{"id":270705,"date":"2026-02-13T09:21:46","date_gmt":"2026-02-13T01:21:46","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=270705"},"modified":"2026-02-13T09:21:46","modified_gmt":"2026-02-13T01:21:46","slug":"%e4%b8%8a%e6%b5%b7%e4%ba%a4%e9%80%9a%e5%a4%a7%e5%ad%a6%e8%8b%8f%e5%b7%9e%e5%a4%a7%e5%ad%a6%e4%bb%8a%e6%97%a5%e6%9c%80%e6%96%b0science","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=270705","title":{"rendered":"\u4e0a\u6d77\u4ea4\u901a\u5927\u5b66&amp;\u82cf\u5dde\u5927\u5b66\u4eca\u65e5\u6700\u65b0Science"},"content":{"rendered":"\n<h2 class=\"wp-block-heading\"><strong>\u4e00\u3001\u3010\u79d1\u5b66\u80cc\u666f\u3011<\/strong><\/h2>\n\n\n\n<p>\u4e00\u4e2a\u4e16\u7eaa\u524d\u95ee\u4e16\u7684\u54c8\u4f2f-\u535a\u65bd\u6cd5\u5f7b\u5e95\u9769\u65b0\u4e86\u5316\u80a5\u751f\u4ea7\u5de5\u827a\uff0c\u81f3\u4eca\u4ecd\u662f\u4eba\u5de5\u5408\u6210\u6c28\u7684\u4e3b\u6d41\u6280\u672f\uff0c\u4e3a\u519c\u4e1a\u751f\u4ea7\u4e0e\u5316\u5de5\u9886\u57df\u7684\u53d1\u5c55\u5960\u5b9a\u4e86\u91cd\u8981\u57fa\u7840\u3002\u4f46\u8be5\u5de5\u827a\u9700\u8981\u4e25\u82db\u7684\u9ad8\u6e29\u9ad8\u538b\u53cd\u5e94\u6761\u4ef6\uff0c\u4e0d\u4ec5\u80fd\u8017\u9ad8\uff0c\u8fd8\u4f34\u968f\u5927\u91cf\u78b3\u6392\u653e\uff0c\u4e0e\u5f53\u524d\u7eff\u8272\u4f4e\u78b3\u7684\u53d1\u5c55\u8d8b\u52bf\u76f8\u6096\uff0c\u56e0\u6b64\u4e9f\u9700\u5f00\u53d1\u5e38\u6e29\u5e38\u538b\u4e0b\u7684\u9ad8\u6548\u5408\u6210\u6c28\u65b0\u65b9\u6cd5\u3002<\/p>\n\n\n\n<p>\u7535\u5316\u5b66\u9502\u4ecb\u5bfc\u6c2e\u6c14\u8fd8\u539f\u5236\u6c28\u6280\u672f\u56e0\u53ef\u5728\u5e38\u6e29\u5e38\u538b\u4e0b\u5b9e\u73b0\u6c2e-\u6c28\u8f6c\u5316\uff0c\u6210\u4e3a\u6781\u5177\u6f5c\u529b\u7684\u66ff\u4ee3\u6280\u672f\u8def\u5f84\uff0c\u4e5f\u88ab\u89c6\u4f5c\u89e3\u51b3\u4f20\u7edf\u5408\u6210\u6c28\u6280\u672f\u56fa\u6709\u7f3a\u9677\u7684\u91cd\u8981\u7a81\u7834\u53e3\u3002\u4f46\u8be5\u6280\u672f\u7684\u6c28\u4ea7\u7387\u4e0e\u53cd\u5e94\u6548\u7387\u957f\u671f\u53d7\u9650\u4e8e\u56fa\u4f53\u7535\u89e3\u8d28\u754c\u9762\uff08SEI\uff09\u5904\u9502\u79bb\u5b50\u8131\u6eb6\u4e0e\u6269\u6563\u52a8\u529b\u5b66\u7f13\u6162\u7684\u95ee\u9898\uff1aSEI\u5185\u9502\u79bb\u5b50\u6269\u6563\u7cfb\u6570\u4f4e\u81f310<sup>-21<\/sup> m<sup>2<\/sup> s<sup>-1<\/sup>\uff0c\u9502\u79bb\u5b50\u4f20\u8f93\u53d7\u963b\u76f4\u63a5\u5bfc\u81f4\u9502\u6c89\u79ef\u8fc7\u7a0b\u88ab\u6291\u5236\uff0c\u53cd\u5e94\u533a\u6301\u7eed\u5411SEI\/\u7535\u89e3\u8d28\u8fb9\u754c\u6536\u7f29\uff0c\u5927\u91cf\u7535\u6781\u8868\u9762\u66b4\u9732\u540e\u4f1a\u4fc3\u8fdb\u6790\u6c22\u526f\u53cd\u5e94\u53d1\u751f\uff0c\u4e0e\u6c2e\u6c14\u8fd8\u539f\u5f62\u6210\u7ade\u4e89\uff0c\u6700\u7ec8\u4f7f\u5f97\u9502\u4ecb\u5bfc\u6c2e\u6c14\u8fd8\u539f\u4f53\u7cfb\u4e2d\u6c28\u7684\u90e8\u5206\u7535\u6d41\u5bc6\u5ea6\u957f\u671f\u53d7\u9650\u57288 mA cm<sup>-2<\/sup>\uff0c\u53cd\u5e94\u6548\u7387\u5927\u5e45\u964d\u4f4e\u3002<\/p>\n\n\n\n<p>\u6b64\u5916\uff0c\u73b0\u6709\u7814\u7a76\u4e2d\u867d\u53ef\u901a\u8fc7\u9ad8\u538b\u6279\u91cf\u7535\u89e3\u4f53\u7cfb\u63d0\u5347\u6c2e\u6c14\u8fd8\u539f\u7684\u7535\u6d41\u5bc6\u5ea6\uff0c\u4f46\u9ad8\u538b\u6761\u4ef6\u4f1a\u663e\u8457\u589e\u52a0\u7cfb\u7edf\u80fd\u8017\uff0c\u4e14\u6279\u91cf\u53cd\u5e94\u5668\u7684\u8bbe\u8ba1\u4f7f\u8be5\u6280\u672f\u7684\u80fd\u91cf\u6548\u7387\u4ec5\u7ea63.0%\uff0c\u540c\u65f6\u65e0\u6cd5\u5b9e\u73b0\u6c28\u7684\u8fde\u7eed\u5316\u751f\u4ea7\uff0c\u96be\u4ee5\u6ee1\u8db3\u5b9e\u9645\u5e94\u7528\u9700\u6c42\u3002\u800c\u4f20\u7edfSEI\u7ed3\u6784\u65e0\u6cd5\u517c\u987e\u9502\u79bb\u5b50\u8131\u6eb6\u4e0e\u4f20\u8f93\u7684\u53cc\u91cd\u9700\u6c42\uff0c\u6210\u4e3a\u5236\u7ea6\u9502\u4ecb\u5bfc\u6c2e\u6c14\u8fd8\u539f\u5236\u6c28\u6280\u672f\u5411\u9ad8\u7535\u6d41\u5bc6\u5ea6\u3001\u9ad8\u6548\u7387\u3001\u8fde\u7eed\u5316\u53d1\u5c55\u7684\u6838\u5fc3\u74f6\u9888\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"1041\" height=\"549\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/02\/\u5fae\u4fe1\u56fe\u7247_20260213090012_379_10.png\" alt=\"\" class=\"wp-image-270723\" \/><\/figure>\n\n\n\n<h2 class=\"wp-block-heading\"><strong>\u4e8c\u3001\u3010\u521b\u65b0\u6210\u679c\u3011<\/strong><\/h2>\n\n\n\n<p>\u4e3a\u89e3\u51b3\u9502\u4ecb\u5bfc\u5e38\u6e29\u5e38\u538b\u6c2e\u6c14\u8fd8\u539f\u5236\u6c28\u4e2d\uff0c SEI\u9502\u79bb\u5b50\u8131\u6eb6\u548c\u6269\u6563\u7f13\u6162\u5bfc\u81f4\u6c28\u4ea7\u7387\u4f4e\u3001\u526f\u53cd\u5e94\u663e\u8457\u7684\u6838\u5fc3\u95ee\u9898\uff0c\u4e0a\u6d77\u4ea4\u901a\u5927\u5b66\u674e\u4fca\u526f\u6559\u6388\u548c\u82cf\u5dde\u5927\u5b66\u7a0b\u6d9b\u6559\u6388\u7b49\u4eba\u8bbe\u8ba1\u51fa LiF\/Li\u2082CO\u2083\/Li\u2083N \u534f\u540c\u8131\u6eb6-\u6269\u6563\u5c42\u72b6 SEI \u7ed3\u6784\uff0c\u89e3\u8026\u9502\u79bb\u5b50\u8131\u6eb6\u4e0e\u6269\u6563\u8fc7\u7a0b\uff0c\u5b9e\u73b0\u9502\u79bb\u5b50\u901a\u91cf\u63d0\u5347\u4e24\u4e2a\u6570\u91cf\u7ea7\u3002\u57282 M LiDFOB\u7535\u89e3\u6db2\u7684\u8fde\u7eed\u6d41\u4f53\u7cfb\u4e2d\uff0c\u8be5\u7ed3\u6784\u4e8e100 mA cm<sup>-2<\/sup>\u9ad8\u7535\u6d41\u5bc6\u5ea6\u4e0b\u5b9e\u73b098 %\u6c28\u6cd5\u62c9\u7b2c\u6548\u7387\u300121%\u80fd\u91cf\u6548\u7387\uff0c40\u5c0f\u65f6\u5185\u7ef4\u630180%\u4ee5\u4e0a\u6548\u7387\uff0c\u8fd8\u901a\u8fc7\u7406\u8bba\u8ba1\u7b97\u4e0e\u8868\u5f81\u660e\u786e\u4e86\u79bb\u5b50\u4f20\u8f93\u673a\u5236\uff0c\u7a81\u7834\u4e86\u8be5\u6280\u672f\u7684\u4f20\u8d28\u9650\u5236\uff0c\u4e3a\u5e38\u6e29\u5e38\u538b\u7535\u5316\u5b66\u5236\u6c28\u63d0\u4f9b\u4e86\u65b0\u7684\u9ad8\u6548\u7b56\u7565\u3002\u8be5\u6210\u679c\u4ee5\u201cEnhanced Li-ion diffusion improves N<sub>2<\/sub>-to-NH<sub>3<\/sub>&nbsp;current efficiency at 100 mA cm<sup>-2<\/sup>\u201d\u4e3a\u9898\u53d1\u8868\u5728\u56fd\u9645\u5b66\u672f\u671f\u520a\u300aScience\u300b\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full is-resized\"><img loading=\"lazy\" decoding=\"async\" width=\"1264\" height=\"833\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/02\/1.jpg\" alt=\"\" class=\"wp-image-270714\" style=\"width:840px;height:auto\" \/><\/figure>\n\n\n\n<p>\u56fe1. \u9502\u4ecb\u5bfc\u6c2e\u6c14\u7535\u89e3\u7684\u6781\u9650\u7535\u6d41\u4e0e\u79bb\u5b50\u4f20\u8f93\u578b\u56fa\u4f53\u7535\u89e3\u8d28\u754c\u9762\u819c\u3002<a>\u00a9 2026 AAAS<\/a><\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"1000\" height=\"676\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/02\/2.png\" alt=\"\" class=\"wp-image-270721\" \/><\/figure>\n\n\n\n<p>\u56fe2. \u534f\u540c\u8131\u6eb6-\u6269\u6563\u5c42\u72b6\u7ed3\u6784\u3002\u00a9 2026 AAAS<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"2560\" height=\"1004\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/02\/3-scaled.jpg\" alt=\"\" class=\"wp-image-270715\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/02\/3-scaled.jpg 2560w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/02\/3-1536x603.jpg 1536w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/02\/3-2048x804.jpg 2048w\" sizes=\"(max-width: 2560px) 100vw, 2560px\" \/><\/figure>\n\n\n\n<p>\u56fe3. DFT\u8ba1\u7b97\u3002\u00a9 2026 AAAS<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"2560\" height=\"2222\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/02\/4-scaled.jpg\" alt=\"\" class=\"wp-image-270716\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/02\/4-scaled.jpg 2560w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/02\/4-1536x1333.jpg 1536w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/02\/4-2048x1778.jpg 2048w\" sizes=\"(max-width: 2560px) 100vw, 2560px\" \/><\/figure>\n\n\n\n<p>\u56fe4. 100 mA cm<sup>-2<\/sup>\u4e0b\u9502\u4ecb\u5bfc\u6c2e\u6c14\u8fd8\u539f\u5408\u6210\u6c28\u7684\u7535\u5316\u5b66\u6027\u80fd\u3002\u00a9 2026 AAAS<\/p>\n\n\n\n<h2 class=\"wp-block-heading\"><strong>\u4e09\u3001\u3010\u79d1\u5b66\u542f\u8fea\u3011<\/strong><\/h2>\n\n\n\n<p>\u8fd9\u9879\u5de5\u4f5c\u89e3\u51b3\u4e86\u9502\u4ecb\u5bfc\u5e38\u6e29\u5e38\u538b\u7535\u5316\u5b66\u6c2e\u8fd8\u539f\u5236\u6c28\u4e2d\uff0cSEI\u9502\u79bb\u5b50\u8131\u6eb6\u4e0e\u6269\u6563\u7f13\u6162\u3001\u9ad8\u7535\u6d41\u5bc6\u5ea6\u4e0b\u6548\u7387\u4f4e\u4e14\u526f\u53cd\u5e94\u663e\u8457\u7684\u6838\u5fc3\u95ee\u9898\uff0c\u901a\u8fc7\u8bbe\u8ba1\u529f\u80fd\u5206\u5c42\u7684\u534f\u540c\u8131\u6eb6-\u6269\u6563\u5c42\u72b6SEI\u7ed3\u6784\uff0c\u5b9e\u73b0\u4e86\u9502\u79bb\u5b50\u4f20\u8f93\u6548\u7387\u7684\u5927\u5e45\u63d0\u5347\uff0c\u8ba9\u9ad8\u7535\u6d41\u5bc6\u5ea6\u4e0b\u9ad8\u6548\u3001\u7a33\u5b9a\u7684\u6c28\u5408\u6210\u6210\u4e3a\u53ef\u80fd\uff0c\u8fd8\u660e\u786e\u4e86\u8be5\u4f53\u7cfb\u7684\u79bb\u5b50\u4f20\u8f93\u4e0e\u6027\u80fd\u8870\u51cf\u673a\u5236\u3002\u8fd9\u4e00\u601d\u8def\u53ef\u63a8\u5e7f\u81f3\u9502\u57fa\u7535\u6c60\u3001\u5176\u4ed6\u6c14\u4f53\u7535\u8fd8\u539f\u7b49\u6d89\u53ca\u79bb\u5b50\u4f20\u8f93\u7684\u7535\u5316\u5b66\u4f53\u7cfb\uff0c\u4e3a\u754c\u9762\u7ed3\u6784\u4f18\u5316\u63d0\u4f9b\u901a\u7528\u8303\u5f0f\u3002<\/p>\n\n\n\n<p>\u539f\u6587\u4fe1\u606f\uff1aQiang Zhang et al. ,Enhanced Li-ion diffusion improves N<sub>2<\/sub>-to-NH<sub>3<\/sub> current efficiency at 100 mA cm<sup>\u22122<\/sup>. Science 391, 724-729 (2026).<\/p>\n\n\n\n<p><a href=\"https:\/\/www.science.org\/doi\/10.1126\/science.adw5462\">https:\/\/www.science.org\/doi\/10.1126\/science.adw5462<\/a><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4e00\u3001\u3010\u79d1\u5b66\u80cc\u666f\u3011 \u4e00\u4e2a\u4e16\u7eaa\u524d\u95ee\u4e16\u7684\u54c8\u4f2f-\u535a\u65bd\u6cd5\u5f7b\u5e95\u9769\u65b0\u4e86\u5316\u80a5\u751f\u4ea7\u5de5\u827a\uff0c\u81f3\u4eca\u4ecd\u662f\u4eba\u5de5\u5408\u6210\u6c28\u7684\u4e3b\u6d41\u6280\u672f\uff0c\u4e3a\u519c\u4e1a\u751f\u4ea7\u4e0e\u5316\u5de5\u9886\u57df\u7684\u53d1\u5c55\u5960\u5b9a\u4e86\u91cd\u8981\u57fa\u7840\u3002\u4f46\u8be5\u5de5\u827a\u9700\u8981\u4e25\u82db\u7684&#8230;<\/p>\n","protected":false},"author":186431,"featured_media":0,"comment_status":"open","ping_status":"","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[155],"class_list":["post-270705","post","type-post","status-publish","format-standard","hentry","category-keji","tag-science"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/270705"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/186431"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=270705"}],"version-history":[{"count":4,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/270705\/revisions"}],"predecessor-version":[{"id":270726,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/270705\/revisions\/270726"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=270705"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=270705"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=270705"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}