{"id":270249,"date":"2026-01-11T08:39:00","date_gmt":"2026-01-11T00:39:00","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=270249"},"modified":"2026-01-10T22:44:39","modified_gmt":"2026-01-10T14:44:39","slug":"%e4%b8%ad%e5%9b%bd%e7%a7%91%e5%ad%a6%e9%99%a2%e5%b1%b1%e8%a5%bf%e7%85%a4%e5%8c%96%e6%89%80%e8%8b%8f%e6%96%b9%e8%bf%9c%e5%9b%a2%e9%98%9f%e3%80%8aelectrochimica-acta%e3%80%8b%ef%bc%9a%e9%92%a0","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=270249","title":{"rendered":"\u4e2d\u56fd\u79d1\u5b66\u9662\u5c71\u897f\u7164\u5316\u6240\u82cf\u65b9\u8fdc\u56e2\u961f\u300aElectrochimica\u00a0Acta\u300b\uff1a\u94a0\u7535\u786c\u70ad\u8d1f\u6781\u5728\u916f\u7c7b\u548c\u919a\u7c7b\u7535\u89e3\u6db2\u4e2d\u500d\u7387\u6027\u80fd\u5dee\u5f02\u7684\u5f71\u54cd\u56e0\u7d20"},"content":{"rendered":"\n<p><strong>\u3010\u6587\u7ae0\u4fe1\u606f\u3011<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u6587\u7ae0\u6807\u9898\uff1aUncovering Electrochemical Performance in Ester and Ether Electrolytes in Sodium-ion Batteries from Interfacial Perspective of Hard Carbon Anodes<\/p>\n\n\n\n<p>\u7b2c\u4e00\u4f5c\u8005\uff1a\u6d2a\u707f\u707f<\/p>\n\n\n\n<p>\u901a\u8baf\u4f5c\u8005\uff1a\u9648\u666f\u9e4f\uff0c\u82cf\u65b9\u8fdc<\/p>\n\n\n\n<p>\u5355\u4f4d\uff1a\u4e2d\u56fd\u79d1\u5b66\u9662\u5c71\u897f\u7164\u70ad\u5316\u5b66\u7814\u7a76\u6240<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"500\" height=\"267\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/01\/2382c315a6ba396-6.png\" alt=\"\" class=\"wp-image-270250\"\/><\/figure>\n\n\n\n<p><strong>\u3010\u7814\u7a76\u80cc\u666f\u3011<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u76ee\u524d\uff0c\u94a0\u79bb\u5b50\u7535\u6c60\u4e3b\u8981\u91c7\u7528\u916f\u7c7b\u4e0e\u919a\u7c7b\u4e24\u7c7b\u6709\u673a\u7535\u89e3\u6db2\u3002\u916f\u7c7b\u7535\u89e3\u6db2\u56e0\u5176\u6210\u672c\u8f83\u4f4e\u3001\u4e0e\u9ad8\u538b\u6b63\u6781\u6750\u6599\u517c\u5bb9\u6027\u4f18\u5f02\u7b49\u4f18\u52bf\uff0c\u88ab\u5e7f\u6cdb\u7528\u4e8e\u5546\u4e1a\u5316\u94a0\u79bb\u5b50\u7535\u6c60\u3002\u919a\u7c7b\u7535\u89e3\u6db2\u867d\u7136\u8010\u9ad8\u7535\u538b\u6027\u5dee\uff0c\u4f46\u5f80\u5f80\u80fd\u8868\u73b0\u51fa\u8f83\u4e3a\u4f18\u5f02\u7684\u52a8\u529b\u5b66\u884c\u4e3a\u548c\u5bb9\u91cf\u6027\u80fd\u3002\u76ee\u524d\u4ece\u70ad\u6750\u6599\u7ed3\u6784\u89d2\u5ea6\u601d\u8003\u786c\u70ad\u5728\u916f\u7c7b\u4e0e\u919a\u7c7b\u7535\u89e3\u6db2\u4ea7\u751f\u7535\u5316\u5b66\u6027\u80fd\u5dee\u5f02\u539f\u56e0\u7684\u5de5\u4f5c\u4ecd\u8f83\u4e3a\u7f3a\u4e4f\u3002<\/p>\n\n\n\n<p><strong>\u3010\u6587\u7ae0\u7b80\u4ecb\u3011<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u8fd1\u65e5\uff0c\u4e2d\u56fd\u79d1\u5b66\u9662\u5c71\u897f\u7164\u70ad\u5316\u5b66\u7814\u7a76\u6240\u82cf\u65b9\u8fdc\u7814\u7a76\u5458\u56e2\u961f\u5728\u300aElectrochimica&nbsp;Acta\u300b\u4e0a\u53d1\u8868\u7814\u7a76\u8bba\u6587\u3002\u8be5\u7814\u7a76\u4ece\u70ad\u6750\u6599\u7684\u89d2\u5ea6\u63ed\u793a\u4e86\u94a0\u79bb\u5b50\u7535\u6c60\u786c\u70ad\u8d1f\u6781\u5728\u916f\u7c7b\u548c\u919a\u7c7b\u7535\u89e3\u6db2\u4e2d\u7535\u5316\u5b66\u6027\u80fd\u5dee\u5f02\u7684\u539f\u56e0\u3002\u7814\u7a76\u53d1\u73b0\u786c\u70ad\u7684\u8868\u9762\u7f3a\u9677\u548c\u6709\u5e8f\u5ea6\u4f1a\u5bf9SEI\u819c\u7684\u751f\u957f\u4ea7\u751f\u91cd\u8981\u5f71\u54cd\uff0c\u4ece\u800c\u5f71\u54cd\u786c\u70ad\u5728\u4e0d\u540c\u7535\u89e3\u6db2\u4e2d\u7684\u884c\u4e3a\uff1a\u8868\u9762\u6709\u5e8f\u4e14\u7f3a\u9677\u8f83\u5c11\u7684\u6ca5\u9752\u884d\u751f\u786c\u70ad\u5728\u4e24\u79cd\u7535\u89e3\u6db2\u4e2d\u53ef\u5f62\u6210\u7ed3\u6784\u4e0e\u7ec4\u5206\u76f8\u4f3c\u7684SEI \u819c\uff0c\u7535\u5316\u5b66\u6027\u80fd\u5dee\u5f02\u8fdc\u5c0f\u4e8e\u8868\u9762\u7f3a\u9677\u8f83\u591a\u7684\u6930\u58f3\u548c\u6811\u8102\u884d\u751f\u7684\u786c\u70ad\u6750\u6599\u3002<\/p>\n\n\n\n<p><strong>\u3010\u672c\u6587\u8981\u70b9\u3011<\/strong><strong><\/strong><\/p>\n\n\n\n<p><strong>\u8981\u70b9\u4e00\uff1a\u9009\u53d6\u4e09\u79cd\u4e0d\u540c\u524d\u9a71\u4f53\u884d\u751f\u786c\u70ad\u6750\u6599\u63a2\u7a76\u5176<\/strong><strong>\u5728EC\/DEC\u548c<\/strong><strong>D<\/strong><strong>iglyme\u7535\u89e3\u6db2\u4e2d\u7535\u5316\u5b66\u6027\u80fd\u5dee\u5f02<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u9488\u5bf9\u8fd9\u4e00\u95ee\u9898\uff0c\u7814\u7a76\u56e2\u961f\u9009\u53d6\u4ee5\u6930\u58f3\u3001\u6811\u8102\u548c\u6ca5\u9752\u4e3a\u524d\u9a71\u4f53\u7684\u4e09\u79cd\u786c\u70ad\uff0c\u7cfb\u7edf\u8003\u5bdf\u4e86\u5728EC\/DEC\u548cDiglyme\u7535\u89e3\u6db2\u4e2d\u7535\u5316\u5b66\u6027\u80fd\u5dee\u5f02\u3002\u7814\u7a76\u63ed\u793a\uff0c\u6ca5\u9752\u884d\u751f\u786c\u70ad\u5728\u4e24\u79cd\u7535\u89e3\u6db2\u4e2d\u7535\u5316\u5b66\u6027\u80fd\u5dee\u5f02\u6700\u5c0f\uff0c\u6bd4\u5bb9\u91cf\u5dee\u503c\u548cICE\u5dee\u503c\u5206\u522b\u4e3a14.3 mAh g<sup>-1<\/sup>\u548c0.06 %\u3002\u6930\u58f3\u884d\u751f\u786c\u70ad\u5bf9\u5e94\u5dee\u503c\u4e3a16 mAh g<sup>-1<\/sup>\u548c2.95 %\uff0c\u6811\u8102\u884d\u751f\u786c\u70ad\u4e3a21.1 mAh g<sup>-1<\/sup>\u548c3.14 %\u3002100 mA g<sup>-1<\/sup>\u7535\u6d41\u5bc6\u5ea6\u4e0b\u6ca5\u9752\u884d\u751f\u786c\u70ad\u5728\u4e24\u79cd\u7535\u89e3\u6db2\u4e2d\u7684\u5bb9\u91cf\u5dee\u503c\u4e3a63.76 mAh g<sup>-1<\/sup>\uff0c\u6930\u58f3\u548c\u6811\u8102\u884d\u751f\u786c\u70ad\u7684\u5bb9\u91cf\u5dee\u503c\u5206\u522b\u4e3a82.49 mAh g<sup>-1<\/sup>\u548c113.37 mAh g<sup>-1<\/sup>\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"500\" height=\"293\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/01\/ce6e2814f207c93-6.png\" alt=\"\" class=\"wp-image-270251\"\/><\/figure>\n\n\n\n<p>\u56fe1 \u4e09\u79cd\u786c\u70ad\u5728EC\/DEC\u548cDiglyme\u7535\u89e3\u6db2\u4e2d\u7535\u5316\u5b66\u6027\u80fd\u5dee\u5f02<\/p>\n\n\n\n<p><strong>\u8981\u70b9\u4e8c\uff1a\u4ece\u754c\u9762\u89d2\u5ea6\u63a2\u7a76\u7535\u5316\u5b66\u6027\u80fd\u5dee\u5f02\u7684\u539f\u56e0<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u4e3a\u63a2\u7a76\u5dee\u5f02\u4e0d\u540c\u7684\u539f\u56e0\uff0c\u4e09\u79cd\u786c\u78b3\u5206\u522b\u505a\u4e86\u7535\u89e3\u6db2\u4ea4\u6362\u5b9e\u9a8c\u3002\u7ed3\u679c\u663e\u793a\u6ca5\u9752\u884d\u751f\u786c\u70ad\u5728EC\/DEC \u548cDiglyme\u7535\u89e3\u6db2\u4e2d\u7684\u500d\u7387\u6027\u80fd\u5dee\u5f02\u4e3b\u8981\u6765\u81ea\u4e8e\u8131\u6eb6\u5242\u5316\u8fc7\u7a0b\uff0c\u6930\u58f3\u884d\u751f\u786c\u70ad\u7684\u500d\u7387\u6027\u80fd\u5dee\u5f02\u4e3b\u8981\u6765\u81ea\u4e8eSEI\u819c\uff0c\u6811\u8102\u884d\u751f\u786c\u70ad\u5219\u53d7SEI\u819c\u548c\u8131\u6eb6\u5242\u8fc7\u7a0b\u5171\u540c\u5f71\u54cd\u3002\u8fdb\u4e00\u6b65\u7814\u7a76\u53d1\u73b0\uff0c\u6ca5\u9752\u884d\u751f\u786c\u70ad\u5728EC\/DEC\u548cDiglyme\u7535\u89e3\u6db2\u4e2d\u751f\u6210\u7684SEI\u819c\u539a\u5ea6\u548c\u7ec4\u5206\u5dee\u5f02\u6700\u5c0f\u3002\u4e3b\u8981\u8868\u73b0\u4e3a\u5728\u4e24\u79cd\u7535\u89e3\u6db2\u4e2d\u5f62\u6210\u7684SEI\u819c\u65e0\u673a\u7ec4\u5206\u548c\u6709\u673a\u7ec4\u5206\u5360\u6bd4\u66f4\u63a5\u8fd1\uff0c\u4e14SEI\u819c\u7684\u539a\u5ea6\u5dee\u5f02\u57282 nm\u4e4b\u5185\u3002\u6930\u58f3\u548c\u6811\u8102\u884d\u751f\u786c\u70ad\u5728EC\/DEC\u548cDiglyme\u7535\u89e3\u6db2\u4e2d\u751f\u6210\u7684SEI\u819c\u7ec4\u5206\u5dee\u5f02\u8f83\u5927\uff0c\u4e14SEI\u819c\u539a\u5ea6\u5dee\u5f02\u5747\u5927\u4e8e2 nm\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"500\" height=\"631\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/01\/7f88dbbcaa77a1d-6.png\" alt=\"\" class=\"wp-image-270252\"\/><\/figure>\n\n\n\n<p>\u56fe2 \u4e09\u79cd\u786c\u70ad\u7684\u7535\u89e3\u6db2\u4ea4\u6362\u5b9e\u9a8c<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"500\" height=\"447\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/01\/4e9a0ba2491dfde-6.png\" alt=\"\" class=\"wp-image-270253\"\/><\/figure>\n\n\n\n<p>\u56fe3 \u4e09\u79cd\u786c\u70ad\u5728EC\/DEC\u548cDiglyme\u7535\u89e3\u6db2\u4e2d\u5f62\u6210\u7684SEI\u819c<\/p>\n\n\n\n<p><strong>\u8981\u70b9\u4e09\uff1a\u4ece\u70ad\u6750\u6599\u89d2\u5ea6\u63a2\u7a76\u7535\u5316\u5b66\u6027\u80fd\u5dee\u5f02\u7684\u539f\u56e0<\/strong><strong><\/strong><\/p>\n\n\n\n<p>SEI\u819c\u7684\u751f\u957f\u8fc7\u7a0b\u5f80\u5f80\u53d7\u786c\u70ad\u8868\u9762\u7ed3\u6784\u7684\u5f71\u54cd\u3002XRD\u3001Raman\u3001TEM\u4e0eAFM\u7ed3\u679c\u90fd\u8868\u660e\u6ca5\u9752\u884d\u751f\u786c\u70ad\u8868\u9762\u7f3a\u9677\u6700\u5c11\u3001\u8868\u9762\u78b3\u5c42\u6392\u5217\u6700\u6709\u5e8f\uff0c\u6811\u8102\u884d\u751f\u786c\u70ad\u8868\u9762\u7c97\u7cd9\u5ea6\u6700\u9ad8\u3001\u8868\u9762\u6700\u65e0\u5e8f\u3002DFT\u8ba1\u7b97\u63ed\u793a\u6709\u5e8f\u7684\u786c\u70ad\u5bf9\u6eb6\u5242\u5206\u5b50\u7684\u5438\u9644\u80fd\u4f4e\u4e8e\u65e0\u5e8f\u7684\u786c\u70ad\uff0c\u8868\u660e\u6709\u5e8f\u7684\u8868\u9762\u80fd\u591f\u51cf\u5c11\u4e0e\u7535\u89e3\u6db2\u7684\u76f8\u4e92\u4f5c\u7528\uff0c\u4ece\u800c\u6700\u5927\u7a0b\u5ea6\u5730\u51cf\u5c11\u4e86\u526f\u53cd\u5e94\u7684\u53d1\u751f\u3002\u53e6\u5916\uff0c\u8868\u9762\u66f4\u6709\u5e8f\u7684\u786c\u70ad\u5bf9\u916f\u7c7b\u548c\u919a\u7c7b\u6eb6\u5242\u7684\u5438\u9644\u80fd\u66f4\u63a5\u8fd1\uff0c\u53ef\u8c03\u63a7\u4e24\u79cd\u7535\u89e3\u6db2\u4e2dSEI \u819c\u751f\u957f\u8d8b\u4e8e\u4e00\u81f4\uff0c\u8bc1\u660e\u6709\u5e8f\u7684\u8868\u9762\u7ed3\u6784\u80fd\u591f\u201c\u4e2d\u548c\u201d\u786c\u70ad\u4e0e\u916f\u7c7b\u548c\u919a\u7c7b\u7535\u89e3\u6db2\u4e4b\u95f4\u7684\u76f8\u4e92\u4f5c\u7528\u5dee\u5f02\u3002\u8bc1\u5b9e\u4e86\u786c\u70ad\u6709\u5e8f\u7684\u8868\u9762\u7ed3\u6784\u4f7f\u5f97\u5176\u5728EC\/DEC\u548cDiglyme\u7535\u89e3\u6db2\u4e2d\u5f62\u6210\u7ec4\u6210\u4e0e\u7ed3\u6784\u63a5\u8fd1\u7684SEI\u819c\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"500\" height=\"589\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/01\/b14210e1ee30421-5.png\" alt=\"\" class=\"wp-image-270254\"\/><\/figure>\n\n\n\n<p>\u56fe4 \u4e09\u79cd\u786c\u70ad\u7684\u8868\u9762\u7ed3\u6784<\/p>\n\n\n\n<p><strong>\u3010\u603b\u7ed3\u4e0e\u5c55\u671b\u3011<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u7efc\u4e0a\uff0c\u672c\u7814\u7a76\u63ed\u793a\u4e86\u8868\u9762\u6709\u5e8f\u4e14\u7f3a\u9677\u5c11\u7684\u94a0\u79bb\u5b50\u7535\u6c60\u786c\u70ad\u8d1f\u6781\u6750\u6599\u5728\u916f\u7c7b\u548c\u919a\u7c7b\u7535\u89e3\u6db2\u4e2d\u4f1a\u5f62\u6210\u7ed3\u6784\u7ec4\u5206\u76f8\u4f3c\u7684SEI\u819c\uff0c\u8fd9\u4f7f\u5f97\u754c\u9762\u53cd\u5e94\u8fc7\u7a0b\u4e3b\u8981\u53d7\u5230\u8131\u6eb6\u5242\u8fc7\u7a0b\u800c\u975eSEI\u819c\u6269\u6563\u7684\u5f71\u54cd\uff0c\u4ece\u800c\u964d\u4f4e\u786c\u70ad\u5728\u916f\u7c7b\u548c\u919a\u7c7b\u7535\u89e3\u6db2\u4e2d\u7535\u5316\u5b66\u6027\u80fd\u7684\u5dee\u5f02\u3002\u672c\u5de5\u4f5c\u9610\u660e\u4e86\u786c\u70ad\u5fae\u89c2\u7ed3\u6784\u5bf9\u5176\u5728\u916f\u7c7b\u548c\u919a\u7c7b\u7535\u89e3\u6db2\u4e2d\u7535\u5316\u5b66\u6027\u80fd\u5dee\u5f02\u7684\u5f71\u54cd\u673a\u7406\uff0c\u4e3a\u589e\u5f3a\u9ad8\u6027\u80fd\u94a0\u79bb\u5b50\u7535\u6c60\u786c\u70ad\u8d1f\u6781\u548c\u7535\u89e3\u6db2\u5339\u914d\u6027\u63d0\u4f9b\u4e86\u7406\u8bba\u6307\u5bfc\u3002<\/p>\n\n\n\n<p><strong>\u3010\u6587\u7ae0\u94fe\u63a5\u3011<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"https:\/\/doi.org\/10.1016\/j.electacta.2026.148113\"><u>https:\/\/doi.org\/10.1016\/j.electacta.2026.148113<\/u><\/a><\/p>\n\n\n\n<p><strong>\u3010\u901a\u8baf\u4f5c\u8005\u7b80\u4ecb\u3011<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u82cf\u65b9\u8fdc\uff0c\u535a\u58eb\uff0c\u7814\u7a76\u5458\uff0c\u535a\u58eb\u751f\u5bfc\u5e08\uff0c\u8bfe\u9898\u7ec4\u7ec4\u957f\u3002\u5165\u9009\u4e2d\u56fd\u79d1\u5b66\u9662\u9752\u4fc3\u4f1a\u4f1a\u5458\u3001\u4e2d\u56fd\u79d1\u5b66\u9662\u7279\u8058\u7814\u7a76\u5c97\u4f4d\u3001\u5c71\u897f\u7701\u201c\u4e09\u664b\u82f1\u624d\u201d\u4f18\u79c0\u9752\u5e74\u4eba\u624d\u3001IEC TC113\u5de5\u4f5c\u7ec4\u4e13\u5bb6\u3002\u4e3b\u8981\u4ece\u4e8b\u65e0\u5b9a\u5f62\u50a8\u80fd\u70ad\u6750\u6599\u53ef\u63a7\u53ca\u4e2d\u8bd5\u5236\u5907\u3001\u7406\u8bba\u8ba1\u7b97\u4e0e\u4eba\u5de5\u667a\u80fd\u6784\u6548\u5173\u7cfb\u89e3\u6790\u53ca\u7535\u5316\u5b66\u50a8\u80fd\u5e94\u7528\u65b9\u9762\u7684\u7814\u7a76\u5de5\u4f5c\u3002\u8fd15\u5e74\u6765\u4e3b\u6301\u53ca\u53c2\u4e0e\u4e86\u5305\u62ec\u56fd\u5bb6\u91cd\u70b9\u7814\u53d1\u8ba1\u5212\u3001\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u3001\u4e2d\u56fd\u79d1\u5b66\u9662\u3001\u5c71\u897f\u7701\u4ee5\u53ca\u56fd\u5185\u5916\u4f01\u4e1a\u5408\u4f5c\u5728\u5185\u768420\u4f59\u9879\u79d1\u7814\u9879\u76ee\uff0c\u6db5\u76d6\u8d85\u7ea7\u7535\u5bb9\u5668\u3001\u9502\u79bb\u5b50\u7535\u6c60\u3001\u94a0\u79bb\u5b50\u7535\u6c60\u53ca\u9502\u786b\u7535\u6c60\u5173\u952e\u6750\u6599\u53ca\u5668\u4ef6\u3002\u8fd1\u5e74\u6765\u5728npj Comput. Mater., Adv. Mater., Adv. Energy Mater.\uff0cACS Energy Lett.\uff0cEnergy Storage Mater. \u7b49\u671f\u520a\u53d1\u8868\u8bba\u658790\u4f59\u7bc7\uff0c\u7533\u8bf7\u53d1\u660e\u4e13\u522960\u4f59\u9879\u3001\u8f6f\u84575\u9879\uff0c\u53c2\u4e0e\u7f16\u5199\u4e13\u84573\u90e8\u3001\u4e3b\u6301\u53ca\u53c2\u4e0e\u5236\u5b9a\u56fd\u5185\/IEC\u6807\u51c63\u9879\u3002\u83b7\u4e2d\u56fd\u4ea7\u5b66\u7814\u5408\u4f5c\u521b\u65b0\u6210\u679c\u5956\u4e00\u7b49\u5956\u3001\u5929\u6d25\u5e02\u81ea\u7136\u79d1\u5b66\u5956\u4e00\u7b49\u5956\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u6587\u7ae0\u4fe1\u606f\u3011 \u6587\u7ae0\u6807\u9898\uff1aUncovering Electrochemical Performance in Ester and Ether Electrolyt&#8230;<\/p>\n","protected":false},"author":31345,"featured_media":0,"comment_status":"open","ping_status":"","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-270249","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/270249"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/31345"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=270249"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/270249\/revisions"}],"predecessor-version":[{"id":270255,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/270249\/revisions\/270255"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=270249"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=270249"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=270249"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}