{"id":28188,"date":"2016-07-22T08:00:11","date_gmt":"2016-07-22T00:00:11","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=28188"},"modified":"2016-09-28T13:42:03","modified_gmt":"2016-09-28T05:42:03","slug":"%e5%8f%a6%e4%b8%80%e7%a7%8d%e7%a5%9e%e5%a5%87%e7%9a%84%e5%ad%98%e5%9c%a8%ef%bc%9a%e8%8b%8f%e8%81%94%e5%86%9b%e5%b7%a5%e6%9d%90%e6%96%99%e5%ba%94%e7%94%a8%e8%89%ba%e6%9c%af","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=28188","title":{"rendered":"\u53e6\u4e00\u79cd\u795e\u5947\u7684\u5b58\u5728\uff1a\u82cf\u8054\u519b\u5de5\u6750\u6599\u5e94\u7528\u827a\u672f\u4e4b\u7f8e"},"content":{"rendered":"<p>\u63d0\u8d77\u82cf\u8054\u548c\u7ee7\u627f\u8005\u4fc4\u7f57\u65af\uff0c\u5f88\u591a\u4eba\u620f\u79f0\u201c\u6218\u6597\u79cd\u65cf\u201d\u3001\u201c\u6bdb\u5b50\u201d\u3001\u201c\u6bdb\u718a\u201d\u3002\u5b83\u7684\u5de5\u4e1a\u54c1\u4e5f\u5e38\u88ab\u5f88\u591a\u4eba\u770b\u4f5c\u7c97\u7ebf\u6761\u6216\u8005\u201c\u50bb\u5927\u9ed1\u201d\uff0c\u8fd8\u662f\u7cbe\u81f4\u7684\u5fb7\u56fd\u8d27\u3001\u7f8e\u56fd\u8d27\u66f4\u5165\u201c\u6cd5\u773c\u201d\u3002\u8bda\u7136\uff0c\u82cf\u8054\u7684\u5de5\u4e1a\u54c1\u5236\u9020\u548c\u8bbe\u8ba1\u601d\u8def\u8fe5\u5f02\u4e8e\u5fb7\u56fd\u3001\u7f8e\u56fd\uff0c\u4f46\u53ef\u4ee5\u8bf4\u662f\u53e6\u4e00\u79cd\u7f8e\u3002<\/p>\n<p>\u6bd4\u5982\u5728\u82cf\u8054\u7684\u652f\u67f1\u4ea7\u4e1a\u519b\u5de5\u4e0a\uff0c\u6709\u8fd9\u6837\u4e00\u4e9b\u4f8b\u5b50\uff1a\u6216\u8bb8\u5728\u65b0\u6750\u6599\u53ca\u5176\u5236\u5907\u52a0\u5de5\u4e0a\u4e0e\u6b27\u7f8e\u6709\u5dee\u8ddd\uff0c\u4f46\u5f97\u76ca\u4e8e\u9b3c\u624d\u822c\u7684\u8bbe\u8ba1\uff0c\u4e00\u6837\u6027\u80fd\u5353\u8d8a\u3002<\/p>\n<p><strong>\u7c73\u683c-25<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-28192\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/mig25.jpg\" alt=\"mig25\" width=\"700\" height=\"450\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/mig25.jpg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/mig25-300x193.jpg 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u8fd9\u662f\u4e00\u6b3e\u6781\u5176\u7279\u522b\u7684\u98de\u673a\uff0c\u751a\u81f3\u53ef\u4ee5\u8bf4\u662f\u4e00\u6735\u5947\u8469\uff0c\u5b83\u5c31\u662f\u524d\u82cf\u8054\u7c73\u9ad8\u626c\u8bbe\u8ba1\u5c40\u8bbe\u8ba1\u7684\u7c73\u683c-25\u3002<\/p>\n<p>\u8fd9\u662f\u4e00\u79cd\u9ad8\u7a7a\u9ad8\u901f\u7684\u622a\u51fb\u673a\uff0c\u6700\u5f00\u59cb\u662f\u4e13\u95e8\u4e3a\u4e86\u9488\u5bf9\u7f8e\u56fd\u7684\u201c\u9ed1\u9e1f\u201d\u9ad8\u7a7a\u9ad8\u901f\u4fa6\u5bdf\u673a\u800c\u5236\u3002\u7814\u5236\u6210\u529f\u540e\uff0c\u5b83\u7684\u9ad8\u7a7a\u9ad8\u901f\u6027\u80fd\u751a\u4e3a\u8000\u773c\uff1a\u6700\u5927\u98de\u884c\u901f\u5ea6\u8fbe3\u9a6c\u8d6b\uff08\u4e00\u8bf43.2\u9a6c\u8d6b\uff09\uff0c\u53ef\u572824000\u7c73\u9ad8\u5ea62.8\u9a6c\u8d6b\u6301\u7eed\u98de\u884c\u3002\u662f\u4e16\u754c\u4e0a\u552f\u4e8c\u7684\u8d85\u8fc7\u95ef\u8fc7\u201c\u70ed\u969c\u201d\uff082.5\u9a6c\u8d6b\uff09\u7684\uff0c\u6709\u4eba\u9a7e\u9a76\uff0c\u6b63\u5f0f\u4ea4\u4ed8\u7684\u98de\u673a\uff08\u53e6\u4e00\u79cd\u662f\u9ed1\u9e1f\uff09\u3002<\/p>\n<p>\u8981\u8bf43\u9a6c\u8d6b\u6709\u4ec0\u4e48\u7a00\u5947\u7684\uff1f\u822a\u5929\u98de\u673a\u5206\u5206\u949f\u6559\u4f60\u5982\u4f55\u505a\u673a\uff01<\/p>\n<p>\u5176\u5b9e\u96be\u5ea6\u8fd8\u662f\u975e\u5e38\u5927\u7684\uff01\u8d85\u8fc72.5\u9a6c\u8d6b\u7684\u98de\u673a\uff0c\u90fd\u8981\u9762\u4e34\u4e00\u4e2a\u95ee\u9898\u2014\u2014\u201c\u70ed\u969c\u201d\u3002\u6240\u8c13\u70ed\u969c\uff0c\u662f\u9ad8\u901f\u98de\u884c\u7684\u98de\u673a\u4e0e\u7a7a\u6c14\u6469\u64e6\uff0c\u5bfc\u81f4\u673a\u4f53\u5916\u8868\u6e29\u5ea6\u8fc5\u901f\u4e0a\u5347\u3002\u8d85\u8fc72.5\u9a6c\u8d6b\u4e4b\u540e\uff0c\u98de\u673a\u8868\u9762\u6e29\u5ea6\u5c06\u8d85\u8fc7200\u5ea6\uff0c\u8d85\u8fc73\u9a6c\u8d6b\u5219\u8fbe\u5230300\u5ea6\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-28191 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/image.jpg\" width=\"740\" height=\"529\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/image.jpg 740w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/image-300x214.jpg 300w\" sizes=\"(max-width: 740px) 100vw, 740px\" \/><\/p>\n<p style=\"text-align: center;\">\u7f8e\u56fd\u9ed1\u9e1f\u4fa6\u5bdf\u673a\u57283\u9a6c\u8d6b\u901f\u5ea6\u4e0b\u7684\u673a\u4f53\u8868\u9762\u6e29\u5ea6<\/p>\n<p>\u8981\u8bf4300\u5ea6\u4e5f\u4e0d\u662f\u4ec0\u4e48\u9ad8\u6e29\uff0c\u8010\u5f97\u4e86\u8fd9\u4e2a\u6e29\u5ea6\u7684\u6bd4\u6bd4\u7686\u662f\u3002\u4f46\u5bf9\u4e8e\u98de\u673a\u8868\u9762\u6240\u4f7f\u7528\u7684\u94dd\u5408\u91d1\u6765\u8bf4\uff0c\u8fd9\u5c31\u662f\u81f4\u547d\u6e29\u5ea6\u3002\u5373\u4f7f\u662f\u9ad8\u5f3a\u5ea6\u7684\u94dd\u5408\u91d1\uff0c\u7194\u70b9\u4e5f\u4e0d\u8fc7500\u5ea6\u3002\u8d85\u8fc7300\u5ea6\u7684\u9ad8\u6e29\uff0c\u94dd\u5408\u91d1\u7684\u786c\u5ea6\u4f1a\u6025\u5267\u4e0b\u964d\uff0c\u65e0\u6cd5\u4f5c\u4e3a\u7ed3\u6784\u4ef6\uff0c\u66f4\u4f55\u51b5\u8fd8\u6709\u9ad8\u901f\u5e26\u6765\u7684\u538b\u5f3a\u3002<\/p>\n<p>\u8981\u7528\u4ec0\u4e48\u6750\u6599\u6765\u89e3\u51b3\u8fd9\u4e2a\u95ee\u9898\uff1f\u5f53\u65f6\u4e24\u4e2a\u8d85\u7ea7\u5927\u56fd\u4ea4\u51fa\u4e86\u8fe5\u5f02\u7684\u7b54\u6848\u3002<\/p>\n<p>\u8d22\u5927\u6c14\u7c97\u7684\u7f8e\u56fd\u4f6c\u7528\u7684\u662f\u949b\u5408\u91d1\u3002\u4ece\u6027\u80fd\u4e0a\u770b\uff0c\u949b\u5408\u91d1\u7684\u8010\u9ad8\u6e29\u6027\u8981\u6bd4\u94dd\u9ad8\u51fa\u51e0\u4e2a\u6bb5\u4f4d\uff0c\u5176\u5b83\u6027\u80fd\u4e5f\u975e\u5e38\u4f18\u8d8a\uff0c\u81ea\u7136\u662f\u6ca1\u95ee\u9898\u7684\u3002\uff08\u5176\u5b9e\u4e5f\u6709\u95ee\u9898\uff0c\u5168\u949b\u98de\u673a\u53ea\u662f\u770b\u8d77\u6765\u5f88\u7f8e\uff09<\/p>\n<p>\u4e0d\u8fc7\uff0c\u949b\u5408\u91d1\u7684\u52a0\u5de5\u5de5\u827a\u96be\u5ea6\u7cfb\u6570\u5f88\u9ad8\uff0c\u5373\u4f7f\u662f\u4eca\u5929\u4e5f\u6ca1\u4ec0\u4e48\u592a\u597d\u7684\u529e\u6cd5\u3002\u800c\u4e14\u5b83\u8fd8\u6709\u4e2a\u6bdb\u75c5\u2014\u2014\u8d35\u3002\u82cf\u8054\u5728\u949b\u5408\u91d1\u52a0\u5de5\u4e0a\u7565\u5dee\uff0c\u5373\u4f7f\u5b83\u7684\u949b\u77ff\u85cf\u4e30\u5bcc\uff0c\u800c\u4e14\u6ca1\u6709\u90a3\u4e48\u8d22\u5927\u6c14\u7c97\u3002\uff08\u4e0d\u8fc7\uff0c\u8981\u8bf4\u82cf\u8054\u9020\u4e0d\u51fa\u5168\u949b\u98de\u673a\u4e5f\u4e0d\u80fd\u8fd9\u4e48\u7edd\u5bf9\u3002\u540e\u6765\u4e5f\u7814\u5236\u4e86T-4\u5927\u91cf\u4f7f\u7528\u949b\u5408\u91d1\u7684\u98de\u673a\uff0c\u4e0d\u8fc7\u5982\u679c\u91c7\u7528\u949b\u5408\u91d1\uff0c\u7c73\u683c25\u53ef\u80fd\u8981\u665a\u51fa\u6765\u597d\u51e0\u5e74\uff0c\u9020\u4ef7\u592a\u6602\u8d35\uff0c\u4e0d\u7b26\u5408\u82cf\u8054\u7684\u98ce\u683c\uff09<\/p>\n<p>\u94dd\u5408\u91d1\u7528\u4e0d\u4e86\uff0c\u949b\u5408\u91d1\u505a\u4e0d\u5230\uff0c\u8be5\u7528\u4ec0\u4e48\u6750\u6599\u4e3a\u597d\uff1f\u82cf\u8054\u8bbe\u8ba1\u5e08\u4eec\u60f3\u5230\u7528\u4e0d\u9508\u94a2\u3002<\/p>\n<p>\u7528\u4e0d\u9508\u94a2\u4f5c\u4e3a\u673a\u4f53\u6750\u6599\uff0c\u957f\u671f\u4ee5\u6765\u662f\u7c73\u683c25\u7684\u79d8\u5bc6\u3002\u6b27\u7f8e\u4e00\u76f4\u4ee5\u4e3a\u7c73\u683c25\u4e5f\u7528\u7684\u662f\u949b\u5408\u91d1\uff0c\u76f4\u5230\u4e00\u540d\u82cf\u8054\u98de\u884c\u5458\u67b6\u673a\u53db\u9003\uff0c\u624d\u604d\u7136\u5927\u609f\u3002<\/p>\n<p>\u4e3a\u4ec0\u4e48\u6b27\u7f8e\u6ca1\u6709\u60f3\u5230\u7528\u4e0d\u9508\u94a2\uff1f<\/p>\n<p>\u4e0d\u9508\u94a2\u8010300\u5ea6\u6e29\u5ea6\u81ea\u7136\u4e0d\u5728\u8bdd\u4e0b\uff0c\u4e0d\u8fc7\u5b83\u5b9e\u5728\u592a\u91cd\u4e86\u3002\u94a2\u7684\u5bc6\u5ea6\u4e3a 7.9 \u5428\/\u7acb\u65b9\u7c73\uff0c\u51e0\u4e4e\u662f\u94dd\u5408\u91d1\uff082.7 \u5428\/\u7acb\u65b9\u7c73\uff09\u7684\u4e09\u500d\uff0c\u949b\u5408\u91d1\uff084.5 \u5428\/\u7acb\u65b9\u7c73\uff09\u7684\u4e00\u500d\u591a\u3002<\/p>\n<p>\u56e0\u6b64\uff0c\u94a2\u4f5c\u4e3a\u5927\u89c4\u6a21\u673a\u8eab\u6750\u6599\u7684\u65f6\u95f4\u5f88\u77ed\u3002\u65e9\u5728\u6218\u6597\u673a\u8bde\u751f\u7684\u65e9\u671f\uff0c\u98de\u673a\u673a\u8eab\u5c31\u629b\u5f03\u94a2\u6750\u6295\u5411\u94dd\u5408\u91d1\u6000\u62b1\u3002<\/p>\n<p>\u7c73\u683c25\u7684\u673a\u7ffc\u9664\u4e86\u524d\u7f18\u90e8\u5206\u4e3a\u949b\u5408\u91d1\u5916\uff0c\u673a\u7ffc\u4e3b\u4f53\u7ed3\u6784\u5747\u4f7f\u7528\u954d\u57fa\u4e0d\u9508\u94a2\u6750\u6599\uff0c\u91c7\u7528\u5168\u710a\u63a5\u6210\u578b\u7684\u590d\u6742\u94a2\u7ed3\u6784\u3002\u673a\u7ffc\u7684\u5185\u90e8\u7ed3\u6784\u548c\u578b\u6750\u4e5f\u5927\u90fd\u4f7f\u7528\u954d\u57fa\u4e0d\u9508\u94a2\u677f\u6750\u3002<\/p>\n<p>\u4e3a\u4e86\u5c3d\u53ef\u80fd\u51cf\u91cd\uff0c\u7c73\u683c25\u673a\u8eab\u505a\u5f97\u6bd4\u8f83\u8584\uff0c\u5373\u4f7f\u662f\u8fd9\u6837\uff0c\u5b83\u4ecd\u7136\u6709\u7a7a\u91cd\u8fbe\u5230\u4e86 19.6 \u5428\u3002\u5938\u5f20\u4e00\u70b9\u5730\u8bf4\uff0c\u7c73\u683c25\u5c31\u662f\u4e00\u5768\u80fd\u4ee53\u9a6c\u8d6b\u98de\u884c\u7684\u4e0d\u9508\u94a2\u3002<\/p>\n<p>\u91cd\u662f\u91cd\u4e86\u70b9\uff0c\u800c\u4e14\u4ece\u9020\u578b\u6765\u770b\uff0c\u786e\u5b9e\u592a\u4e11\u4e86\u70b9\uff0c\u6bd4\u8d77\u7f8e\u56fd\u9ed1\u9e1f\u90a3\u5dee\u5f97\u4e0d\u662f\u4e00\u661f\u534a\u70b9\u3002\u4e0d\u8fc7\uff0c\u82cf\u8054\u4eba\u4e0d\u5728\u4e4e\u8fd9\u4e2a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-28202 alignnone aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/sr71.jpg\" alt=\"sr71\" width=\"740\" height=\"403\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/sr71.jpg 740w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/sr71-300x163.jpg 300w\" sizes=\"(max-width: 740px) 100vw, 740px\" \/><\/p>\n<p style=\"text-align: left;\">\u9ed1\u9e1f\u9020\u578b\u4e4b\u7280\u5229\uff0c\u4f60\u5f88\u96be\u60f3\u8c61\u8fd9\u662f50\u5e74\u524d\u7684\u53e4\u8463<\/p>\n<p>\u4e0d\u540c\u4e8e\u7f8e\u56fd\u9ed1\u9e1f\uff0c\u7c73\u683c25\u662f\u6210\u672c\u3001\u6027\u80fd\u548c\u4f7f\u7528\u5e73\u8861\u7684\u4ea7\u7269\uff0c\u4e0d\u4ec5\u5728\u98de\u884c\u901f\u5ea6\u548c\u98de\u884c\u9ad8\u5ea6\u4e0a\u4e0d\u901e\u591a\u8ba9\uff0c\u5728\u6210\u672c\u3001\u4f7f\u7528\u4e0a\u66f4\u662f\u7529\u524d\u8005\u51e0\u6761\u8857\u3002<\/p>\n<p>\u949b\u98de\u673a\u81ea\u7136\u8981\u6bd4\u94a2\u98de\u673a\u8d35\u5f88\u591a\uff0c\u6240\u4ee5\u9ed1\u9e1f\u4e00\u76f4\u6ca1\u6709\u91cf\u4ea7\u3002\u800c\u7c73\u683c25\u5219\u6210\u4e3a\u4e00\u6b3e\u5927\u89c4\u6a21\u4f7f\u7528\u7684\u98de\u673a\uff0c\u603b\u4ea7\u91cf\u6570\u4ee5\u5343\u8ba1\uff0c\u4e0d\u4f46\u82cf\u8054\u88c5\u5907\uff0c\u8fd8\u5916\u9500\u4ed6\u56fd\u3002<\/p>\n<p>\u4e0d\u53ea\u662f\u9020\u4ef7\u9ad8\uff0c\u9ed1\u9e1f\u7684\u7ef4\u62a4\u4fdd\u517b\u8fd8\u975e\u5e38\u7e41\u6742\u3001\u9ad8\u6602\uff0c\u65e0\u6cd5\u627f\u62c5\u9ad8\u5f3a\u5ea6\u4f5c\u4e1a\u3002\u800c\u7c73\u683c25\u53ef\u4ee5\u76f4\u63a5\u505c\u5728\u5916\u9762\u627f\u53d7\u98ce\u5439\u96e8\u6253\uff0c\u4e0d\u4f46\u9ad8\u5f3a\u5ea6\u4f7f\u7528\u4e0d\u5728\u8bdd\u4e0b\uff0c\u7ef4\u62a4\u4fdd\u517b\u96be\u5ea6\u4e5f\u975e\u5e38\u4f4e\u3002<\/p>\n<p>\u7531\u4e8e\u672a\u80fd\u89e3\u51b3\u6750\u6599\u53d7\u70ed\u81a8\u80c0\u5bfc\u81f4\u71c3\u6599\u6cc4\u9732\uff0c\u9ed1\u9e1f\u9700\u8981\u91c7\u7528\u9ad8\u71c3\u70b9\u7684\u71c3\u6599\uff0c\u800c\u4e14\u5f80\u5f80\u9700\u8981\u5728\u5347\u7a7a\u540e\uff0c\u7ecf\u8fc7\u7a7a\u4e2d\u52a0\u6cb9\u3002\u8fd9\u5728\u7c73\u683c25\u6765\u8bf4\u4e5f\u6ca1\u8fd9\u56de\u4e8b\u3002<\/p>\n<p>\u867d\u7136\u4f17\u591a\u9ed1\u79d1\u6280\u508d\u8eab\uff0c\u9ed1\u9e1f\u81ea\u670d\u5f79\u8d77\u4e5f\u786e\u5b9e\u505a\u5230\u4e86\u6765\u53bb\u81ea\u5982\u672a\u88ab\u51fb\u843d\uff0c\uff08\u867d\u7136\u7c73\u683c25\u8bbe\u8ba1\u4e4b\u521d\u5c31\u662f\u4e3a\u4e86\u62e6\u622a\u9ed1\u9e1f\uff0c\u4e0d\u8fc7\u6027\u80fd\u4e0a\u786e\u5b9e\u5dee\u4e00\u4e9b\uff0c\u62e6\u622a\u5e76\u4e0d\u6210\u529f\uff09\uff0c\u4f46\u9ad8\u5927\u4e0a\u7684\u9ed1\u9e1f\u4f46\u5374\u6709\u5f88\u5927\u6bd4\u4f8b\u56e0\u4e3a\u6545\u969c\u800c\u5760\u6bc1\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-28215\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/az_mig-25r_4_l.jpg\" alt=\"az_mig-25r_4_l\" width=\"740\" height=\"493\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/az_mig-25r_4_l.jpg 740w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/az_mig-25r_4_l-300x200.jpg 300w\" sizes=\"(max-width: 740px) 100vw, 740px\" \/><\/p>\n<p>\u867d\u7136\uff0c\u7c73\u683c25\u6ca1\u6709\u9ed1\u9e1f\u90a3\u6837\u53ef\u4ee5\u57283\u9a6c\u8d6b\u4e0b\u957f\u671f\u98de\u884c\uff0c\u4e5f\u56e0\u4e3a\u592a\u91cd\u4f5c\u6218\u534a\u5f84\u6bd4\u8f83\u7a84\uff0c\u4e2d\u4f4e\u7a7a\u673a\u52a8\u6027\u8f83\u5dee\u3002\u4f46\u5b83\u540c\u6837\u53ef\u4ee5\u6500\u722c\u5230\u4e0e\u9ed1\u9e1f\u540c\u7b49\u6c34\u5e73\u7684\u9ad8\u5ea6\uff0c\u800c\u4e14\u540c\u6837\u53ef\u4ee5\u501f\u52a9\u9ad8\u7a7a\u9ad8\u901f\u6765\u53bb\u81ea\u5982\u5b8c\u6210\u4fa6\u5bdf\u4efb\u52a1\u3002<\/p>\n<p>\u82cf\u8054\u8bbe\u8ba1\u5e08\u4eec\u5408\u7406\u89e3\u51b3\u95ee\u9898\u7684\u4e3b\u8981\u77db\u76fe\u548c\u6b21\u8981\u77db\u76fe\uff0c\u5408\u7406\u5229\u7528\u73b0\u6709\u7684\u6750\u6599\u548c\u6280\u672f\uff0c\u6700\u7ec8\u6253\u9020\u51fa\u4e00\u6b3e\u53ef\u4ee5\u51fa\u8272\u5b8c\u6210\u622a\u51fb\u548c\u4fa6\u5bdf\u4efb\u52a1\u7684\u98de\u673a\u3002<\/p>\n<p><strong>\u4e09\u660e\u6cbb\u5766\u514b\u88c5\u7532<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-28212\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/T-64\u0410.jpg\" alt=\"T-64\u0410\" width=\"800\" height=\"509\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/T-64\u0410.jpg 800w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/T-64\u0410-300x191.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/T-64\u0410-768x489.jpg 768w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/p>\n<p>\u8bf4\u8d77\u82cf\u8054\u7684\u5766\u514b\uff0c\u7ecf\u5e38\u6d41\u4f20\u7740\u5b83\u4e0e\u5fb7\u56fd\u5766\u514b\u5bf9\u6bd4\u7684\u8bf4\u6cd5\u3002\u4e8c\u6218\u65f6\u671f\uff0c\u5fb7\u56fd\u7684\u864e\u5f0f\u3001\u8c79\u5f0f\u3001\u864e\u738b\u5766\u514b\u5236\u4f5c\u7cbe\u826f\u3001\u6027\u80fd\u5353\u8d8a\uff0c\u4f46\u4ecd\u7136\u88ab\u6027\u80fd\u4e0d\u5982\u7684\u82cf\u8054\u5766\u514b\u6d88\u706d\u3002\u7a76\u5176\u539f\u56e0\uff0c\u5fb7\u56fd\u5766\u514b\u6210\u672c\u592a\u9ad8\u3001\u5de5\u827a\u590d\u6742\u3001\u751f\u4ea7\u5de5\u65f6\u592a\u957f\uff0c\u800c\u82cf\u8054\u7684T-34\u5766\u514b\u6027\u80fd\u7565\u900a\uff0c\u4f46\u6210\u672c\u8f83\u4f4e\u3001\u5de5\u65f6\u77ed\uff0c\u64cd\u4f5c\u4e5f\u7b80\u5355\u3002\u62d6\u62c9\u673a\u5382\u6539\u9020\u4e4b\u540e\u5c31\u80fd\u751f\u4ea7\uff0c\u5de5\u4eba\u76f4\u63a5\u5c31\u53ef\u4ee5\u5f00\u4e0a\u6218\u573a\u3002\u8fd9\u79cd\u8bf4\u6cd5\u4e5f\u66fe\u4fa7\u9762\u5370\u8bc1\u4e86\u82cf\u8054\u519b\u5de5\u5bf9\u6027\u80fd\u3001\u4f7f\u7528\u3001\u6210\u672c\u5747\u8861\u7684\u8ffd\u6c42\u3002<\/p>\n<p>\u4e0d\u8fc7\uff0c\u4e8c\u6218\u4e4b\u540e\u7684\u82cf\u8054\u5766\u514b\uff0c\u540c\u6837\u5728\u6750\u6599\u548c\u5de5\u827a\u7b49\u6574\u4f53\u5de5\u4e1a\u6c34\u5e73\u5e76\u4e0d\u5360\u4f18\u7684\u60c5\u51b5\u4e0b\uff0c\u521b\u9020\u6027\u5730\u4f7f\u7528\u201c\u4e09\u660e\u6cbb\u201d\u88c5\u7532\u7ed3\u6784\uff0c\u5728\u5766\u514b\u88c5\u7532\u4e0a\u72ec\u9886\u98ce\u9a9a\u3002<\/p>\n<p>\u4ece\u5766\u514b\u8bde\u751f\u5230\u4e8c\u6218\u7ed3\u675f\uff0c\u4e16\u754c\u4e0a\u7684\u5766\u514b\u5927\u591a\u91c7\u7528\u5747\u8d28\u94a2\u88c5\u7532\u3002\u4f46\u572820\u4e16\u7eaa50\u5e74\u4ee3\uff0c\u805a\u80fd\u88c5\u836f\u7834\u7532\u5f39\u7684\u8bde\u751f\u548c\u5927\u89c4\u6a21\u5e94\u7528\uff0c\u5747\u8d28\u94a2\u88c5\u7532\u8d70\u5230\u4e86\u5c3d\u5934\u3002\u88c5\u5907\u4e86\u805a\u80fd\u88c5\u836f\u6218\u6597\u90e8\u7684\u53cd\u5766\u514b\u5bfc\u5f39\u548c\u706b\u7bad\u7b52\u7684\u7834\u7532\u80fd\u529b\u8fbe\u5230\u4e86300\u6beb\u7c73\u3002\u5982\u6b64\u4e00\u6765\uff0c\u5355\u7eaf\u4f9d\u9760\u589e\u52a0\u5747\u8d28\u94a2\u7684\u539a\u5ea6\uff0c\u5df2\u7ecf\u65e0\u6cd5\u62b5\u6297\u53cd\u5766\u514b\u6b66\u5668\uff0c\u56e0\u4e3a\u8fc7\u539a\u7684\u88c5\u7532\uff0c\u4f1a\u8ba9\u5766\u514b\u592a\u91cd\u5931\u53bb\u6218\u6597\u529b\u3002<\/p>\n<p>\u5728\u4e25\u5cfb\u7684\u5f62\u52bf\u4e0b\uff0c\u82cf\u8054\u94a2\u94c1\u7814\u7a76\u9662\u7740\u624b\u7814\u53d1\u65b0\u578b\u7684\u88c5\u7532\uff0c\u6253\u9020\u51fa\u4e00\u79cd\u201c\u94a2\uff0b\u5939\u5c42\u6750\u6599\uff0b\u94a2\u201d\u7684\u201c\u4e09\u660e\u6cbb\u201d\u88c5\u7532\u7ed3\u6784\u3002\u8fd9\u79cd\u65b0\u578b\u590d\u5408\u88c5\u7532\uff0c\u6bd4\u897f\u65b9\u590d\u5408\u88c5\u7532\u8db3\u8db3\u65e9\u4e86\u5341\u6765\u5e74\u3002<\/p>\n<p>\u4e09\u660e\u6cbb\u7684\u6838\u5fc3\u662f\u5939\u5c42\u6750\u6599\u3002\u4ed6\u4eec\u627e\u5230\u73bb\u7483\u7ea4\u7ef4\u3002\u73bb\u7483\u7ea4\u7ef4\u5f3a\u5ea6\u9ad8\u3001\u5bc6\u5ea6\u4f4e\u3001\u8010\u9ad8\u6e29\uff0c\u540c\u65f6\u5177\u6709\u51b2\u51fb\u97e7\u6027\u9ad8\u3001\u70ed\u7a33\u5b9a\u6027\u597d\u3001\u8010\u8150\u8680\u7b49\u4f18\u70b9\uff0c\u800c\u4e14\u4ef7\u683c\u4f4e\u5ec9\u3002<\/p>\n<p>\u56e0\u6b64\uff0c\u82cf\u8054T-64A\u5766\u514b\u8f66\u4f53\u9996\u4e0a\u88c5\u7532\u5c31\u91c7\u7528\u4e8680\u6beb\u7c73\u7684\u9ad8\u786c\u5ea6\u5408\u91d1\u94a2+105\u6beb\u7c73\u7684\u7845\u5316\u77f3\u82f1\u73bb\u7483\u7ea4\u7ef4+10\u6beb\u7c73\u7684\u542b\u94c5\u5185\u886c+20\u6beb\u7c73\u7684\u9ad8\u786c\u5ea6\u5408\u91d1\u94a2\u3002\u5e76\u4e14\u901a\u8fc7\u5b9e\u9a8c\u53d1\u73b0\uff0c\u590d\u5408\u88c5\u7532\u7684\u503e\u659c\u89d2\u5ea6\u548c\u590d\u5408\u5939\u5c42\u7684\u5bc6\u5ea6\u5bf9\u88c5\u7532\u9632\u62a4\u80fd\u529b\u6709\u5f88\u5927\u5f71\u54cd\u3002\u6700\u540e\uff0c\u4ed6\u4eec\u5c06\u88c5\u7532\u4ee522\u5ea6\u5927\u89d2\u5ea6\u94fa\u8bbe\uff0c\u4ee5\u8fbe\u5230\u6700\u4f73\u9632\u5fa1\u6548\u679c\u3002<\/p>\n<p>\u88c5\u5907\u8fd9\u79cd\u590d\u5408\u88c5\u7532\u7684T-64A\u5bf9\u7a7f\u7532\u5f39\u3001\u7834\u7532\u5f39\u3001\u788e\u7532\u5f39\u90fd\u6709\u5f88\u597d\u7684\u9632\u62a4\uff0cT-64A\u5bf9\u6297\u9ad8\u901f\u52a8\u80fd\u5f39\u548c\u7834\u7532\u5f39\u7684\u80fd\u529b\u53ef\u8fbe410\u6beb\u7c73\u548c500\u6beb\u7c73\u3002<\/p>\n<p>\u501f\u52a9\u8fd9\u79cd\u5148\u8fdb\u7684\u590d\u5408\u88c5\u7532\u7406\u5ff5\uff0c\u4f7f\u5f97T-64A\u53ef\u4ee5\u6452\u5f03\u539a\u91cd\u7684\u5747\u8d28\u94a2\u88c5\u7532\u300236.5\u5428\u7684\u91cd\u91cf\u4e0e\u4e2d\u578b\u5766\u514b\u76f8\u5f53\uff0c\u5374\u5177\u6709\u91cd\u578b\u5766\u514b\u7684\u706b\u529b\u548c\u9632\u62a4\u80fd\u529b\uff0c\u4ece\u800c\u6d88\u9664\u4e86\u4e2d\u578b\u5766\u514b\u548c\u91cd\u578b\u5766\u514b\u7684\u754c\u9650\uff0c\u4e00\u79cd\u65b0\u7684\u5766\u514b\u7c7b\u578b\u2014\u2014\u4e3b\u6218\u5766\u514b\u5212\u5206\u8bde\u751f\u3002<\/p>\n<p>\u800c\u540e\uff0c\u82cf\u8054\u5728\u6539\u8fdb\u578b\u7684T-64B\u5766\u514b\u4f7f\u7528\u4e86\u4ece\u5916\u5230\u5185\u662f\u9ad8\u786c\u5ea6\u5408\u91d1\u94a2+\u6c27\u5316\u94dd\u9676\u74f7\u7403+\u542b\u94c5\u7684\u7ea4\u7ef4\u677f+\u9ad8\u786c\u5ea6\u5408\u91d1\u94a2\u3002\u4f9d\u9760\u9676\u74f7\u548c\u7ea4\u7ef4\u7a7a\u9699\u963b\u9694\u6324\u538b\uff0c\u8fd9\u79cd\u590d\u5408\u88c5\u7532\u53ea\u9700200\u6beb\u7c73\u4ee578\u5ea6\u659c\u89d2\u5e03\u7f6e\uff0c\u5c31\u53ef\u4ee5\u8fbe\u5230\u7a7f\u7532\u5f39450\u6beb\u7c73\u3001\u7834\u7532\u5f39600\u6beb\u7c73\u7684\u9632\u5fa1\u80fd\u529b\u3002\u8fd9\u79cd\u9632\u62a4\u80fd\u529b\u8db3\u4ee5\u5bf9\u4ed8\u5f53\u65f6\u4e16\u754c\u4e0a\u6240\u6709\u7684\u53cd\u5766\u514b\u6b66\u5668\uff0c\u897f\u65b9\u5766\u514b\u5728\u8fd9\u4e00\u70b9\u4e0a\u96be\u4ee5\u671b\u5176\u9879\u80cc\u3002<\/p>\n<p>\u7ed3\u8bed\uff1a\u867d\u7136\u82cf\u8054\u66fe\u662f\u552f\u4e8c\u7684\u8d85\u7ea7\u5927\u56fd\uff0c\u4f46\u603b\u4f53\u7684\u5de5\u4e1a\u6c34\u5e73\u4e0d\u5982\u7f8e\u56fd\u3002\u4f46\u662f\uff0c\u82cf\u8054\u5728\u81ea\u5df1\u7684\u652f\u67f1\u4ea7\u4e1a\u519b\u5de5\u4e1a\u4e0a\u8d70\u51fa\u81ea\u5df1\u7684\u98ce\u683c\u3002\u4ed6\u4eec\u64c5\u957f\u5229\u7528\u73b0\u6709\u6210\u719f\u6750\u6599\u548c\u5de5\u827a\uff0c\u5229\u7528\u4f18\u79c0\u7684\u5de5\u7a0b\u80fd\u529b\uff0c\u5728\u8bbe\u8ba1\u4e0a\u5206\u6e05\u4e3b\u8981\u77db\u76fe\u6b21\u8981\u77db\u76fe\uff0c\u4e0d\u76f2\u76ee\u8ffd\u6c42\u9ad8\u5927\u4e0a\uff0c\u6253\u9020\u51fa\u5728\u6027\u80fd\u51fa\u4f17\u3001\u6210\u672c\u4f4e\u5ec9\u3001\u4f7f\u7528\u7b80\u5355\u7684\u4ea7\u54c1\u3002\u8fd9\u4e00\u70b9\uff0c\u503c\u5f97\u6211\u4eec\u5b66\u4e60\u3002<\/p>\n<p>\u53c2\u8003\u8d44\u6599<\/p>\n<p>\u65bd\u5f81, \u6797\u6960. \u4fc4\u7f57\u65af\u4e3b\u6218\u5766\u514b\u590d\u5408\u88c5\u7532\u89e3\u8bfb[J]. \u56fd\u5916\u5766\u514b, 2007(10):12-17.<\/p>\n<p>\u90ed\u6b63\u7965. \u4e16\u754c\u9996\u578b\u4e09\u4ee3\u5766\u514b\u95ee\u4e16\u2014\u2014\u82cf\u8054T-64\u4e3b\u6218\u5766\u514b\u7814\u5236\u6e0a\u6e90[J]. \u56fd\u5916\u5766\u514b, 2006(9).<\/p>\n<p>\u5c1a\u667a. \u65ad\u5251\u6467\u67aa \u5766\u514b\u88c5\u7532\u7684\u524d\u4e16\u4eca\u751f[J]. \u6d77\u9646\u7a7a\u5929\u60ef\u6027\u4e16\u754c, 2010(2):40-54.<\/p>\n<p>\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u63d0\u8d77\u82cf\u8054\u548c\u7ee7\u627f\u8005\u4fc4\u7f57\u65af\uff0c\u5f88\u591a\u4eba\u620f\u79f0\u201c\u6218\u6597\u79cd\u65cf\u201d\u3001\u201c\u6bdb\u5b50\u201d\u3001\u201c\u6bdb\u718a\u201d\u3002\u5b83\u7684\u5de5\u4e1a\u54c1\u4e5f\u5e38\u88ab\u5f88\u591a\u4eba\u770b\u4f5c\u7c97\u7ebf\u6761\u6216\u8005\u201c\u50bb\u5927\u9ed1\u201d\uff0c\u8fd8\u662f\u7cbe\u81f4\u7684\u5fb7\u56fd\u8d27\u3001\u7f8e\u56fd\u8d27\u66f4\u5165\u201c\u6cd5\u773c\u201d\u3002\u8bda\u7136\uff0c&#8230;<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[4],"tags":[34,14],"class_list":["post-28188","post","type-post","status-publish","format-standard","hentry","category-ganhuo","tag-history","tag-lightweight"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/28188"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=28188"}],"version-history":[{"count":11,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/28188\/revisions"}],"predecessor-version":[{"id":28220,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/28188\/revisions\/28220"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=28188"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=28188"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=28188"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}