{"id":272727,"date":"2026-08-06T09:01:00","date_gmt":"2026-08-06T01:01:00","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=272727"},"modified":"2026-08-05T23:18:17","modified_gmt":"2026-08-05T15:18:17","slug":"%e8%a5%bf%e5%ae%89%e5%bb%ba%e5%a4%a7%e4%ba%91%e6%96%af%e5%ae%81%e6%95%99%e6%8e%88journal-of-materials-chemistry-a%ef%bc%9a-%e5%b7%a7%e5%80%9f%e7%94%b5%e8%b4%9f%e6%80%a7%e6%a2%af%e5%ba%a6%e6%9e%84","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=272727","title":{"rendered":"\u897f\u5b89\u5efa\u5927\u4e91\u65af\u5b81\u6559\u6388Journal of Materials Chemistry A\uff1a \u5de7\u501f\u7535\u8d1f\u6027\u68af\u5ea6\u6784\u7b51\u5185\u5efa\u7535\u573a\u7684\u9ad8\u71b5\u5408\u91d1\u951a\u5b9a\u516b\u9762\u4f53\u6c2e\u63ba\u6742\u78b3\uff1a\u534f\u540c\u754c\u9762\u52a0\u901f\u6790\u6c22\u53ca\u4e09\u7898\u5316\u7269\/\u94dc\u8fd8\u539f\u53cd\u5e94"},"content":{"rendered":"\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"346\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/08\/2382c315a6ba396-2.png\" alt=\"\" class=\"wp-image-272729\"\/><\/figure>\n\n\n\n<p><strong>\u3010\u6587\u7ae0\u4fe1\u606f\u3011<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u5de7\u501f\u7535\u8d1f\u6027\u68af\u5ea6\u6784\u7b51\u5185\u5efa\u7535\u573a\u7684\u9ad8\u71b5\u5408\u91d1\u951a\u5b9a\u516b\u9762\u4f53\u6c2e\u63ba\u6742\u78b3\uff1a\u534f\u540c\u754c\u9762\u52a0\u901f\u6790\u6c22\u53ca\u4e09\u7898\u5316\u7269\/\u94dc\u8fd8\u539f\u53cd\u5e94<\/p>\n\n\n\n<p>\u7b2c\u4e00\u4f5c\u8005\uff1a\u738b\u6d5a\u97ec<\/p>\n\n\n\n<p>\u901a\u8baf\u4f5c\u8005\uff1a\u4e91\u65af\u5b81*<\/p>\n\n\n\n<p>\u5355\u4f4d\uff1a\u897f\u5b89\u5efa\u7b51\u79d1\u6280\u5927\u5b66<\/p>\n\n\n\n<p><strong>\u3010\u7814\u7a76\u80cc\u666f\u3011<\/strong><\/p>\n\n\n\n<p>\u968f\u7740\u5168\u7403\u80fd\u6e90\u9700\u6c42\u589e\u957f\u548c\u6e29\u5ba4\u6c14\u4f53\u6392\u653e\u52a0\u5267\uff0c\u5411\u6e05\u6d01\u80fd\u6e90\u8f6c\u578b\u6210\u4e3a\u8feb\u5207\u9700\u6c42\u3002\u6c22\u80fd\uff08\u7535\u89e3\u6c34\u5236\u6c22\uff09\u548c\u592a\u9633\u80fd\uff08\u5982\u65b0\u4e00\u4ee3\u592a\u9633\u7535\u6c60\uff09\u88ab\u89c6\u4e3a\u91cd\u8981\u53ef\u518d\u751f\u80fd\u6e90\u3002\u7136\u800c\uff0c\u8fd9\u4e9b\u6280\u672f\u7684\u5173\u952e\u5171\u6027\u6311\u6218\u5728\u4e8e\uff1a\u6790\u6c22\u53cd\u5e94\uff08HER\uff09\u3001\u4e09\u7898\u5316\u7269\u8fd8\u539f\u53cd\u5e94\uff08IRR\uff09\u548c\u94dc\u8fd8\u539f\u53cd\u5e94\uff08CRR\uff09\u5747\u9700\u9ad8\u6548\u3001\u7a33\u5b9a\u7684\u7535\u50ac\u5316\u5242\u6765\u52a0\u901f\u53cd\u5e94\u52a8\u529b\u5b66\u3002\u76ee\u524d\uff0c<a>\u94c2\u57fa\u50ac\u5316\u5242\u5177\u6709\u9ad8\u50ac\u5316\u6d3b\u6027\u548c\u9ad8\u7a33\u5b9a\u6027\uff0c\u4f46\u5176\u9ad8\u6210\u672c\u3001\u8d44\u6e90\u7a00\u7f3a\u53ca\u517c\u5bb9\u6027\u5dee\u4e25\u91cd\u9650\u5236\u4e86\u5927\u89c4\u6a21\u5e94\u7528\u3002\u56e0\u6b64\uff0c\u5f00\u53d1\u9ad8\u6548\u3001\u591a\u529f\u80fd\u3001\u975e\u8d35\u91d1\u5c5e\u7535\u50ac\u5316\u5242\u6210\u4e3a\u7814\u7a76\u70ed\u70b9\u3002<\/a>\u4f20\u7edf\u8fc7\u6e21\u91d1\u5c5e\u5408\u91d1\uff08\u5982Fe\u3001Cr\u3001Co\u7b49\uff09\u901a\u8fc7\u7535\u5b50\u7ed3\u6784\u8c03\u63a7\u53ef\u63d0\u5347\u6027\u80fd\uff0c\u4f46\u6d3b\u6027\u4f4d\u70b9\u4e0d\u8db3\u5236\u7ea6\u5176\u53d1\u5c55\u3002<a>\u9ad8\u71b5\u5408\u91d1\uff08HEAs\uff09\u56e0\u5177\u6709\u591a<\/a>\u79cd\u4e3b\u5143\u5143\u7d20\u548c\u8fd1\u7b49\u539f\u5b50\u6bd4\u7684\u7279\u70b9\uff0c\u5c55\u73b0\u51fa\u9ad8\u71b5\u6548\u5e94\u3001\u6676\u683c\u7578\u53d8\u3001\u8fdf\u6ede\u6269\u6563\u548c\u201c\u9e21\u5c3e\u9152\u201d\u6548\u5e94\uff0c\u5728\u7535\u50ac\u5316\u4e2d\u8868\u73b0\u51fa\u4f18\u5f02\u6f5c\u529b\u3002\u7136\u800c\uff0cHEA\u672c\u8eab\u5bfc\u7535\u6027\u5dee\u3001\u6613\u56e2\u805a\uff0c\u4e14\u591a\u6d3b\u6027\u4f4d\u70b9\u95f4\u7684\u7ade\u4e89\u5438\u9644\u53ef\u80fd\u964d\u4f4e\u9009\u62e9\u6027\u3002\u6b64\u5916\uff0c\u78b3\u57fa\u9ad8\u71b5\u5408\u91d1\uff08HEAs\uff09\u6d3b\u6027\u4f4d\u70b9\u7684\u7cbe\u786e\u7535\u5b50\u8c03\u63a7\u662f\u63d0\u5347\u5176\u7535\u50ac\u5316\u6d3b\u6027\u7684\u5173\u952e\u9014\u5f84\uff0c\u4f46\u4ecd\u9762\u4e34\u6311\u6218\u3002\u4e3a\u6b64\uff0c\u672c\u7814\u7a76\u901a\u8fc7\u5f15\u5165\u5bfc\u7535\u8f7d\u4f53\uff08\u5982\u91d1\u5c5e\u6709\u673a\u6846\u67b6MOF\u884d\u751f\u7684\u6c2e\u63ba\u6742\u78b3\uff09\u6765\u6539\u5584\u5206\u6563\u6027\u4e0e\u7535\u8377\u4f20\u8f93\uff0c\u540c\u65f6\u5229\u7528\u5143\u7d20\u7535\u8d1f\u6027\u5dee\u5f02\u8c03\u63a7HEA\u5185\u90e8\u7535\u5b50\u7ed3\u6784\uff0c\u4f18\u5316\u6d3b\u6027\u4f4d\u70b9\u3002\u6b63\u662f\u57fa\u4e8e\u8fd9\u4e00\u601d\u8def\uff0c\u4f5c\u8005\u8bbe\u8ba1\u4e86\u4e00\u79cdCu-BTC\u884d\u751f\u7684\u516b\u9762\u4f53\u6c2e\u63ba\u6742\u78b3\u8d1f\u8f7dFeCrCoCuMn\u9ad8\u71b5\u5408\u91d1\uff08HEA-NC\uff09\uff0c\u901a\u8fc7\u6784\u5efa\u5185\u90e8\u7535\u573a\u548c\u754c\u9762\u534f\u540c\u6548\u5e94\uff0c\u5b9e\u73b0HER\u3001IRR\u548cCRR\u7684\u9ad8\u6548\u50ac\u5316\uff0c\u5e76\u4e3a\u591a\u529f\u80fd\u975e\u8d35\u91d1\u5c5e\u50ac\u5316\u5242\u8bbe\u8ba1\u63d0\u4f9b\u65b0\u7b56\u7565\u3002<\/p>\n\n\n\n<p><strong>\u3010\u6587\u7ae0\u7b80\u4ecb\u3011<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u8fd1\u65e5\uff0c\u897f\u5b89\u5efa\u7b51\u79d1\u6280\u5927\u5b66<strong>\u4e91\u65af\u5b81\u6559\u6388\u56e2\u961f<\/strong>\u5728\u56fd\u9645\u77e5\u540d\u671f\u520a<strong>\u300a<\/strong><strong>Journal of Materials Chemistry A<\/strong><strong>\u300b<\/strong>\u4e0a\u53d1\u8868\u4e86\u9898\u4e3a\u201c<strong>Internal Electric Field Engineered High-Entropy Alloy on Octahedral N-Doped Carbon via Electronegativity Gradient: Synergistic Interfaces Accelerating Hydrogen Evolution and Triiodide\/Copper <a>Reduction<\/a>&nbsp;Reactions<\/strong>\u201d\u7684\u7814\u7a76\u8bba\u6587\u3002\u8be5\u7814\u7a76\u63d0\u51fa\u4e00\u79cd1,3,5-\u82ef\u4e09\u7fa7\u9178\uff08BTC\uff09\u8f85\u52a9\u5408\u6210\u7b56\u7565\uff0c\u5b9e\u73b00D FeCrCoCuMn\u9ad8\u71b5\u5408\u91d1\u57283D\u516b\u9762\u4f53\u6c2e\u63ba\u6742\u78b3\uff08NC\uff09\u4e0a\u7684\u539f\u4f4d\u751f\u957f\u3002\u9ad8\u71b5\u5408\u91d1\u4e2d\u91d1\u5c5e\u5143\u7d20\u95f4\u7684\u7535\u8d1f\u6027\u5dee\u5f02\u8bf1\u5bfc\u4e86\u7535\u5b50\u4eceMn\u5411Cu\/Co\u8f6c\u79fb\uff0c\u4ece\u800c\u4f18\u5316\u4e86\u9ad8\u71b5\u5408\u91d1\u7684\u7535\u5b50\u7ed3\u6784\u3002\u540c\u65f6\uff0c\u6cbf\u9ad8\u71b5\u5408\u91d1-NC\u754c\u9762\u7684\u7535\u5b50\u6301\u7eed\u4ece\u9ad8\u71b5\u5408\u91d1\u5411NC\u8fc1\u79fb\uff0c\u5bfc\u81f4\u663e\u8457\u7684\u7535\u8377\u8f6c\u79fb\u5e76\u5f62\u6210\u5185\u5efa\u7535\u573a\u3002\u5f97\u76ca\u4e8e\u9ad8\u71b5\u5408\u91d1\u7535\u5b50\u7ed3\u6784\u7684\u6539\u5584\u4ee5\u53ca\u9ad8\u71b5\u5408\u91d1-NC\u754c\u9762\u7684\u534f\u540c\u589e\u5f3a\uff0c\u8be5\u50ac\u5316\u5242HEA-NC\u5728\u6790\u6c22\u53cd\u5e94HER\u4e2d\u5b9e\u73b0\u4e8699 mV\u7684\u8fc7\u7535\u4f4d\u548c64 mV dec<sup>-1<\/sup>\u7684\u5854\u83f2\u5c14\u659c\u7387\u3002\u5728\u592a\u9633\u80fd\u7535\u6c60\u5e94\u7528\u4e2d\uff0c\u7ec4\u88c5\u7684\u5149\u4f0f\u5668\u4ef6\u5728\u4e09\u7898\u5316\u7269\u8fd8\u539fIRR\u548c\u94dc\u8fd8\u539f\u53cd\u5e94CRR\u4e2d\u5206\u522b\u83b7\u5f97\u4e868.52%\u548c5.82%\u7684\u5149\u7535\u8f6c\u6362\u6548\u7387\u3002\u8fd9\u9879\u5de5\u4f5c\u4e0d\u4ec5\u63ed\u793a\u4e86\u9ad8\u71b5\u5408\u91d1\u7684\u7535\u5b50\u8fc1\u79fb\u673a\u7406\uff0c\u4e5f\u4e3a\u8bbe\u8ba1\u9ad8\u6548\u53cc\u529f\u80fd\u50ac\u5316\u5242\u5efa\u7acb\u4e86\u901a\u7528\u7b56\u7565\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"300\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/08\/ce6e2814f207c93-2.png\" alt=\"\" class=\"wp-image-272730\"\/><\/figure>\n\n\n\n<p><strong>\u3010\u672c\u7814\u7a76\u8981\u70b9\u3011<\/strong><\/p>\n\n\n\n<p><strong>\u8981\u70b9\u4e00\uff1a<\/strong><strong>BTC\u8f85\u52a9\u7b56\u7565\u6784\u7b51\u516b\u9762\u4f53\u6c2e\u63ba\u6742\u78b3\u951a\u5b9a\u9ad8\u71b5\u5408\u91d1\u7eb3\u7c73\u590d\u5408\u6750\u6599<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u672c\u7814\u7a76\u4ee5Cu-BTC\u4e3a\u6a21\u677f\uff0c\u7ecf400 \u00b0C\u70ed\u89e3\u5f97\u5230Cu-NC\uff0c\u518d\u5f15\u5165\u7b49\u6469\u5c14\u6bd4Fe\u3001Cr\u3001Co\u3001Cu\u3001Mn\u76d0\uff0c\u7ecf\u6db2\u76f8\u8fd8\u539f\u548c600 \u00b0C\u9ad8\u6e29\u70ed\u89e3\uff0c\u6210\u529f\u5408\u6210FeCrCoCuMn\u9ad8\u71b5\u5408\u91d1\u7eb3\u7c73\u9897\u7c92\u5747\u5300\u951a\u5b9a\u4e8e\u516b\u9762\u4f53NC\u7684\u590d\u5408\u6750\u6599\uff08HEA-NC\uff09\uff08\u56fe1a\uff09\u3002SEM\u8868\u660eHEA\u7eb3\u7c73\u9897\u7c92\u5728NC\u8868\u9762\u5747\u5300\u5206\u6563\u3001\u65e0\u660e\u663e\u56e2\u805a\uff08\u56fe1b-f\uff09\uff1bHR-TEM\u663e\u793a\u6676\u683c\u6761\u7eb9\u5bf9\u5e94FCC\u7ed3\u6784\u7684\uff08111\uff09\u548c\uff08200\uff09\u6676\u9762\uff0cIFFT\u53caFFT\u8bc1\u5b9e\u5176\u9ad8\u7ed3\u6676\u6027\u4e0e\u5355\u76f8\u56fa\u6eb6\u4f53\u7279\u5f81\uff08\u56fe1g-j\uff09\u3002\u5143\u7d20\u9762\u5206\u5e03\u8bc1\u5b9eFe\u3001Cr\u3001Co\u3001Cu\u3001Mn\u3001N\u5747\u5300\u5206\u5e03\uff08\u56fe1k\uff09\u3002XRD\u663e\u793aFCC\u7279\u5f81\u5cf0\uff0844.22\u00b0\u300151.55\u00b0\u300174.83\u00b0\uff09\u76f8\u8f83Cu-NC\u6b63\u79fb\uff0c\u8868\u660e\u5408\u91d1\u5316\u5f15\u8d77\u6676\u683c\u6536\u7f29\uff08\u56fe2a-b\uff09\u3002Raman\u4e2dID\/IG=1.10\uff0c\u9ad8\u4e8e\u4e2d\u71b5\u5408\u91d1MEA-NC\uff081.06\uff09\u548cCu-NC\uff081.03\uff09\uff0c\u8868\u660eHEA-NC\u5177\u6709\u66f4\u9ad8\u7f3a\u9677\u5bc6\u5ea6\u4e0e\u6d3b\u6027\u4f4d\u70b9\uff08\u56fe2c\uff09\u3002\u9ad8\u71b5HEA-NC\u7684BET\u6bd4\u8868\u9762\u79ef\u4e3a184.55 m\u00b2\/g\uff08\u56fe2d-e\uff09\uff0c\u63a5\u89e6\u89d237.8\u00b0\u4f18\u4e8e\u4e2d\u71b5MEA-NC\uff0840.2\u00b0\uff09\uff0c\u4eb2\u6c34\u6027\u6539\u5584\u6709\u5229\u4e8e\u7535\u89e3\u6db2\u6e17\u900f\uff08\u56fe2f\uff09\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"500\" height=\"630\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/08\/7f88dbbcaa77a1d-2.png\" alt=\"\" class=\"wp-image-272731\"\/><\/figure>\n\n\n\n<p>\u56fe1. (a) HEA-NC\u7684\u5408\u6210\u8def\u7ebf\u3002(b) Cu-NC\u3001(c) MEA-NC\u548c(d) HEA-NC\u7684SEM\u56fe\u50cf\u3002(e,&nbsp;f) HEA-NC\u7684HRTEM\u56fe\u50cf\u3002(g) HEA\u7eb3\u7c73\u9897\u7c92\u7684HRTEM\u56fe\u50cf\u3002(h) HEA-NC\u7684\u76f8\u5173FFT\u6a21\u5f0f\u3002(i,&nbsp;j) HEA-NC\u7684(111)\u6676\u9762\u548c(200)\u6676\u9762\u7684FFT\u9006\u56fe\u50cf\u3002(k) HEA-NC\u5143\u7d20\u5206\u5e03\u56fe\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"700\" height=\"418\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/08\/4e9a0ba2491dfde-2.png\" alt=\"\" class=\"wp-image-272732\"\/><\/figure>\n\n\n\n<p>\u56fe2. (a) \u4e09\u79cd\u50ac\u5316\u5242\u7684XRD<a>\u56fe\u8c31<\/a>\u3002(b) XRD\u5cf0\u4f4d\u653e\u5927\u56fe\u8c31\u548c(c)\u4e09\u79cd\u50ac\u5316\u5242\u7684\u62c9\u66fc\u5149\u8c31\u3002(d) HEA-NC\u548c(e) MEA-NC\u7684N\u2082\u5438\u9644-\u8131\u9644\u7b49\u6e29\u7ebf\uff08\u63d2\u56fe\uff1a\u5bf9\u5e94\u5b54\u5f84\u5206\u5e03\u66f2\u7ebf\uff09\u3002(f) Cu-NC\u3001MEA-NC\u548cHEA-NC\u7684\u6c34\u63a5\u89e6\u89d2\u56fe\u3002<\/p>\n\n\n\n<p><strong>\u8981\u70b9\u4e8c\uff1a<\/strong><strong>\u7535\u8d1f\u6027\u68af\u5ea6\u9a71\u52a8\u7535\u5b50\u5b9a\u5411\u8f6c\u79fb<\/strong><strong><\/strong><\/p>\n\n\n\n<p>XPS\u5168\u8c31\u8bc1\u5b9eHEA-NC\u4e2dFe\u3001Cr\u3001Co\u3001Cu\u3001Mn\u3001C\u3001N\u5171\u5b58\uff08\u56fe3a\uff09\uff0cN 1s\u4e2d\u5421\u5576\u6c2e\u3001\u5421\u54af\u6c2e\u3001\u77f3\u58a8\u6c2e\u548c\u6c27\u5316\u6c2e\u7684\u5b58\u5728\u6709\u5229\u4e8e\u50ac\u5316\u6d3b\u6027\u3002\u5bf9\u6bd4\u4e2d\u71b5MEA-NC\u548c\u9ad8\u71b5HEA-NC\u7684\u9ad8\u5206\u8fa8XPS\uff08\u56fe3b-f\uff09\uff0cMn\u5f15\u5165\u540eFe 2p\u548cCr 2p\u7ed3\u5408\u80fd\u5206\u522b\u8d1f\u79fb0.1 eV\u548c0.2 eV\uff0cCu 2p\u548cCo 2p\u5206\u522b\u8d1f\u79fb0.5 eV\u548c0.4 eV\uff0c\u8bc1\u660e\u4f4e\u7535\u8d1f\u6027Mn\u4f5c\u4e3a\u7535\u5b50\u4f9b\u4f53\uff0c\u7ecf\u4e2d\u95f4\u5143\u7d20Fe\/Cr\u5c06\u7535\u5b50\u4f20\u9012\u7ed9\u9ad8\u7535\u8d1f\u6027Cu\/Co\uff0c\u5f62\u6210\u201cMn\u2192Cu\/Co\u201d\u7535\u5b50\u5b9a\u5411\u8f6c\u79fb\u8def\u5f84\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"700\" height=\"416\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/08\/b14210e1ee30421-2.png\" alt=\"\" class=\"wp-image-272733\"\/><\/figure>\n\n\n\n<p>\u56fe3. (a) HEA-NC\u7684XPS\u626b\u63cf\u8c31\u3002MEA-NC\u548cHEA-NC\u4e2d(b)Fe\u3001(c) Cr\u3001(d) Cu\u548c(e) Co\u5143\u7d20\u7684\u7cbe\u7ec6\u8c31\u3002(f) HEA-NC\u4e2dMn\u5143\u7d20\u7684\u7cbe\u7ec6\u8c31\u3002<\/p>\n\n\n\n<p><strong>\u8981\u70b9\u4e09\uff1a<\/strong><strong>\u9ad8\u6548\u6790\u6c22\u53cd\u5e94\uff08HER\uff09\u6027\u80fd\u53ca\u7a33\u5b9a\u6027<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u5c06HEA-NC\u7528\u4e8e\u78b1\u6027\u7535\u89e3\u6c34\u6790\u6c22\u53cd\u5e94\uff08\u56fe4\uff09\u3002\u7535\u5316\u5b66\u6d4b\u8bd5\u8868\u660e\uff0c\u5f97\u76ca\u4e8eHEA\u5185\u90e8&#8221;Mn\u2192Cu\/Co&#8221;\u5b9a\u5411\u7535\u8377\u8f6c\u79fb\uff0c\u9ad8\u71b5HEA-NC\u6709\u6548\u964d\u4f4e\u4e86HER\u53cd\u5e94\u80fd\u5792\uff0c\u52a0\u5feb\u4e86\u7535\u5b50\u8f6c\u79fb\u8fc7\u7a0b\u3002\u572810 mA cm\u207b\u00b2\u4e0b\u8fc7\u7535\u4f4d\u4ec599 mV\uff0c\u4f4e\u4e8e\u4e2d\u71b5MEA-NC\uff08120 mV\uff09\u3001Cu-NC\uff08146 mV\uff09\u548cNF\uff08224 mV\uff09\uff1b\u9ad8\u71b5HEA-NC\u7684Tafel\u659c\u7387\u4e3a64 mV dec\u207b\u00b9\uff0c\u4f4e\u4e8e\u4e2d\u71b5MEA-NC\uff08102 mV dec\u207b\u00b9\uff09\u548cCu-NC\uff08138 mV dec\u207b\u00b9\uff09\uff0c\u8868\u660e\u5176\u9075\u5faa\u9ad8\u6548\u7684Volmer-Heyrovsky\u673a\u5236\uff08\u56fe4a-b\uff09\u3002\u7535\u5316\u5b66\u963b\u6297\u5206\u6790\u8fdb\u4e00\u6b65\u8bc1\u5b9e\uff0cHEA-NC\u7684\u7535\u8377\u8f6c\u79fb\u7535\u963b\uff08R<sub>ct<\/sub>=5.32 \u03a9 cm<sup>2<\/sup>\uff09\u663e\u8457\u4f4e\u4e8e\u5bf9\u6bd4\u7ec4\uff08\u56fe4c\uff09\uff0c\u5f52\u56e0\u4e8e\u5185\u5efa\u7535\u573a\u4e3aHeyrovsky\u6b65\u9aa4\u4e2d\u7535\u5b50\u8f6c\u79fb\u63d0\u4f9b\u4e86\u5feb\u901f\u901a\u9053\u3002\u7535\u5316\u5b66\u6d3b\u6027\u9762\u79ef\u6d4b\u8bd5\u8868\u660eHEA-NC\u5177\u6709\u6700\u5927\u7684Cdl\uff084.61 mF cm\u207b\u00b2\uff09\u548cECSA\uff08115.25 cm\u00b2\uff09\uff08\u56fe4d-e\uff09\uff0c\u516b\u9762\u4f53\u4e09\u7ef4\u7ed3\u6784\u63d0\u4f9b\u4e86\u9ad8\u6bd4\u8868\u9762\u79ef\u548c\u4e30\u5bcc\u7684\u591a\u91d1\u5c5e\u6d3b\u6027\u4f4d\u70b9\u3002\u7a33\u5b9a\u6027\u6d4b\u8bd5\u8868\u660e\uff08\u56fe4f-g\uff09\uff0c\u7ecf1000\u5708CV\u5faa\u73af\u540eLSV\u66f2\u7ebf\u51e0\u4e4e\u91cd\u5408\uff0c30 h\u6052\u7535\u6d41\u6d4b\u8bd5\u540e\u8fc7\u7535\u4f4d\u4fdd\u6301\u7387\u8fbe96.4%\uff0c\u9ad8\u6784\u578b\u71b5\u8d4b\u4e88\u7684\u50ac\u5316\u5242\u7684\u7ed3\u6784\u7a33\u5b9a\u6027\u548cCr\u5143\u7d20\u7684\u8010\u8150\u8680\u6027\uff0c\u5171\u540c\u4fdd\u969c\u4e86\u5176\u957f\u671f\u8010\u4e45\u6027\u3002\u4e0a\u8ff0\u7ed3\u679c\u8868\u660e\uff0c\u9ad8\u71b5\u5408\u91d1HEA\u4e2d\u7684\u5b9a\u5411\u7535\u8377\u8f6c\u79fb\u80fd\u591f\u6709\u6548\u4fc3\u8fdbHER\u8fc7\u7a0b\u4e2d\u7684\u7535\u8377\u4f20\u8f93\u4e0e\u53cd\u5e94\u52a8\u529b\u5b66\uff0c\u4f7fHEA-NC\u5728\u78b1\u6027HER\u4e2d\u5c55\u73b0\u51fa\u4f18\u4e8e\u591a\u6570\u5df2\u62a5\u9053\u975e\u8d35\u91d1\u5c5e\u50ac\u5316\u5242\u7684\u6790\u6c22\u6027\u80fd\uff08\u56fe4h\uff09\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"550\" height=\"610\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/08\/de5bcf7d8eaea98-2.png\" alt=\"\" class=\"wp-image-272734\"\/><\/figure>\n\n\n\n<p>\u56fe4. (a) \u50ac\u5316\u5242\u7684LSV\u66f2\u7ebf\uff0c(b) Tafel\u6781\u5316\u66f2\u7ebf\uff0c(c) <a>Nyquist\u56fe<\/a>\uff0c(d) Cdl\u503c\u3002(e) \u50ac\u5316\u5242\u7684ECSA\u503c\u3002(f) \u50ac\u5316\u5242\u57281000\u6b21CV\u5faa\u73af\u524d\u540e\u7684LSV\u66f2\u7ebf\u548c(g)\u6052\u7535\u4f4d\u65f6\u95f4\u66f2\u7ebf\u3002(h)\u672c\u7814\u7a76\u4e2d\u7684\u50ac\u5316\u5242&nbsp;HEA-NC\u4e0e\u5df2\u6709\u50ac\u5316\u5242\u7684\u6790\u6c22\u6027\u80fd\u6bd4\u8f83\u3002<\/p>\n\n\n\n<p><strong>\u8981\u70b9\u56db\uff1a<\/strong><strong>\u8d85\u8d8aPt\u5bf9\u7535\u6781\u7684<\/strong><strong>\u592a\u9633\u80fd<\/strong><strong>\u5149\u4f0f\u6027\u80fd\u53ca\u7a33\u5b9a\u6027\uff08IRR\/CRR\uff09<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u5c06HEA-NC\u7528\u4f5c\u592a\u9633\u80fd\u7535\u6c60\u5bf9\u7535\u6781\uff0c\u8003\u5bdf\u5176\u5728IRR\u548cCRR\u8fc7\u7a0b\u4e2d\u7684\u50ac\u5316\u6027\u80fd\uff08\u56fe5\uff09\u3002\u5faa\u73af\u4f0f\u5b89\u6d4b\u8bd5\u8868\u660e\uff0cHEA-NC\u5177\u6709\u66f4\u9ad8\u7684\u6c27\u5316-\u8fd8\u539f\u5cf0\u7535\u6d41\u5bc6\u5ea6\uff08-2.51 mA cm\u207b\u00b2\uff09\u548c\u66f4\u5c0f\u7684\u5cf0\u7535\u4f4d\u5206\u79bb\uff080.41 V\uff09\uff0c\u4f18\u4e8eMEA-NC\u548cCu-NC\uff08<a>\u56fe5a<\/a>-c\uff09\uff0c\u8868\u660e\u5176\u80fd\u591f\u6709\u6548\u4fc3\u8fdbI\u2083\u207b\/I\u207b\u6c27\u5316\u8fd8\u539f\u53cd\u5e94\u52a8\u529b\u5b66\u3002\u5728\u7898\u7535\u5bf9\u4f53\u7cfb<a>\uff08<\/a>\u56fe5d-f\uff09\u548c\u94dc\u7535\u5bf9\u4f53\u7cfb\uff08\u56fe5g-i\uff09\u4e2d\uff0c\u7535\u5316\u5b66\u963b\u6297\u8c31\u548c\u5854\u83f2\u5c14\u66f2\u7ebf\u5206\u6790\u8fdb\u4e00\u6b65\u8bc1\u660e\uff0cHEA\u8868\u9762\u5bcc\u7535\u5b50\u533a\u57df\u964d\u4f4e\u4e86I\u2083\u207b\u8fd8\u539f\u7684\u6d3b\u5316\u80fd\u5792\uff0c\u800cHEA\u5185\u90e8\u591a\u91d1\u5c5e\u6d3b\u6027\u4f4d\u70b9\u4e0eHEA\u2192NC\u754c\u9762\u5185\u5efa\u7535\u573a\u7684\u534f\u540c\u4f5c\u7528\u964d\u4f4e\u4e86\u754c\u9762\u7535\u8377\u4f20\u8f93\u963b\u529b\uff0c\u52a0\u5feb\u4e86\u7535\u5b50\u8f6c\u79fb\u8fc7\u7a0b\uff08\u56fe5d-e\uff09\u3002HEA-NC\u8868\u73b0\u51fa\u4f18\u5f02\u7684\u7535\u50ac\u5316\u6d3b\u6027\uff0c\u5728IRR\u548cCRR\u4e2d\u5206\u522b\u5b9e\u73b0\u4e868.52%\u548c5.82%\u7684\u5149\u7535\u8f6c\u6362\u6548\u7387\uff08\u56fe5f\uff0ci\uff09\uff0c\u9ad8\u4e8ePt\u5bf9\u7535\u6781\uff087.34%\u548c4.53%\uff09\u4ee5\u53ca\u5927\u591a\u6570\u5df2\u62a5\u9053\u7684\u540c\u7c7b\u50ac\u5316\u6750\u6599\uff08\u56fe5j\uff09\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"500\" height=\"580\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/08\/aa3023e0288002c-2.png\" alt=\"\" class=\"wp-image-272735\"\/><\/figure>\n\n\n\n<p>\u56fe5. (a) \u56db\u79cd\u50ac\u5316\u5242\u7684\u5faa\u73af\u4f0f\u5b89\u66f2\u7ebf\u3002(b) \u4e0d\u540c\u626b\u63cf\u901f\u7387\u4e0b\u7684HEA-NC\u7684\u5faa\u73af\u4f0f\u5b89\u66f2\u7ebf\u3002(c) I<sub>p<\/sub>\u4e0e\u626b\u63cf\u901f\u7387\u5e73\u65b9\u6839\u4e4b\u95f4\u7684\u7ebf\u6027\u5173\u7cfb\u3002(d-e)<a>&nbsp;\u50ac\u5316\u5242<\/a>\u5728&nbsp;I<sub>3<\/sub><sup>\u2212<\/sup>\/I<sup>\u2212<\/sup>\u4f53\u7cfb\u4e2d\u7684Nyquist\u56fe\u548cTafel\u6781\u5316\u66f2\u7ebf\u3002(f) \u50ac\u5316\u5242\u5728N719-<a>I<\/a><sub>3<\/sub><sup>\u2212<\/sup>\/I<sup>\u2212<\/sup>\u4f53\u7cfb\u4e2d<a><\/a>\u7684J\u2013V\u66f2\u7ebf\u3002(g-h) <a>\u50ac\u5316\u5242<\/a>\u5728<a><\/a>Cu<sup>2+<\/sup>\/Cu<sup>+<\/sup>\u4f53\u7cfb\u4e2d\u7684Nyquist\u56fe\u548cTafel\u6781\u5316\u66f2\u7ebf\u3002(i) \u50ac\u5316\u5242\u5728D35-Cu<sup>2+<\/sup>\/Cu<sup>+<\/sup>\u4f53\u7cfb\u4e2d\u7684J\u2013V\u66f2\u7ebf\u3002(h) \u4e0d\u540c\u50ac\u5316\u5242\u5728I<sub>3<\/sub><sup>\u2212<\/sup>\/I<sup>\u2212<\/sup>\u4f53\u7cfb\u548c\u5728Cu<sup>2+<\/sup>\/Cu<sup>+<\/sup>\u4f53\u7cfb\u4e2d\u7684\u592a\u9633\u80fd\u5149\u7535\u8f6c\u6362\u6548\u7387PCE\u6bd4\u8f83\u3002<\/p>\n\n\n\n<p>\u8fdb\u4e00\u6b65\u7684\u7a33\u5b9a\u6027\u6d4b\u8bd5\u8868\u660e\uff08\u56fe6\uff09\uff0cHEA-NC\u5bf9\u7535\u6781\u572850\u5708\u8fde\u7eedCV\u626b\u63cf\u540e\u66f2\u7ebf\u9ad8\u5ea6\u91cd\u5408\uff0c\u5149\u5f00\u5173\u5faa\u73af\u6d4b\u8bd5\u540e\u5149\u7535\u6d41\u4fdd\u6301\u7387\u8fbe97.2%\uff0c\u9ad8\u71b5\u5408\u91d1\u7684\u70ed\u529b\u5b66\u7a33\u5b9a\u6027\u548cCr\u8bf1\u5bfc\u7684\u8010\u8150\u8680\u6027\u4f7f\u5176\u5728\u8150\u8680\u6027\u7898\u7535\u89e3\u6db2\u4e2d\u5c55\u73b0\u51fa\u663e\u8457\u4f18\u4e8ePt\u57fa\u7535\u6781\u7684\u5faa\u73af\u7a33\u5b9a\u6027\u548c\u6301\u7eed\u5149\u7535\u54cd\u5e94\u80fd\u529b\u3002\u4e0a\u8ff0\u7ed3\u679c\u8868\u660e\uff0c\u7535\u8d1f\u6027\u68af\u5ea6\u9a71\u52a8\u7684\u5185\u5efa\u7535\u573a\u4e0e\u53cc\u7535\u5b50\u901a\u8def\u80fd\u591f\u6709\u6548\u63d0\u5347\u7535\u5b50\u4f20\u8f93\u548c\u53cd\u5e94\u52a8\u529b\u5b66\uff0c\u4f7fHEA-NC\u5728IRR\u548cCRR\u4e2d\u5c55\u73b0\u51fa\u4f18\u5f02\u7684\u50ac\u5316\u6027\u80fd\uff0c\u5c55\u73b0\u51fa\u5176\u5728\u65b0\u578b\u592a\u9633\u80fd\u7535\u6c60\u4e2d\u7684\u5e94\u7528\u6f5c\u529b\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"600\" height=\"532\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/08\/e2f457ec632c1f6.png\" alt=\"\" class=\"wp-image-272736\"\/><\/figure>\n\n\n\n<p>\u56fe6. (a) HEA-NC\u3001(b) MEA-NC\u548c(c) Cu-NC \u768450\u6b21\u5faa\u73afCV\u66f2\u7ebf\u3002(d-f)&nbsp;\u50ac\u5316\u5242\u7684\u6c27\u5316-\u8fd8\u539f\u5cf0\u7535\u6d41\u5bc6\u5ea6\u3002(g) \u5149\u7535\u54cd\u5e94\u6d4b\u8bd5\u53ca(h) \u50ac\u5316\u5242\u7684\u7535\u6d41\u5bc6\u5ea6\u8010\u4e45\u6027\u5bf9\u6bd4\u3002<\/p>\n\n\n\n<p><strong>\u8981\u70b9\u4e94\uff1a<\/strong><strong>\u5185\u5efa\u7535\u573a\u4e0e\u53cc\u7535\u5b50\u901a\u8def\u534f\u540c\u673a\u7406<\/strong><strong><\/strong><\/p>\n\n\n\n<p>DFT\u8ba1\u7b97\u63ed\u793a\u4e86HEA\u5185\u90e8\u7535\u5b50\u5206\u5e03\uff08\u56fe7a-b\uff09\u3002Mn\u539f\u5b50\u5468\u56f4\u7535\u5b50\u5bc6\u5ea6\u964d\u4f4e\uff08\u4f9b\u4f53\uff09\uff0cFe\/Cr\/Co\/Cu\u5468\u56f4\u589e\u52a0\uff08\u53d7\u4f53\uff09\uff0c\u9a8c\u8bc1\u4e86\u201cMn\u2192Cu\/Co\u201d\u7535\u8377\u8f6c\u79fb<a>\uff08\u56fe7c\uff09<\/a>\u3002HEA-NC\u754c\u9762\u7535\u8377\u5bc6\u5ea6\u5dee\u663e\u793a\u7535\u5b50\u4eceHEA\u5411NC\u8f7d\u4f53\u51c0\u8fc1\u79fb\uff0cNC\u4fa7\u5bcc\u7535\u5b50\uff0cHEA\u4fa7\u7f3a\u7535\u5b50\uff0c\u5f62\u6210\u5185\u5efa\u7535\u573a\uff08\u56fe7d\uff09\u3002\u7ed3\u5408UPS\/XPS\u8bc1\u5b9e\uff0c\u786e\u7acb\u4e86\u53cc\u7535\u5b50\u901a\u8def\uff1a\u2460\u5408\u91d1\u5185\u7535\u8d1f\u6027\u68af\u5ea6\u9a71\u52a8\u5b9a\u5411\u7535\u8377\u8f6c\u79fb\uff0c\u4f18\u5316\u6d3b\u6027\u4f4d\u70b9\u7535\u5b50\u7ed3\u6784\uff1b\u2461\u754c\u9762\u5904\u7535\u5b50\u6301\u7eed\u8fc1\u79fb\u81f3NC\u8f7d\u4f53\uff0c\u964d\u4f4e\u6574\u4f53\u529f\u51fd\u6570\uff0c\u4e3aHeyrovsky\u6b65\u9aa4\u548cIRR\u521d\u59cb\u7535\u5b50\u8f6c\u79fb\u63d0\u4f9b\u5feb\u901f\u901a\u9053\uff08\u56fe7e-g\uff09\u3002\u8be5\u534f\u540c\u673a\u5236\u52a0\u901f\u4e86HER\u548cIRR\/CRR\u7684\u53cd\u5e94\u52a8\u529b\u5b66\uff0c\u662fHEA-NC\u4f18\u5f02\u7efc\u5408\u6027\u80fd\u7684\u5fae\u89c2\u6839\u6e90\u3002<\/p>\n\n\n\n<figure class=\"wp-block-image size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"550\" height=\"572\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2026\/08\/bf2e94a56e16c6a-1.png\" alt=\"\" class=\"wp-image-272737\"\/><\/figure>\n\n\n\n<p>\u56fe7. (a) Cu-NC\u3001MEA-NC\u548cHEA-NC\u7684\u529f\u51fd\u6570\u3002(b) MEA-NC\u4e0eHEA-NC\u4e2d\u5404\u5143\u7d20\u7ed3\u5408\u80fd\u7684\u6bd4\u8f83\u3002(c) MEA\u548cHEA\u4e2d\u7684\u7535\u5b50\u5bc6\u5ea6\u5206\u5e03\u3002(d) HEA-NC\u754c\u9762\u5904\u5dee\u5206\u7535\u8377\u5bc6\u5ea6\uff08CDD\uff09\u56fe\u3002(e) \u7535\u5b50\u4f20\u8f93\u8def\u5f84\u793a\u610f\u56fe\u3002(f) HEA-NC\u5728\u6790\u6c22\u53cd\u5e94HER\u4e2d\u7684\u793a\u610f\u56fe\u3002(g) <a>HEA-NC\u5728<\/a>IRR\u50ac\u5316\u4e2d<a>\u7684\u793a\u610f\u56fe<\/a>\u3002<\/p>\n\n\n\n<p>\u603b\u4e4b\uff0c\u201cBTC\u8f85\u52a9\u5408\u6210\u201d\u7b56\u7565\u5b9e\u73b0\u4e86FeCrCoCuMn\u9ad8\u71b5\u5408\u91d1\u5728BTC\u884d\u751f\u6c2e\u63ba\u6742\u78b3\u4e0a\u7684\u539f\u4f4d\u751f\u957f\uff0c\u5e76\u83b7\u5f97\u4e86\u591a\u91d1\u5c5e\u6d3b\u6027\u4f4d\u70b9\u7684\u5747\u5300\u5206\u5e03\u3002\u7efc\u5408UPS\u3001XPS\u548cDFT\u5206\u6790\u8bc1\u5b9e\uff0cHEA-NC\u754c\u9762\u5904\u5b58\u5728\u5b9a\u5411\u5185\u5efa\u7535\u573a\uff0c\u8be5\u7535\u573a\u9a71\u52a8\u4e86\u9ad8\u6548\u7535\u8377\u8f6c\u79fb\u5e76\u52a0\u901f\u4e86\u7535\u50ac\u5316\u52a8\u529b\u5b66\u3002Mn\u7684\u5f15\u5165\u5f15\u8d77\u9ad8\u71b5\u5408\u91d1\u7684\u7535\u5b50\u53d8\u5316\uff0c\u4f18\u5316\u4e86\u8868\u9762\u6d3b\u6027\u4f4d\u70b9\u7684\u7535\u5b50\u7ed3\u6784\uff0c\u5e76\u901a\u8fc7\u754c\u9762\u8026\u5408\u5b9e\u73b0\u4e86\u9ad8\u71b5\u5408\u91d1\u4e0eNC\u8f7d\u4f53\u4e4b\u95f4\u7684\u7535\u8377\u8c03\u63a7\u3002\u8be5\u7b56\u7565\u6539\u5584\u4e86\u4e09\u7ef4\u516b\u9762\u4f53\u7ed3\u6784\u5185\u7684\u4f20\u8d28\uff0c\u6784\u5efa\u4e86\u53cc\u901a\u8def\u7535\u5b50\u4f20\u8f93\u7cfb\u7edf\uff0c\u4ece\u800c\u663e\u8457\u63d0\u5347\u4e86\u50ac\u5316\u6027\u80fd\u3002\u5bf9\u4e8e\u6790\u6c22\u53cd\u5e94\uff0cHEA-NC\u50ac\u5316\u5242\u572810 mA cm\u207b\u00b2\u4e0b\u663e\u793a\u51fa99 mV\u7684\u8fc7\u7535\u4f4d\u548c64 mV dec<sup>-1<\/sup>\u7684\u5854\u83f2\u5c14\u659c\u7387\u3002\u57fa\u4e8eHEA-NC\u5bf9\u7535\u6781\u7684\u592a\u9633\u80fd\u5149\u4f0f\u5668\u4ef6\uff0c\u5728\u4e09\u7898\u5316\u7269\u8fd8\u539fIRR\u548c\u94dc\u8fd8\u539f\u53cd\u5e94CRR\u4e2d\u5206\u522b\u83b7\u5f97\u4e868.52%\u548c5.82%\u7684\u5149\u7535\u8f6c\u6362\u6548\u7387\uff0c\u6027\u80fd\u4f18\u4e8ePt\u57fa\u5bf9\u7535\u6781\u3002\u672c\u7814\u7a76\u4e3a\u6784\u5efa\u57fa\u4e8eMOF\u884d\u751f\u9ad8\u71b5\u5408\u91d1\u7684\u9ad8\u6548\u53cc\u529f\u80fd\u7535\u50ac\u5316\u5242\u63d0\u4f9b\u4e86\u4e00\u79cd\u53ef\u884c\u7684\u8bbe\u8ba1\u8303\u5f0f\uff0c\u4e3a\u9ad8\u6548\u7684\u6e05\u6d01\u80fd\u6e90\u8f6c\u5316\u5960\u5b9a\u4e86\u575a\u5b9e\u7684\u6750\u6599\u57fa\u7840\u3002<\/p>\n\n\n\n<p><strong>\u3010\u6587\u7ae0\u94fe\u63a5\u3011<\/strong><strong><\/strong><\/p>\n\n\n\n<p><a><\/a>Internal Electric Field Engineered High-Entropy Alloy on Octahedral N-Doped Carbon via Electronegativity Gradient: Synergistic Interfaces Accelerating Hydrogen Evolution and Triiodide\/Copper Reduction Reactions<\/p>\n\n\n\n<p><a><\/a>Juntao Wang, Sining Yun,* Tianxiang Yang, Leifei Wang, Yang Yang, Zhiguo Wang, Haijiang Yang, Rou Feng,&nbsp;Ting&nbsp;Lu and Zechang Liu<\/p>\n\n\n\n<p><a href=\"https:\/\/doi.org\/10.1039\/d6ta02832b\">https:\/\/doi.org\/10.1039\/d6ta02832b<\/a><\/p>\n\n\n\n<p><strong>\u3010\u901a\u8baf\u4f5c\u8005\u7b80\u4ecb\u3011<\/strong><strong><\/strong><\/p>\n\n\n\n<p>\u4e91\u65af\u5b81\uff0c\u897f\u5b89\u5efa\u7b51\u79d1\u6280\u5927\u5b66\uff0c\u4e8c\u7ea7\u6559\u6388\uff0c\u535a\u58eb\u751f\u5bfc\u5e08\uff0c\u9655\u897f\u7701\u4e2d\u9752\u5e74\u79d1\u6280\u521b\u65b0\u9886\u519b\u4eba\u624d\uff0c\u9655\u897f\u7701\u201c\u7279\u652f\u8ba1\u5212\u201d\u79d1\u6280\u521b\u65b0\u9886\u519b\u4eba\u624d\uff0c\u9655\u897f\u7701\u91cd\u70b9\u79d1\u6280\u521b\u65b0\u56e2\u961f\u5e26\u5934\u4eba\uff0c\u9655\u897f\u7701\u9ad8\u7b49\u5b66\u6821\u5b66\u79d1\u521b\u65b0\u57fa\u5730\u8d1f\u8d23\u4eba\u3002\u8fde\u7eed7\u5e74\u5165\u9009&nbsp;\u201c\u5168\u7403\u524d2%\u9876\u5c16\u79d1\u5b66\u5bb6\u699c\u5355(World&#8217;s Top 2% Scientists)\u201d\uff0c\u5165\u9009\u201c\u7ec8\u8eab\u79d1\u5b66\u5f71\u54cd\u529b\u6392\u884c\u699c\u201d\u548c\u201c\u79d1\u5b66\u5f71\u54cd\u529b\u6392\u884c\u699c\u201d\u3002\u535a\u58eb\u6bd5\u4e1a\u4e8e\u897f\u5b89\u4ea4\u901a\u5927\u5b66\uff0c\u6b64\u540e\u5206\u522b\u5728\u97e9\u56fd\u5ef6\u4e16\u5927\u5b66\u3001\u7f8e\u56fd\u65af\u5766\u798f\u5927\u5b66\u3001\u7f8e\u56fd\u52a0\u5dde\u5927\u5b66\u3001\u7f8e\u56fd\u52b3\u4f26\u65af\u4f2f\u514b\u5229\u56fd\u5bb6\u5b9e\u9a8c\u5ba4\u3001\u82f1\u56fd\u91cc\u4e01\u5927\u5b66\u3001\u745e\u58eb\u6d1b\u6851\u8054\u90a6\u7406\u5de5\u5b66\u9662\u7b49\u8bbf\u95ee\u3001\u4ea4\u6d41\u4e0e\u5b66\u4e60\u3002\u76ee\u524d\u4e3b\u8981\u4ece\u4e8b\u65b0\u80fd\u6e90\u6750\u6599\u9ad8\u6548\u548c\u8d44\u6e90\u5316\u5229\u7528\u7814\u7a76\uff0c\u5982\u65b0\u4e00\u4ee3\u592a\u9633\u7535\u6c60\u3001\u71c3\u6599\u7535\u6c60\u3001\u8d85\u7ea7\u7535\u5bb9\u5668\u3001\u751f\u7269\u50ac\u5316\u3001\u5236\u6c22\u3001\u591a\u80fd\u4e92\u8865\u7b49\u3002\u4e3b\u6301\u79d1\u6280\u90e8\u56fd\u5bb6\u91cd\u70b9\u7814\u53d1\u8ba1\u5212\uff08\u6c22\u80fd\u4e13\u9879\uff09\u3001\u56fd\u5bb6\u5341\u4e8c\u4e94\u79d1\u6280\u652f\u6491\u8ba1\u5212\u3001\u56fd\u5bb6NSFC\u9762\u4e0a\u3001\u9655\u897f\u7701\u91cd\u70b9\u7814\u53d1\u8ba1\u5212\u3001\u9655\u897f\u7701\u56fd\u9645\u5408\u4f5c\u91cd\u70b9\u7b4920\u4f59\u9879\u79d1\u7814\u8bfe\u9898\u3002\u5728Chem Sov Rev, Prog Polym Sci, Energy Environ Sci, Electrochem Energy Rev, Adv Mater, Adv Energy Mater, Adv Funct Mater, Adv Powder Mater, ACS Energy Lett, Appl Catal B-Environ, Nano Energy, Angew Chem Int Edit, Renew Sust Energy Rev, J Mater Chem A, Chem Eng J, Small, Materials Today\u7cfb\u5217\u7b49\u56fd\u9645\u671f\u520a\u53d1\u8868\u8bba\u6587270\u4f59\u7bc7\uff08IF&gt;10\u7684\u8bba\u6587100\u4f59\u7bc7\uff09\uff0cH-\u56e0\u5b5071\uff0c\u5148\u540e\u670927\u7bc7\u8bba\u6587\u5165\u9009ESI\u70ed\u70b9\/\u9ad8\u88ab\u5f15\u8bba\u6587\uff1b\u4e3b\u7f16\/\u53c2\u7f16\u4e2d\u3001\u82f1\u6587\u4e13\u8457\/\u6559\u675013\u90e8\uff1b\u62e5\u670930\u9879\u56fd\u5bb6\u6388\u6743\u4e13\u5229\u6280\u672f\u30022016\u5e74\u83b7\u201cWiley\u6750\u6599\u5b66\u9ad8\u5cf0\u8bba\u575b-\u897f\u5b89\u201dHighly-cited Author Award\u30022017\u5e74\u83b7\u4e2d\u56fd\u56fd\u9645\u5149\u4f0f\u5927\u4f1aBest Presentation Award\u5956\u30022017-2023\u5e74\uff0c\u5148\u540e\u83b7\u9655\u897f\u7701\u79d1\u5b66\u6280\u672f\u8fdb\u6b65\u5956\u4e00\u7b49\u5956\u3001\u9655\u897f\u7701\u79d1\u5b66\u6280\u672f\u5956\u4e8c\u7b49\u5956\u3001\u9655\u897f\u9ad8\u7b49\u5b66\u6821\u79d1\u5b66\u6280\u672f\u7814\u7a76\u4f18\u79c0\u6210\u679c\u5956\u7279\u7b49\u5956\u3001\u9655\u897f\u9ad8\u7b49\u5b66\u6821\u79d1\u5b66\u6280\u672f\u5956\u4e00\u7b49\u5956\u3001\u5185\u8499\u53e4\u81ea\u6cbb\u533a\u79d1\u6280\u8fdb\u6b65\u4e8c\u7b49\u5956\u7b49\u3002\u5148\u540e\u62c5\u4efb\u56fd\u9645\u671f\u520aInternational Journal of Hydrogen Energy\u548cRenewable &amp; Sustainable Energy Reviews\u5ba2\u5ea7\u7f16\u8f91\uff08Guest Editor\u56fd\u9645\u671f\u520a\uff09\u3002\u76ee\u524d\u62c5\u4efbInternational Journal of Green Energy, Oxford Open Energy\u7b49\u7f16\u59d4\uff1b\u76ee\u524d\u62c5\u4efbESCI\u56fd\u9645\u671f\u520aEnergy Materials\uff08\u5f71\u54cd\u56e0\u5b5011.8\uff09\u526f\u4e3b\u7f16\uff1b170\u4f59\u79cd\u4e3b\u8981\u56fd\u9645SCI\u5b66\u672f\u671f\u520a\u7684\u7279\u9080\u5ba1\u7a3f\u548c\u4ef2\u88c1\u4e13\u5bb6\u3002\u4e3b\u529e\u3001\u627f\u529e\u56fd\u5185\u5916\u65b0\u80fd\u6e90\u6750\u6599\u76f8\u5173\u7684\u7ebf\u4e0b\u3001\u7ebf\u4e0a\u4f1a\u8bae20\u4f59\u6b21\uff0c\u62c5\u4efb\u5927\u4f1a\u4e3b\u5e2d\u3001\u5927\u4f1a\u5171\u540c\u4e3b\u5e2d\uff0c\u53d7\u9080\u5728\u56fd\u5185\u5916\u4f1a\u8bae\u505a\u5927\u4f1a\u62a5\u544a\u3001\u4e3b\u65e8\u62a5\u544a\u3001\u7279\u9080\u62a5\u544a\u3001\u9080\u8bf7\u62a5\u544a80\u4f59\u6b21\u3002<\/p>\n\n\n\n<p>\u66f4\u591a\u8be6\u60c5\uff0c\u8bf7\u8bbf\u95ee\u897f\u5b89\u5efa\u7b51\u79d1\u6280\u5927\u5b66\u5bfc\u5e08\u4e3b\u9875\u548c\u8bfe\u9898\u7ec4\u4e3b\u9875<\/p>\n\n\n\n<p><a href=\"https:\/\/xajzkj.teacher.360eol.com\/teacherBasic\/preview?teacherId=21532\">https:\/\/xajzkj.teacher.360eol.com\/teacherBasic\/preview?teacherId=21532<\/a><\/p>\n\n\n\n<p><a href=\"https:\/\/www.x-mol.com\/groups\/Sining_Yun\">https:\/\/www.x-mol.com\/groups\/Sining_Yun<\/a><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u6587\u7ae0\u4fe1\u606f\u3011 \u5de7\u501f\u7535\u8d1f\u6027\u68af\u5ea6\u6784\u7b51\u5185\u5efa\u7535\u573a\u7684\u9ad8\u71b5\u5408\u91d1\u951a\u5b9a\u516b\u9762\u4f53\u6c2e\u63ba\u6742\u78b3\uff1a\u534f\u540c\u754c\u9762\u52a0\u901f\u6790\u6c22\u53ca\u4e09\u7898\u5316\u7269\/\u94dc\u8fd8\u539f\u53cd\u5e94 \u7b2c\u4e00\u4f5c\u8005\uff1a\u738b\u6d5a\u97ec \u901a\u8baf\u4f5c\u8005\uff1a\u4e91\u65af\u5b81* \u5355\u4f4d\uff1a\u897f\u5b89\u5efa&#8230;<\/p>\n","protected":false},"author":31345,"featured_media":0,"comment_status":"open","ping_status":"","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-272727","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/272727"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/31345"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=272727"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/272727\/revisions"}],"predecessor-version":[{"id":272738,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/272727\/revisions\/272738"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=272727"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=272727"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=272727"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}