6<\/sub>Cu<sub>1<\/sub>(Cu<sup>0<\/sup>\u2013Cu<sup>1+<\/sup>)\/CeO<sub>2<\/sub>\u50ac\u5316\u5242\u3002\u5b9e\u9a8c\u7ed3\u679c\u53d6\u5f97\u7a81\u7834\uff1a\u5728\u5bcc\u6c27\u6761\u4ef6\u4e0b\uff0c\u5c06\u4e59\u70ef\u9009\u62e9\u6027\u4ece\u57fa\u51c6\u76840%\u5927\u5e45\u63d0\u5347\u81f374.3%\u3002\u8be5\u7814\u7a76\u4e3a\u89e3\u51b3\u5bcc\u6c27\u73af\u5883\u4e2d\u9ad8\u6548\u78b3\u94fe\u7cbe\u51c6\u5408\u6210\u96be\u9898\u63d0\u4f9b\u52a8\u6001\u50ac\u5316\u754c\u9762\u8bbe\u8ba1\u65b9\u6cd5\u3002<\/p>\n\n\n\n<p><strong>3\ufe0f<\/strong><strong>\u20e3<\/strong><strong>\u672c\u6587\u4eae\u70b9<\/strong><strong><\/strong><\/p>\n\n\n\n<p>1. <strong>\u7a81\u7834\u4f20\u7edf\u8010\u6c27\u684e\u688f\uff1a\u539f\u521b\u201c\u6c27\u4ecb\u5bfc-\u52a8\u6001\u754c\u9762\u91cd\u6784\u201d\u7b56\u7565<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u6210\u529f\u6784\u7b51\u8010\u6c27\u81ea\u9002\u5e94\u50ac\u5316\u5242Ru<sub>0.6<\/sub>Cu<sub>1<\/sub>(Cu<sup>0<\/sup>\u2013Cu<sup>1+<\/sup>)\/CeO<sub>2\uff0c<\/sub>\u5de7\u5999\u5229\u7528\u9ad8\u6c27\u5206\u538b\u73af\u5883\u8bf1\u5bfc\u5f62\u6210Cu<sup>0<\/sup>\u2013Cu<sup>+<\/sup>\u7535\u8377\u68af\u5ea6\u754c\u9762\uff0c\u7834\u9664\u50ac\u5316\u5931\u6d3b\u4e0eC<sub>2<\/sub>\u8026\u5408\u901f\u7387\u9650\u5236\u7684\u53cc\u91cd\u67b7\u9501\u3002<\/p>\n\n\n\n<p>2. <strong>\u4f18\u5f02\u6027\u80fd<\/strong><strong>\uff1a\u592a\u9633\u80fd\u9a71\u52a8\u9ad8\u9009\u62e9\u6027C<\/strong><strong><sub><strong><sub>2<\/sub><\/strong><\/sub><\/strong><strong>H<\/strong><strong><sub><strong><sub>4<\/sub><\/strong><\/sub><\/strong><strong>\u5408\u6210<\/strong><\/p>\n\n\n\n<p>\u805a\u5149\u8f90\u7167\u6761\u4ef6\u4e0b\u5b9e\u73b0C<sub>2<\/sub>H<sub>4<\/sub>\u4ea7\u7387549 \u00b1 20 \u03bcmol\u00b7g<sup>\u20131<\/sup>\u3001\u9009\u62e9\u602774.3%\uff0cSTC\u8f6c\u5316\u6548\u73870.5%\uff08\u8f83\u975e\u805a\u96c6\u592a\u9633\u80fd\u8f90\u7167\u6761\u4ef6\u63d0\u534725\u500d\uff09\uff0c\u4e3a\u4eba\u5de5\u5149\u5408CO<sub>2<\/sub>\u70c3\u5316\u53d6\u5f97\u91cd\u8981\u8fdb\u5c55\u3002<\/p>\n\n\n\n<p>3.<strong>&nbsp;<\/strong><strong>\u673a\u5236\u6df1\u5ea6\u89e3\u6790\uff1a\u5149\u70ed<\/strong><strong>\u6548\u5e94<\/strong><strong>\u8026\u5408-\u754c\u9762\u7535\u8377\u534f\u540c\u9a71\u52a8\u78b3\u94fe\u589e\u957f<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u9996\u63ed\u201c\u5f3a\u5149\u70ed\u8026\u5408\u6548\u5e94 \u2192&nbsp;O<sub>2<\/sub>\u5bcc\u96c6&nbsp;\u2192&nbsp;\u52a8\u6001\u754c\u9762\u91cd\u6784\u201d\u7684\u7ea7\u8054\u6548\u5e94\uff0c\u901a\u8fc7\u7406\u8bba\u8ba1\u7b97\u548c\u539f\u4f4d\u5149\u8c31\u8bc1\u5b9e\u754c\u9762\u7535\u8377\u7ea7\u8054\u8f6c\u79fb\u4e0e\u51e0\u4f55\u4f4d\u70b9\u534f\u540c\u4f5c\u7528\uff0c\u70ed\u529b\u5b66\u5b9e\u73b0C<sub>1 <\/sub>\u2192&nbsp;C<sub>2<\/sub>\u4ea7\u7269\u6839\u672c\u6027\u8de8\u8d8a\uff0c\u5f00\u8f9f\u78b3\u94fe\u5b9a\u5411\u5408\u6210\u65b0\u9014\u5f84\u3002<\/p>\n\n\n\n<p><strong>4\ufe0f<\/strong><strong>\u20e3<\/strong><strong>&nbsp;\u56fe\u6587\u89e3\u6790<\/strong><strong><\/strong><\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"700\" height=\"416\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/12\/ce6e2814f207c93-25.png\" alt=\"\" class=\"wp-image-270062\"\/><\/figure>\n\n\n\n<p><strong>Fig. 1 | <\/strong><strong>Mechanistic evolution <\/strong><strong>in<\/strong><strong>&nbsp;<\/strong><strong>multiscale<\/strong><strong>&nbsp;metal<\/strong><strong>-site <\/strong><strong>catalysis<\/strong><strong>.<\/strong><strong><\/strong><\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"550\" height=\"540\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/12\/7f88dbbcaa77a1d-24.png\" alt=\"\" class=\"wp-image-270063\"\/><\/figure>\n\n\n\n<p><strong>Fig. <\/strong><strong>2<\/strong><strong>&nbsp;| <\/strong><strong>Structural and electronic characterization<\/strong><strong>&nbsp;of<\/strong><strong>&nbsp;<\/strong><strong>Ru<\/strong><strong><sub><strong><sub>0.6<\/sub><\/strong><\/sub><\/strong><strong>Cu<\/strong><strong><sub><strong><sub>1<\/sub><\/strong><\/sub><\/strong><strong>\/CeO<\/strong><strong><sub><strong><sub>2<\/sub><\/strong><\/sub><\/strong><strong>.<\/strong><\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"422\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/12\/4e9a0ba2491dfde-22.png\" alt=\"\" class=\"wp-image-270064\"\/><\/figure>\n\n\n\n<p><strong>Fig. 3 | O<\/strong><strong><sub><strong><sub>2<\/sub><\/strong><\/sub><\/strong><strong>-mediated photothermal catalytic CO<\/strong><strong><sub><strong><sub>2<\/sub><\/strong><\/sub><\/strong><strong>&nbsp;reduction performance.<\/strong><\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"455\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/12\/b14210e1ee30421-20.png\" alt=\"\" class=\"wp-image-270065\"\/><\/figure>\n\n\n\n<p><strong>Fig. 4 | Active site<\/strong><strong>s<\/strong><strong>&nbsp;verification and operando characterization of C<\/strong><strong><sub><strong><sub>2<\/sub><\/strong><\/sub><\/strong><strong>H<\/strong><strong><sub><strong><sub>4<\/sub><\/strong><\/sub><\/strong><strong>-formation intermediates.<\/strong><\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"574\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/12\/de5bcf7d8eaea98-13.png\" alt=\"\" class=\"wp-image-270066\"\/><\/figure>\n\n\n\n<p><strong>Fig. <\/strong><strong>5<\/strong><strong>&nbsp;| Theoretical calculation.<\/strong><strong><\/strong><\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"800\" height=\"203\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/12\/aa3023e0288002c-10.png\" alt=\"\" class=\"wp-image-270067\"\/><\/figure>\n\n\n\n<p><strong>Fig. <\/strong><strong>6<\/strong><strong>&nbsp;|<\/strong><strong>&nbsp;<\/strong><strong>CO<\/strong><strong><sub><strong><sub>2<\/sub><\/strong><\/sub><\/strong><strong>&nbsp;reduction mechanism<\/strong><strong>.<\/strong><\/p>\n\n\n\n<p><strong>5\ufe0f<\/strong><strong>\u20e3<\/strong><strong>&nbsp;\u603b\u7ed3\u4e0e\u5c55\u671b<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u672c\u7814\u7a76\u7ed3\u5408\u591a\u5c3a\u5ea6\u7406\u8bba\u5efa\u6a21\u4e0e\u5b9e\u9a8c\u5206\u6790\uff0c\u63ed\u793a\u5149\u70ed\u8026\u5408\u6548\u5e94\u5bf9\u91d1\u5c5e\u6d3b\u6027\u4f4d\u70b9\u52a8\u6001\u91cd\u6784\u7684\u9a71\u52a8\u673a\u5236\u3002\u7814\u7a76\u53d1\u73b0\uff0c\u5355\u539f\u5b50Ru\u53d6\u4ee3Ce\u6676\u683c\u5f62\u6210\u626d\u66f2\u4e09\u89d2\u68f1\u67f1\u914d\u4f4d\u7ed3\u6784\uff0c\u663e\u8457\u4fc3\u8fdb\u8d28\u5b50\u8026\u5408\u7535\u5b50\u8f6c\u79fb\u8fc7\u7a0b\uff0c\u8fdb\u800c\u52a0\u901fH<sub>2<\/sub>O\u89e3\u79bb\u3002\u50ac\u5316\u8fc7\u7a0b\u4e2d\uff0c\u539f\u4f4d\u4ea7\u751f\u7684O<sub>2<\/sub>\u6709\u6548\u8bf1\u5bfc\u5177\u5907\u7535\u8377\u68af\u5ea6\u7684Cu<sup>0<\/sup>\u2013Cu<sup>+<\/sup>\u754c\u9762\u5f62\u6210\u3002\u8fd9\u79cd\u5f3a\u5149\u70ed\u8026\u5408\u6548\u5e94\u9a71\u52a8\u7684\u52a8\u6001\u81ea\u7ec4\u88c5\u4f4d\u70b9\u4e0d\u4ec5\u4f18\u5316\u5bf9\u5173\u952e\u4e2d\u95f4\u4f53<sup>*<\/sup>CHOCO\u7684\u5438\u9644\u884c\u4e3a\uff0c\u8fd8\u91cd\u6784C\u2013C\u5076\u8054\u8def\u5f84\u3002\u901a\u8fc7\u539f\u4f4d\u5149\u8c31\u4e0e\u7535\u5b50\u7ed3\u6784\u5206\u6790\u8bc1\u5b9e\uff0c\u7535\u8377\u68af\u5ea6\u754c\u9762\u4e0e\u51e0\u4f55\u4f4d\u70b9\u7684\u534f\u540c\u4f5c\u7528\u662f\u5b9e\u73b0C<sub>2<\/sub>\u4ea7\u7269\u9ad8\u6548\u9009\u62e9\u6027\u7684\u5173\u952e\u3002\u57fa\u4e8e\u6b64\u673a\u7406\u8bbe\u8ba1\u7684Ru<sub>0.6<\/sub>Cu<sub>1<\/sub>(Cu<sup>0<\/sup>\u2013Cu<sup>1+<\/sup>)\/CeO<sub>2<\/sub>\u50ac\u5316\u5242\uff0c\u5728\u805a\u96c6\u592a\u9633\u80fd\u8f90\u7167\u4e0b\u5b9e\u73b0\u4e86549&nbsp;\u00b1&nbsp;20 \u03bcmol\u00b7g<sup>\u20131<\/sup>\u7684C<sub>2<\/sub>H<sub>4<\/sub>\u9ad8\u9009\u62e9\u6027\u751f\u6210\uff0874.3%\uff09\uff0c\u5176\u592a\u9633\u80fd\u81f3\u5316\u5b66\u80fd\u8f6c\u5316\u6548\u7387\uff080.5%\uff09\u76f8\u6bd4\u975e\u805a\u96c6\u592a\u9633\u80fd\u6761\u4ef6\u663e\u8457\u63d0\u534725\u500d\u3002\u8be5\u7814\u7a76\u6df1\u523b\u9610\u660e\u4e86\u5f3a\u5149\u70ed\u8026\u5408\u6548\u5e94\u8bf1\u5bfcO<sub>2<\/sub>\u79ef\u7d2f\u3001\u8fdb\u800c\u4ecb\u5bfc\u7535\u8377\u68af\u5ea6\u754c\u9762\u539f\u4f4d\u5f62\u6210\u7684\u673a\u5236\uff0c\u4e3a\u89e3\u51b3\u50ac\u5316\u78b3\u94fe\u589e\u957f\u4e2d\u6d3b\u6027-\u9009\u62e9\u6027-\u7a33\u5b9a\u6027\u76f8\u4e92\u63a3\u8098\u7684\u4e09\u91cd\u56f0\u5883\u63d0\u4f9b\u4e86\u65b0\u7b56\u7565\u3002<\/p>\n\n\n\n<p><strong>6\ufe0f<\/strong><strong>\u20e3<\/strong><strong>&nbsp;\u6587\u732e\u4fe1\u606f<\/strong><strong><\/strong><\/p>\n\n\n\n<p>Oxygen-modulated engineering of Cu<sup>0<\/sup>\u2013Cu<sup>+<\/sup>&nbsp;interfaces for CO<sub>2<\/sub>-to-C<sub>2<\/sub>H<sub>4<\/sub>&nbsp;photoreduction.&nbsp;<em>Nature Communications.<\/em>&nbsp;2025<\/p>\n\n\n\n<p>DOI\uff1ahttps:\/\/doi.org\/10.1038\/s41467-025-67844-9<\/p>\n\n\n\n<p><strong>7\ufe0f<\/strong><strong>\u20e3<\/strong><strong>\u4f5c\u8005\u4ecb\u7ecd<\/strong><strong><\/strong><\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"149\" height=\"209\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/12\/e2f457ec632c1f6-7.png\" alt=\"\" class=\"wp-image-270068\"\/><\/figure>\n\n\n\n<p>\u4efb\u5b87\u5947\uff0c\u73b0\u4e3a\u4e1c\u5357\u5927\u5b66\u5316\u5b66\u5316\u5de5\u5b66\u9662\u535a\u58eb\u7814\u7a76\u751f\uff0c\u7814\u7a76\u65b9\u5411\u4e3aCO<sub>2<\/sub>\u8d44\u6e90\u5316\u8f6c\u5316\u4e0e\u5229\u7528\u3002\u4ee5\u7b2c\u4e00\u4f5c\u8005\u53ca\u5171\u540c\u7b2c\u4e00\u4f5c\u8005\u8eab\u4efd\u5728Nature Communications (2\u7bc7), Angewandte Chemie International Edition\uff0cACS Nano\uff0cACS Catalysis (2\u7bc7). \u7b49SCI\u6536\u5f55\u520a\u7269\u4e0a\u53d1\u8868\u7814\u7a76\u8bba\u658715\u7bc7\uff0c\u7d2f\u8ba1\u53d1\u886818\u7bc7\u3002\u4e3b\u63012025\u548c2026\u5e74\u5ea6\u4e1c\u5357\u5927\u5b66\u535a\u58eb\u7814\u7a76\u751f\u521b\u65b0\u80fd\u529b\u63d0\u5347\u8ba1\u5212\uff0c\u5e76\u6210\u529f\u5165\u9009\u9996\u5c4a\u4e2d\u56fd\u79d1\u534f\u9752\u5e74\u79d1\u6280\u4eba\u624d\u57f9\u80b2\u5de5\u7a0b\u535a\u58eb\u751f\u4e13\u9879\u8ba1\u5212\uff08\u4e2d\u56fd\u80fd\u6e90\u7814\u7a76\u4f1a\uff09\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"228\" height=\"280\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/12\/bf2e94a56e16c6a-4.png\" alt=\"\" class=\"wp-image-270069\"\/><\/figure>\n\n\n\n<p>\u7a0b\u6dfc\uff0c\u73b0\u4e3a\u4e1c\u5357\u5927\u5b66\u5316\u5b66\u5316\u5de5\u5b66\u9662\u535a\u58eb\u7814\u7a76\u751f\uff0c\u7814\u7a76\u65b9\u5411\u4e3a\u57fa\u4e8e\u7b2c\u4e00\u6027\u539f\u7406\u8ba1\u7b97\u6a21\u62df\u8bbe\u8ba1\u7528\u4e8e\u5149\/\u7535\u50ac\u5316\u6c34\u5206\u89e3\u3001\u4e8c\u6c27\u5316\u78b3\u8fd8\u539f\u53ca\u751f\u7269\u8d28\u8f6c\u5316\u7684\u65b0\u578b\u9ad8\u6548\u50ac\u5316\u5242\u3002\u4ee5\u7b2c\u4e00\u4f5c\u8005\u53ca\u5171\u540c\u7b2c\u4e00\u4f5c\u8005\u8eab\u4efd\u5728Journal of the American Chemical Society\u3001Journal of Materials Chemistry A\u3001Applied Catalysis B: Environment and Energy\u3001Nano Letters. \u7b49SCI\u6536\u5f55\u520a\u7269\u4e0a\u53d1\u8868\u7814\u7a76\u8bba\u658710\u7bc7\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"149\" height=\"209\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/12\/bafe803af52db04-2.png\" alt=\"\" class=\"wp-image-270070\"\/><\/figure>\n\n\n\n<p>\u8d3a\u7ea2\u658c\uff0c\u73b0\u4e3a\u4e1c\u5357\u5927\u5b66\u5316\u5b66\u5316\u5de5\u5b66\u9662\u535a\u58eb\u7814\u7a76\u751f\uff0c\u7814\u7a76\u65b9\u5411\u4e3a\u8fde\u7eed\u6d41\u975e\u5747\u76f8\u50ac\u5316CO<sub>2<\/sub>\u8d44\u6e90\u5316\u8f6c\u5316\u4e0e\u5229\u7528\u3002\u5728ACS Catalysis, Applied Catalysis B: Environment and Energy, Nano energy, Small. \u7b49SCI\u6536\u5f55\u520a\u7269\u4e0a\u53d1\u8868\u7814\u7a76\u8bba\u658716\u7bc7\uff0c\u7533\u8bf7\/\u6388\u6743\u56fd\u5bb6\u4e13\u52299\u9879\u3002\u66fe\u83b7\u5b9d\u94a2\u4f18\u79c0\u5b66\u751f\u5956\u3001\u7814\u7a76\u751f\u56fd\u5bb6\u5956\u5b66\u91d1\u7b49\u8363\u8a89\uff0c\u5728\u7b2c\u4e5d\u5c4a\u4e2d\u56fd\u7814\u7a76\u751f\u80fd\u6e90\u88c5\u5907\u521b\u65b0\u8bbe\u8ba1\u5927\u8d5b\u7b49\u5b66\u79d1\u7ade\u8d5b\u4e2d\u4ee5\u7b2c\u4e00\u5b8c\u6210\u4eba\u83b7\u5f97\u56fd\u5bb6\u7ea7\u5956\u52b15\u9879\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"218\" height=\"302\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2025\/12\/024a2b0801cb335-1.png\" alt=\"\" class=\"wp-image-270071\"\/><\/figure>\n\n\n\n<p>\u674e\u4e43\u65ed\u73b0\u4e3a\u4e1c\u5357\u5927\u5b66\u5316\u5b66\u5316\u5de5\u5b66\u9662\u6559\u6388\uff0c\u535a\/\u7855\u5bfc\u30022003\u5e74~2014\u5e74\u4e8e\u4e1c\u5357\u5927\u5b66\u5206\u522b\u5b8c\u6210\u672c\u79d1\u3001\u7855\u58eb\u548c\u535a\u58eb\u7684\u5b66\u4e60\u548c\u7814\u7a76\u9636\u6bb5\uff1b\u671f\u95f42011\u5e74~2013\u5e74\u5728\u56fd\u5bb6\u7559\u5b66\u57fa\u91d1\u59d4\u7684\u652f\u6301\u4e0b\uff0c\u4e8e\u7f8e\u56fd\u4f50\u6cbb\u4e9a\u7406\u5de5\u5b66\u9662\u8fdb\u884c\u8054\u5408\u57f9\u517b\uff0c\u5bfc\u5e08\u4e3aYounan Xia\u548cKrista Walton\u6559\u6388\u3002\u5165\u9009\u6c5f\u82cf\u7701\u201c333\u9ad8\u5c42\u6b21\u4eba\u624d\u57f9\u517b\u5de5\u7a0b\u201d\u4e2d\u9752\u5e74\u5b66\u672f\u6280\u672f\u5e26\u5934\u4eba\u3001\u5510\u4ef2\u82f1\u57fa\u91d1\u4f1a\u201c\u4ef2\u82f1\u9752\u5e74\u5b66\u8005\u201d\u3001\u6c5f\u82cf\u7701\u201c\u53cc\u521b\u8ba1\u5212\u201d\u79d1\u6280\u526f\u603b\u9879\u76ee\u3001\u5357\u4eac\u9ad8\u5c42\u6b21\u521b\u4e1a\u4eba\u624d\u5f15\u8fdb\u8ba1\u5212\u3002\u4e3b\u6301\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u3001\u6c5f\u82cf\u7701\u6559\u6539\u9879\u76ee\/\u6c5f\u82cf\u7701\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u3001\u4f01\u4e1a\u6a2a\u5411\u7b49\u9879\u76ee\u3002\u4ee5\u7b2c\u4e00\u6216\u901a\u8baf\u4f5c\u8005\u5728Nature Communications, Journal of the American Chemical Society, Angewandte Chemie International Edition, ACS Nano, ACS Catalysis, Science Bulletin, Advanced Functional Materials, Nano Energy, AIChE Journal.\u7b49\u5b66\u672f\u671f\u520a\u53d1\u8868\u7814\u7a76\u8bba\u6587100\u4f59\u7bc7\uff1b\u7533\u8bf7\u56fd\u5bb6\u53d1\u660e\u4e13\u522969\u4ef6\uff0c\u6388\u674340\u4ef6\u3002<\/p>\n\n\n\n<p>\u8bfe\u9898\u7ec4\u5b98\u7f51\uff1ahttps:\/\/www.x-mol.com\/groups\/linaixu191.<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u7b2c\u4e00\u4f5c\u8005\uff1a\u4efb\u5b87\u5947\uff0c\u7a0b\u6dfc\uff0c\u8d3a\u7ea2\u658c \u901a\u8baf\u4f5c\u8005\uff1a\u674e\u4e43\u65ed \u901a\u8baf\u5355\u4f4d\uff1a\u4e1c\u5357\u5927\u5b66 \u8bba\u6587DOI\uff1a10.1038\/s41467-025-67844-9 1\ufe0f\u20e3&nbsp;\u5168\u6587\u901f&#8230;<\/p>\n","protected":false},"author":31345,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-270060","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/270060"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/31345"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=270060"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/270060\/revisions"}],"predecessor-version":[{"id":270072,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/270060\/revisions\/270072"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=270060"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=270060"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=270060"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}